Method for manufacturing a semiconductor package
By aligning the mold and insulating base material to manage linear expansion coefficient differences, the method addresses the issue of conductive via defects in imprinting, achieving miniaturized and reliable conductive vias with improved high-frequency characteristics.
Patent Information
- Application Number
- JP2020151326
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-09-09
- Publication Date
- 2024-11-13
- Estimated Expiration
- 2040-09-09
AI Technical Summary
The formation of conductive vias with a minute width of 5 μm or less using an imprint method often results in short circuits or conduction failures due to improper formation, which is exacerbated by positional deviations caused by differences in linear expansion coefficients between the mold and the insulating base material.
A method is employed to form a wiring structure with conductive vias of 5 μm or less by using a non-photosensitive insulating resin, where the alignment of a mold with the insulating base material is adjusted to minimize positional deviation by controlling the difference in linear expansion coefficients between the mold and the base material during the imprinting process.
This approach effectively suppresses defects in conductive vias, enabling miniaturization and improving high-frequency characteristics while ensuring higher reliability and ease of forming consistent via widths.
Smart Images

Figure 0007581715000003 
Figure 0007581715000004 
Figure 0007581715000005
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a semiconductor package. [Background technology]
[0002] Fan-out wafer level packages (FOWLP) are often used as semiconductor packages that achieve miniaturization and high performance. FOWLPs have a redistribution layer that is larger than the area of the IC chip. The redistribution layer is generally formed by the semi-additive method using photoresist.
[0003] Patent Document 1 discloses a method for manufacturing a multilayer semiconductor package substrate by a method including forming recesses serving as via holes for interlayer connection in a non-photosensitive insulating resin layer by an imprinting technique. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2019-220547 A Summary of the Invention [Problem to be solved by the invention]
[0005] When a wiring structure having conductive vias with a minute width of 5 μm or less is formed by an imprint method, the conductive vias are not formed appropriately, and therefore short circuits or poor continuity in the wiring are likely to occur.
[0006] Therefore, one aspect of the present invention is to suppress the occurrence of defects in conductive vias when manufacturing a semiconductor package by a method that includes forming a wiring structure having conductive vias with a very small width of 5 μm or less by an imprint method using a non-photosensitive insulating resin. [Means for solving the problem]
[0007] One aspect of the present invention provides a method for manufacturing a semiconductor package including a wiring structure including a conductive via having a minimum width of 5 μm or less. The method according to one aspect of the present invention includes the steps of preparing a wiring substrate having an insulating substrate having two opposing main surfaces and a conductive layer provided on one main surface of the insulating substrate and having a pattern including a land electrode, forming a non-photosensitive insulating resin layer covering the conductive layer on the wiring substrate, forming a pattern including a via hole penetrating the insulating resin layer in the insulating resin layer by an imprinting method including pressing the mold into the insulating resin layer from the opposite side to the substrate while heating the insulating substrate and the mold to a predetermined molding temperature, and forming a metal layer including the conductive via that fills the via hole. The mold has a convex portion including a via portion having an inverted shape of the via hole and a tip surface. While the mold is pressed into the insulating resin layer, the mold is aligned to a target position set so that the tip surface of the via portion and the land electrode overlap when viewed from the thickness direction of the insulating resin layer. When the width of the tip face of the via portion is W [μm], the linear expansion coefficient of the insulating substrate is α, the difference between the molding temperature of the insulating substrate and 30°C is ΔT, and the linear expansion coefficient of the mold is β, and the difference between the molding temperature of the mold and 30°C is Δt, the value of (α×ΔT-β×Δt)×1000 is smaller than the value of W×2.5.
[0008] When forming a wiring structure having a conductive via with a minute width of 5 μm or less by the imprint method, misalignment due to the difference in the linear expansion coefficient between the mold and the insulating base material may affect the state of the conductive via formation. When the conductive via is miniaturized and the land electrode is also miniaturized accordingly, the influence of the misalignment cannot be ignored, and as a result, it is considered that the conductive via is difficult to form properly. Therefore, the inventors have found that the occurrence of defects in the conductive via can be suppressed by focusing on the linear expansion coefficients α and β of the insulating base material and the mold, respectively, and the difference ΔT and Δt between the heating temperature (molding temperature) of the insulating base material and the mold and room temperature (here, 30° C.), and by appropriately setting the relationship between the value (α×ΔT-β×Δt)×1000 calculated from these and the width W of the tip surface of the protrusion constituting the mold. Effect of the Invention
[0009] According to one aspect of the present invention, when a semiconductor package is manufactured by a method that includes forming a wiring structure having a conductive via with a minute width of 5 μm or less by an imprint method using a non-photosensitive insulating resin, the occurrence of defects in the conductive via can be suppressed.
[0010] The wiring structure formed by the method according to one aspect of the present invention includes an insulating resin layer formed of a non-photosensitive insulating resin, and therefore is easier to control the dielectric tangent and dielectric constant and has an advantage in terms of high frequency characteristics compared to wiring structures including an insulating resin layer generally formed using a highly hydrophilic photosensitive resin. In addition, non-photosensitive insulating resins tend to achieve higher reliability compared to photosensitive resins.
[0011] A conductive via formed using a photoresist has a shape in which the width increases toward the top, which limits the miniaturization of the wiring. The imprint method is advantageous in terms of miniaturization of the wiring because it can easily form a through hole with a constant width. [Brief description of the drawings]
[0012] [Figure 1]1A to 1C are process diagrams illustrating an embodiment of a method for manufacturing a semiconductor package. [Diagram 2] 1A to 1C are process diagrams illustrating an embodiment of a method for manufacturing a semiconductor package. [Diagram 3] 1A to 1C are process diagrams illustrating an embodiment of a method for manufacturing a semiconductor package. [Figure 4] 1 is a micrograph showing an example of a state of a conductive via. [Diagram 5] 1 is a micrograph showing an example of a state of a conductive via. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] Hereinafter, several embodiments of the present invention will be described in detail. However, the present invention is not limited to the following embodiments.
[0014] 1, 2 and 3 are process diagrams showing one embodiment of a method for manufacturing a semiconductor package. The method shown in FIGS. 1 to 3 includes the steps of preparing a wiring substrate 10 having an insulating substrate 1 having two opposing main surfaces S1, S2 and a conductor layer 2 provided on one of the main surfaces S1 of the insulating substrate 1, and forming a non-photosensitive insulating resin layer 3 covering the conductor layer 2 on the wiring substrate 10, forming a pattern in the insulating resin layer 3 including a via hole 31 penetrating the insulating resin layer 3 and a groove 32 for forming a wiring layer by an imprinting method including pressing the mold 5 into the insulating resin layer 3 while heating the insulating substrate 1 and the mold 5 to a predetermined molding temperature, removing the insulating resin layer 3A remaining at the bottom of the via hole 31, thereby exposing the land electrode 21, forming a metal layer 4 on the insulating resin layer 3 including a conductive via 41 filling the via hole 31 and a wiring layer 42 filling the groove 32, and removing a part of the metal layer 4 and the insulating resin layer 3 from the side opposite to the wiring substrate 10 to form a flat surface S3 on which the metal layer 4 and the insulating resin layer 3 are exposed.
[0015] The wiring structure 7 formed by the method including these steps is used, for example, as a redistribution layer connected to an IC chip in a fan-out wafer level package (FOWLP).
[0016] The insulating substrate 1 may be a sealing resin layer that seals an IC chip. In that case, the method according to the present embodiment can be applied as a method for manufacturing a FOWLP by a die-fast method. Alternatively, a temporary fixing material layer may be provided between the insulating substrate 1 and the conductor layer 2. In that case, the method according to the present embodiment can be applied as a method for manufacturing a FOWLP by a die-fast method. The insulating substrate 1 is selected in consideration of the difference in linear expansion coefficient between the insulating substrate 1 and the mold 5, as described later.
[0017] The conductor layer 2 has a pattern including a land electrode 21 and a wiring layer 22. The conductor layer 2 is formed, for example, by a semi-additive method. In the case of the embodiment illustrated in (a) of Fig. 1, the conductor layer 2 is provided on a flat main surface S1 of the insulating base material 1, but the conductor layer 2 and the insulating base material 1 may form a continuous flat surface.
[0018] As shown in FIG. 1(b), a non-photosensitive insulating resin layer 3 is formed on the wiring substrate 10. The maximum thickness of the insulating resin layer 3 may be, for example, 20 μm or less, or 6 μm or less, or 3 μm or more. The insulating resin layer 3 can be formed, for example, by applying a liquid non-photosensitive insulating resin composition to the wiring substrate 10 by a method such as spin coating or slit coating, or by laminating a dry film-like non-photosensitive insulating resin composition on the wiring substrate 10. The insulating resin layer 3 can be an insulating resin whose dielectric tangent and dielectric constant are adjusted so as to obtain good high-frequency characteristics.
[0019] 1(c), the mold 5 is pressed into the insulating resin layer 3 while the insulating base material 1 and the mold 5 are heated to a predetermined molding temperature. The mold 5 has a convex portion including a via portion 51 having an inverted shape of the via hole 31 and a tip surface 51S, and a portion 52 having an inverted shape of the groove 32 for forming the wiring layer 42. In the mold 5, the height of the portion 52 having the inverted shape of the groove 32 is lower than the height of the via portion 51. The portion 52 having the inverted shape of the groove 32 and the via portion 51 continuously form the convex portion of the mold 5.
[0020] While the mold 5 is pressed into the insulating resin layer 3, it is aligned by a press device having an alignment function and a heating function to a target position set so that the tip surface 51S of the via portion 51 and the land electrode 21 overlap when viewed from the thickness direction of the insulating resin layer 3. The actual position of the mold 5 pressed into the insulating resin layer 3 may differ to some extent from the target position due to constraints such as the accuracy of the device. The actual position of the mold 5 is, for example, within a range of 1.5 μm or less to 2.0 μm or less from the target position in the direction within the main surface S1.
[0021] Considering deviation from the target position of the mold 5, the width of the land electrode 21 may be larger than the width W of the tip surface 51S of the via portion 51. Specifically, the width of the land electrode 21 may be W μm to W+3 μm.
[0022] The mold 5 and the insulating base material 1 are each heated to a molding temperature equal to or higher than the softening temperature of the insulating resin layer 3. When the insulating resin layer 3 is thermosetting, the molding temperature may be equal to or lower than the temperature at which the thermosetting reaction of the insulating resin layer 3 starts. The molding temperature may be, for example, 150 to 300° C. The molding temperature of the mold 5 and the molding temperature of the insulating base material 1 may be the same or different.
[0023] The force with which the mold 5 is pressed is set within a range that does not destroy the via portions 51 and the land electrodes 21. The surface of the mold 5 may be subjected to a release treatment. The release treatment may be performed, for example, by spraying a release agent or by coating the surface of the mold 5 with a silane coupling agent or the like.
[0024] After the temperatures of the mold 5 and the insulating base material 1 drop from the molding temperature to room temperature (e.g., 20 to 30°C), the mold 5 is pulled out from the insulating resin layer 3 to form a pattern including the via holes 31 and the grooves 32. While the temperatures of the mold 5 and the insulating base material 1 are cooled from the molding temperature to room temperature, the relative positions of the land electrodes 21 and the via holes 31 may change due to the difference in the molding temperature and linear expansion coefficient of the mold 5 and the insulating base material 1.
[0025] The width of the tip surface 51S of the via portion 51 is W [μm], the linear expansion coefficients of the insulating substrate 1 and the mold 5 are α and β, respectively, and the difference between the molding temperature of the insulating substrate and 30°C and the difference between the molding temperature of the mold and 30°C are ΔT and Δt, respectively. The mold 5, the insulating substrate 1, and the molding temperature are selected so that the value of (α×ΔT-β×Δt)×1000 is smaller than the value of W×2.5. This makes it possible to suppress the occurrence of defects in the conductive via 41 to be formed. From the same viewpoint, the value of (α×ΔT-β×Δt)×1000 may be equal to or less than W×2.4, W×2.W×2.3, W×2.2, W×2.1, W×2.1, or W×2.0, or may be equal to or greater than W×0.1. The value of (α×ΔT-β×Δt)×1000 corresponds to the amount of misalignment caused by the difference between the product of the thermal expansion coefficient and temperature difference of the insulating substrate 1 and the product of the thermal expansion coefficient and temperature difference of the mold 5 in a 1 mm×1 mm region. From the same viewpoint as above, the value of (α×ΔT-β×Δt) may be 0.007 or less, 0.006 or less, 0.005 or less, 0.004 or less, 0.003 or less, or 0.002 or less, or may be 0.0005 or more. In this specification, the linear expansion coefficient means the linear expansion coefficient in the range of 30°C (room temperature) to 300°C.
[0026] The insulating substrate 1 may be a quartz glass substrate, a stainless steel substrate, or a cured product of an epoxy resin composition. Typical linear expansion coefficients of the respective substrates are shown in Table 1. The insulating substrate 1 may be a quartz glass substrate or a stainless steel substrate, and a temporary fixing material layer may be provided between the insulating substrate 1 and the conductor layer 2.
[0027] [Table 1]
[0028] The mold 5 may be, for example, a molded body integrally formed from quartz glass, silicon, or nickel. Table 2 shows typical thermal expansion coefficients of molds formed from these materials (mold materials).
[0029] [Table 2]
[0030] For example, when the insulating substrate 1 is an encapsulating resin layer consisting of a cured product of an epoxy resin composition, the mold 5 is a molded body of quartz glass, and the molding temperature of the insulating substrate 1 and the mold 5 is 300°C, ΔT and Δt are 270°C, the value of (α×ΔT-β×Δt) is 0.0174, and the value of (α×ΔT-β×Δt)×1000 is 17.4 μm.
[0031] When the insulating substrate 1 is an encapsulating resin layer consisting of a cured product of an epoxy resin composition, the mold 5 is a silicone molded body, and the molding temperature of the insulating substrate 1 and the mold 5 is 300°C, ΔT and Δt are 270°C, the value of (α×ΔT-β×Δt) is 0.0165, and the value of (α×ΔT-β×Δt)×1000 is 16.4 μm.
[0032] When the insulating substrate 1 is a quartz glass substrate, the mold 5 is a silicon molded body, and the molding temperature of the insulating substrate 1 and the mold 5 is 300°C, ΔT and Δt are 270°C, the value of (α×ΔT-β×Δt) is 0.00092, and the value of (α×ΔT-β×Δt)×1000 is 0.92 μm.
[0033] When the insulating substrate 1 is a stainless steel substrate, the mold 5 is a silicon molded body, and the molding temperature of the insulating substrate 1 and the mold 5 is 300°C, ΔT and Δt are 270°C, the value of (α×ΔT-β×Δt) is 0.0038, and the value of (α×ΔT-β×Δt)×1000 is 3.7 μm.
[0034] When the insulating substrate 1 is a stainless steel substrate and the mold 5 is a nickel compact, for example, the molding temperature of the insulating substrate 1 and the mold 5 is 300°C, ΔT and Δt are 270°C, the value of (α×ΔT-β×Δt) is 0.0012, and the value of (α×ΔT-β×Δt)×1000 is 1.2 μm.
[0035] After the mold 5 is removed, the insulating resin layer 3A may remain at the bottom of the via hole 31 as shown in FIG. 2(a). The conditions of the imprinting method may be optimized so that the thickness of the remaining insulating resin layer 3A is 1 μm or less. When the remaining insulating resin layer 3A is removed, the land electrode 21 is exposed at the bottom of the via hole 31 as shown in FIG. 2(b). The method for removing the remaining insulating resin layer 3A may be, for example, plasma processing or laser processing. In the case of plasma processing, the remaining insulating resin layer 3A can be removed while suppressing damage to the via hole 31 and the groove 32 by adjusting the gas and output used. For example, plasma processing using oxygen gas and fluoroform gas can be adopted.
[0036] The angle between the inner wall of the via hole 31 and the main surface S1 of the insulating substrate 1 may be 0 to 5°. If this angle is small, fine wiring can be easily formed.
[0037] After the via holes 31 and the grooves 32 are formed by the imprint method, the metal layer 4 is formed, which includes the conductive vias 41 and the wiring layer 42. The minimum width of the conductive vias 41 to be formed may be 5 μm or less, or 3 μm or less, or may be 1.0 μm or more.
[0038] The metal layer 4 is formed by a method including, for example, forming a seed layer that covers the land electrode 21 and the insulating resin layer 3 and is used as a power supply layer for plating, forming a metal plating layer on the seed layer to form the metal layer 4 including the conductive via 41 that fills the via hole 31 and the wiring layer 42 that fills the groove 32, and removing a part of the metal layer 4 and the insulating resin layer 3 from the side opposite to the wiring substrate 10 to form a flat surface S3 where the metal layer 4 and the insulating resin layer 3 are exposed. The seed layer is a layer formed by, for example, a sputtering method. A metal plating layer is formed on the seed layer. The metal plating layer may be a plating layer containing copper.
[0039] The flat surface S3 is formed by polishing the metal layer 4 and the insulating resin layer 3. A chemical mechanical polishing device or a mechanical polishing device may be used for the flat surface polishing. The metal layer 4 may be removed by immersing it in an etching solution.
[0040] By repeating the steps of forming an additional non-photosensitive insulating resin layer on the flat surface S3, forming a pattern in the additional insulating resin layer by an imprinting method, the pattern including a via hole penetrating the additional insulating resin layer and a portion having an inverted shape of the groove for forming an additional wiring layer, and forming additional conductive vias that fill the via holes and additional wiring layers that fill the grooves, a multilayer wiring structure can be formed by the process of forming one or more additional insulating resin layers, additional conductive vias that penetrate each of the additional insulating resin layers, and additional wiring layers connected to the additional conductive vias. EXAMPLES
[0041] The following shows the results of examining the relationship between the difference in linear expansion coefficient between the insulating substrate and the mold and the state of formation of the conductive vias.
[0042] A quartz glass substrate and a substrate made of a cured product of an epoxy resin composition were prepared as insulating substrates. Conductive vias were formed on these insulating substrates by an imprint method using a mold. A molded silicon body having a convex portion including a cylindrical via portion having a diameter of 2.0 μm was used as the mold. The molding temperature of the insulating substrate and the mold was 300° C. As described above, in the case of a combination of a substrate made of an epoxy resin composition and a mold made of silicon, the value of (α×ΔT-β×Δt) is 0.016, and the value of (α×ΔT-β×Δt)×1000 is 16.4 μm. In the case of a combination of a quartz glass substrate and a mold made of silicon, the value of (α×ΔT-β×Δt) is 0.00092, and the value of (α×ΔT-β×Δt)×1000 is 0.92 μm.
[0043] Figure 4 is a micrograph of conductive vias when a quartz glass substrate is used, and Figure 5 is a micrograph of conductive vias when a substrate made of a cured epoxy resin composition is used. In the case of the combination of the epoxy resin composition substrate and the silicon mold in Figure 5, many conductive vias were broken. In the case of the combination of the quartz glass substrate and the silicon mold in Figure 4, no damage to the conductive vias was confirmed. [Explanation of symbols]
[0044] 1...insulating substrate, 1...insulating substrate, 10...wiring substrate, 2...conductor layer, 22, 42...wiring layer, 3, 3A...insulating resin layer, 5...mold, 4...metal layer, 7...wiring structure, 10...wiring substrate, 21...land electrode, 31...via hole, 32...groove, 41...conductive via, 51...via portion, 51S...tip surface of via portion, 52...portion having an inverted shape of groove 32, S1, S2...main surface, S3...flat surface, W...width of tip surface 51S.
Claims
1. 1. A method for manufacturing a semiconductor package having a wiring structure including a conductive via having a minimum width of 5 μm or less, comprising: The method comprises: A process for forming a wiring substrate having an insulating substrate having two opposing main surfaces and a conductor layer provided on one main surface of the insulating substrate and having a pattern including land electrodes, and forming a non-photosensitive insulating resin layer on the wiring substrate to cover the conductor layer; forming a pattern including via holes penetrating the insulating resin layer in the insulating resin layer by an imprinting method including pressing the mold into the insulating resin layer from the side opposite to the wiring substrate while heating the insulating substrate and the mold to respective predetermined molding temperatures; forming a metal layer including a conductive via filling the via hole on the insulating resin layer; Including, the mold has a protrusion including a via portion having an inverted shape of the via hole and a tip surface, while the mold is pressed into the insulating resin layer, the mold is aligned to a target position set so that a tip end surface of the via portion and the land electrode overlap when viewed from a thickness direction of the insulating resin layer; a value of (α×ΔT−β×Δt)×1000 is equal to or greater than W×0.1 and smaller than W×2.5, where W [μm] is the width of the tip face of the via portion, α is the linear expansion coefficient of the insulating base material, ΔT is the difference between the molding temperature of the insulating base material and 30° C., and Δt is the linear expansion coefficient of the mold, β is the difference between the molding temperature of the mold and 30° C.
2. 2. The method of claim 1, wherein the value of α×ΔT−β×Δt is 0.007 or less.
3. The method of claim 1 or 2, wherein the conductive via has a minimum width of 3 μm or less.
4. The method according to any one of claims 1 to 3, wherein an angle between an inner wall of the via hole and a plane perpendicular to a main surface of the insulating substrate is 0 to 5°.
5. The method according to any one of claims 1 to 4, wherein the insulating resin layer has a thickness of 6 µm or less.
6. The method according to any one of claims 1 to 5, further comprising the step of removing the insulating resin layer remaining at the bottom of the via hole after the mold is pulled out from the insulating resin layer, thereby exposing the land electrode.
7. The metal layer is forming a seed layer covering the land electrodes and the insulating resin layer; forming a metal plating layer on the seed layer to form a metal layer including the seed layer and the metal plating layer, the metal layer including the conductive via filling the via hole; The method of any one of claims 1 to 6, wherein the compound is formed by a process comprising:
8. the convex portion of the mold further includes a portion that is lower than the via portion and has an inverted shape of a groove for forming a wiring layer, the inverted shape of the groove and the via portion continuously form the convex portion, a pattern including the via hole and the groove is formed from the insulating resin layer by the imprint method; The method according to any one of claims 1 to 7, wherein the metal layer is formed to include the conductive via filling the via hole and the wiring layer filling the trench.
9. The method comprises: removing a portion of the metal layer and the insulating resin layer from a side opposite to the wiring substrate to form a flat surface on which the metal layer and the insulating resin layer are exposed; The method according to any one of claims 1 to 8, further comprising the steps of forming an additional non-photosensitive insulating resin layer on the flat surface, forming a pattern in the additional insulating resin layer by the imprint method, the pattern including a via hole penetrating the additional insulating resin layer, and forming an additional conductive via filling the via hole, thereby forming one or more additional insulating resin layers and additional conductive vias penetrating each of the additional insulating resin layers.
10. The method according to any one of claims 1 to 9, wherein the semiconductor package is a fan-out type wafer-level package including an IC chip, and the wiring structure is a redistribution layer connected to the IC chip.
Citation Information
Patent Citations
Multilayer printed wiring board and its manufacturing method
JP2005108924A
Method for performing imprint and imprint mould, imprint device
JP2009218554A
Semiconductor device and manufacturing method of the same
JP2016048742A
Manufacturing method of multilayer semiconductor package substrate and the multilayer semiconductor package substrate
JP2019220547A