Methods for producing organic-inorganic hybrid materials
The combination of ALD and MPI techniques provides a method for producing organic-inorganic hybrid materials with controlled hybridization, addressing the limitations of existing methods by enhancing durability and mechanical properties while maintaining flexibility and UV resistance.
Patent Information
- Application Number
- JP2021503861
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2018-07-24
- Filing Date
- 2019-07-24
- Publication Date
- 2024-11-20
- Estimated Expiration
- 2039-07-24
AI Technical Summary
Existing methods for producing organic-inorganic hybrid materials often result in physical mixing without synergistic interactions, lack control over hybridization levels, and are hindered by solvent molecules that degrade material properties, while current vapor phase techniques face challenges in selective impregnation and coating, leading to reduced mechanical properties and stability.
A method combining atomic layer deposition (ALD) and multi-pulsed vapor phase impregnation (MPI) techniques, allowing selective impregnation and coating by pulsing metal, metalloid, or semiconductor precursors with co-reactants to control the interaction between materials, ensuring the second precursor penetrates the surface without binding to it, forming impregnated layers with distinct properties.
This approach enables the production of organic-inorganic hybrid materials with enhanced durability and mechanical properties, maintaining flexibility and stability, and improves resistance to environmental factors like UV light.
Smart Images

Figure 0007587100000001 
Figure 0007587100000002 
Figure 0007587100000003
Abstract
Description
[Technical field]
[0001] FIELD OF THEINVENTION The present invention relates to the field of gas phase processing for the preparation of organic-inorganic hybrid materials. More specifically, the present invention relates to a method for the preparation of organic-inorganic hybrid materials, to organic-inorganic hybrid materials obtainable by said method, to organic-inorganic hybrid materials and to uses of said organic-inorganic hybrid materials. [Background technology]
[0002] Hybrid organic-inorganic materials are used in various applications due to their unique properties. These materials not only combine the characteristic inorganic properties of organic materials (flexibility, lightness, ease of processing, etc.) and inorganic materials (good thermal and chemical stability, electrical conductivity, etc.), but also sometimes surpass their individual properties or introduce new properties. The most common strategy to synthesize hybrid materials is based on wet chemical methods. However, these methods frequently result in physical mixing without synergistic interactions. Moreover, they do not allow sufficient control over the hybridization level. Moreover, solvent molecules can severely damage the properties of the resulting hybrid material by shielding the reaction or by simply generating cavities in the material that negatively affect the mechanical, electronic or optical properties. In contrast, solvent-free gas-phase processes are a good alternative to synthesize high-quality hybrid materials.
[0003] Atomic layer deposition (ALD) is a vapor-phase coating technique in which one or more precursors are Base material By sequentially delivering to the surface and allowing them to bond and react sequentially, thereby forming a coating with excellent thickness control, Base materialJW Elam et al. [Spatially controlled atomic layer deposition in porous materials, Applied Physics Letters 91, 243105 (2007)] reported a method for producing a thin film on porous substrates based on the ALD technique using two types of precursors. Base material It is described that the ALD technique deposits material into the film to produce a "striped coating." Base material It reacts only with the surface of Base material As a result, products obtained by ALD techniques are limited to layered structures.
[0004] A recently developed modification of ALD, the vapor phase impregnation (VPI) technique, involves the chemical Base material VPI produces hybrid organic-inorganic materials by allowing inorganic materials to not only adhere to the surface of the polymer but also to diffuse and react with the bulk of the polymer. VPI allows the introduction of inorganic materials into densely packed, ordered polymers that would not normally have inorganic properties. Methods based on VPI include multiple pulsed vapor phase impregnation (VPI), sequential vapor infiltration (SVI) and sequential impregnation synthesis (SIS) and are disclosed in several prior art documents. For example, US Patent Application 2018127870 (A1) describes the introduction of a precursor into a polymer. Base material A method of diffusion into the polymer, in which the polymer is exposed to the gas precursor for extended periods in a static atmosphere environment created in a reaction chamber, without the need for a continuous deposition process, is described. However, this technique also involves the use of impregnation, in addition to Base material A coating layer of the impregnating material is produced on the surface of the substrate.
[0005] The use of impregnation techniques followed by ALD has also been disclosed. For example, US Patent Application No. US2014346142 (A1) describes a method for producing patterned nanostructures having inorganic characteristics, comprising the steps of: Base material A method is described that comprises the sequential impregnation synthesis (SIS) of inorganic materials (alumina, titanium dioxide or ZnO) in a polymer and, optionally, a sequential ALD process for growing an inorganic coating on the surface. Gong et al. [Hydrophilic mechanical buffer layers and stable hydrophilic finishes, J. Va. Sic. Technol. A 30(1), Jan / Feb 202] describes a method for the preparation of polymers containing SiO2 and ZnO. Base material The method for producing a hydrophilic and stable polymeric material by impregnating and then coating the polymer with water is described. Base material was exposed to organometallic precursors for several hours, purged, exposed to water for several minutes, and then subjected to several ALD cycles and impregnated. Base material Nevertheless, the processing time is long and the combination of different materials is not well controlled with this technique. Moreover, during the impregnation process, the first precursor Base material non-specifically reacts with the functional groups available on both the surface and in the bulk of the coating, thus Base material This can be undesirable in some applications and can reduce the effectiveness of the impregnation.
[0006] Among technical polymers, Kevlar® (polyparaphenylene terephthalamide) has gained a reputation as a high-strength polymer and material of choice for mechanically demanding applications, such as personal safety, sporting goods and aviation. Kevlar's outstanding mechanical properties result from a highly ordered crystalline structure that develops during the extrusion of the polymeric fiber. In most of its applications, Kevlar is exposed to ultraviolet light, moisture and / or high temperatures. These environmental factors can disrupt its ordered structure and significantly affect the polymer's mechanical performance, thereby compromising its reliability.
[0007] Since its discovery in 1965, considerable efforts have been made with the aim of improving Kevlar's stability against UV radiation and high temperatures. It was found that embedding Kevlar fibers in resins prevented UV radiation from reaching the Kevlar fibers and prevented degradation, but the resulting composites consisted of heavy and stiff materials whose thermal stability was still rather low. Subsequent studies showed that coating Kevlar fibers with metal oxides had a positive effect on their mechanical properties and stability, preserving their light weight. However, due to the brittle nature of inorganic coatings, they can peel off from the fibers by mechanical treatment. Atomic layer deposition (ALD) has been shown to be effective in depositing metal oxides on polymer fibers to improve their mechanical properties. The inorganic films deposited by ALD are chemically bonded to the surface of the polymer, so their adhesion is high even when stretched. However, for UV protection of the fiber, very thick metal oxide films need to be deposited on top of the Kevlar, compromising its flexibility. Finally, Azpitarte et al. [Suppressing the Thermal and Ultraviolet Sensitivity of Kevlar by Infiltration and Hybridization with ZnO, Chem. Mater. 2017, 29, 10068-10074] found that the thermal and UV sensitivity of Kevlar can be suppressed by infiltration with ZnO via multiple pulsed infiltration (MPI). However, this method reduces the mechanical properties of the fibers. In particular, the toughness modulus of the fibers is reduced compared to the original Kevlar fibers.
[0008] In summary, prior art methods for producing organic-inorganic hybrid materials rely on impregnating materials. Base material To prevent the coating of different materials, Base materialHowever, it is not possible to selectively impregnate and coat organic-inorganic hybrid materials with improved stability, mechanical properties, and durability. Therefore, selective methods remain necessary. Furthermore, new and versatile methods for producing organic-inorganic hybrid materials with enhanced stability, mechanical properties, and durability are also needed. Summary of the Invention
[0009] Brief description of the invention The inventors of the present invention have discovered that Base material while avoiding the undesirable characteristic coating of the impregnating material on the surface of Base material Instead, the method of the present invention makes it possible to produce an organic-inorganic hybrid material that is impregnated with a first material and coated with a second material, so that the first (impregnated) material is Base material The surface of the second (coating) material is not coated. Base material directly interacts with the surface of the
[0010] The method is based on a combination of ALD and MPI techniques. For example, if a metal, semi-metal or semiconductor coating is required, the method consists of an ALD-type pulse of a metal, semi-metal or semiconductor-containing precursor, followed by an MPI-type pulse of a second metal, semi-metal or semiconductor-containing precursor, and a final MPI-type pulse of one or more counter precursors that react with the two immobilized metal, semi-metal or semiconductor-containing precursors. Thus, the first precursor pulsed in an ALD-type subcycle is Base material The first precursor reacts only with the surface functional groups of the first precursor and saturates them. This saturation prevents the binding of the second metal-, metalloid- or semiconductor-containing precursor during the subsequent MPI-type pulse. As a result, during this stage, the second precursor does not bind to the surface, but penetrates the surface and binds to further available functional groups in the subsurface region, resulting in Base material Finally, the pulsed counter precursor is beThe material reacts with both the metal, metalloid or semiconductor containing precursor to produce the coating and with the impregnated metal compound, which is another material.
[0011] Alternatively, two different counter precursors or co-reactants can be used. In this case, a first co-reactant that is selective for one of the first and second metal, metalloid or semiconductor-containing precursors is pulsed first. Then, a second co-reactant that reacts with the other unreacted metal, metalloid or semiconductor-containing precursor is pulsed. In this way, impregnation and coating layers of different properties can be formed.
[0012] The ALD / MPI combination according to the invention can also be used with organic molecules or organic molecule-containing coatings. For example, Base material or an ALD-type subcycle of a metal, semi-metal or semiconductor-containing precursor and an organic molecule that reacts with the surface functional group of Base material When exposed, the surface is saturated with a non-reactive layer, so the precursor used in the following MPI subcycles is Base material It does not bond to the surface of the Base material It reacts with the functional groups of.
[0013] This new method represents a breakthrough in the control of the synthesis of hybrid organic-inorganic materials. Base material This gives the user the opportunity to determine the choice of material to be coated with and the choice of another material to be impregnated with, Base material This approach is of great importance for the wide variety of applications of hybrid materials in various technical fields, since it overcomes the current limitations of such methods for producing hybrid materials.
[0014] The method of the present invention allows for a wide range of tunability of the properties of the resulting organic-inorganic hybrid material as a result of the variable selection of different materials for coating and impregnation. Materials with precisely tunable properties can thus be obtained. In particular, by following the method of the present invention, organic-inorganic hybrid materials with improved durability and mechanical properties have been obtained.
[0015] Thus, in a first aspect, the present invention provides a method for producing a pharmaceutical composition comprising the steps of: i) placing a polymer in the reaction chamber; Base material preparing a ii) pulsing a first metal, semi-metal or semiconductor precursor, or a mono- or oligo-functional organic molecule into the reaction chamber and then purging the reaction chamber, with no exposure time between the pulse and the purge; iii) pulsing a second metal, metalloid or semiconductor precursor into the reaction chamber, followed by an exposure time, and then purging the reaction chamber, wherein the exposure time between the pulse and the purge is 5 seconds or more; iv) pulsing a co-reactant into the reaction chamber, optionally followed by an exposure time, and then purging the reaction chamber, wherein the co-reactant reacts with the first metal, metalloid or semiconductor precursor if the mono- or oligo-functional organic molecule was not pulsed in step (ii) and / or the co-reactant reacts with the second metal, metalloid or semiconductor precursor; and v) optionally pulsing a co-reactant into the reaction chamber, optionally followed by an exposure time, and then purging the reaction chamber, where the co-reactant reacts with any unreacted first or second metal, metalloid or semiconductor precursors. 1. A method for producing an organic-inorganic hybrid material comprising: said co-reactant in step (iv) is different from said co-reactant in step (v); wherein the first metal, metalloid or semiconductor precursor is different from the second metal, metalloid or semiconductor precursor.
[0016] In a second aspect, the present invention relates to an organic-inorganic hybrid material obtainable by the method of the present invention.
[0017] In a third aspect, the present invention provides a method for producing a composition comprising the steps of: polymer Base material and, said polymer comprising a first metal, semimetal or semiconductor compound or moiety, or a mono- or oligo-functional organic molecule, or a mixture thereof; Base material a coating layer on the surface of the polymer comprising a second metal, semimetal or semiconductor compound or moiety; Base material The impregnated layer inside An organic-inorganic hybrid material comprising: the first metal, metalloid or semiconductor compound or component is different from the second metal, metalloid or semiconductor compound or component; and The coating layer is free of the second metal, metalloid or semiconductor compound or component with respect to the organic-inorganic hybrid material.
[0018] In a further aspect, the present invention relates to the use of the organic-inorganic hybrid materials of the present invention in the manufacture of flexible, lightweight polymer transistors, capacitors, optoelectronic devices, barriers, absorbers, personal safety equipment (e.g., bulletproof vests and military equipment), sporting goods, protective laminates, building materials, textiles, automotive materials and aircraft materials. [Brief description of the drawings]
[0019] [Figure 1]FIG. 1 shows TEM images of FIB-prepared cross sections of a) alumina-coated Kevlar (C-Al2O3), b) alumina-impregnated Kevlar (I-Al2O3), and c) alumina-coated, ZnO-impregnated Kevlar (TMA-pulsed), as well as d) EDS color map of the TMA-pulsed sample. [Diagram 2] FIG. 2 shows the mechanical properties [a) toughness, b) stress] of untreated Kevlar fibers, fibers impregnated (I-Al2O3) or coated (C-Al2O3) with Al2O3, and fibers impregnated with ZnO and coated with Al2O3 (TMA pulse). [Diagram 3] FIG. 3 shows SEM images of a) a Kevlar fiber before UV light exposure and b) the original Kevlar fiber, c) the coated Kevlar fiber, d) the impregnated Kevlar fiber, and e) the broken end of the coated and impregnated Kevlar fiber after UV light exposure. [Figure 4] Figure 4 shows the ATR-FTIR spectra in the fingerprint region (1200–800 cm-1) of Kevlar fibers before and after coating, impregnation, and coating + impregnation. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0020] Detailed Description of the Invention Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this disclosure belongs. As used herein, the singular forms "a," "an," and "the" include plural references unless the context clearly dictates otherwise.
[0021] Methods for producing organic-inorganic hybrid materials The present invention relates in a first aspect to a method for preparing an organic-inorganic hybrid material as defined above.
[0022] The term "optional" in step v) means that this step is included in the method if the co-reactant used in step iv) reacts with only one of the first and second precursors, i.e., is selective for one of them (and not the other), in which case a different co-reactant is pulsed in step v) to react with any unreacted first or second precursor.
[0023] An "unreacted" first or second precursor refers to a precursor that does not react with the co-reactant of step iv), i.e., a precursor for which the co-reactant of step iv) is not selective. In other words, if the co-reactant of step iv) is selective for (and therefore reactive with) the first precursor, then the unreacted precursor is a precursor of a second metal, metalloid or semiconductor. If the co-reactant of step iv) is selective for (and therefore reactive with) the second precursor, then the unreacted precursor is a precursor of a first metal, metalloid or semiconductor. The co-reactant of step v) does not need to be selective for the unreacted precursor, since other metal, metalloid or semiconductor precursors are no longer available for reaction with the co-reactant.
[0024] Step (iv) or step (v) of the method may independently have an exposure time after pulsing the co-reactant into the reaction chamber.
[0025] If the co-reactant of step iv) reacts only with the second precursor, then step iv) preferably includes an exposure time of 5 seconds or more, so that the co-reactant can react with the impregnated second precursor. If the co-reactant of step iv) reacts only with the first precursor, then no exposure time is required. Nevertheless, in certain embodiments, step iv) may include an exposure time, preferably 1 second or more, or 2 seconds or more, or 3 seconds or more, or 4 seconds or more, or preferably 5 seconds or more.
[0026] Similarly, if the co-reactant of step v) reacts with the second precursor, step v) preferably includes an exposure time of 5 seconds or more, so that the co-reactant can react with the impregnated second precursor. If the co-reactant of step v) reacts only with the first precursor, no exposure time is required. Nevertheless, in certain embodiments, step v) includes an exposure time, preferably 1 second or more, or 2 seconds or more, or 3 seconds or more, or 4 seconds or more, or preferably 5 seconds or more.
[0027] In certain embodiments, step iv) comprises pulsing a first co-reactant into the reaction chamber, followed by an exposure time, and then purging the reaction chamber, where the exposure time between the pulse and the purge is 5 seconds or more, and the first co-reactant reacts only with the precursor of the second metal, metalloid or semiconductor; and step v) comprises pulsing a second co-reactant into the reaction chamber, followed by an optional exposure time, and then purging the reaction chamber, where the second co-reactant reacts with the precursor of the first metal, metalloid or semiconductor, resulting in a coated or impregnated polymer. Base material get.
[0028] In another embodiment, step iv) comprises pulsing a first co-reactant into the reaction chamber, then optionally allowing an exposure time, then purging the reaction chamber, where the first co-reactant reacts only with the first metal, metalloid or semiconductor precursor, and step v) comprises pulsing a second co-reactant into the reaction chamber, then allowing an exposure time, then purging the reaction chamber, where the exposure time between the pulse and the purge is 5 seconds or more, where the second co-reactant reacts with the second metal, metalloid or semiconductor precursor, resulting in a coated impregnated polymer. Base material get.
[0029] Precursors that have selectivity for one co-reactant over the others are known in the art. Thus, one skilled in the art knows how to select appropriate first and second precursors, as well as co-reactants that selectively react with only the first or second precursor. For example, it is known that DEZ (zinc precursor) can react with sulfides (e.g., H2S) to form ZnS, but TMA (aluminum precursor) does not. Thus, the method using TMA-DEZ-H2S-H2O results in ZnS being impregnated and coated with Al2O3.
[0030] Preferably, the co-reactant of step iv) reacts with both the first and second metal, semi-metal or semiconductor precursors, i.e. is not selective for one of them, and therefore step v) is not performed. In that case, there is an exposure time of 5 seconds or more between the pulse and the purge, so that the co-reactant reacts with the first and second precursors. In this case, the coating layer and the impregnated layer are of the same nature, since the same co-reactant is used for the two precursors. Thus, in one embodiment, the method of the present invention comprises the following steps: i) placing a polymer in the reaction chamber; Base material preparing a ii) pulsing a first metal, metalloid or semiconductor precursor, or a mono- or oligo-functional organic molecule into the reaction chamber, and then purging the reaction chamber, with no exposure time between the pulse and the purge; iii) pulsing a precursor of a second metal, metalloid or semiconductor into the reaction chamber, followed by an exposure time, and then purging the reaction chamber, wherein the exposure time between the pulse and the purge is 5 seconds or more; and iv) The coreactant is pulsed into the reaction chamber, followed by an exposure period, and then the reaction chamber is purged to leave a coated and impregnated polymer. Base materialwherein the exposure time between the pulse and the purge is 5 seconds or more, the co-reactant reacts with a precursor of a first metal, metalloid or semiconductor (if the mono- or oligo-functional organic molecule is not pulsed), and the co-reactant reacts with a precursor of a second metal, metalloid or semiconductor. 1. A method comprising: The method, wherein the first metal, metalloid or semiconductor precursor is different from the second metal, metalloid or semiconductor precursor.
[0031] Each step of the method can be independently repeated a desired number of times, for example until a desired thickness (of coating and impregnation) is achieved, particularly 10 or more times, more particularly 100 or more times.
[0032] As described above, step ii) comprises the step of: Base material and saturating the surface of the polymer with the second metal, semimetal or semiconductor precursor of step iii). Base material Does not react with the surface of Base material Thus, in one embodiment, the polymer Base material Step ii) is carried out until the functional groups on the surface of are saturated, i.e., are no longer available for reaction with the second metal, metalloid or semiconductor precursor of step iii).
[0033] Thus, in certain embodiments, the coated polymer obtained after step ii) and after step iv) Base material The surface of is completely coated, preferably completely and uniformly coated.
[0034] A precursor of a metal, metalloid or semiconductor may be understood to be a precursor that includes a metal, metalloid or semiconductor component, hi one embodiment, it is a metal precursor.
[0035] The mono- or oligo-functional organic molecule is preferably a mono-functional organic molecule. In one embodiment, the metal, semi-metal or semiconductor precursor is a metal precursor and the mono- or oligo-functional organic molecule is a mono-functional organic molecule.
[0036] In a particular embodiment, step ii) comprises pulsing a precursor of the first metal, metalloid or semiconductor. Thus, in one embodiment, the method of the invention comprises the steps of: i) placing a polymer in the reaction chamber; Base material preparing a ii) pulsing a first metal, metalloid or semiconductor precursor into the reaction chamber and then purging the reaction chamber to produce a polymer coated with the first metal, metalloid or semiconductor precursor; Base material wherein there is no exposure time between the pulse and the purge; iii) pulsing a second metal, metalloid or semiconductor precursor into the reaction chamber, followed by an exposure period, and then purging the reaction chamber to produce a polymer coated with the first metal, metalloid or semiconductor precursor and impregnated with the second metal, metalloid or semiconductor precursor. Base material wherein the exposure time between the pulse and the purge is 5 seconds or more; and iv) pulsing the co-reactant into the reaction chamber, optionally followed by an exposure time, and then purging the reaction chamber, where the co-reactant reacts with the first and / or second metal, metalloid or semiconductor precursors; and v) Optionally, pulsing the co-reactant into the reaction chamber, then optionally providing an exposure time, then purging the reaction chamber to produce a polymer coated with the first metal, semi-metal or semiconductor compound or component and impregnated with the second metal, semi-metal or semiconductor compound or component. Base material wherein the co-reactant reacts with unreacted first or second metal, metalloid or semiconductor precursor to obtain The present invention relates to a method for producing a semiconductor device comprising the steps of:
[0037] Preferably, the co-reactant in step (iv) reacts with the first and second precursors and therefore step v) is not required.
[0038] In a specific embodiment, steps ii) to iv) are each repeated 1 to 1,000 times, preferably 50 to 1,000 times. In one embodiment, a cycle of steps ii) to iii) or ii) to iv) is repeated 1 to 1,000 times, preferably 50 to 1,000 times.
[0039] In a preferred embodiment, steps ii) to iv) are carried out continuously, and the cycle of steps ii) to iv) is repeated 1 to 1,000 times, preferably 10 to 1,000 times, more preferably 50 to 1,000 times, and even more preferably 50 to 500 times.
[0040] In the context of the present invention, the term "cycle" includes, for example, a sequence of steps of the method of the present invention, such as steps (ii) to (iv).
[0041] In one embodiment of this method, the mono- or oligo-functional organic molecule is coupled to a polymer coated with a first metal, semi-metal or semiconductor precursor. Base material In this case, one or more of the functional groups of the mono- or oligofunctional organic molecule reacts with a first metal, semimetal or semiconductor precursor to produce a non-reactive organic layer, which is in turn pulsed onto a polymeric substrate by reacting with a second metal, semimetal or semiconductor precursor. Base material Preferably, the mono- or oligo-functional organic molecule is a co-reactant of the first metal, metalloid or semiconductor precursor, i.e., it reacts with the first metal, metalloid or semiconductor precursor to produce the first metal, metalloid or semiconductor compound or component. In this case, the mono- or oligo-functional organic molecule is attached to a polymer coated with the first metal, metalloid or semiconductor precursor. Base material When pulsed onto a first metal, semimetal or semiconductor compound or component (polymer Base materiala polymer coated with a mono- or oligo-functional organic molecule (coated on the surface of a first metal, semi-metal or semiconductor compound or component); Base material is obtained.
[0042] Thus, in certain embodiments, the method comprises the steps of: i) placing a polymer in the reaction chamber; Base material preparing a ii) pulsing a first metal, metalloid or semiconductor precursor into the reaction chamber and then purging the reaction chamber to produce a polymer coated with the first metal, metalloid or semiconductor precursor; Base material wherein there is no exposure time between the pulse and the purge; ii') pulsing the mono- or oligo-functional organic molecule into the reaction chamber and then purging the reaction chamber to produce a polymer coated with the first metal, semi-metal or semiconductor compound or component and the mono- or oligo-functional organic molecule. Base material A process for obtaining There is no exposure time between the pulse and the purge, and reacting a mono- or oligo-functional organic molecule with a first metal, metalloid or semiconductor precursor; iii) pulsing the second metal, semi-metal or semiconductor precursor into the reaction chamber, followed by an exposure time, then purging the reaction chamber to produce a polymer coated with the first metal, semi-metal or semiconductor precursor and the mono- or oligo-functional organic molecules and impregnated with the second metal, semi-metal or semiconductor precursor. Base material wherein the exposure time between the pulse and the purge is 5 seconds or more; iv) pulsing the coreactant into the reaction chamber, followed by an exposure time, then purging the reaction chamber to produce a polymer coated with the first metal, semi-metal or semiconductor compound or component and the mono- or oligo-functional organic molecules and impregnated with the second metal, semi-metal or semiconductor compound or component. Base material A process for obtaining Pulseand purging, the exposure time being 5 seconds or more, and the co-reactant reacting with the precursor of the second metal, metalloid or semiconductor. The present invention relates to a method for producing a semiconductor device comprising the steps of:
[0043] In a specific embodiment, steps ii) to iv) are each repeated 1 to 1,000 times, preferably 50 to 1,000 times. In one embodiment, a cycle of steps ii) to iii) or ii) to iv) is repeated 1 to 1,000 times, preferably 50 to 1,000 times. In one embodiment, steps ii) to iv) are performed continuously, and a cycle of steps ii) to iv) is repeated 1 to 1,000 times, preferably 10 to 1,000 times, more preferably 50 to 1,000 times, and even more preferably 50 to 500 times. In another embodiment, steps ii) to ii') are performed continuously, and a cycle of steps ii) to ii') is repeated 1 to 1,000 times, preferably 10 to 1,000 times, more preferably 10 to 500 times, and even more preferably 50 to 500 times, and then step iii) is performed. In one embodiment, steps iii) and iv) are repeated, separately or consecutively, 1 to 1,000 times, preferably 10 to 1,000 times, more preferably 50 to 1,000 times, and even more preferably 50 to 500 times.
[0044] In another alternative of the method of the invention, step ii) comprises polymerizing a mono- or oligo-functional organic molecule. Base material In this case, one or more of the functional groups of the mono- or oligo-functional organic molecule are pulsing with a polymer. Base material to form a non-reactive organic layer, and a second metal, semi-metal or semiconductor precursor is added to the polymer. Base material Thus, in another embodiment, the process of the present invention comprises the steps of: i) placing a polymer in the reaction chamber; Base material preparing a ii) pulsing the mono- or oligo-functional organic molecule into the reaction chamber and then purging the reaction chamber to form a polymer coated with the mono- or oligo-functional organic molecule; Base materialwherein there is no exposure time between the pulse and the purge; iii) pulsing the second metal, metalloid or semiconductor precursor into the reaction chamber, followed by an exposure period, then purging the reaction chamber to yield a polymer coated with mono- or oligo-functional organic molecules and impregnated with the second metal, metalloid or semiconductor precursor; Base material wherein the exposure time between the pulse and the purge is 5 seconds or more; iv) Optionally, a co-reactant is pulsed into the reaction chamber, followed by an exposure period, and then purging the reaction chamber to produce a polymer coated with mono- or oligo-functional organic molecules and impregnated with a second metal, semi-metal or semiconductor compound or component. Base material wherein the exposure time between the pulse and the purge is 5 seconds or more, and the co-reactant reacts with the precursor of the second metal, metalloid or semiconductor. The present invention relates to a method for producing a semiconductor device comprising the steps of:
[0045] Each of steps ii) to iv) is repeated 1 to 1,000 times, preferably 50 to 1,000 times. In one embodiment, a cycle of steps ii) to iii) or ii) to iv) is repeated 1 to 1,000 times, preferably 50 to 1,000 times. In one embodiment, steps ii) to iv) are performed continuously, and a cycle of steps ii) to iv) is repeated 1 to 1,000 times, preferably 10 to 1,000 times, more preferably 50 to 1,000 times, and even more preferably 50 to 500 times. In another embodiment, steps ii) to ii') are performed continuously, and a cycle of steps ii) to ii') is repeated 1 to 1,000 times, preferably 10 to 1,000 times, more preferably 10 to 500 times, and even more preferably 50 to 500 times, and then step iii) is performed. In one embodiment, steps iii) and iv) are repeated, separately or consecutively, 1 to 1,000 times, preferably 10 to 1,000 times, more preferably 50 to 1,000 times, and even more preferably 50 to 500 times.
[0046] Certain preferred embodiments disclosed herein below apply to all of the above methods of the invention.
[0047] In one embodiment, steps (ii) to (iv) are carried out continuously, and the cycle of steps (ii) to (iv) is repeated 1 to 1,000 times, preferably 10 to 1,000 times, more preferably 10 to 500 times, and even more preferably 50 to 500 times. In this case, the obtained Base material shows a coating of a first material, impregnated with a second material.
[0048] In another embodiment, step ii) and / or ii') are carried out once, and then steps (iii) and (iv) are carried out, and the cycle of steps (iii) to (iv) is repeated 1 to 1,000 times, preferably 10 to 1,000 times, more preferably 10 to 500 times, and even more preferably 50 to 500 times. In this case, the obtained Base material shows substantially no coating of the first material. A single coating of a first metal, metalloid or semiconductor precursor and / or mono- or oligo-functional organic molecule may be sufficient to inhibit coating with a second metal, metalloid or semiconductor precursor.
[0049] In the context of the present invention, "polymer Base material The term refers to organic-based polymeric materials that can be coated and impregnated, such as polymers, biopolymers, hybrid materials, layered structures and combinations thereof.
[0050] In one embodiment, the polymer Base material is an organic-based polymer. In an embodiment, it may be selected from a homopolymer, a copolymer, a multicomponent polymer, or a combination thereof.
[0051] In an embodiment of the present invention, the polymer of the present invention Base material contains an organic polymer having one or more functional groups selected from hydroxyl, ether, amino, ketone, halogen, carboxylic acid, ester, amide, acid halide, imide, imine, acrylate, terephthalate, alkenyl, and aryl.
[0052] In certain embodiments, the polymer Base material is selected from polyamides, polyamines, polyimides, polyalkylenes, polyacrylates, polyalcohols, polyethers, polyesters, polyvinyls, polypyrroles, polythiophenes, polystyrenes and polyketones. Base material is selected from polyamides, polyamines, polyimides, polyalkylenes, polyacrylates, polymethacrylates, polyalcohols, polyethers, polyesters, polyvinyls, halopolymers, polypyrroles, polythiophenes, polystyrenes and polyketones, preferably selected from aromatic polyamides, nylons, polyanilines, polystyrenes, polypropylenes, poly(butyl methacrylate), poly(propyl methacrylate), poly(ethyl methacrylate), poly(methyl methacrylate), polybutylene terephthalate, polyethylene terephthalate, polyvinyl alcohols, polyvinyl chloride, polytetrafluoroethylene, polychlorotrifluoroethylene, polyimides, polyetherimides and polyetheretherketones. More preferably, it is selected from aromatic polyamides (aramids), such as para-aramid and meta-aramid polymers. Even more preferably, it is polyparaphenylene terephthalamide.
[0053] In one embodiment, the polymer Base material is Kevlar or Kevlar fiber.
[0054] In another particular embodiment, the polymer Base material may be selected from homopolymers and copolymers, such as alternating copolymers, block copolymers and random copolymers.
[0055] In another embodiment, the polymer Base materialAlternatively, it may be an inorganic-organic hybrid polymer, or a blend of an organic polymer and an inorganic-organic hybrid material. The inorganic-organic hybrid polymer can be produced by conventional methods from the prior art.
[0056] In one embodiment, the biopolymer is selected from polypeptides, nucleic acids, and polysaccharides, such as starch, pectin, chitosan, alginates, carrageenan, cellulose and cellulose derivatives (eg, methylcellulose, hydroxymethylcellulose, hydroxypropylcellulose, carboxymethylcellulose).
[0057] In certain embodiments, the polymers of the present invention Base material comprises one or more layers, for example one or more layers of different polymers.
[0058] In another embodiment, the polymer of the present invention Base material is porous, preferably having macroporosity or microporosity.
[0059] In certain embodiments, the polymers of the present invention Base material is a sphere, a cylinder, Lamella It may be in the form of a lamella, a thin film, a fiber or a bicontinuous structure. Preferably, it is a polymer fiber.
[0060] In one embodiment, the polymer Base material In another embodiment, the polymer has a thickness of 1 to 250 μm, preferably 1 to 100 μm, and more preferably 1 to 50 μm. Base material has a length of 0.5 to 40 cm, preferably between 0.5 to 20 cm, more preferably 1 to 10 cm, and even more preferably 1 to 8 cm.
[0061] In one embodiment, the polymer Base materialIn another embodiment, the polymer fiber has a diameter of 1 to 100 μm, preferably 1 to 50 μm, more preferably 2 to 30 μm, and even more preferably 5 to 20 μm. Base material is a polymer fiber having a diameter of 1 to 100 μm, preferably 2 to 20 μm, and a length of 0.5 to 40 cm, preferably 0.5 to 10 cm.
[0062] Non-limiting examples of discrete fibers suitable for the present invention include straight fibers, crimped fibers, or roving fibers.
[0063] In certain embodiments, the reaction chamber of the present invention is arranged for the reaction of a gas with a surface. Preferably, the term "reaction chamber" refers to a chemical vapor processing apparatus known in the art, such as a chemical vapor deposition (CVD), vapor phase impregnation (VPI) or atomic layer deposition (ALD) apparatus chamber. Preferably, the reaction chamber of the present invention is an atomic layer deposition reaction chamber, such as those available from Cambridge Nanotech, Inc., Cambridge, Massachusetts. In one embodiment, the reaction chamber is an atomic layer deposition chamber.
[0064] All reagents used in the method of the present invention (metal, semi-metal or semiconductor precursors, mono- or oligo-functional organic molecules, co-reactants, purge gases) are injected or pulsed into the reaction chamber in gaseous form.
[0065] In the context of the present invention, the term "pulse" relates to the period during which a compound (e.g., a metal, semimetal or semiconductor precursor; an organic molecule; water; or any other reactant or co-reactant) is introduced into the reaction chamber. In this sense, the term "pulse" refers to the introduction of a compound into the reaction chamber of the present invention for a (short) period of time. The pulse time can be adapted by the expert in the art depending on the precursor, the type of reactor, the volume of the chamber, etc., and lasts from a few hundredths of a second to a few seconds.
[0066] In certain embodiments, the pulse times are independently 0.01 to 20 seconds, preferably 0.01 to 10 seconds, more preferably 0.01 to 5 seconds, and even more preferably 0.01 to 2 seconds. In further embodiments, the pulse times are independently 0.01 to 1 second, preferably 0.02 to 0.50 seconds, more preferably 0.02 to 0.15 seconds, and even more preferably 0.05 to 0.1 seconds.
[0067] In the context of the present invention, the term "purging" refers to a period during which unreacted compounds in the reaction chamber are removed. The purge time can be adapted by the expert in the art depending on the precursor, the characteristics of the reaction chamber, the pulse time, etc., and may last from a few seconds to a few minutes per cycle. In a particular embodiment, the purge of the present invention is performed by flowing a purge gas into the reaction chamber or by evacuating the reaction chamber by vacuum, preferably by flowing an inert purge gas. In one embodiment, the inert purge gas is selected from nitrogen, argon, helium, neon and mixtures thereof, preferably it is nitrogen.
[0068] In certain embodiments, the purge times are independently between 1 and 300 seconds, preferably between 1 and 200 seconds, more preferably between 5 and 200 seconds, and even more preferably between 5 and 200 seconds. In further embodiments, the pulse times are independently between 5 and 150 seconds, preferably between 5 and 90 seconds, more preferably between 10 and 60 seconds, and even more preferably between 20 and 40 seconds.
[0069] In the context of the present invention, the term "exposure time" refers to the time during which a static or non-flowing atmosphere is created in the chamber and during which a compound or mixture of compounds previously introduced into the chamber (by one or more pulses) is absorbed by the polymer. Base material The exposure time is related to the period or "retention" time during which the polymer is able to diffuse beneath the surface of the polymer. Base material Properties, Precursors, Polymers Base materialIt can be adapted by the expert in the art depending on the density of the powder, the desired impregnation depth, etc. It may last from a few seconds to a few minutes. In special cases, it may last for several hours. As used in the art, exposure time generally refers to the time between the end of the pulse and the start of the purge.
[0070] In a particular embodiment, the exposure time is 5 seconds or more, preferably 5 to 300 seconds, more preferably 1 to 200 seconds, more preferably 5 to 200 seconds, and even more preferably 5 to 200 seconds. In a further embodiment, the exposure time is 5 to 150 seconds, preferably 5 to 90 seconds, more preferably 10 to 60 seconds, and even more preferably 20 to 40 seconds.
[0071] The expression "no exposure time between pulse and purge" or "without exposure time between pulse and purge" means performing step ii) or ii') without a time delay between pulse and purge, i.e. performing the pulse immediately or immediately after the purge. Preferably, the time interval between pulse and purge is zero or substantially zero seconds, i.e. as close to zero as possible according to the tolerances of the system used to perform the method. In a particular embodiment, it means that the exposure time between pulse and purge is less than 0.01 seconds, preferably less than 0.001 seconds.
[0072] Monofunctional or oligofunctional organic molecules, i.e., organic molecules with one or several functional groups, can be used in all embodiments of the present invention, as long as the non-binding portion is inert (i.e., does not react) with respect to the second metal, metalloid or semiconductor precursor. Suitable monofunctional or oligofunctional organic molecules can be determined by those skilled in the art taking into account the polymer substrate, the first precursor and the second precursor used. In one embodiment, the monofunctional or oligofunctional organic molecule does not contain a metal, metalloid or semiconductor component. Preferably, the monofunctional or oligofunctional organic molecule is a monofunctional organic molecule.
[0073] In one embodiment, the mono- or oligo-functional organic molecule of step (ii) or (ii') is an organic molecule having one or more functional groups selected from hydroxyl, amino, carboxylic acid, ester, amide, silane, thiol, epoxy, nitro and acid halide. Preferably, it is an organic molecule having 1 to 3 functional groups, more preferably, it is difunctional (having 2 functional groups) or monofunctional (having 1 functional group), more preferably, it is a monofunctional organic molecule.
[0074] In a more particular embodiment, the mono- or oligo-functional organic molecule of step (ii) or (ii') is an aliphatic or aromatic mono- or oligo-functional organic molecule, preferably an aliphatic molecule. In a preferred embodiment, the mono- or oligo-functional organic molecule is a C1-C substituted with at least one functional group selected from hydroxyl, amino, carboxylic acid, sulfonic acid, ester, ether, amide, halogen, silane, thiol, halide, epoxy, acid halide. 12 Alkanes, perfluorinated compounds or C6-C 18 In one embodiment, the mono- or oligofunctional organic molecule is a C-C 12 It is an alkanol.
[0075] In another embodiment, the mono- or oligo-functional organic molecule is a mono- or oligo-functional perfluoro compound, preferably a perfluoro C1-C 12 Alkanes, Perfluorinated C2-C 12 Alkenes or Perfluoro C6-C 18 It's Arene.
[0076] In one embodiment, the monofunctional or oligofunctional organic molecule is a monofunctional organic molecule, preferably an organic molecule having one functional group selected from hydroxyl, amino, carboxylic acid, ester, amide, silane, thiol, epoxy, nitro and acid halide. In one embodiment, it is an aliphatic or aromatic monofunctional organic molecule, preferably an aliphatic molecule. In a preferred embodiment, the monofunctional organic molecule is a C1-C substituted with one functional group selected from hydroxyl, amino, carboxylic acid, sulfonic acid, ester, ether, amide, halogen, silane, thiol, halide, epoxy, acid halide. 12 Alkanes, perfluorinated compounds or C6-C 18 In one embodiment, the monofunctional organic molecule is a C-C 12 In another embodiment, the monofunctional organic molecule is a monofunctional perfluoro compound, preferably a perfluoro C1-C 12 Alkanes, Perfluorinated C2-C 12 Alkenes or Perfluoro C6-C 18 The first metal, semi-metal or semiconductor precursor or mono- or oligo-functional organic molecule of step (ii) of the present invention is preferably a polymer, more preferably a perfluorocarboxylic acid, such as trifluoroacetic acid, heptafluorobutyric acid, pentafluorobenzoic acid, perfluorooctanoic acid or perfluorononanoic acid. Base material Thus, in certain embodiments, the first metal, semimetal or semiconductor precursor or mono- or oligo-functional organic molecule of step (ii) can react with the functional groups of the surface. Base material The functional groups on the surface of the
[0077] In one embodiment, the coated polymer obtained after step (ii) Base material is a polymer Base materialThe surface of the substrate is provided with a coating layer of a first metal, semimetal or semiconductor precursor, or a mono- or oligo-functional organic molecule. Preferably, the first metal, semimetal or semiconductor precursor, or the mono- or oligo-functional organic molecule is a polymer. Base material More preferably, the first metal, metalloid or semiconductor precursor, or the mono- or oligo-functional organic molecule is bonded to a functional group on the surface of the polymer. Base material It is bonded to all functional groups on the surface.
[0078] Polymer after step (ii) or (ii') Base material Complete saturation of the surface of the polymer can be achieved, for example, by using an excess of a first metal, semimetal or semiconductor precursor and / or a mono- or oligo-functional organic molecule. Base material In steps (ii) and (ii'), no exposure time is allocated between the pulse and the purge, so that the unreacted excess of the polymer Base material Alternatively, the polymer Base material The saturation of the surface of the polymer may be carried out prior to carrying out step (iii). Base material This can be achieved by repeating steps (ii) and / or (ii') several times until all functional groups on the surface of the catalyst have been reacted.
[0079] In a specific embodiment, step (ii) or a cycle of steps (ii) to (ii') is repeated at least twice, preferably at least five times. Preferably, it is repeated 1 to 1000 times, more preferably 5 to 500 times, and even more preferably 10 to 200 times. Thus, by repeating step (ii), the polymer Base material The surface of is saturated with a first metal, semi-metal or semiconductor precursor and / or mono- or oligo-functional organic molecules.
[0080] When a first metal, metalloid or semiconductor precursor is used in step (ii), the thickness of the coating layer can be controlled, for example, by controlling the number of repetitions of the cycle of steps (ii)-(iv) or (ii)-(v).
[0081] The first metal, metalloid or semiconductor precursor is different from the second metal, metalloid or semiconductor precursor, more preferably the metal in the first metal, metalloid or semiconductor precursor is different from the metal in the second metal, metalloid or semiconductor precursor.
[0082] In certain embodiments, the first and second metal, metalloid or semiconductor precursors of the present invention are independently selected from metal halides, metal alkoxides, metal alkyls, metal diketonates, metal alkylamides, metal amidinates, metal aryls and cyclopentadienyl metals, preferably independently selected from metal halides and metal alkoxides, more preferably selected from metal alkoxides.
[0083] In the context of the present invention, the term "metal" refers to its commonly understood in the art and includes earth metals, alkaline earth metals, transition metals, lanthanides, actinides and other metals (e.g., B, Al, Ga, In, Tl, Nh, Sn, Pb, Fl, Me and Lv). In the context of the present invention, the term "metalloid" or metalloid refers to its commonly understood in the art and includes As, Sb, Te, Se and Bi. In the context of the present invention, the term "semiconductor" refers to its commonly understood in the art and includes Ge and Si.
[0084] In certain embodiments, the first and second metal, metalloid or semiconductor precursors of the present invention independently comprise a metal selected from Al, Zn, Si, Ti, W, Sb, As, Ba, Bi, B, Cd, Ca, Ce, Cr, Co, Cu, Er, Eu, Gd, Ga, Ge, Hf, Fe, La, Mg, Mn, Mo, Ni, Nb, Os, Pt, Pr, Re, Rh, Ru, Sm, Se, Si, Sr, Ta, Te, Tb, Tm, Sn, Ti, W, V, Yb, Y, Zr, Pd, In, Ir and Li, preferably selected from Al, Zn, Si, Ti and In.
[0085] Non-limiting examples of first and second metal, semimetal or semiconductor precursors suitable for the present invention include trimethylaluminum, triisobutylaluminum, aluminum tris(2,2,6,6-tetramethyl-3,5-heptanedionate), tris(dimethylamido)aluminum, aluminum trichloride, triphenylantimony, tris(dimethylamido)antimony, antimony pentachloride, triphenylarsine, triphenylarsine oxide, barium bis(2,2,6,6-tetramethyl-3,5-heptanedionate), tris(dimethylamido)aluminum, ... onate), barium nitrate, bis(pentamethylcyclopentadienyl)barium, bis(triisopropylcyclopentadienyl)barium, bis(aceto-O)triphenylbismuth, tris(2-methoxyphenyl)bismuthine, triisopropylborate, triphenylborane, tris(pentafluorophenyl)borane, cadmium acetylacetonate, dimethylcadmium, calcium bis(2,2,6,6-tetramethyl-3,5-heptanedionate), tris(tetramethylcyclopentadienyl) ) cerium(III), bis(cyclopentadienyl)chromium(II), bis(pentamethylcyclopentadienyl)chromium(II), chromium(III) tris(2,2,6,6-tetramethyl-3,5-heptanedionate), bis(cyclopentadienyl)cobalt(II), bis(pentamethylcyclopentadienyl)cobalt(II), bis(ethylcyclopentadienyl)cobalt(II), cobalt tris(2,2,6,6-tetramethyl-3,5-heptanedionate), copper bis(2,2,6,6-tetramethyl-3,5-heptanedionate), copper bis(6,6,7,7,8,8,8,-heptafluoro-2,2-dimethyl-3,5-octanedionate), copper hexafluoroacetylacetonate, bis(N,N'-diisopropylacetamidinato)copper(I), erbium tris(2,2,6,6-tetramethyl-3,5-heptanedionate), tris(N,N-bis(trimethylsilyl)amido)europium(III), tris(tetramethylcyclopentadienyl)europium(III), tris(N,N-bis(trimethylsilyl)amido)gadolinium(III), tris(tetramethylcyclopentadienyl)gadolinium(III), tris(cyclopentadienyl)gadolinium(III), triethylgallium, trimethylgallium, tris(dimethylamido)gallium(III), hexamethyldigermanium(IV), tetramethylgermanium, tributylgermanium hydride, triethylgermanium hydride, triphenylgermanium hydride, bis(methyl-η, 5-cyclopentadienyl)methoxymethylhafnium, bis(trimethylsilyl)amidohafnium(IV) chloride, dimethylbis(cyclopentadienyl)hafnium(IV), hafnium(IV) tert-butoxide, hafnium isopropoxide, ethrakis(diethylamido)hafnium, ethrakis(dimethylamido)hafnium, tetrakis(ethylmethylamido)hafnium(IV), [1,1'-bis(diphenylphosphino)ferrocene]tetracarbonylmolybdenum(0), bis(pentamethyl Cyclopentadienyl)iron(II), 1,1'-diethylferrocene, iron(0) pentacarbonyl, iron(III) tris(2,2,6,6-tetramethyl-3,5-heptanedionate), cyclohexadieneiron tricarbonyl, ferrocene, lanthanum(III) isopropoxide, tris(N,N-bis(trimethylsilyl)amido)lanthanum(III), tris(cyclopentadienyl)lanthanum(III), tris(tetramethylcyclopentadienyl)lanthanum(III), tris(isopropylcyclopentadiene) (bicyclo[2.2.1]hepta-2,5-diene)tetracarbonylmolybdenum(0), bis(cyclopentadienyl)lanthanum(III), bis(cyclopentadienyl)magnesium(II), bis(pentamethylcyclopentadienyl)magnesium, bis(pentamethylcyclopentadienyl)manganese(II), bis(tetramethylcyclopentadienyl)manganese(II), bromopentacarbonylmanganese(I), cyclopentadienylmanganese(I) tricarbonyl, manganese(0) carbonyl, (bicyclo[2.2.1]hepta-2,5-diene)tetracarbonylmolybdenum(0), bis(cyclopentadienyl) (aryl)molybdenum(IV) dichloride, cyclopentadienylmolybdenum(II) tricarbonyl, molybdenum hexacarbonyl, (propylcyclopentadienyl)molybdenum(I) tricarbonyl dimer, molybdenum hexafluoride, allyl(cyclopentadienyl)nickel(II), bis(cyclopentadienyl)nickel(II), bis(ethylcyclopentadienyl)nickel(II), bis(triphenylphosphine)nickel(II) dichloride, nickel(II) bis(2,2,6,6-tetramethyl-3,5-heptanedionate), nickel(II) acetylacetonate, bis(cyclopentadienyl)niobium(IV) dichloride, niobium pentafluoride, niobium pentachloride, niobium pentaethoxide, niobium(V) iodide, triosmium dodecacarbonyl, trimethyl(methylcyclopentadienyl)platinum(IV), praseodymium(III) hexafluoroacetylacetonate, dirhenium decacarbonyl, (acetylacetonato)(1,5-cyclooctadiene)rhodium(I), bis(cyclopentadienyl) )ruthenium(II), bis(ethylcyclopentadienyl)ruthenium(II), triruthenium dodecacarbonyl, tris(tetramethylcyclopentadienyl)samarium(III), dimethyl selenide, (3-aminopropyl)triethoxysilane, N-sec-butyl(trimethylsilyl)amine, chloropentamethyldisilane, 1,2-dichlorotetramethyldisilane, 1,3-diethyl-1,1,3,3-tetramethyldisilazane, dodecamethylcyclohexasilane, hexamethyldisilane, hexa Methyldisilazane, 2,4,6,8,10-pentamethylcyclopentasiloxane, pentamethyldisilane, silicon tetrabromide, silicon tetrachloride, tetraethylsilane, 2,4,6,8-tetramethylcyclotetrasiloxane, 1,1,2,2-tetramethyldisilane, N,N',N''-tri-tert-butylsilanetriamine, tris(tert-butoxy)silanol, tris(tert-pentoxy)silanol, disilane, strontium tetramethylheptanedionate, bis(pentamethylcyclopenta dienyl)strontium, pentakis(dimethylamino)tantalum(V), tantalum(V) ethoxide, tris(diethylamido)(tert-butylimido)tantalum(V), tris(ethylmethylamido)(tert-butylimido)tantalum(V), tellurium tetrachloride, terbium(III) tris(2,2,6,6-tetramethyl-3,5-heptanedionate), tris(cyclopentadienyl)terbium(III), tris(tetramethylcyclopentadienyl)terbium(III), tris(N,N-bis(trimethylsilyl)amido)thulium(III), tris(cyclopentadienyl)thulium(III), bis[bis(trimethylsilyl)amino]tin(II), hexaphenylditin(IV), tetraallyltin, tetrakis(diethylamido)tin, tetrakis(dimethylamido)tin, tin(IV) iodide, tetramethyltin, tetravinyltin, tin(II) acetylacetonate, trimethyl(phenylethynyl)tin, trimethyl(phenyl)tin, tetrakis(diethylamido)titanium(IV), Tetrakis(dimethylamido)titanium(IV), tetrakis(ethylmethylamido)titanium(IV), titanium(IV) diisopropoxide bis(2,2,6,6-tetramethyl-3,5-heptanedionate), titanium(IV) isopropoxide, titanium tetrachloride, bis(tert-butylimino)bis(tert-butylamino)tungsten, bis(tert-butylimino)bis(dimethylamino)tungsten(VI), bis(cyclopentadienyl)tungsten(IV) dichloride, bis(cyclopentadienyl)tungsten Tungsten(IV), tungsten hexafluoride, bis(isopropylcyclopentadienyl)tungsten(IV), tetracarbonyl(1,5-cyclooctadiene)tungsten(0), triaminetungsten(IV) tricarbonyl, tungsten hexacarbonyl, bis(cyclopentadienyl)vanadium(II), bis(ethylcyclopentadienyl)vanadium(II), vanadium(V) oxytriisopropoxide, tris(N,N-bis(trimethylsilyl)amido)ytterbium(III), tris( cyclopentadienyl)ytterbium(III), tris(N,N-bis(trimethylsilyl)amido)yttrium, tris(butylcyclopentadienyl)yttrium(III), tris(cyclopentadienyl)yttrium(III), yttrium 2-methoxyethoxide, yttrium(III) tris(isopropoxide), yttrium(III) tris(2,2,6,6-tetramethyl-3,5-heptanedionate), bis(pentafluorophenyl)zinc, bis(2,2,6,6-tetramethyl-3,5-heptanedione)zinc(II), diethylzinc, diphenylzinc, bis(cyclopentadienyl)zirconium(IV), bis(cyclopentadienyl)dimethylzirconium, bis(methyl-η), 5 -cyclopentadienyl)methoxyethylzirconium, dimethylbis(pentamethylcyclopentadienyl)zirconium(IV), tetrakis(diethylamido)zirconium(IV), tetrakis(dimethylamido)zirconium(IV), tetrakis(ethylmethylamido)zirconium(IV), zirconium(IV) dibutoxide (bis-2,4-pentanedionate), zirconium(IV) 2-ethylhexanoate, zirconium tetrakis(2,2,6,6-tetramethyl-3,5-heptanedionate), palladium(II) hexafluoroacetylacetonate, cyclopentadienyl indium, trimethyl indium, iridium(III) acetylacetonate, and lithium tert-butoxide.
[0086] In a preferred embodiment, the first and second metal, metalloid or semiconductor precursors of the present invention are independently selected from trimethylaluminum, triisobutylaluminum, aluminum tris(2,2,6,6-tetramethyl-3,5-heptanedionate), tris(dimethylamido)aluminum, aluminum trichloride, triphenylantimony, bis(pentafluorophenyl)zinc, bis(2,2,6,6-tetramethyl-3,5-heptanedionate)zinc(II), diethylzinc, diphenylzinc, tetrakis(diethylamido)titanium(IV), tetrakis(dimethylamido)titanium(IV), tetrakis(ethylmethylamido)titanium(IV), titanium(IV) diisopropoxide bis(2,2,6,6-tetramethyl-3,5-heptanedionate), titanium(IV) isopropoxide, titanium tetrachloride, cyclopentadienyl indium and trimethyl indium.
[0087] In certain embodiments, the exposure time between the pulse and the purge in steps (iii) and (iv) is 5 seconds or more, preferably 5 to 300 seconds, more preferably 10 to 180 seconds, more preferably 20 to 60 seconds, and even more preferably 20 to 40 seconds.
[0088] In the context of the present invention, the term "impregnate" or "impregnation" refers in particular to the process of impregnating a polymer with a precursor in the gaseous state, for example a precursor of a metal, semimetal or semiconductor. Base material The precursor is a polymer Base material In certain embodiments, the precursor can react with a functional group in a polymer Base material and in particular, this reaction does not degrade the polymer.
[0089] The thickness of the impregnated layer of the organic-inorganic hybrid material can be controlled by controlling the exposure time in step (iii), while the density of the impregnated layer can be controlled by the number of repetitions of step (iii). All these parameters are dependent on the polymer used to obtain a final material with an impregnated layer of the desired density and thickness. Base material and can be controlled by one skilled in the art depending on the precursor. In certain embodiments, the thickness of the impregnation layer is understood as the depth reached by the impregnation layer in the polymer.
[0090] In certain embodiments, the second metal, metalloid or semiconductor precursor of step (iii) is a precursor of the coated polymer of step (ii) or (ii'). Base material Impregnated with polymer Base material Among these, preferably polymer Base material It bonds with functional groups within the bulk of the molecule.
[0091] In one embodiment, the precursor of the second metal, metalloid or semiconductor in step (iii) is incapable of reacting with the coating layer obtained in step (ii) or (ii'). In a particular embodiment, the precursor of the second metal, metalloid or semiconductor in step (iii) is incapable of reacting with the coating layer obtained in step (ii) or (ii'). Base materialand thus cannot react with the first metal, semimetal or semiconductor precursor and / or mono- or oligo-functional organic molecule attached to the functional groups on the surface of the coated polymer. Base material The ions diffuse into the bulk of the
[0092] In one embodiment, the coated and impregnated polymer obtained in step (iii) Base material teeth, a precursor of a first metal, semi-metal or semiconductor; a mono- or oligo-functional organic molecule; or a polymer of a compound or component of a first metal, semi-metal or semiconductor, and a mono- or oligo-functional organic molecule. Base material a coating layer on the surface of A polymer of a precursor of a second metal, semimetal or semiconductor. Base material The impregnated layer inside Preferably, the first metal, semimetal or semiconductor precursor or the mono- or oligo-functional organic molecule is a polymer. Base material A second metal, metalloid or semiconductor precursor is attached to the surface functional group and then bonded to the polymer. Base material and more preferably, a first metal, semimetal or semiconductor precursor, or a mono- or oligo-functional organic molecule is bonded to a bulk functional group of the polymer. Base material A second metal, semimetal or semiconductor precursor is bonded to all functional groups on the surface of the polymer. Base material It bonds to the functional groups in the bulk of the molecule.
[0093] The term co-reactant refers to a compound that activates a metal, semi-metal or semiconductor precursor, modifies a metal, semi-metal or semiconductor precursor, or catalyzes the reaction of a metal, semi-metal or semiconductor precursor to convert it into the desired metal, semi-metal or semiconductor compound or component, and couples it to a polymer to form either a coating or an impregnated layer. Base material Suitable co-reactants are well known in the art.
[0094] In a particular embodiment, the co-reactant in step (iv) or step (v) is selected from an oxygen source, a hydrogen source, a sulfur source and a nitrogen source, preferably an oxygen source. In a more particular embodiment, the co-reactant in step (iv) or step (v) is selected from HO, O, O, hydrogen, BH, BH, H, S, a metal hydride, NH and hydrazine, preferably HO, O or O, more preferably HO.
[0095] In certain embodiments, the co-reactant of step (iv) or step (v) reacts with the first metal, metalloid or semiconductor precursor and / or the second metal, metalloid or semiconductor precursor to provide a metal, metalloid or semiconductor compound or component independently selected from a metal oxide, a metal nitride, a metal sulfide and a zero-valent metal, preferably a metal oxide.
[0096] In one embodiment, the coated and impregnated polymer obtained in step (iv) or step (v) Base material teeth, a first metal, semi-metal or semiconductor compound or component; a mono- or oligo-functional organic molecule; or a polymer of a first metal, semi-metal or semiconductor compound or component and a mono- or oligo-functional organic molecule. Base material a coating layer on the surface of A polymer containing a second metal, semimetal or semiconductor compound or component. Base material The impregnated layer inside wherein the first and second metal, metalloid or semiconductor compounds or components are different, and the coating layer does not include the second metal, metalloid or semiconductor compound or component.
[0097] In certain embodiments, the coating layer comprising a first metal, semi-metal or semiconductor compound or component and / or the impregnated layer comprising a second metal, semi-metal or semiconductor compound or component comprises a metal selected from Al, Zn, Si, Ti and In. In more specific embodiments, the coating layer comprising a first metal, semi-metal or semiconductor compound or component and / or the impregnated layer comprising a second metal, semi-metal or semiconductor compound or component comprises a metal oxide, preferably a metal oxide independently selected from Al2O3, ZnO, SiO2, TiO2 and In2O3, more preferably a metal oxide independently selected from Al2O3, ZnO, TiO2 and In2O3.
[0098] In certain embodiments, the co-reactant is an oxygen source, preferably HO, and the polymer Base material The metallic, semi-metallic or semiconducting compounds or components coated and / or impregnated in the substrate are preferably metal oxides, preferably Al2O3, ZnO, SiO2, TiO2 or It is In2O3, and more preferably selected from Al2O3, ZnO, TiO2 and In2O3.
[0099] In certain embodiments, the metal, metalloid, or semiconductor compound or component is a metal, metalloid, or semiconductor that contains one or more metal, metalloid, or semiconductor components and one or more additional components, hi other embodiments, it is a metal, metalloid, or semiconductor component that has an oxidation state of zero.
[0100] In a particular embodiment, the process of the invention is carried out at a temperature between 50 and 300° C., preferably between 100 and 200° C., more preferably at about 150° C. In one embodiment, the process of the invention is carried out at a pressure between 1 mbar and 1034 mbar, preferably between 100 mbar and 800 mbar, more preferably between 500 mbar and 700 mbar. In a more particular embodiment, the process of the invention is carried out under a constant nitrogen gas flow between 10 and 500 standard cubic centimeters per minute (sccm), preferably between 15 and 50 standard cubic centimeters per minute (sccm), more preferably between 20 standard cubic centimeters per minute (sccm).
[0101] In a particular embodiment, the coating layer of the present invention has a thickness of 1 to 200 nm, preferably 5 to 100 nm, and more preferably 10 to 50 nm.
[0102] In a particular embodiment, the impregnated layer of the present invention has a thickness of 1 to 1000 nm, preferably 5 to 500 nm, and more preferably 10 to 100 nm.
[0103] In a more particular embodiment, the method of the present invention comprises the steps of: i) placing an aromatic polyamide in the reaction chamber; Base material , preferably polyparaphenylene terephthalamide Base material preparing a ii) pulsing a first metal, metalloid or semiconductor precursor selected from trimethylaluminum (TMA), titanium tetraisopropoxide (TTIP), diethylzinc (DEZ) and trimethylindium into the reaction chamber, then purging the reaction chamber to produce a polymer coated with trimethylaluminum (TMA), titanium tetraisopropoxide (TTIP), diethylzinc (DEZ) or trimethylindium; Base material wherein there is no exposure time between the pulse and the purge; iii) pulsing a precursor of a second metal, metalloid or semiconductor selected from trimethylaluminum (TMA), titanium tetraisopropoxide (TTIP), diethylzinc (DEZ) and trimethylindium into the reaction chamber, then allowing an exposure time, then purging the reaction chamber to produce a polymer coated with the precursor of a first metal, metalloid or semiconductor selected from trimethylaluminum (TMA), titanium tetraisopropoxide (TTIP), diethylzinc (DEZ) and trimethylindium and impregnated with the precursor of a first metal, metalloid or semiconductor selected from trimethylaluminum (TMA), titanium tetraisopropoxide (TTIP), diethylzinc (DEZ) and trimethylindium. Base material wherein the exposure time between the pulse and the purge is 5 seconds or more; and iv) pulsing water into the reaction chamber, then providing an exposure time, then purging the reaction chamber to form a coating layer selected from Al2O3, TiO2, ZnO, and In2O3, and providing an inorganic characteristic selected from Al2O3, TiO2, ZnO, and In2O3. Have Impregnated polymer Base material wherein the exposure time between the pulse and the purge is 5 seconds or more, and the water reacts with the first and second metal, metalloid, or semiconductor precursors. with the proviso that the metallic, semi-metallic or semi-conductive compound or component of the coating layer is different from the metallic, semi-metallic or semi-conductive compound or component of the impregnated layer.
[0104] In another particular embodiment, the method of the present invention comprises the steps of: i) polyparaphenylene terephthalamide in the reaction chamber Base material preparing a ii) Trimethylaluminum (TMA) is pulsed into the reaction chamber, and then the reaction chamber is purged to obtain a polymer coated with trimethylaluminum (TMA). Base material wherein there is no exposure time between the pulse and the purge; iii) Diethylzinc (DEZ) is pulsed into the reaction chamber, followed by an exposure period, then the reaction chamber is purged to prepare a polymer coated with trimethylaluminum (TMA) and impregnated with diethylzinc (DEZ). Base material wherein the exposure time between the pulse and the purge is 10 to 50 seconds; and iv) Optionally, water is pulsed into the reaction chamber, followed by an exposure period, and then the reaction chamber is purged to prepare the Al2O3 coated, ZnO impregnated polymer. Base material wherein the exposure time between the pulse and the purge is 10 to 50 seconds, and the water is a first and a second metal Precursor The process of reacting with The present invention relates to a method for producing a semiconductor device comprising the steps of:
[0105] In certain embodiments, the cycle of steps (ii)-(iii) or (ii)-(iv) or (ii)-(v) of the method of the invention in any of its specific embodiments is repeated 50 or more times, preferably 1-1000 times, more preferably between 10-400 times, and even more preferably 50-300 times.
[0106] In certain embodiments, each step of the method of the present invention in any of the specific embodiments thereof is independently repeated a desired number of times, preferably 2 or more times, more preferably 2 to 200 times, and even more preferably 5 to 100 times.
[0107] In certain embodiments, the method of the present invention comprises steps (i)-(iv) or (i)-(v) as disclosed herein. However, the method of the present invention may also be used to impregnate the polymer by pulsing with other precursors to add additional impregnation materials. Base material The method may also include the further step of pulsing with other precursors or reactants to produce sections of different composition in the subsurface region of the polymer. Base material The method may include the further step of adding additional coating material onto the surface of the substrate.
[0108] In a second aspect, the present invention relates to an organic-inorganic hybrid material obtainable by the method of the invention in any of its embodiments described above.
[0109] In a third aspect, the present invention provides a method for producing a method for treating a cancer cell comprising the steps of: polymer Base material and, A polymer comprising a first metal, semimetal or semiconductor compound or moiety, or a mono- or oligo-functional organic molecule, or a mixture thereof. Base material a coating layer on the surface of A polymer comprising a second metal, semimetal or semiconductor compound or component. Base material The impregnated layer inside An organic-inorganic hybrid material comprising: The first metal, metalloid or semiconductor compound or component is different from the second metal, metalloid or semiconductor compound or component; and The coating layer is an organic-inorganic hybrid material that does not include a second metal, semi-metal or semiconductor compound or component.
[0110] In certain embodiments, the organic-inorganic hybrid material of the present invention comprises: polymer Base material and, A polymer comprising a first metal, semimetal or semiconductor compound or moiety. Base material a coating layer on the surface of A polymer comprising a second metal, semimetal or semiconductor compound or component. Base material The impregnated layer inside Equipped with.
[0111] In another particular embodiment, the organic-inorganic hybrid material of the present invention comprises: polymer Base material and, polymer Base material a first layer in contact with the surface of the polymer; and a second layer in contact with the first layer. Base materiala coating layer on the surface of the substrate, wherein a first layer comprises a first metal, semi-metal or semiconductor compound or component and a second layer comprises a mono- or oligo-functional organic molecule; A polymer comprising a second metal, semimetal or semiconductor compound or component. Base material The impregnated layer inside Equipped with.
[0112] In another particular embodiment, the organic-inorganic hybrid material of the present invention comprises: polymer Base material and, Polymers comprising mono- or oligo-functional organic molecules Base material a coating layer on the surface of gold Polymers comprising metal, semimetal or semiconductor compounds or components Base material The impregnated layer inside Equipped with.
[0113] Polymers related to organic-inorganic hybrid materials Base material Certain preferred embodiments for the coating layer; the impregnating layer; the first metal, semi-metal or semiconductor compound or component; the second metal, semi-metal or semiconductor compound or component; and the mono- or oligo-functional organic molecule have already been defined for the method of the present invention.
[0114] In a particular embodiment, the coating layer of the organic-inorganic hybrid material of the present invention comprises a metal, semi-metal or semiconductor compound or component selected from metal oxides, metal nitrides and metals in the metallic state, preferably metal oxides, more preferably Al2O3, ZnO, In2O3 or TiO2. In a preferred embodiment, the coating layer comprises Al2O3.
[0115] In certain embodiments, the impregnated layer of the organic-inorganic hybrid material of the present invention comprises a metal, semimetal or semiconductor compound or component selected from metal oxides, metal nitrides and metals in the metallic state, preferably metal oxides, more preferably Al2O3, ZnO, In2O3 or TiO2. In a preferred embodiment, the impregnated layer comprises ZnO.
[0116] In a preferred embodiment, the organic-inorganic hybrid material of the present invention comprises: Aromatic Polyamide Base material , preferably polyparaphenylene terephthalamide Base material and, Selected from Al2O3, ZnO, In2O3 and TiO2; Base material a coating layer on the surface of Comprising Al2O3, ZnO, In2O3 or TiO2; Base material and an impregnation layer therein, the coating layer and the impregnation layer being made of different materials.
[0117] In a more preferred embodiment, the organic-inorganic hybrid material of the present invention comprises: Polyparaphenylene terephthalamide Base material and, Al2O3, polyparaphenylene terephthalamide Base material a coating layer on the surface of Paraphenylene terephthalamide containing ZnO Base material The impregnated layer inside Equipped with.
[0118] In a particular embodiment, the coating layer of the organic-inorganic hybrid material of the present invention has a thickness of 0.06 nm to 200 nm, preferably 1 to 200 nm, preferably 1 to 150 nm, preferably 5 to 100 nm, more preferably 10 to 50 nm.
[0119] In one embodiment, the impregnated layer of the organic-inorganic hybrid material of the present invention has a thickness of more than 1 nm, preferably more than 2 nm, more preferably more than 10 nm. In a specific embodiment, the impregnated layer of the organic-inorganic hybrid material of the present invention has a thickness of 1 to 1000 nm, preferably 5 to 200 nm, more preferably 5 to 100 nm, and even more preferably 10 to 100 nm.
[0120] In one embodiment, the coating layer has a thickness of 1 to 200 nm and the impregnation layer has a thickness of 1 to 1000 nm. In another embodiment, the coating layer has a thickness of 5 to 100 nm and the impregnation layer has a thickness of 5 to 200 nm. In a further embodiment, the coating layer has a thickness of 10 to 50 nm and the impregnation layer has a thickness of 5 to 100 nm.
[0121] The thickness of the impregnated or coated layer can be determined by electron microscopy, in particular transmission electron microscopy, preferably focused ion beam. Base material can be determined after examination of a cross-sectional sample, obtained by cutting and thinning the slice by sputtering with Ar to a thickness suitable for examination by transmission electron microscopy.
[0122] In another embodiment of the present invention, the thickness of the impregnation layer is Base material This represents 0.05% to 15%, preferably 0.05% to 10%, more preferably 0.05% to 5%, and even more preferably 0.1% to 1% of the total thickness.
[0123] In certain embodiments, the toughness modulus of the organic-inorganic hybrid material of the present invention is improved by the polymer Base material In certain embodiments, the break strain value of the organic-inorganic hybrid material of the present invention is increased by 10% or more compared to the toughness coefficient of the polymer. Base material The breaking strain value is equal to or greater than that of the polymer Base material Preferably, the organic-inorganic hybrid material of the present invention is a polymer Base materialIn certain embodiments, the toughness modulus of the irradiated organic-inorganic hybrid material of the present invention is greater than or equal to 10% of the polymer. Base material In the context of the present invention, the term "irradiated" refers to exposure to UV light having a wavelength of 365 nm for 24 hours. In certain embodiments, the toughness factor of the irradiated organic-inorganic hybrid material of the present invention is 30 MJ / m or more at room temperature (20-25° C.). 3 The value is greater than or equal to this.
[0124] In one embodiment, the organic-inorganic hybrid material of the present invention is a fiber, preferably having a diameter of 5-20 microns and a length of 1-5 cm, more preferably having a diameter of about 10 microns and a length of about 3 cm.
[0125] In the present invention, the mechanical properties of the samples are measured according to ASTM standard C1557-03 test (2008) [ASTM C1557-03(2008), Standard Test Method for Tensile Strength and Young's Modulus of Fibers, ASTM International, West Conshohocken, PA, 2008].
[0126] The inventors have found that the organic-inorganic hybrid materials of the present invention surprisingly maintain or even surpass the distinct properties of their substituents, particularly in the case of polymers. Base material In particular, the inventors have found that the mechanical properties of polyparaphenylene terephthalamide are maintained or improved. Base material and polyparaphenylene terephthalamide Base material A coating layer of Al2O3 on the surface of the α-phenylene terephthalamide Base material and an impregnated layer of ZnO in the organic-inorganic hybrid material maintains or improves the mechanical properties of the substrate, and the properties of the organic-inorganic hybrid material are Base material It has been found that the individual properties (especially resistance to ultraviolet light) of
[0127] In a further aspect, the present invention relates to the use of the organic-inorganic hybrid materials of the present invention in the manufacture of flexible, lightweight polymer transistors, capacitors, optoelectronic devices, barriers, absorbers, personal safety equipment (e.g., bulletproof vests and military gear), sporting goods, protective laminates, building materials, textiles, automobiles and aircraft. EXAMPLES
[0128] The present invention is illustrated by the following examples which in no way limit the scope of the invention.
[0129] Example 1: Al 2 O 3 Kevlar fiber coated with Al 2 O 3 Kevlar fiber impregnated with Al 2 O 3 of ZnO-coated and ZnO-impregnated Kevlar fibers and characterization of their tensile strength and UV resistance Different fibers: a) Kevlar fibre coated with Al2O3; b) Kevlar fibres impregnated with Al2O3; c) ZnO-coated Kevlar fibre; d) Kevlar fibre impregnated with ZnO; e) Kevlar fibers coated with Al2O3 and impregnated with ZnO were prepared.
[0130] Poly(p-paraphenylene terephthalamide) fibers, referred to as Kevlar fibers (Kevlar® 29 fibers from DuPont), were used in all tests. The fiber diameter was about 10 μm, and the fiber length was about 3 cm. Furthermore, all modifications of the samples were performed in a commercial atomic layer deposition (ALD) reactor (Savannah S100, Cambridge NanoTech Inc). Impregnation and coating of the fibers were performed at 150° C. under a constant nitrogen gas flow of 20 standard cubic centimeters per minute (sccm).
[0131] Trimethylaluminum (TMA, Al(CH3)3, Strem Chemicals) was used as the aluminum source, diethylzinc (DEZ, Zn(C2H5)2) was used as the zinc source, and demineralized water was used as the oxygen source.
[0132] Al2O3-coated fibers were prepared according to a typical ALD process with cycles of pulse (TMA, 0.08 s) / purge (N2, 30 s) / pulse (H2O, 0.08 s) / purge (N2, 30 s). ZnO-coated fibers were prepared according to a typical ALD process with cycles of pulse (DEZ, 0.08 s) / purge (N2, 30 s) / pulse (H2O, 0.08 s) / purge (N2, 30 s). Meanwhile, impregnated fibers were prepared by MPI, where: Base material was exposed to the precursor for a defined period of time and then purged to allow diffusion of the precursor into the polymer. The MPI cycle for the Al2O3-impregnated fibers consisted of pulse (TMA, 0.08 s) / exposure (30 s) / purge (N2, 30 s) / pulse (H2O, 0.08 s) / exposure (30 s) / purge (N2, 30 s). The MPI cycle for the ZnO-impregnated fibers consisted of pulse (DEZ, 0.08 s) / exposure (30 s) / purge (N2, 30 s) / pulse (H2O, 0.08 s) / exposure (30 s) / purge (N2, 30 s). Finally, a combination of ALD and MPI was used to fabricate the alumina-coated and ZnO-impregnated samples. Each cycle consisted of pulse (TMA, 0.08 s) / purge (N2, 30 s) / pulse (DEZ, 0.08 s) / expose (30 s) / purge (N2, 30 s) / pulse (HO, 0.08 s) / expose (30 s) / purge (N2, 30 s). In all cases, the number of repetitions of the ALD, MPI or ALD / MPI cycles was 200.
[0133] Fiber characterization, tensile strength and UV resistance testing TEM / EDS characterization Characterization by transmission electron microscopy (TEM) and analysis by energy dispersive X-ray spectroscopy (EDS) were performed on an FEI Titan microscope using 300 kV in STEM mode and an EDAX SDD detector.
[0134] The Kevlar fiber was gently stretched across a convex aluminum SEM stub (prepared in-house) and secured at both ends of the fiber with carbon tape, creating a FIB Lamella By selecting the position of the block extraction, the fiber was attached with deposited Pt. Base material The samples were locally fixed in a 300-well plate and the blocks were extracted using standard methods. The sample surface was first protected using Pt e-beam deposition, followed by ion beam deposition. For the final surface treatment, the blocks were thinned to transparency on a copper "omniprobe" grid using a 5 kV gallium ion beam at 8 pA.
[0135] Figure 1 shows TEM images of FIB-prepared cross sections of (a) alumina-coated Kevlar (C-Al2O3), (b) alumina-impregnated Kevlar (I-Al2O3), and (c) alumina-coated and ZnO-impregnated Kevlar (TMA pulse). Figure 1(d) shows the TMA / MPI ED of pulsed samples S-Ma The images show the clear differences between the ALD coating method (Fig. 1a) and MPI impregnation (Fig. 1b), as well as the mixed ALD / MPI method using two different materials (Fig. 1c). In particular, the alumina-coated Kevlar fiber (C-Al2O3) had a sharp interface between the Al2O3 thin film and the polymer core (Fig. 1a), whereas in the alumina-impregnated Kevlar fiber, TMA diffused into the polymer and formed a second, less dense Al2O3 layer in the subsurface region of the polymer (Fig. 1b).
[0136] TEM images of alumina-coated, ZnO-impregnated Kevlar fibers show a thin film of Al2O3 of about 20 nm on the surface of the fiber and a layer of ZnO of about 10 nm in the subsurface region of the polymer (Figure 1c and d).
[0137] Thus, by combining ALD / MPI techniques it is possible to synthesize Kevlar fibers coated with a homogenous and sharp layer of Al2O3 and impregnated with a different material (ZnO).
[0138] Mechanical properties and UV exposure Tensile tests were performed using a BRUKER universal mechanical tester with a resolution of 50 μN and according to ASTM standard C1557-03(2008) [ASTM C1557-03(2008), Standard Test Method for Tensile Strength and Young's Modulus of Fibers, ASTM International, West Conshohocken, PA, 2008]. The fiber was clamped in a cardboard sample holder with a punched hole of 6 mm diameter in the center. After vertical alignment and clamping of the fiber across the hole, the sample holder was placed in the mechanical tester with no strain on the fiber. Finally, the sample holder was cut along the central guide and a tensile force was applied to the fiber until it broke, while simultaneously measuring the strain at room temperature.
[0139] To measure the stability of the fibers under UV light, samples were exposed to light with a wavelength of 365 nm for 24 hours, and the strain-stress curves were then measured and compared to the mechanical properties of unexposed fibers.
[0140] Figure 2 shows a comparison of the mechanical properties of untreated Kevlar fibers, fibers after impregnation (I-Al2O3) or coating (C-Al2O3) with Al2O3, fibers after impregnation (I-ZnO) or coating (C-ZnO) with ZnO, and fibers after impregnation with ZnO and coating with Al2O3 (TMA pulse). I-Al2O3 and C-Al2O3 with Al2O3, as well as TMA pulse samples, showed an increase in the toughness factor compared to untreated Kevlar (Figure 2a). However, despite showing a 13% increase in toughness factor, the samples coated with Al2O3 showed a significant decrease in the breaking strain values compared to untreated Kevlar. Conversely, I-Al2O3 had similar breaking strain values to Kevlar, but only a 5% increase in toughness factor. C-ZnO and I-ZnO showed a decrease in the toughness factor compared to untreated Kevlar (Figure 2a). Nevertheless, the ZnO-impregnated and Al2O3-coated samples (TMA pulse samples) showed the greatest increase in toughness modulus (over 17% of untreated Kevlar fibers), with similar breaking strain values to Kevlar and similar Young’s modulus or UTS values to the Al2O3-coated samples (C-Al2O3).
[0141] Thus, the ZnO impregnated and Al2O3 coated Kevlar fibers (TMA pulse samples) exhibited better mechanical properties than the remaining samples.
[0142] After exposing the fibers to UV light for 24 h, the mechanical properties of the coated and impregnated samples were further analyzed. Figure 2a shows the toughness modulus results before and after UV light exposure, and Figure 2b shows the stress-strain curves before and after UV light exposure.
[0143] Untreated Kevlar maintained only 45% of its toughness factor after exposure to UV light (Figure 2a). I-Al2O3 and C-Al2O3 samples showed higher UV resistance, maintaining 65% and 70% of their toughness factor, respectively. I-ZnO and C-ZnO samples showed a 70% and less than 5% decrease in toughness factor. However, samples impregnated with ZnO and coated with Al2O3 (TMA pulse samples) showed a significant improvement in resistance to UV light. In fact, even after exposure to UV light, 100% of the toughness factor was maintained and a complete suppression of UV sensitivity was observed.
[0144] SEM The morphology of the fibers after tensile testing was also analyzed by SEM. SEM micrographs were taken with an environmentally controlled scanning electron microscope Quanta 250FEG equipped with a large field detector (LFD). Broken fibers were attached to carbon tape and images were taken at 10 kV and 70 Pa.
[0145] Figure 3 shows SEM images of the broken ends of untreated, coated, and impregnated Kevlar samples after UV light exposure compared to Kevlar before exposure. The broken ends of the fibers show that the break mode is either fibrillary or brittle, depending on the pretreatment, which is coating or impregnation. Figure 3 shows that the break of the Kevlar fiber was mainly caused by fibrillation and splitting along the fiber axis. In contrast, the broken area of the UV-irradiated sample showed negligible fibrillation. This break mode is characteristic of brittle materials and is caused by UV-induced polymer chain scission reactions, which weaken the tensile modulus and strength of the fiber. The same break mode was observed in C-Al2O3 and I-Al2O3 Kevlar samples after UV exposure, indicating that the Al2O3 coating does not prevent UV-induced chain scission reactions. In contrast, after exposure to UV light, the ZnO-impregnated and Al2O3-coated Kevlar fibers (TMA Pulsed UV samples) showed fibrous-type fracture characteristic of untreated Kevlar. Longitudinal splitting and fibrillation indicated that the combination of alumina coating and ZnO impregnation did not significantly embrittle the fibers.
[0146] Attenuated total reflectance-Fourier transform infrared spectroscopy (ATR-FTIR) Attenuated total reflectance-Fourier transform infrared spectroscopy (ATR-FTIR) spectra of the samples were acquired on a Perkin Elmer Frontier spectrometer equipped with an ATR sampling stage. -1 Resolution of 520 to 4000 cm -1 All spectra were measured by collecting 20 scans in the range of 0.01 μm to 0.01 μm. Each sample was measured five times and the results were averaged.
[0147] Figure 4 shows the fingerprint region (1200–800 cm) of the ATR-FTIR spectrum of Kevlar fiber before and after coating and impregnation. -1 ) is shown. Here, the fingerprint region (1000–800 cm) of the ATR-FTIR spectrum of the sample is shown. -1The stretching signatures of the CN, CO and CC bonds in The 940 cm peak is related to the presence of a CO single bond due to the binding of TMA, a Lewis acid, to the oxygen of the C=O bond of the amide on the surface of Kevlar fiber. -1 Peak of, Approximately 960 cm assigned to the C-C stretching due to the newly generated C-C bond -1 Peak of, and 980cm associated with C-N bond -1 This can be seen as a prominent peak.
[0148] 940 and 960cm -1 The intensity of the peak is lower in the TMA-pulsed sample, indicating a milder degree of chemical modification than the Al2O3-coated and Al2O3-impregnated samples. In addition, the 980 cm peak associated with the C-N bond in untreated Kevlar is -1 The peak of is visible in the ATR-FTIR spectrum of the ZnO-impregnated and Al2O3-coated sample, but this peak almost disappeared in the C-Al2O3 and I-Al2O3 samples. Thus, the alumina-treated sample has more strongly decomposed polymer chains.
[0149] Thus, the ZnO-impregnated and Al2O3-coated Kevlar fibers showed improved mechanical properties (strength and flexibility) over the original Kevlar fibers, with no degradation of properties after UV exposure.
[0150] Example 2: TiO 2 Coated with In 2 O 3 Preparation of Kevlar fibers impregnated with. Kevlar fibers were coated and impregnated according to the process described in Example 1, but using ALD / MPI cycles consisting of a 0.08 second pulse of titanium tetraisopropoxide (TTIP), followed by a 30 second purge (ALD-like pulse); a 0.08 second pulse of trimethylindium, followed by a 30 second exposure, followed by a 30 second purge (MPI-like pulse); and a 0.08 second pulse of water, followed by a 30 second exposure, followed by a 30 second purge (MPI-like pulse). The coating and impregnation process consisted of 200 cycles of ALD / MPI.
[0151] Example 3: Al 2 O 3 Coated with In 2 O 3 Preparation of Kevlar fibers impregnated with. Kevlar fibers were coated and impregnated according to the process described in Example 1, using ALD / MPI cycles consisting of a 0.08 second pulse of trimethylaluminum followed by a 30 second purge (ALD-like pulse); a 0.08 second pulse of trimethylindium followed by a 30 second exposure followed by a 30 second purge (MPI-like pulse); and a 0.08 second pulse of water followed by a 30 second exposure followed by a 30 second purge (MPI-like pulse). The coating and impregnation process consisted of 200 cycles of ALD / MPI.
[0152] The present invention is further defined in the following embodiments.
[0153] EMBODIMENT 1 The process is as follows: i) placing a polymer in the reaction chamber; Base material preparing a ii) pulsing a first metal precursor or a monofunctional organic molecule into the reaction chamber and then purging the reaction chamber with no exposure time between the pulse and the purge; iii) pulsing a second metal precursor into the reaction chamber, followed by an exposure time, and then purging the reaction chamber, wherein the exposure time between the pulse and the purge is 5 seconds or more; and iv) pulsing a co-reactant into the reaction chamber followed by an exposure time and then purging the reaction chamber, wherein the exposure time between the pulse and the purge is 5 seconds or more and the co-reactant reacts with the first metal precursor and the co-reactant reacts with the second metal precursor if the monofunctional organic molecule is not pulsed in step (ii).
[0154] EMBODIMENT 2 The process is as follows: i) placing a polymer in the reaction chamber; Base material preparing a ii) pulsing a first metal precursor into the reaction chamber and then purging the reaction chamber to produce a polymer coated with the first metal precursor; Base material with no exposure time between the pulse and the purge; iii) pulsing the second metal precursor into the reaction chamber, then allowing an exposure time, then purging the reaction chamber to leave a polymer coated with the first metal precursor and impregnated with the second metal precursor; Base material wherein the exposure time between the pulse and the purge is 5 seconds or more; and iv) pulsing the co-reactant into the reaction chamber, followed by an exposure time, and then purging the reaction chamber to leave a polymer coated with the first metal compound and impregnated with the second metal compound; Base material wherein the exposure time between the pulse and the purge is 5 seconds or more, and the co-reactant reacts with the first and second metal precursors. 2. The method of embodiment 1, comprising:
[0155] EMBODIMENT 3 The process is as follows: i) placing a polymer in the reaction chamber; Base material preparing a ii) pulsing a first metal precursor into the reaction chamber and purging the reaction chamber to produce a polymer coated with the first metal precursor; Base materialwith no exposure time between the pulse and the purge; ii') pulsing the monofunctional organic molecule into the reaction chamber and then purging the reaction chamber to leave a polymer coated with the first metal compound and the monofunctional organic molecule; Base material wherein the monofunctional organic molecule reacts with the first metal precursor with no exposure time between the pulse and the purge; iii) pulsing the second metal precursor into the reaction chamber, followed by an exposure time, and then purging the reaction chamber to produce a polymer coated with the first metal precursor and the monofunctional organic molecule, and impregnated with the second metal precursor; Base material wherein the exposure time between the pulse and the purge is 5 seconds or more; and iv) pulsing the coreactant into the reaction chamber, followed by an exposure time, and then purging the reaction chamber to produce a polymer coated with the first metal compound and the monofunctional organic molecule, and impregnated with the second metal compound. Base material wherein the exposure time between the pulse and the purge is 5 seconds or more, and the co-reactant reacts with the second metal precursor. 3. The method of embodiment 1 or 2, comprising:
[0156] EMBODIMENT 4 The process is as follows: i) placing a polymer in the reaction chamber; Base material preparing a ii) pulsing the monofunctional organic molecule into the reaction chamber and then purging the reaction chamber to obtain a polymer coated with the monofunctional organic molecule; Base material with no exposure time between the pulse and the purge; iii) pulsing the metal precursor into the reaction chamber, followed by an exposure time, then purging the reaction chamber to leave a polymer coated with the monofunctional organic molecule and impregnated with the second metal precursor; Base material wherein the exposure time between the pulse and the purge is 5 seconds or more; and iv) The coreactant is pulsed into the reaction chamber, followed by an exposure period, and then the reaction chamber is purged to produce a polymer coated with the monofunctional organic molecule and impregnated with the metal compound. Base material wherein the exposure time between the pulse and the purge is 5 seconds or more, and the co-reactant reacts with the second metal precursor. 2. The method of embodiment 1, comprising:
[0157] EMBODIMENT 5 The method of any of embodiments 1-4, wherein the first metal precursor is different from the second metal precursor.
[0158] EMBODIMENT 6 An organic-inorganic hybrid material obtainable by the method according to any one of the first to fifth embodiments.
[0159] EMBODIMENT 7 polymer Base material and, A polymer comprising a first metal compound or a monofunctional organic molecule or a mixture thereof. Base material a coating layer on the surface of A polymer comprising a second metal compound. Base material The impregnated layer inside An organic-inorganic hybrid material comprising: the first and second metal compounds are different; The coating layer is an organic-inorganic hybrid material that does not include a second metal compound.
[0160] EMBODIMENT 8 polymer Base material and, A polymer comprising a first metal compound. Base material a coating layer on the surface of A polymer comprising a second metal compound. Base material The impregnated layer inside or polymer Base material and, Polymers comprising monofunctional organic molecules Base material a coating layer on the surface of A polymer comprising a second metal compound. Base material The impregnated layer inside or polymer Base material and, polymer Base material a first layer in contact with the surface of the polymer; and a second layer in contact with the first layer. Base material a coating layer on the surface of the substrate, wherein a first layer comprises a first metal compound and a second layer comprises a monofunctional organic molecule; A polymer comprising a second metal compound. Base material The impregnated layer inside The organic-inorganic hybrid material of embodiment 7, comprising:
[0161] EMBODIMENT 9 polymer Base material 9. The method of any of embodiments 1-5, or the organic-inorganic hybrid material of any of embodiments 6-8, wherein is selected from polyamides, polyamines, polyimides, polyalkylenes, polyacrylates, polyalcohols, polyethers, polyesters, polyvinyls, polypyrroles, polythiophenes, polystyrenes, and polyketones.
[0162] EMBODIMENT 10 polymer Base material The method of any of embodiments 1-5 and 9, or the organic-inorganic hybrid material of any of embodiments 6-9, wherein is selected from aromatic polyamides, such as para-aramid and meta-aramid polymers.
[0163] EMBODIMENT 11 11. The method of any of embodiments 1-5 and 9-10, or the organic-inorganic hybrid material of any of embodiments 6-10, wherein the first and second metal compounds independently comprise a metal selected from Al, Zn, Si, Ti, W, Sb, As, Ba, Bi, B, Cd, Ca, Ce, Cr, Co, Cu, Er, Eu, Gd, Ga, Ge, Hf, Fe, La, Mg, Mn, Mo, Ni, Nb, Os, Pt, Pr, Re, Rh, Ru, Sm, Se, Sr, Ta, Te, Tb, Tm, Sn, Ti, W, V, Yb, Y, Zr, Pd, In, Ir, and Li.
[0164] EMBODIMENT 12 The method of any of embodiments 1-5 and 9-11, or the organic-inorganic hybrid material of any of embodiments 6-11, wherein the first and second metal compounds are independently selected from metal oxides, metal nitrides, and zero-valent metals.
[0165] EMBODIMENT 13 The method of any of embodiments 1-5 and 9-12, or the organic-inorganic hybrid material of any of embodiments 6-12, wherein the first and second metal compounds are independently selected from Al2O3, ZnO, SiO2, In2O3, and TiO2.
[0166] EMBODIMENT 14 The method of any of embodiments 1-5 and 9-13, or the organic-inorganic hybrid material of any of embodiments 6-13, wherein the monofunctional organic molecule is an aliphatic or aromatic monofunctional organic molecule having one functional group selected from hydroxyl, amino, carboxylic acid, ester, amide, silane, thiol, epoxy, nitro and acid halide.
[0167] EMBODIMENT 15 Use of the organic-inorganic hybrid material as defined in any of embodiments 6 to 13 in the manufacture of flexible and light polymer transistors, capacitors, optoelectronic devices, barriers, absorbers, personal safety devices, sporting goods, protective laminates, building materials, textiles, automotive materials and aircraft materials.
Claims
1. The following steps: i) providing a polymeric substrate in a reaction chamber; ii) pulsing a first metal, metalloid or semiconductor precursor, or a mono- or oligo-functional organic molecule, into the reaction chamber and then purging the reaction chamber to obtain a polymer substrate coated with the first metal, metalloid or semiconductor precursor, or the mono- or oligo-functional organic molecule, with no exposure time between the pulse and the purge; iii) pulsing a second metal, metalloid or semiconductor precursor into the reaction chamber, followed by an exposure time and then purging the reaction chamber to obtain a polymer substrate coated with the first metal, metalloid or semiconductor precursor or the mono- or oligo-functional organic molecule and impregnated with the second metal, metalloid or semiconductor precursor, wherein the exposure time between the pulse and the purge is 5 seconds or more; and iv) pulsing a co-reactant into the reaction chamber, optionally followed by an exposure time, and then purging the reaction chamber; a polymeric substrate coated with a first metal, metalloid or semiconductor compound or component and impregnated with a second metal, metalloid or semiconductor compound or component; or a polymer substrate coated with said mono- or oligo-functional organic molecules and impregnated with a second metal, semi-metal or semiconductor compound or component. A process for obtaining if the mono- or oligo-functional organic molecule is not pulsed in step (ii), the co-reactant reacts with the first metal, metalloid or semiconductor precursor and with the second metal, metalloid or semiconductor precursor; If a mono- or oligo-functional organic molecule is pulsed in step (ii), the co-reactant reacts with the precursor of the second metal, metalloid or semiconductor.
1. A method for making an organic-inorganic hybrid material comprising, in the order listed, The method, wherein the first metal, metalloid or semiconductor precursor is different from the second metal, metalloid or semiconductor precursor.
2. A process comprising the steps of: i) providing a polymeric substrate in a reaction chamber; ii) pulsing a first metal, metalloid or semiconductor precursor into the reaction chamber and then purging the reaction chamber to obtain a polymer substrate coated with the first metal, metalloid or semiconductor precursor, with no exposure time between the pulse and the purge; iii) pulsing a second metal, metalloid or semiconductor precursor into the reaction chamber, followed by an exposure time, and then purging the reaction chamber to obtain a polymer substrate coated with the first metal, metalloid or semiconductor precursor and impregnated with the second metal, metalloid or semiconductor precursor, wherein the exposure time between the pulse and the purge is 5 seconds or more; iv) pulsing a co-reactant into the reaction chamber, optionally followed by an exposure time, and then purging the reaction chamber, wherein the co-reactant reacts with the first metal, metalloid or semiconductor precursor or reacts with the second metal, metalloid or semiconductor precursor; and v) pulsing a co-reactant into the reaction chamber, optionally followed by an exposure time, and then purging the reaction chamber to obtain a polymer substrate coated with a first metal, semi-metal or semiconductor compound or component and impregnated with a second metal, semi-metal or semiconductor compound or component, wherein the co-reactant reacts with any unreacted precursor of the first or second metal, semi-metal or semiconductor.
1. A method for making an organic-inorganic hybrid material comprising, in the order listed, said co-reactant in step (iv) is different from said co-reactant in step (v); The method, wherein the first metal, metalloid or semiconductor precursor is different from the second metal, metalloid or semiconductor precursor.
3. The following steps: i) providing the polymer substrate in the reaction chamber; ii) pulsing the first metal, metalloid or semiconductor precursor, or the mono- or oligo-functional organic molecule, into the reaction chamber and then purging the reaction chamber to obtain a polymer substrate coated with the first metal, metalloid or semiconductor precursor, or the mono- or oligo-functional organic molecule, with no exposure time between the pulse and the purge; iii) pulsing the second metal, metalloid or semiconductor precursor into the reaction chamber, followed by an exposure time and then purging the reaction chamber to obtain the first metal, metalloid or semiconductor precursor or polymer substrate coated with the mono- or oligo-functional organic molecule and impregnated with the second metal, metalloid or semiconductor precursor, wherein the exposure time between the pulse and the purge is 5 seconds or more; and iv) pulsing the co-reactant into the reaction chamber, followed by an exposure time, and then purging the reaction chamber; a polymeric substrate coated with a first metal, metalloid or semiconductor compound or component and impregnated with a second metal, metalloid or semiconductor compound or component; or a polymer substrate coated with said mono- or oligo-functional organic molecules and impregnated with a second metal, semi-metal or semiconductor compound or component. wherein the exposure time between the pulse and the purge is 5 seconds or more; and if the mono- or oligo-functional organic molecule is not pulsed in step (ii), the co-reactant reacts with the first metal, metalloid or semiconductor precursor and with the second metal, metalloid or semiconductor precursor; If a mono- or oligo-functional organic molecule is pulsed in step (ii), the co-reactant reacts with the precursor of the second metal, metalloid or semiconductor.
2. The method of claim 1, comprising:
4. The following steps: i) providing the polymer substrate in the reaction chamber; ii) pulsing the first metal, metalloid or semiconductor precursor into the reaction chamber and then purging the reaction chamber to obtain a polymer substrate coated with the first metal, metalloid or semiconductor precursor, wherein there is no exposure time between the pulse and the purge; iii) pulsing the second metal, metalloid or semiconductor precursor into the reaction chamber, followed by an exposure time and then purging the reaction chamber to obtain a polymer substrate coated with the first metal, metalloid or semiconductor precursor and impregnated with the second metal, metalloid or semiconductor precursor, wherein the exposure time between the pulse and the purge is 5 seconds or more; and iv) pulsing the co-reactant into the reaction chamber, followed by an exposure time and then purging the reaction chamber to obtain a polymer substrate coated with a first metal, metalloid or semiconductor compound or component and impregnated with a second metal, metalloid or semiconductor compound or component, wherein the exposure time between the pulse and the purge is 5 seconds or more and the co-reactant reacts with the first and second metal, metalloid or semiconductor precursors. The method of claim 1 or 3, comprising:
5. The following steps: i) providing a polymeric substrate in a reaction chamber; ii) pulsing a first metal, metalloid or semiconductor precursor into the reaction chamber and purging the reaction chamber to obtain a polymer substrate coated with the first metal, metalloid or semiconductor precursor, wherein there is no exposure time between the pulse and the purge; ii') pulsing a mono- or oligo-functional organic molecule into the reaction chamber and then purging the reaction chamber to obtain a polymer substrate coated with a first metal, metalloid or semiconductor compound or component and said mono- or oligo-functional organic molecule, where there is no exposure time between the pulse and the purge, and where the mono- or oligo-functional organic molecule reacts with the first metal, metalloid or semiconductor precursor; iii) pulsing a second metal, metalloid or semiconductor precursor into the reaction chamber, followed by an exposure time and then purging the reaction chamber to obtain a polymer substrate coated with the first metal, metalloid or semiconductor compound or component and the mono- or oligo-functional organic molecule and impregnated with the second metal, metalloid or semiconductor precursor, wherein the exposure time between the pulse and the purge is 5 seconds or more; and iv) pulsing a co-reactant into the reaction chamber, followed by an exposure time and then purging the reaction chamber to obtain a polymer substrate coated with the first metal, semi-metal or semiconductor compound or component and the mono- or oligo-functional organic molecule and impregnated with a second metal, semi-metal or semiconductor compound or component, wherein the exposure time between the pulse and the purge is 5 seconds or more and the co-reactant reacts with the precursor of the second metal, semi-metal or semiconductor.
1. A method for making an organic-inorganic hybrid material comprising, in the order listed, The method, wherein the first metal, metalloid or semiconductor precursor is different from the second metal, metalloid or semiconductor precursor.
6. The following steps: i) providing the polymer substrate in the reaction chamber; ii) pulsing the mono- or oligo-functional organic molecule into the reaction chamber and then purging the reaction chamber to obtain a polymer substrate coated with the mono- or oligo-functional organic molecule, with no exposure time between the pulse and the purge; iii) pulsing the second metal, metalloid or semiconductor precursor into the reaction chamber, followed by an exposure time and then purging the reaction chamber to obtain a polymer substrate coated with the mono- or oligo-functional organic molecule and impregnated with the second metal, metalloid or semiconductor precursor, wherein the exposure time between the pulse and the purge is 5 seconds or more; and iv) pulsing the co-reactant into the reaction chamber, followed by an exposure time and then purging the reaction chamber to obtain a polymer substrate coated with the mono- or oligo-functional organic molecule and impregnated with the second metal, metalloid or semiconductor compound or component, wherein the exposure time between the pulse and the purge is 5 seconds or more and the co-reactant reacts with the second metal, metalloid or semiconductor precursor. The method of claim 1 or 3, comprising:
7. The method of claim 1, 3, 5 or 6, wherein the mono- or oligo-functional organic molecule is an aliphatic or aromatic mono- or oligo-functional organic molecule having one or more functional groups selected from hydroxyl, amino, carboxylic acid, ester, amide, silane, thiol, epoxy, nitro and acid halide.
8. The method of claim 1, 3, or 5-7, wherein the monofunctional or oligofunctional organic molecule is a monofunctional organic molecule.
9. The method according to any one of claims 1 to 8, wherein the polymer substrate is selected from polyamides, polyamines, polyimides, polyalkylenes, polyacrylates, polyalcohols, polyethers, polyesters, polyvinyls, polypyrroles, polythiophenes, polystyrenes and polyketones.
10. The method according to any one of claims 1 to 9, wherein the polymer substrate is selected from aromatic polyamides, such as para-aramid and meta-aramid polymers.
11. 11. The method of any one of claims 1 to 10, wherein the first and second metal, metalloid or semiconductor precursors, or the first and second metal, metalloid or semiconductor compounds or components, independently comprise Al, Zn, Si, Ti, W, Sb, As, Ba, Bi, B, Cd, Ca, Ce, Cr, Co, Cu, Er, Eu, Gd, Ga, Ge, Hf, Fe, La, Mg, Mn, Mo, Ni, Nb, Os, Pt, Pr, Re, Rh, Ru, Sm, Se, Sr, Ta, Te, Tb, Tm, Sn, Ti, W, V, Yb, Y, Zr, Pd, In, Ir, or Li.
12. 12. The method of any one of claims 1 to 11, wherein the first and second metal, metalloid or semiconductor compounds or components are independently selected from metal oxides, metal nitrides, metal sulfides and zero-valent metals.
13. The first and second metal, semimetal or semiconductor compounds or components are selected from the group consisting of Al 2 O 3 , ZnO, SiO 2 , In 2 O 3 and TiO 2 The method of any one of claims 1 to 12, wherein the
14. A polymer substrate; a coating layer formed directly on the surface of said polymeric substrate, said coating layer comprising a first metal, semi-metal or semiconductor compound or component, or a mono- or oligo-functional organic molecule, or a mixture thereof; an impregnated layer within said polymeric substrate comprising a second metal, semi-metal or semiconductor compound or component; An organic-inorganic hybrid material comprising: the first metal, metalloid or semiconductor compound or component is different from the second metal, metalloid or semiconductor compound or component; and The organic-inorganic hybrid material, wherein the coating layer does not include the second metal, semi-metal or semiconductor compound or component.
15. The polymer substrate; the coating layer formed directly on the surface of the polymer substrate, comprising the first metal, semi-metal or semiconductor compound or component; the impregnated layer within the polymeric substrate comprising the second metal, semi-metal or semiconductor compound or component; or The polymer substrate; said coating layer formed directly on the surface of said polymer substrate comprising said mono- or oligo-functional organic molecules; the impregnated layer within the polymeric substrate comprising the second metal, semi-metal or semiconductor compound or component; or The polymer substrate; a coating layer formed directly on the surface of the polymer substrate, the coating layer comprising a first layer in contact with the surface of the polymer substrate and a second layer in contact with the first layer, the first layer comprising the first metal, semi-metal or semiconductor compound or component and the second layer comprising the mono- or oligo-functional organic molecule; the impregnated layer within the polymeric substrate comprising the second metal, semi-metal or semiconductor compound or component; The organic-inorganic hybrid material of claim 14, comprising:
16. The organic-inorganic hybrid material according to claim 14 or 15, wherein the polymer substrate is selected from polyamides, polyamines, polyimides, polyalkylenes, polyacrylates, polyalcohols, polyethers, polyesters, polyvinyls, polypyrroles, polythiophenes, polystyrenes and polyketones.
17. The organic-inorganic hybrid material according to any one of claims 14 to 16, wherein the polymer substrate is selected from aromatic polyamides, such as para-aramid and meta-aramid polymers.
18. 18. The organic-inorganic hybrid material of any one of claims 14 to 17, wherein the first and second metal, metalloid or semiconductor compounds or components independently comprise Al, Zn, Si, Ti, W, Sb, As, Ba, Bi, B, Cd, Ca, Ce, Cr, Co, Cu, Er, Eu, Gd, Ga, Ge, Hf, Fe, La, Mg, Mn, Mo, Ni, Nb, Os, Pt, Pr, Re, Rh, Ru, Sm, Se, Sr, Ta, Te, Tb, Tm, Sn, Ti, W, V, Yb, Y, Zr, Pd, In, Ir, or Li.
19. 19. The organic-inorganic hybrid material of any one of claims 14 to 18, wherein the first and second metal, metalloid or semiconductor compounds or components are independently selected from metal oxides, metal nitrides, metal sulfides and zero-valent metals.
20. The first and second metal, semimetal or semiconductor compounds or components are selected from the group consisting of Al 2 O 3 , ZnO, SiO 2 , In 2 O 3 and TiO 2 The organic-inorganic hybrid material according to any one of claims 14 to 19, wherein the organic-inorganic hybrid material is independently selected from the following:
21. 21. The organic-inorganic hybrid material according to any one of claims 14 to 20, wherein the mono- or oligo-functional organic molecules are aliphatic or aromatic mono- or oligo-functional organic molecules having one or more functional groups selected from hydroxyl, amino, carboxylic acid, ester, amide, silane, thiol, epoxy, nitro and acid halide.
22. The organic-inorganic hybrid material according to any one of claims 14 to 21, wherein the mono- or oligo-functional organic molecule is a monofunctional organic molecule.
23. The organic-inorganic hybrid material according to any one of claims 14 to 22, wherein the impregnated layer has a thickness of more than 1 nm.
24. The organic-inorganic hybrid material according to any one of claims 14 to 22, wherein the impregnated layer has a thickness of 1 to 200 nm.
25. Use of the organic-inorganic hybrid material according to any one of claims 14 to 24 in the manufacture of flexible and light polymer transistors, capacitors, optoelectronic devices, barriers, absorbers, personal safety equipment, sporting goods, protective laminates, building materials, textiles, automotive materials and aerospace materials.
Citation Information
Patent Citations
Atomic layer deposition process for tungsten material
JP2009024252A
Gas barrier film, method for producing the same, and electronic device using the same
JP2018089976A
Boron-containing compounds, compositions, and methods for the deposition of a boron containing films
US20160293410A1
Oleophilic foams for oil spill mitigation
US20170166456A1