Blow molding die, metal plate, method for producing composite container, and composite container

The blow molding mold with a metal plate enhances the appearance and functional properties of plastic containers by forming an uneven structure on the outer surface, addressing limitations in conventional methods.

JP7584007B2Active Publication Date: 2024-11-15DAI NIPPON PRINTING CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2020122242
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-07-16
Publication Date
2024-11-15
Estimated Expiration
2040-07-16

AI Technical Summary

Technical Problem

Conventional biaxial stretch blow molding methods are limited in imparting various functions and properties to containers, such as barrier properties and heat retention, and struggle to enhance the appearance and design of plastic bottles by varying these properties across different parts of the container.

Method used

A blow molding mold with a metal plate attached to the mold body, featuring a surface shape that forms an uneven structure on the container's outer surface, allowing for the creation of a composite container with a plastic member that replicates this structure, enhancing the container's appearance and design.

Benefits of technology

The method improves the appearance and design of plastic containers by forming an uneven structure on the outer surface, which can enhance functions like light shielding and heat retention, while maintaining recyclability and durability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007584007000001
    Figure 0007584007000001
  • Figure 0007584007000002
    Figure 0007584007000002
  • Figure 0007584007000003
    Figure 0007584007000003
Patent Text Reader

Abstract

To provide a blow molding mold capable of improving an appearance of a container and improving the design, a metal plate, a method for manufacturing a composite container, and a composite container.SOLUTION: A blow molding mold 50 comprises: a mold body 52; and a metal plate 60 that is attached to the mold body 52 and has a surface shape for forming an uneven structure 21 on the outer surface of a container 10A.SELECTED DRAWING: Figure 11
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a blow molding die, a metal plate, a method for manufacturing a composite container, and a composite container. [Background technology]

[0002] 2. Description of the Related Art Recently, bottles for containing liquid contents such as food and beverages have become common, and such plastic bottles contain liquid contents.

[0003] Such plastic bottles for containing liquid contents are manufactured by inserting a preform into a mold and subjecting it to biaxial stretch blow molding.

[0004] Incidentally, in conventional biaxial stretch blow molding methods, a preform containing a single-layer material, a multilayer material, or a blended material, such as PET or PP, is used to mold the container into a shape. However, in conventional biaxial stretch blow molding methods, it is common to simply mold the preform into a container shape. For this reason, when imparting various functions or characteristics (barrier properties, heat retention, etc.) to the container, the means for doing so are limited, for example by changing the material constituting the preform. In particular, it is difficult to impart different functions or characteristics depending on the parts of the container (for example, the body and the bottom).

[0005] In response to this, the present applicant has proposed in Patent Document 1 a composite container that can be endowed with various functions and properties. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] JP 2015-128858 A

[0007] On the other hand, when producing such containers, there is a demand for improving the appearance of the containers and improving the design. Summary of the Invention [Problem to be solved by the invention]

[0008] The present invention has been made in consideration of these points, and aims to provide a blow molding mold, a metal plate, a manufacturing method for a composite container, and a composite container that can improve the appearance of the container and enhance its design. [Means for solving the problem]

[0009] A blow molding mold according to one embodiment is a blow molding mold for producing a container, comprising a mold body and a metal plate attached to the mold body and having a surface shape for forming a concave-convex structure on the outer surface of the container.

[0010] In one embodiment of a blow molding mold, the mold body may be provided with a recess extending outward from its inner surface, the metal plate may be attached within the recess, and the surface of the metal plate may be recessed outward from the inner surface.

[0011] In one embodiment of the blow mould, the mould body and the metal plate may be made of different materials.

[0012] In one embodiment of the blow mould, the mould body may comprise aluminium and the metal plate may comprise nickel.

[0013] In one embodiment of the blow molding die, the metal plate may be made by electroforming.

[0014] In one embodiment of the blow molding die, the metal plate may have a thickness of 0.03 mm or more and 0.20 mm or less.

[0015] In one embodiment of the blow molding die, the rear surface of the metal plate may have a linear shape in a cross section along the vertical direction.

[0016] In the blow molding die according to one embodiment, the metal plate may be removably attached to the die body.

[0017] In one embodiment of the blow molding die, the metal plate may be attached to the die body by double-sided tape.

[0018] In one embodiment of the blow mould, the metal plate may be attached to the mould body by magnetic force.

[0019] The blow mold according to one embodiment may be a biaxially stretched blow mold.

[0020] In one embodiment of the blow molding die, the container is a composite container having a container body and a plastic member provided in close contact with the outside of the container body, and the uneven structure may be formed on the outer surface of the plastic member.

[0021] The blow mold according to one embodiment may be a direct blow mold or an injection blow mold.

[0022] The metal plate according to one embodiment is a metal plate that is attached to a blow molding mold for producing a container, has a surface shape for forming a concave-convex structure on the outer surface of the container, and is produced by electroforming.

[0023] The metal plate according to one embodiment may include nickel.

[0024] In the metal plate according to one embodiment, the metal plate may have a thickness of 0.03 mm or more and 0.20 mm or less.

[0025] In the metal plate according to one embodiment, the rear surface of the metal plate may be a flat surface.

[0026] A manufacturing method for a composite container according to one embodiment is a manufacturing method for a composite container comprising a container body and a plastic member provided in close contact with the outside of the container body, the manufacturing method for a composite container comprising the steps of: preparing a preform; providing the plastic member on the outside of the preform; preparing a blow molding mold according to one embodiment; and blow molding the preform and the plastic member in the blow molding mold, thereby expanding the preform and the plastic member as a unit, wherein in the step of expanding the preform and the plastic member as a unit, the surface shape of the metal plate attached to the mold body is transferred, and an uneven structure is formed on the outer surface of the plastic member after blow molding.

[0027] In one embodiment of a manufacturing method for a composite container, in the process of expanding the preform and the plastic member together, a convex portion protruding outward may be formed at a position on the container body corresponding to the metal plate.

[0028] In one embodiment of the manufacturing method for a composite container, the uneven structure may be located on the outer surface of the plastic member outside an outer surface of a region surrounding the uneven structure.

[0029] A composite container according to one embodiment comprises a container body and a plastic member provided in close contact with the outside of the container body, the container body being formed with a convex portion that protrudes outward, and an uneven structure being formed on the outer surface of the plastic member at a position corresponding to the convex portion.

[0030] In one embodiment of the composite container, the uneven structure may be located on the outer surface of the plastic member outside the outer surface of the area surrounding the uneven structure. Effect of the Invention

[0031] According to the present disclosure, the appearance of the container can be improved and the design can be enhanced. [Brief description of the drawings]

[0032] [Figure 1] FIG. 1 is a partial vertical sectional view showing a composite container according to one embodiment. [Diagram 2] FIG. 2 is a horizontal cross-sectional view (cross-sectional view taken along line II-II in FIG. 1) showing a composite container according to one embodiment. [Diagram 3] FIG. 3 is a cross-sectional view showing a composite container according to one embodiment (a cross-sectional view corresponding to part III in FIG. 1). [Figure 4A] FIG. 4A is a perspective view showing a composite container according to one embodiment, in which the relief structure is a reflective hologram structure. [Figure 4B] FIG. 4B is a perspective view showing a composite container according to an embodiment, in which the relief structure is a transmission type hologram structure. [Diagram 5] FIG. 5 is a cross-sectional view (corresponding to the V portion in FIG. 2) showing the concave-convex structure of the composite container according to one embodiment. [Figure 6] FIG. 6 is a schematic plan view showing the planar structure of the concave-convex structure in the state where the plastic member is unfolded. [Figure 7] FIG. 7 is a cross-sectional view showing an element having a concave-convex structure (a cross-sectional view taken along line VII-VII in FIG. 6). [Figure 8] FIG. 8 is a partial vertical cross-sectional view showing a composite preform according to one embodiment. [Figure 9] FIG. 9 is a horizontal cross-sectional view (cross-sectional view taken along line IX-IX in FIG. 8) showing a composite preform according to one embodiment. [Figure 10] 10(a)-(d) are perspective views showing various plastic members. [Figure 11] FIG. 11 is a cross-sectional view showing a blow molding die according to one embodiment. [Figure 12] FIG. 12 is a cross-sectional view showing a blow molding die according to one embodiment (a cross-sectional view corresponding to part XII in FIG. 11). [Figure 13]FIG. 13 is a cross-sectional view showing a metal plate according to an embodiment. [Figure 14] 14(a)-(c) are schematic diagrams showing a method for manufacturing a metal plate according to one embodiment. [Figure 15] 15(a)-(f) are schematic diagrams showing a method for manufacturing a composite container according to one embodiment. [Figure 16] FIG. 16 is a perspective view showing a first modified example of the composite container according to one embodiment. [Figure 17] FIG. 17 is a cross-sectional view showing a first modified example of the blow molding die according to one embodiment. [Figure 18] FIG. 18 is a perspective view showing a second modified example of the composite container according to the embodiment. [Figure 19] FIG. 19 is a cross-sectional view showing a second modified example of the blow molding die according to one embodiment. [Figure 20] FIG. 20 is a schematic plan view showing the planar structure of the concave-convex structure in a state in which the plastic member is developed in a fourth modified example of the composite container according to one embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0033] An embodiment will be described below with reference to the drawings. FIGS. 1 to 15 are diagrams showing an embodiment. Each of the figures shown below is a schematic diagram. Therefore, the size and shape of each part are appropriately exaggerated to facilitate understanding. In addition, it is possible to carry out appropriate modifications within the scope of the technical idea. In each of the figures shown below, the same parts are given the same reference numerals, and some detailed explanations may be omitted. In addition, the numerical values ​​such as the dimensions of each member and the material names described in this specification are examples of an embodiment, and are not limited to these, and can be appropriately selected and used. In this specification, terms that specify shapes and geometric conditions, such as parallel, orthogonal, and vertical, are intended to include substantially the same state in addition to their strict meanings.

[0034] Composite container structure First, an outline of the composite container according to the present embodiment will be described with reference to Figs. In this specification, "upper" and "lower" refer to the upper and lower sides, respectively, of the composite container 10A when it is held upright (FIG. 1).

[0035] The composite container 10A shown in Figures 1 and 2 is obtained by performing biaxial stretch blow molding on a composite preform 70 (see Figures 8 and 9) including a preform 10a and a plastic member 40a using a blow molding mold 50, as described below, to expand the preform 10a and the plastic member 40a of the composite preform 70 as a single unit.

[0036] Such a composite container 10A comprises a container body 10 made of a plastic material located on the inside, and a plastic member 40 provided in close contact with the outside of the container body 10. In this specification, the "inside" refers to the side located closer to the inside of the container, and the "outside" refers to the side located closer to the outside of the container.

[0037] Of these, the container body 10 comprises a mouth 11, a neck 13 provided below the mouth 11, a shoulder 12 provided below the neck 13, a body 20 provided below the shoulder 12, and a bottom 30 provided below the body 20.

[0038] On the other hand, the plastic member 40 is thinly stretched and adhered closely to the outer surface of the container body 10, and is attached in a state in which it does not easily move or rotate relative to the container body 10.

[0039] Next, a detailed description will be given of the container body 10. The container body 10 has the mouth portion 11, the neck portion 13, the shoulder portion 12, the body portion 20, and the bottom portion 30 as described above.

[0040] Of these, the mouth portion 11 has a threaded portion 14 that is screwed onto a cap (not shown), and a flange portion 17 provided below the threaded portion 14. The shape of the mouth portion 11 may be a conventionally known shape. The container body 10 is filled with contents such as a liquid content, and a cap (not shown) is screwed onto the mouth portion 11, thereby producing a composite container containing the contents.

[0041] Neck 13 is located between flange 17 and shoulder 12, and has a generally cylindrical shape with a generally uniform diameter. Shoulder 12 is located between neck 13 and body 20, and has a shape whose diameter gradually increases from the neck 13 side toward the body 20 side (a shape whose area gradually increases in horizontal cross section).

[0042] The body portion 20 has a cylindrical shape with a generally uniform diameter as a whole, except for a region where a convex portion 25 described below is formed. However, this is not limited thereto, and the body portion 20 may have a polygonal cylindrical shape such as a rectangular cylindrical shape or an octagonal cylindrical shape. Alternatively, the body portion 20 may have a cylindrical shape with a non-uniform horizontal cross section from top to bottom.

[0043] A protrusion 25 that protrudes outward (diametrically outward) is formed on this body portion 20. In this embodiment, the protrusion 25 is formed around the entire circumference of the body portion 20, and is formed in approximately the center in the up-down direction of the body portion 20. Note that the body portion 20 may have irregularities other than the protrusion 25, such as vacuum absorption panels or grooves.

[0044] On the other hand, the bottom 30 has a recessed portion 31 located in the center and a grounding portion 32 provided around the recessed portion 31. The shape of the bottom 30 is not particularly limited, and may have a conventionally known bottom shape (for example, a petaloid bottom shape, a rounded bottom shape, etc.).

[0045] The thickness of the container body 10 at the trunk 20 can be, for example, thinned to about 50 μm or more and 250 μm or less, but is not limited thereto. Furthermore, the weight of the container body 10 can be, for example, thinned to about 10 g or more and 20 g or less, but is not limited thereto. By thinning the thickness of the container body 10 in this way, the weight of the container body 10 can be reduced.

[0046] Such a container body 10 can be produced by biaxially stretching and blow molding a preform 10a (described later) produced by injection molding a synthetic resin material. The material of the container body 10 is preferably a thermoplastic resin, particularly PE (polyethylene), PP (polypropylene), PET (polyethylene terephthalate), PEN (polyethylene naphthalate), or PC (polycarbonate). The container body 10 may be colored in colors such as red, blue, yellow, green, brown, black, and white, but is preferably colorless and transparent in consideration of ease of recycling. In addition, the above-mentioned various resins may be blended and used. Furthermore, a vapor deposition film such as a diamond-like carbon film or a silicon oxide thin film may be formed on the inner surface of the container body 10 in order to improve the barrier property of the container.

[0047] The container body 10 can also be formed as a multi-layered bottle having two or more layers. That is, by injection molding, a preform 10a having three or more layers is injection molded with an intermediate layer being a resin having gas barrier properties (intermediate layer) such as MXD6, MXD6+fatty acid salt, PGA (polyglycolic acid), EVOH (ethylene vinyl alcohol copolymer), or PEN (polyethylene naphthalate), and then blow molded to form a multi-layered bottle having gas barrier properties. Note that the intermediate layer may be a resin obtained by blending the various resins described above.

[0048] Alternatively, a foamed preform having a foam cell diameter of 0.5 μm or more and 100 μm or less may be molded by mixing an inert gas (nitrogen gas, argon gas) with a melt of a thermoplastic resin, and the foamed preform may be blow molded to produce the container body 10. Since such a container body 10 has foam cells built-in, the light-shielding property of the entire container body 10 can be improved.

[0049] The container body 10 may be a bottle having a full capacity of, for example, 100 ml to 2000 ml, or a large bottle having a full capacity of, for example, 10 L to 60 L.

[0050] Next, a description will be given of the plastic member 40. As will be described later, the plastic member 40 (40a) is provided so as to surround the outside of the preform 10a, and is obtained by being closely attached to the outside of the preform 10a and then being biaxially stretch-blow molded together with the preform 10a.

[0051] The plastic member 40 is attached to the outer surface of the container body 10 without being glued, and is in close contact with the container body 10 so that it does not move or rotate relative to the container body 10. This plastic member 40 is thinly stretched on the outer surface of the container body 10 to cover the container body 10. As shown in Fig. 2, the plastic member 40 is provided over the entire circumferential direction of the container body 10 so as to surround it, and has a horizontal cross section that is approximately circular.

[0052] In this case, the plastic member 40 is provided so as to cover the neck portion 13, shoulder portion 12, body portion 20, and bottom portion 30 of the container body 10, excluding the mouth portion 11. This makes it possible to impart desired functions and characteristics to the neck portion 13, shoulder portion 12, body portion 20, and bottom portion 30 of the container body 10.

[0053] The plastic member 40 may be provided on the entire or partial area of ​​the container body 10 except for the mouth 11. For example, the plastic member 40 may be provided so as to cover the entire shoulder 12, body 20, and bottom 30 of the container body 10, excluding the mouth 11 and neck 13. Alternatively, the plastic member 40 may be provided so as to cover the shoulder 12, body 20, and bottom 30 of the container body 10, excluding the mouth 11, neck 13, and the central portion of the bottom 30.

[0054] Since the plastic member 40 is not welded or bonded to the container body 10, it can be peeled off and removed from the container body 10. Specifically, for example, the plastic member 40 can be cut off using a blade or the like, or a cutting line (not shown) can be provided in advance on the plastic member 40, and the plastic member 40 can be peeled off along this cutting line. This allows the plastic member 40 to be separated and removed from the container body 10.

[0055] Such a plastic member 40 may be one that does not have a shrinking effect relative to the preform 10a, or may be one that has a shrinking effect.

[0056] When the plastic member 40 has the ability to shrink relative to the preform 10a, the plastic member 40 is provided on the outside of the preform 10a, and is obtained by being heated together with the preform 10a and being biaxially stretched and blow molded.

[0057] Examples of the plastic member 40 include polyethylene, polypropylene, polyethylene terephthalate, polyethylene naphthalate, poly-4-methylpentene-1, polystyrene, AS resin, ABS resin, polyvinyl chloride, polyvinylidene chloride, polyvinyl acetate, polyvinyl alcohol, polyvinyl acetal, polyvinyl butyral, diallyl phthalate resin, fluorine-based resin, polymethyl methacrylate, polyacrylic acid, polymethyl acrylate, polyacrylonitrile, polyacrylamide, polybutadiene, polybutene-1, polyisoprene, polychloroprene, ethylene propylene rubber, butyl rubber, nitrile rubber, etc. Examples of the resin include rubber, acrylic rubber, silicone rubber, fluororubber, nylon 6, nylon 6,6, aromatic polyamide, polycarbonate, polyethylene terephthalate ethylene, polyethylene butylene terephthalate, polynaphthalene ethylene, U polymer, liquid crystal polymer, modified polyphenylene ether, polyether ketone, polyether ether ketone, unsaturated polyester, alkyd resin, polyimide, polysulfone, polyphenylene sulfide, polyether sulfone, silicone resin, polyurethane, phenolic resin, urea resin, polyethylene oxide, polypropylene oxide, polyacetal, and epoxy resin. Among these, it is preferable to use thermoplastic non-elastic resins such as polyethylene (PE) such as low-density polyethylene (LDPE), polypropylene (PP), polyethylene terephthalate (PET), and polyethylene naphthalate (PEN). In addition, blends, multilayer structures, and partial multilayer structures of these may be used. Furthermore, various additives may be added to the material of the plastic member 40 in addition to the resin as the main component, as long as the characteristics are not impaired. Examples of additives that can be added include plasticizers, UV stabilizers, coloring inhibitors, matting agents, deodorants, flame retardants, weather resistance agents, antistatic agents, thread friction reducers, slip agents, mold release agents, antioxidants, ion exchange agents, and color pigments. Also, by mixing an inert gas (nitrogen gas, argon gas) into the molten thermoplastic resin, a foamed material having a foam cell diameter of 0.5 μm or more and 100 μm or less is used, and this foamed preform is molded, thereby improving the light blocking property.

[0058] The plastic member 40 may be made of a material having a light barrier property that blocks invisible light such as ultraviolet light. In this case, the light barrier property of the composite container 10A can be improved and the liquid contained therein can be prevented from being deteriorated by ultraviolet light or the like without using a multi-layer preform or a preform containing a blended material as the preform 10a. Such a material may be a blended material, or a material in which a light-shielding resin is added to PET, PE, or PP. A foamed member having a foam cell diameter of 0.5 μm or more and 100 μm or less, which is produced by mixing an inert gas (nitrogen gas, argon gas) with a melt of a thermoplastic resin, may also be used.

[0059] The plastic member 40 may be made of a material (material with low thermal conductivity) with higher cold insulation or heat insulation than the plastic material constituting the container body 10 (preform 10a). In this case, it is possible to make it difficult for the temperature of the content liquid to be transmitted to the surface of the composite container 10A without increasing the thickness of the container body 10 itself. This improves the cold insulation or heat insulation of the composite container 10A. In addition, when a user grasps the composite container 10A, it is prevented that the composite container 10A becomes difficult to hold due to being too cold or too hot. Such materials include foamed polyurethane, polystyrene, PE (polyethylene), PP (polypropylene), phenolic resin, polyvinyl chloride, urea resin, silicone, polyimide, melamine resin, etc. It is preferable to mix hollow particles into a resin material containing these resins. The average particle diameter of the hollow particles is preferably 1 μm or more and 200 μm or less, and more preferably 5 μm or more and 80 μm or less. The term "average particle size" means the volume average particle size, and can be measured by a known method using a particle size distribution / particle size distribution measuring device (for example, Nanotrack particle size distribution measuring device, manufactured by Nikkiso Co., Ltd.). The hollow particles may be organic hollow particles made of resin or inorganic hollow particles made of glass, but organic hollow particles are preferred because of their excellent dispersibility. Examples of resins constituting organic hollow particles include styrene resins such as crosslinked styrene-acrylic resins, (meth)acrylic resins such as acrylonitrile-acrylic resins, phenolic resins, fluorine resins, polyamide resins, polyimide resins, polycarbonate resins, and polyether resins. In addition, commercially available hollow particles such as Ropeake HP-1055, Ropeake HP-91, Ropeake OP-84J, Ropeake Ultra, Ropeake SE, and Ropeake ST (manufactured by Rohm and Haas Co., Ltd.), Nipol MH-5055 (manufactured by Zeon Corporation), SX8782, and SX866 (manufactured by JSR Corporation) can also be used.The content of the hollow particles is preferably 0.01 parts by mass or more and 50 parts by mass or less, and more preferably 1 part by mass or more and 20 parts by mass or less, relative to 100 parts by mass of the resin material contained in the plastic member 40.

[0060] The plastic member 40 may be made of a material that is less slippery than the plastic material constituting the container body 10 (preform 10a). In this case, the user can easily grip the composite container 10A without changing the material of the container body 10.

[0061] The plastic member 40 may be colored in a color such as red, blue, yellow, green, brown, black, or white, and may be transparent or opaque.

[0062] Furthermore, the thickness of the plastic member 40 is not limited to this, but can be, for example, about 5 μm or more and 500 μm or less when attached to the container body 10.

[0063] In the present embodiment, an uneven structure 21 (shaded portion in FIG. 1) is formed on the outer surface of the plastic member 40. In the present embodiment, the uneven structure 21 is formed on a part of the outer surface of the plastic member 40 located in the trunk portion 20 of the container body 10. The shape of this uneven structure 21 is a shape transferred from the surface shape of a metal plate 60 of a blow molding die 50 that molds the composite container 10A, as described below.

[0064] The uneven structure 21 is formed at a position corresponding to the convex portion 25 formed on the trunk portion 20 of the container body 10. In this embodiment, the uneven structure 21 is formed on the entire outer surface of the plastic member 40 corresponding to the convex portion 25. As shown in FIG. 3, the uneven structure 21 is located outside the outer surface of the plastic member 40 in the region surrounding the uneven structure 21. In this case, the protrusion amount L1 of the uneven structure 21 (the radial distance from the outer surface of the region surrounding the uneven structure 21 on the outer surface of the plastic member 40 to the uneven structure 21) may be, for example, 0.05 mm or more and 1.00 mm or less. When the protrusion amount L1 is 0.05 mm or more, it is possible to prevent the plastic member 40a described later from being caught on the side surface 63 of the metal plate 60 when blow molding is performed using the blow molding die 50, as described later. When the protrusion amount L1 is 1.00 mm or less, it is possible to improve the moldability of the container body 10.

[0065] In this embodiment, the concave-convex structure 21 is configured to reproduce the optical image 102 (see FIG. 4A and FIG. 4B) by modulating the phase of the incident light. In this case, the concave-convex structure 21 is configured by a phase modulation type hologram structure that modulates the phase of the incident reproduction light to reproduce the optical image 102, and in particular includes an element element 22, described later, that is configured by a Fourier transform hologram. A Fourier transform hologram is a hologram produced by recording wavefront information of a Fourier transform image of an original image, and functions as a so-called Fourier transform lens. In particular, a phase modulation type Fourier transform hologram is a hologram having a concave-convex shape produced by multi-valuing the phase information of a Fourier transform image and recording it as depth in a medium, and reproduces the optical image 102 of the original image from the reproduction light by utilizing the diffraction phenomenon based on the optical path length difference of the medium. This Fourier transform hologram is advantageous in that, for example, the desired optical image 102 (i.e., the original image) can be reproduced with high accuracy, while being relatively easy to produce. Such a phase modulation type hologram is also called a kinoform. However, the element elements 22 of the concave-convex structure 21 are not limited to Fourier transform holograms, and may have a hologram or other structure that reconstructs the optical image 102 by other methods.

[0066] In the following description, white light containing various wavelengths is given as an example of the reconstructed light incident on the concave-convex structure 21, but the reconstructed light does not necessarily have to be white light. In other words, the wavelength contained in the reconstructed light is not particularly limited as long as it contains light of a wavelength corresponding to the color of the light image 102 reconstructed by the concave-convex structure 21. Furthermore, in the following description, the specific value of the refractive index is based on light with a wavelength of 589.3 nm, unless otherwise specified. Furthermore, in the following description, the characteristic values ​​of the refractive index and concave-convex shape shown for the hologram structure (convex-convex structure) 21 are values ​​derived assuming that the composite container 10A is used in an air environment with a refractive index of 1.0, unless otherwise specified.

[0067] The concave-convex structure 21 can be classified into a reflection type hologram structure in which the observer 100 and the light source 101 are arranged on the same side of the concave-convex structure 21 as shown in FIG. 4A, and a transmission type hologram structure in which the observer 100 and the light source 101 are arranged on different sides of the concave-convex structure 21 as shown in FIG. 4B. As the reflection type hologram structure, for example, in addition to a structure in which an additional layer for reflecting the reproduced light is provided on the plastic member 40, there is a structure in which the concave-convex shape of the element element 22 described later is exposed to air without providing an additional reflection layer, and the reproduced light is reflected by utilizing the difference in refractive index between the plastic member 40 and the air. On the other hand, the transmission type hologram structure does not have such a reflection layer. These reflection type hologram structures and transmission type hologram structures have in common that the desired light image 102 is reproduced by the diffraction phenomenon caused by the optical path length difference of the concave-convex shape of the element element 22. Note that, regarding the specific concave-convex depth of the concave-convex shape of the element element 22, there is an optimal value for each of the transmission type hologram structure and the reflection type hologram structure. In the following, the contents described only with respect to either the reflection type hologram structure or the transmission type hologram structure can basically be applied to both the reflection type hologram structure and the transmission type hologram structure, unless otherwise specified.

[0068] In this embodiment, the outer surface of the region of the outer surface of the container body 10 that is covered by the uneven structure 21 has a curved shape. Specifically, the uneven structure 21 is provided so as to cover a part of the body 20 of the container body 10, which has a cylindrical shape with a substantially uniform diameter as a whole. In this case, when the container body 10 is filled with the contents, the light irradiated from the point light source and incident on the composite container 10A spreads in an elliptical shape between the container body 10 and the contents due to the lens effect, and the light source cannot be considered as a point light source. As a result, when the uneven structure 21 is a transmission type hologram structure, when the container body 10 is filled with the contents, the uneven structure 21 does not reproduce the light image 102. On the other hand, when the container body 10 is not filled with the contents, the light irradiated from the point light source is incident on the uneven structure 21 without being affected by the lens effect, and the uneven structure 21 reproduces the light image 102.

[0069] 5 and 6, the concave-convex structure 21 has element elements (also called "hologram cells") 22 including a concave-convex shape. The concave-convex structure 21 of this embodiment includes a plurality of element elements 22, which are regularly arranged two-dimensionally. Each element element 22 has a planar size of several μm to several mm square (for example, 2 mm square), and reconstructs the optical image 102 by modulating the phase of the incident reconstruction light.

[0070] In this embodiment, the element element 22 is a Fourier transform hologram. That is, the element element 22 is a hologram created by Fourier transforming the original image 102a (see FIG. 6) to be reproduced. The concave-convex shape of this element element 22 has a concave-convex pattern corresponding to the Fourier transform image of the original image, and has a concave-convex depth corresponding to each pixel of the Fourier transform image. When forming the concave-convex structure 21 having such element elements 22, for example, when performing blow molding using a blow molding die 50, the concave-convex structure 21 can be formed by transferring the surface shape of a die body 52 to the outer surface of a plastic member 40.

[0071] Furthermore, the size and shape of each element element 22 in a plan view are not particularly limited, and each element element 22 may have any size and shape. For example, the shape of each element element 22 in a plan view may be a quadrangle such as a square, a rectangle, or a trapezoid, another polygonal shape (e.g., a triangle, a pentagon, a hexagon, etc.), a perfect circle, an ellipse, another circle, a star shape, a heart shape, etc., and the concavo-convex structure 21 may have element elements 22 with two or more types of shapes in a plan view.

[0072] Here, since the uneven structure 21 includes the element elements 22 including an uneven shape, the design of the composite container 10A can be improved without using ink that deteriorates due to ultraviolet rays or the like. As a result, the design can be maintained for a long period of time compared to, for example, a case in which printing is performed on the outer surface of the plastic member 40. Furthermore, in the composite container 10A according to this embodiment, the plastic member 40 may be separated and removed from the container body 10, and the colorless and transparent container body 10 may be recycled. On the other hand, in this embodiment, the uneven structure 21 can improve the design of the composite container 10A without adding a pigment or dye to the plastic member 40, and therefore the recyclability of the container body 10 can be improved.

[0073] Moreover, the uneven structure 21 according to the present embodiment uses the element elements 22 including the uneven shape to modulate the phase of the incident reconstructed light to reconstruct the light image 102. In this case, since it is difficult to produce similar products, the reliability of the product can be improved, and the cosmetic properties of the composite container 10A can be improved.

[0074] When light from a point light source (e.g., an LED light source) is incident on such a concave-convex structure 21, an optical image 102 (i.e., an original image (the character "OK" in the example shown in FIG. 4A and FIG. 4B)) according to the concave-convex pattern of the concave-convex shape is reproduced. This type of concave-convex structure 21 does not require a screen or the like for projecting the optical image 102, and reproduces the optical image 102 particularly well when light is incident from the light source 101, which is a point light source. For this reason, the concave-convex structure 21 can be used for entertainment purposes and design purposes, such as reproducing a character image, and can improve the design of the composite container 10A. In addition, since it is difficult to produce a similar product as described above, the concave-convex structure 21 can be conveniently and widely used for security purposes such as authenticity determination or other purposes. The optical image that can be reproduced by such a concave-convex structure 21 is not particularly limited, and in addition to characters, for example, symbols, line drawings, designs, patterns, and combinations thereof can be used as the original image and the reproducible optical image.

[0075] Next, the uneven shape of the element element 22 will be described. As shown in Fig. 7, the uneven shape of the element element 22 has a multi-step shape (i.e., a step shape with two or more steps). Fig. 7 is a cross-sectional view of the element element 22 showing an outline of the step structure of the uneven shape, and Fig. 7 shows a four-step type uneven shape. Note that the number of steps of the uneven shape is not particularly limited. Also, as shown in Fig. 7, the uneven shape has a random step shape according to the reproduced optical image 102 (i.e., the original image).

[0076] When the optical image 102 is reproduced by a plurality of colors, the concave-convex shape of the element element 22 preferably has three or more steps, and in particular, a concave-convex shape having four or more steps allows an original image having a complex composition to be reproduced with high resolution. The pitch P1 (i.e., pixel pitch) of the concave-convex pattern of the concave-convex shape of the element element 22 is preferably 0.38 μm or more and 500 μm or less, and more preferably 0.5 μm or more and 100 μm or less. When the pitch P1 of the concave-convex shape is 0.38 μm or more, the shapeability during blow molding can be improved and high diffraction efficiency can be exhibited in the visible range. Furthermore, when the pitch P1 of the concave-convex shape is 500 μm or less, the optical image 102 can be reproduced with high accuracy, and high diffraction efficiency can be exhibited in the visible range, allowing an image of a size that is easy to view to be reproduced. In this specification, the "pitch of the uneven shape of the element" refers to the pitch (the distance between adjacent topmost portions 220) measured in the unfolded state of the plastic member 40 after peeling it off from the container body 10, and refers to the average value of five pitches measured by selecting different topmost portions 220.

[0077] When the concave-convex structure 21 is a reflective type, the depth d per step of the concave-convex shape is preferably 10 nm or more and 10 μm or less, and more preferably 20 nm or more and 8 μm or less. When the depth d is 10 nm or more, the shapeability during blow molding can be improved and high diffraction efficiency can be exhibited in the visible range. When the depth d is 10 μm or less, the optical image 102 can be reproduced with high accuracy and high diffraction efficiency can be exhibited in the visible range. When the concave-convex structure 21 is a transmissive type, the depth d is preferably 60 nm or more and 60 μm or less, and more preferably 120 nm or more and 48 μm or less. When the depth d is 60 nm or more, the shapeability during blow molding can be improved and high diffraction efficiency can be exhibited in the visible range. When the depth d is 60 μm or less, the optical image 102 can be reproduced with high accuracy and high diffraction efficiency can be exhibited in the visible range.

[0078] As an example, in the transmissive uneven structure 21, when the refractive index of the plastic member 40 is 1.5, the uneven shape has a four-step depth structure, and the depth d per step is 660 nm, the uneven structure 21 reproduces a blue light image 102. Note that the color (wavelength band) of the light image 102 reproduced by the transmissive uneven structure 21 is assumed to be used in an air environment with a refractive index of 1.0.

[0079] Furthermore, when the observer 100 observes the light image 102 reproduced by the reflective uneven structure 21, the reflected image from the uneven structure 21 observed by the observer 100 is composed of light reflected by the uneven shape formed on the surface without passing through the plastic member 40. In such a case, it is necessary to set the depth d per step of the uneven shape based on the optical path length based on the refractive index of the medium closer to the observer 100 than the plastic member 40, for example, the refractive index of air (1.0), rather than the refractive index of the plastic member 40. Therefore, by designing the uneven shape structure while assuming that the refractive index of the plastic member 40 is the refractive index of air (1.0), the observer 100 can observe a desired image. Specifically, when the refractive index of air is 1.0 and the depth d per step of the uneven shape is 165 nm, the optical path length per step of the uneven shape is 330 nm. In this case, since the uneven shape has a four-step depth structure, the uneven structure 21 exhibits maximum diffraction efficiency in the blue wavelength band, and reproduces a blue optical image 102.

[0080] Composite preform composition Next, the structure of the composite preform will be described with reference to Figs.

[0081] As shown in Figs. 8 and 9, the composite preform 70 includes a preform 10a made of a plastic material, and a bottomed cylindrical plastic member 40a provided on the outside of the preform 10a.

[0082] The preform 10a includes a mouth portion 11a, a body portion 20a connected to the mouth portion 11a, and a bottom portion 30a connected to the body portion 20a. The mouth portion 11a corresponds to the mouth portion 11 of the container body 10 described above, and has substantially the same shape as the mouth portion 11. The body portion 20a corresponds to the neck portion 13, shoulder portion 12, and body portion 20 of the container body 10 described above, and has a substantially cylindrical shape. The bottom portion 30a corresponds to the bottom portion 30 of the container body 10 described above, and has a substantially hemispherical shape.

[0083] The plastic member 40a is attached to the outer surface of the preform 10a without being bonded, and is in close contact with the preform 10a so as not to move or rotate relative to the preform 10a, or to such an extent that it will not fall under its own weight. The plastic member 40a is provided over the entire circumferential area so as to surround the preform 10a, and has a circular horizontal cross section.

[0084] In this case, the plastic member 40a is provided so as to cover the entire body portion 20a and the entire bottom portion 30a.

[0085] The plastic member 40a may be provided on the entire area other than the mouth portion 11a or on a part of the area. Alternatively, the plastic member 40a may be provided so as to cover the body portion 20a except for the bottom portion 30.

[0086] Such a plastic member 40a may be one that does not have a shrinking effect relative to the preform 10a, or may be one that has a shrinking effect.

[0087] When the plastic member 40a has a shrinking function, the plastic member 40a may be one that shrinks (e.g., thermally shrinks) relative to the preform 10a when an external action (e.g., heat) is applied to it. Alternatively, the plastic member 40a may be one that itself has shrinkability or elasticity and can shrink without the application of an external action.

[0088] In addition, if the plastic member 40a has a thermal shrinkage function, after the cylindrical plastic member 40a is fitted into the preform 10a, the margin formed at the lower end portion (the end portion opposite the mouth portion 11a) of the plastic member 40a may be thermally compressed.

[0089] Examples of the plastic member 40a that can be used include a direct blow tube produced by direct blow molding, a sheet molded tube produced by sheet molding, an extrusion tube produced by extrusion molding, an injection molded tube produced by injection molding, and an inflation molded tube produced by inflation molding, but the plastic member 40a is not limited to these and molding methods other than those mentioned above may also be used.

[0090] The plastic member 40a may be colored in a color such as red, blue, yellow, green, brown, black, or white, and may be transparent or opaque.

[0091] Next, the shape of the plastic member 40a will be described.

[0092] As shown in FIG. 10(a), the plastic member 40a may be formed in a cylindrical shape with a bottom as a whole, and may have a cylindrical body 41 and a bottom 42 connected to the body 41. In this case, the bottom 42 of the plastic member 40a covers the bottom 30a of the preform 10a, so that various functions and characteristics such as barrier properties can be imparted to the bottom 30 as well as the body 20 of the composite container 10A. The plastic member 40a may also be formed in a cylindrical shape with no seams around the entire circumference. Examples of such a plastic member 40a include the above-mentioned direct blow tube, sheet molding tube, and injection molding tube.

[0093] 10(b), the plastic member 40a may be formed in a circular tube shape (bottomless cylindrical shape) as a whole, and may have a cylindrical body 41. The plastic member 40a may be formed in a cylindrical shape without joints along the entire circumference. In this case, the plastic member 40a may be, for example, the above-mentioned blow tube, extrusion tube, inflation molding tube, or sheet molding tube.

[0094] 10(c) and 10(d), the plastic member 40a may be produced by forming a film into a cylindrical shape and bonding the ends together. In this case, the plastic member 40a may be configured in a tubular shape (bottomless cylindrical shape) having a body 41 as shown in Fig. 10(c), or may be configured in a bottomed cylindrical shape by bonding a bottom 42 together as shown in Fig. 10(d).

[0095] Blow mold configuration Next, the configuration of the blow molding die 50 according to this embodiment will be described with reference to Figures 11 and 12. This blow molding die 50 is for producing a composite container (container) 10A, and is a biaxially stretched blow molding die.

[0096] As shown in FIG. 11, the blow molding mold 50 comprises a mold body 52 which is a metal or resin mold, and a metal plate 60 attached to the mold body 52 and having a surface shape for forming a concave-convex structure 21 on the outer surface of the composite container 10A (i.e., the outer surface of the plastic member 40).

[0097] Of these, the mold body 52 is composed of a pair of body dies 50a, 50b, which are separated from each other, and a bottom die 50c. The inner surface of the mold body 52 has a shape corresponding to the shoulder 12, neck 13, body 20, and bottom 30 of the container body 10. Meanwhile, the metal plate 60 is provided at a position of the mold body 52 corresponding to the uneven structure 21. In addition, in Fig. 11, the regions of the inner surface 52a of the mold body 52 that correspond to the neck 13, shoulder 12, and body 20 of the container body 10 are indicated by corresponding symbols using virtual lines (two-dot chain lines).

[0098] As shown in Figs. 11 and 12, the mold body 52 is provided with a recess 55 recessed outward from the inner surface 52a. The recess 55 is provided at a position corresponding to the protrusion 25 of the trunk 20 of the container body 10. The metal plate 60 is attached in the recess 55. As shown in Fig. 12, the surface 61 of the metal plate 60 is recessed outward from the inner surface 52a. That is, the entire metal plate 60 is accommodated in the recess 55. In this way, since the surface 61 of the metal plate 60 is recessed outward from the inner surface 52a, it is possible to prevent the expanding plastic member 40a from getting caught on the side surface 63 of the metal plate 60 when blow molding is performed using the blow molding mold 50. In Figs. 11 and 12, the inner surface 52a of the mold body 52 when the recess 55 is not formed is shown by a virtual line (two-dot chain line).

[0099] In this case, the recession amount (radial distance) L2 of the surface 61 of the metal plate 60 from the inner surface 52a of the mold body 52 may be, for example, 0.05 mm or more and 1.00 mm or less. When the recession amount L2 is 0.05 mm or more, it is possible to prevent the plastic member 40a described below from getting caught on the side surface 63 of the metal plate 60 when performing blow molding using the blow molding mold 50, as will be described later. Furthermore, when the recession amount L2 is 1.00 mm or less, it is possible to improve the moldability of the container body 10.

[0100] In addition, in a cross section along the vertical direction, the back surface 62 of the metal plate 60 may have a linear shape. In this case, as described later, the back surface 62 of the metal plate 60 is a flat surface. This makes it possible to easily attach the metal plate 60 to the mold body 52.

[0101] In this embodiment, it is preferable that the metal plate 60 is detachably attached to the mold body 52. ​​In this case, by removing the metal plate 60 from the mold body 52, it is possible to return the mold body 52 to the state before the metal plate 60 was attached. In this case, it is also possible to attach a metal plate 60 having a different surface shape to the mold body 52 again.

[0102] In this embodiment, the metal plate 60 is attached to the mold body 52 by a double-sided tape 65. In this case, the metal plate 60 can be removed from the mold body 52 by manual or mechanical work. Even if an adhesive layer (not shown) of the double-sided tape 65 remains on the mold body 52, it can be removed by cleaning with water or alcohol. As the double-sided tape 65, for example, No. 5000NS manufactured by Nitto Denko Corporation can be used.

[0103] Such a mold body 52 and metal plate 60 may be made of different materials. In this case, the metal plate 60 may be made of a material harder than the material of the mold body 52. ​​This makes it possible to suppress deformation of the concave and convex shape of a surface shape portion 64 (described later) of the metal plate 60 during blow molding, thereby improving the durability of the metal plate 60. For example, the mold body 52 may contain aluminum, and the metal plate 60 may contain nickel.

[0104] metal plate Next, the metal plate 60 attached to the above-mentioned blow molding die 50 will be described in detail with reference to FIG.

[0105] 13, a surface shape portion 64 for forming the concave-convex structure 21 on the outer surface of the plastic member 40 is provided on a surface 61 of a metal plate 60. The surface shape portion 64 has a concave-convex shape corresponding to the concave-convex shape of the element elements 22 of the concave-convex structure 21.

[0106] The metal plate 60 is produced by electroforming. This allows the concave-convex shape of the surface shape portion 64 to be produced with high precision, and also allows a plurality of metal plates 60 having the same concave-convex shape to be produced easily. In this case, it is preferable that the metal plate 60 contains nickel.

[0107] The thickness T of the metal plate 60 is preferably 0.03 mm or more and 0.20 mm or less, and more preferably 0.04 mm or more and 0.17 mm or less. When the thickness T of the metal plate 60 is 0.03 mm or more, the durability of the metal plate 60 can be improved, and when the metal plate 60 is produced by electroforming, the formability of the metal plate 60 can be improved. When the thickness T of the metal plate 60 is 0.20 mm or less, the attachment property of the metal plate 60 when attached to the blow molding die 50 can be improved. That is, as described above, the inner surface of the die body 52 of the blow molding die 50 has a shape corresponding to the trunk part 20 of the container body 10, and the inner surface of the die body 52 may have a curved shape. In this case, the inner surface of the recess 55 to which the metal plate 60 is attached may also have a curved shape. Therefore, when the thickness T of the metal plate 60 is 0.20 mm or less, the metal plate 60 can be easily bent to match the curved shape, and the attachment property when attached to the blow molding die 50 can be improved.

[0108] The back surface 62 of the metal plate 60 is a flat surface. In other words, no dents visible to the naked eye or curved portions with a predetermined radius of curvature are formed on the back surface 62 of the metal plate 60. Since the back surface 62 of the metal plate 60 is a flat surface, the metal plate 60 can be easily attached to the mold body 52.

[0109] Next, the operation of this embodiment will be described below. First, a method for manufacturing the metal plate 60 of the blow molding die 50 for producing the composite container 10A will be described, and then a method for manufacturing the composite container 10A will be described.

[0110] Metal plate manufacturing method First, a method for manufacturing a metal plate 60 according to the present embodiment will be described with reference to FIGS. 14(a) to 14(c).

[0111] When producing the metal plate 60, first, as shown in FIG. 14(a), a matrix 60a is prepared on which concave and convex portions 64a (see FIG. 14(a)) corresponding to the surface shape portion 64 of the metal plate 60 are formed.

[0112] In this case, first, a two-dimensional image of an original image reproduced by the concave-convex structure 21 formed on the outer surface of the plastic member 40 is read by a computer (Step 1).

[0113] Next, the computer obtains a two-dimensional complex amplitude image by taking each pixel value of the read two-dimensional image as an amplitude value and assigning a random value between 0 and 2π to each pixel as a phase value (Step 2).

[0114] Next, the computer performs a two-dimensional Fourier transform on this two-dimensional complex amplitude image to obtain a two-dimensional Fourier transform image (Step 3). Note that the computer may perform any optimization process, such as an iterative Fourier transform method or a genetic algorithm, as necessary (Step 4).

[0115] Next, the computer discretizes the phase value of each pixel in the two-dimensional Fourier transform image into multiple levels (for example, four levels: "0", "π / 2", "π", and "3π / 2", or eight levels: "0", "π / 4", "π / 2", "3π / 4", "π", "5π / 4", "3π / 2", and "7π / 4") (Step 5).

[0116] Then, a matrix 60a is fabricated in which concave-convex portions 64a (particularly concave-convex shapes) corresponding to the two-dimensional Fourier transform image are formed so that each pixel has a depth according to the corresponding discretized phase value (Step 6). For example, if the pixel values ​​of the two-dimensional Fourier transform image are discretized into four stages in Step 5 described above, a concave-convex shape having four stages of depth (see FIG. 7) is formed in the matrix 60a in Step 6.

[0117] The depth of the uneven shape is determined by a computer, taking into consideration not only the diffraction efficiency characteristics to be realized but also various other related parameters (for example, the refractive index of the material constituting the plastic member 40). For example, when forming a reflective uneven structure 21 for reproducing a blue light image 102 on the plastic member 40, an uneven portion 64a having four steps of the uneven shape and an optical path length of 330 nm per step can be created. Note that the reflective uneven structure 21 and the transmissive uneven structure 21 each have a unique uneven shape depth structure, and even when trying to realize similar diffraction characteristics, for example, the specific value of the depth of the uneven shape of the uneven structure 21 differs between the reflective type and the transmissive type. For this reason, the specific value of the depth of the uneven shape of the uneven portion 64a formed on the matrix 60a also differs between the reflective type and the transmissive type.

[0118] The manufacturing device for the master die 60a is not particularly limited, and may be, for example, a device controlled by a computer that executes the above-mentioned Steps 1 to 5, or may be a device provided separately from the computer.

[0119] In this manner, a mother die 60a having projections and recesses 64a formed therein is obtained.

[0120] Next, the matrix 60a is immersed in a plating tank filled with a plating solution. As a result, as shown in FIG. 14(b), metal is deposited on the matrix 60a, and a metal plate 60 having a surface feature 64 is produced. At this time, by appropriately adjusting the plating process conditions (current, processing time, etc.), The thickness T of the metal plate 60 can be set to a desired thickness.

[0121] 14(c), the metal plate 60 is peeled off from the matrix 60a, thus obtaining the metal plate 60.

[0122] The components of the plating solution used are appropriately determined depending on the properties required for the metal plate 60. For example, a solution containing nickel can be used as the plating solution. The plating solution may also contain various additives.

[0123] Manufacturing method of composite container Next, a manufacturing method (blow molding method) for the composite container 10A according to this embodiment will be described with reference to FIGS. 15(a)-(f).

[0124] First, a preform 10a made of a plastic material is prepared (see FIG. 15(a)). In this case, the preform 10a may be produced by injection molding using, for example, an injection molding machine (not shown). Alternatively, a preform that is generally used in the past may be used as the preform 10a.

[0125] Next, a plastic member 40a is provided on the outside of the preform 10a to produce a composite preform 70 having the preform 10a and the plastic member 40a attached to the outside of the preform 10a (see FIG. 15(b)). In this case, the plastic member 40a has a bottomed cylindrical shape as a whole, and has a cylindrical body 41 and a bottom 42 connected to the body 41.

[0126] At this time, a plastic member 40a having an inner diameter equal to or slightly smaller than the outer diameter of the preform 10a may be pressed into the preform 10a to be brought into close contact with the outer surface of the preform 10a. Alternatively, as described below, a heat-shrinkable plastic member 40a may be provided on the outer surface of the preform 10a, and the plastic member 40a may be heated to 50°C to 100°C to cause heat shrinkage and bring the plastic member 40a into close contact with the outer surface of the preform 10a.

[0127] In this way, by first adhering plastic member 40a to the outside of preform 10a to produce composite preform 70, it becomes possible to carry out the series of steps for producing composite preform 70 (Figures 15(a)-(b)) and the series of steps for producing composite container 10A by blow molding (Figures 15(c)-(f)) in separate locations (factories, etc.).

[0128] Next, the composite preform 70 is heated by the heating device 51 (see FIG. 15(c)). At this time, the composite preform 70 is heated uniformly in the circumferential direction by the heating device 51 while rotating with the mouth portion 11a facing downward. The heating temperature of the preform 10a and the plastic member 40a in this heating process may be, for example, 90°C to 130°C.

[0129] Also, the blow molding die 50 is prepared. Then, the composite preform 70 heated by the heating device 51 is sent to the blow molding die 50 for producing the composite container 10A (see FIG. 15(d)).

[0130] The composite container 10A is molded using this blow molding die 50. In the blow molding die 50, the metal plate 60 is attached in a recess 55 (see FIG. 12) provided in a pair of body dies 50a, 50b, and is provided at a position corresponding to the above-mentioned concave-convex structure 21.

[0131] 15(d), the pair of body dies 50a, 50b are open from each other, and the bottom die 50c is raised upward. In this state, the composite preform 70 is inserted between the pair of body dies 50a, 50b of the die main body 52.

[0132] 15(e), the pair of body dies 50a, 50b are closed after the bottom die 50c is lowered, and a sealed blow molding die 50 is formed by the pair of body dies 50a, 50b and the bottom die 50c of the die body 52. ​​Next, air is forced into the preform 10a, and the composite preform 70 is subjected to biaxial stretch blow molding.

[0133] As a result, the composite preform 70 is shaped into a shape corresponding to the inner surface of the blow molding die 50, and the container body 10 is obtained from the preform 10a in the blow molding die 50. At this time, since the surface 61 (see FIG. 12) of the metal plate 60 of the blow molding die 50 is recessed outward from the inner surface 52a (see FIG. 12), a convex portion 25 protruding outward is formed in the body 20 of the container body 10 (see FIG. 3). During this time, the body dies 50a and 50b are heated to 30°C to 80°C, and the bottom die 50c is cooled to 5°C to 25°C. In addition, in the blow molding die 50, the surface shape of the metal plate 60 attached to the blow molding die 50 (die body 52) is transferred, and the uneven structure 21 is formed on the outer surface of the plastic member 40 after blow molding. At this time, in the blow molding die 50, the preform 10a of the composite preform 70 and the plastic member 40a are expanded as a unit. As a result, the preform 10a and the plastic member 40a are integrally shaped into a shape that corresponds to the inner surface of the blow molding die 50.

[0134] In this manner, a composite container 10A including the container body 10 and the plastic member 40 provided on the outer surface of the container body 10 is obtained.

[0135] 15(f), the pair of body dies 50a, 50b and the bottom die 50c of the die body 52 are separated from each other, and the composite container 10A is removed from the blow molding die 50. In this manner, the composite container 10A shown in Figs. 1 and 2 is obtained.

[0136] As described above, according to this embodiment, the blow molding die 50 includes the die body 52 and the metal plate 60 attached to the die body 52 and having a surface shape for forming the uneven structure 21 on the outer surface of the plastic member 40 of the composite container 10A. As a result, the surface shape of the metal plate 60 attached to the die body 52 is transferred to the outer surface of the plastic member 40, so that the uneven structure 21 having the uneven shape on the surface of the composite container 10A can be easily formed. Such an uneven structure 21 can be used for entertainment purposes such as reproducing character images and for design purposes, and can improve the design of the composite container 10A. In addition, since no ink that deteriorates due to ultraviolet rays or the like is used, the design can be maintained for a long period of time compared to, for example, when printing is performed on the outer surface of the plastic member 40. In addition, since the metal plate 60 can be attached to the existing die body 52, it is possible to impart various desired uneven shapes to the surface of the composite container 10A while maintaining the overall shape of the existing die body 52.

[0137] Furthermore, according to this embodiment, the mold body 52 is provided with a recess 55 recessed outward from the inner surface 52a, and the metal plate 60 is attached in the recess 55. Furthermore, the surface 61 of the metal plate 60 is recessed outward from the inner surface 52a of the mold body 52. ​​This makes it possible to prevent the expanding plastic member 40a from getting caught on the side surface 63 of the metal plate 60 when blow molding is performed using the blow molding mold 50. This makes it possible to prevent the expanding plastic member 40a from breaking.

[0138] Moreover, according to this embodiment, the mold body 52 and the metal plate 60 are made of different materials. In this case, the metal plate 60 may be made of a material harder than the material of the mold body 52. ​​This makes it possible to suppress deformation of the uneven shape of the surface shape portion 64 of the metal plate 60 during blow molding, thereby improving the durability of the metal plate 60.

[0139] Moreover, according to this embodiment, the die body 52 contains aluminum, and the metal plate 60 contains nickel. This can improve the workability of the die body 52. ​​Furthermore, deformation of the uneven shape of the surface shape portion 64 of the metal plate 60 during blow molding can be effectively suppressed, and the durability of the metal plate 60 can be effectively improved.

[0140] Moreover, according to this embodiment, the metal plate 60 is produced by electroforming. This makes it possible to produce the concave-convex shape of the surface shape portion 64 with high precision, and also makes it possible to easily produce a plurality of metal plates 60 having the same concave-convex shape.

[0141] Furthermore, according to this embodiment, the back surface 62 of the metal plate 60 attached to the mold body 52 has a linear shape in a cross section along the vertical direction. In this case, the back surface 62 of the metal plate 60 before being attached to the mold body 52 is a flat surface. This makes it possible to easily attach the metal plate 60 to the mold body 52.

[0142] Furthermore, according to this embodiment, the metal plate 60 is detachably attached to the mold body 52. ​​This allows the metal plate 60 attached to the mold body 52 to be easily peeled off and replaced with another metal plate 60. This allows the uneven shape of the surface of the composite container 10A to be easily changed in a short time. In this case, since there is no need to remanufacture the mold body 52 itself, the cost and time required for manufacturing the mold body 52 can be reduced.

[0143] Furthermore, according to this embodiment, the metal plate 60 is attached to the mold body 52 with double-sided tape 65. This makes it possible to easily attach and detach the metal plate 60 to and from the mold body 52.

[0144] Also, according to this embodiment, in the composite container 10A, the container body 10 is formed with a convex portion 25 that protrudes outward, and the uneven structure 21 is formed at a position on the outer surface of the plastic member 40 that corresponds to the convex portion 25. Even in this case, the mold body 52 for producing the composite container 10A is provided with a concave portion 55 that is recessed outward from the inner surface 52a, and the surface 61 of the metal plate 60 can be recessed outward from the inner surface 52a of the mold body 52. ​​This makes it possible to prevent the expanding plastic member 40a from getting caught on the side surface 63 of the metal plate 60 when blow molding is performed using the blow molding mold 50. This makes it possible to prevent the expanding plastic member 40a from breaking.

[0145] Furthermore, according to this embodiment, the concave-convex structure 21 is located outside the outer surface of the region surrounding the concave-convex structure 21 on the outer surface of the plastic member 40. Even in this case, the surface 61 of the metal plate 60 can be recessed outside the inner surface 52a of the mold body 52. ​​This makes it possible to prevent the expanding plastic member 40a from getting caught on the side surface 63 of the metal plate 60 when blow molding is performed using the blow molding mold 50, and thus makes it possible to prevent the expanding plastic member 40a from breaking.

[0146] Furthermore, according to the present embodiment, the composite container 10A is produced by blow molding using the blow molding die 50. At this time, the surface shape of the metal plate 60 is transferred to the outer surface of the plastic member 40. This makes it possible to easily form the uneven structure 21 on the surface of the composite container 10A.

[0147] Furthermore, according to this embodiment, since the plastic member 40 can be separated and removed from the container body 10, the colorless and transparent container body 10 can be recycled in the same manner as in the conventional case.

[0148] Furthermore, according to this embodiment, it is possible to use, as the plastic member 40, a material (e.g., polyethylene or polypropylene) that has better formability than the material (e.g., polyethylene terephthalate) of the container body 10. Therefore, the surface shape of the metal plate 60 can be transferred more clearly to the plastic member 40, compared to the case where the surface shape of the metal plate 60 is directly transferred to the container body 10. This allows a finer uneven shape (e.g., 3 μm or less) to appear on the surface of the plastic member 40.

[0149] Variations Next, modified examples of the composite container 10A and the blow molding die 50 according to the present embodiment will be described with reference to Figures 16 to 20. In Figures 16 to 20, the same parts as those in the embodiment shown in Figures 1 to 15 are designated by the same reference numerals and detailed description thereof will be omitted.

[0150] (First Modification) In the above embodiment, an example has been described in which the uneven structure 21 is formed on a part of the outer surface of the plastic member 40 located on the trunk 20 of the container body 10, but this is not limiting. For example, as shown in Fig. 16, the uneven structure 21 may be formed on the entire outer surface of the plastic member 40 located on the trunk 20 of the container body 10.

[0151] In this modification, the convex portion 25 is formed over the entire body portion 20. That is, the entire body portion 20 protrudes radially outward beyond the lower end 121 of the shoulder portion 12 and the upper end 301 of the bottom portion 30. The uneven structure 21 is formed over the entire outer surface of the plastic member 40 that corresponds to the convex portion 25.

[0152] In this case, as shown in Fig. 17, the recess 55 provided in the mold body 52 of the blow molding mold 50 is provided in a region corresponding to the entire trunk 20 of the container body 10. The recess 55 is recessed outward from the inner surface 52b of the mold body 52, which corresponds to the lower end 121 of the shoulder 12 of the container body 10, and the inner surface 52c of the inner surface 52a of the mold body 52, which corresponds to the upper end 301 of the bottom 30. The surface 61 of the metal plate 60 is recessed outward from the inner surfaces 52b and 52c. Even in this case, it is possible to prevent the expanding plastic member 40a from getting caught on the side surface 63 of the metal plate 60 when blow molding is performed using the blow molding mold 50.

[0153] (Second Modification) 18, the uneven structure 21 may be formed on a part of the outer surface of a plastic member 40 located on the shoulder portion 12 of the container body 10. As shown in FIG.

[0154] In this modification, the convex portion 25 that protrudes outward is formed on the shoulder portion 12. Moreover, the convex portion 25 is formed on a part of the shoulder portion 12 in the circumferential direction. In this modification, of the convex portion 25, at least a part of a connecting portion 251 that connects to the upper end 201 of the body portion 20 protrudes radially outward beyond the upper end 201 of the body portion 20. Moreover, the uneven structure 21 is formed on the entire outer surface of the plastic member 40 that corresponds to the convex portion 25. The convex portion 25 may be formed around the entire circumference of the shoulder portion 12.

[0155] 19, the recess 55 provided in the mold body 52 of the blow molding mold 50 is provided at a position corresponding to the protrusion 25 of the shoulder 12 of the container body 10. The recess 55 is recessed outward from an inner surface 52d of an inner surface 52a of the mold body 52 at a portion corresponding to the upper end 201 of the trunk 20 of the container body 10. The surface 61 of the metal plate 60 is recessed outward from the inner surface 52d. Even in this case, it is possible to prevent the expanding plastic member 40a from getting caught on the side surface 63 of the metal plate 60 when blow molding is performed using the blow molding mold 50.

[0156] (Third Modification) In the above embodiment, an example has been described in which the uneven structure 21 is formed on the entire outer surface of the plastic member 40 that corresponds to the convex portion 25, but this is not limiting. For example, although not shown, the uneven structure 21 may be formed on only a portion of the outer surface of the plastic member 40 that corresponds to the convex portion 25. In this case, the surface shape portion 64 of the metal plate 60 is provided on only a portion of the surface 61 of the metal plate 60, so that the uneven structure 21 can be formed on only a portion of the outer surface of the plastic member 40 that corresponds to the convex portion 25.

[0157] (Fourth Modification) Further, although an example in which the concave-convex structure 21 is composed of a plurality of element elements 22 has been described, each element element 22 can also reproduce the optical image 102 with a color having any gradation. In other words, the concave-convex structure 21 may include a plurality of types of element elements having different gradations. For example, as shown in FIG. 20, the concave-convex structure 21 may include a first element element 22a that reproduces a red optical image 102, a second element element 22b that reproduces a blue optical image 102, and a third element element 22c that reproduces a green optical image 102.

[0158] Also, when each element 22 is designed based on an original image having any gradation, it is possible to reproduce the optical image 102 in colors having any gradation. In these cases, the concave-convex structure 21 can also reproduce the full-color optical image 102 when white light is incident thereon.

[0159] In the concave-convex structure 21 shown in Fig. 20 described above, the types of element elements 22 arranged adjacently in both the vertical and horizontal directions are different from each other, but the arrangement of the multiple types of element elements 22 is not particularly limited. For example, the concave-convex structure 21 may include multiple types of element elements 22 arranged in a stripe pattern, and the types of element elements 22 arranged adjacently in one of the vertical and horizontal directions may be different, but the types of element elements 22 arranged adjacently in the other direction may be the same. Furthermore, the multiple types of element elements 22 may be arranged in an arrangement that combines a checkerboard arrangement and a stripe arrangement.

[0160] (Fifth Modification) In the above embodiment, the concave-convex structure 21 is configured from a plurality of element elements 22. However, the present invention is not limited to this. For example, although not shown, the concave-convex structure 21 may be configured from a single element element 22.

[0161] (Sixth Modification) In the above embodiment, the metal plate 60 is attached to the mold body 52 by the double-sided tape 65, but the present invention is not limited to this. For example, although not shown, the metal plate 60 may be attached to the mold body 52 by magnetic force. In this case, the metal plate 60 can be attached to and detached from the mold body 52 even more easily.

[0162] (Seventh Modification) In the above embodiment, the blow molding die 50 is a biaxially stretched blow molding die, but the present invention is not limited to this. For example, the blow molding die 50 may be a direct blow molding die or an injection blow molding die, although not shown in the drawings. Even in this case, the surface shape of the metal plate 60 attached to the die body 52 is transferred to the outer surface of the container, so that the uneven structure 21 having an uneven shape can be easily formed on the outer surface of the container. This can improve the design of the container.

[0163] (Eighth Modification) Furthermore, in the above embodiment, the container produced by the blow molding die 50 is the composite container 10A, but the present invention is not limited to this. For example, although not shown, the container produced by the blow molding die 50 may be a container manufactured by biaxial stretch blow molding, direct blow molding, or injection blow molding.

[0164] It is also possible to combine the multiple components disclosed in the above embodiment and each modification as necessary. Alternatively, some components may be deleted from all the components shown in the above embodiment and each modification. [Explanation of symbols]

[0165] 10 Container body 10A composite container 10a Preform 21 Uneven structure 25 Convex 40 Plastic parts 40a Plastic parts 50 Blow mold 52-inch body 52a Inside 52b Inside 52c Inside 52d Inside 55 Recess 60 metal plate 61 Surface 62 Back side 65 Double-sided tape

Claims

1. A blow mold for producing a container, comprising: A mold body; A metal plate attached to the mold body; the inner surface of the mold body defines a molding space having a shape corresponding to the container; The mold body is provided with a recess that is recessed from the inner surface toward the molding space, The metal plate is entirely contained within the recess, the metal plate has a surface facing the molding space and having a surface shape for forming a concave-convex structure on the outer surface of the container; A blow molding die, wherein the surface of the metal plate is recessed outwardly with respect to the molding space relative to the inner surface surrounding the recess.

2. The blow molding mold of claim 1 , wherein the mold body and the metal plate are made of different materials.

3. The blow mould according to claim 1 or 2, wherein the mould body comprises aluminium and the metal plate comprises nickel.

4. The blow molding die according to claim 1 , wherein the metal plate is produced by electroforming.

5. The blow molding die according to claim 1 , wherein the metal plate has a thickness of 0.03 mm or more and 0.20 mm or less.

6. The blow molding die according to claim 1 , wherein the rear surface of the metal plate has a linear shape in a cross section along the vertical direction.

7. The blow molding die according to claim 1 , wherein the metal plate is removably attached to the die body.

8. The blow molding die according to claim 1 , wherein the metal plate is attached to the die body by double-sided tape.

9. The blow mould according to claim 1 , wherein the metal plate is attached to the mould body by magnetic force.

10. 10. The blow mould of claim 1 which is a biaxially stretched blow mould.

11. The blow molding die according to claim 10, wherein the container is a composite container having a container body and a plastic member provided in close contact with the outside of the container body, and the surface of the metal plate forms the uneven structure only on the outer surface of the plastic member.

12. The blow molding mold according to claim 1 , which is a direct blow molding mold or an injection blow molding mold.

13. A method for manufacturing a composite container having a container body and a plastic member provided in close contact with the outside of the container body, comprising: Preparing a preform; providing a plastic member on the exterior of the preform; Providing a blow mould according to any one of claims 1 to 12; and expanding the preform and the plastic member together by blow molding the preform and the plastic member in the blow mold, A method for manufacturing a composite container, in which, in a process of expanding the preform and the plastic member together, the surface shape of the metal plate attached to the mold body is transferred, and a concave-convex structure is formed on the outer surface of the plastic member after blow molding.

14. The method for manufacturing a composite container according to claim 13, wherein in the step of expanding the preform and the plastic member as a unit, a convex portion that protrudes outward is formed at a position of the container body corresponding to the metal plate.

15. The method for manufacturing a composite container according to claim 13 , wherein the uneven structure is located on the outer surface of the plastic member outside an outer surface of a region surrounding the uneven structure.

Citation Information

Patent Citations

  • Blow mold

    JP1986037416A

  • Production of molded product having hologram

    JP1988185621A

  • Hollow container having hologram and production thereof

    JP1995040426A

  • Method for manufacturing resin molded product, molding die, and facing member

    JP2009190312A

  • Blow molding method, complex preform, composite container, inside label member, and plastic-made member

    JP2015128858A