Semiconductor package and manufacturing method thereof
A thermally conductive layer with varying hardness and adhesive strength addresses peeling and damage issues in semiconductor packages by ensuring conformability and reliability.
Patent Information
- Application Number
- JP2022565313
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-11-25
- Filing Date
- 2021-11-22
- Publication Date
- 2024-11-13
- Estimated Expiration
- 2041-11-22
AI Technical Summary
Existing semiconductor packages face issues with thermally conductive layers peeling off or damaging the semiconductor chip due to warpage, as conventional methods either lack sufficient adhesive strength or risk damaging the chip with high elastic modulus materials.
A thermally conductive layer with varying hardness and adhesive strength is used, where the central portion is softer and less adhesive than the peripheral portion, ensuring the layer can conform to the chip without causing damage during operation.
This design prevents peeling of the thermally conductive layer while protecting the semiconductor chip from damage, maintaining effective heat conduction.
Smart Images

Figure 0007582326000010 
Figure 0007582326000011 
Figure 0007582326000012
Abstract
Description
[Technical field]
[0001] The present invention relates to a semiconductor package and a method for manufacturing the same. [Background technology]
[0002] It is widely known that IC chips such as CPUs and GPUs generate heat during use and the associated performance degradation, and various heat dissipation technologies are used as a means to solve this problem. For example, it is known that a cooling component such as a heat sink is placed near the heat generating component, and the two are placed in close contact to promote efficient heat transfer to the cooling component, and then the cooling component is cooled, thereby efficiently dissipating heat from the heat generating component. In this case, if there is a gap between the heat generating component and the cooling component, the heat transfer becomes inefficient due to the presence of air with low thermal conductivity, and the temperature of the heat generating component does not decrease sufficiently.
[0003] To solve these problems, it is common to use a thermally conductive material that can fill the gap between the heat generating component and the cooling component. When a semiconductor chip (IC chip) is actually in operation, the semiconductor chip may "warp" and the thermally conductive layer may peel off from the cooling component or the heat generating element. When this phenomenon occurs, the thermal conduction between the cooling component and the heat generating element becomes insufficient. Various studies have been conducted to solve these problems.
[0004] In JP 2014-090135 A (Patent Document 1), the adhesive strength of the thermally conductive material is increased to prevent peeling. However, there is a concern that the high elastic modulus of the thermally conductive material may destroy the chip or damage the chip surface. In addition, in JP 4395753 A (Patent Document 2), a skin hardening layer is formed on the periphery, but the adhesive strength between the skin hardening layer and the chip is insufficient, and there is a concern that the thermally conductive material may peel off from the chip or cooling member, especially in large chips. All of these methods involve using one type of thermally conductive material by laying it between the heat generating part and the cooling member. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2014-090135 A [Patent Document 2] Patent No. 4395753 Summary of the Invention [Problem to be solved by the invention]
[0006] The present invention has been made in consideration of the above circumstances, and aims to provide a highly reliable semiconductor package that can accommodate the thermal conduction layer of a semiconductor chip without damaging the semiconductor chip when the element is in operation. [Means for solving the problem]
[0007] As a result of intensive research into achieving the above-mentioned object, the inventors discovered that the above-mentioned problem could be solved by using a specific thermally conductive layer in which two or more types of thermally conductive materials are laid on a semiconductor chip between the semiconductor chip and a cooling member, and thus arrived at the present invention.
[0008] Therefore, the present invention provides the following inventions. 1. A semiconductor package having a thermally conductive layer between a semiconductor chip and a cooling member, A semiconductor package comprising a thermally conductive layer having portions with different hardness and adhesive strength, the hardness and adhesive strength of a central portion of the thermally conductive layer being smaller than the hardness and adhesive strength of a peripheral portion of the thermally conductive layer. 2. A semiconductor package as described in 1, in which two or more types of thermally conductive materials are laid on a semiconductor chip from the center to the periphery, and the hardness and adhesive strength of the thermally conductive material constituting the center of the thermally conductive layer when hardened (hardness and adhesive strength of the center of the thermally conductive layer) are less than the hardness and adhesive strength of the thermally conductive material constituting the periphery of the thermally conductive layer when hardened (hardness and adhesive strength of the peripheral part of the thermally conductive layer). 3. A semiconductor package according to 1 or 2, wherein the minimum thickness of the center portion of the thermally conductive layer after compression is thinner than the minimum thickness of the peripheral portion of the thermally conductive layer after compression. 4. A semiconductor package according to claim 3, wherein the difference between the minimum thickness of the center of the thermally conductive layer after compression and the minimum thickness of the outermost periphery of the thermally conductive layer after compression is 10 μm or more. 5. A semiconductor package according to any one of 1 to 4, wherein the thermally conductive layer has a central portion with a hardness of 50 or less in terms of Asker C hardness. 6. A semiconductor package according to any one of 1 to 5, wherein the adhesive strength of the outermost periphery of the thermally conductive layer is 2.0 MPa or more. 7. A method for producing a semiconductor package described in any one of 1 to 6, comprising the steps of laying two or more types of thermally conductive materials on a semiconductor chip from the center to the periphery of the semiconductor chip, and overlaying a cooling member on the laid thermally conductive materials. Effect of the Invention
[0009] According to the present invention, it is possible to provide a highly reliable semiconductor package in which the thermally conductive layer of the semiconductor chip can follow the semiconductor chip without being damaged and with little peeling when the element is in operation. [Brief description of the drawings]
[0010] [Figure 1] FIG. 2 is a plan view showing the arrangement of a thermally conductive material according to the present invention. [Diagram 2] FIG. 2 is a plan view showing the arrangement of thermally conductive materials when only two types of thermally conductive materials are used according to an embodiment of the present invention. [Diagram 3] FIG. 2 is a plan view showing the arrangement of heat conductive materials when three types of heat conductive materials are used according to an embodiment of the present invention. [Figure 4] FIG. 2 is a plan view showing the arrangement of heat conductive materials when four types of heat conductive materials are used according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] The present invention will be described in detail below. The semiconductor package of the present invention is a semiconductor package having a thermally conductive layer, the thermally conductive layer having portions with different hardness and adhesive strength, the hardness and adhesive strength of the center of the thermally conductive layer being smaller than those of the peripheral portion of the thermally conductive layer. Specifically, the semiconductor package has a thermally conductive layer between a semiconductor chip and a cooling member, the thermally conductive layer is characterized in that two or more types of thermally conductive materials are laid on the semiconductor chip from the center to the peripheral portion, and the hardness and adhesive strength of the cured product of the thermally conductive material constituting the center of the thermally conductive layer are smaller than those of the cured product of the thermally conductive material constituting the peripheral portion of the thermally conductive layer.
[0012] [Semiconductor chips and cooling materials] The semiconductor package has a thermally conductive layer between a semiconductor chip and a cooling member. [Heat conductive layer] The thermal conductive layer is such that, when viewed from above the semiconductor chip, the hardness and adhesive strength of the center of the thermal conductive layer are smaller than those of the peripheral part of the thermal conductive layer, and two or more types of thermal conductive materials are laid on the semiconductor chip from the center to the peripheral part, and the hardness and adhesive strength of the thermal conductive material constituting the center of the thermal conductive layer when hardened are smaller than those of the thermal conductive material constituting the peripheral part of the thermal conductive layer when hardened. The thermal conductive material is not particularly limited and a known material can be used, but a liquid material may be applied, or the liquid material may be hardened by heating, moisture, UV, or the like, or a molded product such as a thermal conductive pad sheet, phase change material, or thermal conductive adhesive tape may be laid, or a liquid material and a molded product may be used in combination, or a molded product may be laid after hardening a liquid material, or a hardened product obtained by hardening a liquid material after placing a molded product, but is not limited thereto.
[0013] In addition, examples of thermally conductive materials include, but are not limited to, silicone resin, acrylic resin, epoxy resin, urethane resin, etc., mixed with a thermally conductive filler. Examples of thermally conductive fillers include, but are not limited to, aluminum powder, copper powder, silver powder, iron powder, nickel powder, gold powder, tin powder, metal silicon powder, aluminum nitride powder, boron nitride powder, aluminum oxide (alumina) powder, titanium oxide powder, magnesium oxide powder, diamond powder, carbon powder, indium powder, gallium powder, zinc oxide powder, etc.
[0014] Examples of the thermally conductive material constituting the thermally conductive layer of the present invention include: (A) an alkenyl group-containing organopolysiloxane, (B) Thermally conductive filler (C) organohydrogenpolysiloxane, and (D) Platinum catalyst Examples include those containing:
[0015] [Component (A)] The organopolysiloxane of component (A) of the present invention has at least two alkenyl groups directly bonded to silicon atoms in each molecule, and is represented by the following average composition formula (1): R 1 a SiO (4-a) / 2 (1) (In the formula, R 1 are the same or different, unsubstituted or substituted monovalent hydrocarbon groups having 1 to 10 carbon atoms, preferably 1 to 8 carbon atoms, and a is a positive number of 1.5 to 2.8, preferably 1.8 to 2.5, and more preferably 1.95 to 2.05. can be used.
[0016] Here, the above R 1Examples of the unsubstituted or substituted monovalent hydrocarbon group bonded to a silicon atom represented by the formula (I) include alkyl groups such as methyl, ethyl, propyl, isopropyl, butyl, isobutyl, tert-butyl, pentyl, neopentyl, hexyl, cyclohexyl, octyl, nonyl, and decyl; aryl groups such as phenyl, tolyl, xylyl, and naphthyl; aralkyl groups such as benzyl, phenylethyl, and phenylpropyl; alkenyl groups such as vinyl, allyl, propenyl, isopropenyl, butenyl, hexenyl, cyclohexenyl, and octenyl; and groups in which some or all of the hydrogen atoms of these groups have been substituted with halogen atoms such as fluorine, bromine, and chlorine, or with cyano groups, for example, chloromethyl, chloropropyl, bromoethyl, trifluoropropyl, and cyanoethyl. 1 It is preferable that 90 mol % or more of the groups are methyl groups.
[0017] Also, all R 1 At least two of the groups must be alkenyl groups (preferably having 2 to 8 carbon atoms, more preferably having 2 to 6 carbon atoms, and even more preferably being vinyl groups). The content of alkenyl groups in the organopolysiloxane is 2.0×10 -5 ~1.0×10 -2 It is preferable that the alkenyl group is bonded to a silicon atom at the molecular chain terminal, a silicon atom in the middle of the molecular chain, or both. The structure of this organopolysiloxane is usually a straight-chain structure in which the main chain is basically composed of a repetition of diorganosiloxane units and both molecular chain terminals are blocked with triorganosiloxy groups, but it may also be a partially branched structure, cyclic structure, etc.
[0018] The kinetic viscosity of component (A) at 25°C is 100 to 100,000 mm 2 / s is preferable, and 200 to 100,000 mm 2 / s is more preferable, and 200 to 10,000 mm 2 / s is more preferred.
[0019] Examples of the component (A) include dimethylpolysiloxanes blocked at both ends with dimethylvinylsilyl groups, and these can be used alone or in combination of two or more.
[0020] [(B) Component] As for the thermally conductive filler having the thermal conductivity of the component (B), if the thermal conductivity of the filler is less than 10 W / m·°C, the thermal conductivity of the silicone grease composition itself will be small, so the thermal conductivity of the filler is preferably 10 W / m·°C or more, and more preferably 10 to 5,000 W / m·°C. As such a thermally conductive filler, an inorganic compound powder can be used. As the inorganic compound powder used in the component (B), one or more selected from aluminum powder, zinc oxide powder, titanium oxide powder, magnesium oxide powder, alumina powder, aluminum hydroxide powder, boron nitride powder, aluminum nitride powder, diamond powder, gold powder, silver powder, copper powder, carbon powder, nickel powder, indium powder, gallium powder, metal silicon powder, and silicon dioxide powder can be used. In the present invention, the thermal conductivity is a value measured by a thermal conductivity measuring device, for example, QTM-500 manufactured by Kyoto Electronics Manufacturing Co., Ltd.
[0021] The inorganic compound powder used in component (B) has an average particle size in the range of 0.5 to 200 μm, preferably 1 to 150 μm. In the present invention, the average particle size is a volume-based average diameter [MV] that can be measured by a laser diffraction / scattering method, for example, Microtrack MT330OEX manufactured by Nikkoki Co., Ltd. In addition, the inorganic compound powder used in the present invention may be subjected to a hydrophobic treatment with organosilane, organosilazane, organopolysiloxane, organic fluorine compound, etc., if necessary. The hydrophobic treatment method may be a generally known method, for example, a method of mixing the inorganic compound powder with organosilane or a partial hydrolyzate thereof in a mixer such as Trimix, Twinmix, Planetary Mixer (all registered trademarks of mixers manufactured by Inoue Seisakusho Co., Ltd.), Ultra Mixer (registered trademark of mixers manufactured by Mizuho Kogyo Co., Ltd.), or Hivis Dispermix (registered trademark of mixers manufactured by Tokushu Kika Kogyo Co., Ltd.). If necessary, it may be heated to 50 to 100° C. For mixing, a solvent such as toluene, xylene, petroleum ether, mineral spirits, isoparaffin, isopropyl alcohol, or ethanol may be used, and in this case, it is preferable to remove the solvent after mixing using a vacuum device or the like. It is also possible to use the organopolysiloxane of component (A), which is the liquid component of the present invention, as a dilution solvent. Compositions produced by this method are also within the scope of the present invention.
[0022] The blending amount of the (B) thermally conductive filler (inorganic compound powder) is preferably 500 to 4,000 parts by mass, and more preferably 1,000 to 4,000 parts by mass, per 100 parts by mass of the (A) component.
[0023] [(C) component] The organohydrogenpolysiloxane of the component (C) is, for example, a compound represented by the following average composition formula (3): R 3 c H d SiO (4-c-d) / 2 (3) (In the formula, R 3is an unsubstituted or substituted monovalent hydrocarbon group having 1 to 12 carbon atoms, preferably 1 to 10 carbon atoms. In addition, c is 0.7 to 2.1, preferably 0.8 to 2.05, d is 0.001 to 1.0, preferably 0.005 to 1.0, and c+d is a positive number that satisfies the range of 0.8 to 3.0, preferably 1.0 to 2.5. can be used.
[0024] Residual organic group R bonded to silicon atom 3 Examples of the alkyl group include alkyl groups such as methyl, ethyl, propyl, butyl, hexyl, and dodecyl, aryl groups such as phenyl, aralkyl groups such as 2-phenylethyl and 2-phenylpropyl, halogen-substituted hydrocarbon groups such as chloromethyl and 3,3,3-trifluoropropyl, and epoxy ring-containing organic groups (glycidyl or glycidyloxy-substituted alkyl groups) such as 2-glycidoxyethyl, 3-glycidoxypropyl, and 4-glycidoxybutyl. Such organohydrogenpolysiloxanes having Si-H groups may be linear, branched, or cyclic, or may be a mixture of these.
[0025] The amount of component (C) blended is preferably an amount such that there are 0.3 to 2.5 silicon-bonded hydrogen atoms (Si-H / Si-alkenyl groups) in component (C) per silicon-bonded alkenyl group in component (A), and more preferably an amount such that there are 0.5 to 2.0 silicon-bonded hydrogen atoms per silicon-bonded alkenyl group in component (A).
[0026] [(D) component] The catalyst selected from platinum and platinum compounds of component (D) is a component that promotes the addition reaction between the alkenyl group of component (A) and the Si-H group of component (C). Examples of component (D) include platinum alone, chloroplatinic acid, platinum-olefin complex, platinum-alcohol complex, platinum coordination compound, etc. The amount of component (F) to be blended is in the range of 0.1 to 5,000 ppm, since there is no catalytic effect if the platinum atom amount is less than 0.1 ppm relative to the mass of component (A), and there is no increase in the effect if the amount exceeds 5,000 ppm, which is uneconomical.
[0027] [Other ingredients] In addition to the above-mentioned components (A) to (D), the present invention may also use a reaction inhibitor (E) if necessary. The reaction inhibitor may be a conventional reaction inhibitor used in addition curing silicone compositions. Examples of the reaction inhibitor include acetylene compounds such as acetylene alcohols (e.g., 1-ethynyl-1-cyclohexanol, 3,5-dimethyl-1-hexyn-3-ol), various nitrogen compounds such as tributylamine, tetramethylethylenediamine, and benzotriazole, organic phosphorus compounds such as triphenylphosphine, oxime compounds, and organic chloro compounds. In addition, an adhesion promoter, an antioxidant, and the like may also be added.
[0028] [Manufacturing method] To produce the thermally conductive composition of the present invention, the components (A) to (D) and, if necessary, other components can be mixed using a mixer such as Trimix, Twinmix, or Planetary Mixer (all of which are registered trademarks of mixers manufactured by Inoue Seisakusho Co., Ltd.), Ultra Mixer (registered trademark of mixers manufactured by Mizuho Kogyo Co., Ltd.), or Hivis Dispermix (registered trademark of mixers manufactured by Tokushu Kika Kogyo Co., Ltd.).
[0029] The thermal conductivity of the thermally conductive layer (as a whole) is not particularly limited, but in order to sufficiently dissipate heat from the semiconductor chip, it is preferably 1.5 (W / m·°C) or more, more preferably 1.8 (W / m·°C) or more, and even more preferably 1.8 to 500 (W / m·°C). The thermal conductivity of the thermally conductive layer is measured by a method conforming to ISO22007-2.
[0030] The two or more different types of thermally conductive materials may be three or more, four or more, or more types of materials may be used. The most central part made of one type of thermally conductive material is defined as the central part, and the rest are defined as the peripheral part. When three or more types of thermally conductive materials are used, the outermost peripheral part is defined as the outermost peripheral part. When only one type of material is used, if a soft material is used to avoid damaging the central part of the semiconductor chip, peeling will occur at the peripheral part of the semiconductor chip due to insufficient adhesive strength. On the other hand, if a material with high adhesive strength is used to prevent peeling, the material will become hard, and there is a risk of damaging the surface of the chip at the central part.
[0031] In the present invention, the thermally conductive layer has portions with different hardness and adhesive strength, and the hardness and adhesive strength of the central part of the thermally conductive layer are smaller than those of the peripheral part of the thermally conductive layer. For example, when two or more types of thermally conductive materials are laid from the central part to the peripheral part of the semiconductor chip when viewed from above, and are cured, they become a cured product. At this time, they are laid in order from the central part so that the hardness and adhesive strength of the cured product of the thermally conductive material constituting the central part of the thermally conductive layer (hardness and adhesive strength of the central part of the thermally conductive layer) are smaller than the hardness and adhesive strength of the cured product of the thermally conductive material constituting the peripheral part of the thermally conductive layer (hardness and adhesive strength of the peripheral part of the thermally conductive layer). When three or more types are used, it is sufficient that the most central layer and the most peripheral layer satisfy the above, and in the case of four layers, it is preferable that they satisfy the above in order.
[0032] Using a soft material in the center and a hard material in the periphery can prevent the semiconductor chip from being scratched or peeled off. Using a hard material in the center and a soft material in the periphery can cause the semiconductor chip to be scratched in the center and peeled off in the periphery. Using a material with low adhesive strength in the center and high adhesive strength in the periphery can prevent peeling off of the thermally conductive layer. Hereinafter, the hardness, adhesive strength, thermal conductivity, and minimum thickness after compression of the thermally conductive layer in the center, periphery, etc., are measured by the methods described below and in detail in the Examples.
[0033] The hardness of the center portion is preferably 50 or less, more preferably 40 or less in Asker C hardness so as not to damage the semiconductor chip even if the semiconductor chip is warped during operation of the element. The lower limit is not particularly limited, but can be selected from 1 or more. The hardness of the outermost periphery portion is preferably 40 or more, more preferably 40 to 90 in Shore A hardness. The adhesive strength at the center is preferably 0.01 MPa or more, more preferably 0.01 MPa or more and less than 2.0 MPa.The adhesive strength at the outermost periphery is preferably 2.0 MPa or more, more preferably 2.5 MPa or more, and even more preferably 2.5 to 20 MPa.
[0034] The hardness of the thermally conductive layer, such as the center and periphery, is measured by preparing a test piece for hardness measurement by curing the prepared thermally conductive material at 150℃ for 90 minutes. Note that the hardness according to Asker C and Shore A is measured based on JIS K6249 and 6253. Note that when Shore A is 20 or less, it is measured by Asker C.
[0035] The adhesive strength is measured by sandwiching a thermally conductive material between a semiconductor chip (Si wafer) and a cooling member (Ni-plated copper plate) and curing the test piece at 150°C for 90 minutes, then measuring the vertical tensile strength.
[0036] The hardness can be adjusted by the type and amount of dimethylpolysiloxane and organohydrogenpolysiloxane used in preparing the thermally conductive layer. The adhesive strength can be adjusted by the type and amount of dimethylpolysiloxane and organohydrogenpolysiloxane used in preparing the thermally conductive layer.
[0037] The semiconductor chip has a structure in which the center is convex upward in a process before laying the thermally conductive material, so that the distance between the chip and the cooling member is thin in the center and thick in the peripheral part. Therefore, it is preferable that the thickness of the thermally conductive layer is thin in the center and thick in the peripheral part. Specifically, in order to fully absorb the thickness difference caused by the warping of the package, the difference between the minimum thickness after compression of the center of the thermally conductive layer and the minimum thickness after compression of the outermost peripheral part of the thermally conductive layer is preferably 10 μm or more, more preferably 20 μm or more, and even more preferably 20 to 100 μm. The minimum thickness after compression of the center of the thermally conductive layer, the outermost peripheral part of the thermally conductive layer, etc. is measured by sandwiching the thermally conductive material between the semiconductor chip and the cooling member, and heating and curing it at 150° C. for 90 minutes at a pressure of 0.2 (MPa). The size of the semiconductor chip is not particularly limited, and the major axis (X1) of the center (first portion) of the thermal conductive layer is preferably 20 to 80% of the major axis (Z) of the semiconductor chip, and more preferably 30 to 80%.
[0038] [Cooling material] The cooling member is appropriately selected depending on the semiconductor package, but examples include Ni-plated copper plate, aluminum die-cast, thermally conductive epoxy resin, and resin substrate.
[0039] [Manufacturing method] The method for manufacturing the semiconductor package of the present invention is not particularly limited, but may include, for example, a method including a step of laying two or more types of thermally conductive materials on a semiconductor chip from the center to the periphery of the semiconductor chip, and a step of placing a cooling member on the laid thermally conductive materials. In the case of hardening, a method including a further step of hardening the laid thermally conductive materials may be included. Specifically, the method may include a method including the following steps. (I) fixing a semiconductor chip onto a substrate; (II) laying two or more types of thermally conductive materials on the semiconductor chip from the center to the periphery of the semiconductor chip; (III) a step of overlaying a cooling member on the thermally conductive material and fixing the substrate and the cooling member; (IV) curing the thermally conductive material after fixing. In the above (IV), the curing conditions are not particularly limited as long as they are conditions under which the thermally conductive material can be cured. In the case of thermal curing, heating at 80 to 200° C. for 30 minutes to 1 hour is sufficient. EXAMPLES
[0040] The present invention will be specifically described below with reference to examples and comparative examples, but the present invention is not limited to the following examples.
[0041] [Examples and Comparative Examples] [Preparation of thermally conductive materials] The following components for forming the composition of the present invention were prepared. [Component (A)] A-1: Both ends are blocked with dimethylvinylsilyl groups, and the kinetic viscosity at 25°C is 600mm 2 / s dimethylpolysiloxane (vinyl value 0.015mol / 100g) A-2: Both ends are blocked with dimethylvinylsilyl groups, and the kinetic viscosity at 25°C is 400mm 2 / s dimethylpolysiloxane (vinyl value 0.0185mol / 100g)
[0042] [(B) Component] The aluminum powder and zinc oxide powder shown below were mixed at room temperature for 15 minutes in the mixing ratios shown in Table 1 below using a 5-liter planetary mixer (manufactured by Inoue Seisakusho Co., Ltd.) to obtain B-1 to B-5. Aluminum powder with an average particle size of 2.0 μm (thermal conductivity: 237 W / m°C) Aluminum powder with an average particle size of 10.0 μm (thermal conductivity: 237 W / m°C) Aluminum powder with an average particle size of 15.0 μm (thermal conductivity: 237 W / m°C) Aluminum powder with an average particle size of 25.0 μm (thermal conductivity: 237 W / m°C) Zinc oxide powder with an average particle size of 1.0 μm (thermal conductivity: 25 W / m°C)
[0043] [Table 1]
[0044] [(C) component] Organohydrogenpolysiloxane represented by the following formula (the bonding order of each siloxane unit is not limited to the order shown below): C-1: [ka] C-2: [ka] C-3: [ka] [(D) component] D-1: A-1 solution of platinum-divinyltetramethyldisiloxane complex, containing 1% by mass of platinum atoms
[0045] [(E) component] E-1: 1-ethynyl-1-cyclohexanol
[0046] [Component (F)] F-1: [ka]
[0047] Thermally conductive materials were prepared in the amounts (parts by mass) shown in the table below. The Si-H / Si-Vi value represents the number of silicon-bonded hydrogen atoms in component (C) per silicon-bonded vinyl group in component (A).
[0048] [Table 2]
[0049] [Table 3]
[0050] The thermally conductive materials thus obtained were subjected to the following evaluations, and the results are shown in Tables 2 and 3. [Hardness measurement method] The thermally conductive material was heat cured at 150°C for 90 minutes, and the Asker C hardness of the test pieces for hardness measurement was measured. The Shore A hardness of some of the test pieces was also measured (hardness measurement was performed in accordance with JIS K6249 and 6253).
[0051] [Method of measuring adhesive strength] 0.1 g of the thermally conductive material was sandwiched between a 10 mm x 10 mm Si wafer and a 20 mm x 20 mm Ni-plated copper plate as a cooling member, and the test piece was heated and cured at 150°C for 90 minutes. The tensile strength in the vertical direction was measured and the adhesive strength was calculated.
[0052] [Method of measuring thermal conductivity] The test pieces for hardness measurement were measured using a method conforming to ISO22007-2.
[0053] [Minimum thickness after compression] The minimum thickness after compression was measured for a test piece in which 0.1 g of thermal conductive material was sandwiched between a 10 mm x 10 mm Si wafer and a 10 mm x 10 mm Ni-plated copper plate, and then heated and cured at 150°C for 90 minutes under a pressure of 0.2 (MPa).
[0054] [Method of manufacturing semiconductor packages] Using the above thermally conductive material, a semiconductor package test piece having a thermally conductive layer was produced by the following method. A 20mm x 20mm Si wafer (semiconductor chip) was fixed on an organic resin substrate with adhesive. A thermally conductive material was laid on top of it so that the first, second, third, and fourth parts had a predetermined area. The application area and shape of each thermally conductive material were specified as shown in Figure 1. Then, adhesive was applied on the resin substrate so as to surround the Si wafer. A Ni-plated copper plate was placed on top and then heated to fix it to the resin substrate. Furthermore, the thermally conductive material was heated at 150°C for 90 minutes to harden it and form a thermally conductive layer. In the examples and comparative examples, the thermally conductive material of the first part was T1, the thermally conductive material of the second part was T2, the thermally conductive material of the third part was T3, and the thermally conductive material of the fourth part was T4. In addition, when only two types of thermally conductive materials were used, the characteristics of each thermally conductive material were described in T1 and T4, and none was described in T2 and T3. When three types of thermally conductive materials were used, the characteristics of each thermally conductive material were described in T1, T2, and T4 using the following method, and none was described in T3. When four types of thermal conductive materials are used, the characteristics of each thermal conductive material obtained in the above measurement are recorded in T1, T2, T3, and T4. The obtained semiconductor package test pieces were evaluated for "peeling of the thermal conductive layer" and "scratches in the center of the semiconductor chip" using the methods below. Figure 1 shows the arrangement of thermal conductive materials as viewed from above. Figure 2 shows the case where only two types of thermal conductive materials are used, Figure 3 shows the case where three types of thermal conductive materials are used, and Figure 4 shows the case where four types of thermal conductive materials are used.
[0055] [Peeling of the thermal conductive layer, damage to the center of the semiconductor chip] The semiconductor package test piece prepared above was placed in a heat cycle tester at -55℃⇔150℃ and a 1,000 cycle test was performed. After the heat cycle test, the adhesive between the resin substrate and the Ni-plated copper plate was removed, and the test piece was immersed in red ink and then the Ni-plated copper plate was peeled off to check for peeling of the thermal conductive layer from the semiconductor chip. If the red ink had penetrated to the inside, it was determined that peeling had occurred. The results were shown as (peeling) yes or (peeling) no. After that, the thermal conductive layer was peeled off and the surface of the center of the semiconductor chip was checked under a microscope for scratches. The results were shown as (scratches) present or (scratches) absent.
[0056]
Table 4
[0057]
Table 5
Claims
1. A semiconductor package having a thermally conductive layer between a semiconductor chip and a cooling member, the thermally conductive layer has portions having different hardness and adhesive strength, the hardness and adhesive strength of the central portion of the thermally conductive layer being smaller than the hardness and adhesive strength of the peripheral portion of the thermally conductive layer; The hardness of the center portion of the thermal conductive layer is 50 or less in Asker C hardness, The adhesive strength of the outermost peripheral portion of the thermal conductive layer is 2.0 MPa or more; The thermally conductive layer is a cured product obtained by laying two or more types of liquid thermally conductive materials containing a thermally conductive filler on a semiconductor chip and curing the liquid thermally conductive materials. Semiconductor package.
2. 2. The semiconductor package of claim 1, wherein two or more types of thermally conductive materials are laid on a semiconductor chip from the center to the periphery of the semiconductor chip, and the hardness and adhesive strength of the thermally conductive material constituting the center of the thermally conductive layer when hardened (the hardness and adhesive strength of the center of the thermally conductive layer) are smaller than the hardness and adhesive strength of the thermally conductive material constituting the peripheral portion of the thermally conductive layer when hardened (the hardness and adhesive strength of the peripheral portion of the thermally conductive layer).
3. 3. The semiconductor package according to claim 1, wherein the minimum thickness of the central portion of the thermally conductive layer after compression is smaller than the minimum thickness of the peripheral portion of the thermally conductive layer after compression.
4. 4. The semiconductor package according to claim 3, wherein the difference between the minimum thickness of the central portion of the thermally conductive layer after compression and the minimum thickness of the outermost peripheral portion of the thermally conductive layer after compression is 10 [mu]m or more.
5. A liquid thermally conductive material, (A) an alkenyl group-containing organopolysiloxane, (B) Thermally conductive filler (C) organohydrogenpolysiloxane, and (D) Platinum catalyst The semiconductor package according to any one of claims 1 to 4, which is a curable composition comprising:
6. A method for producing a semiconductor package according to any one of claims 1 to 5, comprising the steps of laying two or more types of thermally conductive material on a semiconductor chip from the center to the periphery of the semiconductor chip, overlaying a cooling member on the laid thermally conductive material, and hardening the thermally conductive material.
Citation Information
Patent Citations
Multi-chip semiconductor device
JP1999111897A
Semiconductor device
JP2008244238A
Package structure, printed circuit board mounted with the same, and electronic apparatus including the printed circuit board
JP2009218603A
Bonding structure of substrate
JP2011035320A
Semiconductor device
JP2014090135A