Apparatus and method for providing wafer planarity during growth - Patents.com

The apparatus addresses wafer bending by using individually controlled heating zones and a bending measurement system to maintain planarity, ensuring crack-free and uniform semiconductor growth.

JP7581608B2Active Publication Date: 2024-11-13ヴェエコ エスアイシー シーブイディ システムズ エービー
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2021560636
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-04-12
Filing Date
2020-04-08
Publication Date
2024-11-13
Estimated Expiration
2040-04-08

AI Technical Summary

Technical Problem

Bending of semiconductor wafers during growth processes leads to catastrophic cracking upon cooling, as internal stresses from growth layers cannot be compensated, affecting the uniformity and quality of the semiconductor material.

Method used

An apparatus with separate upper and lower individually controlled heating zones and a bending measurement system adjusts the temperature profile across the wafer surface to maintain planarity, using an automatic control circuit to compensate for bending by varying the temperature of these zones.

Benefits of technology

The apparatus effectively maintains wafer flatness during high-temperature growth, preventing cracking and ensuring uniform semiconductor quality by continuously monitoring and adjusting the temperature to counteract internal stresses.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007581608000001
    Figure 0007581608000001
  • Figure 0007581608000002
    Figure 0007581608000002
  • Figure 0007581608000003
    Figure 0007581608000003
Patent Text Reader

Abstract

An apparatus for ensuring planarity of semiconductor wafers (4) during growth at elevated temperatures in a growth chamber (14) disposed within a reactor housing (11, 12, 13), comprising a growth chamber (14) having a port for depositing at least one wafer (4) onto a rotating susceptor (2) within the growth chamber (14) and for allowing the wafer (4) to be withdrawn from the growth chamber, the growth chamber (14) having an inlet channel (17) for supplying a process gas (5) and an outlet channel (18) for exhausting unconsumed process gas (5). The growth chamber (14) further includes separate heaters (V1-V6) disposed adjacent to the growth chamber (14) for generating process gas flow between the channels and for heating the rotating wafer (4) with separately controlled heating zones both above and below the wafer (4), and an instrument (6) disposed for measuring bending of the wafer (4), wherein the automatic control circuit uses data from the temperature sensors (20) or measurement data of the power supplied to the heaters, and the instrument (6) is disposed to measure the bending of the wafer and vary the temperature of the temperature zones to minimize bending of the wafer (4).
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an apparatus for monitoring, during growth of a wafer of semiconductor material in a growth chamber at elevated temperatures, a predetermined planarity of the wafer achieved during the growth process. [Background technology]

[0002] When producing semiconductor materials by chemical vapor deposition (CVD), it is important to obtain a uniform quality of the material, which depends on the various conditions prevailing during the growth process, often referred to as the growth of the material.

[0003] Growth occurs on a wafer that is usually placed on a base disk (susceptor) made of a solid material, for example graphite. The wafer is heated, in particular by the susceptor, during which growth takes place at an elevated temperature in a growth chamber. Gases, including vapors containing the elements necessary for growth, i.e. the creation of the crystalline structure to be worked up in the semiconductor material, are admitted in a controlled manner into the chamber. The wafer is usually rotated during growth. In some cases, the wafer bends during the growth process. This can be caused by non-uniform temperatures around the wafer, internal stresses in the wafer, or stresses caused by the growth occurring on the wafer. Usually, internal stresses are material properties that cannot be determined before the start of the growth process. DISCLOSURE OF THEINVENTION [Problem to be solved by the invention]

[0004] For larger diameter wafers, when the growth process is finished, the wafer can bend again to room temperature, resulting in catastrophic cracking. As the wafer tries to return to its original shape, internal stresses are increased by the added growth layers, and these internal stresses cannot be offset by the changed distance between the crystal planes built by the atoms from the gases used to achieve a given semiconductor material. This causes cracks to form in the grown material.

[0005] Methods exist to measure the bending of the wafer and to control it during the growth process. The bending can be compensated for, for example, by a modified distribution between the various gases in the growth chamber, generating forces that cause the bending in the opposite direction. However, if the distribution between the different gases changes, the properties of the resulting semiconductor also change in undesirable ways.

[0006] The patent document EP 1275135 is assumed to constitute the closest prior art in the relevant technical field. It describes the arrangement of different temperature zones in the gas before and after the gas flow over the wafer in order to create the requirement to avoid bending of the wafer. However, there is no mention in said document of the detection of possible deviations in the planarity of the wafer during the growth process as well as any arrangement to counteract bending of the wafer in real time based on the detected deviations from the wafer planarity. [Means for solving the problem]

[0007] According to one aspect, the present invention provides an apparatus for ensuring flatness of a semiconductor wafer during growth at an increased temperature in a growth chamber, the apparatus being contained within a reactor housing surrounding a growth chamber, the growth chamber allowing deposition of at least one wafer onto a rotating susceptor in the growth chamber and having a port for withdrawing the wafer from the growth chamber, the growth chamber further having an inlet channel for supplying process gas and an outlet channel for exhausting unconsumed process gas to generate a process gas flow between said channels, and separate heaters are disposed adjacent to the growth chamber for heating the rotating wafer with separately controlled heating zones both above and below the wafer. Additionally, an instrument is disposed to measure the bending of the wafer at at least one location. An automatic control circuit uses data from the temperature sensors and the bending measuring instrument to vary the temperature of the heating zones to minimize the bending of the wafer.

[0008] Measurement of the wafer curvature can be performed with optical methods, for example with the EpiCurve® TT Gen 3. The magnitude of the curvature depends on the diameter of the wafer and is therefore often expressed as the radius of the curvature, km -1 The larger the radius, the smaller the curvature. The measurement method tested in connection with the present invention is 7000 km -1 The convex radius is equivalent to 800 km, and the concave radius is equivalent to 800 km. -1 During growth, the radius of curvature is often as large as 50 km. -1 before and after, well within the range required by this measurement method. The bending is measured at independent positions at different distances from the center of the wafer by measuring the reflection of a laser beam sent towards the wafer. By measuring the difference between the angle of the reflected beam in those reflections from the two different positions, the bending can be determined. The bending of the wafer is measured continuously.

[0009] The temperature of the heater is adjusted at regular time intervals by an automatic control circuit, which can be done with a period of 30 seconds. The adjustment is made according to table values ​​in relation to the measured bending. If the bending is concave, i.e. if the edge of the wafer is higher than the central part of the wafer, the temperature of the upper side must generally be increased with respect to the lower side. In this specification, it is mentioned that the heaters are arranged adjacent to the growth chamber. The concept "separate heaters" refers here to heaters whose temperature is measured and whose power is controlled separately with respect to each other.

[0010] The susceptor rotates around a shaft that is positioned perpendicular to the gas flow above the susceptor. The heater design is not given, instead they can be positioned according to the conduct of the gas flow in the growth chamber. In the solution disclosed herein, a horizontal gas flow is shown, where the process gas flow passes mainly horizontally across the horizontally positioned susceptor with one or more wafers on its surface. In other applications, the process gas can be introduced above the center of the susceptor and pumped away towards its periphery. Today, several methods of process gas flow configurations are used.

[0011] The process gases flowing into the growth chamber cool the susceptor, so the heater must be designed according to the gas flow behavior. The heaters above and below the susceptor are controlled separately. In the disclosed embodiment of the invention, a linear heater is used that runs perpendicular to the horizontal gas flow through the growth chamber, where the heater is located both above and below the susceptor. The principles of the apparatus according to the invention can be used for other designs of growth chamber, susceptor position, and process gas flow as well, by positioning the heaters such that those designs establish controlled heating zones above and below the susceptor and thereby above and below the growing wafer. When the wafer tends to bow due to internal stresses or stresses caused by additional growth layers, the wafer can be kept flat by the present invention by establishing a controlled variation of the temperature profile across the surface of the wafer, a process that is automatically monitored with a feedback control circuit. [Brief description of the drawings]

[0012] [Figure 1] FIG. 1 shows a schematic diagram of an apparatus according to an embodiment of the present invention. [Diagram 2] FIG. 2 shows a schematic perspective view of an apparatus according to the invention, in which the reactor, the growth chamber and the channels for the process gases are shown in a longitudinal section through the growth chamber when the apparatus is placed in the illustrated reactor. [Diagram 3] FIG. 3 shows a longitudinal section through the growth chamber according to FIG. 2, where the position of the heater relative to the growth chamber and the wafer is shown. [Figure 4] FIG. 4 shows a plan view from above of the lower half of the growth chamber shown in FIG. 3, revealing the susceptor, wafer, and heater group below the growth chamber. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] In the following, some embodiments of the present invention will be described with reference to the accompanying drawings, which merely illustrate the principles of the present invention in a schematic manner and do not require the proportions between the different elements to be shown to scale.

[0014] Here, an embodiment of the device according to the invention is presented. As mentioned above, the configuration of the growth chamber and the channels for the process gases can be designed in various ways. The principles of the invention can be transferred to other shapes of reactors by adapting the elements shown in the embodiment presented here.

[0015] FIG. 1 shows only the internal elements used in a reactor for growing layers of semiconductor material on a wafer. The illustrated example of the device is used in a reactor for growing gallium nitride on silicon. This type of growth requires very high temperatures, usually between 900° C. and 1500° C., which can lead to defects in the crystalline material mentioned above. The device according to the invention is referred to as 1. Here, a susceptor 2 is shown, which is arranged to rotate around a shaft 3. A wafer 4 is arranged on the susceptor 2, whereby the wafer rotates together with the susceptor. The growth of the semiconductor material takes place on the upper side of the wafer 4. In the figure, the process gases used for the growth of the semiconductor material are shown to flow horizontally from left to right towards the outlet in the figure. The process gas flow is indicated with the reference 5. Heaters are arranged both below and above the susceptor 2, six different heaters are arranged in the illustrated example, indicated as V1, V2, V3, V4, V5, V6. The heaters are manufactured as graphite members (or elements) by way of example. As mentioned above, the bending of the wafer is measured by a laser beam 6 which is directed at a very close distance, but to at least one point slightly towards the centre of the wafer and one point slightly towards the periphery of the wafer, between the heaters.

[0016] The device 1 is shown very diagrammatically inside a reactor 10 in FIG. 2, which consists of a cylindrical housing designed with a bottom 11, a lid 12 and a cylindrical wall 13. The reactor according to FIG. 2 is usually made of stainless steel. This figure shows a cross section through the reactor 10, which easily reveals inside it a growth chamber 14 open in longitudinal section. The growth chamber is made of a very heat-resistant material. The growth chamber 14 here comprises a bottom 15 and an upper wall 16. The susceptor 2 is shown submerged in the bottom 15 of the growth chamber and is arranged rotatably in the same plane as the susceptor. The reactor 10 has a port for feeding process gas, which is introduced into the growth chamber 14 via an inlet channel 17. Here, the process gas is symbolized by an arrow inside the inlet channel 17. Furthermore, the reactor 10 has a port for discharging unused process gas, which is discharged from the growth chamber 14 via an outlet channel 18. In this outlet channel 18, the flow of this unused process gas is indicated by arrows inside the outlet channel 18. Heaters V1-V6 are not shown in FIG. 2 for clarity.

[0017] The heater configuration V1-V6 arranged in the device 1 applied in the reactor 10 according to the example of FIG. 2 is visualized in FIG. 3. From this figure it can be seen that three groups of heaters are arranged, with heaters both below the bottom 15 of the growth chamber and above the upper wall 16. The heaters V1-V6 are organized in groups. The growth chamber is thus heated by the heaters V1 and V4 of the first group at the inflow of process gas into the growth chamber. The heaters V2 and V5 of the second group heat the growth chamber 14 in its central part, while the heaters V3 and V6 of the third group heat the growth chamber at the outflow of process gas from the growth chamber. The process gas is indicated here by the arrows 5. Thus, the arrangement of these heaters V1-V6 at different positions with respect to the extent of the growth chamber 14 in the length direction, the supply of heat to the central part of the wafer 4 and to its peripheral part, can be controlled and varied independently of each other, since the heater groups are individually controlled with respect to the supply of energy to them. The temperature of the upper or lower part of the growth chamber 14 can be controlled in each heater group by controlling the upper heater and the lower heater of each heater group which are independent of each other. In this embodiment, the heaters V1 to V6 are made of graphite members.

[0018] FIG. 4 shows the bottom 15 of the growth chamber 14 in a plan view from above. Here it can be clearly read how the different heater groups heat different parts of the growth chamber 14 and thus how the change in the supply of heat to the wafer 4 is established. An automatic control circuit (not shown) detects the bending value and then controls the supply of energy to the heaters V1 to V6, so that the monitored temperature profile is achieved over the entire surface of the wafer 4 so as to maintain a flat wafer. For example, if the measured bending of the wafer placed on the susceptor 2 indicates that the temperature is higher at the edge of the wafer 4 than in the central part of the wafer, the automatic control circuit increases the temperature of the upper side of the wafer at the outer parts of the wafer, thereby compensating for the upward bending of the wafer edge. This is achieved by increasing the energy supply in the heaters V4 and V6 or decreasing the energy supply via the heaters V1 and V3.

[0019] How a laser light according to a prior art measurement method is directed to a position on the wafer is shown in figure 3. By measuring the angle formed between the light beam incident on the wafer and the reflected beam, indicated at 6, and comparing it with the corresponding angle for another light beam directed to a different position on the wafer, any bending of the wafer can be determined and therefore responded to by automatic adjustment of the energy supply to the different heaters. This control is performed via the control circuit. The bending value (or amount of bending) is determined by the measurement method.

[0020] The temperature measurements are made by optical methods (use of pyrometers). There is one temperature sensor 20 in the form of a pyrometer for each heater. The pyrometers measure perpendicular to the direction of gas flow. The pyrometers are located outside the growth chamber and measure through an optical window. This is indicated by the arrows pointing from the temperature sensor 20 outside the growth chamber. The measurements are not made directly to the heaters but to the bottom 15 and top wall 16.

[0021] Instead of measuring the temperature in the growth chamber, data can be derived regarding the power applied to the heater, whereby the measured power data, along with the amount of bending, is used as a control for the control circuitry.

[0022] The electrical energy supplied to the heaters V1-V6 is introduced through the outer cylindrical wall 13 of the reactor 10 via vacuum-tight electrical bushings. These bushings also hold the heaters in their position. Between the heaters and the cold outer wall there is isolation that withstands the process gases and the high temperatures inside the reactor. The following is an invention described at the beginning of the present application. <Claim 1> 1. An apparatus for ensuring planarity of a semiconductor wafer (4) during growth at high temperatures in a growth chamber (14) disposed within a reactor housing (11, 12, 13), comprising: - a growth chamber (14) for depositing at least one wafer (4) on a rotating susceptor (2) therein and having a port allowing the wafer (4) to be withdrawn from said growth chamber (14), said growth chamber (14) further having an inlet channel (17) for the supply of a process gas (5) and an outlet channel (18) for the discharge of unconsumed process gas (5) thereby generating a process gas flow between said channels (17, 18); having separate heaters V1-V6 are positioned adjacent to the growth chamber (14) for heating the rotating wafer (4) with separately controlled heating zones both above and below the wafer (4); An instrument (6) is arranged to measure the bending of the wafer (4); an automatic control circuit arranged to vary the temperature of said temperature zones so as to minimize bending of said wafer (4) using data from any one of a) a temperature sensor (20), b) measurement data of the power to the heater, and an instrument (6) for measuring bending of the wafer. <Claim 2> 2. The apparatus according to claim 1, wherein the heaters V1 to V6 are arranged to include three heaters V1 to V3 below the growth chamber and three heaters V4 to V6 above the growth chamber. <Claim 3> 3. The apparatus according to claim 2, wherein the heaters V1 to V6 are arranged in groups, whereby the growth chamber (14) is heated at the inlet of the process gas (5) into the growth chamber using a first group of the heaters V1 and V4, the heaters V2 and V5 of a second group heat the growth chamber in its central part, and the heaters V3 and V6 of a third group heat the growth chamber (14) at the outlet of the process gas (5) from the growth chamber. <Claim 4> 2. The apparatus according to claim 1, wherein the bending of the wafer (4) is measured by an instrument that calculates the bending by means of a laser light (6) that is sent towards the wafer (4) and reflected from at least two points on the wafer (4) surface. <Claim 5> 5. The apparatus of claim 4, wherein the instrument (6) is configured to calculate an angle between a laser beam (6) incident on the wafer (4) and a laser beam (6) reflected from the wafer at at least two points on the wafer, thereby calculating whether a bending of the wafer is present. <Claim 6> A method for ensuring flatness of a semiconductor wafer (4) during high temperature growth in a growth chamber (14) according to claim 1, comprising the steps of: The bending of the wafer (4) is measured by an instrument that directs a laser beam (6) towards the wafer (4); A method in which an automatic control circuit adjusts the supply of energy to one or some of said heaters (V1-V6) to correspond to the initiated and measured bending. <Claim 7> The method according to claim 6, further comprising the step of: each of the heaters V1-V6 being individually controlled with respect to their energy supply. <Claim 8> 8. The method of claim 7, further comprising the step of controlling the temperature of the upper or lower part of the growth chamber by controlling the upper and lower heaters V1-V6 independently of each other. <Claim 9> 9. The method of claim 8, further comprising the step of ensuring that the automatic control circuitry increases the temperature of an upper outer side of the wafer (4) by increasing the energy supply to any of the heaters (V4-V6) located on the upper outer side of the wafer (4) when a bending measurement at the edge of the wafer (4) is indicated to be higher than at the center of the wafer (4). <Claim 10> 10. The method of claim 9, further comprising the step of ensuring that when bending measurements at the edge of the wafer (4) are indicated to be lower than at the center of the wafer (4), the automatic control circuit increases the temperature of the outer underside of the wafer (4) by increasing the energy supply to any of the heaters (V1-V3) located under the outer side of the wafer (4).

Claims

1. 1. An apparatus for ensuring planarity of a semiconductor wafer (4) during growth at high temperature in a growth chamber (14) disposed in a reactor housing (11, 12, 13), comprising: a growth chamber (14) for depositing at least one wafer (4) on a rotating susceptor (2) in said growth chamber (14) and having a port allowing the withdrawal of said wafer (4) from said growth chamber (14), said growth chamber (14) further having an inlet channel (17) for the supply of a process gas (5) and an outlet channel (18) for the discharge of unconsumed process gas (5) thereby generating a process gas flow between said channels (17, 18); and individual heaters (V1-V6) positioned adjacent the growth chamber (14) for heating the rotating wafer (4) with individually controlled heating zones both above and below the wafer (4); An instrument (6) is arranged to measure the bending of the wafer (4); an automatic control circuit is arranged to vary the temperature of said individually controlled heating zones so as to minimise bending of said wafer (4) using data from any one of: a) a temperature sensor (20); b) measured data from the power to the heater; and c) an instrument (6) for measuring bending of the wafer; The heaters (V1 to V6) include three heaters (V1 to V3) below the growth chamber (14) and three heaters (V4 to V6) above the growth chamber, the heaters (V1 to V6) being arranged in groups.

2. 2. Apparatus according to claim 1, wherein the heaters (V1-V6) are arranged in groups, whereby the growth chamber (14) is heated at the inlet of the process gas (5) into the growth chamber with a first group of the heaters (V1 and V4), the heaters (V2 and V5) of a second group heat the growth chamber in its central part, and the heaters (V3 and V6) of a third group heat the growth chamber (14) at the outlet of the process gas (5) from the growth chamber.

3. 2. The apparatus according to claim 1, wherein the bending of the wafer (4) is measured by an instrument that calculates the bending by means of a laser light (6) sent towards the wafer (4) and reflected from at least two points on the wafer (4) surface.

4. 4. The apparatus of claim 3, wherein the instrument (6) is configured to calculate an angle between a laser beam (6) incident on the wafer (4) and a laser beam (6) reflected from the wafer at at least two points on the wafer, thereby calculating whether a bending of the wafer is present.

5. A method for ensuring flatness of a semiconductor wafer (4) during high temperature growth in an apparatus according to claim 1, comprising the steps of: The bending of the wafer (4) is measured by an instrument that directs a laser beam (6) towards the wafer (4); A method in which an automatic control circuit adjusts the supply of energy to one or several of said heaters (V1-V6) to correspond to the initiated and measured bending.

6. The method of claim 5, further comprising the step of: each of the heaters V1-V6 being individually controlled with respect to their energy supply.

7. 7. The method of claim 6, further comprising the step of controlling the temperature of the upper or lower part of the growth chamber (14) by controlling the upper and lower heaters (V1-V6) independently of each other.

8. 8. The method of claim 7, further comprising the step of ensuring that the automatic control circuitry increases the temperature of an upper outer side of the wafer (4) by increasing the energy supply to any of the heaters (V4-V6) located on the upper outer side of the wafer (4) when bending measurements at the edge of the wafer (4) are indicated to be higher than at the center of the wafer (4).

9. 9. The method of claim 8, further comprising the step of ensuring that when bending measurements at the edge of the wafer (4) are indicated to be lower than at the center of the wafer (4), the automatic control circuitry increases the temperature of the outer underside of the wafer (4) by increasing the energy supply to any of the heaters (V1-V3) located under the outer side of the wafer (4).

Citation Information

Patent Citations

  • Epitaxial growth device and method

    JP1993259082A

  • Semiconductor manufacturing device

    JP1995283155A

  • Manufacture of single crystal thin film

    JP1997007953A

  • Stress measuring device and semiconductor manufacturing apparatus

    JP1997126913A

  • Heat treating method and heat treating device

    JP2002246318A