Coating method and undercoat paint composition

The undercoat paint composition with a high butyral resin content addresses the issue of cracking in paint films by forming a multilayered film that adapts to spacing changes, enhancing film extensibility and adhesion.

JP7578873B2Active Publication Date: 2024-11-07FUJIKURA KASEI CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2020181220
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-10-29
Publication Date
2024-11-07
Estimated Expiration
2040-10-29

AI Technical Summary

Technical Problem

Existing seam treatment methods for wall materials require additional materials and are time-consuming, leading to potential cracks in paint films due to spacing fluctuations between wall materials.

Method used

A coating method using an undercoat paint composition with a butyral resin content of 10% or more, applied to cover seams between wall materials, followed by a top coat, to form a multilayered film that reduces cracking.

Benefits of technology

The method forms a coating film that is less prone to cracking due to spacing variations without requiring additional seam treatment materials, ensuring excellent elongation and toughness.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007578873000004
    Figure 0007578873000004
  • Figure 0007578873000001
    Figure 0007578873000001
  • Figure 0007578873000002
    Figure 0007578873000002
Patent Text Reader

Abstract

To provide a coating method capable of forming a coated film hard to generate a crack caused by variation of a distance between wall materials without preliminarily applying a joint treatment material to a joint between wall materials.SOLUTION: A coating method includes: coating a surface of a plurality of wall materials arranged side by side with an under coating material composition so as to cover a joint between wall materials adjacent each other to form an under coated film; and coating the under coated film with a top coating material composition, where the under coating material composition includes a resin component, and an aqueous medium, the resin component includes a butyral resin, and the ratio of the butyral resin to 100 mass% of the resin component is 10 mass% or more.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a coating method and an undercoat coating composition. [Background technology]

[0002] In the wall surface of a building, a plurality of wall materials such as exterior wall boards are laid out and a coating film is applied to the surface by painting. In such a wall surface, the spacing between the wall materials at the joints between the wall materials may change due to temperature changes, etc., and as a result, cracks may occur in the coating film at the joints between the wall materials.

[0003] One method for preventing cracking of the coating at the joints between wall materials is to provide a band-shaped joint treatment material to cover the joints between wall materials and the side edges of the wall materials on both sides of the joint, and to apply a coating film to the surface of the joint treatment material and the surfaces of the wall materials on both sides of the joint treatment material. The band-shaped joint treatment material reduces the force in the expanding direction when the space between the wall materials expands, so as to prevent it from being transmitted to the coating.

[0004] For example, the following joint treatment materials have been proposed: A strip-shaped joint treatment material having an adhesive layer that is affixed so as to cover the joints between wall materials, a reinforcing layer made of acrylic rubber reinforced with nonwoven fabric that is provided on the outside of the adhesive layer, and a buffer section that is partially provided with a buffer material made of silicone resin formed between the adhesive layer and the reinforcing layer (Patent Document 1). [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2006-233611 A Summary of the Invention [Problem to be solved by the invention]

[0006] However, the joint treatment method using the joint treatment material described in Patent Document 1 requires a lot of work to apply, and also requires the joint treatment material in addition to the paint.

[0007] The object of the present invention is to provide a coating method and an undercoat paint composition that can form a coating film that is less susceptible to cracking due to variations in the gap between wall materials, even without the need to previously apply a joint treatment material to the joints between wall materials. [Means for solving the problem]

[0008] The present invention has the following aspects. [1] A method for forming an undercoat coating film by applying an undercoat coating composition to the surfaces of a plurality of wall materials arranged side by side so as to cover the joints between adjacent wall materials, and applying a topcoat coating composition on the undercoat coating film, comprising the steps of: A coating method characterized in that the undercoat paint composition comprises a resin component and an aqueous medium, the resin component comprises a butyral resin, and the proportion of the butyral resin relative to 100% by mass of the resin component is 10% by mass or more. [2] A primer coating composition that is applied to the surfaces of multiple wall materials arranged side by side so as to cover the joints between adjacent wall materials, 1. An undercoat paint composition comprising a resin component and an aqueous medium, the resin component comprising a butyral resin, the proportion of the butyral resin relative to 100% by mass of the resin component being 10% by mass or more. Effect of the Invention

[0009] According to the present invention, a coating method and an undercoat paint composition can be provided that can form a coating film that is less susceptible to cracking due to variations in the gap between wall materials, even without the need to previously apply a joint treatment material to the joints between wall materials. [Brief description of the drawings]

[0010] [Figure 1] 1 is a schematic cross-sectional view illustrating a coating method according to one embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] [Painting method] Hereinafter, one embodiment of the coating method of the present invention will be described with reference to Fig. 1. Note that the dimensional ratio in Fig. 1 is different from the actual one for the sake of convenience of explanation. In the coating method according to this embodiment, a specific undercoat paint composition is applied to the surfaces of a plurality of wall materials 10 arranged side by side so as to cover the joints C between adjacent wall materials 10 to form an undercoat coating film 1 (step (a)), and a topcoat paint composition is applied on the undercoat coating film 1 to form a topcoat coating film 3 (step (b)). As a result, a coating film with a multilayer structure in which the undercoat coating film 1 and the topcoat coating film 3 are laminated is formed on the surfaces of the plurality of wall materials 10 so as to cover the joints C between adjacent wall materials 10.

[0012] <Undercoat paint composition> The undercoat paint composition includes a resin component and an aqueous medium. The resin component includes a butyral resin. The proportion of the butyral resin relative to 100% by mass of the resin component is 10% by mass or more. The resin component may further contain other resins than the butyral resin. The undercoat coating composition may further contain an emulsifier, if necessary. The undercoat coating composition may further contain a plasticizer, if necessary. The undercoat coating composition may further contain other components in addition to those described above, as necessary.

[0013] Butyral resin is also called polyvinyl butyral resin, and is typically a butyralized product of polyvinyl alcohol. The butyralized product of polyvinyl alcohol is obtained by reacting polyvinyl alcohol with butyraldehyde in the presence of an acid catalyst. The butyral resin may be soluble or insoluble in an aqueous medium, but is preferably soluble in an aqueous medium. If the butyral resin is soluble in an aqueous medium, it is not necessary to add an emulsifier to disperse the butyral resin in the aqueous medium.

[0014] The butyral resin may be a commercially available product, such as S-LEC (registered trademark) BM-5, S-LEC KW-10, or S-LEC KW-M manufactured by Sekisui Chemical Co., Ltd.

[0015] The other resins are not particularly limited, and known resins for paints can be used, such as urethane, acrylic, epoxy, polyvinyl acetate, polystyrene, acrylonitrile, Veova (branched fatty acid vinyl ester), natural or synthetic rubber, and emulsions of copolymers thereof. These resins may be used alone or in combination of two or more. From the standpoint of water resistance of the coating film, the other resin is preferably a resin dispersible in an aqueous medium, and from the standpoint of adhesion to the topcoat coating film 3, a urethane resin dispersible in an aqueous medium or an acrylic resin dispersible in an aqueous medium is more preferable, with a urethane resin dispersible in an aqueous medium being particularly preferable. The resin dispersible in the aqueous medium is typically blended in the form of an emulsion or dispersion. Specific examples include acrylic resin emulsion, acrylic resin dispersion, and urethane resin dispersion. Commercially available products can be used for these emulsions and dispersions.

[0016] The aqueous medium is a medium consisting of only water, or a medium in which a solvent compatible with water has been added to water. The water that can be used may be ion-exchanged water, tap water, or the like. Examples of the solvent that is compatible with water include alcohols such as ethanol and isopropyl alcohol, and ethylene glycol. The aqueous medium is preferably water.

[0017] When the butyral resin is insoluble in an aqueous medium, an emulsifier can be included in the undercoat paint composition to enhance the dispersibility of the butyral resin in the aqueous medium. As the emulsifier, a known emulsifier can be used, and examples thereof include anionic surfactants, nonionic surfactants, cationic surfactants, and zwitterionic surfactants.

[0018] A plasticizer may be included in the basecoat composition to soften the butyral resin. As the plasticizer, known plasticizers can be used, and examples thereof include butyl ricinoleate, methyl ricinoleate, didecyl phthalate, and diisobutyl adipate.

[0019] Examples of other components include antifoaming agents, dispersants, thickeners, film-forming agents, preservatives, and leveling agents.

[0020] In the undercoat paint composition, the proportion of butyral resin relative to 100% by mass of the resin component is 10% by mass or more, and preferably 30% by mass or more. If the proportion of butyral resin is equal to or more than the lower limit, the undercoat coating film 1 formed is excellent in extensibility and toughness, and when the gap between the wall materials 10 widens, the undercoat coating film 1 can expand in accordance with the movement, and the occurrence of cracks in the topcoat coating film 3 formed thereon can be suppressed. The proportion of the butyral resin relative to 100% by mass of the resin component may be 100% by mass.

[0021] When the resin component contains other resins, the proportion of butyral resin relative to 100% by mass of the resin component is preferably 80% by mass or less. If the proportion of butyral resin is equal to or less than the upper limit, the water resistance of the undercoat coating film 1 and the adhesion to the topcoat coating film 3 are superior.

[0022] The content of the resin component is preferably 10 to 50% by mass relative to 100% by mass of the undercoat paint composition. If the content of the resin component is within the above range, the coating workability is excellent.

[0023] The content of the aqueous medium is preferably 10 to 80% by mass relative to 100% by mass of the undercoat paint composition. If the content of the aqueous medium is within the above range, the coating workability is excellent.

[0024] The content of the emulsifier is preferably 0 to 10 parts by mass relative to 100 parts by mass of the butyral resin. If the content of the emulsifier exceeds the upper limit, the water resistance of the coating film may deteriorate and blistering may occur. The undercoat coating composition preferably does not contain an emulsifier.

[0025] The content of the plasticizer is preferably 0 to 50 parts by mass relative to 100 parts by mass of the butyral resin. If the content of the plasticizer exceeds the upper limit, the plasticizer may bleed out, causing the topcoat coating film 3 to blister or peel off. The undercoat coating composition preferably does not contain a plasticizer.

[0026] The content of the other components can be appropriately selected within a range that does not impair the effects of the present invention, and is, for example, about 0 to 30 parts by mass per 100 parts by mass of the resin component.

[0027] The undercoat paint composition can be produced, for example, by mixing a butyral resin with an aqueous medium, and if necessary, other resins, emulsifiers, plasticizers, other components, etc. may be mixed therewith.

[0028] <Process (a)> In step (a), an undercoat paint composition is applied to the surfaces of a plurality of wall materials 10 arranged side by side so as to cover the joints C between adjacent wall materials 10.

[0029] Examples of the wall material 10 include exterior and interior wall materials for buildings. Examples of the material for the wall material 10 include mortar, concrete, ceramic materials, plastics, metals, and wood. The surface of the wall material 10 may be smooth or may have irregularities. A coating film may be provided on the surface of the wall material 10. If necessary, a joint material may be filled into the joints C between adjacent wall materials 10. Examples of the joint material include a sealing material and a putty material.

[0030] The method for applying the undercoat paint composition may, for example, be a method in which the undercoat paint composition is applied by a known application method such as with a roller, spray, brush or trowel, and then dried. The drying may be performed at room temperature or by heating as long as the aqueous medium can be removed. The drying temperature is, for example, 5 to 70° C. The drying time varies depending on the drying temperature, but is, for example, 10 minutes to 4 hours.

[0031] The amount of the undercoat paint composition applied is set according to the thickness of the undercoat paint film 1 to be formed. The thickness of the undercoat coating film 1 is preferably 20 to 300 μm, and more preferably 50 to 100 μm. If the thickness of the undercoat coating film 1 is within the above range, the undercoat coating film 1 has an excellent balance between extensibility and toughness, and is easily able to follow the expansion of the gap between wall materials.

[0032] <Process (b)> In step (b), a topcoat paint composition is applied onto the undercoat coating film 1. There is no particular limitation on the topcoat paint composition, and various known paint compositions can be used. Examples of the topcoat paint composition include paint compositions containing resins, coloring pigments, etc. Examples of the resin include the other resins described above. The method for applying the topcoat coating composition is not particularly limited, and any known application method can be used. The coating amount of the topcoat paint composition is, for example, 100 to 450 g / m 2 It is.

[0033] It should be noted that the configurations and combinations thereof in the above-described embodiment are merely examples, and additions, omissions, substitutions, and other modifications of the configurations are possible without departing from the spirit of the present invention. EXAMPLES

[0034] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these examples. In the following, "parts" refers to "parts by mass."

[0035] (Materials used) Butyral resin aqueous solution A: "S-LEC KW-10" manufactured by Sekisui Chemical Co., Ltd., resin content 24 mass%, calculated molecular weight of butyral resin 27858, butyralization degree 9 mol%. Butyral resin aqueous solution B: "S-LEC KW-M" manufactured by Sekisui Chemical Co., Ltd., resin content 20 mass%, calculated molecular weight of butyral resin 30288, butyralization degree 24 mol%. Butyral resin dispersion C: According to the formula (parts) shown in Table 1, butyral resin (Sekisui Chemical's "S-LEC BL-5", resin content 100 mass%, calculated molecular weight 3200, butyralization degree 77 mol%), water, and plasticizer (butyl ricinoleate) were mixed, and then emulsifier (Nippon Nyukazai's "Newcol 2360") was added while stirring to forcibly emulsify. Urethane resin dispersion: "Superflex 420" manufactured by Daiichi Kogyo Seiyaku Co., Ltd., resin content 32% by mass. Acrylic resin emulsion: "Mowinyl LDM7522" manufactured by Japan Coating Resins, resin content 51% by mass.

[0036] [Table 1]

[0037] (Examples 1 to 14, Comparative Examples 1 to 2) <Production of Undercoat Paint Composition> Undercoat paint compositions were obtained by mixing the raw materials in the amounts (converted into resin content) shown in Tables 2-3, and water as required, using a disperser. The amount of water was set so that the ratio (mass%) of the resin component to 100 mass% of the undercoat paint composition would be the value shown in Tables 2-3. Tables 2 and 3 show the proportions (mass %) of butyral resin relative to 100 mass % of the resin component.

[0038] <Preparation of test specimen> Two slate boards (width 10 mm, length 20 mm, thickness 4 mm) were arranged on a horizontal surface with no gap between them so that one end of each slate board in the longitudinal direction was abutted against each other. The undercoat paint composition was applied to the slate boards with a brush so that the thickness after drying was 50 μm or 100 μm, and the resulting mixture was dried at room temperature for 12 hours to form an undercoat paint film. Next, an acrylic resin paint was applied to the undercoat paint film at 150 g / m as a topcoat paint. 2The coating was applied in an amount of 1000 ml and dried at room temperature for 12 hours to form a topcoat coating film. This resulted in a test piece in which two slate boards were connected by a coating film consisting of the undercoat coating film and the topcoat coating film.

[0039] <Evaluation of elongation> Both longitudinal ends of the test piece were attached to the chucks of a tensile testing machine (Orientec Co., Ltd. "Tensilon RTC-1210") and stretched 3 mm in the longitudinal direction under conditions of a measurement atmosphere of 23°C, a rated load of 250 N, and a tensile speed of 20 mm / min, and then returned to the original position. This operation was repeated a total of three times. The appearance of the coating film on the test piece was then visually observed and evaluated according to the following criteria. The results are shown in Tables 2 to 3. "Evaluation criteria for extensibility" ○: No cracks or breaks. △: There are cracks but no cracks. ×: Cracks are present. When the test piece is stretched, the coating is stretched mainly near the boundary between the two slate boards. If the undercoat coating has low extensibility, a break will appear in the coating and the two sides of the break will separate. When the test piece is returned to its original position, if the two sides of the break come together to form a stripe, it is called a "crack," and if the two sides of the break remain separated, it is called a "split."

[0040] <Cycle test> A test piece with a 50 μm thick undercoat was left in a -5°C environment for 4 hours, and then left in a 65°C environment for 4 hours, with this cycle being repeated 20 or 40 times. The test piece's coating was then visually observed, and the appearance and adhesion were evaluated according to the following criteria. The results are shown in Tables 2 to 3. "Appearance Evaluation Criteria" ○: No cracks, breaks or swelling. △: No cracks or breaks, but swelling of 10% or less in area. ×: Cracks, breaks, and swelling are present. "Adhesion evaluation criteria" ◯: The peeled area between the undercoat film and the topcoat film is 0% (no peeling is observed). △: The peeled area between the undercoat film and the topcoat film is more than 0% and 10% or less. ×: The peeled area between the undercoat film and the topcoat film is more than 10%.

[0041] [Table 2]

[0042] [Table 3]

[0043] The coating films of the test pieces of Examples 1 to 14 had excellent elongation. These results show that cracks caused by variations in the gap between the wall materials are unlikely to occur. Among Examples 1 to 14, the coating films of the test pieces of Examples 1, 2, and 6 to 14 in which the undercoat paint composition did not contain a plasticizer were excellent in appearance after the cycle test. In the coating films of the test pieces of Examples 4 to 14 in which the resin component of the undercoat paint composition contained other resins, the undercoat coating film and the topcoat coating film maintained good adhesion even after 40 cycles of the cycle test. On the other hand, the coating films of the test pieces of Comparative Examples 1 and 2, in which the undercoat paint composition did not contain a butyral resin, were poor in elongation. [Industrial Applicability]

[0044] The coating film formed by the undercoat paint composition of the present invention has excellent extensibility and toughness, and can expand and contract in accordance with the change in the gap between the wall materials. Therefore, even if a joint treatment material is not applied to the joint between the wall materials before applying the topcoat paint composition, the occurrence of cracks in the topcoat paint film when the gap between the wall materials widens can be suppressed by applying the undercoat paint composition of the present invention. [Explanation of symbols]

[0045] 1 Undercoat 3 Topcoat C seam 10. Wall Materials

Claims

1. A method for coating a surface of a plurality of wall materials arranged side by side with an undercoat coating composition so as to cover joints between adjacent wall materials to form an undercoat coating film, and then coating a topcoat coating composition on the undercoat coating film, comprising the steps of: the undercoat paint composition comprises a resin component and an aqueous medium, the resin component comprises a butyral resin, and a ratio of the butyral resin to 100% by mass of the resin component is 10% by mass or more; A coating method characterized in that the content of the emulsifier in the undercoat paint composition is 0 parts by mass or more and less than 10 parts by mass per 100 parts by mass of the butyral resin.

2. The content of the emulsifier is 0 parts by mass relative to 100 parts by mass of the butyral resin, The coating method according to claim 1 , wherein the butyral resin is soluble in the aqueous medium.

3. A painting method as described in claim 1 or 2, wherein the resin component further contains a urethane resin that is dispersible in the aqueous medium.

4. A primer coating composition that is applied to the surfaces of a plurality of wall materials arranged side by side so as to cover the joints between adjacent wall materials, The composition includes a resin component and an aqueous medium, the resin component includes a butyral resin, and a ratio of the butyral resin to 100% by mass of the resin component is 10% by mass or more; An undercoat paint composition comprising an emulsifier in an amount of 0 parts by mass or more and less than 10 parts by mass per 100 parts by mass of the butyral resin.

5. The content of the emulsifier is 0 parts by mass relative to 100 parts by mass of the butyral resin, The undercoat coating composition of claim 4, wherein said butyral resin is soluble in said aqueous medium.

6. The undercoat paint composition described in claim 4 or 5, wherein the resin component further contains a urethane resin that is dispersible in the aqueous medium.

Citation Information

Patent Citations

  • Structure of building wall surface using board for construction

    JP1998159292A

  • Decorative material

    JP2001001453A

  • Joint finishing material

    JP2006233611A

  • Method of treating joint part of plate-like material and surface finish method of plate- like material provided with joint part

    JP2009148718A

  • Substrate preparation material and method for coating finishing of cement-based substrate

    JP2009149767A