Method and apparatus for producing cannabinoid granules that are soluble in a substantially aqueous environment

Convective drying methods like spray granulation in a fluidization device improve cannabinoid granule absorption and bioavailability by forming stable, homogeneous emulsions, addressing issues of non-uniformity and low bioavailability in existing cannabinoid formulations.

JP7576606B2Active Publication Date: 2024-10-31ADD ADVANCED DRUG DELIVERY TECH LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2022500676
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-07-26
Filing Date
2020-06-23
Publication Date
2024-10-31
Estimated Expiration
2040-06-23

AI Technical Summary

Technical Problem

Existing cannabinoid solid dosage forms have non-homogeneous particle size distribution, limited flowability, and low bioavailability due to poor absorption by the body.

Method used

Cannabinoid granules are produced through convective drying, specifically spray granulation or spray encapsulation in a fluidization device, forming a stable emulsion with improved absorption and bioavailability by reducing emulsion particle size and enhancing homogeneity.

Benefits of technology

The method results in cannabinoid granules with enhanced absorption and bioavailability, improved flowability, and uniform particle size, suitable for packaging and formulation into tablets or capsules.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007576606000001
    Figure 0007576606000001
  • Figure 0007576606000002
    Figure 0007576606000002
  • Figure 0007576606000003
    Figure 0007576606000003
Patent Text Reader

Abstract

The present invention relates to a method and apparatus (1) for producing cannabinoid granules that dissolve in a substantially aqueous environment, wherein a matrix liquid is produced from a first liquid that dissolves the cannabinoid, or from a first liquid that dissolves the cannabinoid, a second liquid that forms an emulsion with the first liquid, and the cannabinoid dissolved in the first liquid or emulsion, and the matrix liquid is convectively dried, the apparatus (1) comprising a container system (2) having an inlet (5, 6, 11, 12) and a matrix liquid outlet (14) for producing the matrix liquid, and a dryer in fluid connection with the matrix liquid outlet (14) of the container system (2).
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for producing cannabinoid granules soluble in a substantially aqueous environment, wherein the matrix liquid is produced from a first liquid that dissolves the cannabinoid or from a first liquid that dissolves the cannabinoid and a second liquid that forms an emulsion with the first liquid and the cannabinoid dissolved in the first liquid or emulsion.

[0002] The present invention further relates to an apparatus for producing cannabinoid granules that are soluble in a substantially aqueous environment. [Background technology]

[0003] Methods and devices for producing, particularly oral dosage forms of cannabinoids, have long been part of the prior art.

[0004] WO02 / 064109A2 (Patent Document 1) discloses a pharmaceutical formulation for use in administering a fat-soluble drug to a mucosal surface. In particular, a pharmaceutical formulation for use in administering a fat-soluble drug to a mucosal surface is provided, which forms an emulsion upon hydration, and which contains a fat-soluble drug, in particular a drug comprising a specific combination of cannabinoids in a predetermined ratio as active substances, which can adhere to the mucosal surface and allow for a controlled release of the drug.

[0005] US2016 / 0143972A1 (Patent Document 2) discloses a method for producing a solid dosage form of a cannabinoid, which is substantially soluble in an aqueous solution. The method includes dissolving a cannabinoid and one or more emulsifiers in one or more solvents to obtain one or more combined solutions, and drying the one or more solvents from the combined solutions containing the one or more solvents to obtain a solid dosage form of the cannabinoid.

[0006] The drawback of the solid dosage forms of cannabinoids mentioned in the prior art is that they do not exhibit sufficient systemic absorption and therefore low bioavailability of the cannabinoids due to the not very homogeneous particle size distribution of the solid dosage forms and also due to the poor flowability of the solid dosage forms, when administered orally, in some cases. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] WO02 / 064109A2 [Patent Document 2] US2016 / 0143972A1 Summary of the Invention [Problem to be solved by the invention]

[0008] The object of the present invention is therefore to expand the scope of application for the user and to increase the systemic absorption of cannabinoids, thereby improving their bioavailability, and at the same time improving the flowability of solid dosage forms of cannabinoids. [Means for solving the problem]

[0009] This problem is solved in the above-mentioned type of method by convective drying of the matrix liquid. Preference is given to spray drying the matrix liquid or drying it in a fluidizer by spray granulation, spray agglomeration or spray encapsulation under convection to cannabinoid granules. Surprisingly, it has been found that in the case of convective drying of the matrix liquid containing the cannabinoid by spray granulation, spray agglomeration or spray encapsulation in a fluidizer, in particular in a spouted bed or fluidized bed apparatus, a stable emulsion of the first and second liquid is formed by redissolving the cannabinoid granules in an aqueous environment, in which the absorption of the cannabinoid is significantly improved and therefore a more optimal bioavailability is ensured. The improved absorption and more optimal bioavailability of the cannabinoid results from more homogeneous and smaller emulsion particles (oil-in-water droplets) after redissolving the cannabinoid granules in an aqueous environment compared to the emulsion particles (oil-in-water droplets) contained in the matrix liquid before convective drying in a fluidizer. The dissolution behavior of the granules in an aqueous environment is also improved compared to conventional products such as pellets (Pressling).In addition, unexpectedly, a reduction in the average diameter x and equivalent diameter was observed after convective drying in a fluidizer.The cannabinoid granules can be very well packed into stick packs or compressed into tablets or further processed into capsules.

[0010] The conversion products and synthetic analogues of some terpene phenols are referred to as cannabinoid(s). Endogenous substances with similar pharmacological properties to cannabinoid(s), so-called endocannabinoid(s), and substances from plants other than the cannabis plant that have similar or the same action as cannabinoids, so-called phytocannabinoid(s), are also referred to as cannabinoid(s) in this case. For example, cannabinoids can include one or more of cannabidiol (CBD), cannabinol (CBN), and Δ9-tetrahydrocannabinol (THC), etc.

[0011] According to one development of the method in this respect, the cannabinoid is first dissolved in a first liquid, which is then mixed with a second liquid to form an emulsion.

[0012] Additionally, in one aspect of this method, the first liquid and the second liquid are first mixed to form an emulsion, and then the cannabinoid is dissolved in the emulsion.

[0013] The first liquid is preferably from the group of lipids, alcohols, oils, and / or any mixtures thereof.The selection of the first liquid is very important for the absorbability of cannabinoids, for example, in the human digestive tract.At the same time, the selection of the first liquid is also important in terms of possible taste masking.Here, oils, for example orange oil, are considered in particular.

[0014] More preferably, the second liquid is an aqueous solution or water.

[0015] In one very advantageous form of the method, the first liquid is an oil or a mixture of different oils, in particular rapeseed oil, orange oil or coconut oil, and / or an alcohol or a mixture of different alcohols, in particular ethanol, preferably with a purity of >80%, and the second liquid is water, thus an oil-in-water emulsion or an alcoholic solution.

[0016] Auxiliaries for producing and stabilizing emulsions are called emulsifiers, which are preferably surface-active substances that help to mix two mutually immiscible liquids, such as oil and water, into a finely dispersed mixture, the so-called emulsion, and to stabilize this emulsion.

[0017] According to one advantageous variant of the method, an emulsifier is added to the second liquid before it is mixed with the first liquid.

[0018] According to a further advantageous variant of the process, an emulsifier is added to the emulsion before convective drying.

[0019] Additionally, an emulsifier is added to the matrix liquid, preferably prior to convective drying.

[0020] The addition of one emulsifier or of several emulsifiers also has the advantage that the first and second liquids are finely dispersed in the emulsion, which also makes it possible to produce a matrix liquid that is better suited for convection drying in a convection dryer, for example a drum dryer, a vacuum dryer or especially a fluidizing device, preferably a spouted bed device or a fluidized bed device. The addition of the emulsifier or emulsifiers, for example Hi-Cap 100 (modified starch) or similar, is preferably carried out with stirring, preferably using a stirring device or similar, and / or under the effect of temperature, i.e. while supplying or extracting heat.

[0021] Furthermore, according to an additional advantageous embodiment of the method, the matrix liquid is homogenized before convective drying. The emulsion is preferably homogenized at high pressure, particularly preferably at a pressure between 50 bar and 250 bar, particularly preferably at a pressure between 100 bar and 200 bar, most preferably at a pressure between 125 bar and 175 bar. This homogenization significantly reduces the average diameter of the droplets of the first liquid present in the emulsion, so that the mixture of the first and second liquids that are not dissolved in each other becomes more homogenous, i.e. more uniform. By homogenization, especially high pressure homogenization, a matrix liquid is generated that is optimized for convective drying, especially in a fluidizer.

[0022] It is advantageous to apply the matrix liquid onto one or more carrier materials before convective drying, especially in a fluidizer.Preferably, the matrix liquid is applied onto one or more carrier materials before convective drying, so that wet granules containing cannabinoids are produced simultaneously with the compaction of the carrier materials.Preferably, the matrix liquid is applied onto one or more carrier materials before extrusion, or the matrix liquid is applied onto one or more carrier materials before pelletization.

[0023] According to a further advantageous embodiment of the method, carrier particles are provided in the fluidizer. Carrier particles, in particular maltrodextrin, mannitol, cellulose, lactose, xylitol or mixtures thereof, are used as nuclei for forming the cannabinoid granules. The matrix liquid is partially evaporated, resulting in spray-dried granulation nuclei consisting of the matrix liquid itself.

[0024] It is advantageous to add additives to the solution, emulsion or matrix liquid before convection drying.The taste masking of the cannabinoid granules can be achieved by adding additives, especially carbohydrates such as maltrodextrin, starch, sugars such as fructose or saccharose, salts such as magnesium stearate, flavorings, or the like.In addition, additives can be applied when the compressibility of the cannabinoid granules must be adapted, for example when producing tablets, or when the release profile of the cannabinoid is to be adapted.

[0025] According to a preferred variant of the process, the process is carried out batchwise or continuously. By varying the installation and process parameters, the desired end product properties, such as particle size distribution, dissolution rate, bulk density or residual moisture, can be individually and optimally adjusted.

[0026] Furthermore, in the above mentioned type of device, the above problem is solved in that the device comprises a container system for producing a matrix liquid, having an inlet and a matrix liquid outlet, and a convection dryer fluidly connected to the matrix liquid outlet of the container system. It is preferred that the convection dryer is configured as a spray drying device, as a drum dryer, as a vacuum dryer or as a fluidizing device. Surprisingly, it has been found that in the case of convection drying of a matrix liquid containing cannabinoids by spray granulation, spray agglomeration or spray encapsulation in a fluidizing device, in particular a spouted bed device or a fluidized bed device, by redissolving the cannabinoid granules in an aqueous environment, a stable emulsion of the first and second liquid is formed, in which the absorption of the cannabinoid is significantly improved and thus a more optimal bioavailability is ensured. The improved absorption and more optimal bioavailability of the cannabinoids result from more homogeneous and smaller emulsion particles (oil-in-water droplets) after redissolving the cannabinoid granules in an aqueous environment, for example obtained by spraying the matrix liquid onto the carrier particles and drying, especially by thin film drying, compared to the emulsion particles (oil-in-water droplets) contained in the matrix liquid before convection drying, preferably before convection drying in a fluidizer.In addition, unexpectedly, a decrease in the average diameter x and equivalent diameter after convection drying in a fluidizer was confirmed.The cannabinoid granules can be very well packed into stick packs and can be administered directly into the mouth or into a glass of liquid, or can be compressed into tablets or further processed into capsules.

[0027] According to an advantageous embodiment of the device, the fluidizer is configured as a spouted bed device or as a fluidized bed device, which, in comparison with a fluidized bed device, for example, allows atomization with a very low filling weight, and also the high shear forces in the spraying area, on the one hand, favor the formation of a uniform liquid film and, on the other hand, minimize the tendency to agglomeration.

[0028] Advantageously, the container system comprises one or more containers. Preferably, the containers are at least partially fluidly connected to one another. Particularly preferably, the device comprises a first container for the first liquid, a second container for the second liquid, and a container for the emulsion. It is especially preferred that the container for the emulsion corresponds to the first or second container. This ensures a simple production of the matrix liquid, even if the starting materials are to be processed separately.

[0029] According to a further advantageous variant of the preferred device, the convection dryer, preferably the fluidizer, is equipped with a nozzle for atomizing the emulsion or solution. The nozzle, preferably the two-fluid nozzle, is preferably configured to spray droplets with a droplet diameter between 1 μm and 200 μm, preferably between 10 μm and 100 μm, particularly preferably between 20 μm and 60 μm. The droplets to be sprayed have a droplet diameter of 25 μm to 40 μm, most preferably 30 μm. The adjustment of the droplet diameter by the nozzle and the compressed air fed into the nozzle allows the shear forces occurring during spraying to be precisely adjusted, so that a very homogeneous droplet diameter of the emulsion or solution to be sprayed can be obtained or achieved. The droplets are added to carrier particles, for example cellulose, lactose or xylitol, and preferably a thin-film evaporation takes place. This thin-film evaporation results in a very homogeneous evaporation of the emulsion or solution on the carrier particles.

[0030] According to an advantageous variant of the device, a homogenizer is arranged between the vessel system and the dryer, preferably the fluidizer, for homogenizing the matrix liquid. This homogenization significantly reduces the average diameter of the first liquid present in the emulsion, which makes the mixture of the first and second liquids that are not dissolved in each other more homogeneous, i.e. more uniform. Due to the homogenization, especially the high-pressure homogenization, a matrix liquid is generated that is optimized for convective drying, especially in a fluidizer.

[0031] In a further preferred development of the apparatus, a granulation unit for granulating the matrix liquid is arranged between the container system and the dryer, preferably a wet mixer, particularly preferably a high shear granulator, vertical granulator, rotor disk granulator or the like. According to a related development of the apparatus, an extruder for extruding the granules is arranged after the granulation unit.

[0032] It is preferred that the homogenizer and / or the granulating unit and / or the extruder are fluidly connected to each other.

[0033] According to a further advantageous embodiment of the device, the inlet and the matrix liquid outlet are formed as one container system opening. The advantage of such an embodiment of the inlet and the matrix liquid outlet is the structurally simple dissolution and the relatively easy sealing.

[0034] The invention will now be explained in more detail with reference to the accompanying drawings. [Brief description of the drawings]

[0035] [Figure 1] FIG. 1 is a schematic diagram of a first exemplary embodiment of a preferred apparatus for producing cannabinoid granules that are soluble in a substantially aqueous environment. [Diagram 2] FIG. 2 is a schematic diagram of a second exemplary embodiment of a preferred apparatus for producing cannabinoid granules that are soluble in a substantially aqueous environment. [Diagram 3] 1 shows the cumulative and density distribution curves of oil droplets (rapeseed oil was used) of an oil-in-water emulsion before drying in a spouted bed apparatus. [Figure 4] FIG. 1 shows the cumulative and density distribution curves of oil droplets (rapeseed oil was used) in an oil-in-water emulsion after dissolving cannabinoid granules dried in a spouted bed apparatus in water. [Diagram 5]1 shows the cumulative and density distribution curves of oil droplets (using coconut oil) of an oil-in-water emulsion before drying in a spouted bed apparatus. [Figure 6] FIG. 1 shows the cumulative and density distribution curves of oil droplets (using coconut oil) in an oil-in-water emulsion after dissolving cannabinoid granules dried in a spouted bed apparatus in water. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0036] FIG. 1 shows a schematic diagram of a first exemplary embodiment of a preferred apparatus 1 for producing cannabinoid granules that are soluble in a substantially aqueous environment.

[0037] The device 1 comprises a container system 2 for producing a matrix liquid. In the exemplary embodiment according to Fig. 1, the container system 2 comprises three containers 3 which are fluidly connected to one another. The fluid connection of the containers 3 is realized here by means of pipes 4.

[0038] The first container 3a of the container system 2, which is formed with a double wall for heating or cooling, is provided with a cannabinoid inlet 5 and a liquid inlet 6 for a first liquid consisting of the group of lipids, alcohols, oils and / or any mixtures thereof, but particularly preferably consisting of rapeseed oil, orange oil or coconut oil.

[0039] Due to the vessel jacket space 9 extending between the vessel inner wall 7 and the vessel outer wall 8, the first vessel 3a can be temperature regulated by means of a heat transfer medium flowing through the vessel jacket space 9. It is preferable to heat the vessel 3a in order to better dissolve the cannabinoids which are possibly not well soluble in the first liquid. A temperature regulation device is not necessarily required.

[0040] Moreover, the first vessel 3a is provided with a motor-driven stirring device 10 for stirring the first liquid. A stirring device is not necessarily required.

[0041] For a second liquid, in particular an aqueous solution or water, the container system 2 comprises a second container 3 b having a liquid inlet 11 .

[0042] The first and second containers 3a, 3b are each connected to an inlet 12 of a third container 3c via a pipe 4. The first liquid containing cannabinoids and the second liquid are transported into the third container 3c via the pipe 4, for example by using a pump.

[0043] In the third vessel 3c, the first liquid containing cannabinoids and the second liquid are mixed together to form an emulsion, producing a matrix liquid, which is preferably produced under stirring using a motor-driven stirring device 13 in the third vessel 3c. The produced matrix liquid leaves the vessel system 2 for producing matrix liquid via a matrix liquid outlet 14.

[0044] The matrix liquid can also be produced by different partial steps, for example by mixing all the components at once in only one container.

[0045] The matrix liquid is conveyed, e.g., by a pump, via line 15 into a homogenizer 16, preferably a high pressure homogenizer, for homogenizing the matrix liquid. The homogenized matrix liquid is then conveyed, e.g., by a pump, from the homogenizer 16 via line 17 into a fluidizer 18.

[0046] In the exemplary embodiment of Figure 1, the dryer is formed as a fluidizer 18 for producing cannabinoid granules soluble in a substantially aqueous environment, which is formed here as a spouted bed apparatus 19. The structure of the spouted bed apparatus 19 comprises, from bottom to top, a diffusion chamber 20, a process space 21, an expansion zone 22 and an exhaust section 23.

[0047] The process gas 24 required for drying the cannabinoid granules to be produced is supplied to the diffusion chamber 20, where it diffuses and enters the process space 21 via a slit opening 25 and a process gas deflector 26, preferably as a sort of free jet.

[0048] Furthermore, the machine cross section of the expansion zone 22 can optionally be enlarged, which causes the process gas flow velocity to decrease upwards. The process gas 24 preferably leaves the spouted bed apparatus 19 as exhaust gas 28 which has been purified by a dust removal system 27, in particular by filter cartridges or textile filter elements.

[0049] In the process space 21, there are carrier particles, referred to as starting material, e.g. mannitol, cellulose, xylitol or similar, which are carried away by the process gas 24 upwards in the direction of the dust removal system 27. In the upper region of the process space 21 and in the expansion zone 22 above, the process gas velocity decreases so that the upwardly flowing carrier particles are forced to leave the process gas flow to the side and fall back into the process space 21. The lower region of the process space 21 is delimited by an inclined side surface 28, which causes the carrier particles to be carried under the action of gravity through a reflux zone 29 in the direction of the slit opening 25, where they are subsequently carried away by the process gas 24 again into the process space 21.

[0050] By this mechanism a very uniform solid circulation 30 of the support particles is created. In the lower region of the process space 21 one or more spraying devices 31, preferably spray nozzles or the like, are arranged, which are used to spray and introduce the matrix liquid upwards in the same direction as the process gas 24. Such introduction of the matrix liquid in the lower region of the process space 21 is called bottom spray.

[0051] The nozzle, preferably a two-fluid nozzle, is configured to spray droplets with a droplet diameter between 1 μm and 200 μm, preferably between 10 μm and 100 μm, particularly preferably between 20 μm and 60 μm. The droplets sprayed have a droplet diameter of 25 μm to 40 μm, most preferably 30 μm. The adjustment of the droplet diameter by the nozzle and the compressed air pumped into the nozzle allows the shear forces occurring during spraying to be precisely adjusted, so that a very homogeneous droplet diameter of the sprayed emulsion or solution can be obtained or achieved. The droplets are added to carrier particles, such as cellulose, lactose or xylitol, and preferably thin-film evaporation occurs.

[0052] Due to the very favorable heat and mass transfer in the spraying area 32 of the process space 21 of the spouted bed apparatus 19 and the high carrier particle circulation, most of the matrix liquid is deposited on the carrier particles, which achieves a uniform wetting of the particle surfaces of the carrier particles. This uniform wetting, in the case of a simultaneous high particle circulation between the spraying area 32 and the reflux zone 29, results in the formation of a very uniform thin liquid film on the carrier particles. Due to the drying process, the matrix liquid evaporates and leaves the spouted bed apparatus 19 together with the exhaust gas 28. The cannabinoids contained in the matrix liquid remain on the particle surfaces of the carrier particles, so that the resulting cannabinoid granules grow very evenly and homogeneously.

[0053] The discharge 33 of the cannabinoid granules can be achieved, for example, by an overflow or by a metered discharger, in particular a rotary valve, or even by a gravity separator, preferably a zigzag separator or a riser tube separator into which a separation gas is fed.

[0054] A mechanical assembly 34, such as a grinder, chopper, etc., may be arranged in the process space 21, preferably in the reflux zone 29, if necessary, to generate by grinding particles fine enough to serve as granulation nuclei for the granulation process.

[0055] In the process space 21 or in the machine parts above it, in the expansion zone 22 and in the exhaust 23, one or more spraying devices 35 can optionally be arranged, which preferably spray downwards. A liquid matrix liquid can likewise be injected into the process space 21 of the spouted bed apparatus 19 via the spraying devices 35. Alternatively, additives 36 or further components 37 in liquid form can be sprayed via some of the spraying devices 31, 35 and thus homogeneously embedded in the granule structure.

[0056] In the preferred apparatus 1, a granulation unit (not shown) for granulating the matrix liquid can be arranged between the vessel system 2 and the fluidizer 18 configured as a spouted bed apparatus 19. In addition to this, an extruder for extruding the granules can be arranged after the granulation unit. The homogenizer 16 and / or the granulation unit and / or the extruder are preferably fluidly connected to one another.

[0057] In FIG. 2, a schematic diagram of a second exemplary embodiment of a preferred apparatus 1 for producing cannabinoid granules that are soluble in a substantially aqueous environment is shown.

[0058] The device 1 comprises a container system 2 for producing a matrix liquid. In a second exemplary embodiment according to FIG.

[0059] The double-walled container 3 of the container system 2 for heating or cooling is provided with a cannabinoid inlet 5, a liquid inlet 6 for a first liquid from the group of lipids, alcohols, oils and / or any mixtures thereof, but particularly preferably rapeseed oil, orange oil or coconut oil, and a liquid inlet 11 for a second liquid, in particular an aqueous solution or water.

[0060] Due to the vessel jacket space 9 extending between the vessel inner wall 7 and the vessel outer wall 8, the first vessel 3a can be temperature regulated by means of a heat transfer medium flowing through the vessel jacket space 9. It is preferable to heat the vessel 3a in order to better dissolve the cannabinoids, which may not be well soluble in the first liquid. A temperature regulation device is not necessarily required.

[0061] Moreover, the first vessel 3a is provided with a motor-driven stirring device 10 for stirring the first liquid. A stirring device is not necessarily required.

[0062] In the vessel 3, the first liquid containing cannabinoids is mixed with the second liquid, whereby the first and second liquids form an emulsion together to produce a matrix liquid. This matrix liquid is preferably produced under stirring using a motor-driven stirring device 13 in the vessel 3. The produced matrix liquid leaves the vessel system 2 for producing matrix liquid via a matrix liquid outlet 14. The inlets 5, 6, 11 and the matrix liquid outlet 14 are formed as one vessel system opening 38 in this exemplary embodiment.

[0063] The matrix liquid is conveyed, e.g., by a pump, via line 15 into a homogenizer 16, preferably a high pressure homogenizer, for homogenizing the matrix liquid. The homogenized matrix liquid is then conveyed, e.g., by a pump, from the homogenizer 16 via line 17 into a fluidizer 18.

[0064] The further convective drying process using a fluidizer is carried out corresponding to the first exemplary embodiment described in FIG.

[0065] Additionally, the produced cannabinoid granules can be coated, for example in a drum coater, which has the advantage that the cannabinoid granules can be provided with, for example, a gastric juice-resistant coating or taste masking.

[0066] Below, examples are given for the production of a matrix liquid and its further processing in a fluidizer. EXAMPLES

[0067] Example 1 The production of cannabinoid granules in a fluidizer configured as a spouted bed apparatus was carried out in a batch or batch operation with bottom spray mode.

[0068] 500 g of mannitol was used as starting material in the fluidizer.

[0069] The matrix liquid has 200g Hi-Cap 100, 200g maltrodextrin, 1365g water, 5g cannabidiol (CBD), and 50g rapeseed oil. In this case, cannabidiol (CBD) was dissolved in rapeseed oil as a first liquid, and maltrodextrin and Hi-Cap 100 were dissolved in water as a second liquid. Then, the rapeseed oil containing CBD and the water containing maltrodextrin and Hi-Cap 100 were mixed together to form an emulsion, thereby producing a matrix liquid. In this case, maltrodextrin and Hi-Cap 100 are used as additives to form a matrix structure in the matrix liquid.

[0070] The spray rate was selected between 10 and 15 g / min. The produced cannabinoid granules were well dissolved in water, where they formed a stable oil-in-water emulsion. The residual moisture of the cannabinoid granules was 1.8%.

[0071] The matrix liquid was analyzed following its preparation by a laser diffraction system Cilas 1190 LD (Quantachrome). The particle size of the CBD-containing oil droplets present in the matrix liquid emulsion is shown in Figure 3. The cumulative distribution curve is the equivalent diameter x 10 = 1.17 μm, x 50 = 7.97 μm, and x 90= 18.37 μm, and the average diameter x = 8.87 μm. In addition, the density distribution curve shows a bimodal distribution with two peaks.

[0072] Cannabinoid granules were prepared and redissolved in water to form a stable oil-in-water emulsion in an aqueous environment.

[0073] The cannabinoid granules, which are soluble in an aqueous environment, were dissolved in water and the particle size of the CBD-containing oil droplets was analyzed again by the laser diffraction system Cilas 1190 LD (Quantachrome). Figure 4 shows this analysis. In this case, the cumulative distribution curve is 10 = 0.82 μm, x 50 = 2.33 μm, and x 90 = 6.26 μm, showing an average diameter x = 3.01 μm. In addition, the density distribution curve shows a unimodal distribution. The oil droplets show a very homogeneous density distribution, with a clearly smaller diameter. This results in a clearly improved absorption of CBD and therefore a more optimal bioavailability of CBD. This improved absorption of cannabinoids results from more homogeneous and smaller emulsion particles.

[0074] Example 2 The production of cannabinoid granules in a fluidizer configured as a spouted bed apparatus was carried out in a batch or batch operation with bottom spray mode.

[0075] As starting materials in the fluidizer, 250 g mannitol and 250 g maltrodextrin were used, ie in a 1:1 ratio.

[0076] The matrix liquid has 200g Hi-Cap 100, 200g maltrodextrin, 1417g water, 5.5g cannabidiol (CBD), and 51g coconut oil. In this case, cannabidiol (CBD) was dissolved in coconut oil as a first liquid, and maltrodextrin and Hi-Cap 100 were dissolved in water as a second liquid. Then, coconut oil containing CBD and water containing maltrodextrin and Hi-Cap 100 were mixed together to form an emulsion, thereby producing a matrix liquid. In this case, maltrodextrin and Hi-Cap 100 are used as additives to form a matrix structure in the matrix liquid.

[0077] The spray rate was increased compared to Example 1. In addition, the volumetric flow rate of the process air was reduced to minimize product losses in the filter. The cannabinoid granules produced were well soluble in water, where they formed a stable oil-in-water emulsion. The residual moisture of the cannabinoid granules was 3.4%.

[0078] The matrix liquid was analyzed following its preparation by a laser diffraction system Cilas 1190 LD (Quantachrome). The particle size of the CBD-containing oil droplets present in the matrix liquid emulsion is shown in Figure 5. The cumulative distribution curve is the equivalent diameter x 10 = 1.18 μm, x 50 = 6.99 μm, and x 90 = 15.17 μm, and the average diameter x = 7.58 μm. In addition, the density distribution curve shows a bimodal distribution with two peaks.

[0079] Cannabinoid granules were prepared and redissolved in water to form a stable oil-in-water emulsion in an aqueous environment.

[0080] The cannabinoid granules, which are soluble in an aqueous environment, were dissolved in water and the particle size of the CBD-containing oil droplets was analyzed again by the laser diffraction system Cilas 1190 LD (Quantachrome). Figure 6 shows this analysis. In this case, the cumulative distribution curve is 10 = 0.90 μm, x 50 = 2.48 μm, and x 90 = 6.24 μm, showing an average diameter x = 3.08 μm. In addition, the density distribution curve shows a unimodal distribution. The oil droplets show a very homogeneous density distribution, with a clearly smaller diameter. This results in a clearly improved absorption of CBD and therefore a more optimal bioavailability of CBD. This improved absorption of cannabinoids results from more homogeneous and smaller emulsion particles. In addition, the present application relates to the invention described in the claims, but may also include the following as other aspects. 1. A method for producing cannabinoid granules soluble in a substantially aqueous environment, wherein the matrix liquid is produced from a first liquid that dissolves the cannabinoid or from a first liquid that dissolves the cannabinoid, a second liquid that forms an emulsion with said first liquid and the cannabinoid dissolved in said first liquid or in said emulsion, characterized in that the matrix liquid is convectively dried. 2. The method according to claim 1, characterized in that the matrix liquid is spray-dried or dried in a fluidizer (18) by spray granulation, spray agglomeration or spray encapsulation into cannabinoid granules under convection. 3. The method according to claim 1 or 2, wherein the cannabinoid is first dissolved in the first liquid, and then the first liquid is mixed with the second liquid to form an emulsion. 4. The method according to claim 1 or 2, characterized in that the first liquid and the second liquid are first mixed to form an emulsion, and then the cannabinoid is dissolved in the emulsion. 5. A method according to any one of 1 to 4 above, characterized in that the first liquid is comprised in the group consisting of lipids, alcohols, oils and / or any mixture thereof. 6. The method according to any one of 1 to 5 above, wherein the second liquid is an aqueous solution or water. 7. The method according to any one of 1 to 6 above, wherein an emulsifier is added to the second liquid before mixing with the first liquid. 8. The method according to any one of 1 to 7 above, characterized in that an emulsifier is added to the emulsion before convective drying. 9. The method according to any one of 1 to 7 above, characterized in that an emulsifier is added to the matrix liquid before convective drying. 10. The method according to any one of claims 1 to 9, characterized in that the matrix liquid is homogenized prior to convective drying. 11. The method according to claim 10, characterized in that the emulsion is high-pressure homogenized, preferably at a pressure between 50 bar and 250 bar, particularly preferably at a pressure between 100 bar and 200 bar, and especially preferably at a pressure between 125 bar and 175 bar. 12. The method according to any one of claims 1 to 11, characterized in that the matrix liquid is applied onto one or more support materials prior to convective drying in a fluidizer (18). 13. The method according to claim 12, characterized in that the matrix liquid is applied onto one or more carrier materials and then extruded. 14. The method according to claim 12, characterized in that the matrix liquid is applied onto one or more carrier materials and then pelletized. 15. The method according to any one of claims 1 to 11, characterized in that carrier particles are provided in a fluidizer (18). 16. The method according to any one of 1 to 15 above, characterized in that an additive (36) is added to the solution, emulsion or matrix liquid before convective drying. 17. The method according to any one of 1 to 16 above, characterized in that the method is carried out batchwise or continuously. 18. An apparatus (1) for producing cannabinoid granules soluble in a substantially aqueous environment as described in any one of 1 to 17 above, characterized in that the apparatus (1) comprises a container system (2) having an inlet (5, 6, 11, 12) and a matrix liquid outlet (14) for producing the matrix liquid, and a convection dryer fluidly connected to the matrix liquid outlet (14) of the container system (2). 19. The device (1) according to claim 18, characterized in that the convection dryer is configured as a spray drying device, as a drum dryer, as a vacuum dryer or as a fluidization device (18). 20. Apparatus (1) according to claim 18 or 19, characterized in that the fluidizer (18) is configured as a spouted bed apparatus (19) or as a fluidized bed apparatus. 21. The device (1) described in any one of claims 18 to 20, characterized in that the container system (2) has one or more containers (3, 3a, 3b, 3c). 22. The device (1) according to claim 21, characterized in that a plurality of containers (3, 3a, 3b, 3c) are at least partially fluidly connected to each other. 23. Apparatus (1) according to claim 21 or 22, characterized in that the apparatus has a first container (3a) for the first liquid, a second container (3b) for the second liquid and a container (3c) for the emulsion. 24. Apparatus (1) according to claim 23, characterized in that the container (3c) for emulsion corresponds to the first or second container (3a, 3b). 25. The apparatus (1) described in any one of the above items 18 to 24, characterized in that the fluidizer (18) is equipped with a nozzle for atomizing the emulsion or solution. 26. The device (1) described in claim 25, characterized in that the nozzle, preferably a two-fluid nozzle, is configured to spray droplets having a diameter between 1 μm and 200 μm, preferably between 10 μm and 100 μm, particularly preferably between 20 μm and 60 μm. 27. The apparatus (1) described in any one of the above items 18 to 26, characterized in that a homogenizer (16) for homogenizing the matrix liquid is disposed between the container system (2) and the fluidization device (18). 28. The apparatus (1) according to any one of claims 18 to 27, characterized in that a granulation unit for granulating the matrix liquid, preferably a high shear granulator, vertical granulator or rotor disc granulator, is arranged between the container system (2) and the dryer (18). 29. The apparatus (1) described in claim 28, characterized in that an extruder for extruding the granules is arranged after the granulation unit. 30. The apparatus (1) according to any one of claims 27 to 29, characterized in that the homogenizer (16) and / or the granulation unit and / or the extruder are fluidly connected to each other. 31. The device (1) described in any one of claims 18 to 30, characterized in that the inlet (5, 6, 11, 12) and the matrix liquid outlet (14) are formed as one container system opening (38).

Claims

1. 1. A method for producing cannabinoid granules soluble in a substantially aqueous environment, wherein a matrix liquid is produced from a first liquid that dissolves the cannabinoid, a second liquid that forms an emulsion with said first liquid, and the cannabinoid dissolved in said first liquid or in said emulsion, characterized in that the matrix liquid is dried into cannabinoid granules by spray granulation, spray agglomeration or spray encapsulation in a fluidizer (18) under convection.

2. 2. The method of claim 1, wherein the cannabinoid is first dissolved in the first liquid, and then the first liquid is mixed with the second liquid to form an emulsion.

3. 2. The method of claim 1, wherein the first liquid and the second liquid are first mixed to form an emulsion, and then a cannabinoid is dissolved in the emulsion.

4. The method according to any one of claims 1 to 3, characterized in that the first liquid is comprised in the group of lipids, alcohols, oils and / or any mixtures thereof.

5. The method according to any one of claims 1 to 4, characterized in that the second liquid is an aqueous solution or water.

6. The method according to any one of claims 1 to 5, characterized in that an emulsifier is added to the second liquid before mixing with the first liquid.

7. The method according to any one of claims 1 to 6, characterized in that an emulsifier is added to the emulsion before convective drying.

8. The method according to any one of claims 1 to 6, characterized in that an emulsifier is added to the matrix liquid before convective drying.

9. The method according to any one of claims 1 to 8, characterized in that the matrix liquid is homogenized before convective drying.

10. 10. The method according to claim 9, characterized in that the emulsion is high pressure homogenized at a pressure between 50 bar and 250 bar.

11. The method according to any one of claims 1 to 10, characterized in that the matrix liquid is applied onto one or more support materials prior to convective drying in a fluidizer (18).

12. 12. The method according to claim 11, characterized in that the matrix liquid is applied onto one or more carrier materials and then extruded.

13. 12. The method according to claim 11, characterized in that the matrix liquid is pelletized after being applied onto one or more carrier materials.

14. The method according to any one of claims 1 to 10, characterized in that the carrier particles are provided in a fluidizer (18).

15. The method according to any one of the preceding claims, characterized in that an additive (36) is added to the solution, emulsion or matrix liquid prior to convective drying.

16. The process according to any one of claims 1 to 15, characterized in that the process is carried out batchwise or continuously.

17. Use of an apparatus (1) for producing cannabinoid granules soluble in a substantially aqueous environment according to any one of claims 1 to 16, comprising: The device (1) comprises a container system (2) having one or more containers (3), the container system (2) having a cannabinoid inlet (5), a liquid inlet (6) for a first liquid consisting of the group of lipids, alcohols, oils and / or any mixtures thereof, a liquid inlet (11) for a second liquid and a matrix liquid outlet (14), characterized in that it further comprises a dryer formed as a convection fluidizer (18) in fluid connection with the matrix liquid outlet (14) of the container system (2). The above uses.

18. 18. Use according to claim 17, characterized in that the fluidizer (18) is designed as a spouted bed apparatus (19) or as a fluidized bed apparatus.

19. 18. Use according to claim 17, characterised in that a plurality of containers (3, 3a, 3b, 3c) are at least partially fluidly connected to one another.

20. 20. Use according to claim 19, characterised in that the device (1) comprises a first container (3a) for the first liquid, a second container (3b) for the second liquid and a container (3c) for the emulsion.

21. 21. Use according to claim 20, characterised in that the container (3c) for emulsion corresponds to the first or second container (3a, 3b).

22. Use according to any one of claims 17 to 21, characterised in that the fluidiser (18) is equipped with a nozzle for atomising the emulsion or solution.

23. 23. Use according to claim 22, characterised in that the nozzle is adapted to spray droplets with a droplet diameter between 1 μm and 200 μm.

24. Use according to any one of claims 17 to 23, characterised in that a homogeniser (16) for homogenising the matrix liquid is arranged between the container system (2) and the fluidiser (18).

25. Use according to any one of claims 17 to 24, characterised in that a granulation unit for granulating the matrix liquid is arranged between the container system (2) and the fluidizer (18).

26. 26. Use according to claim 25, characterised in that the granulation unit is a high shear granulator, a vertical granulator or a rotor disc granulator.

27. 27. Use according to claim 25 or 26, characterised in that the granulation unit is followed by an extruder for extruding the granules.

28. Use according to any one of claims 24 to 27, characterised in that the homogenizer (16) and / or the granulating unit and / or the extruder are fluidly connected to each other.

29. An emulsifier is added to the second liquid prior to mixing with the first liquid, or an emulsion formed from the first liquid and the second liquid, in which the cannabinoid is dissolved in the first solution or emulsion, has an emulsifier added to it prior to convective drying in a fluidizer (18), or an emulsifier is added to the matrix liquid prior to convective drying in a fluidizer (18), and The matrix liquid is applied onto one or more support materials prior to convective drying in a fluidizer (18) or support particles are provided in the fluidizer (18). Use according to any one of claims 17 to 28.

Citation Information

Patent Citations

  • Powder treating apparatus

    JP2000334288A

  • Compositions with cannabinoids

    JP2001526221A

  • Method for producing coated bioactive particle

    JP2002219349A

  • mononuclear filled microcapsules

    JP2005525093A

  • Granule, tablet, and method for producing the same

    JP2012072190A