Method for manufacturing semiconductor element mounting package substrate
The method of forming interlayer connections on a core resin layer before peeling improves the yield and handling of thinner package substrates by maintaining substrate integrity and reducing warpage, addressing rigidity and alignment challenges in semiconductor element manufacturing.
Patent Information
- Application Number
- JP2020559777
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2018-12-14
- Filing Date
- 2019-10-21
- Publication Date
- 2024-11-14
- Estimated Expiration
- 2039-10-21
AI Technical Summary
The manufacturing of thinner package substrates for semiconductor elements faces challenges such as reduced rigidity leading to warpage and handling issues, which decrease yield due to increased susceptibility to breakage and alignment problems during processing.
A method involving the formation of a first substrate with a metal layer, insulating resin layer, and a second metal layer on a core resin layer, followed by electrolytic and electroless copper plating of non-through holes, and subsequent lamination and peeling steps to form a second substrate, which is then patterned to create a wiring conductor, ensuring interlayer connections without separating from the core resin layer until completion.
This approach enhances the yield of package substrates by maintaining substrate integrity and reducing warpage and handling issues, improving manufacturing efficiency and product quality.
Smart Images

Figure 0007583362000001
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a package substrate for mounting a semiconductor element. [Background technology]
[0002] In recent years, the trend toward high functionality and miniaturization of semiconductor packages, which are widely used in electronic devices, communication devices, personal computers, etc., has been accelerating. Accordingly, there is a demand for thinner printed wiring boards and package substrates for mounting semiconductor elements in semiconductor packages. Usually, printed wiring boards and package substrates for mounting semiconductor elements are fabricated by laminating a layer that will become a circuit pattern (hereinafter also simply referred to as "wiring conductor") and an insulating material on a support substrate.
[0003] As a manufacturing method of such a package substrate for mounting a semiconductor element, for example, a method has been disclosed in which a circuit-forming substrate made of an ultra-thin copper foil with a carrier foil having a first insulating resin provided on the carrier foil surface is used, a first wiring conductor is formed by pattern electrolytic copper plating, a second insulating resin is further laminated, and then a second wiring conductor is formed (see, for example, Patent Document 1 below). As a manufacturing technique related to these package substrates for mounting a semiconductor element, a method has been disclosed in which a plurality of layers are laminated on a core substrate, a laminate is formed, and then the laminate is separated from the core substrate to produce a semiconductor package substrate or the like (see, for example, Patent Documents 2 to 4 below). [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2005-101137 A [Patent Document 2] JP 2014-220402 A [Patent Document 3] JP 2012-099857 A [Patent Document 4] JP 2011-119722 A Summary of the Invention [Problem to be solved by the invention]
[0005] As a manufacturing technique related to the package substrate for mounting semiconductor elements as described above, a method using a circuit-forming substrate formed by building up an insulating layer such as prepreg and a metal foil on both sides of a copper-clad laminate with a core resin layer as a core, is known. When the circuit-forming substrate has four layers of metal foil, it is also called a "four-layer coreless shield plate." For example, the four-layer coreless shield plate is then turned into a six-layer coreless shield plate through a patterning process or the like, and each substrate (laminate) provided on both sides of the core resin layer is peeled off.
[0006] In recent years, there has been an increasing demand for a package substrate for mounting a semiconductor element to be made thinner, for example, to a thickness of about 40 μm. As the package substrate becomes thinner, issues that were not previously considered problematic have become apparent as new problems. For example, in the manufacturing process of the package substrate, it is necessary to perform processes such as hole processing, desmear processing, and plating on the laminate, which is an intermediate product. When hole processing is performed, the rigidity of the laminate temporarily decreases until the holes are blocked by a plating process or the like. In addition, such a decrease in rigidity increases the possibility of warping of the laminate. In each process, the laminate needs to be transported to move to the next process, but if the thinned laminate is in a state of reduced rigidity, it is more likely to be damaged, and its handling properties decrease. In addition, as the substrate becomes thinner, the influence of the warping of the substrate (laminate) on each process, such as alignment, becomes greater. In this way, as the substrate becomes thinner, the yield may ultimately decrease due to various causes.
[0007] SUMMARY OF THE PRESENT DISCLOSURE In order to solve the above problems, an object of the present invention is to provide a method for manufacturing a package substrate for mounting semiconductor elements with excellent yield. [Means for solving the problem]
[0008] <1> A method for manufacturing a package substrate for mounting a semiconductor element, the method comprising the steps of: a first substrate forming step (a) of forming a first substrate on one or both sides of a core resin layer, the first substrate including a first metal layer having a thickness of 1 μm to 70 μm and capable of being peeled off from the core resin layer, a first insulating resin layer, and a second metal layer in this order; a first interlayer connection step (b) of forming non-through holes in the surface of the first substrate, the non-through holes reaching the surface of the first metal layer, and applying electrolytic copper plating and / or electroless copper plating to the inner walls of the non-through holes to connect the second metal layer and the first metal layer; a second substrate forming step (c) of forming a second substrate by heating and pressurizing a laminate formed by arranging a second insulating resin layer and a third metal layer in this order on a surface of the second metal layer of the first substrate; a second interlayer connection step (d) of forming non-through holes in the surface of the second substrate, the non-through holes reaching the surface of the second metal layer, and applying electrolytic copper plating and / or electroless copper plating to the inner walls of the non-through holes to connect the second metal layer and the third metal layer; a peeling step (e) of peeling a third substrate having the first metal layer, the first insulating resin layer, the second metal layer, the second insulating resin layer, and the third metal layer in this order from the core resin layer; a wiring conductor forming step (f) of patterning the first metal layer and the third metal layer of the third substrate to form the wiring conductor; A method for manufacturing a package substrate for mounting a semiconductor element, comprising: <2> The first substrate forming step (a) includes: (i) disposing the first metal layer on one or both sides of the core resin layer, laminating them by heating and pressing, and then disposing the first insulating resin layer and the second metal layer in this order on the surface of the first metal layer, and forming the first substrate by heating and pressing; or (ii) forming a laminate in which the first metal layer, the first insulating resin layer, and the second metal layer are disposed in this order on both sides of the core resin layer, and the laminate is heated and pressurized all at once to form a first substrate; <1> 2. A method for manufacturing the package substrate for mounting a semiconductor element according to claim 1 . <3> The third substrate has a thickness of 5 μm to 100 μm. <1> or <2> 2. A method for manufacturing the package substrate for mounting a semiconductor element according to claim 1 . <4> The first metal layer has a release layer, and the first substrate has the first metal layer disposed so that the release layer and the core resin layer are in contact with each other. <1> ~ <3> 2. A method for producing a package substrate for mounting a semiconductor element according to claim 1 , <5> the third metal layer includes a carrier layer, and after the first substrate is heated and pressed in the second substrate forming step (c), the carrier layer is removed from the third metal layer. <1> ~ <4> 2. A method for producing a package substrate for mounting a semiconductor element according to claim 1 , <6> At least one of the first metal layer, the second metal layer, and the third metal layer is a copper foil. <1> ~ <5> 2. A method for producing a package substrate for mounting a semiconductor element according to claim 1 , <7> At least one of the core resin layer, the first insulating resin layer, and the second insulating resin layer is a prepreg in which a base material is impregnated with a resin. <1> ~ <6> 2. A method for producing a package substrate for mounting a semiconductor element according to claim 1 , <8> 8. The method for producing a package substrate for mounting a semiconductor element according to claim 1, wherein the core resin layer has a thickness of 1 μm to 90 μm. Effect of the Invention
[0009] According to the present invention, a method for manufacturing a package substrate for mounting a semiconductor element with excellent yield can be provided. [Brief description of the drawings]
[0010] [Figure 1] 1A to 1C are schematic diagrams illustrating an embodiment of a method for manufacturing a package substrate for mounting a semiconductor element according to the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Hereinafter, the present invention will be described by way of an embodiment, but the aspects of the present invention are not limited to the embodiment described below.
[0012] The method for manufacturing a package substrate for mounting a semiconductor element according to the present embodiment (hereinafter, sometimes simply referred to as the "manufacturing method according to the present embodiment") is as follows: A method for manufacturing a package substrate for mounting a semiconductor element, the method comprising the steps of: a first substrate forming step (a) of forming a first substrate on one or both sides of a core resin layer, the first substrate including a first metal layer having a thickness of 1 μm to 70 μm and capable of being peeled off from the core resin layer, a first insulating resin layer, and a second metal layer in this order; a first interlayer connection step (b) of forming non-through holes in the surface of the first substrate, the non-through holes reaching the surface of the first metal layer, and applying electrolytic copper plating and / or electroless copper plating to the inner walls of the non-through holes to connect the second metal layer and the first metal layer; a second substrate forming step (c) of forming a second substrate by heating and pressurizing a laminate formed by arranging a second insulating resin layer and a third metal layer in this order on a surface of the second metal layer of the first substrate; a second interlayer connection step (d) of forming non-through holes in the surface of the second substrate, the non-through holes reaching the surface of the second metal layer, and applying electrolytic copper plating and / or electroless copper plating to the inner walls of the non-through holes to connect the second metal layer and the third metal layer; a peeling step (e) of peeling a third substrate having the first metal layer, the first insulating resin layer, the second metal layer, the second insulating resin layer, and the third metal layer in this order from the core resin layer; a wiring conductor forming step (f) of patterning the first metal layer and the third metal layer of the third substrate to form the wiring conductor; Includes.
[0013] In the conventional method, in many cases, after forming a first substrate, a laminate including a first metal layer, a first insulating resin layer, a second metal layer, a second insulating resin layer, and a third metal layer is peeled off from both sides of the substrate that is the core, and then the peeled laminate is subjected to hole processing, desmearing, plating, etc., to manufacture a package substrate for mounting a semiconductor element. However, according to such a conventional method, as the substrate becomes thinner, the handleability of the laminate decreases and the laminate is more likely to warp. As a result, the yield of the package substrate for mounting a semiconductor element, which is the final product, decreases. These problems such as the deterioration of handleability and warping are problems that often become apparent after the laminate is peeled off from the substrate that is the core.
[0014] In contrast, according to the manufacturing method of the present embodiment, after forming the second substrate, the laminate is not peeled off from the core resin layer, but a non-through hole is formed in the second substrate, and the inner wall is electrolytically plated with copper and / or electroless copper to connect the second metal layer and the third metal layer. Then, the third substrate having the first metal layer, the first insulating resin layer, the second metal layer, the second insulating resin layer, and the third metal layer in this order is peeled off from the core resin layer. The third substrate, which is the laminate after peeling, is already in a state where each layer is connected, and there is no need to perform hole processing or the like that reduces the rigidity of the laminate separated from the core resin layer. Therefore, according to the manufacturing method of the present embodiment, the burden on the third substrate after peeling is small, and it is possible to reduce the deterioration of the handleability due to the decrease in rigidity of the third substrate and the damage of the substrate due to the occurrence of warping. The manufacturing method of this embodiment will be described in detail below.
[0015] [First substrate formation step (a)] The first board formation step (a) is a step of forming a first board having a first metal layer having a thickness of 1 μm to 70 μm and peelable from the core resin layer, a first insulating resin layer, and a second metal layer in this order on one or both sides of the core resin layer. The configuration of the first board (board for circuit formation) will be described with reference to FIG. 1. FIG. 1 is a schematic diagram for explaining one embodiment of the manufacturing method of a package board for mounting a semiconductor element of the present invention. As shown in FIG. 1(A) and FIG. 1(B), the board for circuit formation (first board) 1 has a first metal layer 3, a first insulating resin layer 4, and a second metal layer provided on both sides of a core resin layer 2 (e.g., a prepreg) in the order from the front side of the core resin layer 2. Here, the "board for circuit formation" means a laminate including a core resin layer, a metal foil, and a resin layer, and means a state in which the metal foil is not patterned.
[0016] In the first substrate formation step (a), the method for forming the first substrate is not particularly limited, but the first substrate can be formed, for example, by either the following step (i) or (ii). (i) disposing the first metal layer on one or both sides of the core resin layer, laminating them by heating and pressing, and then disposing the first insulating resin layer and the second metal layer in this order on the surface of the first metal layer, and forming the first substrate by heating and pressing; or (ii) forming a laminate in which the first metal layer, the first insulating resin layer, and the second metal layer are arranged in this order on both sides of the core resin layer, and the laminate is heated and pressurized all at once to form a first substrate;
[0017] In the above (i), a pressing step (first press) is performed to form a copper-clad laminate (a state in which only the first metal layer is laminated on one or both sides of the core resin layer), and then a pressing step (second press) is performed by laminating the first insulating resin layer and the second metal layer. The method and conditions for laminating each layer are not particularly limited, but for example, the laminate can be vacuum-pressed under conditions of a temperature of 220±2°C, a pressure of 5±0.2MPa, and a holding time of 60 minutes. In addition, in order to obtain adhesion between each metal layer and the core resin layer or each insulating resin layer, the surface of each metal layer may be roughened. The roughening treatment is not particularly limited, and a known means can be appropriately used, for example, a means using a copper surface roughening liquid can be mentioned.
[0018] In the above (ii), the core resin layer is placed at the center, and the first metal layer, the first insulating resin layer, and the second metal layer are arranged in this order on both sides of the core resin layer to form a laminate, and then the laminate is heated and pressed all at once to form the first substrate. Here, "forming the first substrate (substrate for forming a circuit) all at once" means that in the first substrate forming step (a), the core resin layer is placed at the center, and the first metal layer, the first insulating resin layer, and the second metal layer are arranged in this order on both sides of the core resin layer, and then the laminate is heated and pressed (pressed) to form the first substrate (substrate for forming a circuit), and the first substrate is formed by performing a single press step. That is, in (ii), the press step for forming a copper-clad laminate is not performed, and the first insulating resin layer and the second metal layer are laminated, and then the first substrate is formed by performing a single press step.
[0019] In (ii), the lamination method and conditions for forming the laminate are not particularly limited, but for example, the laminate can be vacuum pressed under conditions of a temperature of 220±2°C, a pressure of 5±0.2 MPa, and a holding time of 60 minutes to form the first substrate. In addition, in order to obtain adhesion between each metal layer and the core resin layer or each insulating resin layer, a roughening treatment may be applied to the surface of each metal layer. The roughening treatment is not particularly limited, and known means can be used as appropriate, for example, a means using a copper surface roughening liquid can be mentioned.
[0020] As described above, when the circuit-forming substrate is formed in a single operation, one pressing step can be omitted, and therefore the production efficiency of the circuit-forming substrate and the semiconductor element mounting package substrate using the same can be improved.
[0021] (Core resin layer) The core resin layer in the substrate formation process (a) is not particularly limited, but may be, for example, a prepreg in which a base material such as glass cloth is impregnated with an insulating resin material (insulating material) such as a thermosetting resin, or an insulating film material. The thickness of the core resin layer is not particularly limited. However, when the first substrate is formed by the above-mentioned (ii) process, the thickness of the core resin layer is preferably 1 μm to 90 μm, and more preferably 1 μm to 80 μm. When the thickness of the core resin layer is 1 μm to 90 μm (preferably 1 μm to 80 μm), the moldability of the resin is sufficient, and when the first substrate is formed in a lump, the occurrence of wrinkles and unevenness in the metal layer on the surface of the third substrate peeled off from the core resin layer after the peeling step can be suppressed. Therefore, by forming the first substrate (substrate for forming a circuit) in a lump, the production efficiency is improved, and further, the occurrence of wrinkles and unevenness in the metal layer that causes patterning defects is suppressed, so that the yield of the package substrate for mounting a semiconductor element can be improved. From the viewpoint of lamination moldability, the thickness of the core resin layer is more preferably 3 μm to 40 μm, and particularly preferably 10 μm to 25 μm.
[0022] "Prepreg" is a material obtained by impregnating or coating a substrate with an insulating material such as a resin composition. The substrate is not particularly limited, and any well-known substrate used in various laminates for electrical insulating materials can be used as appropriate. Materials constituting the substrate include, for example, inorganic fibers such as E glass, D glass, S glass, or Q glass; organic fibers such as polyimide, polyester, or tetrafluoroethylene; and mixtures thereof. The substrate is not particularly limited, and may be, for example, a woven fabric, a nonwoven fabric, a roving, a chopped strand mat, a surfacing mat, or the like. The material and shape of the substrate are selected according to the intended use and performance of the molded product, and one or more types of materials and shapes may be used as necessary.
[0023] The thickness of the substrate can be appropriately set according to the thickness of the core resin layer, and is not particularly limited, but is usually 10 μm to 30 μm. The substrate can be surface-treated with a silane coupling agent or mechanically opened, and these substrates are suitable in terms of heat resistance, moisture resistance, and processability.
[0024] The insulating material is not particularly limited, and a known resin composition used as an insulating material for printed wiring boards can be appropriately selected and used. The resin composition can be based on a thermosetting resin having good heat resistance and chemical resistance. The thermosetting resin is not particularly limited, but examples thereof include phenol resin, epoxy resin, cyanate resin, maleimide resin, isocyanate resin, benzocyclobutene resin, vinyl resin, etc. The thermosetting resin may be used alone or in combination of two or more types.
[0025] Among thermosetting resins, epoxy resins are excellent in heat resistance, chemical resistance, and electrical properties, and are relatively inexpensive, so they can be suitably used as insulating materials. Examples of epoxy resins include bisphenol A type epoxy resins, bisphenol F type epoxy resins, bisphenol S type epoxy resins, alicyclic epoxy resins, aliphatic chain epoxy resins, phenol novolac type epoxy resins, cresol novolac type epoxy resins, bisphenol A novolac type epoxy resins, diglycidyl ethers of biphenols, diglycidyl ethers of naphthalene diols, diglycidyl ethers of phenols, diglycidyl ethers of alcohols, and alkyl-substituted, halogenated, and hydrogenated versions of these. One type of epoxy resin may be used alone, or two or more types may be mixed together. The curing agent used together with this epoxy resin can be any agent capable of curing the epoxy resin, and examples of such agents include polyfunctional phenols, polyfunctional alcohols, amines, imidazole compounds, acid anhydrides, organic phosphorus compounds, and halides thereof. These epoxy resin curing agents may be used alone or in combination of two or more.
[0026] The cyanate resin is a resin that generates a cured product having a triazine ring as a repeating unit by heating, and the cured product has excellent dielectric properties. Therefore, it is suitable for cases where high frequency properties are particularly required. The cyanate resin is not particularly limited, but examples thereof include 2,2-bis(4-cyanatophenyl)propane, bis(4-cyanatophenyl)ethane, 2,2-bis(3,5dimethyl-4-cyanatophenyl)methane, 2,2-(4-cyanatophenyl)-1,1,1,3,3,3-hexafluoropropane, α,α'-bis(4-cyanatophenyl)-m-diisopropylbenzene, cyanate esters of phenol novolac and alkylphenol novolac, and the like. Among them, 2,2-bis(4-cyanatophenyl)propane is preferable because it has a particularly good balance between the dielectric properties and curability of the cured product and is inexpensive. These cyanate resins such as cyanate ester compounds may be used alone or in combination of two or more. The cyanate ester compounds may be partially oligomerized in advance to a trimer or a pentamer.
[0027] Furthermore, a curing catalyst or a curing accelerator can be used in combination with the cyanate resin. As the curing catalyst, for example, metals such as manganese, iron, cobalt, nickel, copper, zinc, etc. can be used, and specifically, organic metal salts such as 2-ethylhexanoate and octylate, and organic metal complexes such as acetylacetone complex can be mentioned. The curing catalyst may be used alone or in combination of two or more kinds. As the curing accelerator, it is preferable to use phenols, and it is possible to use monofunctional phenols such as nonylphenol and paracumylphenol, bifunctional phenols such as bisphenol A, bisphenol F and bisphenol S, and polyfunctional phenols such as phenol novolac and cresol novolac. One type of curing accelerator may be used alone, or two or more types may be mixed and used.
[0028] The resin composition used as the insulating material may be blended with a thermoplastic resin in consideration of dielectric properties, impact resistance, film processability, etc. The thermoplastic resin is not particularly limited, but examples thereof include fluororesin, polyphenylene ether, modified polyphenylene ether, polyphenylene sulfide, polymethyl ether, polyetherimide, polyetheretherketone, polyacrylate, polyamide, polyamideimide, polybutadiene, etc. The thermoplastic resin may be used alone or in combination of two or more types.
[0029] Among thermoplastic resins, polyphenylene ether and modified polyphenylene ether are useful in terms of improving the dielectric properties of the cured product. Examples of polyphenylene ether and modified polyphenylene ether include poly(2,6-dimethyl-1,4-phenylene) ether, an alloy polymer of poly(2,6-dimethyl-1,4-phenylene) ether and polystyrene, an alloy polymer of poly(2,6-dimethyl-1,4-phenylene) ether and styrene-butadiene copolymer, an alloy polymer of poly(2,6-dimethyl-1,4-phenylene) ether and styrene-maleic anhydride copolymer, an alloy polymer of poly(3,6-dimethyl-1,4-phenylene) ether and polyamide, and an alloy polymer of poly(2,6-dimethyl-1,4-phenylene) ether and styrene-butadiene-acrylonitrile copolymer. In order to impart reactivity or polymerizability to the polyphenylene ether, a functional group such as an amine group, an epoxy group, a carboxyl group, or a styryl group may be introduced to a polymer chain end, or a functional group such as an amine group, an epoxy group, a carboxyl group, a styryl group, or a methacryl group may be introduced to a polymer chain side chain.
[0030] Among thermoplastic resins, polyamideimide resins are useful from the viewpoints of excellent moisture resistance and good adhesive properties for metals. The raw materials for polyamideimide resins are not particularly limited, but examples of the acidic components include trimellitic anhydride and trimellitic anhydride monochloride, and examples of the amine components include metaphenylenediamine, paraphenylenediamine, 4,4'-diaminodiphenyl ether, 4,4'-diaminodiphenylmethane, bis[4-(aminophenoxy)phenyl]sulfone, 2,2'-bis[4-(aminophenoxy)phenyl]sulfone, and 2,2'-bis[4-(aminophenoxy)phenyl]sulfone. Polyamide-imide resins may be modified with siloxane to improve drying properties, in which case siloxane diamines can be used as the amino component. Considering film processability, it is preferable to use polyamide-imide resins with a molecular weight of 50,000 or more.
[0031] Although the above-mentioned thermoplastic resins have been described as insulating materials mainly used for prepregs, the use of these thermoplastic resins is not limited to prepregs. For example, the above-mentioned thermoplastic resins processed into a film (film material) may be used as the core resin layer in the circuit-forming substrate.
[0032] The resin composition used as the insulating material may be mixed with an inorganic filler. The inorganic filler is not particularly limited, but examples thereof include alumina, aluminum hydroxide, magnesium hydroxide, clay, talc, antimony trioxide, antimony pentoxide, zinc oxide, fused silica, glass powder, quartz powder, and shirasu balloons. These inorganic fillers may be used alone or in combination of two or more.
[0033] The resin composition used as an insulating material may contain an organic solvent. The organic solvent is not particularly limited, and may be an aromatic hydrocarbon solvent such as benzene, toluene, xylene, or trimethylbenzene; a ketone solvent such as acetone, methyl ethyl ketone, or methyl isobutyl ketone; an ether solvent such as tetrahydrofuran; an alcohol solvent such as isopropanol or butanol; an ether alcohol solvent such as 2-methoxyethanol or 2-butoxyethanol; or an amide solvent such as N-methylpyrrolidone, N,N-dimethylformamide, or N,N-dimethylacetamide, if desired. The amount of the solvent in the varnish used to prepare the prepreg is preferably in the range of 40 to 80% by mass based on the entire resin composition. The viscosity of the varnish is preferably in the range of 20 to 100 cP (20 to 100 mPa·s).
[0034] The resin composition used as the insulating material may contain a flame retardant. The flame retardant is not particularly limited, but may be any of the known flame retardants such as bromine compounds such as decabromodiphenyl ether, tetrabromobisphenol A, tetrabromophthalic anhydride, and tribromophenol, phosphorus compounds such as triphenyl phosphate, trixylyl phosphate, and cresyl diphenyl phosphate, metal hydroxides such as magnesium hydroxide and aluminum hydroxide, red phosphorus and its modified products, antimony compounds such as antimony trioxide and antimony pentoxide, and triazine compounds such as melamine, cyanuric acid, and melamine cyanurate.
[0035] If necessary, the resin composition used as the insulating material may further contain the above-mentioned curing agent and curing accelerator, as well as various additives and fillers such as thermoplastic particles, colorants, ultraviolet opacifiers, antioxidants, and reducing agents.
[0036] In this embodiment, the prepreg can be obtained as a semi-cured (B-stage) prepreg by, for example, impregnating or coating a base material with a resin composition (including varnish) so that the amount of the resin composition adhering to the base material is 20 to 90 mass % in terms of the resin content in the dried prepreg, and then drying by heating for 1 to 30 minutes at a temperature of 100 to 200° C. As such a prepreg, for example, GHPL-830NS series and GHPL-830NSF series (product names) manufactured by Mitsubishi Gas Chemical Company can be used.
[0037] (First metal layer) The first metal layer is made of a metal foil having a thickness of 1 μm to 70 μm and capable of being peeled off from the core resin layer. If the thickness of the first metal layer is less than 1 μm, the first to third substrates will be poorly molded, and if it exceeds 70 μm, the surface will be defective. From the viewpoint of circuit formation, the thickness of the first metal layer is preferably 1 μm to 12 μm, and more preferably 2 μm to 5 μm.
[0038] As described later, the third substrate is peeled off from the interface between the core resin layer and the first metal layer in the peeling step. The surface roughness (10-point average roughness (Rzjis) shown in JIS B0601:2001) of the first metal layer when peeled off from the core resin layer in the peeling step is preferably 1 μm to 3 μm, more preferably 1 μm to 2 μm, and particularly preferably 1 μm to 1.5 μm, from the viewpoint of preventing pattern defects. The surface roughness of the first metal layer can be measured, for example, by cutting a sample to a size of 5×5 cm, and then measuring an area of 1×1 cm using a microscope VR-3100 (manufactured by Keyence Corporation).
[0039] The first metal layer may be, for example, a copper foil. The copper foil may be, for example, a peelable type. The "peelable type" copper foil is an extremely thin copper foil having a peelable layer, and the peelable layer is, for example, a peelable copper foil. When a peelable type copper foil is used, the first metal layer is laminated so that the peelable layer is in contact with the core resin layer.
[0040] The release layer may be, for example, a layer containing at least a silicon compound, and may be formed, for example, by applying a silicon compound consisting of a single or multiple combinations of silane compounds to a copper foil or an ultra-thin copper foil. The means for applying the silicon compound is not particularly limited, and for example, known means such as coating can be used. The bonding surface of the copper foil with the release layer may be subjected to a rust-proofing treatment (a rust-proofing layer may be formed). The rust-proofing treatment may be performed using nickel, tin, zinc, chromium, molybdenum, cobalt, or an alloy thereof.
[0041] The thickness of the release layer is not particularly limited, but from the viewpoint of removability and peelability, it is preferably 5 nm to 100 nm, more preferably 10 nm to 80 nm, and particularly preferably 20 nm to 60 nm.
[0042] (First insulating resin layer) The first insulating resin layer can be made of the same material as the core resin layer (e.g., prepreg). The thickness of the first insulating resin layer is not particularly limited since it is appropriately set according to the desire, but can be, for example, 10 μm to 100 μm, preferably 10 μm to 50 μm, and more preferably 10 μm to 30 μm.
[0043] (Second metal layer) The second metal layer may be made of the same material as the first metal layer (e.g., copper foil). The thickness of the second metal layer is not particularly limited since it is appropriately set according to the need, but may be, for example, 2 μm to 70 μm, preferably 2 μm to 18 μm, and more preferably 2 μm to 12 μm. The second metal layer may be, for example, an ultra-thin copper foil with a carrier. In this case, the second metal layer is disposed so that the copper foil or the like is in contact with the second insulating resin layer, and the carrier is peeled off after the first substrate is formed by heating and pressing.
[0044] [First interlayer connection process (b)] The first interlayer connection step (b) is a step of forming a non-through hole on the surface of the first substrate, which reaches the surface of the first metal layer, and applying electrolytic copper plating and / or electroless copper plating to the inner wall of the non-through hole to connect the second metal layer and the first metal layer. Through the first interlayer connection step (b), as shown in FIG. 1(E), the first metal layer 3 and the second metal layer 5 are interlayer connected via the copper plating film 5A in the first substrate 1, and electrical conduction is ensured.
[0045] (Formation of non-through holes) In the first interlayer connection process (b), non-through holes reaching the surface of the first metal layer are formed on the surface of the first substrate 1. As shown in FIG. 1(C), non-through holes 6A are provided on both sides of the first substrate 1. The means for forming the non-through holes is not particularly limited, and for example, known means such as a laser such as a carbon dioxide gas laser or a drill can be used. The number and size of the non-through holes can be appropriately selected as desired. After the non-through holes are formed, a desmear treatment can be performed using an aqueous solution of sodium permanganate or the like.
[0046] (Interlayer connection) In the first interlayer connection step (b), after forming the non-through holes 6A, as shown in FIG. 1(D), electrolytic copper plating and / or electroless copper plating are performed to form a copper plating film 5A on the inner wall of the non-through hole, and the first metal layer 3 and the second metal layer 5 are electrically connected. At this time, the thickness of the second metal layer on both sides of the first substrate may be increased by the electrolytic copper plating and / or electroless copper plating, and the layer thickness may be adjusted by film thickness adjustment described later. The method of performing electrolytic copper plating and / or electroless plating is not particularly limited, and a known method can be adopted. The copper plating may be either electrolytic copper plating or electroless plating, but it is preferable to perform both electrolytic copper plating and electroless plating.
[0047] (Film thickness adjustment) In the first interlayer connection process (b), as shown in FIG. 1(E), after the electrolytic / electroless copper plating process, if necessary, the second metal layer 5 can be subjected to a known process such as an etching process so that the second metal layer 5 has a desired thickness, thereby adjusting the film thickness. The thickness of the second metal layer after adjustment is not particularly limited since it is appropriately set as desired, but can be, for example, 2 μm to 30 μm, preferably 2 μm to 20 μm, and more preferably 2 μm to 12 μm.
[0048] (Patterning) In the first interlayer connection process (b), after the surface of the second metal layer 5 is adjusted as necessary, a pattern can be formed on the second metal layer 5 of the first substrate 1 as shown in Fig. 1(F). The means for forming the pattern of the second metal layer is not particularly limited, but it can be formed, for example, by the following process.
[0049] The patterning is not particularly limited, but for example, the second metal layer is surface-treated, a dry film resist or the like is laminated, and a negative mask is then attached, after which a circuit pattern is printed using an exposure machine, and the dry film resist is developed using a developer to form an etching resist. Thereafter, an etching process is performed, and copper in the area without the etching resist is removed using an aqueous ferric chloride solution or the like, and the resist is then removed, thereby forming a pattern on the second metal layer.
[0050] The resist is not particularly limited, and for example, a known resist such as a commercially available dry film resist can be appropriately selected and used. In addition, the photolithography (including exposure, development, and removal of the resist) for forming a pattern on the second metal layer is not particularly limited, and can be performed using known means and devices.
[0051] The pattern width of the second metal layer is not particularly limited and can be appropriately selected depending on the application, and can be, for example, 5 to 100 μm, and preferably 10 to 30 μm.
[0052] [Second substrate formation process (c)] The second substrate forming step (c) is a step of forming a second substrate by heating and pressurizing a laminate formed by arranging a second insulating resin layer and a third metal layer in this order on the surface of the second metal layer of the first substrate. Through the second substrate forming step (c), a second substrate 7 can be obtained in which a second insulating resin layer 8 and a third metal layer 9 are laminated on a second metal layer 5, as shown in FIG. 1(G).
[0053] (Second insulating resin layer) The second insulating resin layer can be made of the same material as the core resin layer (e.g., prepreg). The thickness of the second insulating resin layer is not particularly limited because it is appropriately set according to the need, but can be, for example, 10 μm to 100 μm, preferably 10 μm to 50 μm, and more preferably 10 μm to 30 μm.
[0054] (Third metal layer) The third metal layer may be made of the same material as the first metal layer (e.g., copper foil). The thickness of the third metal layer is not particularly limited since it is appropriately set according to the desire, but may be, for example, 2 μm to 70 μm, preferably 2 μm to 18 μm, and more preferably 2 μm to 5 μm. The third metal layer may be, for example, an ultra-thin copper foil with a carrier. In this case, the third metal layer is disposed so that the copper foil or the like is in contact with the second insulating resin layer, and the carrier is peeled off after the second substrate is formed by heating and pressing.
[0055] (Lamination method and conditions) The method and conditions for laminating the second insulating resin layer and the third metal layer to obtain the second substrate are not particularly limited, but for example, the second substrate can be formed by laminating the second insulating resin layer and the third metal layer on the first substrate, and then performing vacuum pressing under conditions of a temperature of 220±2° C., a pressure of 5±0.2 MPa, and a holding time of 60 minutes. In addition, in order to obtain adhesion between the second metal layer and the second insulating resin layer, the surface of the second metal layer may be subjected to a roughening treatment.
[0056] [Second interlayer connection process (d)] The second interlayer connection step (d) is a step of forming a non-through hole on the surface of the second substrate, which reaches the surface of the second metal layer, and applying electrolytic copper plating and / or electroless copper plating to the inner wall of the non-through hole to connect the second metal layer and the third metal layer. Through the second interlayer connection step (d), as shown in FIG. 1(J), the second metal layer 5 and the third metal layer 9 are interlayer connected via the copper plating film 9A in the second substrate 7, and electrical conduction is ensured.
[0057] (Formation of non-through holes) In the second interlayer connection process (d), blind holes are formed on the surface of the first substrate, reaching the surface of the second metal layer. As shown in FIG. 1(H), blind holes 6B are provided on both sides of the second substrate 7. The means for forming the non-through holes is not particularly limited as described above, and for example, known means such as a laser such as a carbon dioxide gas laser or a drill can be used. The number and size of the non-through holes can be appropriately selected as desired. After the non-through holes are formed, a desmear treatment can be performed using an aqueous solution of sodium permanganate or the like.
[0058] (Interlayer connection) In the second interlayer connection step (d), after forming the non-through holes 6B, as shown in FIG. 1(I), electrolytic copper plating and / or electroless copper plating are performed to form a copper plating film 9A on the inner wall of the non-through hole, and the second metal layer 5 and the third metal layer 9 are electrically connected. At this time, the thickness of the third metal layer on both sides of the second substrate may be increased by the electrolytic copper plating and / or electroless copper plating, and the film thickness may be adjusted by film thickness adjustment described later. The method of performing electrolytic copper plating and / or electroless plating is not particularly limited, and a known method can be adopted. The copper plating may be either electrolytic copper plating or electroless plating, but it is preferable to perform both electrolytic copper plating and electroless plating.
[0059] (Film thickness adjustment) In the second interlayer connection process (d), as shown in FIG. 1(J), after the electrolytic / electroless copper plating process, if necessary, a known process such as an etching process can be carried out so that the third metal layer 9 has a desired thickness, thereby adjusting the film thickness. The thickness of the adjusted third metal layer is not particularly limited since it is appropriately set as desired, but can be, for example, 2 μm to 30 μm, preferably 2 μm to 20 μm, and more preferably 2 μm to 12 μm.
[0060] [Peeling process (e)] The peeling step (e) is a step of peeling off the third substrate having the first metal layer, the first insulating resin layer, the second metal layer, the second insulating resin layer, and the third metal layer in this order from the core resin layer. After the peeling step (e), as shown in FIG. 1(K), the second substrate 7 is separated at the interface between the core resin layer 2 and the first metal layer 3 arranged on both sides thereof, to obtain two third substrates 10 having the first metal layer 3, the first insulating resin layer 4, the second metal layer 5, the second insulating resin layer 8, and the third metal layer 9 in this order. The thickness of the third substrate is not particularly limited since it is appropriately set according to desire, but can be, for example, 5 μm to 400 μm, preferably 5 μm to 200 μm, and more preferably 5 μm to 100 μm.
[0061] In the peeling step (e), it is preferable that the core resin layer is peeled off at the interface between the core resin layer and the first metal layer, but for example, when the first metal layer has a peeling layer, a part of it may be peeled off together with the core resin layer. Also included is an embodiment in which the core resin layer is peeled off together with the peeling layer at the interface between the peeling layer of the first metal layer and the copper foil. When the peeling layer remains on the first metal layer, for example, the peeling layer can be removed using a sulfuric acid-based or hydrogen peroxide-based etching solution. The sulfuric acid-based or hydrogen peroxide-based etching solution is not particularly limited, and one used in the industry can be used.
[0062] [Wiring conductor formation process (f)] The wiring conductor forming step (f) is a step of forming the wiring conductor by patterning the first metal layer and the third metal layer of the third substrate. Through the wiring conductor forming step (f), a package substrate 13 for mounting a semiconductor element can be obtained in which wiring conductors 12 are formed on both sides of an insulating layer 11, as shown in FIG. 1(L). The insulating layer 11 is composed of a first insulating resin layer 4 and a second insulating resin layer 8, and the wiring conductor 12 is formed by interlayer connection of the first metal layer 3, the second metal layer 5, and the third metal layer 9, which are patterned, respectively, by electrolytic copper plating and / or electroless copper plating.
[0063] (Patterning) In the wiring conductor forming process (f), after the first metal layer 3 and the third metal layer 9 (see FIG. 1(K)) are surface-treated as necessary, a dry film resist or the like is laminated, and a negative mask is then attached, after which a circuit pattern is printed using an exposure machine, and the dry film resist is developed using a developer to form an etching resist. Thereafter, an etching process is performed, and copper in the areas without the etching resist is removed using an aqueous ferric chloride solution or the like, and the resist is then removed, whereby the wiring conductors 12 can be formed on both sides of the insulating layer 11.
[0064] Other interlayer connection methods that can be applied in this embodiment include a method in which chemical copper plating is applied to a known laser-formed blind via portion (a method in which a wiring circuit is formed by laser processing, and then patterning and interlayer connection are performed by chemical copper plating), a method in which a metal bump (preferably a copper bump) formed in advance by plating or etching a metal foil is used to pierce the insulating layer to perform interlayer connection, and a method in which a metal paste containing solder or a metal filler such as silver or copper in an insulating resin is bump-printed at predetermined locations by screen printing or the like, the paste is hardened by drying, and electrical conductivity between the inner and outer layers is ensured by heating and pressurization.
[0065] 1, which illustrates the present embodiment, the package substrate 13 for mounting a semiconductor element is a package substrate for mounting a semiconductor element having a three-layer structure, but the present invention is not limited thereto, and a package substrate for mounting a semiconductor element having a further build-up structure such as a five-layer structure can be formed. For example, in the wiring conductor forming step (f), after the wiring conductor is formed, an insulating resin layer and a metal layer are further laminated, and patterning and interlayer connection are repeatedly performed, thereby making it possible to manufacture a package substrate for mounting a semiconductor element having a build-up structure.
[0066] <<Method of manufacturing a package substrate for mounting semiconductor elements>> In the method for manufacturing a package substrate for mounting a semiconductor element of this embodiment, after the package substrate for a semiconductor element is formed as described above, a semiconductor element such as a bare chip can be mounted thereon as desired.
[0067] The semiconductor element is not particularly limited and a desired element can be used as appropriate. For example, a bare chip having gold bumps formed on aluminum electrodes by ball bonding of gold wires can be used. The semiconductor element can be mounted on the wiring conductor of the package substrate for mounting the semiconductor element via a bonding material. The bonding material is not particularly limited as long as it has a conductive means, and for example, solder (for example, solder balls, solder paste, etc.) can be used. In addition, after surface treatment is performed on the wiring conductor of the package substrate for mounting the semiconductor element, the semiconductor element can be mounted via the bonding material. The surface treatment is not particularly limited, and examples include the formation of a nickel layer or a gold plating layer. When solder is used as the bonding material, a process such as reflow can be performed after mounting the semiconductor element on the wiring conductor. At this time, the reflow temperature is appropriately selected depending on the melting point of the bonding material, and can be, for example, 260°C or higher.
[0068] In the above, an example has been described in which each layer is provided on both sides of the core resin layer, but the present invention is not limited to this, and each layer may be provided on only one side of the core resin layer. EXAMPLES
[0069] The production method of the present invention will now be described in detail with reference to examples.
[0070] [Example 1] A prepreg (core resin layer 2 in Fig. 1(A); thickness 0.100 mm: manufactured by Mitsubishi Gas Chemical Company, product name: GHPL-830NS ST56) made by impregnating bismaleimide triazine resin (BT resin) into glass cloth (glass fiber) to bring it to the B stage was placed on both sides of the prepreg, and a copper foil with a release layer (first metal layer 3 in Fig. 1(A); manufactured by JX Nippon Mining & Metals Corporation, product name: PCS), which was a copper foil with a thickness of 8 μm and a release layer applied thereto, was placed so that the release layer surface was adhered to the prepreg. A vacuum press was performed at a temperature of 220 ± 2°C, a pressure of 5 ± 0.2 MPa, and a holding time of 60 minutes to produce a copper-clad laminate with copper foil having a surface roughness of 3 μm.
[0071] <First substrate forming step (a)> A 2μm copper foil with an 18μm carrier copper foil (second metal layer 5 in FIG. 1(A); manufactured by Mitsui Mining & Smelting Co., Ltd., product name: MTEx) was laminated on both sides of the obtained copper-clad laminate via a prepreg (first insulating resin layer 4 in FIG. 1(A); thickness 0.017 mm: manufactured by Mitsubishi Gas Chemical Co., Ltd., product name: GHPL-830NS SF62) in which bismaleimide triazine resin (BT resin) was impregnated into glass cloth (glass fiber) to make it into the B stage) under conditions of a pressure of 2.5±0.2MPa, a temperature of 220±2°C, and a holding time of 60 minutes, after which the 18μm carrier copper foil was peeled off to produce a first substrate (circuit-forming substrate (first substrate) 1 in FIG. 1(B)).
[0072] <First interlayer connection process (b)> Next, a carbon dioxide gas laser processing machine (manufactured by Hitachi Via Mechanics, Ltd., product name: LC-1C / 21) was used to process one hole at a time on both sides of the first substrate under conditions of a beam irradiation diameter of Φ0.21 mm, a frequency of 500 Hz, and a pulse width of 10 μs, to form a non-through hole (non-through hole 6A in FIG. 1(C)) on both sides of the first substrate. Next, a desmear treatment was performed using a sodium permanganate aqueous solution having a concentration of 55±10 g / L at a temperature of 80±5° C. Further, electroless copper plating was performed to a thickness of 0.4 to 0.8 μm, and then electrolytic copper plating was performed to a thickness of 8 μm to form a copper plating film (copper plating film 5A in FIG. 1(D)). As a result, the first and second metal layers were electrically connected by non-through holes via the copper plating film. Next, the surface of the first substrate was smoothed, and a dry film resist (manufactured by Nichigo-Morton Co., Ltd., product name: NIT225) was laminated at a temperature of 110±10° C. and a pressure of 0.50±0.02 MPa. Thereafter, a negative mask was attached, and a circuit pattern was baked using a parallel exposure machine, and the dry film resist was developed with a 1% sodium carbonate aqueous solution to form an etching resist, and the copper in the portion without the etching resist was removed with a ferric chloride aqueous solution, and then the dry film resist was removed with a sodium hydroxide aqueous solution, and a pattern was formed on the second metal layer 5 (see FIG. 1(F)).
[0073] <Second substrate forming step (c)> Next, the surface of the patterned second metal layer was roughened using a copper surface roughening solution (manufactured by MEC Co., Ltd., product name: CZ-8100), and a B-stage resin sheet (thickness 0.010 mm: manufactured by Mitsubishi Gas Chemical Co., Ltd., product name: CRS-381NSI) coated with 2 μm copper foil with 18 μm carrier copper foil (manufactured by Mitsui Mining & Smelting Co., Ltd., product name: MTEx) was laminated on the surface of the second metal layer provided on both sides of the first substrate using a vacuum press under conditions of a pressure of 2.5 ± 0.2 MPa, a temperature of 220 ± 2 ° C, and a holding time of 60 minutes, after which the 18 μm carrier copper foil was peeled off to produce a second substrate (second substrate 7 in FIG. 1 (G)).
[0074] <Second Interlayer Connection Process (d)> A carbon dioxide gas laser processing machine (manufactured by Hitachi Via Mechanics, product name: LC-1C / 21) was used to process one hole at a time on both sides of the second substrate under conditions of a beam irradiation diameter of Φ0.21 mm, a frequency of 500 Hz, and a pulse width of 10 μs, to form a non-through hole (non-through hole 6B in FIG. 1(H)) on both sides of the second substrate. Next, a desmear treatment was performed using a sodium permanganate aqueous solution having a concentration of 55±10 g / L at a temperature of 80±5°C. Further, electroless copper plating was performed to a thickness of 0.4 to 0.8 μm, and then electrolytic copper plating was performed to a thickness of 8 μm to form a copper plating film (copper plating film 9A in FIG. 1(I)). As a result, the second and third metal layers were electrically connected by the blind holes via the copper plating film.
[0075] <Peeling process (e)> In the second substrate, physical force was applied to the boundary between the copper foil with a release layer (first metal layer 3) and the prepreg (core resin layer 2) to separate them, thereby obtaining a third substrate (third substrate 10 in Figure 1 (K)).
[0076] <Wiring conductor formation process (f)> After forming guide holes in the third substrate using a router processing machine manufactured by Hitachi Via Mechanics Co., Ltd., the surface was etched to about 1 to 2 μm using a soft etching solution based on sulfuric acid peroxide, and a dry film resist (manufactured by Nichigo-Morton Co., Ltd., product name: NIT225) was laminated at a temperature of 110 ± 10 ° C. and a pressure of 0.50 ± 0.02 MPa. The circuit pattern was baked using a parallel exposure machine based on the guide holes, and then the dry film resist was developed using a 1% sodium carbonate aqueous solution, and a pattern of about 15 to 20 μm of electrolytic copper plating was performed using a copper sulfate plating line with a copper sulfate concentration of 60 to 80 g / L and a sulfuric acid concentration of 150 to 200 g / L. Thereafter, the dry film resist was peeled off and removed using an amine-based resist stripping solution, and a pattern was formed on the third metal layer, to produce a package substrate for mounting a semiconductor element (a package substrate for mounting a semiconductor element 13 in which wiring conductors 12 are formed on both sides of the insulating layer 11 in FIG. 1 (L)).
[0077] The obtained package substrate for mounting a semiconductor element was subjected to a solder resist forming process and a gold plating finish, and then cut to a package size to obtain a package substrate for mounting a semiconductor element of Example 1. The package substrate for mounting a semiconductor element of Example 1 was easy to handle, and had a yield of 99% when produced multiple times.
[0078] [Example 2] In the first substrate forming step (a) of Example 1, a package substrate for mounting a semiconductor element of Example 2 was obtained in the same manner, except that a first substrate (substrate for forming a circuit (first substrate) 1 in FIG. 1(B)) was produced as follows.
[0079] A prepreg (core resin layer 2 in FIG. 1(A); thickness 0.08 mm: manufactured by Mitsubishi Gas Chemical Company, product name: GHPL-830NS SH65) made by impregnating bismaleimide triazine resin (BT resin) into glass cloth (glass fiber) to make it into the B stage) was placed on both sides of a copper foil with a release layer (first metal layer 3 in FIG. 1(A); manufactured by JX Nippon Mining & Metals Corporation, product name: PCS, surface roughness Rz 3.7 μm) in which a release layer was applied to a copper foil thickness of 8 μm, so that the release layer surface was bonded to the prepreg. Further on top of that, a prepreg (first insulating resin layer 4 in FIG. 1(A); thickness 0.017 mm: manufactured by Mitsubishi Gas Chemical Company, product name: GHPL-830NS A 2 μm copper foil with an 18 μm carrier copper foil (second metal layer 5 in FIG. 1(A); Mitsui Mining & Smelting Co., Ltd., product name: MTEx) was laminated via a 18 μm carrier copper foil (SF62) in a vacuum press under conditions of a pressure of 2.5±0.2 MPa, a temperature of 220±2°C, and a holding time of 60 minutes. The 18 μm carrier copper foil was then peeled off to produce a second circuit board, and a first board (a board for forming a circuit (first board) 1 in FIG. 1(B)).
[0080] The package substrate for mounting a semiconductor element of Example 2 was excellent in handleability, and the yield rate when produced multiple times was 99%.
[0081] [Comparative Example 1] A prepreg (core resin layer: thickness 0.100 mm: manufactured by Mitsubishi Gas Chemical Company, product name: GHPL-830NS ST56) made by impregnating bismaleimide triazine resin (BT resin) into glass cloth (glass fiber) to bring it to the B stage was placed on both sides of the prepreg, and copper foil (manufactured by JX Nippon Mining & Metals Corporation, product name: PCS) with a copper foil thickness of 2 μm and a release layer applied thereto was placed so that the release layer surface was adhered to the prepreg. Vacuum pressing was then performed under conditions of a temperature of 220±2°C, a pressure of 5±0.2 MPa, and a holding time of 60 minutes to produce a copper-clad laminate with copper foil surface roughness of 3 μm.
[0082] On both sides of the obtained copper-clad laminate, a 12 μm copper foil (manufactured by Mitsui Mining & Smelting Co., Ltd., product name: 3LC-VLP) was laminated via a prepreg (thickness: 0.017 mm: manufactured by Mitsubishi Gas Chemical Company, product name: GHPL-830NS SF62) made by impregnating bismaleimide triazine resin (BT resin) into glass cloth (glass fiber) to bring it to the B stage, using a vacuum press under conditions of a pressure of 2.5 ± 0.2 MPa, a temperature of 220 ± 2°C, and a holding time of 60 minutes.
[0083] Next, the obtained substrate surface was subjected to a surface preparation treatment, and a dry film resist (manufactured by Nichigo-Morton Co., Ltd., product name: NIT225) was laminated at a temperature of 110±10°C and a pressure of 0.50±0.02MPa. After that, a negative mask was attached, and a circuit pattern was printed using a parallel exposure machine. The dry film resist was developed using a 1% aqueous solution of sodium carbonate to form an etching resist. The copper in the areas without the etching resist was removed using an aqueous solution of ferric chloride, and then the dry film resist was removed using an aqueous solution of sodium hydroxide to form a circuit pattern.
[0084] The surface of the obtained substrate was roughened using a copper surface roughening solution (manufactured by MEC Co., Ltd., product name: CZ-8100), and a B-stage resin sheet (thickness 0.010 mm: manufactured by Mitsubishi Gas Chemical Co., Ltd., product name: CRS-381NSI) in which bismaleimide triazine resin (BT resin) was applied to a 2 μm copper foil with an 18 μm carrier copper foil (manufactured by Mitsui Mining & Smelting Co., Ltd., product name: MTEx) was laminated on both sides of the substrate using a vacuum press under conditions of a pressure of 2.5 ± 0.2 MPa, a temperature of 220 ± 2°C, and a holding time of 60 minutes, after which the 18 μm carrier copper foil was peeled off.
[0085] For the obtained substrate, a physical force was applied to the boundary between the core resin layer and the PCS to separate them.
[0086] A carbon dioxide laser processing machine (manufactured by Hitachi Via Mechanics, Ltd., product name: LC-1C / 21) was used to process one hole at a time on both sides of the substrate that had been peeled off from the core resin layer under conditions of a beam irradiation diameter of Φ0.21 mm, a frequency of 500 Hz, and a pulse width of 10 μs in an attempt to form blind holes in the substrate, but the substrate was very thin and was damaged.
[0087] The disclosure of Japanese Patent Application No. 2018-234584, filed on December 14, 2018, is incorporated herein by reference in its entirety. In addition, all publications, patent applications, and technical standards mentioned in the specification are herein incorporated by reference to the same extent as if each individual publication, patent application, and technical standard was specifically and individually indicated to be incorporated by reference. [Explanation of symbols]
[0088] 1 Circuit forming substrate (first substrate), 2 Core resin layer, 3 First metal layer, 4 First insulating resin layer, 5 Second metal layer, 5A, 9A Copper plating film, 6A, 6B Non-penetrating hole, 7 Second substrate, 8 Second insulating resin layer, 9 Third metal layer, 10 Third substrate, 11 Insulating layer, 12 Wiring conductor, 13 Package substrate for mounting semiconductor element
Claims
1. A method for manufacturing a package substrate for mounting a semiconductor element, the method comprising the steps of: a first substrate forming step (a) of forming a first substrate on one or both sides of a core resin layer, the first substrate having a first metal layer having a thickness of 1 μm to 70 μm and capable of being peeled off from the core resin layer, a first insulating resin layer, and a second metal layer in this order; a first interlayer connection step (b) of forming non-through holes on the surface of the first substrate, the non-through holes reaching the surface of the first metal layer, and applying electrolytic copper plating and / or electroless copper plating to the inner walls of the non-through holes to connect the second metal layer and the first metal layer; a second substrate forming step (c) of forming a second substrate by heating and pressurizing a laminate formed by arranging a second insulating resin layer and a third metal layer in this order on a surface of the second metal layer of the first substrate; a second interlayer connection step (d) of forming non-through holes on the surface of the second substrate, the non-through holes reaching the surface of the second metal layer, and applying electrolytic copper plating and / or electroless copper plating to the inner walls of the non-through holes to connect the second metal layer and the third metal layer; a peeling step (e) of peeling a third substrate having the first metal layer, the first insulating resin layer, the second metal layer, the second insulating resin layer, and the third metal layer in this order from the core resin layer; a wiring conductor forming step (f) of patterning the first metal layer and the third metal layer of the third substrate to form the wiring conductor; Including, The first substrate forming step (a) includes forming a laminate in which the first metal layer, the first insulating resin layer, and the second metal layer are disposed in this order on both sides of the core resin layer, and heating and pressing the laminate together to form a first substrate; The thickness of the core resin layer is 1 μm to 90 μm, The second interlayer connection step (d) includes a step of adjusting a thickness of the third metal layer on both sides of the second substrate. A method for manufacturing a package substrate for mounting a semiconductor element.
2. 2. The method for manufacturing a package substrate for mounting a semiconductor element according to claim 1, wherein the third substrate has a thickness of 5 μm to 100 μm.
3. 3. The method for manufacturing a package substrate for mounting a semiconductor element according to claim 1, wherein the first metal layer has a peel-off layer, and the first substrate is arranged such that the peel-off layer is in contact with the core resin layer.
4. The method for manufacturing a package substrate for mounting a semiconductor element according to any one of claims 1 to 3, wherein the third metal layer has a carrier layer, and after the first substrate is heated and pressurized in the second substrate formation process (c), the carrier layer is removed from the third metal layer.
5. 5. The method for manufacturing a package substrate for mounting a semiconductor element according to claim 1, wherein at least one of the first metal layer, the second metal layer, and the third metal layer is a copper foil.
6. The method for manufacturing a package substrate for mounting a semiconductor element according to any one of claims 1 to 5, wherein at least one of the core resin layer, the first insulating resin layer, and the second insulating resin layer is a prepreg having a base material impregnated with a resin.
Citation Information
Patent Citations
Substrate for supporting circuit formation, and substrate for packaging semiconductor element and its manufacturing method
JP2005101137A
Manufacturing method of wiring board
JP2007335700A
Multilayer wiring board, and method of manufacturing the same
JP2011119722A
Supporting substrate for circuit formation, and method of manufacturing package substrate for mounting semiconductor element