elongated SiC fuel element

The elongated SiC cladding design addresses hermeticity and mechanical interaction issues by accommodating fuel swelling with minimal distortion and improved thermal conductivity, enabling safer and more efficient use of UO2, U3Si2, UN, and uranium alloys in nuclear reactors.

JP7583015B2Active Publication Date: 2024-11-13WESTINGHOUSE ELECTRIC CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2022500142
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-07-02
Filing Date
2020-07-02
Publication Date
2024-11-13
Estimated Expiration
2040-07-02

AI Technical Summary

Technical Problem

SiC cladding in nuclear fuel rods faces challenges with hermeticity and mechanical interaction issues, leading to potential cladding failure due to fuel swelling and low thermal conductivity, which limits its use in conventional cylindrical geometries.

Method used

An elongated SiC cladding design with specific gap dimensions and shapes to accommodate fuel swelling, allowing for minimal distortion and improved thermal conductivity, using UO2, U3Si2, UN, and uranium alloys as fuels.

Benefits of technology

The elongated SiC cladding design minimizes cladding distortion, reduces fuel temperatures, and enhances thermal conductivity, enabling higher fuel loading and safer operation in light water reactors.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007583015000001
    Figure 0007583015000001
  • Figure 0007583015000002
    Figure 0007583015000002
  • Figure 0007583015000003
    Figure 0007583015000003
Patent Text Reader

Abstract

An elongated fuel element is described having a silicon carbide cladding that encapsulates a fuel such as UO2, where the fuel is dimensioned relative to the cladding to define a gap at each lateral end of the enclosure large enough that the fuel does not increase cladding distortion outside of cladding distortion tolerances when swelling with use. The lateral gaps at the ends of the fuel allow for lateral expansion during swelling, thereby reducing cladding distortion.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] (CROSS REFERENCE TO RELATED APPLICATIONS) This application claims the benefit of 16 / 459,764, entitled “Elongate SIC Fuel Elements,” filed July 2, 2019, the contents of which are incorporated herein by reference.

[0002] (Government Rights Statement) This invention was made with Government support under Contract No. DE-NE0008824 awarded by the Department of Energy. The United States Government has certain rights in this invention.

[0003] The present invention relates to fuel elements for nuclear power plants, and more particularly to elongated fuel segments housed within elongated SiC cladding. [Background technology]

[0004] Silicon carbide (SiC) has been shown to be a very promising accident tolerant fuel (ATF) cladding, but one of the major challenges of SiC is that the fuel pellets contained within the SiC cladding tube cannot have strong contact with the cladding without risking losing the hermeticity in the SiC cladding.

[0005] UO2 fuel has a long and successful history of use in the nuclear industry. UO2 has low reactivity with light water coolant, moderate swelling, and a stable structure in radiation, but suffers from low thermal conductivity, which limits its use to small diameter fuel rods. In use, fission products cause UO2 to swell, and unless there is a large enough initial gap between the fuel pellets and a non-ductile cladding such as SiC, the inevitable swelling leads to cladding failure due to strong pellet-cladding mechanical interaction (PCMI). Increasing the initial pellet-cladding gap to solve the PCMI problem would result in even higher fuel centerline temperatures due to the low thermal conductivity of the helium gas in the gap and reduced uranium loading. This drawback becomes apparent when UO2 is used in fuel rods containing highly accident-resistant cladding such as SiC, which requires minimal fuel-cladding mechanical interaction to avoid cracking and loss of hermeticity. Thus, the use of UO2 in SiC cladding is not possible for cylindrical fuel rod geometries without severe economic penalties.

[0006] On the other hand, fuels such as U3Si2, UN, and uranium alloys can mitigate the PCMI problem due to their high fuel thermal conductivity and lower fuel centerline temperatures by leaving a larger pellet-cladding gap, but at the expense of reduced uranium loading. Furthermore, these fuels have poor water corrosion resistance, which compromises the accident resistance of the fuel and thus has adverse effects during a leaking fuel event in light water reactors.

[0007] For metallic cladding such as Zr, which has a strain capability of 2 to 4%, the gap only needs to be large enough to load the fuel pellets, which is not a PCMI issue. However, if a leak occurs, for example, U3Si2 will oxidize and increase the internal volume within the Zr cladding. The increased volume will cause the cladding to bulge, resulting in blockage of the coolant paths.

[0008] SiC cladding has improved high temperature capability during accident conditions compared to conventional Zr-based materials. However, rod-shaped fuel designs have limited the potential of SiC materials because SiC has limited strain capability (~0.04 to 0.1%) to mitigate local stress buildup and minimize mechanical interaction between the fuel and cladding. Efforts to solve this problem have been to leave large fuel-cladding gaps. However, large gaps significantly increase fuel centerline temperatures, resulting in large amounts of fission gas release and / or swelling, especially for low thermal conductivity materials such as UO2, and also reduce uranium loading, resulting in severe economic penalties.

[0009] Initially developed in the 1960s and 1970s, plate-shaped fuel such as those disclosed in U.S. Patents Nos. 3,173,843, 3,297,543, 3,586,745, 3,855,061, 4,038,135, and 4,224,106 used metal cladding (e.g., aluminum or zirconium alloys) and metallic fuel or fuel dispersed in a metal matrix (e.g., UZr or UMo). Such plate-shaped fuel was found to be unsuitable for practical reactors and was abandoned, but is currently being used in test reactors and evaluated for use in small modular reactors. See Mark D. DeHart, "Fuel Element Design and Analysis for Potential LEU Conversion of the Advanced Test Reactor," INL / JOU-17-41538 Revision 0, April 2018; Samuel J. Miller et al., "Evaluation of U10Mo Fuel Plate Irradiation Behavior Via Numerical and Experimental Benchmarking," INL / CON-12-25074, November 2012; and Min-Gil Kim et al., "Comparison of Thermal Hydraulic Performances of Rod Type Fuel to Plate-Type Fuel for Small Modular Reactor Application," Proceedings of ICAPP, April 2014. Summary of the Invention [Problem to be solved by the invention]

[0010] The following summary is provided to facilitate an understanding of some of the innovative features unique to the disclosed embodiments and is not intended to be a complete description, A full appreciation of the various aspects of the embodiments may be gained by taking the entire specification, claims, and abstract together.

[0011] To address issues arising from pellet cladding mechanical interactions between the SiC cladding and the nuclear fuel while providing larger uranium loadings and better safety margins, particularly in light water reactors, a novel fuel element is described herein consisting of an elongated shaped fuel with an elongated shaped SiC cladding. [Means for solving the problem]

[0012] In various aspects, a fuel element for use in a nuclear reactor includes a silicon carbide cladding and a nuclear fuel contained within the cladding. The cladding has two opposing elongated walls and two opposing end walls shorter than the elongated walls. The elongated walls and the end walls together define an enclosure. The enclosure has an end-wall-to-end-wall length and an elongated-wall-to-wall width, and the cladding has a longitudinal axis and a transverse axis orthogonal to the longitudinal axis. The nuclear fuel has two elongated surfaces and two end faces shorter than the elongated surfaces. Each of the two elongated surfaces is minimally spaced a first distance (e.g., between about 0.05 and 2.0 mm) in opposed relationship from a different one of the elongated walls of the cladding prior to swelling in use, and each of the end faces is spaced a second distance in opposed relationship from a different one of the end walls of the cladding, the second distance being greater than the first distance. The first and second distances are dimensioned such that, when the fuel swells in use, the swelling fuel swells beyond the first distance to no more than the second distance to deform the elongated walls of the cladding without deforming the end walls of the cladding and without distorting the cladding by more than 0.1%.

[0013] Cladding distortion due to fuel swelling is, in various embodiments, 0.05% or less.

[0014] The second distance defines a gap between the fuel end face and the cladding end wall, the gap being dimensioned to allow maximum swelling of the selected fuel in addition to space for fission gases generated during use. One skilled in the art can determine the second distance by calculating by known means or determining by historical use the maximum amount of swelling the selected fuel will experience during use and the amount of fission gases that will be generated during use. The first distance defines a gap between each of the elongated walls of the cladding and the opposing elongated surface of the fuel. The gap of the first distance is sufficient to allow the fuel to be inserted into the cladding prior to use, typically about 0.07 mm.

[0015] In some aspects, the fuel may be configured in cross section with an oval shape defining an apex at each of the shorter end faces, with the two elongated surfaces being convexly curved. The oval shape has a major axis extending from apex to apex and a minor axis perpendicular to the major axis. Each of the convexly curved surfaces has a co-vertex on the minor axis, curving from the co-vertex to each apex and intersecting with each apex. The first distance in this embodiment is a minimum between the co-vertex and the elongated wall of the cladding.

[0016] In some embodiments of the fuel element, the elongated walls of the cladding may be curved inwardly toward the fuel. The elongated walls of the cladding may be concavely curved inwardly toward the fuel prior to deformation in use and may be deformed outwardly during use. End walls of the cladding in various embodiments may be flat prior to use and remain flat during use.

[0017] The elongated surfaces of the fuel may be concavely curved inwardly towards one another prior to swelling in use and swell outwardly in use to form convexly curved elongated surfaces, the convexly curved elongated surfaces extending beyond a first distance to deform the elongated walls of the cladding. Each concavely curved elongated surface defines a minor apex on the minor axis and curves from the minor apex to meet each end face. The end faces of the fuel may be flat prior to swelling in use and swell outwardly in use to form the convexly curved end faces. Alternatively, the end faces of the fuel may be flat prior to swelling in use and remain flat in use.

[0018] In various aspects, the fuel, prior to swelling in use, may be configured in a rectilinear shape in cross section defining a first end face and a flat elongated surface. The rectilinear shape defines a major axis extending from end face to end face and a minor axis perpendicular to the major axis. The fuel expands outwardly along both the major and minor axes in use to form an oval structure in cross section. The cladding, prior to swelling in use, may be configured in a rectilinear shape in cross section defining flat end walls and flat elongated walls that deform outwardly as the fuel swells in use.

[0019] In various aspects, the end walls of the cladding are thicker in cross section than the elongated walls of the cladding.

[0020] The fuel may be a fissile material selected from the group consisting of UO2, U3Si2, UN, and uranium alloys.

[0021] The elongated fuel with elongated SiC cladding allows for the utilization of the proven benefits of fuels such as UO2 in addition to the accident resistance characteristics of the SiC cladding material without compromising fuel performance both during normal operation and under transient conditions. The proposed elongated SiC cladding with elongated fuel and end gaps that allow fuel expansion provides benefits such as improved heat transfer due to small gaps or direct contact between the fuel and the cladding. The elongated SiC cladding with elongated fuel also results in lower fuel temperatures over the life of the fuel due to minimal gaps, resulting in less fission gas release and swelling, less deformation of the cladding during transient events due to lower temperature rise, and reduced tensile stresses during hard contact between the fuel and the cladding due to the increased span of cladding bulge allowed. The elongated cladding surface can optionally be pre-curved to further reduce local stress buildup. The SiC clad elongated fuel described herein allows for the use of UO2 fuel without compromising the economics of UO2 or the accident tolerance characteristics of SiC.

[0022] The features and advantages of the present disclosure may be better understood with reference to the accompanying drawings. [Brief description of the drawings]

[0023] [Figure 1] FIG. 2 is a schematic diagram of a top plan sectional view of one embodiment of an elongated fuel element in its initial configuration.

[0024] [Diagram 2] FIG. 1 is a schematic diagram of a top plan cross-sectional view of an alternative embodiment of an elongated fuel element showing convex shaped fuel segments and elongated cladding in an initial configuration (solid lines) compared to a configuration of swollen fuel segments (dashed lines) and deformed cladding (dashed lines) during use.

[0025] [Diagram 3]FIG. 1 is a schematic diagram of a top plan cross-sectional view of another embodiment of a fuel element showing the pre-curved cladding walls and pre-curved fuel segments in an initial configuration (dashed lines) and the swollen fuel and deformed cladding (solid lines).

[0026] [Figure 4A] FIG. 2 is a schematic diagram of a front cross-sectional view of one embodiment of a fuel segment in an assembly in which the fuel may be fabricated as a single piece (D) or as stacked segments (A) and inserted into the cladding. [Figure 4B] FIG. 2 is a schematic diagram of a top cross-sectional view of one embodiment of a fuel segment in an assembly in which the fuel may be fabricated as a single piece (D) or as stacked segments (A) and inserted into the cladding. [Figure 4C] FIG. 2 is a schematic side cross-sectional view of one embodiment of a fuel segment in an assembly in which the fuel may be fabricated as a single piece (D) or as stacked segments (A) and inserted into the cladding. [Figure 4D] FIG. 1 is a schematic diagram of another front cross-sectional view of an embodiment of a fuel segment in an assembly in which the fuel may be fabricated as a single piece (D) or as stacked segments (A) and inserted into the cladding.

[0027] [Figure 5A] FIG. 5 is a schematic diagram of a front cross-sectional view of the fuel element assembly of FIG. 4 inserted in a reactor core. [Figure 5B] FIG. 5 is a schematic diagram of a top cross-sectional view of the fuel element assembly of FIG. 4 inserted in a reactor core. [Figure 5C] FIG. 5 is a schematic diagram of a cross-sectional side view of the fuel element assembly of FIG. 4 inserted in a reactor core. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0028] As used herein, the singular forms "a," "an," and "the" are intended to include plural references unless the context clearly indicates otherwise. Thus, the articles "a" and "an" are used to refer to one or to more than one (i.e., to at least one) of the grammatical object of the article. By way of example, "an element" means one element or more than one element.

[0029] Directional expressions used herein, such as, but not limited to, up, down, left, right, below, upward, front, rear, and variations thereof, relate to the orientation of elements as shown in the accompanying drawings and do not limit the scope of the claims, unless otherwise specified.

[0030] In this application, including the claims, unless otherwise indicated, all numbers expressing quantities, values, or properties should be understood in all instances to be modified by the term "about", and thus, even if the term "about" is not explicitly expressed in the number, the number can be read as if it were preceded by the term "about". Thus, unless indicated to the contrary, any numerical parameter set forth in the following description may vary depending on the desired properties sought to be obtained in the compositions and methods according to the present disclosure. At the very least, and not as an attempt to limit the application of the doctrine of equivalents to the scope of the claims, each numerical parameter set forth herein should be construed at least in light of the number of significant digits and by applying ordinary rounding techniques.

[0031] Furthermore, any numerical range recited herein is intended to include all subranges subsumed therein. For example, a range of "1 to 10" is intended to include any and all subranges between (and including) a minimum value of 1 and a maximum value of 10, i.e., having a minimum value of 1 or more and a maximum value of 10 or less.

[0032] Referring to FIG. 1 , a fuel element 10 is shown as it is initially configured prior to use. The fuel element 10 includes an elongated shaped SiC cladding 12 that encapsulates a nuclear fuel segment 14. The cladding 12 is shown in cross section as an elongated rectangular shape for housing the elongated fuel segment 14. The cladding 12 has two opposing elongated walls 18 and two opposing shorter end walls 16 in the initial configuration. The fuel segment 14 also has two initially parallel or substantially parallel elongated sides 20 and two end faces 22 that are relatively short relative to the elongated sides of the segment. The fuel segment 14 is sized relative to the cladding 12 such that a small gap 32 exists in a first distance between the elongated walls 18 of the cladding and the elongated sides 20 of the fuel segment 14 to allow just enough space for the segments to be loaded and stacked within the cladding 12. At each end of the cladding 12, at a second distance between the end wall 16 of the cladding 12 and the end face 22 of the segment 14, there is a larger gap 34. The larger gap 34 is larger than the small gap 32. The gap 34 is sized to allow fission gases to accumulate at pressures below the design pressure of the reactor (e.g., 2200 psia at 320° C. for a conventional pressurized water reactor (PWR)).

[0033] In use, at the beginning of the fuel life cycle, the fuel segment 14 swells. Fuel is isotropic, so it expands equally in all directions. With the elongated cladding and fuel configuration described herein, the elongated walls 18 provide a force that prevents the fuel from freely swelling in the transverse direction (i.e., along the Y-axis shown in FIGS. 1 and 2). Due to the smaller gaps 32 along the long edges of the walls 18, the expanding fuel will first compress the walls 18 of the cladding 12, causing the elongated walls 18 to deform outward. However, it is believed that the resistance to swelling from the elongated walls 18 will cause the fuel to become anisotropic and expand more in the direction of less resistance along the longitudinal axis of the cladding (i.e., along the X-axis shown in FIGS. 1 and 2). Due to the larger end gap 34 and the length of the elongated wall 18 of the cladding 12, the swelling fuel segment 14 expands into the gap 34 and the force exerted by the swelling segment 14 on the elongated wall 18 along the axis 44 is spread over a longer distance (from the axis 44 to the end wall 16), resulting in less overall strain on the cladding 12 over the distance from the axis 44 to the end wall 16. The larger end gap 34 allows for longitudinal expansion of the segment 14 without exerting significant force or hard contact between the end face 22 of the segment 14 and the end wall 16 of the cladding 12. As used herein, hard contact means contact between the segment 14 and the cladding, specifically contact that exerts some force against the cladding wall. SiC can withstand approximately 0.04% to 0.1% strain before cracking occurs, and in various embodiments, approximately 0.05% to 0.07% strain, so spreading the strain caused by swelling of the fuel segment 14 over a longer length of wall 18 limits the overall strain increase above an applicable percentage threshold.

[0034] In various embodiments, the center of the cladding wall 18 can withstand large displacements in the Y direction along the axis 44 due to the width of the fuel (in the direction from the axis 44 to the end wall 16), so the fuel segment can have a convex shape as shown in FIG.

[0035] Referring to FIG. 2, an alternative embodiment of a fuel element 100 is shown. In this embodiment, the cladding 12 is the same as the cladding 12 of the fuel element 10 shown in FIG. 1. The cladding 12 of the fuel element 100 is an elongated rectangular structure in cross section, also formed from SiC, and in its initial configuration has two opposing elongated walls 18, shown in solid lines, and two opposing shorter end walls 16. The fuel segment 114 of the fuel element 100 in its initial configuration is elliptical or oval in cross section, having two convexly curved elongated surfaces 120 and two end curves or apexes 122. A major axis is defined along the length of the oval segment 114 from apex to apex 122, and a shorter minor axis, perpendicular to the major axis, is defined across the width of the oval.

[0036] In the preferred loading mode, the major axis of the segments 114 is aligned with and coaxial with the longitudinal axis 40 of the cladding 12, and the minor axis is aligned coaxially with the transverse axis 44 of the cladding. As noted above, some deviation from the preferred arrangement may be tolerated, so long as the end gaps 34 allow for swelling of the segments 114 without increasing distortion of the cladding 12.

[0037] The fuel segments 114 are sized relative to the cladding 12 such that a small gap 32 exists between the elongated wall 18 of the cladding and the widest region of the longer convexly curved elongated surface 120 of the fuel segment 114 (the region considered as the sub-apexes of the ellipse along the minor axis) to allow just enough space in the widest region of the pellet for the segments 114 to be loaded and stacked within the cladding 12 without applying contact pressure against the interior surface 28 of the cladding 12 during loading. Due to the elliptical shape, the gap 32 widens into a gap 36 as the segments 114 curve from each sub-apex toward an end or apex 122. The fuel segments 114 are sized relative to the cladding 12 such that a larger gap 34 exists at each end of the cladding 12 between the end wall 16 of the cladding 12 and the end curve or apex 122 of the segments 114 compared to the small gap 32. This shape promotes lateral expansion of the fuel 114 toward the end gap 34, maximizing fuel loading. Because there is no fuel in the end gap 34, the SiC cladding 12 can be thickened and strengthened at the endwalls 16 without affecting heat transfer and fuel temperature.

[0038] 2 also illustrates in dashed lines the configuration of the cladding 12 and fuel segment 114 after a period of use at the beginning of a fuel life cycle where the segment 114 swells to a swollen configuration 124 and transforms the elongated wall 18 of the cladding 12 into the deformed configuration 26. As the fuel segment 114 swells, the convexly curved elongated side 120 expands outwardly and contacts the elongated sidewall 18 of the cladding 12 at the contact area 30, pushing the cladding wall outward at the maximum width point (sub-apex) along the width of the segment 114. The larger gap 34 between the segment apex 122 and the cladding end wall 16 is sized such that when the segment 114 swells to its maximum dimension, the apex 122 may (but need not) just contact the end wall 16, but does not apply a significant or significant force to the end wall 16 of the cladding 12 that would increase distortion of the cladding 12. Alternatively, when the segment 114 swells to its maximum dimension, the apex 122 does not contact the end wall 16, leaving a smaller gap 34'. In either case, the end wall 16 is not deformed by the swelling of the segment 114. The curved shape of the segment 114, even when expanded within the rectangular cladding 12, leaves a gap 36 to accommodate fission gases released during operation of the reactor using the fuel element 100.

[0039] The second distance, which defines the gap 34 between the fuel end face 22 / 122 in the initial configuration before swelling and the cladding end wall 16, is sized to allow maximum swelling of the selected fuel in addition to space for fission gases generated during use. One skilled in the art can determine the second distance by calculating by known means or determining by historical use the maximum amount of swelling the selected fuel will experience during use and the amount of fission gases that will be generated during use. The gap 34 is sized to allow fission gases to accumulate at pressures below the design pressure of the reactor (e.g., 2200 psia at 320° C. for a conventional PWR).

[0040] The first distance defines a gap 32 between the elongated wall 18 of the cladding 12 and the elongated surface 20 / 120 of the fuel in an initial configuration before swelling. The first distance gap 32 is sufficient to allow fuel to be inserted into the cladding prior to use, and is typically 0.07 mm.

[0041] Because the SiC cladding 12 bulges outward after a short radiation time, in various embodiments, the cladding elongated walls 18 can be pre-curved inwardly, concavely toward the fuel segments, to accommodate displacement during radiation and mitigate local stress buildup. Local stress buildup occurs because the initial expansion of the fuel segments places compressive rather than tensile forces on the cladding. The concave curvature as an initial configuration mitigates stress buildup resulting from SiC swelling gradients. Additionally or alternatively, the fuel can be shaped concavely to minimize stress in the direction of the minor axis 44.

[0042] 3, an alternative initial configuration of the fuel element 200 is shown in dashed lines and a post-swelling configuration is shown in solid lines. In various aspects, the fuel element 200 includes a fuel segment 214 having an elongated surface 220 that is concavely shaped in the initial configuration, which swells to a convex surface 220'. The fuel element 214 has a flat or curved end face 222 that swells outward to a flat surface 222' upon expansion. The cladding 212 can have straight flat walls as in the fuel element 10, or can include elongated walls 218 having an initial concave configuration (dashed lines) that swells to move the walls 218 to a flatter elongated wall 218' configuration (solid lines) to give the cladding 212 a generally rectangular shape. The wall 218 may also be expanded outwardly into a convex shape, in which case the final shape is lenticular and not rectilinear. FIG. 3 shows both the cladding and fuel element in an initial concave shaped configuration. However, the fuel element 214 may be inserted through the top of the fuel element into the cladding 12 as shown in FIGS. 1 and 2.

[0043] Similar to the fuel elements 10, 100, a smaller gap 232 is provided between the elongated wall 218 of the cladding and the elongated surface 220 of the fuel segment in the initial configuration. Upon swelling, the gap 232 closes at the contact area 230 between the wall 218' and the surface 220' along the transverse axis 44 as the elongated concave surface 220 of the fuel element expands in the Y direction to an elongated convex surface 220'. In the initial configuration, a larger gap 234 is provided between each end wall 16 of the cladding 214 and the opposing end face 222 of the fuel segment 214. Upon swelling, the larger end gap 234 on each end closes to a smaller, but still present, gap 234' as the fuel element 214 expands along the longitudinal axis 40 in the X direction. The center of the cladding wall 218 can withstand large displacements in the Y direction along the axis 44 due to the width (in the direction from the axis 44 to the end wall 16) of the fuel segments 214. This shape promotes lateral expansion of the fuel 214 toward the end gap 234 and maximizes fuel loading. Because there is no fuel in the end gap 234, the SiC cladding 212 can be thickened and strengthened at the end wall 16 without affecting heat transfer and fuel temperature.

[0044] The SiC cladding may preferably be made of materials such as SiC monoliths, SiC fibers, or a combination of the two, as taught in U.S. Patent Nos. 6,246,740, 5,391,428, 5,338,576, and 5,182,077, and U.S. Patent Application Publication Nos. 2006 / 0039524, 2007 / 0189952, and 2015 / 0078505, the relevant portions of which are incorporated herein by reference. In various embodiments, the ceramic yarn is formed from SiC fibers. The SiC fibers may preferably be SiC fibers that contain primarily Si and C, and a trace or relatively small amount of O. Exemplary amounts are: Silicon: 50% to 70% by weight (preferably 68% to 70%) C: 30% to 40% by weight (preferably 30% to 32%) O: 0.01% to 14% by weight (preferably 0.01% to 0.5%) The SiC fiber cladding may utilize SiC in the form of fiber tows having between 500 and 5000 fibers per tow and a thickness between 100 and 600 microns.

[0045] The fuel used in the fuel segments 10, 100, or 200 may be selected from known fissile materials for use in commercial nuclear reactors for energy production, such as, but not limited to, UO2, U3Si2, UN, and uranium alloys and other oxide fuels. The fuel element designs described herein can be adapted to any suitable known fuel, but are particularly useful for UO2, which has heretofore been unsuitable for use with SiC cladding.

[0046] The fuel segment 14 (or 114 or 214) in embodiments in which the fuel segment is a single unit is inserted into an elongated cladding 12 column, as shown in FIG. 4D, or multiple fuel segments 14 are stacked one above the other in an elongated cladding 12 column, as shown in FIG. 4A. In either case, the fuel segment 14, 114, or 214 is generally centered along the vertical axis (the axis extending in the Z direction perpendicular to the axes 40, 44) as well as the horizontal axis 44 (the axis extending along the width of the cladding 12 and pellets 14 and through the center of the cladding 12 and pellets 14). Multiple fuel elements 10, 100, or 200 are inserted into a fuel assembly 50 in a nuclear reactor core, as shown in FIGS. 5A-C.

[0047] As noted above, silicon carbide is a very promising accident tolerant fuel cladding, but implementing SiC in conventional rod-shaped fuel has presented challenges that the fuel element configuration described herein overcomes. To prevent excessive distortion of the cylindrical rod-shaped cladding, a uniform annular gap exists between the cylindrical rod cladding and the cylindrical fuel pellets, and this annular gap must be large enough to accommodate the fuel swelling radially after some time in the reactor, typically more than six months. As the SiC cladding swells at the beginning of the fuel life cycle, it expands the cladding further, increasing the initial annular gap. At the beginning of the life cycle, the fuel shrinks. Since the fissile contents are at their best at the beginning of life, the fuel pellets generate the most heat at that time, and the expanding initial gap, coupled with the initial shrinking pellets and swelling cladding, presents a risk that the fuel pellet centerline temperature will exceed its melting point early in life. As the fuel cycle progresses, the pellets stop shrinking and begin to expand due to the accumulation of fission products that are less dense than the original uranium fuel. Because the swelling of the cladding stops early in life, the expanding pellets have the potential to contact and destroy the SiC cladding. Fuels such as UO2 are poor conductors of heat, so wider gaps adversely affect energy production by requiring the reactor to operate at lower power.

[0048] In the embodiments shown herein, the fuel-cladding gap is minimized, thereby minimizing the rise in core temperature during transients and reducing stored energy in the fuel. Additionally, the fuel elements 10, 100, 200 described herein provide a mechanism for the cladding 12 to accommodate thermal expansion and swelling of the fuel without suffering mechanical failure from the forces and resulting high strains that would otherwise be exerted on the cladding in conventional rod-type configurations.

[0049] The elongated shape of the fuel 14, 114, 214 with gaps 34, 234 and the elongated SiC cladding 12 described herein can accommodate contact between the swollen fuel and the elongated walls 18 of the cladding because the cladding 12 has the freedom to move laterally (along axis 44 in the Y direction) and can withstand strain to a significant extent from the fuel 14 / 114 / 214 due to the large spread across the width of the elongated cladding (the distance from axis 44 to each end wall 16). The elongated fuel design described herein also provides more expansion (along axis 40 in the X direction) of the fuel segments 14 / 114 / 214 in the longer walls 18 of the cladding 12 under contact (depending on the length of the end gaps 34 on the two end walls 16). The various embodiments of the fuel elements 10, 100, 200 shown in Figures 1, 2, and 3, respectively, have the potential to significantly reduce fuel temperatures and therefore contact loads on the cladding during transients. Because the overall gap between the cladding and the fuel can be minimized, the elongated designs described herein have the potential to load more fuel and improve fuel cycle costs.

[0050] In summary, the fuel elements 10, 100, 200 provide the following benefits: 1. Improved heat transfer due to smaller gaps or direct contact between the fuel and the cladding compared to cylindrical fuel rods; 2. Larger fuel volume per reactor volume due to the lack of excessive initial clearance to accommodate future fuel swelling; 3. Lower fuel temperatures due to smaller gaps resulting in less fission gas release and swelling; 4. Less distortion in the local deformation of the cladding during the transition due to a larger span of the cladding faces; 5. Reduced tensile stress during strong contact between fuel and cladding, 6. The long walls of the cladding surface may be pre-curved or the fuel may be convexly shaped to further reduce local stress buildup. 7. Allows the use of UO2 fuel without additives to increase thermal conductivity for accident resistance characteristics and additional manufacturing costs; 8. Operates on other innovative fuel materials such as U3Si2, UN, and U-alloys; 9. In the case of concave design, the contact pressure is converted into bending stress, especially at the ends, to ensure compressive stress in the outer layer for sealing.

[0051] The fuel elements 10, 100, 200 described herein may utilize SiC cladding with UO2 fuel with minimal initial gap between the cladding and the fuel. The gaps 34 / 234 on the ends of the fuel elements 10 / 100 / 200 provide volume for fission gases and expansion of the fuel segments 14 / 114 / 214 along the major axis 40, thereby reducing stress on the cladding 12 when the fuel segments 14 / 114 / 214 and the cladding 12 are in contact, as compared to rod designs. In certain embodiments, the elongated sidewalls 18 of the SiC cladding may be pre-curved to mitigate stress buildup from SiC swelling gradients, and / or the fuel may be shaped convexly or concavely to minimize stress in the direction of the minor axis 44.

[0052] The fuel elements 10, 100, and 200 described herein can significantly reduce stress build-up in the SiC cladding and mitigate mechanical failure of SiC from fuel-cladding mechanical interactions. The fuel elements 10, 100, and 200 enable compatibility of SiC cladding with UO2 in light water reactors and also operate with other high thermal conductivity fuels such as U3Si2, UN, and uranium alloys.

[0053] The present invention has been described according to several embodiments, which are intended to be illustrative in all respects, not limiting. Thus, the present invention is capable of many variations in its detailed implementation, which can be derived by those skilled in the art from the description contained herein.

[0054] All patents, patent applications, publications, or other disclosure materials mentioned herein are incorporated herein by reference in their entirety, as if each individual reference were expressly incorporated by reference. All references and any material, or portions thereof, that are said to be incorporated herein by reference are incorporated herein only to the extent that the incorporated material does not contradict existing definitions, statements, or other disclosure material set forth in this disclosure. Thus, to the extent necessary, the disclosure set forth herein supersedes any conflicting material incorporated herein by reference and the disclosure expressly set forth in the control of this application.

[0055] The present invention has been described with reference to various exemplary and illustrative embodiments. The embodiments described herein are understood to provide illustrative features of various details of various embodiments of the disclosed invention, and therefore, unless otherwise specified, it should be understood that, to the extent possible, one or more features, elements, components, components, ingredients, structures, modules, and / or aspects of the disclosed embodiments may be combined, separated, interchanged, and / or rearranged with one or more other features, elements, components, components, ingredients, structures, modules, and / or aspects of the disclosed embodiments without departing from the scope of the disclosed invention. Thus, it will be appreciated by those skilled in the art that various substitutions, modifications, or combinations of any of the exemplary embodiments may be made without departing from the scope of the invention. Moreover, those skilled in the art will recognize, or be able to ascertain using no more than routine experimentation, many equivalents to the various embodiments of the invention described herein upon reviewing this specification. Thus, the present invention is not limited by the description of the various embodiments, but rather by the scope of the claims.

Claims

1. 1. An elongated fuel element for use in a nuclear reactor, comprising: a silicon carbide cladding; It has nuclear fuel and the silicon carbide cladding has two opposing elongated walls and two opposing end walls that are shorter than the elongated walls; the elongated wall and the end wall define an enclosure; the enclosure has an end wall-to-end wall length and an elongated wall-to-elongated wall width; the cladding has a longitudinal axis and a transverse axis perpendicular to the longitudinal axis; the nuclear fuel is disposed within the enclosure; The fuel has two elongated surfaces and two end faces shorter than the elongated surfaces; each of the two elongated surfaces being minimally spaced a first distance in opposed relationship from a different one of the elongated walls of the cladding prior to swelling in use; each of the end faces being spaced a second distance in opposed relation from a different one of the end walls of the cladding prior to swelling in use; the second distance is greater than the first distance; the first and second distances are dimensioned such that, when the fuel swells in use, the swelling fuel swells beyond the first distance to less than or equal to the second distance to deform the elongated wall of the cladding without deforming the end wall of the cladding and without distorting the cladding by more than 0.1%; the fuel is configured in cross section as an oval shape defining a vertex at each of the shorter end faces and two convexly curved elongated surfaces; The fuel element, wherein the oval shape has a major axis extending from apex to apex and a minor axis perpendicular to the major axis.

2. each of the convexly curved elongate surfaces defines a minor vertex on said minor axis and curves from said minor vertex to and intersects with each of the vertices; 2. The fuel element of claim 1, wherein the first distance is a minimum between the minor apex and the elongated wall of the cladding.

3. 1. An elongated fuel element for use in a nuclear reactor, comprising: a silicon carbide cladding; It has nuclear fuel and the silicon carbide cladding has two opposing elongated walls and two opposing end walls that are shorter than the elongated walls; the elongated wall and the end wall define an enclosure; the enclosure has an end wall-to-end wall length and an elongated wall-to-elongated wall width; the cladding has a longitudinal axis and a transverse axis perpendicular to the longitudinal axis; the nuclear fuel is disposed within the enclosure; The fuel has two elongated surfaces and two end faces shorter than the elongated surfaces; each of the two elongated surfaces being minimally spaced a first distance in opposed relationship from a different one of the elongated walls of the cladding prior to swelling in use; each of the end faces being spaced a second distance in opposed relation from a different one of the end walls of the cladding prior to swelling in use; the second distance is greater than the first distance; the first and second distances are dimensioned such that, when the fuel swells in use, the swelling fuel swells beyond the first distance to less than or equal to the second distance to deform the elongated wall of the cladding without deforming the end wall of the cladding and without distorting the cladding by more than 0.1%; A fuel element wherein the elongated wall of the cladding is curved concavely inwardly toward the fuel prior to deformation in use and is deformed outwardly in use.

4. 4. The fuel element of claim 3, wherein the elongated surfaces of the fuel are concavely curved inwardly toward one another prior to swelling in use and swell outwardly in use to form convexly curved elongated surfaces that extend beyond the first distance and deform the elongated walls of the cladding.

5. 5. The fuel element of claim 4, wherein the end surface of the fuel is flat prior to swelling with use and swells outwardly during use to form a convexly curved end surface.

6. 5. The fuel element of claim 4, wherein the end surface of the fuel is flat prior to swelling due to use and wherein the end surface remains flat during use.

7. 4. The fuel element of claim 3, wherein the end walls of the cladding are flat prior to swelling with use.

8. The fuel element of claim 7 , wherein the end wall remains flat in use.

9. 1. An elongated fuel element for use in a nuclear reactor, comprising: a silicon carbide cladding; It has nuclear fuel and the silicon carbide cladding has two opposing elongated walls and two opposing end walls that are shorter than the elongated walls; the elongated wall and the end wall define an enclosure; the enclosure has an end wall-to-end wall length and an elongated wall-to-elongated wall width; the cladding has a longitudinal axis and a transverse axis perpendicular to the longitudinal axis; the nuclear fuel is disposed within the enclosure; The fuel has two elongated surfaces and two end faces shorter than the elongated surfaces; each of the two elongated surfaces being minimally spaced a first distance in opposed relationship from a different one of the elongated walls of the cladding prior to swelling in use; each of the end faces being spaced a second distance in opposed relation from a different one of the end walls of the cladding prior to swelling in use; the second distance is greater than the first distance; the first and second distances are dimensioned such that, when the fuel swells in use, the swelling fuel swells beyond the first distance to less than or equal to the second distance to deform the elongated wall of the cladding without deforming the end wall of the cladding and without distorting the cladding by more than 0.1%; the elongated surfaces of the fuel are concavely curved inwardly towards each other prior to swelling in use and swell outwardly in use to form convexly curved elongated surfaces, the convexly curved elongated surfaces extending beyond the first distance to deform the elongated walls of the cladding; The fuel element has a major axis extending from end face to end face and a minor axis perpendicular to the major axis.

10. 10. The fuel element of claim 9, wherein each concavely curved surface defines a minor apex on the minor axis and curves from the minor apex to and meets a respective end face.

11. 11. The fuel element of claim 10, wherein the end face of the fuel defines a flat surface prior to swelling in use and swells outwardly in use to form a convexly curved end face.

12. 11. The fuel element of claim 10, wherein the end face of the fuel defines a flat surface prior to swelling due to use, and wherein the end face remains flat in use.

13. 1. An elongated fuel element for use in a nuclear reactor, comprising: a silicon carbide cladding; It has nuclear fuel and the silicon carbide cladding has two opposing elongated walls and two opposing end walls that are shorter than the elongated walls; the elongated wall and the end wall define an enclosure; the enclosure has an end wall-to-end wall length and an elongated wall-to-elongated wall width; the cladding has a longitudinal axis and a transverse axis perpendicular to the longitudinal axis; the nuclear fuel is disposed within the enclosure; The fuel has two elongated surfaces and two end faces shorter than the elongated surfaces; each of the two elongated surfaces being minimally spaced a first distance in opposed relationship from a different one of the elongated walls of the cladding prior to swelling in use; each of the end faces being spaced a second distance in opposed relation from a different one of the end walls of the cladding prior to swelling in use; the second distance is greater than the first distance; the first and second distances are dimensioned such that, when the fuel swells in use, the swelling fuel swells beyond the first distance to less than or equal to the second distance to deform the elongated wall of the cladding without deforming the end wall of the cladding and without distorting the cladding by more than 0.1%; the fuel, prior to swelling due to use, is configured in cross section into a rectilinear shape defining a flat end face and a flat elongated surface; The rectilinear shape has a major axis extending from end face to end face and a minor axis perpendicular to the major axis.

14. 14. The fuel element of claim 13, wherein the fuel swells outwardly along both the major axis and the minor axis in use to form an oval configuration in cross section.

15. the cladding, prior to swelling in use, is configured in cross section into a rectilinear shape defining a flat end wall and a flat elongated wall; 14. The fuel element of claim 13, wherein the elongated wall deforms outwardly as the fuel swells with use.

16. The fuel is UO 2 , U 3 S 2 16. The fuel element of claim 1, wherein the fuel element is selected from the group consisting of uranium, UN, and uranium alloys.

17. The fuel is UO 2 16. The fuel element according to claim 1, wherein

18. 16. The fuel element of any one of claims 1 to 15, wherein the end walls of the cladding are thicker in cross-section than the elongated walls of the cladding.

19. 16. The fuel element of any one of claims 1 to 15, wherein the distortion of the cladding due to fuel swelling is less than or equal to 0.05%.

Citation Information

Patent Citations

  • Nuclear fuel rods and methods for manufacturing pellets for such nuclear fuel rods

    JP2013513099A

  • Fuel rod and fuel assembly

    JP2016200465A

  • Fuel element with multiple smear density fuels

    JP2018529095A

  • Fuel element for nuclear reactor

    US3244599A

  • Engineered sic-sic composite and monolithic sic layered structures

    WO2018031596A2