Semiconductor device and its manufacturing method
By ensuring the Ag bonding material's thickness exceeds the metal burr height by 2 μm and optimizing the back electrode structure, voids are minimized, enhancing heat dissipation and reliability in semiconductor devices.
Patent Information
- Application Number
- JP2021175883
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-10-27
- Publication Date
- 2024-11-13
- Estimated Expiration
- 2041-10-27
AI Technical Summary
Voids occur in Ag bonding material due to thermal contraction and solvent volatilization, leading to decreased heat dissipation and variations in heat dissipation, with metal burrs from the semiconductor chip's back electrode obstructing solvent discharge.
The Ag bonding material is designed with a thickness of 2 μm or more than the height of the metal burr, providing a path for void release during solvent volatilization or contraction, and the back electrode is structured to minimize burr formation.
This design reduces voids in the Ag bonding material, improving heat dissipation and reducing variations, while maintaining high reliability and minimizing thermal resistance and costs.
Smart Images

Figure 0007582156000002 
Figure 0007582156000003 
Figure 0007582156000004
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a semiconductor device and a manufacturing method thereof. [Background technology]
[0002] Solder is generally used as a bonding material between the back electrode and die pad of a semiconductor chip. In particular, when mounting on a board by reflow, high melting point solder with a high lead content has been used (see Patent Document 1, for example). However, even in applications requiring high melting point solder, such as board reflow compatible or high reliability applications, the lead content in solder is beginning to be regulated in consideration of environmental impact. In consideration of environmental impact, sintering bonding using Ag paste is being applied. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2005-150595 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, there is a problem that voids are easily generated in the Ag bonding material due to thermal contraction and evaporation of the solvent. Dicing of the semiconductor chip causes a metal burr that is roughly annular in plan view to protrude from the outer periphery of the back electrode of the semiconductor chip. It was found that this metal burr prevents the volatilized solvent generated in the Ag paste from being discharged to the outside air. There was a problem that the generation of voids caused a decrease and variation in heat dissipation.
[0005] The present disclosure has been made to solve the above-mentioned problems, and has an object to provide a semiconductor device and a manufacturing method thereof that can improve heat dissipation and reduce variations in heat dissipation. [Means for solving the problem]
[0006] The semiconductor device according to the present disclosure comprises a conductive die pad, a semiconductor chip, a back electrode provided on the back surface of the semiconductor chip, an Ag bonding material that bonds the back electrode and the die pad and contains 50-85% Ag, a terminal connected to the semiconductor chip, and an insulating sealing resin that covers the die pad, the semiconductor chip, the Ag bonding material, and a portion of the terminal, wherein a metal burr protrudes from the outer periphery of the underside of the back electrode that contacts the Ag bonding material, and the thickness of the Ag bonding material is at least 2 μm greater than the vertical height of the metal burr. Effect of the Invention
[0007] In the present disclosure, the thickness of the Ag bonding material is 2 μm or more larger than the vertical height of the metal burr. This ensures a path for discharging voids that occur due to the evaporation or shrinkage of the solvent when the Ag paste is sintered. This reduces the number of voids in the Ag bonding material. This improves heat dissipation and reduces the variation in heat dissipation. [Brief description of the drawings]
[0008] [Figure 1] 1 is a top view showing a semiconductor device according to a first embodiment. [Diagram 2] FIG. 2 is a cross-sectional view taken along line I-II of FIG. [Diagram 3] 2 is an enlarged cross-sectional view of a semiconductor chip of the semiconductor device according to the first embodiment. FIG. [Figure 4] 1A to 1C are cross-sectional views showing a method for manufacturing a semiconductor device according to a first embodiment. [Diagram 5] 1A to 1C are cross-sectional views showing a method for manufacturing a semiconductor device according to a first embodiment. [Figure 6] 1 is a cross-sectional view showing a state in which the package according to the first embodiment is surface-mounted on an insulating substrate. [Figure 7] 11 is an enlarged cross-sectional view of a mounting portion of a semiconductor chip of a semiconductor device according to a second embodiment. FIG. [Figure 8] 10A to 10C are cross-sectional views showing a manufacturing process of a semiconductor device according to a second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] A semiconductor device and a manufacturing method thereof according to an embodiment will be described with reference to the drawings. The same or corresponding components are denoted by the same reference numerals, and repeated description may be omitted.
[0010] Embodiment 1 1 is a top view showing a semiconductor device according to embodiment 1. Sealing resin 1 is rectangular in plan view. Terminals 2 and 3 protrude from opposing long sides of sealing resin 1, respectively.
[0011] Figure 2 is a cross-sectional view taken along line I-II in Figure 1. Terminals 2 and 3 and die pad 4 are conductive lead frames made of metal such as copper. Die pad 4 and terminal 2 are connected. Terminal 2 and terminal 3 are electrically isolated.
[0012] The semiconductor chip 5 is a power chip made of Si or SiC. A back electrode 6 is provided on the back surface of the semiconductor chip 5, and a front electrode 7 is provided on the front surface. An Ag bonding material 8 bonds the back electrode 6 of the semiconductor chip 5 to the die pad 4. The terminal 2 is connected to the semiconductor chip 5 via the die pad 4 and the Ag bonding material 8.
[0013] The semiconductor chip 9 is a control IC that controls the conductivity of the semiconductor chip 5. A back electrode 10 is provided on the back surface of the semiconductor chip 9, and a front electrode 11 is provided on the front surface. An Ag bonding material 12 bonds the back electrode 10 of the semiconductor chip 9 to a terminal 3. The terminal 3 is connected to the semiconductor chip 9 via the Ag bonding material 12. The Ag bonding materials 8 and 12 contain 50-85% Ag.
[0014] Wires 13 electrically connect front surface electrodes 7 of semiconductor chip 5 and front surface electrodes 11 of semiconductor chip 9. Wires 13 are made of a material such as Cu, Al, or Au. Semiconductor chip 5 is bonded to the front surface of die pad 4, and insulating layer 14 is bonded to the rear surface. Heat sink 15 is bonded to the rear surface of insulating layer 14. Heat sink 15 is made of, for example, a copper material.
[0015] An insulating sealing resin 1 covers the die pad 4, the semiconductor chips 5, 9, the Ag bonding materials 8, 12, the wires 13, and a portion of the terminals 2, 3. The back surface of the heat sink 15 is exposed from the sealing resin 1, and dissipates heat generated by the semiconductor chip 5 when current is applied to the outside. The terminals 2, 3 protruding from the side surfaces of the sealing resin 1 bend downward. The tips of the terminals 2, 3 are adjusted to a position lower than the sealing resin 1, and have board bonding portions that are parallel to the back surface of the sealing resin 1 or the heat sink 15. Having a board bonding surface allows the package to be surface-mounted on a board.
[0016] 3 is an enlarged cross-sectional view of the semiconductor chip of the semiconductor device according to the first embodiment. The back electrode 6 has an ohmic electrode 6a, an adhesive layer 6b, and an anti-oxidation electrode 6c, which are stacked in this order from the semiconductor chip 5 side. The ohmic electrode 6a is ohmic-bonded to the semiconductor chip 5. The anti-oxidation electrode 6c on the outermost surface is in contact with the Ag bonding material 8. A metal burr 16 having a substantially ring shape in a plan view protrudes downward from the outer periphery of the lower surface of the back electrode 6. The thickness t of the Ag bonding material 8 is 2 μm or more larger than the vertical height h of the metal burr 16.
[0017] Next, a method for manufacturing the semiconductor device according to the present embodiment will be described. Figures 4 and 5 are cross-sectional views showing the method for manufacturing the semiconductor device according to the first embodiment.
[0018] 4, a semiconductor wafer 18 is diced using a dicing blade 17 to separate it into individual semiconductor chips 5. During this process, the back surface electrode 6 is deformed by high temperature to form metal burrs 16.
[0019] Next, as shown in Fig. 5, Ag paste 19 is applied onto the conductive die pad 4. A semiconductor chip 5 having a back electrode 6 is placed on the Ag paste 19. The Ag paste 19 is heated at 200°C for about two hours to sinter-bond the die pad 4 and the back electrode 6. The sintered Ag paste 19 becomes the Ag bonding material 8. The thickness of the Ag paste 19 applied onto the die pad 4 is set so that the thickness of the sintered Ag bonding material 8 is at least 2 µm greater than the vertical height of the metal burrs 16.
[0020] The viscosity of the Ag paste 19 before sintering is preferably 20 Pa·S or more, and more preferably about 25 Pa·S. By using Ag paste 19 with such a high viscosity, it is possible to make the Ag paste 19 thicker with a small amount of the paste. In addition, the amount of Ag paste 19 supplied can be reduced. This prevents the Ag paste 19 from scattering due to an oversupply of Ag paste 19, from flowing onto the front surface of the semiconductor chip 5, or onto the back surface of the die pad 4, and prevents the semiconductor chip 5 from tilting. The upper limit of the thickness of the Ag paste 19 is determined by the package height, the area of the die pad 4, the paste viscosity, the tilt accuracy of the semiconductor chip 5, and the like.
[0021] Since the Ag paste 19 contains a solvent, the Ag content after sintering is 85% or less, whereas a non-paste Ag bonding material has an Ag content higher than 85%. When a non-paste Ag bonding material is used, there is no problem of voids, and therefore it is outside the scope of this disclosure.
[0022] 6 is a cross-sectional view showing a state in which the package according to the first embodiment is surface-mounted on an insulating substrate. The insulating substrate 20 has an insulating material 21 and metal wiring 22 provided on the surface of the insulating material 21. The substrate bonding surface of the terminal 2 protruding from the sealing resin 1 is bonded to the metal wiring 22 by a conductive bonding material 23.
[0023] The Ag bonding material 8, which contains 50-85% Ag, has a remelting temperature of 960° C. On the other hand, the bonding material 23 is, for example, 95% lead solder, and has a melting temperature of 300° C. Therefore, the melting temperature of the bonding material 23 is lower than the remelting temperature of the Ag bonding material 8.
[0024] After the die pad 4 and the back electrode 6 are bonded with the Ag bonding material 8 and resin-sealed, the terminals 2, 3 protruding from the sealing resin 1 are bonded to the metal wiring 22 with the bonding material 23. During this reflow, the Ag bonding material 8 in the package is also exposed to high temperatures. Therefore, the heating temperature when bonding the terminals 2, 3 to the metal wiring 22 by reflow is set lower than the remelting temperature of the Ag bonding material 8. This makes it possible to prevent the Ag bonding material 8 from remelting. Since the Ag bonding material 8 does not remelt, the reliability of the product can be maintained at a high level. Therefore, there are great benefits to using the Ag bonding material 8 in a surface-mounted semiconductor device.
[0025] As described above, in this embodiment, the thickness of the Ag bonding material 8 is 2 μm or more larger than the vertical height of the metal burr 16. This makes it possible to secure a path for discharging voids that are generated due to the evaporation or shrinkage of the solvent when the Ag paste 19 is sintered. This makes it possible to reduce voids in the Ag bonding material 8. This makes it possible to improve heat dissipation and reduce variations in heat dissipation.
[0026] It has been found that when the thickness of the Ag bonding material 8 is 2 μm or more larger than the height of the metal burr 16, the number of voids tends to decrease, and when it is 5 μm or more larger, the number of voids decreases significantly. Therefore, it is preferable that the thickness of the Ag bonding material 8 is 5 μm or more larger than the height of the metal burr 16.
[0027] The height of the metal burr 16 is proportional to the thickness of the back electrode 6. As a result of an experiment using a back electrode 6 in which Al-Si, Ti, Ni, and Au are laminated, the following relationship between the thickness of the back electrode 6 and the height of the metal burr 16 was obtained. The Al-Si layer is an ohmic electrode 6a that has good ohmic properties with the Si / SiC substrate, i.e., low contact resistance. The Au layer is an anti-oxidation electrode 6c, and the Ti layer and Ni layer are adhesive layers 6b. The thickness of the Al-Si layer is fixed at 800 μm, and the total thickness of the Au layer, Ti layer, and Ni layer is changed. The following data shows the total thickness of the anti-oxidation electrode 6c and adhesive layer 6b, excluding the ohmic electrode 6a, in the laminated structure of the back electrode 6.
[0028] [Table 1]
[0029] It was found that the occurrence of metal burrs 16 can be suppressed by reducing the total thickness of the back electrode 6. The ohmic electrode 6a can be made 100 μm or less, and can be omitted depending on the material selected for the anti-oxidation electrode 6c. It was confirmed that the occurrence of metal burrs 16 can be suppressed even when the ohmic electrode 6a is thin, just as in the case of reducing the total thickness of the anti-oxidation electrode 6c and the adhesive layer 6b.
[0030] It was also found that the area occupied by voids on the entire lower surface of the back electrode 6 can be reduced by setting the thickness of the back electrode 6 to 1650 μm or less (sample 1). Therefore, it is preferable that the thickness of the back electrode 6 is 1650 μm or less. It is more preferable that the thickness of the back electrode 6 is 1000 μm or less, and most preferable that the thickness is 100 μm or less. Furthermore, by reducing the height of the metal burrs 16, the thickness of the Ag bonding material 8 can be reduced, which can reduce the thermal resistance and cost.
[0031] The back electrode 6 may have a laminated structure of one ohmic electrode 6a and one anti-oxidation electrode 6c. Since there is no adhesive layer 6b such as Ti or Ni, the total thickness of the back electrode 6 can be reduced. For example, when the ohmic electrode 6a has a laminated structure of Al-Si and the anti-oxidation electrode 6c has a laminated structure of Au, the total thickness can be reduced to 100 μm or less.
[0032] The ohmic electrode 6a may be changed to a metal other than Al-Si that can make ohmic contact with Si / SiC. The anti-oxidation electrode 6c may be changed to a metal other than Au, such as Ag, that can provide measures against oxidation and sulfurization. The anti-oxidation electrode 6c in contact with the Ag bonding material 8 may be an Ag layer. This can improve the adhesion and conductivity between the back electrode 6 and the Ag bonding material 8. The ohmic electrode 6a may be an Ag alloy layer. This can ensure ohmic properties between the semiconductor chip 5 and the back electrode 6.
[0033] If the anti-oxidation electrode 6c on the outermost surface of the back electrode 6 is an Au layer, it is possible to prevent the back electrode 6 from being oxidized / sulfurized, and the electrical and mechanical bond between the back electrode 6 and the die pad 4 can be stably ensured.
[0034] The back electrode 6 may have a structure in which Ag alloy-Ag-Au is laminated from the semiconductor chip 5 side, or a structure in which Ag alloy-Au is laminated. This reduces the number of materials, improves manufacturability, and reduces costs. In addition, by reducing the thickness of the back electrode 6, the height of the metal burr 16 can be reduced, thereby reducing voids. In addition, since the Ag alloy can obtain ohmic contact with Si, the Al-Si, Ti, and Ni layers can be reduced.
[0035] Embodiment 2 7 is an enlarged cross-sectional view of the mounting portion of the semiconductor chip of the semiconductor device according to the second embodiment. The end of the back electrode 6 is disposed inside the end of the back surface of the semiconductor chip 5. Although the end of only two sides of the rectangular power chip is shown in the figure, the end of the back electrode 6 of the remaining two sides is also disposed inside the end of the back surface of the semiconductor chip 5. There is no metal burr 16 on the back electrode 6. The other configuration is the same as that of the first embodiment.
[0036] FIG. 8 is a cross-sectional view showing a manufacturing process of a semiconductor device according to the second embodiment. When forming the back electrode 6 on the semiconductor wafer 18, patterning is performed so that the back electrode 6 is not formed at a position that will later become the end of the semiconductor chip 5. When the semiconductor wafer 18 is diced to divide it into individual semiconductor chips 5, the back electrode 6 is not diced. Therefore, metal burrs 16 are not formed on the back electrode 6. Therefore, a path for discharging voids generated by the volatilization or shrinkage of the solvent when the Ag paste 19 is sintered can be secured. Therefore, the voids in the Ag bonding material 8 can be reduced. Therefore, the heat dissipation can be improved and the variation in the heat dissipation can be reduced. In addition, since the thickness of the Ag bonding material 8 can be reduced due to the absence of the metal burrs 16, the thermal resistance and the cost can be reduced.
[0037] The semiconductor chip 5 is not limited to those formed of silicon, but may be formed of a wide band gap semiconductor having a larger band gap than silicon. The wide band gap semiconductor is, for example, silicon carbide, gallium nitride-based material, or diamond. A semiconductor chip formed of such a wide band gap semiconductor has high voltage resistance and allowable current density, and can be miniaturized. By using this miniaturized semiconductor chip, a semiconductor device incorporating this semiconductor chip can also be miniaturized and highly integrated. In addition, since the heat resistance of the semiconductor chip is high, the heat dissipation fins of the heat sink can be miniaturized, and the water-cooled part can be air-cooled, so the semiconductor device can be further miniaturized. In addition, since the power loss of the semiconductor chip is low and highly efficient, the efficiency of the semiconductor device can be increased. [Explanation of symbols]
[0038] 1 sealing resin, 2 terminal, 4 die pad, 5 semiconductor chip, 6 back electrode, 6a ohmic electrode, 6c anti-oxidation electrode, 8 Ag bonding material, 16 metal burr, 19 Ag paste, 21 insulating material, 20 insulating substrate, 22 metal wiring, 23 bonding material
Claims
1. A conductive die pad; A semiconductor chip; a back surface electrode provided on a back surface of the semiconductor chip; an Ag bonding material that bonds the back electrode and the die pad and contains 50 to 85% Ag; A terminal connected to the semiconductor chip; an insulating sealing resin that covers the die pad, the semiconductor chip, the Ag bonding material, and a portion of the terminal; the terminals protrude from the sealing resin and have a substrate bonding surface at their tips, a metal burr protrudes from an outer periphery of a lower surface of the back electrode that is in contact with the Ag bonding material; A semiconductor device, characterized in that the thickness of the Ag bonding material is at least 2 μm greater than the vertical height of the metal burr.
2. 2. The semiconductor device according to claim 1, wherein the thickness of the Ag bonding material is at least 5 [mu]m greater than the vertical height of the metal burr.
3. 3. The semiconductor device according to claim 1, wherein the thickness of the back electrode excluding the metal burrs is 1650 [mu]m or less.
4. 4. The semiconductor device according to claim 1, wherein the back electrode has a laminated structure of an ohmic electrode ohmic-contacted to the semiconductor chip and an anti-oxidation electrode in contact with the Ag bonding material.
5. 5. The semiconductor device according to claim 4, wherein the back electrode comprises only one layer of the ohmic electrode and one layer of the anti-oxidation electrode.
6. 6. The semiconductor device according to claim 4, wherein the ohmic electrode is made of an Al--Si or Ag alloy.
7. 7. The semiconductor device according to claim 4, wherein the anti-oxidation electrode is made of Au.
8. 7. The semiconductor device according to claim 4, wherein the anti-oxidation electrode is made of Ag.
9. An insulating substrate having an insulating material and metal wiring provided on a surface of the insulating material, the substrate bonding surface of the terminal is bonded to the metal wiring by a conductive bonding material; 9. The semiconductor device according to claim 1, wherein the melting temperature of the bonding material is lower than the re-melting temperature of the Ag bonding material.
10. 10. The semiconductor device according to claim 1, wherein the semiconductor chip is made of a wide band gap semiconductor.
11. A method for manufacturing a semiconductor device according to any one of claims 1 to 8, comprising the steps of: applying Ag paste onto the die pad; placing the semiconductor chip on the Ag paste; a step of heating the Ag paste to sinter-bond the die pad and the back electrode of the semiconductor chip; The Ag paste after sintering is the Ag bonding material, A method for manufacturing a semiconductor device, characterized in that the thickness of the Ag paste applied onto the die pad is set so that the thickness of the Ag bonding material after sintering is at least 2 μm greater than the vertical height of the metal burr.
12. 12. The method for manufacturing a semiconductor device according to claim 11, wherein the Ag paste has a viscosity of 20 Pa.s or more before sintering.
13. A method for manufacturing a semiconductor device according to claim 9, comprising the steps of: a step of bonding the die pad and the back electrode with the Ag bonding material, and then bonding the substrate bonding surface of the terminal to the metal wiring with the bonding material; A method for manufacturing a semiconductor device, wherein a heating temperature when the terminal is joined to the metal wiring by reflow is lower than a remelting temperature of the Ag bonding material.
Citation Information
Patent Citations
JP1991045668U
Semiconductor device for electric power
JP2005150595A
Semiconductor device and manufacturing method thereof
JP2007305772A
Cutting method of multilayer substrate, manufacturing method of semiconductor device, semiconductor device, light-emitting device, and backlight device
JP2008288285A
Semiconductor device and method of manufacturing the same
JP2015216314A