Solid state battery

By designing electrode bodies with controlled undulations, the battery addresses resistance issues from temperature unevenness, ensuring stable performance through increased contact points and reduced resistance.

JP7586139B2Active Publication Date: 2024-11-19TOYOTA JIDOSHA KK
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2022081337
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-05-18
Publication Date
2024-11-19
Estimated Expiration
2042-05-18

AI Technical Summary

Technical Problem

Solid-state batteries experience significant resistance increases after repeated charging and discharging due to temperature unevenness caused by heat generation and non-uniform confining pressure.

Method used

The battery design incorporates electrode bodies with predetermined undulations, ensuring the undulation height is greater than the thickness difference and the waviness number per unit length is within a specific range, increasing contact points and reducing temperature unevenness.

Benefits of technology

This design results in a solid-state battery with minimal resistance increase even after repeated charging and discharging, maintaining performance stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007586139000002
    Figure 0007586139000002
  • Figure 0007586139000003
    Figure 0007586139000003
  • Figure 0007586139000004
    Figure 0007586139000004
Patent Text Reader

Abstract

To provide a solid-state battery in which an increase in resistance is suppressed even with repeated charging and discharging.SOLUTION: The present disclosure provides a solid-state battery including a plurality of electrode bodies stacked in a thickness direction. Each of the electrode body includes a positive electrode collector layer, a positive electrode active material layer, a solid electrolyte layer, a negative electrode active material layer, and a negative electrode collector layer, in this order, in the thickness direction. When distances from a front side and a rear side of the electrode body to the electrode body are respectively measured along a short side direction of the electrode body using a laser displacement meter, the waviness height of the electrode body is greater than a thicknesses difference of the electrode body, and the number of waviness (per unit length) of the electrode body is 0.23 times / mm or more and 0.40 times / mm or less.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to solid-state batteries. [Background technology]

[0002] A solid-state battery is a battery that has a solid electrolyte layer between a positive electrode active material layer and a negative electrode active material layer, and has the advantage that it is easier to simplify safety devices compared to liquid batteries that have an electrolyte solution containing a flammable organic solvent.

[0003] Patent Document 1 discloses an all-solid-state battery having two or more monopolar stacked battery units, the stacked battery units being configured by stacking a first current collector layer, a first active material layer, a solid electrolyte layer, a second active material layer, a second current collector layer, a second active material layer, a solid electrolyte layer, a first active material layer, and a first current collector layer in this order, and the adjacent first current collector layer and the first active material layer are bonded to each other with an adhesive. Patent Document 1 also discloses that the stacked battery units are constrained at a constraining pressure of 1.0 MPa or less. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2020-140932 A Summary of the Invention [Problem to be solved by the invention]

[0005] A solid-state battery that exhibits little increase in resistance even when repeatedly charged and discharged is desired. The present disclosure has been made in view of the above circumstances, and has as its main object to provide a solid-state battery that exhibits little increase in resistance even when repeatedly charged and discharged. [Means for solving the problem]

[0006] In order to solve the above problems, the present disclosure provides a solid-state battery including a plurality of electrode bodies stacked in a thickness direction, the electrode bodies having a positive electrode current collecting layer, a positive electrode active material layer, a solid electrolyte layer, a negative electrode active material layer, and a negative electrode current collecting layer, in that order in the thickness direction, and when the distance to the electrode bodies is measured along the short side direction from each of the front and back sides of the electrode bodies using a laser displacement meter, the waviness height of the electrode bodies is greater than the difference in thickness of the electrode bodies, and the number of wavinesses of the electrode body (per unit length) is 0.23 times / mm or more and 0.40 times / mm or less.

[0007] According to the present disclosure, the waviness height of the electrode body is greater than the difference in thickness of the electrode body, and further, the number of waviness of the electrode body is within a predetermined range, resulting in a solid-state battery with little increase in resistance even when repeatedly charged and discharged. Effect of the Invention

[0008] The present disclosure has an effect of providing a solid-state battery in which the increase in resistance is small even when the battery is repeatedly charged and discharged. [Brief description of the drawings]

[0009] [Figure 1] FIG. 1 is a schematic cross-sectional view illustrating a solid-state battery according to the present disclosure. [Diagram 2] 1 is a schematic cross-sectional view illustrating an electrode body according to the present disclosure. [Diagram 3] FIG. 2 is a schematic plan view illustrating measurement points for waviness measurement in the present disclosure. [Figure 4] FIG. 2 is a schematic diagram illustrating the swell height and the swell number in the present disclosure. [Diagram 5] 1 is a schematic cross-sectional view illustrating an electrode body according to the present disclosure. [Figure 6] 1 is a schematic cross-sectional view illustrating an electrode body according to the present disclosure. [Figure 7] 1 is a schematic cross-sectional view illustrating an electrode body according to the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] The solid-state battery according to the present disclosure will be described in detail below.

[0011] Fig. 1 is a schematic cross-sectional view illustrating a solid-state battery according to the present disclosure. Fig. 2 is a schematic cross-sectional view illustrating an electrode assembly according to the present disclosure. As shown in Fig. 1, the solid-state battery 100 has a thickness direction D T 2, the electrode body 10 includes a positive electrode current collecting layer 1, a positive electrode active material layer 2, a solid electrolyte layer 3, a negative electrode active material layer 4, and a negative electrode current collecting layer 5, which are stacked in a thickness direction D. T In this disclosure, the electrode body has the above-mentioned characteristics in this order. In addition, in this disclosure, a laser displacement meter is used to measure the distance to the electrode body from the front side and back side of the electrode body along the short side direction of the electrode body, and the "waviness height of the electrode body," "difference in thickness of the electrode body," and "number of waviness of the electrode body (per unit length)" are obtained. In this disclosure, the electrode body has a characteristic that the waviness height is greater than the difference in thickness of the electrode body. In addition, in this disclosure, the electrode body has a characteristic that the number of waviness (per unit length) is within a predetermined range.

[0012] According to the present disclosure, the waviness height of the electrode body is greater than the difference in thickness of the electrode body, and the number of waviness of the electrode body is within a predetermined range, resulting in a solid-state battery with little resistance increase even when repeatedly charged and discharged. As described above, Patent Document 1 discloses that a stacked battery unit is constrained at a constraining pressure of 1.0 MPa or less. When the constraining pressure is set to a low pressure, the constraining pressure becomes uneven in the surface direction in the adjacent electrode bodies. As a result, temperature unevenness occurs due to heat generation, and the resistance increase becomes large. In particular, when a charge / discharge test is performed under durability conditions, the resistance increase is large. In contrast, in the present disclosure, by imparting a predetermined waviness to the electrode body, the number of contact points becomes large in the adjacent electrode bodies, making it difficult for temperature unevenness due to heat generation to occur. As a result, a solid-state battery with little resistance increase even when repeatedly charged and discharged is obtained.

[0013] 1. Waviness measurement In the present disclosure, a laser displacement meter is used to measure the distance to the electrode body from the front side and back side of the electrode body along the short side direction, and the "waviness height of the electrode body," "difference in thickness of the electrode body," and "number of waviness of the electrode body (per unit length)" are obtained. These are measured as follows.

[0014] FIG. 3 is a schematic plan view for explaining measurement points for waviness measurement in the present disclosure. In FIG. 3, for convenience, the solid electrolyte layer is omitted. In FIG. 3, the area of ​​the positive electrode active material layer is smaller than the area of ​​the negative electrode active material layer in the thickness direction (depth direction of the paper), so the measurement points are determined based on the positive electrode active material layer. In this way, when the area of ​​the positive electrode active material layer and the area of ​​the negative electrode active material layer are different, the measurement points are determined based on the layer with the relatively smaller area. Next, as shown in FIG. 3, the positive electrode active material layer is divided into four equal parts along the short side direction of the electrode body (direction perpendicular to the transport direction), and the three line segments created by the equal division are measured.

[0015] Next, the distance to the electrode body is measured from the front side and the back side of the electrode body using a laser displacement meter. Specifically, when the electrode body is viewed in plan from the thickness direction, the distance to the electrode body is measured from the front side of the electrode body using a laser displacement meter, and the distance to the electrode body is measured from the back side of the electrode body using a laser displacement meter. The difference between these distances is continuously obtained along the short side direction of the electrode body, and the difference between the maximum value and the minimum value is defined as the "difference in thickness of the electrode body". In addition, the average of these distances is continuously obtained along the short side direction of the electrode body, and the difference between the maximum value and the minimum value is defined as the "waviness height of the electrode body". Specifically, as shown in FIG. 4, the average of the above distances is continuously obtained along the short side direction of the electrode body to create a waviness profile, and the difference between the maximum value and the minimum value is defined as the "waviness height of the electrode body". In addition, the slope is obtained every 5 μm for the waviness profile, and the number of times the sign changes is defined as the "waviness number of the electrode body". For example, in FIG. 4, the number of waviness of the electrode body is 7 times. In addition, the "number of undulations of the electrode body" is divided by the length of the measurement point to determine the "number of undulations of the electrode body (per unit length)."

[0016] One feature of the present disclosure is that the waviness height of the electrode body is greater than the difference in thickness of the electrode body. The difference between the two is, for example, 5 μm or more, and may be 10 μm or more, or 15 μm or more. On the other hand, the difference between the two is, for example, 50 μm or less. Another feature of the present disclosure is that the number of wavinesses (per unit length) of the electrode body is 0.23 times / mm or more and 0.40 times / mm or less. The number of wavinesses (per unit length) of the electrode body may be 0.31 times / mm or more and 0.38 times / mm or less.

[0017] 2. Electrode body The electrode body in the present disclosure has a positive electrode current collecting layer, a positive electrode active material layer, a solid electrolyte layer, a negative electrode active material layer, and a negative electrode current collecting layer in this order in the thickness direction. The electrode body preferably has a positive electrode active material layer, a solid electrolyte layer, and a negative electrode active material layer between a first current collecting layer and a second current collecting layer. The first current collecting layer and the second current collecting layer may be current collecting layers having the same polarity, or may be current collecting layers having polarities different from each other.

[0018] 5, the first current collecting layer and the second current collecting layer are both positive current collecting layers 1. That is, in the electrode body 10, the positive current collecting layer 1, the positive active material layer 2, the solid electrolyte layer 3, the negative active material layer 4, the negative current collecting layer 5, the negative active material layer 4, the solid electrolyte layer 3, the positive active material layer 2, and the positive current collecting layer 1 are arranged in a thickness direction D T In the electrode assemblies 10, they are arranged in this order. As shown in Fig. 5, in adjacent electrode assemblies 10, the first current collecting layer (positive electrode current collecting layer 1) in one electrode assemblies 10 is in contact with the second current collecting layer (positive electrode current collecting layer 1) in the other electrode assemblies 10. Although not particularly shown, in the electrode assemblies of the present disclosure, both the first current collecting layer and the second current collecting layer may be negative electrode current collecting layers. In this case, the polarity of each layer in the electrode assemblies 10 shown in Fig. 5 may be reversed.

[0019] 6, the first current collecting layer is a positive electrode current collecting layer 1, and the second current collecting layer is a negative electrode current collecting layer 5. That is, the electrode body 10 has the positive electrode current collecting layer 1, the positive electrode active material layer 2, the solid electrolyte layer 3, the negative electrode active material layer 4, and the negative electrode current collecting layer 5 arranged in a thickness direction D T 6, in adjacent electrode bodies 10, the first current collecting layer (positive electrode current collecting layer 1) of one electrode body 10 is in contact with the first current collecting layer (positive electrode current collecting layer 1) of the other electrode body 10. In addition, in adjacent electrode bodies 10, the second current collecting layer (negative electrode current collecting layer 5) of one electrode body 10 is in contact with the second current collecting layer (negative electrode current collecting layer 5) of the other electrode body 10.

[0020] 7, the first current collecting layer is the positive electrode current collecting layer 1, and the second current collecting layer is the negative electrode current collecting layer 5. That is, the electrode body 10 has the positive electrode current collecting layer 1, the positive electrode active material layer 2, the solid electrolyte layer 3, the negative electrode active material layer 4, and the negative electrode current collecting layer 5 arranged in a thickness direction D T 7, in adjacent electrode bodies 10, the first current collecting layer (positive electrode current collecting layer 1) of one electrode body 10 and the second current collecting layer (negative electrode current collecting layer 5) of the other electrode body 10 are in contact with each other.

[0021] The electrode assembly according to the present disclosure has a positive electrode current collecting layer, a positive electrode active material layer, a solid electrolyte layer, a negative electrode active material layer, and a negative electrode current collecting layer, in this order in the thickness direction.

[0022] The positive electrode active material layer contains at least a positive electrode active material, and may further contain at least one of a solid electrolyte, a conductive material, and a binder. Examples of the positive electrode active material include rock salt layer type active materials such as LiCoO2, spinel type active materials such as LiMn2O4, and olivine type active materials such as LiFePO4. Examples of the solid electrolyte include inorganic solid electrolytes such as sulfide solid electrolytes, oxide solid electrolytes, and halide solid electrolytes. Examples of the conductive material include carbon materials, and examples of the binder include fluorine-based binders. Examples of the material of the positive electrode current collecting layer include SUS and aluminum. Examples of the shape of the positive electrode current collecting layer include foil and mesh.

[0023] The negative electrode active material layer contains at least a negative electrode active material, and may further contain at least one of a solid electrolyte, a conductive material, and a binder. Examples of the negative electrode active material include metal active materials such as Li, Si, In, Al, and Sn, carbon active materials such as graphite, and oxide active materials such as lithium titanate. The solid electrolyte, conductive material, and binder are the same as those described above. Examples of the material of the negative electrode current collector layer include SUS and copper. Examples of the shape of the negative electrode current collector layer include a foil shape and a mesh shape. The solid electrolyte layer contains at least a solid electrolyte, and may further contain a binder. The solid electrolyte and binder are the same as those described above.

[0024] 3. Solid state battery The solid-state battery of the present disclosure includes a plurality of electrode bodies stacked in the thickness direction. The number of electrode bodies in the solid-state battery is 2 or more, may be 10 or more, or may be 50 or more. On the other hand, the number of electrode bodies in the solid-state battery is, for example, 150 or less.

[0025] The solid-state battery of the present disclosure may include an exterior body that seals the multiple electrode bodies stacked in the thickness direction. The exterior body may be a laminate-type exterior body or a case-type exterior body. The solid-state battery may also include a restraining tool that applies a restraining pressure to the multiple electrode bodies stacked in the thickness direction. The restraining pressure may be, for example, 0.1 MPa or more and 20 MPa or less, or may be 0.1 MPa or more and 1.0 MPa or less. The solid-state battery of the present disclosure has a small increase in resistance even when repeatedly charged and discharged, even when restrained at a low restraining pressure.

[0026] The solid-state battery in the present disclosure is typically a lithium-ion secondary battery. Examples of applications of the solid-state battery include power sources for vehicles such as hybrid electric vehicles (HEVs), plug-in hybrid electric vehicles (PHEVs), electric vehicles (BEVs), gasoline-powered vehicles, and diesel-powered vehicles. In particular, the solid-state battery is preferably used as a driving power source for hybrid electric vehicles (HEVs), plug-in hybrid electric vehicles (PHEVs), or electric vehicles (BEVs). The solid-state battery in the present disclosure may also be used as a power source for moving objects other than vehicles (e.g., railways, ships, and aircraft), and may also be used as a power source for electrical products such as information processing devices.

[0027] The present disclosure is not limited to the above-described embodiment. The above-described embodiment is merely an example, and any configuration that is substantially the same as the technical idea described in the claims of the present disclosure and that exhibits similar effects is included in the technical scope of the present disclosure. EXAMPLES

[0028] [Example 1] (Preparation of Positive Electrode Active Material Having a Coating Layer) Cathode active material (Li 1.15 Ni 1 / 3 Co 1 / 3 Mn 1 / 3The particles (main phase of which is O2) were coated with lithium niobate in an air atmosphere using a rolling fluidized coating device (manufactured by Powrex Corporation), and sintered in an air atmosphere. This resulted in a positive electrode active material having a coating layer of lithium niobate.

[0029] (Preparation of Positive Electrode Active Material Layer) A positive electrode active material, a sulfide solid electrolyte (Li2S-P2S5-based glass ceramic), a binder (PVDF), a conductive material (VGCF, manufactured by Showa Denko K.K.) and a dispersion medium were added to a polypropylene container, and the mixture was stirred for 30 seconds with an ultrasonic dispersion device (UH-50 manufactured by SMT K.K.). Next, the container was shaken for 3 minutes with a shaker (TTM-1 manufactured by Shibata Scientific Co., Ltd.), and further stirred for 30 seconds with an ultrasonic dispersion device. Next, the mixture was shaken for 3 minutes with a shaker to obtain a slurry. The obtained slurry was applied to a substrate (aluminum foil) by a blade method using an applicator. Next, the mixture was naturally dried, and further dried for 30 minutes on a hot plate at 100 ° C. This formed a positive electrode active material layer on the aluminum foil as a substrate. The amount of the slurry applied was adjusted so that the thickness of the positive electrode active material layer was 15 μm in a state after densification described later.

[0030] (Preparation of negative electrode) A negative electrode active material (LTO particles), a sulfide solid electrolyte (Li2S-P2S5-based glass ceramic), a binder (PVDF), a conductive material (VGCF, manufactured by Showa Denko K.K.) and a dispersion medium were added to a polypropylene container, and the mixture was stirred for 30 seconds with an ultrasonic dispersion device (UH-50 manufactured by SMT Corporation) to obtain a slurry. The obtained slurry was applied to the negative electrode current collector layer (copper foil) by the blade method using an applicator. Next, the mixture was naturally dried, and then dried for 30 minutes on a hot plate at 100°C. As a result, a negative electrode active material layer was formed on one surface of the negative electrode current collector layer (copper foil). A negative electrode active material layer was also formed on the other surface of the negative electrode current collector layer (copper foil) by the same operation. In this way, a negative electrode in which a negative electrode active material layer was arranged on both sides of the negative electrode current collector layer (copper foil) was obtained.

[0031] (Preparation of solid electrolyte layer) A sulfide solid electrolyte (Li2S-P2S5-based glass ceramic), a binder (BR), and a dispersion medium (heptane) were added to a polypropylene container, and the mixture was stirred for 30 seconds with an ultrasonic dispersion device (UH-50 manufactured by SMT Corporation). Next, the container was shaken for 30 minutes with a shaker (TTM-1 manufactured by Shibata Scientific Co., Ltd.), and further stirred for 30 seconds with an ultrasonic dispersion device. Next, the mixture was shaken for 3 minutes with a shaker to obtain a slurry. The obtained slurry was applied to a substrate (aluminum foil) by a blade method using an applicator. Next, the mixture was naturally dried, and further dried on a hot plate at 100°C for 30 minutes. As a result, a solid electrolyte layer was formed on the aluminum foil substrate.

[0032] (Preparation of positive electrode current collecting layer having carbon layer) A conductive material (acetylene black, AB) and a binder (acrylic binder) were weighed out so that the volume ratio of conductive material:binder was 40:60. Next, a dispersion medium (ethyl acetate) was added to these to obtain a slurry. The obtained slurry was applied onto a positive electrode current collector layer (aluminum foil) by a blade method using an applicator. Next, it was dried at 100°C for 1 hour. As a result, a positive electrode current collector layer having a carbon layer (thickness 2 μm) was obtained. The obtained positive electrode current collector layer was cut to 69.0 mm x 73.0 mm. The size of the carbon layer was 69.0 mm x 71.0 mm.

[0033] (Fabrication of solid-state batteries) A solid electrolyte layer was placed on each side of the negative electrode, and pressed at a linear pressure of 1.6 t / cm. Next, the base material (aluminum foil) was peeled off from the solid electrolyte layer to obtain a laminate X having a solid electrolyte layer A, a negative electrode, and a solid electrolyte layer B. Next, a positive electrode active material layer was placed on the surface of each of the solid electrolyte layer A and the solid electrolyte layer B, and pressed at a linear pressure of 1.6 t / cm. Next, the base material (aluminum foil) was peeled off from the positive electrode active material layer to obtain a laminate Y. Next, the laminate Y was pressed at a linear pressure of 5 t / cm to be densified. This resulted in a precursor laminate having a positive electrode active material layer A, a solid electrolyte layer A, a negative electrode, a solid electrolyte layer B, and a positive electrode active material layer B. Next, the positive electrode was laser trimmed to 70.0 mm x 70.0 mm, and the negative electrode was cut to 72.0 mm x 72.0 mm. Next, a positive electrode current collecting layer having a carbon layer was disposed on each of the positive electrode active material layer A and the positive electrode active material layer B, and pressed under conditions of 140°C and 5 MPa to obtain an electrode body. Twenty of the obtained electrode bodies were stacked, terminals were attached by welding, and the electrodes were enclosed in a laminate cell to obtain a solid-state battery.

[0034] [Examples 2 to 5 and Comparative Examples 1 to 3] An electrode assembly and a solid-state battery were obtained in the same manner as in Example 1, except that the conditions (roll rigidity, number of times) for densifying the laminate Y were changed.

[0035] [Comparative Example 4] A positive electrode current collecting layer having a carbon layer was obtained in the same manner as in Example 1, except that a carbon layer (thickness 2 μm) was formed on both sides of the positive electrode current collecting layer (aluminum foil). Next, an electrode body was obtained in the same manner as in Example 1, except that the positive electrode current collecting layer having a carbon layer was disposed on the positive electrode active material layer A of the laminate Y, and was not disposed on the positive electrode active material layer B. Twenty of the obtained electrode bodies were laminated, and a positive electrode current collecting layer having a carbon layer was disposed on the exposed positive electrode active material layer B, and a terminal was attached by welding, and the laminate cell was sealed to obtain a solid-state battery.

[0036] [evaluation] [Waviness measurement] Waviness measurements were performed on the electrode assemblies obtained in Examples 1 to 5 and Comparative Examples 1 to 4. The measurement conditions were as described above. The results are shown in Table 1. Note that, for the number of wavinesses (per unit length), the value for the line segment with the greatest number of wavinesses among the three line segments that were the measurement points was used.

[0037] (Resistance measurement) The resistance of the solid-state batteries obtained in Examples 1 to 5 and Comparative Examples 1 to 4 was measured. Specifically, CCCV charging (cut current: 0.01C) was performed at a current value of 1C to 2.95V, and then CCCV discharging (cut current: 0.01C) was performed at a current value of 1C to 1.50V. Next, CC charging and discharging were repeated 500 times under conditions of a current value of 45C, 1.5V to 2.8V, and 40°C (durability test). Next, the voltage of the solid-state battery was adjusted to 2.36V, and CC charging was performed under conditions of a current value of 2C and 10 seconds, and the resistance was calculated from the voltage change at that time. The results are shown in Table 1. The resistance values ​​in Examples 1 to 5 and Comparative Examples 1 to 4 are relative values ​​when the resistance value in Example 1 is set to 1.

[0038] [Table 1]

[0039] As shown in Table 1, it was confirmed that the resistance value was lower in Examples 1 to 5 than in Comparative Examples 1 to 4. In Comparative Example 1, the waviness height was smaller than the difference in thickness of the electrode bodies, and there were few contact points between adjacent electrode bodies, so it is presumed that the temperature unevenness due to heat generation increased, resulting in a high resistance value. In Comparative Example 2, although the waviness height was larger than the difference in thickness of the electrode bodies, the number of wavinesses was small, and it is presumed that the temperature unevenness due to heat generation could not be sufficiently suppressed, resulting in a high resistance value. On the other hand, in Comparative Example 3, since the number of wavinesses was large, peeling occurred between the layers constituting the electrode body with charging and discharging, resulting in a high resistance value. In Comparative Example 4, since there was only one positive electrode current collecting layer between the adjacent electrode bodies, peeling occurred between the positive electrode current collecting layer and the positive electrode active material layer with charging and discharging, resulting in a high resistance value. In this way, it was confirmed that a solid-state battery in which the waviness height of the electrode body is greater than the difference in thickness of the electrode body and further the number of wavinesses (per unit length) of the electrode body is within a specified range results in a battery in which the resistance increase is small even when the battery is repeatedly charged and discharged. [Explanation of symbols]

[0040] 1... Positive electrode current collecting layer 2... Positive electrode active material layer 3 … Solid electrolyte layer 4 … Negative electrode active material layer 5 ... Negative electrode current collecting layer 10 … Electrode body 100 … solid state battery

Claims

[Claim 1] A solid-state battery having a plurality of electrode bodies stacked in a thickness direction, the electrode body has a positive electrode current collecting layer, a positive electrode active material layer, a solid electrolyte layer, a negative electrode active material layer, and a negative electrode current collecting layer, in this order in the thickness direction; When the distance to the electrode body is measured from the front side and the back side of the electrode body along the short side direction of the electrode body using a laser displacement meter, The waviness height of the electrode body is greater than the difference in thickness of the electrode body, A solid-state battery, wherein the number of undulations (per unit length) of the electrode body is 0.23 times / mm or more and 0.40 times / mm or less.

Citation Information

Patent Citations

  • Method for manufacturing all-solid type secondary battery, and coating device

    JP2017183025A

  • All-solid-state battery and manufacturing method thereof

    JP2020140932A

  • Glass substrate and laminated substrate

    WO2016190303A1