AI Technical Summary

Benefits of technology

【0014】 本発明によれば、隣り合う集電体の間を封止する部材によって密閉空間が形成されている蓄電装置において、活物質層の面積を増大させた場合に生じる集電体の皺及び破れを抑制できる。

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007585760000002
    Figure 0007585760000002
  • Figure 0007585760000003
    Figure 0007585760000003
  • Figure 0007585760000004
    Figure 0007585760000004
Patent Text Reader

Abstract

To suppress wrinkles and tears of a current collector that occur when the area of an active material layer is increased in a power storage device in which a closed space is formed by a member that seals between adjacent current collectors.SOLUTION: A power storage device includes a positive electrode, a negative electrode 22, a separator, and a spacer 24. A negative electrode active material layer 22b of the negative electrode 22 has a rectangular shape in a plan view when viewed from the stacking direction. In a region where the spacer 24 is not adhered on a first surface 22a1 of a negative electrode current collector 22a of the negative electrode 22, a region where the negative electrode active material layer 22b is formed and a negative electrode unbonded portion 22c1 where the negative electrode active material layer 22b is not formed are provided. The ratio of the width L2 of the negative electrode unbonded portion 22c1 to the length L1 of the long side of the negative electrode active material layer 22b in a plan view is 0.02 or less. The corner portion C of the negative electrode active material layer 22b has a chamfered shape in an arc shape, and the radius of curvature of the portion having the maximum curvature in the corner portion C is 5 mm or more.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an electricity storage device. [Background technology]

[0002] Patent Document 1 discloses a flat-type electricity storage device constructed by stacking a plurality of individually manufactured electricity storage cells in series. The electricity storage cell includes a positive electrode having a positive electrode active material layer formed in the center of one side of a resin current collector, a negative electrode having a negative electrode active material layer formed in the center of one side of the resin current collector and arranged so that the negative electrode active material layer faces the positive electrode active material layer of the positive electrode, and a separator arranged between the positive electrode and the negative electrode.

[0003] The storage cell further includes a seal portion disposed on the outer periphery of the resin current collector and liquid-tightly sealing between adjacent resin current collectors in the stacking direction. The seal portion maintains the distance between the resin current collectors to prevent short circuits between the resin current collectors, and liquid-tightly seals between the resin current collectors to form an enclosed space for accommodating an electrolyte. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2019-175778 A Summary of the Invention [Problem to be solved by the invention]

[0005] A method for increasing the capacity of a stacked type power storage cell in which multiple positive electrodes and negative electrodes are stacked with separators interposed therebetween is to increase the area of ​​the active material layer, which can increase the capacity of the power storage cell while maintaining the flat shape of the power storage cell.

[0006] However, when a configuration in which the area of ​​the active material layer is increased is applied to a storage cell in which a seal portion that forms a sealed space between a positive electrode and a negative electrode is bonded, wrinkles and tears are likely to occur in the current collector. In detail, the current collector of the storage cell in which a seal portion that forms a sealed space is provided is fixed by the seal portion around the portion where the active material layer is bonded. In this case, the only portion of the current collector that can tolerate deformation is the unbonded portion located between the portion where the active material layer is bonded and the portion where the seal portion is bonded. Therefore, when the portion of the current collector to which the active material layer is bonded expands and contracts with the expansion and contraction of the active material layer during charging and discharging of the storage cell, local deformation is repeated in the unbonded portion. Specifically, the unbonded portion is repeatedly bent or folded due to the expansion of the active material layer, and the bent or folded portion is repeatedly stretched due to the contraction of the active material layer.

[0007] Here, when the area of ​​the active material layer is increased to increase the capacity of the storage cell, the amount of expansion of the active material layer during charging and discharging increases with the increase in the area of ​​the active material layer, and the amount of deformation of the unbonded portion due to the expansion and contraction of the active material layer also increases. As a result, the load acting on the unbonded portion due to the expansion and contraction of the active material layer increases, making the unbonded portion more likely to wrinkle or break. [Means for solving the problem]

[0008] The object of the present invention is to provide an electricity storage device comprising: a first electrode having a first active material layer formed on a first surface of a first current collector; a second electrode having a second active material layer formed on a first surface of a second current collector, the second active material layer being disposed so as to face the first active material layer of the first electrode; a separator disposed between the first active material layer and the second active material layer; and a spacer disposed between first surfaces of the first current collector and the second current collector, the spacer being disposed so as to surround the periphery of the first active material layer and the second active material layer, and being bonded to the first surfaces of the first current collector and the second current collector to form an enclosed space between the first electrode and the second electrode, the active material layer has a rectangular shape when viewed in a planar view from the stacking direction, and in an area of ​​the first surface of the first current collector to which the spacer is not adhered, there is provided an area where the first active material layer is formed and an area where the first active material layer is not formed, and when the length of a long side of the first active material layer in the planar view is L1 and the length between the spacer and the first active material layer in a direction parallel to the long side of the first active material layer is L2, the ratio (L2 / L1) is 0.02 or less, and at least one corner of the first active material layer is chamfered into an arc, and the radius of curvature of the part of the corner with the maximum curvature is 5 mm or more.

[0009] The present inventors have found that when the area of ​​the rectangular active material layer in plan view is increased, wrinkles and tears occurring in the unbonded portion, which is the region of the current collector where the spacer is not bonded and the active material layer is not formed, are concentrated near the tip of the corner of the active material layer. According to the above configuration, the corner of the rectangular first active material layer in plan view in the first electrode is chamfered in an arc shape. In this case, when the first active material layer expands, the concentration of stress at the tip of the corner of the first active material layer is alleviated, and the stress transmitted from the corner of the first active material layer to the unbonded portion of the first current collector is dispersed over a wide range. As a result, the maximum strain occurring in the unbonded portion of the first current collector when the first active material layer expands can be reduced, and wrinkles and tears occurring in the unbonded portion can be suppressed.

[0010] At least one corner of the first active material layer is preferably arcuate and convex outward. According to the above-mentioned configuration, since no protruding corners are formed, the stress of the expansion of the first active material layer can be prevented from concentrating on a part of the corners. Therefore, the effect of preventing wrinkles and tears from occurring in the unbonded part of the first current collector can be more significantly obtained. In addition, compared to a shape in which the corners are C-chamfered, the reduction in the area of ​​the first active material layer caused by chamfering the corners can be kept small, and the capacity reduction of the first electrode can be suppressed.

[0011] The radius of curvature is preferably 10 mm or more. According to the above-mentioned configuration, the maximum strain occurring in the unbonded portion of the first current collector can be further reduced. The radius of curvature is preferably 30 mm or less.

[0012] The effect of reducing the maximum strain generated in the above range of the first current collector by increasing the radius of curvature of the corners of the arc-chamfered shape converges when the radius of curvature exceeds 30 mm. Therefore, with the above configuration, it is possible to suppress a decrease in capacity of the first electrode caused by the corners of the arc-chamfered shape being formed larger than necessary and the area of ​​the first active material layer being reduced.

[0013] It is preferable that the first current collector is a copper foil, and the first active material layer contains a carbon-based active material. In a configuration in which a first active material layer containing a carbon-based active material with a large expansion rate during charging and discharging is combined with copper foil, the first current collector is particularly prone to wrinkles and tears due to the expansion and contraction of the first active material layer during charging and discharging. Therefore, the above-mentioned effect of forming the corners of the first active material layer into a specific shape can be more significantly achieved. Effect of the Invention

[0014] According to the present invention, in an electricity storage device in which an enclosed space is formed between adjacent current collectors by a member that seals the space, wrinkling and tearing of the current collectors that occurs when the area of ​​the active material layer is increased can be suppressed. [Brief description of the drawings]

[0015] [Figure 1] FIG. [Diagram 2] FIG. [Diagram 3] 13 is a graph showing the results of a simulation test. [Figure 4] (a) is an elliptical corner, (b) is a corner in which multiple curved sections are directly connected, and (c) is a corner in which multiple curved sections are connected via straight line sections. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0016] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. The power storage device 10 shown in Fig. 1 is, for example, a power storage module used in batteries of various vehicles such as forklifts, hybrid cars, and electric cars. The power storage device 10 is, for example, a secondary battery such as a nickel-metal hydride secondary battery or a lithium-ion secondary battery. The power storage device 10 may be an electric double layer capacitor. In this embodiment, the case where the power storage device 10 is a lithium-ion secondary battery is illustrated.

[0017] As shown in Fig. 1, the energy storage device 10 includes a cell stack 30 (laminate) in which a plurality of energy storage cells 20 are stacked in a stacking direction. Hereinafter, the stacking direction of the plurality of energy storage cells 20 will be simply referred to as the stacking direction. Each energy storage cell 20 includes a positive electrode 21, a negative electrode 22, a separator 23, and a spacer 24.

[0018] The positive electrode 21 includes a positive electrode collector 21a and a positive electrode active material layer 21b provided on a first surface 21a1 of the positive electrode collector 21a. In a plan view from the stacking direction (hereinafter simply referred to as a plan view), the positive electrode active material layer 21b is formed in the center of the first surface 21a1 of the positive electrode collector 21a. The peripheral portion of the first surface 21a1 of the positive electrode collector 21a in the plan view is a positive electrode uncoated portion 21c where the positive electrode active material layer 21b is not provided. The positive electrode uncoated portion 21c is arranged so as to surround the periphery of the positive electrode active material layer 21b in the plan view.

[0019] The negative electrode 22 includes a negative electrode current collector 22a and a negative electrode active material layer 22b provided on a first surface 22a1 of the negative electrode current collector 22a. In a plan view, the negative electrode active material layer 22b is formed in the center of the first surface 22a1 of the negative electrode current collector 22a. In a plan view, the peripheral portion of the first surface 22a1 of the negative electrode current collector 22a is a negative electrode uncoated portion 22c where the negative electrode active material layer 22b is not provided. The negative electrode uncoated portion 22c is arranged so as to surround the periphery of the positive electrode active material layer 21b in a plan view. The positive electrode 21 and the negative electrode 22 are arranged so that the positive electrode active material layer 21b and the negative electrode active material layer 22b face each other in the stacking direction. That is, the facing direction of the positive electrode 21 and the negative electrode 22 coincides with the stacking direction. The negative electrode active material layer 22b is formed to have the same size as the positive electrode active material layer 21b, or is formed to be slightly larger than the positive electrode active material layer 21b. When the negative electrode active material layer 22b is formed to be slightly larger than the positive electrode active material layer 21b, the entire formation region of the positive electrode active material layer 21b is located within the formation region of the negative electrode active material layer 22b in a plan view.

[0020] The positive electrode current collector 21a has a second surface 21a2 opposite to the first surface 21a1. The positive electrode 21 is an electrode having a monopolar structure in which neither the positive electrode active material layer 21b nor the negative electrode active material layer 22b is formed on the second surface 21a2 of the positive electrode current collector 21a. The negative electrode current collector 22a has a second surface 22a2 opposite to the first surface 22a1. The negative electrode 22 is an electrode having a monopolar structure in which neither the positive electrode active material layer 21b nor the negative electrode active material layer 22b is formed on the second surface 22a2 of the negative electrode current collector 22a.

[0021] The separator 23 is disposed between the positive electrode 21 and the negative electrode 22, and is a component that separates the positive electrode 21 and the negative electrode 22 to prevent a short circuit due to contact between the two electrodes, while allowing charge carriers such as lithium ions to pass through.

[0022] The separator 23 is, for example, a porous sheet or nonwoven fabric containing a polymer that absorbs and retains an electrolyte. Examples of materials constituting the separator 23 include polyolefins such as polypropylene and polyethylene, and polyesters. The separator 23 may have a single-layer structure or a multi-layer structure. The multi-layer structure may include, for example, an adhesive layer, a ceramic layer as a heat-resistant layer, and the like.

[0023] The spacer 24 is disposed between the first surface 21a1 of the positive electrode collector 21a of the positive electrode 21 and the first surface 22a1 of the negative electrode collector 22a of the negative electrode 22, and on the outer periphery side of the positive electrode active material layer 21b and the negative electrode active material layer 22b, and is bonded to both the positive electrode collector 21a and the negative electrode collector 22a. The spacer 24 maintains a gap between the positive electrode collector 21a and the negative electrode collector 22a to prevent a short circuit between the collectors and to liquid-tightly seal the space between the collectors.

[0024] The spacer 24 extends along the peripheral edge of the positive electrode current collector 21a and the negative electrode current collector 22a in a plan view, and is formed in a frame shape surrounding the periphery of the positive electrode current collector 21a and the negative electrode current collector 22a. The spacer 24 is disposed between the positive electrode uncoated portion 21c of the first surface 21a1 of the positive electrode current collector 21a and the negative electrode uncoated portion 22c of the first surface 22a1 of the negative electrode current collector 22a.

[0025] Examples of materials constituting the spacer 24 include various resin materials such as polyethylene (PE), modified polyethylene (modified PE), polystyrene (PS), polypropylene (PP), modified polypropylene (modified PP), ABS resin, and AS resin.

[0026] An enclosed space S is formed inside the energy storage cell 20 and is surrounded by a frame-shaped spacer 24, a positive electrode 21, and a negative electrode 22. A separator 23 and an electrolyte are contained in the enclosed space S. The peripheral portion of the separator 23 is embedded in the spacer 24.

[0027] Examples of the electrolyte include liquid electrolytes and polymer gel electrolytes containing an electrolyte held in a polymer matrix. Examples of the liquid electrolyte include liquid electrolytes containing a non-aqueous solvent and an electrolyte salt dissolved in the non-aqueous solvent. As the electrolyte salt, known lithium salts such as LiClO4, LiAsF6, LiPF6, LiBF4, LiCF3SO3, LiN(FSO2)2, and LiN(CF3SO2)2 can be used. In addition, as the non-aqueous solvent, known solvents such as cyclic carbonates, cyclic esters, chain carbonates, chain esters, and ethers can be used. Note that two or more of these known solvent materials may be used in combination.

[0028] The spacer 24 can prevent the electrolyte contained in the sealed space S from leaking out to the outside by sealing the sealed space S between the positive electrode 21 and the negative electrode 22. The spacer 24 can also prevent moisture from entering the sealed space S from the outside of the electricity storage device 10. Furthermore, the spacer 24 can prevent gas generated from the positive electrode 21 or the negative electrode 22 due to, for example, a charge / discharge reaction or the like from leaking out to the outside of the electricity storage device 10.

[0029] 2 shows the arrangement of the negative electrode active material layer 22b and the spacer 24 on the first surface 22a1 of the negative electrode current collector 22a, and the planar shapes of the negative electrode active material layer 22b and the spacer 24. The negative electrode active material layer 22b has a rectangular shape in a planar view, and is formed in the center of the first surface 22a1 of the negative electrode current collector 22a. The outer periphery of the first surface 22a1 of the negative electrode current collector 22a where the negative electrode active material layer 22b is not provided is the negative electrode uncoated portion 22c.

[0030] The spacer 24 has a rectangular frame shape in plan view with rectangular inner and outer peripheries, and is bonded to the negative electrode uncoated portion 22c of the first surface 22a1 of the negative electrode collector 22a. The rectangular inner periphery of the spacer 24 is formed larger than the rectangular negative electrode active material layer 22b, and the negative electrode uncoated portion 22c of the negative electrode collector 22a has a negative electrode unbonded portion 22c1 to which the spacer 24 is not bonded. In other words, in the region of the first surface 22a1 of the negative electrode collector 22a to which the spacer 24 is not bonded, a region where the negative electrode active material layer 22b is formed and a region where the negative electrode active material layer 22b is not formed are provided, and the region where the negative electrode active material layer 22b is not formed becomes the negative electrode unbonded portion 22c1.

[0031] Each side constituting the rectangular inner periphery of the spacer 24 is parallel to the opposing side of the negative electrode active material layer 22b. Therefore, the negative electrode non-bonded portion 22c1 has a rectangular frame shape in plan view, with the inner periphery and outer periphery being rectangular.

[0032] Here, the length of the long side of the negative electrode active material layer 22b in a plan view is defined as L1, and the length between the spacer 24 and the negative electrode active material layer 22b in a direction parallel to the long side of the negative electrode active material layer 22b is defined as the width L2 of the negative electrode unbonded portion 22c1. In this case, the ratio (L2 / L1) of the width L2 of the negative electrode unbonded portion 22c1 to the length L1 of the long side of the negative electrode active material layer 22b is 0.02 or less, and preferably 0.01 or less. Moreover, the ratio (L2 / L1) is, for example, 0.002 or more.

[0033] The above-mentioned ratio (L2 / L1) means that the ratio of the area of ​​the negative electrode active material layer 22b to the first surface 22a1 of the negative electrode collector 22a is large, and the area of ​​the negative electrode non-bonded portion 22c1 is relatively small compared to the area of ​​the negative electrode active material layer 22b. In detail, the area of ​​the first surface 22a1 of the negative electrode collector 22a is set based on the application of the electricity storage device 10, such as the mounting space, and then the area to which the frame-shaped spacer 24 is bonded is set to ensure the sealing of the sealed space S. Next, the area to which the negative electrode non-bonded portion 22c1 and the negative electrode active material layer 22b are formed is set with respect to the area located inside the area to which the spacer 24 is bonded on the first surface 22a1 of the negative electrode collector 22a. At this time, the formation range of the negative electrode active material layer 22b is set so that an excess space for accommodating gas generated during charging and discharging is formed within the sealed space S, while ensuring a negative electrode unbonded portion 22c1 on the first surface 22a1 of the negative electrode current collector 22a, and making the battery capacity (negative electrode capacity) as large as possible.

[0034] The length L1 of the long side of the negative electrode active material layer 22b is preferably 800 mm or more, more preferably 1000 mm or more. The length L1 of the long side is preferably 2500 mm or less, more preferably 1600 mm or less. The width L2 of the negative electrode unbonded portion 22c1 is preferably 3 mm or more, more preferably 5 mm or more. The width L2 of the negative electrode unbonded portion 22c1 is, for example, 30 mm or less. When the planar shape of the negative electrode active material layer 22b is a square, one of two pairs of opposing sides of the square is regarded as the long side.

[0035] Although not shown, the arrangement of the positive electrode active material layer 21b and the spacers 24 on the first surface 21a1 of the positive electrode current collector 21a, and the planar shapes of the positive electrode active material layer 21b and the spacers 24 are also similar to the configuration of the negative electrode 22 described above.

[0036] More specifically, the positive electrode active material layer 21b has a rectangular shape in plan view and is bonded to the center of the first surface 21a1 of the positive electrode collector 21a. The outer peripheral portion of the first surface 21a1 of the positive electrode collector 21a where the positive electrode active material layer 21b is not provided is the positive electrode uncoated portion 21c. The positive electrode uncoated portion 21c has a positive electrode unbonded portion 21c1 (not shown) to which the spacer 24 is not bonded. Each side constituting the rectangular inner peripheral edge of the spacer 24 is parallel to the opposing side of the positive electrode active material layer 21b. Therefore, the positive electrode unbonded portion 21c1 has a rectangular frame shape in plan view with rectangular inner peripheral edge and outer peripheral edge.

[0037] Here, similarly to the negative electrode 22, the length of the long side of the positive electrode active material layer 21b in a planar view is defined as L1, and the length between the spacer 24 and the positive electrode active material layer 21b, which is the length in the direction parallel to the long side of the positive electrode active material layer 21b, is defined as the width L2 of the positive electrode unbonded portion 21c1.

[0038] As described above, the positive electrode active material layer 21b may be formed to have the same size as the negative electrode active material layer 22b, or may be formed to be one size smaller than the negative electrode active material layer 22b. Assume that the positive electrode active material layer 21b is formed to have the same size as the negative electrode active material layer 22b. In this case, the ratio (L2 / L1) of the width L2 of the positive electrode non-bonded portion 21c1 to the length L1 of the long side of the positive electrode active material layer 21b is 0.02 or less, and preferably 0.01 or less. Moreover, the ratio (L2 / L1) is, for example, 0.002 or more. The length L1 of the long side of the positive electrode active material layer 21b is preferably 800 mm or more, and more preferably 1000 mm or more. Moreover, the length L1 of the long side is preferably 2500 mm or less, and more preferably 1600 mm or less. The width L2 of the positive electrode non-bonded portion 21c1 is preferably 3 mm or more, and more preferably 5 mm or more. The width L2 of the positive electrode non-bonded portion 21c1 is, for example, 30 mm or less. When the shape of the positive electrode active material layer 21b in a plan view is a square, one of two pairs of opposing sides of the square is regarded as the long side.

[0039] Next, assume that the positive electrode active material layer 21b is formed slightly smaller than the negative electrode active material layer 22b. In this case, the length L1 of the long side of the positive electrode active material layer 21b is shorter than the length L1 of the long side of the negative electrode active material layer 22b. The width L2 of the positive electrode unbonded portion 21c1 is longer than the width L2 of the negative electrode unbonded portion 22c1 in accordance with the shortened length L1 of the long side of the positive electrode active material layer 21b.

[0040] In this case, the ranges of the length L1 of the long side of the positive electrode active material layer 21b, the width L2 of the positive electrode unbonded portion 21c1, and the ratio (L2 / L1) are shifted in accordance with the shortening of the length L1 of the long side of the positive electrode active material layer 21b, compared to the ranges when the positive electrode active material layer 21b and the negative electrode active material layer 22b are of equal size. Specifically, the range of the length L1 of the long side of the positive electrode active material layer 21b shifts toward smaller values, the width L2 of the positive electrode unbonded portion 21c1 shifts toward larger values, and the range of the ratio (L2 / L1) shifts toward larger values.

[0041] Each of the positive electrode active material layer 21b and the negative electrode active material layer 22b, which are rectangular in plan view, has four corners C. Only the negative electrode active material layer 22b is shown in Fig. 2. Each corner C is formed into an arc-shaped chamfered shape.

[0042] Examples of arc-chamfered shapes include a circular arc shape with a constant curvature, an elliptical arc shape with a gradually changing curvature, and a shape in which multiple curved segments made of circular or elliptical arcs are connected directly or via straight line segments.

[0043] The arc shape may be, for example, an outwardly convex arc shape or an inwardly convex arc shape. In Fig. 2, an outwardly convex arc corner C is illustrated as an example. Examples of the elliptical arc shape include an elliptical arc shape that is convex outward and an elliptical arc shape that is convex inward. Fig. 4(a) illustrates a corner C of an elliptical arc shape that is convex outward.

[0044] FIG. 4(b) shows a corner C having a shape in which two outwardly convex circular arcs X1 and X2 are connected, as an example of a shape in which multiple curved portions are connected. Note that in a shape in which multiple curved portions are connected, the number of curved portions to be connected is not particularly limited. The lengths of the circular or elliptical arcs constituting the multiple curved portions and the curvatures of the circular or elliptical arcs may be the same, or some or all of them may be different. Also, some of the curved portions may be arc-shaped with an inwardly convex shape.

[0045] 4(c) shows an example of a shape in which multiple curved segments are connected via a straight line segment, in which two outwardly convex arcs X1 and X2 are connected by a straight line Y1 at a corner C. The straight line Y1 is a tangent to the arc X1 at a connection point P1 with the straight line Y1, and is also a tangent to the arc X2 at a connection point P2 with the straight line Y1.

[0046] In a shape in which multiple curved segments are connected via straight line segments, the number of curved segments and straight line segments to be connected is not particularly limited. The lengths of the circular or elliptical arcs constituting a shape in which multiple circular or elliptical arcs are connected, and the curvatures of the circular or elliptical arcs may be the same, or some or all of them may be different. The straight lines connecting the circular or elliptical arcs are not limited to tangents at the connection points of the circular or elliptical arcs.

[0047] The shape in which a plurality of curved portions are connected directly or via straight portions is preferably a shape in which a plurality of curved portions, including a curved portion connected to a long side of the active material layer on which corner C is provided and a curved portion connected to a short side, are connected directly or via straight portions. In addition, the shape in which a plurality of curved portions are connected directly or via straight portions is preferably a shape in which the curved portions are connected such that no corners protruding toward the outer periphery are formed.

[0048] The radius of curvature of the portion with the maximum curvature at the arc-shaped corner C is 5 mm or more, and preferably 10 mm or more. Also, the radius of curvature is preferably 30 mm or less, and more preferably 20 mm or less.

[0049] The formation range A1 of the corner C in the direction parallel to the long side of the active material layer on which the corner C is provided, which is the formation range of the corner C having an arc-shaped chamfer, is preferably 5 mm or more, more preferably 10 mm or more. The formation range A1 is, for example, 30 mm or less. The formation range A2 of the corner C in the direction parallel to the short side of the active material layer on which the corner C is provided, is preferably 5 mm or more, more preferably 10 mm or more. The formation range A2 is, for example, 30 mm or less. In the case of the corner C having an outwardly convex arc or elliptical arc, the formation range of the corner C is, for example, a range in which the central angle θ of the arc is 30 degrees or more and 90 degrees or less, and preferably a range in which the central angle θ is 90 degrees.

[0050] The shapes of the corners C of the negative electrode active material layer 22b may all be the same or different as long as the above-mentioned numerical values ​​are satisfied. Similarly, the shapes of the corners C of the positive electrode active material layer 21b may all be the same or different as long as the above-mentioned numerical values ​​are satisfied.

[0051] In this embodiment, the negative electrode 22, the negative electrode current collector 22a, and the negative electrode active material layer 22b correspond to the first electrode, the first current collector, and the first active material layer, respectively. The negative electrode unbonded portion 22c1 corresponds to a region on the first surface of the first current collector where the spacer is not bonded and where the first active material layer is not formed. The positive electrode 21, the positive electrode current collector 21a, and the positive electrode active material layer 21b correspond to the second electrode, the second current collector, and the second active material layer, respectively.

[0052] 1, the cell stack 30 has a structure in which a plurality of storage cells 20 are directly or indirectly stacked so that the second surface 21a2 of the positive electrode current collector 21a and the second surface 22a2 of the negative electrode current collector 22a are in electrical contact with each other. As a result, the plurality of storage cells 20 constituting the cell stack 30 are connected in series.

[0053] Here, in the cell stack 30, two storage cells 20 adjacent to each other in the stacking direction form a pseudo bipolar electrode 25 in which the positive electrode current collector 21a and the negative electrode current collector 22a in contact with each other are regarded as one current collector. The pseudo bipolar electrode 25 includes a current collector having a structure in which the positive electrode current collector 21a and the negative electrode current collector 22a are stacked, a positive electrode active material layer 21b formed on one surface of the current collector, and a negative electrode active material layer 22b formed on the other surface.

[0054] The energy storage device 10 includes a pair of current conductors, consisting of a positive electrode current conductor plate 40 and a negative electrode current conductor plate 50, disposed on either side of the cell stack 30 in the stacking direction of the cell stack 30. The positive electrode current conductor plate 40 and the negative electrode current conductor plate 50 are each made of a material having excellent electrical conductivity.

[0055] The positive electrode current-carrying plate 40 is electrically connected to the second surface 21a2 of the positive electrode current collector 21a of the positive electrode 21 arranged at the outermost side at one end in the stacking direction. The negative electrode current-carrying plate 50 is electrically connected to the second surface 22a2 of the negative electrode current collector 22a of the negative electrode 22 arranged at the outermost side at the other end in the stacking direction.

[0056] The electricity storage device 10 is charged and discharged through terminals provided on the positive electrode current-carrying plate 40 and the negative electrode current-carrying plate 50. The material constituting the positive electrode current-carrying plate 40 may be, for example, the same material as the material constituting the positive electrode current-collector 21a. The positive electrode current-carrying plate 40 may be made of a metal plate thicker than the positive electrode current-collector 21a used in the cell stack 30. The material constituting the negative electrode current-carrying plate 50 may be, for example, the same material as the material constituting the negative electrode current-collector 22a. The negative electrode current-carrying plate 50 may be made of a metal plate thicker than the negative electrode current-collector 22a used in the cell stack 30.

[0057] Next, the positive electrode current collector 21a, the negative electrode current collector 22a, the positive electrode active material layer 21b, and the negative electrode active material layer 22b will be described in detail. <Positive electrode current collector and negative electrode current collector> The positive electrode collector 21a and the negative electrode collector 22a are chemically inactive electrical conductors for continuously passing current to the positive electrode active material layer 21b and the negative electrode active material layer 22b during discharging or charging of the lithium ion secondary battery. The positive electrode collector 21a and the negative electrode collector 22a are in the form of foil. The foil-shaped positive electrode collector 21a and the negative electrode collector 22a each have a thickness of, for example, 1 μm or more and 100 μm or less, and preferably 10 μm or more and 60 μm or less. For example, a metal material, a conductive resin material, a conductive inorganic material, etc. can be used as the material for the positive electrode collector 21a and the negative electrode collector 22a.

[0058] Examples of the metal material include copper, aluminum, nickel, titanium, and stainless steel. Examples of the conductive resin material include resins obtained by adding a conductive filler to a conductive polymer material or a non-conductive polymer material as necessary.

[0059] Either or both of the positive electrode collector 21a and the negative electrode collector 22a may have a plurality of layers including one or more layers containing the above-mentioned metal material or conductive resin material. Either or both of the surfaces of the positive electrode collector 21a and the negative electrode collector 22a may be covered with a known protective layer. Either or both of the surfaces of the positive electrode collector 21a and the negative electrode collector 22a may be surface-treated by a known method such as plating. Examples of the surface treatment include chromate treatment and chromate phosphate treatment.

[0060] A preferred example of the positive electrode current collector 21a and the negative electrode current collector 22a is a case in which the positive electrode current collector 21a is made of aluminum foil and the negative electrode current collector 22a is made of copper foil.

[0061] <Positive Electrode Active Material Layer and Negative Electrode Active Material Layer> The positive electrode active material layer 21b includes a positive electrode active material capable of absorbing and releasing charge carriers such as lithium ions. As the positive electrode active material, for example, a lithium composite metal oxide having a layered rock salt structure, a metal oxide having a spinel structure, a polyanion-based compound, or the like that can be used as a positive electrode active material for a lithium ion secondary battery may be used. Two or more types of positive electrode active materials may be used in combination. In this embodiment, the positive electrode active material layer 21b includes olivine-type lithium iron phosphate (LiFePO4) as a polyanion-based compound.

[0062] The negative electrode active material layer 22b can be used without any particular limitation as long as it is a simple substance, an alloy, or a compound capable of absorbing and releasing charge carriers such as lithium ions. For example, the negative electrode active material can be Li, a carbon-based active material, a metal compound, and an element or a compound thereof capable of alloying with lithium. For example, the carbon-based active material can be natural graphite, artificial graphite, hard carbon (hardly graphitizable carbon), and soft carbon (easily graphitizable carbon). For example, the artificial graphite can be highly oriented graphite, mesocarbon microbeads, and the like. For example, the element capable of alloying with lithium can be silicon, tin, and the like. In this embodiment, the negative electrode active material layer 22b contains a carbon-based active material.

[0063] The positive electrode active material layer 21b and the negative electrode active material layer 22b (hereinafter also simply referred to as the active material layer) may each further contain, as necessary, a conductive assistant for enhancing electrical conductivity, a binder, an electrolyte (polymer matrix, ion-conductive polymer, liquid electrolyte, etc.), an electrolyte supporting salt for enhancing ion conductivity (lithium salt), etc. The components contained in the active material layer or the blending ratio of the components and the thickness of the active material layer are not particularly limited, and conventionally known knowledge about lithium ion secondary batteries may be appropriately referred to.

[0064] The conductive assistant is added to increase the conductivity of the positive electrode 21 or the negative electrode 22. Examples of the conductive assistant include acetylene black, carbon black, and graphite. Examples of the binder include fluorine-containing resins such as polyvinylidene fluoride, polytetrafluoroethylene, and fluorine rubber, thermoplastic resins such as polypropylene and polyethylene, imide resins such as polyimide and polyamideimide, alkoxysilyl group-containing resins, acrylic resins such as polyacrylic acid and polymethacrylic acid, styrene-butadiene rubber, carboxymethyl cellulose, alginates such as sodium alginate and ammonium alginate, water-soluble cellulose ester crosslinkers, and starch-acrylic acid graft polymers. These binders can be used alone or in combination. Examples of the solvent or dispersion medium include water and N-methyl-2-pyrrolidone.

[0065] The thickness and basis weight of the active material layer are not particularly limited, and conventionally known knowledge about lithium ion secondary batteries may be referred to as appropriate. However, from the viewpoint of increasing the energy density of the power storage cell 20, it is preferable to increase the thickness and basis weight of the active material layer. Specifically, the thickness of the positive electrode active material layer 21b is, for example, 100 μm or more and 400 μm or less, and preferably 200 μm or more. The basis weight of the positive electrode active material layer 21b is, for example, 40 mg / cm 2 More than 80mg / cm 2 Less than 50 mg / cm 2 The thickness of the negative electrode active material layer 22b is 100 μm or more and 400 μm or less, and preferably 200 μm or more. The weight per unit area of ​​the negative electrode active material layer 22b is, for example, 20 mg / cm 2 More than 40mg / cm 2 25 mg / cm or less 2 More preferably, it is equal to or greater than this.

[0066] Examples of a method for forming an active material layer on the surface of the positive electrode current collector 21a and the negative electrode current collector 22a include a conventionally known method such as a roll coating method. In order to improve the thermal stability of the positive electrode 21 or the negative electrode 22, the above-mentioned heat-resistant layer may be provided on the surface of the active material layer.

[0067] Next, the operation of this embodiment will be described. In the electricity storage device 10 of this embodiment, a spacer 24 is provided to form an enclosed space S between the positive electrode 21 and the negative electrode 22, and an outer peripheral portion of the first surface 22a1 of the negative electrode current collector 22a is fixed by the spacer 24. In addition, in the first surface 22a1 of the negative electrode current collector 22a, a negative electrode unbonded portion 22c1 located between a portion where the negative electrode active material layer 22b is formed and a portion where the spacer 24 is bonded is significantly smaller than the range where the negative electrode active material layer 22b is formed bonded to the center portion.

[0068] In the case of an electricity storage device employing the above-mentioned configuration, the negative electrode active material layer 22b expands significantly in the planar direction during charging and discharging, while the negative electrode unbonded portion 22c1, which is a portion that deforms with the negative electrode active material layer 22b, is small, so that the negative electrode unbonded portion 22c1 deforms significantly with the expansion and contraction of the negative electrode active material layer 22b. As a result, the load acting on the negative electrode unbonded portion 22c1 due to the expansion and contraction of the negative electrode active material layer 22b increases, and the negative electrode unbonded portion 22c1 is likely to wrinkle or break.

[0069] In particular, when the negative electrode active material layer 22b has a rectangular shape in a plan view, the stress of the expansion of the negative electrode active material layer 22b when the negative electrode active material layer 22b expands is concentrated at one point at the tip of the corner C. Therefore, a large load is locally applied to the negative electrode unbonded portion 22c1 located in the vicinity of the tip of the corner C, and the largest strain occurs in that portion.

[0070] Therefore, in this embodiment, the corners C of the negative electrode active material layer 22b are formed into an arc-shaped chamfered shape. As a result, when the negative electrode active material layer 22b expands, the concentration of stress on the tip of the corners C of the negative electrode active material layer 22b is alleviated, and the stress transmitted from the corners C to the negative electrode unbonded portion 22c1 is dispersed over a wide range. As a result, the maximum strain generated in the negative electrode unbonded portion 22c1 when the negative electrode active material layer 22b expands can be reduced, and wrinkles and tears generated in the negative electrode unbonded portion 22c1 can be suppressed. Note that, in this embodiment, the positive electrode 21 is configured in the same way, and wrinkles and tears generated in the positive electrode unbonded portion 21c1 can also be suppressed by the same mechanism.

[0071] Here, a computer simulation was performed on the relationship between the thickness of the current collector, the shape of the corners of the active material layer, and the maximum strain generated in the current collector by one charge and discharge. The electrodes of models 1 to 4 used in this simulation were negative electrodes using copper foil as the current collector and carbon-based active material as the active material, and their detailed configurations are as shown in Table 1. For each model, the corners of the active material layer were made arc-shaped, and the electrode angle R (radius of curvature) of the arc-shaped corners was changed to 0, 5, 10, 15, 20, 25, and 30 mm. In addition, the width L2 of the unbonded part of the current collector was 8 mm, and the formation range of the arc-shaped corners was a range in which the central angle θ was 90 degrees in all cases. Then, assuming that the expansion rate in the surface direction of the active material layer accompanying one charge and discharge was 9%, the maximum foil strain in one charge and discharge was obtained. The results are shown in the graph of FIG. 3.

[0072] [Table 1] The simulation results will be considered with reference to FIG. 3. From the results of models 1, 2, and 3, which differ only in the thickness of the copper foil that is the current collector, it can be seen that the thinner the current collector is, the larger the maximum strain that occurs in the current collector is. Also, from the results of models 1 and 4, which differ only in the size of the active material layer, it can be seen that the larger the size (area) of the active material layer is, that is, the smaller the width of the unbonded portion relative to the length of the long side of the current collector is, the larger the maximum strain that occurs in the current collector is. This tendency for the maximum strain to increase when the current collector is thin and when the active material layer is large is common regardless of the shape of the corners of the active material layer.

[0073] In all of the models 1 to 4, the maximum strain generated in the current collector is smaller when the corners of the active material layer are arc-shaped with a radius of curvature of 5 mm than when the corners of the active material layer are right angles (radius of curvature 0 mm). The maximum strain generated in the current collector when the corners of the active material layer are arc-shaped decreases as the radius of curvature of the arc-shaped corner increases to 5 mm, 10 mm, and 30 mm. The effect of reducing the maximum strain is remarkable when the radius of curvature is between 0 mm and 5 mm, and between 5 mm and 10 mm. However, when the radius of curvature is in the range of 25 to 30 mm, the effect of further reducing the maximum strain by increasing the radius of curvature is almost nonexistent.

[0074] Therefore, from the viewpoint of reducing the maximum strain, it is found that it is effective to set the radius of curvature of the circular corner to 5 mm or more or 10 mm or more, and from the viewpoint of forming a large active material layer to ensure battery capacity, it is found that it is effective to set the radius of curvature of the circular corner to 30 mm or less.

[0075] In addition, based on the above results, a computer simulation was performed to determine how the maximum strain during a single charge / discharge cycle affects the number of cycles and foil breakage. The simulation showed that if the maximum strain during a single charge / discharge cycle could be kept below 2.8%, foil breakage could be suppressed up to 3,000 cycles, which is the cycle life of general power storage devices such as automotive power storage devices.

[0076] Referring to the simulation results shown in Figure 3, when the radius of curvature of the circular corners is 5 mm or more, the maximum strain generated by one charge / discharge is suppressed to 2.8% or less even in models 1 and 4 using a thin copper foil with a thickness of 6 μm. Therefore, it can be said that by making the radius of curvature of the circular corners 5 mm or more, foil breakage can be suppressed up to 3000 cycles, which is the cycle life of a general energy storage device.

[0077] Compared to other metal foils used as current collectors, copper foil is often used in a thin thickness. Also, from the viewpoint of suppressing pinholes, copper foil is often used in a thickness of 10 μm or more. Therefore, the fact that the effect of sufficiently suppressing the maximum strain was obtained in models 1 and 4, which used a thin copper foil with a thickness of 6 μm, suggests that a similar effect can be obtained when using current collectors made of other materials.

[0078] According to this embodiment, the following effects can be obtained. (1) The electricity storage device 10 includes a positive electrode 21 having a positive electrode current collector 21a and a positive electrode active material layer 21b, a negative electrode 22 having a negative electrode current collector 22a and a negative electrode active material layer 22b, a separator 23 disposed between the positive electrode active material layer 21b and the negative electrode active material layer 22b, and a spacer 24 disposed between the positive electrode 21 and the negative electrode 22. The spacer 24 is disposed so as to surround the periphery of the positive electrode active material layer 21b and the negative electrode active material layer 22b, and is bonded to each first surface of the positive electrode current collector 21a and the negative electrode current collector 22a to form an enclosed space between the positive electrode 21 and the negative electrode 22. The negative electrode active material layer 22b has a rectangular shape in a plan view seen from the stacking direction. In a region of the first surface 22a1 of the negative electrode current collector 22a where the spacer 24 is not bonded, there are provided a region where the negative electrode active material layer 22b is formed and a negative electrode unbonded portion 22c1 where the negative electrode active material layer 22b is not formed. A ratio (L2 / L1) of a width L2 of the negative electrode unbonded portion 22c1 to a length L1 of a long side of the negative electrode active material layer 22b in a plan view is 0.02 or less. A corner C of the negative electrode active material layer 22b is chamfered into an arc shape, and a radius of curvature of a portion of the corner C with a maximum curvature is 5 mm or more.

[0079] According to the above-mentioned configuration, it is possible to reduce the maximum strain generated in the negative electrode unbonded portion 22c1 when the negative electrode active material layer 22b expands, and it is possible to suppress wrinkles and tears generated in the negative electrode unbonded portion 22c1.

[0080] (2) The corners C of the negative electrode active material layer 22b are arc-shaped and protrude outward. According to the above-mentioned configuration, since no protruding corners are formed, it is possible to suppress the stress caused by the expansion of the negative electrode active material layer 22b from concentrating on a part of the corner C. Therefore, the above-mentioned effect (1) can be obtained more significantly. Also, compared to a shape in which the corner C is chamfered, it is possible to suppress the amount of reduction in the area of ​​the negative electrode active material layer 22b caused by chamfering the corner C to be small, and it is possible to suppress a decrease in the capacity of the negative electrode 22.

[0081] In addition, when the corner C is made into an arc shape, the effect of suppressing the concentration of the stress due to the expansion of the negative electrode active material layer 22b is greater than when the corner C is made into an elliptical arc shape. In addition, when the corner C is made into an elliptical arc shape, it is possible to suppress the reduction in the area of ​​the negative electrode active material layer 22b caused by chamfering the corner C to a smaller amount than when the corner C is made into an arc shape. For example, when the shape of the negative electrode active material layer 22b in a plan view is a rectangle having long sides and short sides, the formation range of the arc-shaped corner C is set according to the length in the direction parallel to the long side, which is the direction in which the expansion amount is large. In this case, when the arc-shaped corner C with a constant curvature is adopted, the formation range A1 of the corner C in the direction parallel to the long side and the formation range A2 of the corner C in the direction parallel to the short side become equal, so that the formation range A2 of the corner C in the direction parallel to the short side becomes larger than necessary. On the other hand, when the corner C is formed in an elliptical arc shape with a curvature gradually increasing from the long side toward the short side as shown in Fig. 4(a), the formation area A2 of the corner C parallel to the short side can be made smaller than the formation area A1 of the corner C parallel to the long side. Therefore, the reduction in the area of ​​the negative electrode active material layer 22b caused by chamfering the corner C can be kept small. The effect of (2) is also applicable to the positive electrode 21.

[0082] (3) The radius of curvature of corner C is 10 mm or more. According to the above configuration, the maximum strain generated in the positive electrode unbonded portion 21c1 and the negative electrode unbonded portion 22c1 can be further reduced.

[0083] (4) The radius of curvature of corner C is 30 mm or less. The effect of reducing the maximum strain generated in the positive electrode unbonded portion 21c1 and the negative electrode unbonded portion 22c1 by increasing the radius of curvature of the corner C converges when the radius of curvature exceeds 30 mm. Therefore, according to the above configuration, it is possible to suppress a decrease in the capacity of the positive electrode 21 and the negative electrode 22, which would be caused by forming the arc-shaped corner C larger than necessary and reducing the areas of the positive electrode active material layer 21b and the negative electrode active material layer 22b.

[0084] (5) The negative electrode current collector 22a is a copper foil, and the negative electrode active material layer 22b contains a carbon-based active material. In a configuration in which the negative electrode active material layer 22b containing a carbon-based active material with a large expansion rate during charging and discharging is combined with copper foil, the negative electrode current collector 22a is particularly prone to wrinkles and tears due to the expansion and contraction of the negative electrode active material layer 22b during charging and discharging, and therefore the effect of (1) above is more pronounced.

[0085] (6) The positive electrode 21, the negative electrode 22, and the separator 23 are repeatedly stacked in a stacked structure, and a second surface 21a2 opposite to the first surface 21a1 of the positive electrode current collector 21a is in contact with a second surface 22a2 opposite to the first surface 22a1 of the negative electrode current collector 22a.

[0086] In this case, if wrinkles occur in the positive electrode unbonded portion 21c1 and the negative electrode unbonded portion 22c1, the contact area between the second surface 21a2 of the positive electrode current collector 21a and the second surface 22a2 of the negative electrode current collector 22a may decrease, resulting in an increase in resistance. Therefore, when the above technique (1) is applied to such a configuration, in addition to the effect of suppressing wrinkles occurring in the positive electrode unbonded portion 21c1 and the negative electrode unbonded portion 22c1, the effect of suppressing deterioration of battery performance can be obtained.

[0087] This embodiment can be modified as follows: This embodiment and the following modifications can be combined with each other to the extent that no technical contradiction occurs. In the above embodiment, all of the four corners C of the negative electrode active material layer 22b are chamfered into an arc shape, but it is sufficient that at least one corner C of the negative electrode active material layer 22b is chamfered into an arc shape. When multiple corners C are chamfered into an arc shape, the shapes of the corners C may be the same or may be partially or entirely different.

[0088] When the negative electrode 22 has the configuration described in the above embodiment, the configuration of the positive electrode 21 is not limited to the configuration of the above embodiment. The shape of the positive electrode active material layer 21b, the ratio of the width L2 of the positive electrode non-bonded portion 21c1 to the length L1 of the long side of the positive electrode active material layer 21b, and the shape of the corner C of the positive electrode active material layer 21b are not limited to the configurations of the above embodiment, and conventionally known configurations can be applied. In this case, the negative electrode 22 becomes the first electrode.

[0089] The positive electrode active material layer 21b and the negative electrode active material layer 22b may have the same size in a plan view. Between the positive electrode current-carrying plate 40 and the positive electrode current-collector 21a, a conductive layer that adheres closely to the positive electrode current-collector 21a may be disposed in order to improve the conductive contact between the two members. Examples of the conductive layer include a layer containing carbon such as acetylene black or graphite, and a layer having a lower hardness than the positive electrode current-collector 21a, such as a plating layer containing Au or the like. A similar conductive layer may be disposed between the negative electrode current-carrying plate 50 and the negative electrode current-collector 22a.

[0090] There is no particular limitation on the number of storage cells 20 constituting the energy storage device 10. The number of storage cells 20 constituting the energy storage device 10 may be one. The positive electrode active material layer 21b or the negative electrode active material layer 22b may be provided on the second surface 21a2 of the positive electrode current collector 21a. The positive electrode active material layer 21b or the negative electrode active material layer 22b may be provided on the second surface 22a2 of the negative electrode current collector 22a.

[0091] The electrodes may be bipolar electrodes in which the positive electrode current collector 21a and the negative electrode current collector 22a are integrated into one current collector using a bimetal or the like. In the cell stack 30, the second surface 21a2 of the positive electrode current collector 21a and the second surface 22a2 of the negative electrode current collector 22a, which are contact portions between adjacent power storage cells 20 in the stacking direction, may be bonded to each other. Examples of a method for bonding the second surface 21a2 of the positive electrode current collector 21a and the second surface 22a2 of the negative electrode current collector 22a include a method using a conductive adhesive.

[0092] Next, technical ideas that can be understood from the above embodiment and modified examples will be described below. (i) The energy storage device has a structure in which the positive electrode, the negative electrode, and the separator are repeatedly stacked, and a second surface of the positive electrode current collector opposite the first surface is in contact with a second surface of the negative electrode current collector opposite the first surface. [Explanation of symbols]

[0093] C...corner, S...sealed space, 10...energy storage device, 20...energy storage cell, 21...positive electrode, 21a...positive electrode current collector, 21b...positive electrode active material layer, 21c1...positive electrode unbonded portion, 22...negative electrode, 22a...negative electrode current collector, 22b...negative electrode active material layer, 22c1...negative electrode unbonded portion, 23...separator, 24...spacer, 30...cell stack, 40...positive electrode current-carrying plate, 50...negative electrode current-carrying plate.

Claims

1. a first electrode having a first active material layer formed on a first surface of a first current collector; a second electrode including a second active material layer formed on a first surface of a second current collector, the second active material layer being disposed so as to face the first active material layer of the first electrode; a separator disposed between the first active material layer and the second active material layer; a spacer disposed between the first surfaces of the first current collector and the second current collector; the spacer is disposed so as to surround the first active material layer and the second active material layer, and is bonded to first surfaces of the first current collector and the second current collector to form an enclosed space between the first electrode and the second electrode; the first active material layer has a rectangular shape in a plan view seen from the stacking direction, a region on the first surface of the first current collector to which the spacer is not attached is provided with a region in which the first active material layer is formed and a region in which the first active material layer is not formed, a length of a long side of the first active material layer in the plan view is defined as L1, and a length between the spacer and the first active material layer in a direction parallel to the long side of the first active material layer is defined as L2, where L2 / L1 is a ratio of 0.02 or less, At least one corner of the first active material layer is chamfered into an arc shape, and the radius of curvature of the corner at the maximum curvature is 10 mm or more.

2. a first electrode having a first active material layer formed on a first surface of a first current collector; a second electrode including a second active material layer formed on a first surface of a second current collector, the second active material layer being disposed so as to face the first active material layer of the first electrode; a separator disposed between the first active material layer and the second active material layer; a spacer disposed between the first surfaces of the first current collector and the second current collector; the spacer is disposed so as to surround the first active material layer and the second active material layer, and is bonded to first surfaces of the first current collector and the second current collector to form an enclosed space between the first electrode and the second electrode; A liquid electrolyte is contained in the sealed space, the first active material layer has a rectangular shape in a plan view seen from the stacking direction, a region on the first surface of the first current collector to which the spacer is not attached is provided with a region in which the first active material layer is formed and a region in which the first active material layer is not formed, a length of a long side of the first active material layer in the plan view is defined as L1, and a length between the spacer and the first active material layer in a direction parallel to the long side of the first active material layer is defined as L2, where L2 / L1 is a ratio of 0.02 or less, At least one corner of the first active material layer is chamfered into an arc shape, and the radius of curvature of the corner at the maximum curvature is 5 mm or more.

3. The power storage device according to claim 1 , wherein at least one corner of the first active material layer is arc-shaped and protrudes outward.

4. The power storage device according to any one of claims 1 to 3, wherein the radius of curvature is 30 mm or less.

5. 5. The power storage device according to claim 1, wherein the first current collector is a copper foil, and the first active material layer contains a carbon-based active material.

Citation Information

Patent Citations

  • Battery

    JP2012221608A

  • Battery and method of manufacturing the same

    JP2013084410A

  • Battery

    JP2014175247A

  • Power storage device

    JP2015065229A

  • Bipolar battery unit and bipolar battery

    JP2019175778A