Wafer processing method

By employing a protective member and translucent film on the wafer, the method addresses internal stress-related cracks, ensuring high-quality chip division and ease of handling in laser processing.

JP7578451B2Active Publication Date: 2024-11-06DISCO CORP
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2020170100
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-10-07
Publication Date
2024-11-06
Estimated Expiration
2040-10-07

AI Technical Summary

Technical Problem

The formation of modified layers on both the front and back sides of wafers during laser processing leads to internal stress, causing unintended cracks and deteriorating the quality of device chips, especially as chip sizes decrease to 1 mm x 1 mm or less, making it difficult to handle the chips after processing.

Method used

A method involving the use of a protective member on the front side and a translucent film on the back side of the wafer, followed by laser irradiation through the film to form modified layers, and subsequent removal of the film before applying an external force to divide the wafer into chips, using a grinding device to thin the back side.

Benefits of technology

Reduces unintended cracks and maintains chip quality by suppressing internal stress, allowing easier handling and transport of wafers post-processing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007578451000001
    Figure 0007578451000001
  • Figure 0007578451000002
    Figure 0007578451000002
  • Figure 0007578451000003
    Figure 0007578451000003
Patent Text Reader

Abstract

To provide a method for working a wafer, which reduces a crack occurring from a modified layer that is formed on a rear face side.SOLUTION: A method includes: a protective member arranging step of arranging a protective tape T1 on a surface 10a of the wafer; a light transmissive film arranging step of arranging a light transmissive film TA on a rear face 10b of the wafer; a chuck table keeping step of keeping a protective member side of the wafer, on a chuck table 27; a first modified layer forming step of forming a modified layer 150, by positioning a focused light spot of a laser beam LB having such a wavelength as to transmit through the wafer, on an inner surface side of the wafer through the light transmissive film, and irradiating the wafer along a scheduled division line; a second modified layer forming step of forming a modified layer 160, by positioning the focused light spot of the laser beam, on an inner rear face side of the wafer through the light transmissive film, and irradiating the wafer along the scheduled division line, after the first modified layer forming step; and a dividing step of removing the light transmissive film from the rear face of the wafer, applying an external force to the modified layer, and dividing the wafer into individual device chips.SELECTED DRAWING: Figure 6
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a wafer processing method for dividing a wafer into individual device chips. [Background technology]

[0002] Wafers, on whose surface multiple devices such as ICs and LSIs are formed, are divided along division lines. These are then separated into individual device chips using a dicing machine or laser processing machine. These are then used in electrical devices such as mobile phones and personal computers.

[0003] A technique has been proposed for dividing a wafer into individual device chips using a laser processing device, in which a focal point of a laser beam having a wavelength that is transparent to the wafer is positioned inside the intended division line from the back surface of the wafer and irradiated to form a continuous modified layer inside the intended division line, and then an external force is applied to divide the wafer into individual device chips (see, for example, Patent Document 1). [Prior art documents] [Patent documents]

[0004] In addition, in order to facilitate division of the wafer, the present application proposes a technique for forming a modified layer on the front side of the interior of the wafer and also on the back side (see Patent Document 2).

[0005] [Patent Document 1] Patent No. 3408805 [Patent Document 2] JP 2008-131008 A Summary of the Invention [Problem to be solved by the invention]

[0006] According to the technology described in the above-mentioned Patent Document 2, by forming modified layers on the front and back sides, the wafer is prevented from curving, and the wafer can be efficiently divided into individual device chips, which is a recommended processing method.

[0007] However, as the size of device chips becomes smaller, such as 1 mm x 1 mm or less, internal stress in the modified layer formed on the front side of the wafer can cause unintended cracks to occur in the modified layer formed on the back side, resulting in a deterioration in the quality of the separated device chips and making it difficult to remove them from the laser processing equipment.

[0008] The present invention has been made in consideration of the above-mentioned facts, and its main technical object is to provide a wafer processing method that reduces cracks from a modified layer formed on the back side, does not result in a deterioration in the quality of the separated device chips, and can facilitate removal from a laser processing apparatus. [Means for solving the problem]

[0009] In order to solve the above-mentioned main technical problem, according to the present invention, there is provided a wafer processing method for dividing a wafer having a surface on which a plurality of devices are partitioned by dividing lines into individual device chips, the method comprising the steps of: providing a protective member on the surface of the wafer; providing a light-transmitting film on the back surface of the wafer; holding the protective member side of the wafer on a chuck table; and positioning a focal point of a laser beam having a wavelength that is transparent to the wafer through the light-transmitting film. a first modified layer forming step of forming a modified layer by positioning the focal point of a laser beam on the front side of the interior of the wafer and irradiating the laser beam along the planned dividing lines, after the first modified layer forming step, positioning the focal point of a laser beam on the back side of the interior of the wafer through the light-transmitting film and irradiating the laser beam along the planned dividing lines, to form a modified layer; and a dividing step of removing the light-transmitting film from the back side of the wafer and applying an external force to the modified layer formed along the planned dividing lines to divide the wafer into individual device chips. The dividing step includes holding the front side of the wafer via the protective member on a chuck table constituting a grinding device, removing the light-transmitting film from the back side of the wafer, grinding the back side of the wafer to thin it, and dividing the wafer into individual device chips.A method for processing a wafer is provided.

[0010] The light-transmitting film disposing step is preferably any one of a step of disposing the light-transmitting film by thermocompression bonding a polyolefin film to the back surface of the wafer, a step of disposing the light-transmitting film by applying a water-soluble liquid resin to the back surface of the wafer and solidifying it, and a step of attaching an adhesive tape to the back surface of the wafer to dispose the light-transmitting film. , applicable After carrying out the dividing step, it is preferable to carry out a frame supporting step in which the wafer is positioned in a frame having openings for accommodating the wafer divided into individual device chips, a dicing tape is attached to the back surface of the wafer and the frame, and the wafer is disposed in the frame via the dicing tape. Effect of the Invention

[0011] The wafer processing method of the present invention is a wafer processing method for dividing a wafer having a surface on which a plurality of devices are partitioned by division lines into individual device chips, the method including a protective member providing step of providing a protective member on the surface of the wafer, a light-transmitting film providing step of providing a light-transmitting film on the back surface of the wafer, a chuck table holding step of holding the protective member side of the wafer on a chuck table, and a focusing step of a laser beam having a wavelength that is transparent to the wafer, the focusing point of the laser beam being focused on the wafer through the light-transmitting film. a first modified layer forming step of irradiating a laser beam along the planned dividing line by positioning the focal point of the laser beam on the front side inside the wafer (c) and forming a modified layer; a second modified layer forming step of irradiating a laser beam along the planned dividing line by positioning the focal point of the laser beam on the back side inside the wafer (c) through the light-transmitting film and forming a modified layer after the first modified layer forming step; and a dividing step of removing the light-transmitting film from the back side of the wafer and applying an external force to the modified layer formed along the planned dividing line to divide the wafer into individual device chips. The dividing step includes holding the front side of the wafer via the protective member on a chuck table constituting a grinding device, removing the light-transmitting film from the back side of the wafer, grinding the back side of the wafer to thin it, and dividing the wafer into individual device chips.Therefore, even when the modified layer is formed on the front side and the back side, the internal stress is suppressed by the light-transmitting film disposed on the back side, and the occurrence of unintended cracks from the modified layer formed on the back side can be reduced, and the deterioration of the quality of the device chips generated by the division step is prevented. Furthermore, even if the wafer is unintendedly cracked, the wafer is sandwiched between the protective tape and the light-transmitting film, which has the effect of facilitating the removal of the wafer after the modified layer is formed. [Brief description of the drawings]

[0012] [Figure 1] FIG. 11 is a perspective view showing an embodiment of a protective member disposing step. [Diagram 2] 1A to 1C are perspective views showing first to third examples of the embodiment of the light-transmitting film providing step. [Diagram 3] 1 is an overall perspective view of a laser processing apparatus suitable for this embodiment; [Figure 4] FIG. 11 is a perspective view showing an embodiment of a chuck table holding step. [Diagram 5] 4A and 4B are a perspective view and a partially enlarged cross-sectional view showing an embodiment of a first modified layer forming step. [Figure 6] 1A and 1B are a perspective view and a partially enlarged cross-sectional view showing an embodiment of a second modified layer forming step. [Figure 7] FIG. 13 is a perspective view showing a mode of carrying a wafer into a grinding device that performs a dividing step. [Figure 8] FIG. 13 is a perspective view showing an embodiment of a dividing step. [Figure 9] FIG. 13 is a perspective view showing an embodiment of a frame support step. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, an embodiment of a wafer processing method according to the present invention will be described in detail with reference to the accompanying drawings.

[0014] In carrying out the wafer processing method of this embodiment, as shown in Fig. 1, a wafer 10 is prepared in which a plurality of devices 12 are partitioned by planned division lines 14 and formed on a surface 10a. The wafer 10 is, for example, a silicon wafer, and the thickness of the wafer 10 before processing is 710 µm, and the target finishing thickness is 50 µm. Furthermore, the devices 12 to be individually divided are set to have dimensions of 1 mm x 1 mm in a plan view. Note that in Fig. 1, the dimensions of the devices 12 are drawn larger than they actually are for convenience of explanation, and are not in accordance with the actual dimensional ratio.

[0015] Once the above-mentioned wafer 10 is prepared, a protective member disposing step is performed in which a protective tape T1 is disposed as a protective member on the front surface 10a of the wafer 10, as shown in FIG. 1. More specifically, the protective tape T1 can be, for example, an EVA (ethylene-vinyl acetate copolymer) film with an adhesive layer disposed on its front surface, and is attached to the front surface 10a of the wafer 10 to form an integral unit, as shown in FIG. 1. Once the wafer 10 and the protective tape T1 are integrated, they are turned over in preparation for the next step, with the back surface 10b of the wafer 10 facing upward. The protective tape T1 is not limited to the above-mentioned EVA film, and may be, for example, a PET (polyethylene terephthalate) film.

[0016] As described above, after the protective member providing step is performed, a light-transmitting film providing step is performed in which a light-transmitting film is provided on the back surface 10b of the wafer 10. The light-transmitting film in this embodiment is made of a material that includes transparent and semi-transparent materials and transmits the laser beam LB irradiated in the first and second modified layer forming steps described below. An embodiment of the light-transmitting film providing step will be described in more detail with reference to FIG. 2.

[0017] FIG. 2(1) shows an embodiment of a first example of the light-transmitting film disposing step. In the first example, for example, a polyolefin film T2 is prepared as the light-transmitting film. The polyolefin film T2 is formed to the same dimensions as the wafer 10 and placed on the back surface 10b of the wafer 10. No adhesive layer is formed on the surface of the polyolefin film T2, and the film is not stuck as it is. Therefore, a thermocompression roller 100 shown by a two-dot chain line is prepared on the lower side of FIG. 2(1). The thermocompression roller 100 is provided with a heating means for heating the surface of the thermocompression roller 100 to a predetermined temperature, and the surface is coated with a fluororesin. The heating means is operated, and the thermocompression roller 100 is pressed from above the polyolefin film T2, rotated in the direction indicated by the arrow R1, and moved in the direction indicated by the arrow R2. The predetermined temperature is preferably set to 120° C. to 140° C. when a polyethylene sheet is selected as the polyolefin film T2, 160° C. to 180° C. when a polypropylene sheet is selected, and 220° C. to 240° C. when a polystyrene sheet is selected. Each of the above temperatures is a temperature close to the melting temperature of each sheet, and by setting such a temperature, the polyolefin film T2 exerts its adhesive force without excessive melting, and the polyolefin film T2 is satisfactorily thermocompression-bonded to the back surface 10b of the wafer 10 as the light-transmitting film TA.

[0018] FIG. 2(2) shows an embodiment of a second example of the light-transmitting film disposing step. In the second example, in order to dispose a light-transmitting film on the back surface 10b of the wafer 10, the wafer 10 is transported to a spin coater (not shown), and the back surface 10b of the wafer 10 is placed on the chuck table of the spin coater with the back surface 10b facing upward and held by suction. Next, as shown in the figure, a nozzle 112 of a water-soluble liquid resin supplying means 110 is positioned above the center of the wafer 10, and a predetermined amount of molten water-soluble liquid resin L, for example, polyvinyl alcohol (PVA), is dropped from the nozzle 112 while the wafer 10 is rotated in the direction indicated by the arrow R3. The dropped water-soluble liquid resin L spreads evenly on the back surface 10b of the wafer 10 by centrifugal force, and solidifies after a predetermined time has passed, and a PVA film T3 is disposed as the light-transmitting film TA. The water-soluble liquid resin L is not limited to PVA, but may be selected from other water-soluble liquid resins such as polyvinylpyrrolidone (PVP).

[0019] Further, FIG. 2(3) shows an embodiment of a third example of the light-transmitting film disposing step. In this third example, an EVA film T4 made of an adhesive tape, for example, having an adhesive layer on its surface, is adopted as the light-transmitting film. The EVA film T4 is first placed on the back surface 10b of the wafer 10 as shown in FIG. 2(3). Next, as shown on the lower side of the figure, a pressure-fitting roller 120 shown by a two-dot chain line is positioned on the EVA film T4 and pressed from above, and while rotating in the direction shown by the arrow R4, it is moved in the direction shown by the arrow R5, so that the EVA film T4 as the light-transmitting film TA is attached to the back surface 10b of the wafer 10 to be integrated. The adhesive tape is not limited to the above-mentioned EVA, and may be PET, as in the case of the above-mentioned protective tape T1.

[0020] As described above, after the light-transmitting film disposing step is performed and the light-transmitting film TA (any of the polyolefin film T2, PVA film T3, and EVA film T4) is disposed on the back surface 10b of the wafer 10, the wafer 10 is transported to the laser processing apparatus 1 shown in Fig. 3. The outline of the laser processing apparatus 1 will be described below with reference to the figure.

[0021] 3 shows an overall perspective view of the laser processing apparatus 1 according to the present embodiment. The laser processing apparatus 1 includes a base 2, a frame 3, a laser beam application means 4, an imaging means 5, a holding means 20 for holding a wafer 10 as a workpiece, a moving means 30 for moving the holding means 20, and a control means (not shown).

[0022] The holding means 20 includes a rectangular X-axis direction movable plate 21 mounted on the base 2 so as to be movable in the X-axis direction indicated by the arrow X in the figure, a rectangular Y-axis direction movable plate 23 mounted on the X-axis direction movable plate 21 so as to be movable in the Y-axis direction indicated by the arrow Y in the figure, a cylindrical support 24 fixed to the upper surface of the Y-axis direction movable plate 23, and a rectangular cover plate 25 fixed to the upper end of the support 24. A disk-shaped chuck table 27 extending upward through a long hole 26 is disposed on the cover plate 25, and the chuck table 27 is configured to be rotatable by a rotation drive means (not shown). A holding surface 28 defined by the X-axis coordinate and the Y-axis coordinate constituting the upper surface of the chuck table 27 is made of a porous material and has air permeability, and is connected to a suction means (not shown) by a flow path passing through the inside of the support 24.

[0023] The moving means 30 is disposed on the base 2 and includes an X-axis direction feed means 31 for feeding the holding means 20 in the X-axis direction for processing, and a Y-axis direction feed means 32 for indexing and feeding the Y-axis direction movable plate 23 in the Y-axis direction. The X-axis direction feed means 31 converts the rotational motion of the pulse motor 33 into linear motion via a ball screw 34 and transmits it to the X-axis direction movable plate 21, and moves the X-axis direction movable plate 21 forward and backward in the X-axis direction along the guide rails 2a, 2a on the base 2. The Y-axis direction feed means 32 converts the rotational motion of the pulse motor 35 into linear motion via a ball screw 36 and transmits it to the Y-axis direction movable plate 23, and moves the Y-axis direction movable plate 23 forward and backward in the Y-axis direction along the guide rails 22, 22 on the X-axis direction movable plate 21. Although not shown, the X-axis direction feed means 31, the Y-axis direction feed means 32, and the chuck table 27 are provided with position detection means, which accurately detect the X-axis coordinate, the Y-axis coordinate, and the circumferential rotational position of the chuck table 27, and the position information is sent to a control means (not shown). Then, the control means issues an instruction signal based on the position information to drive the X-axis direction feed means 31, the Y-axis direction feed means 32, and the rotation drive means (not shown) of the chuck table 27, so that the chuck table 27 can be positioned at a desired position on the base 2.

[0024] The frame 3 is erected on the base 2 to the side of the moving means 30. The frame 3 includes a vertical wall 3a disposed on the base 2, and a horizontal wall 3b extending horizontally from the upper end of the vertical wall 3a. An optical system (not shown) of the laser beam application means 4 is housed inside the horizontal wall 3b of the frame 3, and a condenser 4a constituting a part of the optical system is disposed on the underside of the tip of the horizontal wall 3b.

[0025] The imaging means 5 is disposed on the lower surface of the tip of the horizontal wall portion 3b at a position spaced apart in the X-axis direction from the condenser 4a of the laser beam application means 4. The imaging means 5 includes an infrared irradiation means for irradiating the workpiece with infrared rays, an optical system for capturing the infrared rays irradiated by the infrared irradiation means, an imaging element (infrared CCD) for outputting an electrical signal corresponding to the infrared rays captured by the optical system, etc. The image captured by the imaging means 5 is sent to the control means and appropriately displayed on a display means (not shown).

[0026] The control means is composed of a computer, and includes a central processing unit (CPU) that performs calculations according to a control program, a read-only memory (ROM) that stores the control program, etc., and a readable / writable random access memory (RAM) that stores the calculation results, etc. The control means is electrically connected to the laser beam application means 4, the imaging means 5, the moving means 30, etc., and controls the operation of each means.

[0027] The wafer 10 that has been subjected to the above-mentioned light-transmitting film disposing step is transferred to the chuck table 27 of the above-mentioned laser processing device 1, and placed on the holding surface 28 of the chuck table 27 with the light-transmitting film TA (any of the polyolefin film T2, PVA film T3, and EVA film T4) side facing upward and the protective tape T1 side facing downward, as shown in Fig. 4. Next, a suction means (not shown) is operated to supply negative pressure onto the holding surface 28 via the chuck table 27, thereby suction-holding the wafer 10 (chuck table holding step). Note that the light-transmitting film TA shown in Fig. 4 and subsequent figures will be described as being a film obtained by thermocompression bonding the polyolefin film T2.

[0028] After the chuck table holding step is performed, a first modified layer forming step is performed to form a modified layer 150, which will be described below. More specifically, the moving means 30 is first operated to position the chuck table 27 directly under the imaging means 5, infrared rays are irradiated from the light-transmitting film TA side, i.e., the back surface 10b side of the wafer 10, an image is taken, the planned dividing lines 14, which are the positions for laser processing of the wafer 10, are detected, and the position information is stored in the control means.

[0029] Next, the wafer 10 is moved together with the chuck table 27 directly below the condenser 4a of the laser beam application means 4, and the division lines 14 formed in a predetermined direction are aligned in the X-axis direction. Once the laser processing start position on the predetermined division lines 14 is positioned directly below the condenser 4a, the position of the condenser 4a is adjusted by the condenser 4a, as shown in Fig. 5, and the condenser P of the laser beam LB is positioned on the front surface 10a side inside the wafer 10 through the light-transmitting film TA. Next, the laser beam application means 4 is operated to apply the laser beam LB, and the X-axis direction feed means 31 of the moving means 30 described based on Fig. 3 is operated to move the chuck table 27 in the X-axis direction, and a modified layer 150 is formed along the division lines 14. In this embodiment, the modified layer 150 is formed in two layers at different depth positions as shown on the right side of Figure 5. First, the focal point P is positioned near the surface 10a of the wafer 10 along a predetermined dividing line 14 and irradiated to form the lower layer side of the modified layer 150. Then, the position of the focal point P is slightly raised and a second laser beam LB is irradiated along the same dividing line 14 to form the upper layer side of the modified layer 150 along the dividing line 14 of the wafer 10.

[0030] After the modified layer 150 is formed along the predetermined dividing lines 14, the Y-axis direction feed means 32 is operated to index and feed the chuck table 27 in the Y-axis direction, and the unprocessed dividing lines 14 adjacent to the dividing lines 14 on which the modified layer 150 has already been formed are positioned directly under the condenser 4a. Next, in the same manner as described above, the X-axis direction feed means 31 is operated while irradiating the laser beam LB, and two modified layers 150 are formed inside the wafer 10 along the dividing lines 14. This laser processing is repeated to form the modified layers 150 along all the dividing lines 14 along the predetermined direction. Next, the chuck table 27 is rotated 90 degrees, and the unprocessed dividing lines 14 perpendicular to the dividing lines 14 on which the modified layer 150 has been formed are aligned with the X-axis direction, and the modified layers 150 are formed on the front surface 10a side of the wafer 10 along all the dividing lines 14 by the same procedure as described above. This completes the first modified layer forming step.

[0031] After the first modified layer forming step is performed as described above, the focal point P of the laser beam LB is positioned on the back surface 10b side inside the wafer 10 through the light-transmitting film TA, and the laser beam LB is irradiated along the dividing line 14 to form the modified layer 160, as described below, in the second modified layer forming step. More specifically, the moving means 30 is operated to align the dividing line 14 in a predetermined direction, along which the first modified layer 150 was formed, with the X-axis direction. Next, the laser processing start position of the dividing line 14 is positioned directly below the condenser 4a, and the condenser 4a is adjusted as shown in FIG. 6 to position the focal point P of the laser beam LB on the back surface 10b side inside the wafer 10 along the dividing line 14 through the light-transmitting film TA. Next, the laser beam application means 4 is operated to apply the laser beam LB, and the X-axis direction feed means 31 of the moving means 30 described based on Fig. 3 is operated to move the chuck table 27 in the X-axis direction to form a modified layer 160 along the planned dividing line 14. The modified layer 160 formed in this embodiment is also formed in two layers having different depth positions, similar to the modified layer 150 described above, and the first layer of the laser beam LB is applied by first positioning the focal point P on the back surface 10b side of the wafer 10 along a predetermined planned dividing line 14, and then the focal point position P is slightly raised and positioned further closer to the back surface 10b, and the second layer of the laser beam LB is applied along the same planned dividing line 14 to form two layers of modified layers 160 on the back surface 10b side inside along the planned dividing line 14 of the wafer 10.

[0032] After the modified layer 160 is formed along the dividing lines 14 in the predetermined direction, the Y-axis direction feed means 32 is operated to index and feed the chuck table 27 in the Y-axis direction, and the dividing line 14 adjacent to the dividing line 14 on which the modified layer 160 has already been formed and on which the modified layer 160 has not yet been formed is positioned directly under the light collector 4a. Next, in the same manner as described above, the X-axis direction feed means 31 is operated while irradiating the laser beam LB, to form two modified layers 160 inside the wafer 10 along the dividing lines 14. Such laser processing is repeated to form modified layers 160 along all the dividing lines 14 along the X-axis direction. Next, the chuck table 27 is rotated 90 degrees, the unprocessed dividing lines 14 perpendicular to the dividing lines 14 on which the modified layers 160 have been formed earlier are aligned with the X-axis direction, and the modified layers 160 are formed on the back surface 10b of the wafer 10 along all the dividing lines 14 in the same manner as described above, completing the second modified layer forming step. Note that, for convenience of explanation, the modified layers 150, 160 are indicated by dashed lines in Figures 5 and 6, but the modified layers 150, 160 are formed inside the wafer 10 and cannot actually be seen.

[0033] The laser processing conditions when carrying out the first modified layer forming step and the second modified layer forming step of this embodiment are set, for example, as shown below. Wavelength: 1342nm Repetition frequency: 90kHz Average power output: 1.2~1.5W Feed speed in the X-axis direction: 70 mm / sec

[0034] After the first modified layer forming step and the second modified layer forming step are performed as described above, the light-transmitting film TA is removed from the back surface 10b of the wafer 10, and an external force is applied to the modified layers 150, 160 formed on the intended dividing lines 14 to divide the wafer 10 into individual device chips 12' as described below. The dividing step will be described below with reference to Figs. 7 and 8.

[0035] The wafer 10 that has been subjected to the first and second modified layer forming steps is transferred to a grinding device 80 (only a part of which is shown) shown in FIG.

[0036] The grinding device 80 includes a chuck table 82 shown in Fig. 7 and a grinding means 84 shown in Fig. 8. The chuck table 82 includes a porous, breathable suction chuck 82a that sucks the wafer 10. The suction chuck 82a is connected to suction means (not shown), and a negative suction pressure is supplied to the upper surface of the suction chuck 82a by the action of the suction means. The chuck table 82 includes a rotating means and a moving means (not shown), and is configured to be rotatable by the action of the rotating means, and is moved by the action of the moving means between a transfer area where the wafer 10 is transferred on and off the chuck table 82 and a grinding area where the wafer 10 is ground by the grinding means 84. The grinding means 84 shown in Figure 8 comprises a rotating spindle 842 rotated by an electric motor (not shown), a wheel mount 844 arranged at the lower end of the rotating spindle 842, a grinding wheel 846 attached to the underside of the wheel mount 844, and a plurality of grinding stones 848 arranged in a ring shape on the underside of the grinding wheel 846.

[0037] The wafer 10 transported to the grinding device 80 is placed on the suction chuck 82a of the chuck table 82 with the protective tape T1 side (front surface 10a side) facing downward as shown in Fig. 7, and is held by suction by supplying negative suction pressure to the suction chuck 82a by the action of a suction means (not shown). In conjunction with this, the light-transmitting film TA is heated or cooled to reduce its adhesive force, and the light-transmitting film TA is removed from the back surface 10b of the wafer 10. If the light-transmitting film TA is a PVA film T3 formed by solidifying a water-soluble liquid resin L, cleaning water can be supplied from above the chuck table 22 to melt and remove the PVA film T3, and if the light-transmitting film TA is, for example, an EVA film T4 similar to the protective tape T1, it can be peeled off by reducing its adhesive force by irradiating it with ultraviolet light or the like.

[0038] Next, the chuck table 32 is moved by the moving means to a position directly below the grinding means 84 shown in Fig. 8, i.e., to the grinding processing area, and the center O of the wafer 10 held on the chuck table 82 is positioned at a position where the grinding stone 848 arranged in an annular shape on the lower surface of the grinding wheel 846 passes, as viewed from above. When the wafer 10 is positioned in the grinding processing area in this manner, the chuck table 82 is rotated in the direction indicated by the arrow R6 in Fig. 8 at, for example, 300 rpm, and at the same time, the grinding wheel 846 of the grinding means 84 is rotated in the direction indicated by the arrow R7 in Fig. 8 at, for example, 6000 rpm. Then, the grinding feed means (not shown) is operated to lower the grinding means 84 in the direction indicated by the arrow R8, so that the grinding means 84 comes into contact with the back surface 10b of the wafer 10 on the chuck table 82 from above, and is fed for grinding at a grinding feed speed of, for example, 1.0 µm / sec. At this time, the thickness of the wafer 10 is measured by a measurement gauge (not shown) while the grinding process is continued until the wafer 10 reaches a desired thickness (for example, 50 μm).

[0039] As described above, by performing the grinding process to grind off a predetermined amount of the back surface 10b of the wafer 10, an external force is applied to the modified layers 150, 160 formed on the dividing lines 14. As a result, as shown in Fig. 8, the wafer 10 is divided along the modified layers 150, 160 formed inside the wafer 10, and the wafer 10 is divided into individual device chips 12'. This completes the dividing process.

[0040] After the above-mentioned division step is performed, a frame holding step shown in FIG. 9 may be performed as necessary. More specifically, first, an annular frame F having an opening Fa large enough to accommodate the wafer 10 is prepared as shown in FIG. 9. Next, the wafer 10 divided into individual device chips 12' by performing the above-mentioned division step is positioned in the center of the opening Fa of the frame F with the back surface 10b side facing downward, and a dicing tape T5 is attached to the back surface 10b of the wafer 10 and the frame F. As a result, the wafer 10 is held and integrated by the frame F via the dicing tape T5. The dicing tape T5 can be a tape similar to the protective tape T1 described above. As a result, the device chips 12' individually divided from the wafer 10 can be easily transported to the next step, for example, a pick-up step can be performed. It is preferable that the protective tape T1 attached to the front surface 10a side of the wafer 10 is peeled off at the same time as performing this frame arrangement step.

[0041] According to this embodiment, as described above, the protective tape T1 is disposed as a protective member on the front surface 10a side of the wafer 10, and the light-transmitting film TA (for example, any one of the polyolefin film T2, the PVA film T3, and the EVA film T4) is disposed on the back surface 10b side, and the first modified layer forming step and the second modified layer forming step are performed. As a result, even when the modified layers 150 and 160 are formed inside the wafer 10, the light-transmitting film TA disposed on the back surface 10b side prevents the internal stress caused by the modified layer 150 formed on the front surface 10a side from reaching the back surface 10b side, and the occurrence of unintended cracks from the modified layer 160 formed on the back surface 10b side can be reduced, and the deterioration of the quality of the device chips 12' generated by the division step is prevented. Furthermore, even if the wafer 10 is unintendedly cracked, the wafer 10 is sandwiched between the protective tape T1 and the light-transmitting film TA, which has the effect of making it easy to carry out the wafer 10 from the laser processing apparatus 1.

[0042] In the above embodiment, when dividing the wafer 10 into individual device chips 12' along the modified layers 150, 160 formed on the dividing lines 14 in the dividing step, an external force is applied using the grinding device 80, but the present invention is not limited to this. For example, the wafer 10 before the dividing step can be supported on an annular frame F as shown in FIG. 9 via an elastic tape, and the tape can be expanded to apply an external force to the modified layers 150, 160, thereby dividing the wafer 10 into individual device chips 12'. Alternatively, the wafer 10 before the dividing step can be placed on a soft urethane mat or the like, and a roller can be pressed against the entire wafer 10 from the back surface 10b side of the wafer 10 to apply an external force, thereby dividing the wafer 10 into individual device chips 12' along the modified layers 150, 160.

[0043] In addition, in the above-described embodiment, the modified layer 150 and the modified layer 160 formed by carrying out the first and second modified layer formation processes were each two layers, but the present invention is not limited to this and may also be composed of one layer or three or more layers. [Explanation of symbols]

[0044] 1: Laser processing equipment 2: Base 3: Frame 3a: Vertical wall 3b:Horizontal wall part 4: Laser beam irradiation means 4a: Concentrator 5: Imaging method 10: Wafer 10a: surface 10b: Back side 12: Device 12': Device chip 14: Planned division line 20: Holding means 27: Chuck table 28: Holding surface 30: Transportation 31: X-axis direction feed means 32: Y-axis direction feed means 80: Grinding equipment 82: Chuck table 82a: Suction chuck 84: Grinding means 846: Grinding wheels 848: Grinding wheel 100: Heat pressing roller 110: Water-soluble resin supply means 112: Nozzle 120: Crimping roller TA: Light-transmitting film T1: Protective tape T2: Polyolefin film T3: PVA film T4: EVA film L: Water-soluble liquid resin LB: Laser beam

Claims

1. A wafer processing method for dividing a wafer having a surface on which a plurality of devices are formed by dividing lines into individual device chips, comprising the steps of: a protective member providing step of providing a protective member on a front surface of the wafer; a light-transmitting film providing step of providing a light-transmitting film on the back surface of the wafer; a chuck table holding step of holding the protective member side of the wafer on a chuck table; a first modified layer forming step of irradiating a laser beam having a wavelength that is transparent to the wafer with a focal point located on the front side of the wafer through the light-transmitting film along the intended dividing lines to form a modified layer; a second modified layer forming step of forming a modified layer by irradiating a laser beam along a planned dividing line through the light-transmitting film at a focal point on the back side of the wafer inside the wafer after the first modified layer forming step; a dividing step of removing the light-transmitting film from the back surface of the wafer and dividing the wafer into individual device chips by applying an external force to the modified layer formed along the dividing lines; The present invention includes: The dividing step is a wafer processing method in which the front side of the wafer is held via the protective member on a chuck table constituting a grinding device, the light-transmitting film is removed from the back side of the wafer, the back side of the wafer is ground to thin it, and the wafer is divided into individual device chips.

2. 2. The wafer processing method according to claim 1, wherein the light-transmitting film disposing step is any one of a step of disposing the light-transmitting film by thermocompression bonding a polyolefin film to the rear surface of the wafer, a step of disposing the light-transmitting film by applying a water-soluble liquid resin to the rear surface of the wafer and solidifying it, and a step of attaching an adhesive tape to the rear surface of the wafer to dispose the light-transmitting film.

3. 3. The wafer processing method according to claim 1 or 2, further comprising the steps of: after carrying out the dividing step, positioning the wafer in a frame having openings for accommodating the wafer divided into individual device chips; attaching a dicing tape to the back surface of the wafer and the frame; and mounting the wafer in the frame via the dicing tape.

Citation Information

Patent Citations

  • Laser beam machining method

    JP2006148175A

  • Laser processing method and laser processing apparatus of wafer

    JP2008131008A

  • Game machine

    JP2008207010A

  • Substrate for dicing tape, the dicing tape, and method for manufacturing semiconductor device

    JP2011040449A

  • Division method of optical device wafer

    JP2012104778A