Stacked III-V semiconductor diode
The stacked III-V semiconductor diode with a GaAs cathode and anode layers and optimized dopant profiles addresses high voltage resistance and switching efficiency challenges, achieving high cut-off voltages and low resistance.
Patent Information
- Application Number
- JP2022017432
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-02-08
- Filing Date
- 2022-02-07
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2042-02-07
AI Technical Summary
Existing stacked III-V semiconductor diodes face challenges in achieving high voltage resistance with low on-resistance and capacitance, particularly in GaAs-based devices.
A stacked III-V semiconductor diode configuration with a GaAs cathode and anode layer, a drift region, and a delta layer section in the cathode layer, combined with a lightly doped second section and optional transition layer, to enhance dopant concentration profiles for improved switch-off behavior and reduced series resistance.
The configuration enables diodes with high cut-off voltages above 1100 V, low on-resistance, and low capacitance per unit area, enhancing the switching behavior and efficiency.
Smart Images

Figure 0007576802000001 
Figure 0007576802000002 
Figure 0007576802000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a stacked III-V semiconductor diode including or consisting of GaAs, comprising a heavily n-doped cathode layer, a heavily p-doped anode layer, and a drift region disposed between the cathode and anode layers. [Background technology]
[0002] Gallium arsenide p + -nn + A high-voltage resistant semiconductor diode with the structure is known from pages 8 and 9 of "GaAs Power Devices" by German Ashkinazi, ISBN 965-7094-19-4.
[0003] Other stacked III-V semiconductor diodes are known from EP 3321971 and EP 3321970, in which the semiconductor diode has an additional intermediate layer between the drift region and the cathode or anode. Summary of the Invention [Problem to be solved by the invention]
[0004] Against this background, the object of the present invention is to provide a device which advances the prior art. [Means for solving the problem]
[0005] This problem is solved by a stacked III-V semiconductor diode which has the features of claim 1. Advantageous embodiments of the invention are the subject of the dependent claims.
[0006] In accordance with the subject matter of the present invention, a stacked III-V semiconductor diode includes or consists of GaAs having a heavily n-doped cathode layer and a heavily p-doped anode layer.
[0007] Between the cathode and anode layers, there is a maximum of 8 × 10 15 cm -3 and a layer thickness of at least 10 μm. Preferably, the total layer thickness of the drift region is at most 50 μm or at most 100 μm.
[0008] The cathode layer has a first section and a second section.
[0009] The first section is configured as a delta layer section having a layer thickness of 0.1 μm to 1 μm, or 0.1 μm to 2 μm.
[0010] The delta layer section is at least 1×10 19 cm -3 or at least 2×10 19 cm -3 The dopant concentration is
[0011] It is self-evident that all semiconductor layers of a semiconductor diode consisting of or including GaAs, i.e. in particular the cathode layer, the anode layer and the drift region, respectively, consist of or at least include GaAs, in other words, each semiconductor layer of a III-V semiconductor diode has at least the elements Ga and As.
[0012] Furthermore, it is self-evident that a pn junction is formed within the drift region.
[0013] It should be noted that the semiconductor layers of the semiconductor diode are configured in a stacked manner on top of one another. The semiconductor layers preferably have the same area. Preferably, one of the semiconductor layers is configured as or includes a substrate layer. In one development, the substrate layer has a larger area than the stack of semiconductor layers arranged on the substrate layer.
[0014] The substrate layer preferably has a thickness of 50 μm to 120 μm or 50 μm to 250 μm. In one development, the substrate layer has a thickness of 1×10 17 cm -3 From 2 × 10 18 cm -3 Up to or 8×10 18 cm -3 The concentrations range from
[0015] The semiconductor layers are preferably epitaxially grown one on top of the other. Particularly preferably, the cathode or anode layer is constituted by a substrate layer on which all other semiconductor layers are epitaxially grown in sequence. Alternatively, the layers are joined by means of wafer bonding.
[0016] It is furthermore self-evident that the semiconductor diode preferably has further layers made of other materials, in particular metallic connection contact layers.
[0017] Furthermore, it should be noted that the term anode is used synonymously with the term anode layer, and the term cathode is used synonymously with the term cathode layer.
[0018] The connecting contact layer, for example, consists completely or partly of a metal, for example gold, or of a metal alloy and is produced, for example, by means of electron beam evaporation or by means of sputtering.
[0019] In order to achieve the lowest possible resistance of electrical contact and to keep the series resistance or power losses of the semiconductor diode as small as possible, the regions of the cathode and anode layers in contact with the connection contact layer preferably have a higher dopant concentration than the respective remaining parts of the cathode and anode layers.
[0020] At least, the relatively small thickness, i.e. preferably less than 1 μm, makes it possible to impart a very high doping concentration, in particular of at least 1×10 19 cm-3 The object of the present invention is to produce a doping of the cathode layer with good layer quality. In this respect, suitable dopants, in particular for the cathode layer, are, for example, tellurium or selenium.
[0021] Correspondingly, the thickness of the second section of the cathode layer essentially follows the lifetime or penetration depth of the minority charge carriers, i.e. holes. Typically, a thickness of a few hundred nanometers up to a maximum of 2 μm is sufficient for the second layer.
[0022] In other words, the thickness of the second section of the cathode layer is preferably as large as the free path length of the minority charge carriers, ie holes, in the cathode.
[0023] Furthermore, the delta layer section forms a sort of barrier for minority charge carriers and reduces the connection resistance, which in particular improves the switch-off behavior and therefore the switching behavior of the diode.
[0024] Tests have shown that the combination of a thin but very highly doped delta layer section with a more lightly doped second section of the cathode layer can improve the emitter efficiency, and therefore the efficiency of the cathode.
[0025] In combination with a lightly doped drift region, diodes can be made with particularly high blocking voltages of more than 1100 V or even more than 1200 V, small on-resistance and particularly small capacitance per unit area.
[0026] In one embodiment, the cathode layer has a second layer section having a dopant concentration lower than the dopant concentration of the delta layer section, whereby the delta layer section complements the typical cathode layer with a delta doping peak, so to speak.
[0027] The delta layer section preferably has a materially bonded connection to a second metallic connection contact, in other words a metallic connection contact which is arranged on the top surface of the cathode layer.
[0028] A first metallic connection contact is provided on the underside of the anode layer. Preferably, the two metallic connection contacts cover the anode layer and / or the cathode layer in the central region or almost completely or completely in order to achieve a low connection resistance. Even in the case of complete coverage, it is self-evident that the surrounding edge portion is not metallized in order to increase the process reliability.
[0029] In one development, the second layer section of the cathode layer has a lower dopant concentration than the delta layer section. Preferably, the second layer section of the cathode layer has a layer thickness D greater than the delta layer section. K2 has.
[0030] Preferably, the second layer section of the cathode layer has a thickness of at least 0.5 μm and up to 1.5 μm, or at least 0.5 μm and up to 2.5 μm, or at least 0.5 μm and up to 5 μm.
[0031] It should be noted that the terms doping and dopant concentration are used interchangeably. mosquito It should be noted that the change in doping between the second section of the cathode layer is preferably abrupt, in other words the doping preferably varies within a thickness range of less than 0.1 μm or less than 0.05 μm.
[0032] The dopant concentration of the second layer section of the cathode layer is 1×10 19 cm -3 Preferably, the dopant concentration of the second layer section of the cathode layer is less than 1×10 18 cm -3 or 2×10 18 cm -3 or 5×1018 cm -3 It exceeds.
[0033] In one development, the cathode layer has a transition layer section that is arranged between the second section of the cathode layer and the drift region and has a layer thickness of at least 3 μm, a doping that is less than the doping of the second section and more than the doping of the drift region, and a doping concentration profile that drops convexly or concavely or linearly or stepwise in the direction of the drift region.
[0034] In another embodiment, the delta layer section has Te and / or Se as dopants.
[0035] The invention will be explained in more detail below with reference to the drawings, in which like parts are provided with the same reference numerals, and in which the illustrated embodiments are largely schematic, i.e. the spacings as well as the lateral and vertical lengths are not to scale and, unless expressly stated, have no derivable geometrical relationship to one another. [Brief description of the drawings]
[0036] [Figure 1] 1 is a diagram showing a first embodiment of a stacked III-V semiconductor diode. [Diagram 2] 1 is a diagram showing a first embodiment of a dopant concentration profile of a III-V semiconductor diode; [Diagram 3] FIG. 13 shows another embodiment of a stacked III-V semiconductor diode. [Figure 4] FIG. 13 shows yet another embodiment of a stacked III-V semiconductor diode. [Diagram 5] FIG. 13 shows yet another embodiment of a stacked III-V semiconductor diode. [Figure 6] FIG. 4 is a diagram showing another embodiment of a dopant concentration profile. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0037] In the diagram of Figure 1, a diagram of a first embodiment of a stacked III-V semiconductor diode 10 having or consisting of GaAs is shown. A The heavily doped p-doped substrate layer having a thickness of D constitutes the anode layer 12. D The drift region 14 is followed by a highly n-doped layer having a thickness D K A cathode layer 16 having a
[0038] It is obvious that a pn junction is formed in the drift region 14 .
[0039] The cathode layer 16 has a first section 16.1 and a second section 16.2.
[0040] The first section 16.1 of the cathode layer 16 has a thickness of at least 1×10 19 cm -3 or at least 2×10 19 cm -3 with extremely high dopant concentrations of 0.1 μm to 1 μm or small layer thicknesses D of 0.1 μm up to 2 μm K1 and a delta layer section having
[0041] The second layer section 16.2 has a lower dopant concentration and a larger layer thickness D than the delta layer section 16.1. K2 And, it has.
[0042] The second layer section 16.2 of the cathode layer 16 has a thickness in the range of 0.5 μm to 1.5 μm, or in the range of 0.5 μm to 2.5 μm, or in the range of 0.5 μm to 5 μm.
[0043] The dopant concentration of the second layer section 16.2 is 1×10 19 cm -3 The dopant concentration of the second layer section 16.2 is preferably less than 1×10 18 cm -3 or 2×1018 cm -3 or 5×10 18 cm -3 It exceeds.
[0044] On the underside of the anode layer 12 a metallic connection contact M1 is arranged, or on the upper side of the cathode layer 16 a metallic connection contact M2 is arranged.
[0045] The two metallic connection contacts M1, M2 preferably almost completely cover the anode layer 12 and / or the cathode layer 16 in order to achieve a low connection resistance. The delta layer section 16.1 preferably also has a material-bonded connection with the metallic connection contact M2.
[0046] In the diagram of FIG. 2, the dopant concentration profile along the thickness of a stacked III-V semiconductor diode 10 is shown and plotted in relation to FIG.
[0047] Plotted is dopant concentration D versus position x along the stack of group III-V semiconductor diode 10.
[0048] The dopant concentration profile is plotted against the thickness D of each of the two sections 16.2 and 16.1 of the cathode layer 16. K2 and D. K1 16.2 and 16.3, respectively, so that a dopant concentration jump is formed between the second layer section 16.2 and the delta layer section.
[0049] The dopant concentration is then increased to a maximum of 8×10 15 cm -3 At the transition from the drift region 14 to the anode layer the dopant concentration abruptly increases to a constant high level of p-dopant concentration.
[0050] The dopant concentration along the anode 12 is constant and the height of the dopant concentration is less than the dopant concentration in the second region 16.2 of the cathode 16.
[0051] In the illustrated embodiment, the drift region has a low and substantially constant dopant concentration. The doping along the entire layer thickness varies between n-dopants and p-dopants, thereby forming a pn junction in the drift region 14.
[0052] In the embodiment shown in FIG. 3, the metallic connection contacts M1 and M2 are configured as flat surfaces.
[0053] The cathode layer 16 has a transition layer section 16.3 in addition to a first section 16.1 and a second section 16.2. The transition layer section 16.3 has a layer thickness D of at least 3 μm and, for example, at most 10 μm or at most 5 μm. K3 has.
[0054] The transition layer section 16.3 of the cathode layer 16 has a doping that is less than the doping of the second section 16.2 of the cathode layer 16 and is higher than the doping of the drift region 14.
[0055] The concentration profile of the doping falling in the transition layer section 16.3 towards the drift region 14 can be designed as a convex or concave, linear or step-like.
[0056] In the embodiment of Fig. 4, the two metallic connection layers M1, M2 cover only the central part of the anode or cathode, respectively. The transition layer section 16.3 is not constructed, so that the second section 16.2 of the cathode continues directly to the drift region 14.
[0057] In the embodiment shown in FIG. 5, the cathode layer 16 comprises a transition layer section 16.3 in addition to the second layer section 16.2.
[0058] Between the drift region 14 and the second section 12.2 of the anode layer 12, a p-doped transition layer section 12.3 is configured as part of the anode layer 12.
[0059] The dopant concentration in the anode transition layer section 12.3 increases along the layer thickness of the transition layer section 12.3 in the direction of the second section 12.2 of the anode layer 12. The doping increase is configured concave or convex or linear or stepwise.
[0060] In the diagram of Figure 6 the dopant concentration course is plotted for the embodiment described in connection with Figure 5. In the following only the differences with respect to the embodiment of Figure 2 will be described.
[0061] The delta layer section 16.1 of the cathode layer 16 is arranged on the side of the second layer section 16.2 facing away from the drift region 14, so that the dopant concentration along the cathode layer drops abruptly in the direction of the drift region 14.
[0062] Between the second section 16.2 of the cathode layer 16 and the drift region 14, a transition layer section 16.3 is again configured as part of the cathode layer 16.
[0063] The dopant concentration of the transition layer section 16.3 of the cathode layer 16 decreases in the subsequent course in the direction of the drift region 14.
[0064] Between the drift region 14 and the second section 12.2 of the anode layer 12, a p-doped transition layer section 12.3 is configured as part of the anode layer 12. The dopant concentration of the transition layer section 12.3 of the anode layer 12 increases in the course of the process in the direction of the second section 12.2 of the anode layer 12.
Claims
1. A stacked III-V semiconductor diode (10) containing GaAs or consisting of GaAs, the stacked III-V semiconductor diode (10) comprising: a heavily n-doped cathode layer (16); a highly p-doped anode layer (12); Between the cathode layer (16) and the anode layer (12), up to 8×10 15 cm -3 and a layer thickness (D D ) and a drift region (14) having In a stacked III-V group semiconductor diode (10) having said cathode layer (16) having a first section (16.1) and a second section (16.2); The first section (16.1) has a layer thickness (D K1 ) and configured as a delta layer section having at least 1×10 19 cm-3 dopant concentration, the second section (16.2) has a lower dopant concentration than the first section (16.1), the dopant concentration of the second section (16.2) being less than 1×10 18 cm -3 the second section (16.2) being higher and being arranged between the first section (16.1) and the drift region (14); the anode layer (12) has a first section (12.1) and a second section (12.2) arranged between the first section (12.1) and the drift region (14), the dopant concentration of the second section (12.2) being lower than the dopant concentration of the first section (12.1) or the dopant concentration of the second section (12.2) being equal to the dopant concentration of the first section (12.1); A stacked III-V semiconductor diode (10).
2. the delta layer section (16.1) is in contact with a metallic cathode contact layer (M1), The stacked III-V semiconductor diode (10) of claim 1.
3. the change in doping between the delta layer section (16.1) and the second section (16.2) of the cathode layer is effected in a stepwise manner; A stacked III-V semiconductor diode (10) according to claim 1 or 2.
4. The second section (16.2) of the cathode layer (16) has a thickness of 1×10 19 cm -3 Lower than and 2×10 18 cm -3 having a dopant concentration greater than A stacked III-V semiconductor diode (10) according to any one of claims 1 to 3.
5. The second section (16.2) of the cathode layer (16) has a layer thickness (D K2 ) A stacked III-V semiconductor diode (10) according to any one of claims 1 to 4.
6. The cathode layer (16) has a transition layer section (16.3) that is arranged between the second section (16.2) and the drift region (14) and has a layer thickness (D K3 ), the transition layer section (16.3) has a lower dopant concentration than the second section (16.2) and a higher dopant concentration than the drift region (14), the dopant concentration profile of the transition layer section (16.3) having a convex or concave or linear or stepwise drop in the direction of the drift region (14). A stacked III-V semiconductor diode (10) according to any one of claims 1 to 5.
7. The dopant concentration of the first section (12.1) of the anode layer (12) is at least 8×10 17 cm -3 And a maximum of 8 x 10 18 cm -3 and the dopant concentration of the second section of the anode layer (12) is at least 1×10 17 cm -3 And a maximum of 8 x 10 17 cm -3 That is, A stacked III-V semiconductor diode (10) according to any one of claims 1 to 6.
8. the anode layer (12) has a transition section (12.3) bordering the drift region (14), the transition section (12.3) having a dopant concentration profile that drops convexly or concavely or linearly or stepwise in the direction of the drift region (14), the dopant concentration being higher than the dopant concentration of the p-doped drift region and lower than the dopant concentration of the second section (12.2) of the anode layer (12), A stacked III-V semiconductor diode (10) according to any one of claims 1 to 7.
9. the second section (12.2) of the anode layer (12) has a lower doping than the second section (16.2) of the cathode layer (16); A stacked III-V semiconductor diode (10) according to any one of claims 1 to 8.
10. The delta layer section (16.1) has Te or Se as a dopant. A stacked III-V semiconductor diode (10) according to any one of claims 1 to 9.
11. the change in doping between the delta layer section (16.1) and the second section (16.2) of the cathode layer is effected within a thickness range of less than 0.1 μm; The stacked III-V semiconductor diode (10) of claim 3.
12. the drift region (14) having a substantially constant dopant concentration; A stacked III-V semiconductor diode (10) according to any one of claims 1 to 11.
Citation Information
Patent Citations
Fast recovery epitaxial diode (FRED) and preparation method thereof
CN103178120A
Deep pn junction power semiconductor device
DE102011006675A1
Semiconductor device and manufacture thereof
JP1991155125A
MANUFACTURING METHOD OF n-InGaAs SEMICONDUCTOR AND GROUP III-V COMPOUND SEMICONDUCTOR DEVICE
JP2005032928A
Epitaxial wafer for transistor
JP2012164753A