By strategically arranging conductivity type regions in semiconductor devices, the semiconductor device reduces current loss in silicon carbide substrates by optimizing depletion layer distribution and current path resistance.

JP7579687B2Active Publication Date: 2024-11-08NISSAN MOTOR CO LTD +1
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2020199367
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-12-01
Publication Date
2024-11-08
Estimated Expiration
2040-12-01

AI Technical Summary

Technical Problem

The high electrical resistance and high on-resistance of pn junction diodes in semiconductor devices using silicon carbide substrates result in significant losses due to low impurity concentration and mobility, which are not effectively addressed by existing technologies.

Method used

The semiconductor device design includes a specific arrangement of drift, well, and contact regions with controlled distances and conductivity types, where the distance from the connecting surface of the first region to the second well region is one-tenth or less of the distance to the second region, reducing current path resistance and enhancing current flow.

Benefits of technology

This design effectively reduces the loss in current flow through the pn junction diode, particularly in wide bandgap semiconductor substrates like silicon carbide, by optimizing the depletion layer distribution and current path.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007579687000001
    Figure 0007579687000001
  • Figure 0007579687000002
    Figure 0007579687000002
  • Figure 0007579687000003
    Figure 0007579687000003
Patent Text Reader

Abstract

To provide a semiconductor device and a method of manufacturing the same capable of suppressing increase in loss.SOLUTION: A semiconductor device has: a drift region; a first well region adjacent to the drift region; a first region opposed to the drift region via the first well region; a second well region opposed to the drift region via the first well region while being adjacent to the first region; and a second region connected with the drift region at a position separated from the first well region. A distance from a connection surface between the first region and the second well region to an opposed surface of the first region to the connection surface is one-tenth or less of a distance from the first region to the second region.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a semiconductor device and a manufacturing method thereof. [Background technology]

[0002] Planar-structure transistors have been proposed in which an impurity region is formed in an insulating silicon carbide (SiC) substrate by ion implantation. The impurity concentration in the base region that forms the inversion layer (channel) of the transistor must be relatively low. For example, the impurity concentration in the p-type base region is set to 1E18 cm -3 To the following: [Prior art documents] [Non-patent literature]

[0003] [Non-Patent Document 1] Ogyun Soek etc. “High-voltage lateral double-implanted MOSFETs implemented on high-purity semi-insulating 4H-SiC substrates with gate field plates” Japanese Journal of Applied Physics, Volume 57, Number 6S1 June 2018 Summary of the Invention [Problem to be solved by the invention]

[0004] Since the impurity concentration in the base region cannot be made high, the electrical resistance of the base region during operation of the body diode of the transistor is high. This results in high transistor loss. In addition, SiC materials have low hole mobility and a low impurity activation rate. For this reason, semiconductor devices using silicon carbide substrates have a higher on-resistance of the pn junction diode than semiconductor devices using silicon (Si) substrates.

[0005] An object of the present invention is to provide a semiconductor device and a method for manufacturing the semiconductor device that suppresses an increase in loss. [Means for solving the problem]

[0006] A semiconductor device according to an embodiment of the present invention includes a drift region, a first well region, a first region and a second well region each facing the drift region via the first well region, and a second region connected to the drift region. A distance from a connection surface between the first region and the second well region to a surface facing the connection surface of the first region is one-tenth or less of a distance from the first region to the second region. Effect of the Invention

[0007] According to the present invention, it is possible to provide a semiconductor device and a method for manufacturing the semiconductor device that suppresses an increase in loss. [Brief description of the drawings]

[0008] [Figure 1] 1 is a schematic cross-sectional view showing a configuration of a semiconductor device according to a first embodiment of the present invention. [Diagram 2] FIG. 1 is a schematic diagram showing the configuration of a simulation model (part 1). [Diagram 3] FIG. 2 is a schematic diagram showing the configuration of the simulation model (part 2). [Figure 4] FIG. 3 is a schematic diagram showing the configuration of the simulation model (part 3). [Diagram 5] 3 is a graph showing the results of a simulation using the simulation model of FIG. 2. [Figure 6] 4 is a graph showing the results of a simulation using the simulation model of FIG. 3. [Figure 7] 5 is a graph showing the results of a simulation using the simulation model of FIG. 4. [Figure 8] FIG. 13 is a schematic diagram showing a range in which the results of a simulation are displayed. [Figure 9]13 is a simulation result of a current distribution when the first distance is 0.1 μm. [Figure 10] 13 is a simulation result of a current distribution when the first distance is 0.8 μm. [Figure 11] 1A to 1C are schematic cross-sectional views for explaining a method for manufacturing a semiconductor device according to a first embodiment of the present invention (part 1). [Figure 12] 5A to 5C are schematic cross-sectional views for explaining the method for manufacturing the semiconductor device according to the first embodiment of the present invention (part 2). [Figure 13] 5A to 5C are schematic cross-sectional views for explaining the method for manufacturing the semiconductor device according to the first embodiment of the present invention (part 3). [Figure 14] 4 is a schematic cross-sectional view for explaining the method for manufacturing the semiconductor device according to the first embodiment of the present invention (part 4). FIG. [Figure 15] 5 is a schematic cross-sectional view for explaining the method for manufacturing the semiconductor device according to the first embodiment of the present invention (part 5). FIG. [Figure 16] 6 is a schematic cross-sectional view for explaining the method for manufacturing the semiconductor device according to the first embodiment of the present invention (part 6). FIG. [Figure 17] 7 is a schematic cross-sectional view for explaining the method for manufacturing the semiconductor device according to the first embodiment of the present invention (part 7). FIG. [Figure 18] FIG. 4 is a schematic cross-sectional view showing a configuration of a semiconductor device according to a second embodiment of the present invention. [Figure 19] 13 is a result of a simulation of current distribution in the semiconductor device according to the second embodiment of the present invention. [Figure 20] 5A to 5C are schematic cross-sectional views for illustrating a method for manufacturing a semiconductor device according to a second embodiment of the present invention. [Figure 21] FIG. 11 is a schematic cross-sectional view showing a configuration of a semiconductor device according to a third embodiment of the present invention. [Figure 22] 11A to 11C are schematic cross-sectional views for illustrating a method for manufacturing a semiconductor device according to a third embodiment of the present invention. [Figure 23]FIG. 13 is a schematic perspective view showing a configuration of a semiconductor device according to a fourth embodiment of the present invention. [Figure 24] 24 is a schematic cross-sectional view taken along the AA direction in FIG. 23. [Diagram 25] FIG. 11 is a schematic perspective view (part 1) for explaining a method for manufacturing a semiconductor device according to a fourth embodiment of the present invention. [Figure 26] FIG. 13 is a schematic perspective view (part 2) for explaining the method for manufacturing a semiconductor device according to a fourth embodiment of the present invention. [Figure 27] FIG. 13 is a schematic cross-sectional view showing a configuration of a semiconductor device according to a fifth embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Hereinafter, the embodiments will be described with reference to the drawings. In the description of the drawings, the same parts are given the same reference numerals and the description will be omitted. However, the drawings are schematic, and the relationship between thickness and planar dimensions, the thickness ratio of each layer, and the like include parts that differ from the actual ones. In addition, there are parts where the dimensional relationships and ratios differ between the drawings.

[0010] (First embodiment) The configuration of a semiconductor device 1 according to a first embodiment of the present invention is shown in Fig. 1. The semiconductor device 1 includes a drift region 21 of a first conductivity type, a first well region 22 of a second conductivity type, and a first region 24 of the first conductivity type and a second well region 23 of the second conductivity type, which face the drift region 21 via the first well region 22.

[0011] The drift region 21 and the first well region 22 are formed adjacent to each other in the substrate 10. The first region 24 and the second well region 23 are formed adjacent to each other in the substrate 10. Specifically, the first region 24 is disposed on the upper surface of the second well region 23. The second well region 23 has a higher impurity concentration than the first well region 22.

[0012] Furthermore, the semiconductor device 1 includes a second region 25 of the first conductivity type connected to the drift region 21 at a position spaced apart from the first well region 22, and a contact region 26 of the second conductivity type arranged on the upper surface of the second well region 23 and adjacent to the first region 24.

[0013] The first conductivity type and the second conductivity type are opposite conductivity types. That is, if the first conductivity type is n-type, the second conductivity type is p-type, and if the first conductivity type is p-type, the second conductivity type is n-type. In the following, a case where the first conductivity type is n-type and the second conductivity type is p-type will be described.

[0014] The substrate 10 may be a semiconductor substrate, a semi-insulating substrate, or an insulating substrate. Here, an insulating substrate refers to a semiconductor substrate having a resistivity of several kΩ / cm or more. For example, the substrate 10 is an insulating silicon carbide substrate.

[0015] The semiconductor device 1 also includes a first main electrode 41 electrically connected to the first region 24 and the second well region 23, and a second main electrode 42 electrically connected to the second region 25. The first main electrode 41 is disposed on the upper surface of the first region 24 and the contact region 26. The second well region 23 is electrically connected to the first main electrode 41 via the contact region 26. The second main electrode 42 is disposed on the upper surface of the second region 25. An interlayer insulating film 50 is disposed between the first main electrode 41 and the second main electrode 42, covering the surfaces of the drift region 21 and the first well region 22. In an opening formed in the interlayer insulating film 50, the first main electrode 41 is connected to the first region 24 and the contact region 26, and the second main electrode 42 is connected to the second region 25.

[0016] 1, the distance from the connection surface 241 between the first region 24 and the second well region 23 to the opposing surface 242 opposing the connection surface 241 of the first region 24 is defined as a first distance d. The distance from the first region 24 to the second region 25 is defined as a second distance h. In the semiconductor device 1, the first distance d is 10 times the second distance h. minutes is less than or equal to 1.

[0017] 1 functions as a pn junction diode with the first region 24 as the anode and the second region 25 as the cathode. That is, a predetermined potential (for example, about −3 V) is applied to the second main electrode 42 with the potential of the first main electrode 41 as the reference. As a result, the pn junction diode formed between the first well region 22 and the drift region 21 of the semiconductor device 1 becomes conductive, and a current flows from the first main electrode 41 to the second main electrode 42.

[0018] In the semiconductor device 1, the first distance d is 10 times the second distance h. minutes Losses are reduced by keeping the ratio of the resistance to pressure drop at or below 1. The reason for this will be explained below with reference to a simulation using the simulation model shown in FIGS.

[0019] In this simulation, the second distance h was fixed and the first distance d was changed to calculate the current Id flowing from the first main electrode 41 to the second main electrode 42. In order to facilitate the simulation, a simulation model was used in which a stacked structure of the second well region 23 and the first region 24 was arranged in a part of the upper part of the first well region 22, and the first main electrode 41 was arranged on the side of the second well region 23, as shown in Figures 2 to 4. The simulation model shown in Figures 2 to 4 makes it possible to calculate the current flowing through the semiconductor device 1 having the structure shown in Figure 1.

[0020] In the simulation model shown in Fig. 2, the second distance h is 4.5 µm. In the simulation model shown in Fig. 3, the second distance h is 8.5 µm. In the simulation model shown in Fig. 4, the second distance h is 10.5 µm. The simulation was performed with the potential of the first main electrode 41 set to 4 V and the potential of the second main electrode 42 set to 0 V.

[0021] Figure 5 shows the results of a simulation of the current Id using the simulation model shown in Figure 2. As shown in Figure 5, as the first distance d increases, the current Id decreases. Then, when the first distance d is 0.4 μm or more, the current Id becomes almost constant.

[0022] Figure 6 shows the results of a simulation of the current Id using the simulation model shown in Figure 3. As shown in Figure 6, as the first distance d increases, the current Id decreases. Then, when the first distance d is 0.8 μm or more, the current Id becomes almost constant.

[0023] Figure 7 shows the results of a simulation of the current Id using the simulation model shown in Figure 4. As shown in Figure 7, as the first distance d increases, the current Id decreases. Then, when the first distance d is 1.1 μm or more, the current Id becomes almost constant.

[0024] As shown in Figs. 5 to 7, when the second distance h is between 4.5 µm and 10.5 µm, the current Id decreases as the first distance d increases. Then, when the first distance d exceeds a certain length, the current Id is constant. The current Id is constant when the first distance d is approximately 10 times the second distance h. minutes In other words, the first distance d is greater than 10 of the second distance h. minutes When the first distance d is greater than 1, the current Id is limited and loss occurs. Therefore, the condition for suppressing loss is when the first distance d is 10 times the second distance h. minutes The first distance d is 10 times the second distance h. minutes The reason why the current Id becomes constant when Id is greater than 1 will be explained below.

[0025] FIG. 8 shows area A displaying the results of simulating the current distribution. The results of the simulation in area A are shown in FIGS. 9 and 10. The simulation results shown in FIG. 9 are for the case where the first distance d is 0.1 μm. The simulation results shown in FIG. 10 are for the case where the first distance d is 0.8 μm. Note that in the simulation results in FIG. 9 and FIG. 10, the direction along the first distance d is shown as the X direction, and the direction along the second distance h is shown as the Y direction (the same applies below).

[0026] 9, when the first distance d is 0.1 μm, a current also flows on the surface of the semiconductor device. This is because the width of the depletion layer extending from the first region 24 to the first well region 22 is narrow. Therefore, the paths of the current passing through the first main electrode 41 are a path that flows through the first well region 22 and the second well region 23 in a region deeper than the first region 24, and a path that flows on the surface of the semiconductor device.

[0027] 10, when the first distance d is 0.8 μm, the current flowing to the surface of the semiconductor device is small. This is because the width of the depletion layer extending from the first region 24 to the first well region 22 is large. For this reason, the only path for the current flowing through the first main electrode 41 is the path through the first well region 22 and the second well region 23 in a region deeper than the first region 24. Therefore, the current Id is smaller when the first distance d is 0.8 μm than when the first distance d is 0.1 μm.

[0028] As described above, the first distance d is 10 times the second distance h. minutes In the semiconductor device 1, where the ratio is 1 or less, a reduction in the path of the current Id flowing from the first main electrode 41 to the second main electrode 42 caused by a depletion layer spreading from the first region 24 to the first well region 22 is suppressed. Therefore, the semiconductor device 1 can reduce the loss of the current flowing through the pn junction.

[0029] For example, in the semiconductor device 1, the first distance d is 0.3 μm and the second distance h is 4.5 μm. The first distance d may be set to 1 / 10.5 or less of the second distance h. For example, as shown in FIG. 7, when the first distance d is 1 μm, the effect of increasing the current Id can be confirmed by setting the second distance h to 10.5 μm.

[0030] A substrate made of a wide bandgap semiconductor may be used for the substrate 10. In a substrate made of a wide bandgap semiconductor, the conduction voltage of a pn junction diode is large, and the loss is larger than that of a pn junction diode made of a substrate made of a semiconductor material such as Si. Therefore, when the substrate 10 is made of a wide bandgap semiconductor, the effect of reducing loss by the semiconductor device 1 is more effective.

[0031] A silicon carbide substrate (SiC substrate) may be used for the substrate 10. Since p-type SiC has low carrier mobility, the use of a SiC substrate for the substrate 10 has a significant effect of reducing the electrical resistance of the pn junction diode. There are several polytypes (crystal polymorphism) of SiC, and a typical 4H SiC substrate can be used for the substrate 10.

[0032] A semi-insulating substrate or an insulating substrate may be used for the substrate 10. In this case, the current of the pn junction diode does not easily flow through the substrate 10. For this reason, the path of the current flowing through the surface of the semiconductor device 1 is important. Therefore, the effect of reducing loss by the semiconductor device 1 is more effective when the substrate 10 is a semi-insulating substrate or an insulating substrate.

[0033] A method for manufacturing the semiconductor device 1 according to the first embodiment will be described below with reference to the drawings. Note that the method for manufacturing the semiconductor device 1 described below is one example, and various other manufacturing methods, including modifications thereof, can be used. In the following, a case where an insulating silicon carbide substrate is used as the substrate 10 will be described.

[0034] First, as shown in FIG. 11, a mask material 101 formed on the main surface of the substrate 10 is patterned so as to cover the remaining region of the region where the drift region 21 is to be formed.

[0035] A typical mask material may be, for example, a silicon oxide film. A thermal CVD method or a plasma CVD method may be used as a method for depositing the mask material. A photolithography technique may be used as a patterning method. That is, the mask material is etched using a patterned photoresist film as a mask. A dry etching method such as a reactive ion etching method using ions reactive with the silicon oxide film may be used as an etching method. The photoresist film is then removed with oxygen plasma, sulfuric acid, or the like. In this way, the mask material is patterned (the same applies below).

[0036] Next, the substrate 10 is doped with an n-type impurity by ion implantation using the patterned mask material 101 as a mask to selectively form the drift region 21. For example, the n-type impurity is nitrogen, and the drift region 21 is doped to a depth of 1 μm and an impurity concentration of 1E16 cm -3 12 shows a state in which the mask material 101 is removed after the drift region 21 is formed. The mask material 101, which is a silicon oxide film, may be removed by wet etching using hydrofluoric acid or the like.

[0037] Next, the substrate 10 is doped with a p-type impurity by ion implantation using the patterned mask material as a mask to form a first well region 22 as shown in Fig. 13. For example, the p-type impurity is aluminum, and the first well region 22 is doped with aluminum at a depth of 1.0 µm and an impurity concentration of 1E17 cm -3 The first well region 22 is formed.

[0038] 14, the first region 24 and the second region 25 are formed. At this time, the first region 24 and the second region 25 may be formed simultaneously by ion implantation using a patterned mask material as a mask. For example, nitrogen ions are used as n-type impurities, and the depth is 0.3 μm and the impurity concentration is 1E19 cm -3 14, the first region 24 is selectively formed above the first well region 22. The second region 25 is formed above the drift region 21 at a position spaced apart from the first well region 22.

[0039] The distance from the bottom surface of the first region 24 to the top surface of the first region 24 corresponds to the first distance d. Therefore, when the thickness of the first region 24 is 10 times the second distance h from the first region 24 to the second region 25, minutes The first region 24 and the second region 25 are formed so that the first distance d is equal to or smaller than 1 / 2 the second distance h in the completed semiconductor device 1. minutes will be less than 1.

[0040] 15, a contact region 26 is formed by ion implantation, which selectively dopes the first well region 22 with a p-type impurity. For example, aluminum ions as p-type impurities are implanted into a predetermined region of the first well region 22 to a depth of 0.3 μm and an impurity concentration of 1E20 cm -3 The contact region 26 is formed.

[0041] 16, the second well region 23 is formed below the first region 24 and the contact region 26. For example, the lower part of the first well region 22 is doped with a p-type impurity by ion implantation using a patterned mask material as a mask to form the second well region 23. At this time, the position of the second well region 23 in the film thickness direction of the substrate 10 is set by appropriately setting the implantation energy of the ion implantation. For example, the second well region 23 is doped with a p-type impurity in a range of 0.3 μm to 1 μm deep from the substrate surface with an impurity concentration of 1E19 cm. -3 The second well region 23 is formed under the conditions set so that the lower surfaces of the first region 24 and the contact region 26 are connected to the second well region 23.

[0042] Thereafter, the impurities doped in the substrate 10 are activated by heat treatment. For example, the heat treatment is performed at about 1700° C. in an argon atmosphere or a nitrogen atmosphere.

[0043] In the above ion implantation method, the depth and impurity concentration of each region are set according to the application of the semiconductor device 1. For example, nitrogen is used as the n-type impurity, and aluminum or boron is used as the p-type impurity. By implanting ions in a state in which the temperature of the substrate 10 is heated to about 600°C, it is possible to suppress the occurrence of crystal defects in the ion-implanted region. Furthermore, by adopting box implantation as the ion implantation method, it is possible to realize a uniform impurity concentration distribution in the depth direction. Hereinafter, the substrate 10 in which each region is formed by doping impurities is also referred to as a "base".

[0044] 17, an interlayer insulating film 50 is formed on the surface of the base body 100. For example, a silicon oxide film is formed as the interlayer insulating film 50. The silicon oxide film may be formed by thermal CVD or plasma CVD.

[0045] Thereafter, a part of the interlayer insulating film 50 is selectively removed to form the first main electrode 41 and the second main electrode 42. For example, a photoresist film formed on the surface of the interlayer insulating film 50 is patterned by photolithography technology to expose the region of the interlayer insulating film 50 to be removed to arrange the first main electrode 41 and the second main electrode 42. Then, using the patterned photoresist film as a mask, a part of the interlayer insulating film 50 is selectively etched. The etching method may be a dry etching method using ions reactive with a silicon oxide film, or a wet etching method using hydrofluoric acid. Then, the first main electrode 41 and the second main electrode 42 are formed on the upper surface of the base 100 exposed by removing a part of the interlayer insulating film 50. The first main electrode 41 and the second main electrode 42 may be formed by a lift-off method or the like. The conductive material of the first main electrode 41 and the second main electrode 42 may be, for example, a nickel film or other metal material. With the above, the semiconductor device 1 shown in FIG. 1 is completed.

[0046] By the above manufacturing method, the first distance d is 10 times the second distance h. minutes The semiconductor device 1 is manufactured so that the thickness of the first region 24 is 3 μm and the distance between the first region 24 and the second region 25 along the main surface direction of the substrate 10 is 4.5 μm. This allows the current flowing between the first main electrode 41 and the second main electrode 42 to also flow on the surface of the base 100. As a result, the loss of the pn junction diode can be reduced.

[0047] In the above manufacturing method, the second well region 23 is formed after the first region 24 and the contact region 26 are formed. However, the first region 24 and the contact region 26 may be formed after the second well region 23 is formed.

[0048] Second Embodiment As shown in Fig. 18, the semiconductor device 1a according to the second embodiment includes a gate electrode 31 disposed between a first main electrode 41 and a second main electrode 42. The gate electrode 31 faces the drift region 21, the first well region 22, and the first region 24 via an interlayer insulating film 50. The semiconductor device 1a shown in Fig. 18 differs from the first embodiment in that it further includes a gate electrode 31. In other respects, the semiconductor device 1a according to the second embodiment is similar to the first embodiment.

[0049] 18 is a transistor with a planar structure in which a first main electrode 41 serves as a source electrode and a second main electrode 42 serves as a drain electrode. The first region 24 is a source region, and the second region 25 is a drain region. The regions of the interlayer insulating film 50 that contact the drift region 21, the first well region 22, and the first region 24 function as a gate insulating film.

[0050] In the semiconductor device 1a, the main current flowing between the first main electrode 41 and the second main electrode 42 is controlled by the potential of the gate electrode 31. For this reason, the gate electrode 31 is disposed in the path of the main current flowing between the first main electrode 41 and the second main electrode 42. During ON operation, an inversion layer is formed in a region of the first well region 22 that contacts the interlayer insulating film 50 (hereinafter also referred to as a "channel region"). The operation of the semiconductor device 1a will be described below.

[0051] In an on operation, a positive potential is applied to the second main electrode 42 with respect to the potential of the first main electrode 41. The first main electrode 41 is electrically connected to the first region 24, the first well region 22, the contact region 26, and the second well region 23. Therefore, the first region 24, the first well region 22, the contact region 26, and the second well region 23 are all at the reference potential.

[0052] With the potentials of the first main electrode 41 and the second main electrode 42 set as described above, the potential of the gate electrode 31 is controlled. This causes the semiconductor device 1a to operate as a transistor. That is, by setting the voltage between the gate electrode 31 and the first main electrode 41 to a predetermined threshold voltage or higher, an inversion layer is formed in the channel region of the first well region 22. This causes the semiconductor device 1a to be turned on, and a main current flows between the first main electrode 41 and the second main electrode 42. At this time, the potential of the second main electrode 42 is, for example, 1 V or less, depending on the on-resistance of the semiconductor device 1a.

[0053] On the other hand, in the off operation, the voltage between the gate electrode 31 and the first main electrode 41 is set to a predetermined threshold voltage or less, whereby the inversion layer in the first well region 22 disappears and the main current is cut off between the first main electrode 41 and the second main electrode 42.

[0054] In the return operation in the off state of the semiconductor device 1a, when a potential of -3V or more is applied to the second main electrode 42 with respect to the potential of the first main electrode 41 as a reference, the body diode of the semiconductor device 1a becomes conductive, and a current flows from the first main electrode 41 to the second main electrode 42. The result of simulating the current distribution inside the semiconductor device 1a at this time is shown in FIG. 19. The conditions of the simulation are that the first distance d is 0.3 μm and the second distance h is 4.5 μm. Since the width of the depletion layer extending from the first region 24 to the first well region 22 is narrow, a current also flows on the surface of the semiconductor device 1a as shown in FIG. 19. Therefore, the loss of the current flowing through the body diode of the pn junction formed between the first well region 22 and the drift region 21 is small. Therefore, the loss of the semiconductor device 1a can be reduced.

[0055] As described above, the semiconductor device 1a according to the second embodiment can realize a transistor having a body diode with low loss. The rest is substantially the same as the first embodiment, and therefore a duplicated description will be omitted.

[0056] A method for manufacturing the semiconductor device 1a according to the second embodiment will be described below. Note that the method for manufacturing the semiconductor device 1a described below is one example, and various other manufacturing methods, including modifications, can be used. Also, detailed descriptions of parts that overlap with the method for manufacturing the semiconductor device 1 according to the first embodiment will be omitted. Below, a case where an insulating silicon carbide substrate is used for the substrate 10 will be described.

[0057] First, the drift region 21, the first well region 22, the second well region 23, the first region 24, the second region 25, and the contact region 26 are formed in the substrate 10 in the same manner as described with reference to FIGS. 11 to 16. Then, as shown in FIG. 20, an interlayer insulating film 50 that becomes a gate insulating film and a gate electrode 31 are formed. The gate insulating film may be formed by a thermal oxidation method or a deposition method. When the gate insulating film is formed by a thermal oxidation method, the base body 100 is heated to a temperature of about 1100° C. in an oxygen atmosphere. As a result, a silicon oxide film is formed in all parts of the base body 100 that are in contact with oxygen. Alternatively, the gate insulating film may be formed by thermal oxidation in an NO or N2O atmosphere. In that case, the temperature is preferably 1100° C. to 1400° C. The thickness of the gate insulating film is, for example, about several tens of nm. The thickness of the gate insulating film can be appropriately set according to the application of the semiconductor device 1.

[0058] After forming the interlayer insulating film 50 that will become the gate insulating film, the gate electrode 31 is formed on a part of the upper surface of the interlayer insulating film 50. The material of the gate electrode 31 is generally a polysilicon film. Here, a case where the polysilicon film is used for the gate electrode 31 will be described. A low pressure CVD method or the like may be used as a deposition method of the polysilicon film. The film thickness of the gate electrode 31 may be, for example, about 1 μm. After the polysilicon film is deposited, an annealing process is performed at 950° C. in phosphorus oxychloride (POCl3) to form an n-type polysilicon film and make the polysilicon film conductive. Thereafter, the formed polysilicon film is etched to form the gate electrode 31 into a predetermined shape. The etching method may be an isotropic etching method or an anisotropic selective etching method. The etching mask may be a resist film. After etching the polysilicon film, the resist film of the etching mask is removed by oxygen plasma, sulfuric acid, or the like.

[0059] Next, the first main electrode 41 and the second main electrode 42 are formed by the same steps as in the first embodiment. In this manner, the semiconductor device 1a shown in FIG.

[0060] (Third embodiment) The configuration of the semiconductor device 1b according to the third embodiment is shown in FIG. 21. The semiconductor device 1b has a configuration in which a buffer region 251, a drift region 21, and a first well region 22 are stacked on the upper surface of a substrate 10. A first region 24 is selectively disposed on a part of the upper surface of the first well region 22. A second well region 23 is disposed adjacent to the first region 24 on the upper surface of the first well region 22 in the remaining region of the region in which the first region 24 is disposed. A contact region 26 is disposed on the upper surface of the second well region 23. A first main electrode 41 is disposed across the upper surface of the first region 24 and the upper surface of the contact region 26. A second main electrode 42 is disposed on the entire lower surface of the substrate 10.

[0061] In the semiconductor device 1b, the buffer region 251 and the substrate 10 function as the second region 25. The buffer region 251 is a region of the first conductivity type having a higher impurity concentration than the drift region 21. By disposing the buffer region 251 between the substrate 10 and the drift region 21, it is possible to control the electric field distribution. The buffer region 251 is formed in the substrate 10 by, for example, an epitaxial growth method.

[0062] A trench is formed in the base 100b, extending from the upper surface of the first region 24, penetrating the first region 24 and the first well region 22, and having its bottom reach the drift region 21. A gate insulating film 30 is formed on the inner wall surface of the trench in contact with the drift region 21, the first well region 22, and the first region 24. A gate electrode 31 is disposed inside the trench. In other words, the semiconductor device 1b is a transistor with a trench gate structure. This differs from the second embodiment in that the gate electrode 31 is disposed inside a trench (hereinafter referred to as a "gate trench") provided in the base 100b.

[0063] 21, the surface of the first region 24 that contacts the gate insulating film 30 is the opposing surface 242. In other words, the first distance d is the width of the first region 24 along the main surface of the substrate 10. The second distance h is the sum of the film thickness of the first well region 22 and the film thickness of the drift region 21.

[0064] The basic operation of the semiconductor device 1b is similar to that of the semiconductor device 1a according to the second embodiment. That is, in the semiconductor device 1b, the main current flowing between the first main electrode 41 and the second main electrode 42 is controlled by the potential of the gate electrode 31. During the ON operation, an inversion layer is formed in the channel region of the first well region 22 that contacts the gate insulating film 30.

[0065] In the semiconductor device 1b, a channel region is formed on the sidewall of the gate groove, so the channel width is proportional to the depth of the gate groove. Therefore, by deepening the gate groove, the channel width increases and the channel resistance can be reduced. In the semiconductor device 1b, an increase in the channel width does not increase the substrate area, so the semiconductor device 1b can be made smaller. In other words, the on-resistance per unit area of ​​the substrate is reduced. According to the semiconductor device 1b, a semiconductor device with reduced loss can be realized.

[0066] A method for manufacturing the semiconductor device 1b according to the third embodiment will be described below. Note that the method for manufacturing the semiconductor device 1b described below is an example, and various other manufacturing methods, including modifications, can be used. Also, detailed descriptions of parts that overlap with the method for manufacturing the semiconductor device 1 according to the first embodiment will be omitted.

[0067] First, a laminate of the substrate 10 and the buffer region 251 is formed. An insulating silicon carbide substrate (SiC substrate) may be used for the substrate 10. For example, an n-type silicon carbide substrate having a thickness of about several tens of nm to several hundreds of μm is used for the substrate 10. Then, an n-type silicon carbide epitaxial layer having a thickness of 0.1 μm to several μm is formed on the substrate 10 as the buffer region 251.

[0068] Next, the drift region 21 is formed by epitaxial growth. For example, the impurity concentration of the drift region 21 is 1E14 to 1E18 cm -3 The film thickness is several μm to several tens of μm.

[0069] Thereafter, a first well region 22 is formed above the drift region 21 by ion implantation or the like. For example, a p-type impurity is aluminum, the depth is 0.8 μm, and the impurity concentration is 1E17 cm -3 The first well region 22 is formed.

[0070] Next, the first region 24 is formed by ion implantation or the like in a part of the upper part of the first well region 22. For example, using a silicon oxide film patterned on the upper surface of the first well region 22 as a mask, a 1 μm deep ion implantation is performed with nitrogen as an n-type impurity and an impurity concentration of 1E19 cm -3 The first region 24 is then formed. Furthermore, a contact region 26 adjacent to the first region 24 is formed in a portion of the upper part of the first well region 22 by ion implantation or the like. For example, the p-type impurity is aluminum, and the contact region 26 is implanted to a depth of 0.3 μm and to a dopant concentration of 1E20 cm -3 The contact region 26 is formed.

[0071] Further, the second well region 23 is formed below the contact region 26 by ion implantation or the like. For example, the p-type impurity is aluminum, the depth is 0.3 μm to 1 μm, and the impurity concentration is 1E19 cm -3 Thus, the second well region 23 is formed. Through the above steps, the base body 100b shown in FIG.

[0072] Thereafter, a gate trench is formed so as to extend from the upper surface of the first region 24, penetrate the first region 24 and the first well region 22, and have a bottom portion reaching the drift region 21. For example, the gate trench is formed by anisotropic etching using a mask material patterned by photolithography. As a method for forming the gate trench, a dry etching method is preferably used for the substrate 10, which is a silicon carbide substrate.

[0073] After the gate groove is formed, a gate insulating film 30 is formed so as to cover the inner wall surface of the gate groove. The method for forming the gate insulating film 30 may be a thermal oxidation method or a deposition method.

[0074] Next, the inside of the gate groove is filled to form the gate electrode 31. For example, a polysilicon film is used for the gate electrode 31. A method for depositing the polysilicon film can be a low pressure CVD method. For example, the thickness of the polysilicon film to be deposited is set to a value greater than half the width of the gate groove, and the inside of the gate groove is filled with the polysilicon film. Since the polysilicon film is formed from the inner wall surface of the gate groove, the gate groove can be completely filled with the polysilicon film by setting the thickness of the polysilicon film as described above. For example, when the width of the gate groove is 2 μm, the polysilicon film is formed so that the film thickness is greater than 1 μm. After the polysilicon film is deposited, an annealing process is performed in phosphorus oxychloride (POCl3) at 950° C. to form an n-type polysilicon film and make the polysilicon film conductive. Thereafter, the formed polysilicon film is etched to form the gate electrode 31 into a predetermined shape.

[0075] Thereafter, the first main electrode 41 and the second main electrode 42 are formed by using, for example, a lift-off method, etc. In this manner, the semiconductor device 1b shown in FIG.

[0076] (Fourth embodiment) The configuration of a semiconductor device 1c according to the fourth embodiment is shown in Fig. 23. In the semiconductor device 1c, similar to the semiconductor device 1a shown in Fig. 18, a drift region 21 and a first well region 22 are formed adjacent to each other in a plan view on a substrate 10. A first region 24 and a second well region 23 face the drift region 21 via the first well region 22. A second region 25 is connected to the drift region 21 at a position spaced apart from the first well region 22. A gate electrode 31 is disposed between a first main electrode 41 and a second main electrode 42.

[0077] Unlike the semiconductor device 1a shown in FIG. 18, in the semiconductor device 1c, a gate trench having an opening spanning the drift region 21, the first well region 22, and the first region 24 is formed, and a gate insulating film 30 is disposed on the inner wall surface of the gate trench. The side surface of the gate trench contacts the drift region 21, the first well region 22, and the first region 24. A gate electrode 31 is disposed inside the gate trench. As for the other configurations, the semiconductor device 1c shown in FIG. 23 is similar to the semiconductor device 1a according to the second embodiment shown in FIG. 18.

[0078] Fig. 24 shows a cross-sectional view taken along the AA direction in Fig. 23. The gate electrode 31 embedded in the gate groove faces the drift region 21, the first well region 22 and the first region 24 on the side surface of the gate groove via the gate insulating film 30.

[0079] In the semiconductor device 1c, during on-operation, an inversion layer is formed in the channel region in contact with the side surface of the gate groove in the first well region 22. Therefore, the deeper the gate groove in which the gate electrode 31 is embedded, the wider the inversion layer becomes. Therefore, in the semiconductor device 1c, by forming the gate groove deep in the first well region 22, the width of the inversion layer can be increased without increasing the size in a plan view, thereby reducing the channel resistance. As a result, the on-resistance per unit area is reduced. In this way, the semiconductor device 1c can realize a semiconductor device with further reduced losses. The rest is substantially the same as the first to third embodiments, and duplicated descriptions will be omitted.

[0080] A method for manufacturing the semiconductor device 1c according to the fourth embodiment will be described below. Note that the method for manufacturing the semiconductor device 1c described below is an example, and various other manufacturing methods, including modifications, can be used. In the following, a case where a silicon carbide substrate is used as the substrate 10 will be described.

[0081] 11 to 16, the drift region 21, the first well region 22, the second well region 23, the first region 24, the second region 25, and the contact region 26 are formed in the substrate 10. In this manner, the base body 100c shown in FIG.

[0082] 26, a gate groove 300 having an opening that spans the first region 24, the first well region 22, and the drift region 21 on the upper surface of the base body 100c is formed in the base body 100c. For example, the gate groove 300 is formed by anisotropic etching using a mask material patterned by photolithography. As a method for forming the gate groove 300, a dry etching method is preferably used for the substrate 10, which is a silicon carbide substrate.

[0083] After the gate groove 300 is formed, the gate insulating film 30 is formed so as to cover the inner wall surface of the gate groove 300 and the upper surface of the base body 100c. The method for forming the gate insulating film 30 may be a thermal oxidation method or a deposition method.

[0084] Next, the inside of the gate trench 300 is filled to form the gate electrode 31. For example, a polysilicon film is used for the gate electrode 31. The gate electrode 31 may be formed in the same manner as described in the manufacturing method of the semiconductor device 1b according to the third embodiment. That is, the inside of the gate trench 300 is filled with a polysilicon film. Then, an n-type polysilicon film is formed by annealing to give the polysilicon film conductivity. Thereafter, the polysilicon film is etched to form the gate electrode 31 in a predetermined shape.

[0085] Thereafter, the first main electrode 41 and the second main electrode 42 are formed by using, for example, a lift-off method, etc. Through the above steps, the semiconductor device 1c shown in FIG.

[0086] Fifth embodiment The configuration of a semiconductor device 1d according to the fifth embodiment is shown in Fig. 27. In the semiconductor device 1d, similar to the semiconductor device 1a shown in Fig. 18, the drift region 21 and the first well region 22 are arranged adjacent to each other in a plan view on the substrate 10. The first region 24 and the second well region 23 face the drift region 21 via the first well region 22. The second region 25 is connected to the drift region 21 at a position spaced apart from the first well region 22. The gate electrode 31 is arranged between the first main electrode 41 and the second main electrode 42.

[0087] 18, the semiconductor device 1d further includes a second conductivity type collector region 27 that is connected to the drift region 21 at a position spaced apart from the first well region 22 and electrically connected to a second main electrode 42. For example, as shown in FIG. 27, the second region 25 and the collector region 27 are disposed adjacent to each other. The second main electrode 42 is disposed in contact with the upper surfaces of the second region 25 and the collector region 27. The other configurations of the semiconductor device 1d are similar to those of the semiconductor device 1a according to the second embodiment shown in FIG. 18.

[0088] In the semiconductor device 1d according to the fifth embodiment, the second region 25 and the collector region 27 are at the same potential. This allows the semiconductor device 1d to form a reverse conducting insulated gate bipolar transistor (RC-IGBT). The semiconductor device 1d can realize an RC-IGBT having a body pn junction diode with low loss. Note that the gate electrode 31 may also be disposed inside the gate groove in the semiconductor device 1d.

[0089] The collector region 27 may be formed by ion implantation at the same time as the contact region 26. For example, a silicon oxide film patterned by photolithography is used as a mask to implant a p-type impurity of aluminum to a depth of 0.5 μm and an impurity concentration of 1E20 cm -3 Then, a collector region 27 and a contact region 26 are formed. The other manufacturing methods are the same as those of the semiconductor device 1a according to the second embodiment.

[0090] (Other embodiments) As described above, the present invention has been described by the embodiment, but the description and drawings forming a part of this disclosure should not be understood as limiting the present invention. Various alternative embodiments, examples and operating techniques will become apparent to those skilled in the art from this disclosure.

[0091] For example, although an example in which an n-type polysilicon film is used for the gate electrode 31 has been described above, a p-type polysilicon film may also be used for the gate electrode 31. In addition, other semiconductor materials may also be used for the gate electrode 31, and other conductive materials such as metal materials may also be used for the gate electrode 31. For example, p-type polysilicon carbide, SiGe, Al, etc. may also be used as the material for the gate electrode 31.

[0092] Moreover, although an example in which a silicon oxide film is used for the gate insulating film 30 has been described, a silicon nitride film may be used for the gate insulating film 30. Alternatively, a laminated film of a silicon oxide film and a silicon nitride film may be used for the gate insulating film 30. When a silicon nitride film is used for the gate insulating film 30, isotropic etching can be performed by cleaning with hot phosphoric acid at 160°C.

[0093] Thus, it goes without saying that the present invention includes various embodiments that are not described here. [Explanation of symbols]

[0094] 1...Semiconductor device 10...Substrate 21…Drift area 22...First well region 23...Second well region 24...First area 25...Second area 26…Contact area 27…Collector region 30...Gate insulating film 31...Gate electrode 41...1st main electrode 42…Second main electrode 50...Interlayer insulating film

Claims

1. A substrate; a drift region of a first conductivity type formed in the substrate; a first well region of a second conductivity type formed in the substrate adjacent to the drift region; a first region of a first conductivity type facing the drift region via the first well region; a second well region of a second conductivity type, the second well region being adjacent to the first region and having a higher impurity concentration than the first well region, the second well region being opposed to the drift region via the first well region; a second region of the first conductivity type connected to the drift region at a position spaced apart from the first well region; a first main electrode electrically connected to the first region and the second well region; a second main electrode electrically connected to the second region; Equipped with A distance from a connection surface between the first region and the second well region to an opposing surface of the first region that faces the connection surface is equal to or less than one tenth of a distance from the first region to the second region. A semiconductor device comprising:

2. a gate insulating film in contact with the drift region, the first well region, and the first region; a gate electrode disposed between the first main electrode and the second main electrode, facing the drift region, the first well region, and the first region via the gate insulating film; 2. The semiconductor device according to claim 1, further comprising:

3. 3. The semiconductor device according to claim 2, further comprising a collector region of a second conductivity type connected to the drift region at a position spaced apart from the first well region and electrically connected to the second main electrode.

4. the gate insulating film is disposed on an inner wall surface of a trench having a side surface in contact with the drift region, the first well region, and the first region; The gate electrode is disposed inside the groove.

4. The semiconductor device according to claim 2, wherein the first insulating layer is a conductive layer.

5. 5. The semiconductor device according to claim 1, wherein the substrate is made of a wide band gap semiconductor.

6. 6. The semiconductor device according to claim 1, wherein the substrate is a silicon carbide substrate.

7. 7. The semiconductor device according to claim 1, wherein the substrate is a semi-insulating substrate or an insulating substrate.

8. forming a drift region of a first conductivity type in a substrate; forming a first well region of a second conductivity type in the substrate adjacent to the drift region; forming a first region of a first conductivity type facing the drift region via the first well region; forming a second well region of a second conductivity type adjacent to the first region, the second well region facing the drift region with the first well region interposed therebetween and having an impurity concentration higher than that of the first well region; forming a second region of a first conductivity type connected to the drift region at a position spaced apart from the first well region; forming a first main electrode electrically connecting the first region and the second well region; forming a second main electrode electrically connected to the second region; Including, A distance from a connection surface between the first region and the second well region to an opposing surface of the first region that faces the connection surface is equal to or less than one tenth of a distance from the first region to the second region.

4. A method for manufacturing a semiconductor device comprising the steps of:

Citation Information

Patent Citations

  • Power devices in wide bandgap semiconductors

    JP2002506569A

  • Semiconductor device

    JP2013232577A

  • Semiconductor device and semiconductor device production method

    WO2018150467A1

  • Semiconductor device and method of manufacturing semiconductor device

    WO2019202350A1