Method for cleaning chamber of substrate processing apparatus

The chamber cleaning method addresses by-product accumulation by etching with chlorine and hydrogen gases and coating with metal oxides to prevent corrosion and enhance thin film quality.

JP7587534B2Active Publication Date: 2024-11-20JUSUNG ENG
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2021576874
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-07-08
Filing Date
2020-07-07
Publication Date
2024-11-20
Estimated Expiration
2040-07-07

AI Technical Summary

Technical Problem

The accumulation of by-products inside the chamber of a substrate processing apparatus leads to particle generation, which can cause defects in thin films and damage the chamber due to corrosion from hydrogen chloride formation when exposed to moisture.

Method used

A chamber cleaning method involving a stabilization step that includes etching by-products with chlorine and hydrogen gases, followed by a protective film coating using metal oxides like aluminum, zirconium, and hafnium oxides to prevent corrosion, and optionally a seasoning process to mimic the deposition environment.

Benefits of technology

Prevents chamber corrosion and improves thin film properties by blocking impurities and reducing performance variations, ensuring effective protection against hydrogen chloride formation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007587534000001
    Figure 0007587534000001
  • Figure 0007587534000002
    Figure 0007587534000002
  • Figure 0007587534000003
    Figure 0007587534000003
Patent Text Reader

Abstract

A chamber cleaning method according to an embodiment of the present invention includes a chamber stabilization process for removing a substrate from a chamber after a thin film deposition process and processing the interior of the chamber. The chamber stabilization process includes a cleaning process for injecting a cleaning gas into the chamber to etch and clean by-products generated by the thin film deposition, and a coating process for injecting a gas containing at least one of aluminum (Al), zirconium (Zr), and hafnium (Hf) as a coating gas into the chamber to form a protective film on the inner wall of the chamber and on the surface of at least one of components disposed inside the chamber.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for cleaning a chamber of a substrate processing apparatus, and more particularly to a method for cleaning a chamber including a stabilization step for preventing damage to the inside of the chamber. [Background technology]

[0002] In general, semiconductor devices are manufactured by depositing various materials on a substrate in the form of thin films and then patterning the deposited materials. To achieve this, various processes, such as a deposition process, an etching process, a cleaning process, and a drying process, are performed. Here, the deposition process is for forming a thin film having properties required for a semiconductor device on a substrate. However, during the deposition process for forming a thin film, by-products including deposition materials are accumulated not only in desired areas on the substrate but also inside a chamber where the deposition process is performed.

[0003] Furthermore, as the by-products that accumulate inside the chamber increase in thickness, they peel off and become the cause of particle generation. Furthermore, the particles can get into the thin film formed on the substrate or adhere to the surface of the thin film, causing defects and increasing the product failure rate. Therefore, it is necessary to remove the by-products that accumulate inside the chamber before they peel off.

[0004] The cleaning process to remove by-products accumulated inside the chamber uses chlorine (Cl) gas and hydrogen (H) gas, which reacts with chlorine (Cl) gas to produce hydrogen chloride (HCl) gas, which etches the by-products accumulated inside the chamber, thereby removing them.

[0005] Meanwhile, the temperature inside the chamber may vary in different parts, and in parts with a low temperature, for example, below 150°C, products containing chlorine (Cl) generated by the etching reaction between hydrogen chloride (HCl) and by-products may accumulate and remain.

[0006] In addition, there may be cases where the chamber must be opened due to changes in the state of the deposition device, process conditions, and the external environment. When the chamber is opened, the inside of the chamber is exposed to the atmosphere, and at this time, deposits containing chlorine (Cl) that have accumulated inside the chamber during or after cleaning react with moisture in the atmosphere, resulting in the production of hydrogen chloride (HCl). This hydrogen chloride (HCl) may corrode the inside of the chamber, for example, the inner wall, susceptor, and gas injection unit of the chamber, causing damage to the chamber. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] Republic of Korea Patent No. KR 10-1232904 Summary of the Invention [Problem to be solved by the invention]

[0008] The present invention provides a method for cleaning a chamber that can prevent damage to the interior of the chamber.

[0009] The present invention provides a method for cleaning a chamber that can improve thin film properties. [Means for solving the problem]

[0010] A method for cleaning a chamber according to an embodiment of the present invention includes a chamber stabilization process for removing a substrate after a thin film deposition process from the chamber and treating the inside of the chamber, the chamber stabilization process including a cleaning process for etching and cleaning by-products generated by the thin film deposition by injecting a cleaning gas into the inside of the chamber, and a coating process for forming a protective film on an inner wall of the chamber and on at least one surface of components disposed inside the chamber by injecting a gas containing at least one of aluminum (Al), zirconium (Zr) and hafnium (Hf) as a coating gas into the chamber.

[0011] The cleaning gas contains at least one of chlorine (Cl) and hydrogen (H).

[0012] The cleaning step includes generating a plasma within the chamber.

[0013] The protective film formed by the coating process comprises a metal oxide film.

[0014] The protective film includes at least one of aluminum oxide, zirconium oxide, and hafnium oxide.

[0015] The protective film is preferably formed to a thickness of 100 Å or more.

[0016] The chamber stabilization process includes a seasoning process performed after the coating process, and the seasoning process includes a process of injecting a deposition gas used in the deposition process.

[0017] It is preferable that the seasoning thin film deposited on the inside of the chamber by the seasoning process has a thickness of 100 Å or more.

[0018] The thin film deposited on the substrate by the deposition process may be a metal oxide film.

[0019] The metal oxide film deposited on the substrate by the deposition process may be an active layer of a thin film transistor.

[0020] In forming the active layer in the deposition process, zinc oxide (ZnO) may be doped with at least one of indium (In) and gallium (Ga). Effect of the Invention

[0021] In the chamber stabilization process according to the embodiment of the present invention, after the interior of the chamber is cleaned, a protective film coating process is performed in situ.

[0022] The protective film coating process may cause damage to the inner parts of the chamber and the inner wall surface of the chamber during or after a cleaning process of the chamber using a corrosive gas.

[0023] Therefore, by carrying out the protective film coating process, it is possible to suppress the reaction of the parts exposed to corrosion after the cleaning process with moisture. Therefore, it is possible to prevent or suppress the generation of corrosive substances, such as hydrogen chloride (HCl), and to suppress the corrosion, i.e., damage, of the inside of the chamber.

[0024] In addition, after the protective film coating process, a seasoning process may be further performed in situ inside the chamber. When the seasoning process is performed, the inside of the chamber is created in an atmosphere substantially the same as that during the subsequent thin film deposition process, and elements that act as impurities during the thin film deposition process can be reduced, resulting in improved thin film characteristics after the protective film coating process and the seasoning process. In addition, the performance of the device, for example, a thin film transistor, is improved and performance variations are reduced.

[0025] Furthermore, in an embodiment of the present invention, the deposition process and the chamber stabilization process are performed in situ, which effectively blocks the inflow of impurities into the chamber, thereby more effectively preventing or suppressing corrosion in the chamber. [Brief description of the drawings]

[0026] [Figure 1] 1 is a diagram showing a substrate processing apparatus that performs a chamber cleaning method according to an embodiment of the present invention; [Diagram 2] FIG. 2 is a flow chart showing a chamber cleaning method according to the first embodiment of the present invention. [Diagram 3] FIG. 6 is a flowchart showing a chamber cleaning method according to a second embodiment of the present invention. [Figure 4] FIG. 1 is a diagram illustrating a thin film transistor. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0027] Hereinafter, the embodiments of the present invention will be described in more detail with reference to the accompanying drawings. However, the present invention is not limited to the embodiments disclosed below, and may be embodied in various different forms. These embodiments are provided merely to complete the disclosure of the present invention and to fully inform those skilled in the art of the scope of the invention. In describing the present invention, the same reference numerals are used for the same components, and the drawings may be partially exaggerated in size to accurately describe the embodiments of the present invention, and the same numerals in the drawings indicate the same components.

[0028] Fig. 1 is a diagram showing a substrate processing apparatus performing a chamber cleaning method according to an embodiment of the present invention. Fig. 2 is a flow chart showing a chamber cleaning method according to a first embodiment of the present invention. Fig. 3 is a flow chart showing a chamber cleaning method according to a second embodiment of the present invention. Fig. 4 is a diagram showing a thin film transistor, and is a diagram for explaining a chamber cleaning method according to an embodiment of the present invention.

[0029] First, a chamber cleaning method according to an embodiment will be briefly described with reference to FIGS.

[0030] The chamber cleaning method according to an embodiment of the present invention includes a process of depositing a thin film on a substrate (hereinafter referred to as a thin film deposition process (S100)), and a process of cleaning and coating the inside of the chamber after the deposition is completed to remove by-products inside and prevent damage (hereinafter referred to as a chamber stabilization process (S200)). Here, the chamber stabilization process method according to the embodiment performs the thin film deposition process (S100) and the chamber stabilization process (S200) in situ in one substrate processing apparatus.

[0031] Here, the chamber stabilization process (S200), like the first embodiment, includes a chamber cleaning process (S210) for removing by-products inside the chamber after the thin film deposition process (S100) is completed, and a protective film coating process (S220) for coating a protective film on the inside of the chamber after cleaning is completed.

[0032] In addition, the chamber stabilization process (S200) may further include a seasoning process (S230) for adjusting the interior of the chamber to approximately the same atmosphere as that of the subsequent deposition process after the protective film coating process (S220) is completed, as in the second embodiment shown in FIG. 3.

[0033] Here, the thin film deposition may be referred to as a thin film deposition process (S100), the cleaning of the chamber may be referred to as a chamber cleaning process (S210), the coating of the protective film may be referred to as a protective film coating process (S220), and the seasoning may be referred to as a seasoning process (S230).

[0034] Hereinafter, a substrate processing apparatus that performs a chamber cleaning method according to an embodiment of the present invention will be described with reference to FIG.

[0035] As described above, the substrate processing apparatus performs the deposition process (S100) of depositing a thin film on the substrate 10 and the chamber stabilization process (S200) in situ, and the deposition process (S100) may be a process of depositing a metal oxide film.

[0036] More specifically, the deposition process (S100) using the substrate processing apparatus may be a process of forming a metal oxide thin film for forming an active layer of a thin film transistor. The metal oxide film, i.e., the active layer, formed in the deposition process (S100) may be, for example, a thin film in which zinc oxide (ZnO) is doped with at least one of indium (In) and gallium (Ga). That is, it may be any one of an IZO thin film in which zinc oxide (ZnO) is doped with indium (In), a GZO thin film in which zinc oxide (ZnO) is doped with gallium (Ga), and an IGZO thin film in which zinc oxide (ZnO) is doped with indium (In) and gallium (Ga).

[0037] Referring to FIG. 1, a substrate processing apparatus according to an embodiment of the present invention includes a chamber 100, first to third gas supply units 200, 300, 400 each supplying a different type of gas, a first path 541 through which gas supplied from the first and third gas supply units 200, 400 moves, and a second path 542 through which gas supplied from the second gas supply unit 300 moves. The apparatus also includes an injection unit 500 disposed inside the chamber 100 for injecting gas, and a susceptor 600 disposed inside the chamber 100 facing the injection unit 500, with a substrate 10 placed on one side facing the injection unit 500.

[0038] The chamber 100 may also be provided with an RF power supply unit 700 that supplies power for generating plasma inside the chamber 100 .

[0039] The chamber 100 may have a process space in which a thin film can be formed on the substrate 10 carried therein. For example, the cross-sectional shape may be a square, an equilateral triangle, a hexagon, etc. Needless to say, the shape of the inside of the chamber 100 may vary in many ways, and is preferably provided to correspond to the shape of the substrate 10.

[0040] The injection section 500 is arranged inside the chamber 100 facing the susceptor 600, and comprises a first plate 510 having holes (hereinafter referred to as injection holes 511) arranged in a line in the extension direction of the susceptor 600 and spaced apart from each other, and a plurality of nozzles 520 arranged to fit into each of the plurality of injection holes 511.

[0041] The injection section 500 also includes a second plate 530 arranged inside the chamber 100 so as to be positioned between the upper wall of the chamber 100 and the first plate 510, and an insulating section 560 positioned between the first plate 510 and the second plate 530.

[0042] Here, the first plate 510 may be connected to the RF power supply unit 700, and the second plate 530 may be grounded. And, the insulating unit 560 serves to prevent electrical connection between the first plate 510 and the second plate 530.

[0043] The first plate 510 may be in the form of a plate extending in the extension direction of the susceptor 600. The first plate 510 is provided with a plurality of injection holes 511, each of which is provided so as to penetrate the first plate 510 in the up-down direction. The plurality of injection holes 511 are arranged side by side in the extension direction of the first plate 510 or the susceptor 600.

[0044] Each of the nozzles 520 may be shaped to extend in the vertical direction, have a passage therein through which gas can pass, and have upper and lower ends open. Each of the nozzles 520 is disposed such that at least its lower portion is fitted into the injection hole 511 provided in the first plate 510, and its upper portion is connected to the second plate 530. For this reason, the nozzles 520 can be described as having a shape that protrudes downward from the second plate 530.

[0045] The outer diameter of nozzle 520 is set smaller than the inner diameter of injection hole 511, and is disposed so that, when nozzle 520 is fitted into injection hole 511, the outer peripheral surface of nozzle 520 is separated from the peripheral wall of injection hole 511, i.e., the inner wall of first plate 510. For this reason, the inside of injection hole 511 is partitioned into an outer space of nozzle 520 and an inner space of nozzle 520.

[0046] The passage in the nozzle 520 in the injection hole 511 is a passage through which the gas provided from the first and third gas supply parts 200 and 400 moves and is injected. The outer space of the nozzle 520 in the injection hole 511 is a passage through which the gas provided from the second gas supply part 300 moves and is injected.

[0047] Therefore, hereinafter, the passage inside the nozzle 520 will be referred to as a first path 541, and the outer space of the nozzle 520 inside the injection hole 511 will be referred to as a second path 542.

[0048] The second plate 530 is disposed such that its upper surface is separated from the upper wall inside the chamber 100 and its lower surface is separated from the first plate 510. Therefore, an empty space is provided between the second plate 530 and the first plate 510 and between the second plate 530 and the upper wall of the chamber 100.

[0049] Here, the upper space of the second plate 530 is a space where the gas provided from the first and third gas supply units 200, 400 described below spreads and moves (hereinafter referred to as a gas diffusion space 550), and is connected to the upper openings of the multiple nozzles 520. In other words, the gas diffusion space 550 is a space connected to the multiple first paths 541. Therefore, the gas provided from the first and third gas supply units 200, 400 and supplied to the gas diffusion space 550 is supplied to the multiple first paths 541 and sprayed.

[0050] In addition, a gundrill (not shown) which is a passage through which gas moves is provided inside the second plate 530, and the gundrill is connected to a second transfer pipe 320 of the second gas supply unit 300 described below and is provided to communicate with the second path 542. Therefore, the gas provided from the second gas supply unit 300 can be sprayed onto the substrate 10 via the gundrill of the second plate 530 and the second path 542.

[0051] The first to third gas supply units 200, 300, 400 may supply different types of gas to the process space of the chamber. In the following, for ease of explanation, the gas provided by the first gas supply unit 200 is referred to as the first gas, the gas provided by the second gas supply unit 300 is referred to as the second gas, and the gas provided by the third gas supply unit 400 is referred to as the third gas.

[0052] Then, a chamber cleaning method may be performed using the substrate processing apparatus according to the embodiment, and a deposition process and a chamber stabilization process may be performed, each of which may be performed by a reactant between the first gas and the second gas.

[0053] For this purpose, the first and second gas supply units 200 and 300 are provided to supply gases for a deposition process and a stabilization process for processing the inside of the chamber. At this time, the second gas supplied from the second gas supply unit 300 is a gas that reacts with the first gas supplied from the first gas supply unit 200. And, the third gas supply unit 400 supplies a gas for purging during the processing process of the chamber.

[0054] In other words, the first gas provided from the first gas supply unit 200 and the second gas provided from the second gas supply unit 300 each include a gas for deposition and a cleaning gas for chamber processing. That is, the first gas and the second gas may each include a gas for deposition, cleaning, and protective film coating. And, the third gas provided from the third gas supply unit 400 includes a purge gas for purging when coating a protective film in the chamber processing process.

[0055] The first to third gas supply units 200, 300, and 400 will be described below.

[0056] The first gas supply unit 200 includes a first storage unit 210 in which a first gas is stored, and a first transfer pipe 220 having one end connected to the first storage unit 210 and the other end connected to the gas diffusion space 550, and having a passage therein through which the first gas moves. Therefore, the first gas provided from the first storage unit 210 can move through the gas diffusion space 550 and the multiple nozzles 520, i.e., the multiple first paths 541, and be sprayed.

[0057] The first storage section 210 may include a first deposition gas storage section 211 in which a first deposition gas for deposition is stored, a first cleaning gas storage section 212 in which a first cleaning gas for cleaning is stored, and a first coating gas storage section 213 in which a first coating gas for protective film coating is stored.

[0058] The first deposition gas stored in the first deposition gas storage unit 211 is a source raw material gas for thin film deposition, and the first deposition gas storage unit 211 may store a raw material gas containing zinc (Zn), a raw material gas containing indium (In), and a raw material gas containing gallium (Ga) in canisters (not shown) of the respective source gases and supply them to the chamber 100. That is, the first deposition gas supplied to the chamber 100 via the first transfer pipe 220 may include a raw material gas containing zinc (Zn), a raw material gas containing indium (In), and a raw material gas containing gallium (Ga).

[0059] In this case, a raw material gas containing zinc (Zn), a raw material gas containing indium (In), and a raw material gas containing gallium (Ga) may be stored in one first deposition gas storage section 211, or the first deposition gas storage section 211 may be divided into three storage sections, each of which stores a raw material gas containing zinc (Zn), a raw material gas containing indium (In), and a raw material gas containing gallium (Ga), respectively.

[0060] Here, at least one of diethyl zinc (Zn(C2H5)2) (DEZ) and dimethyl zinc (Zn(CH3)2) (DMZ) can be used as a source gas containing zinc (Zn), at least one of trimethyl indium (In(CH3)3) (TMIn) and diethylamino propyl dimethyl indium (DADI) can be used as a source gas containing indium (In), and trimethyl gallium (Ga(CH3)3) (TMGa) can be used as a source gas containing gallium (Ga).

[0061] The first cleaning gas stored in the first cleaning gas storage unit 212 is a source raw material gas for removing by-products inside the chamber 100, and may store, for example, a raw material gas containing chlorine (Cl) in the first cleaning gas storage unit 212. That is, the first cleaning gas may contain a raw material gas containing chlorine (Cl). Here, at least one of Cl2, BCl3, and ClF3 may be used as the raw material gas containing chlorine (Cl).

[0062] The first coating gas stored in the first coating gas storage portion 213 is a source raw material gas for coating a protective film on the inside of the chamber 100 after the cleaning process.

[0063] In an embodiment, the inside of the chamber 100 after the cleaning process is coated with a protective film, which may be formed of a metal oxide film. More specifically, the protective film may be formed of any one of aluminum oxide such as Al2O3, zirconium oxide such as ZrO2, and hafnium oxide such as HFO2.

[0064] For this reason, the first coating gas storage section 213 stores a source raw material gas for forming any one of aluminum oxide, zirconium oxide, and hafnium oxide, and may store, for example, at least one of a raw material gas containing aluminum (Al), a raw material gas containing zirconium (Zr), and a raw material gas containing hafnium (Hf). That is, the first coating gas may contain at least one of a raw material gas containing aluminum (Al), a raw material gas containing zirconium (Zr), and a raw material gas containing hafnium (Hf).

[0065] Here, TMA (trimethylaluminum; AC(H3)3) can be used as a source gas containing aluminum (Al), TEMAZr (Tetrakis(ethylmethylamino)Zr) can be used as a source gas containing zirconium (Zr), and TEMAH (tetrakis-ethyl methyl amino hafnium; Hf[NC2H5CH3]4) and TDEAH (tetrakis-diethyl amino hafnium; Hf[NC2H 52 ]4), TDMAH(tetrakis-dimethyl amino hafnium;Hf[NCH 32 ]4), Hf[NC3H 72 ]4, Hf[NC4H 92 ]4 can be used.

[0066] The first transfer pipe 220 is a means for transferring the first gas provided from the first storage section 210 to the first path 541. That is, during the deposition process, the first deposition gas provided from the first deposition gas storage section 211 transfers to the plurality of nozzles 520 through the first transfer pipe 220 and the gas diffusion space 550. During the cleaning process, the first cleaning gas provided from the first cleaning gas storage section 212 transfers to the plurality of nozzles 520 through the first transfer pipe 220 and the gas diffusion space 550. During the coating process, the first coating gas provided from the first coating gas storage section 213 transfers to the plurality of nozzles 520 through the first transfer pipe 220 and the gas diffusion space 550.

[0067] The first transfer pipe 220 may have a pipe shape with a passage through which gas can move inside, and may be provided with valves 230a, 230b, and 230c for controlling communication between the first deposition gas reservoir 211, the first cleaning gas reservoir 212, and the first coating gas reservoir 213 and the first transfer pipe 220, respectively, and adjusting the amount of gas transferred.

[0068] The second gas supply unit 300 includes a second storage unit 310 in which the second gas is stored, and a second transfer pipe 320 having one end connected to the second storage unit 310 and the other end connected to a gun drill provided inside the second plate 530, and having a passage provided therein through which the second gas moves. Therefore, the second gas provided from the second storage unit 310 can be sprayed through the second transfer pipe 320 and the gun drill of the second plate 530, and then through the second path 542 provided inside the first plate 510.

[0069] The second storage section 310 includes a second deposition gas storage section 311 in which a gas for deposition (a second deposition gas) is stored, a second cleaning gas storage section 312 in which a gas for cleaning (a second cleaning gas) is stored, and a second coating gas storage section 313 in which a gas for protective film coating (a second coating gas) is stored.

[0070] The second deposition gas stored in the second deposition gas storage unit 311 may be a reactant gas that reacts with the first deposition gas to generate a reactant for thin film deposition. That is, the second deposition gas may be a reactant gas that is different from the first deposition gas and can react with the first deposition gas, for example, the second deposition gas may be a reactant gas containing oxygen (O). Here, at least one of pure oxygen (O2), nitrogen dioxide (N2O), and ozone (O3) can be used as the reactant gas containing oxygen (O), i.e., the second deposition gas.

[0071] The second cleaning gas stored in the second cleaning gas storage section 312 may be a reactant gas that reacts with the first cleaning gas to generate a reactant for removing by-products. That is, the second cleaning gas may be a reactant gas that is different from the first cleaning gas and can react with the first cleaning gas, and for example, the second cleaning gas may be a reactant gas containing hydrogen (H). Here, at least one of H2, CH4, and H2O can be used as the reactant gas containing hydrogen (H), i.e., the second cleaning gas.

[0072] The second coating gas stored in the second coating gas storage section 313 may be a reactive raw material gas that reacts with the first coating gas to generate a reactant for coating the protective film. That is, the second coating gas may be a gas different from the first coating gas and a reactive raw material gas that can react with the first coating gas. As described above, when the protective film is formed from any one of aluminum oxide, zirconium oxide, and hafnium oxide, and the first coating gas is a raw material gas containing any one of aluminum (Al), zirconium (Zr), and hafnium (Hf), the second coating gas may be a gas containing oxygen (O). Here, as the gas containing oxygen (O), i.e., the second coating gas, at least one of pure oxygen (O2), nitrogen dioxide (N2O), and ozone (O3) can be used.

[0073] The second transfer pipe 320 may be a means for moving the second gas provided from the second storage section 310 to the second path 542. That is, during the deposition process, the second deposition gas provided from the second deposition gas storage section 311 passes through the second transfer pipe 320 and the gun drill provided on the second plate 530 and moves to the second path 542, during the cleaning process, the second cleaning gas provided from the second cleaning gas storage section 312 passes through the second transfer pipe 320 and the gun drill provided on the second plate 530 and moves to the second path 542, and during the coating process, the second coating gas provided from the second coating gas storage section 313 passes through the gun drill provided on the second transfer pipe 320 and the second plate 530 and moves to the second path 542. Then, each of the second deposition gas, the second cleaning gas, and the second coating gas may be sprayed onto the substrate via the second path 542.

[0074] Such a second transport pipe 320 may be in the shape of a pipe having a passage therein through which gas can move, or may be in the shape of a gun drill (not shown) that drills a long, straight hole in the second plate 530 of the chamber 100 to allow the gas to flow.

[0075] Valves 330a, 330b, and 330c may be provided to control communication between the second deposition gas storage section 311, the second cleaning gas storage section 312, and the second coating gas storage section 313, respectively, and the second transport pipe 320, and to adjust the amount of gas transported.

[0076] As described above, the second deposition gas and the second coating gas may both be gases containing oxygen (O), or the same gas may be used. In this manner, when the same gas is used as the second deposition gas for thin film deposition and the second coating gas for protective film coating, the second reservoir 310 may be provided to include either the second deposition gas reservoir 311 or the second coating gas reservoir 313.

[0077] Needless to say, different gases may be used as the second deposition gas and the second coating gas. In this case, the second reservoir 310 may be provided with a second deposition gas reservoir 311 and a second coating gas reservoir 313, each of which stores a different gas.

[0078] The third gas supply unit 400 includes a third storage unit 410 in which a third gas is stored, and a third transfer pipe 420 having one end connected to the third storage unit 410 and the other end connected to the gas diffusion space 550, and having a passage therein through which the third gas moves. Therefore, the third gas provided from the third storage unit 410 can move through the gas diffusion space 550 and the multiple nozzles 520, i.e., the multiple first paths 541, and be sprayed.

[0079] A gas for purging during the formation of a protective film (hereinafter, referred to as a purge gas) is stored in the third storage section 410. The purge gas stored in the third storage section 410 may be an inert gas, for example, nitrogen gas.

[0080] The third transfer pipe 420 is a means for transferring the third gas, i.e., the purge gas, provided from the third reservoir 410 to the injection unit 500. That is, the third deposition gas provided from the third reservoir 410 during the protective film coating process passes through the third transfer pipe 420 and the gas diffusion space 550, and then transfers to the multiple nozzles 520.

[0081] Such third transport pipe 420 may be in the form of a pipe having a passage through which gas can move inside. A valve 430 may be provided to control communication between third storage section 410 and third transport pipe 420 and adjust the amount of gas transported.

[0082] The susceptor 600 is disposed in the chamber 100 so as to face or oppose the ejection unit 500. In this case, the susceptor 600 may be located, for example, below the ejection unit 500 in the chamber 100. The susceptor 600 may be provided in a shape corresponding to the shape of the substrate 10, for example, a square or a circle. The area of ​​the susceptor 600 is preferably larger than that of the substrate 10. The susceptor 600 may be a component incorporating a heater (not shown) and a cooling means (not shown), and at least one of the heater and the cooling means may be operated to adjust the susceptor 600 and the substrate 10 to a target temperature.

[0083] The above-mentioned chamber 100, injection part 500, and susceptor 600 may be formed from a material including a metal, for example, aluminum (Al).

[0084] The RF power supply unit 700 is a means for supplying power to generate plasma inside the chamber 100. More specifically, the RF power supply unit 700 is a means for supplying RF power for generating plasma, and may be connected to the first plate 510 of the injection unit 500. The RF power supply unit 700 may also include an impedance matching circuit for matching a load impedance and a source impedance of a power supply for generating plasma. The impedance matching circuit preferably includes two impedance elements including at least one of a variable capacitor and a variable inductor.

[0085] The susceptor 600 and the second plate 530 arranged to face the ejection unit 500 may each be configured to be grounded.

[0086] Therefore, when the RF power supply unit 700 supplies RF power to the first plate 510 and grounds and connects the susceptor 600 and the second plate 530, plasma can be generated in the second path 542 in the injection unit 500 and in the space between the first plate 510 and the susceptor 600.

[0087] Here, when plasma is generated in the space between the first plate 510 and the susceptor 600, the plasma is generated closer to the injection unit than the susceptor 600. More specifically, the plasma may be generated immediately below the injection unit 500.

[0088] Hereinafter, a chamber cleaning method according to a first embodiment of the present invention will be described with reference to FIGS.

[0089] 2, the chamber cleaning method includes a thin film deposition process (S100) for depositing a thin film on a substrate 10, and a chamber stabilization process (S200) for removing particles due to by-products generated during the deposition process after the thin film deposition is completed and treating the inside of the chamber 100 to prevent damage to the inside of the chamber 100. Here, the thin film deposition process (S100) and the chamber stabilization process (S200) are performed in situ.

[0090] First, for the thin film deposition process (S100), the substrate 10 is carried into the chamber 100 and placed on the susceptor 600.

[0091] Here, the thin film to be deposited in the thin film deposition process (S100) is the active layer 40 of a thin film transistor, and the active layer 40 is an IGZO film in which zinc oxide (ZnO) is doped with indium (In) and gallium (Ga) for example. Therefore, the substrate 10 placed on the susceptor 600 may be a substrate 10 having a gate electrode 20 and a gate insulating film 30 laminated thereon, as shown in FIG.

[0092] For the deposition of a thin film of the active layer 40, a first deposition gas, which is a source gas for depositing the active layer, is injected through a first passage 541 of the injection unit 500, and a second deposition gas, which is a reactant gas for depositing the active layer, is injected through a second passage 542.

[0093] For this purpose, the first gas supply unit 200 supplies the first and second deposition gases for depositing the active layer 40 to the first path 541, and the second gas supply unit 300 supplies the first and second deposition gases to the second path 542. That is, the first deposition gas including a source gas including zinc (Zn), a source gas including indium (In), and a source gas including gallium (Ga) is provided to the first transfer pipe 220 from the first deposition gas storage unit 211. For this purpose, the first deposition gas moves to the gas diffusion space 550 through the first transfer pipe 220, and is then supplied to the multiple first nozzles, i.e., the multiple first paths 541, and is sprayed. Also, the second deposition gas including oxygen is supplied to the second transfer pipe 320 from the second deposition gas storage unit 311. To this end, the second deposition gas may travel via the second transport pipe 320 and be supplied to the second passage 542 in the first plate 510 via a gun drill passage (not shown) inside the second plate 530, and then be injected from the second passage 542 into the process space.

[0094] When the first and second deposition gases are injected, the RF power supply unit 700 may supply RF power to the first plate 510. When the RF power is supplied to the first plate 510, plasma may be generated in the second passage 542 in the injection unit 500 and in a space between the first plate 510 and the susceptor 600. At this time, a reaction occurs between the first deposition gas and the second deposition gas passing through or injected through the first passage 541 and the second passage 542, and thus an IGZO film, i.e., an active layer 40, may be formed on the gate insulating film 30.

[0095] In the above example, the RF power supply unit 700 is operated to generate plasma in the deposition process for forming the active layer 40. However, the present invention is not limited thereto, and a thin film, i.e., the active layer 40, the gate insulating film 30, etc. may be formed by injecting the first deposition gas and the second deposition gas and raising the temperature of the chamber 100 to a high temperature to cause a reaction without generating plasma. After the deposition process of the active layer 40 is completed, the substrate 10 may be taken out of the chamber 100.

[0096] Next, a chamber stabilization step (S200) for treating the chamber 100 may be performed.

[0097] Meanwhile, by-products may accumulate inside the chamber 100 during the deposition process of the active layer 40. More specifically, by-products may accumulate on the inner wall of the chamber 100, the surface of the first plate 510, the surface of the nozzle 520, and the lower surface of the second plate 530. In addition, since the space between the first plate 510 and the second plate 530 is narrow and plasma is generated in this space, more by-products may accumulate on the surface of the first plate 510, the surface of the nozzle 520, and the lower surface of the second plate 530 than on the inner wall of the chamber 100.

[0098] When performing the chamber stabilization step (S200), first, the chamber is cleaned to remove by-products accumulated inside the chamber 100 during the deposition step of the active layer 40 (S210).

[0099] For this purpose, gases for cleaning the chamber are supplied to the injection part 500 from each of the first and second gas supply parts 200 and 300. That is, a first cleaning gas containing chlorine (Cl) is provided from the first cleaning gas storage part 212 to the first conveying pipe 220. For this purpose, the first cleaning gas is supplied to the first path 541 of the injection part 500 via the first conveying pipe 220, and then injected from the first path 541. Also, if a second cleaning gas containing hydrogen (H) is supplied from the second cleaning gas storage part 312 to the second conveying pipe 320, the second cleaning gas moves through the second conveying pipe 320 and is supplied to the second path 542 of the injection part 500, and then injected from the second path 542.

[0100] While the first and second cleaning gases are being injected through the injection unit 500, the RF power supply unit 700 may supply RF power to the first plate 510. This allows plasma to be generated in the second passage 542 in the injection unit 500 and in the space between the first plate 510 and the susceptor 600.

[0101] Thus, a reaction occurs between the first cleaning gas and the second cleaning gas to generate hydrogen chloride (HCl) gas. The generated hydrogen chloride (HCl) gas accumulates inside the chamber during the thin film deposition process and undergoes an etching reaction with by-products including metal oxides such as zinc oxide (see reaction formula 1). Meanwhile, the by-products accumulate not only on the inner wall of the chamber 100 but also on various components exposed to the internal space of the chamber 100, such as the susceptor 600, the nozzle 520, and the injection unit 500.

[0102] Therefore, the generated hydrogen chloride (HCl) gas reacts with the by-products accumulated inside the chamber 100, i.e., the by-products accumulated on the surfaces of the inner walls of the chamber 100, the susceptor 600, the nozzle 520, the injection part 500, etc., and etches and removes them.

[0103] Reaction formula 1) In2Ga2Zn1O7+7H2+4Cl2=2InCl3+ZnCl2+7H2O

[0104] Meanwhile, in the interior of the chamber 100, in a portion where the temperature is low, more specifically, below 150° C., products of the etching reaction between hydrogen chloride (HCl) and by-products, such as 2InCl 3 , ZnCl 2 , etc., may accumulate and remain.

[0105] In addition, after the cleaning of the chamber 100 is completed, there may be a case where the chamber 100 must be opened due to changes in the state of the deposition apparatus, process conditions, and the external environment. When the chamber 100 is opened, the inside of the chamber 100 is exposed to the atmosphere. At this time, residues containing chlorine (Cl), i.e., 2InCl3, ZnCl2, etc., inside the chamber 100 react with moisture in the atmosphere, and hydrogen chloride (HCl) is generated (see reactions 2 to 4). This hydrogen chloride (HCl) may corrode and damage the inside of the chamber 100, for example, the inner wall of the chamber 100, the injection unit 500, and the susceptor 600.

[0106] Reaction scheme 2) InCl3+H2O=InOCl+HCl+H2O

[0107] Reaction scheme 3) ZnCl2+2H2O=ZnCl(OH)+HCl+H2O

[0108] Reaction formula 4) Al(H2O)6Cl3 = AlOH)3 + 3HCl + 3H2O

[0109] Therefore, in an embodiment of the present invention, in order to prevent or suppress corrosion inside the chamber 100 due to residues from the chamber cleaning process, a protective film is coated on the inside of the chamber 100 after the chamber cleaning is completed (S220). At this time, the chamber cleaning process and the protective film coating process are performed in situ.

[0110] The chamber protective film may be formed by atomic layer deposition (ALD) by spraying the following gases in the order of "source gas, purge gas, reactive gas, purge gas." In other words, the protective film is coated by spraying the following gases in the order of "first gas, purge gas, second gas, purge gas" and repeating this spray cycle multiple times. It can also be described as "first coating gas, purge gas, second coating gas, purge gas." More specifically, first, a first coating gas containing at least one raw material gas of aluminum (Al), zirconium (Zr) and hafnium (Hf) is supplied from the first coating gas reservoir 213 to the first transfer pipe 220. Therefore, the first coating gas is supplied to the first path 541 of the injection unit 500 via the first transfer pipe 220, and can be injected into the process space in the chamber 100.

[0111] Next, the third gas is purged. That is, when the third gas, which is a purge raw material, for example, nitrogen gas, is supplied from the third storage section 410 to the first conveying pipe 220, the purge gas is supplied to the first path 541 of the ejection section 500 via the first conveying pipe 220, and then ejected and purged.

[0112] Next, a second coating gas that reacts with the first coating gas is supplied to the injection unit 500. That is, when a second coating gas containing oxygen (O) is supplied from the second coating gas storage unit 313 to the second transfer pipe 320, the second coating gas moves through the second transfer pipe 320 to a gun drill passage (not shown) of the second plate 530, and is then supplied to the second path 542 and injected into the process space in the chamber 100.

[0113] When the second coating gas containing oxygen (O) is injected, the second coating gas reacts with the first coating gas, and thus at least one reactant of aluminum oxide, zirconium oxide, and hafnium oxide is generated. Then, a film of at least one reactant of aluminum oxide, zirconium oxide, and hafnium oxide is deposited or coated on the inside of the chamber 100, for example, the inner wall of the chamber 100, the surface of the susceptor 600, and the injection unit 500. Then, in the injection unit 500, the film may be deposited on the outer circumferential surface of the nozzle 520, the inner surface of the first plate 510 that separates the first passage 541, the outer surface of the first plate 510, and the lower surface of the second plate 530. In this way, the film coated by the reaction between the first coating gas and the second coating gas is the protective film.

[0114] Then, by injecting a purge gas through the third gas supply unit 400, the reaction by-products between the first coating gas and the second coating gas can be purged.

[0115] In the above, a description has been given of forming a protective film by atomic layer deposition (ALD) performed in a cycle of "source gas, purge gas, reaction gas, purge gas."

[0116] However, the present invention is not limited to this in any way, and the protective film may be formed by a method in which a source gas, a purge gas, and a reactive gas are sprayed in this order, and then the RF power supply unit 700 is operated to generate plasma.

[0117] In other words, the protective film may be formed by spraying the first coating gas, the third gas (purge gas), and the second coating gas in that order, and then operating the RF power supply unit 700 to generate plasma.

[0118] According to another method, the protective film may be formed by injecting the source gas and the purge gas in this order, starting to inject the reactive gas before the injection of the purge gas is completed, and operating the RF power supply unit 700 to generate plasma after the injection of the reactive gas is completed.

[0119] In other words, the protective film may be formed by injecting the first coating gas and the third gas, which is a purge gas, in that order, starting to inject the second coating gas before the injection of the purge gas is completed, and operating the RF power supply unit 700 to generate plasma after the injection of the second coating gas is completed.

[0120] By the protective film coating process, residues including chlorine (Cl) remaining after the chamber cleaning process are coated with the subsequently formed protective film. Therefore, even if the chamber 100 is opened and the inside of the chamber 100 is exposed to the atmosphere due to changes in the state of the substrate processing apparatus, process conditions, and external environment, etc., the residues accumulated inside the chamber 100 can be prevented or blocked from being exposed to the atmosphere.

[0121] Therefore, the deposits generated during the cleaning process are prevented from reacting with chlorine (Cl) for several minutes. This prevents the generation of corrosive gases such as hydrogen chloride (HCl) due to the reaction between chlorine (Cl) and moisture, and prevents the inside of the chamber 100 from being corroded, i.e., damaged.

[0122] In this manner, the protective film prevents the deposition film accumulated inside the chamber 100 from reacting with moisture during the cleaning process, and therefore the protective film may be referred to as a moisture permeation prevention film.

[0123] Such a protective film is preferably formed to a thickness of 100 Å or more in order to prevent deposits formed during the cleaning process from being exposed.

[0124] On the other hand, if the thickness of the protective film is less than 100 Å, the surface roughness is not good, and therefore the protective film may not be coated in some areas or may be thin. In such a case, there is a concern that the deposits generated during the cleaning process may react with moisture in the air when the chamber is opened, which may generate corrosive gases such as hydrogen chloride (HCl) and corrode the inside of the chamber 100.

[0125] Therefore, in the embodiment of the present invention, the protective film is formed to a thickness of 100 Å or more.

[0126] Although there is no particular upper limit to the thickness of the protective film, it is sometimes preferable to set the thickness to 1000 Å or less in order to improve the operating efficiency and productivity of the substrate processing apparatus.

[0127] In the embodiment, the protective film coating process is performed in 10 minutes or less. However, the present invention is not limited thereto, and the time is not limited as long as the protective film can be formed to a target thickness of 100 Å or more.

[0128] After the coating of the protective film is completed, the substrate 10, which is the object to be subjected to deposition, may be loaded into the chamber 100, and the deposition process as described above, for example, deposition of an IGZO active layer, may be carried out.

[0129] In the above-described first embodiment, the chamber stabilization step (S200) includes the chamber cleaning step (S210) and the protective film coating step (S220).

[0130] However, the present invention is not limited thereto, and as in the second embodiment shown in FIG. 3, the chamber stabilization process (S200) may further include a seasoning process (S230) performed after the protective film coating process (S220).

[0131] The seasoning process (S230) is a process of treating the inside of the chamber 100 in substantially the same environment as during the subsequent deposition process. That is, the seasoning process may be a process of supplying gases used during the deposition process, i.e., first and second deposition gases, from the first and second gas supply units 200 and 300, respectively, to the injection unit 500 in a state where the substrate 10 is not present inside the chamber 100.

[0132] For example, a first deposition gas including a raw material gas containing zinc (Zn), a raw material gas containing indium (In), and a raw material gas containing gallium (Ga) is supplied to the injection part from the first gas supply unit 200, and a second deposition gas including oxygen is supplied to the injection part from the second gas supply unit 300, and the first and second deposition gases are injected through the injection part 500.

[0133] At this time, a reaction occurs between the first deposition gas and the second deposition gas, which allows a seasoning thin film, i.e., IGZO, to be deposited inside the chamber 100, i.e., on the inner wall of the chamber 100, the susceptor 600, and the surface of the injection part 500.

[0134] Also, when the first deposition gas and the second deposition gas are injected, the RF power supply unit 700 may be operated to supply RF power to the injection unit 500 to generate plasma inside the chamber 100 .

[0135] Needless to say, when the first deposition gas and the second deposition gas are injected, seasoning may be performed without forming plasma.

[0136] In this way, by coating the inside of the chamber 100 with a protective film and then seasoning the inside of the chamber 100 before the subsequent deposition process, it is possible to prevent or suppress at least one of the metal materials forming the protective film, for example, aluminum (Al), zirconium (Zr), and hafnium (Hf), from acting as an impurity in the deposition film, for example, an IGZO thin film, deposited in the subsequent deposition process, thereby improving the performance of the thin film transistor and reducing the performance variation.

[0137] The thickness of the seasoning thin film is preferably 100 Å or more, because when the thickness is 100 Å or more, the protective film can effectively suppress deterioration in the performance of a thin film deposited in a subsequent deposition process, for example, an IGZO thin film for an active layer.

[0138] The upper limit of the thickness of the seasoning thin film is not particularly limited, but is preferably 1000 Å or less in order to improve the operating efficiency and productivity of the substrate processing apparatus.

[0139] After the seasoning step is completed, the substrate 10, which is the object to be vapor-deposited, may be loaded into the chamber 100, and the vapor deposition step as described above may be carried out.

[0140] After the process of forming the active layer 40 is completed, the substrate is transferred to an apparatus for the subsequent process, where a protective film 60 and source and drain electrodes 50a, 50b are formed, thereby completing a thin film transistor.

[0141] As described above, according to the chamber cleaning method of the embodiment of the present invention, after the cleaning process of the inside of the chamber 100 is completed, a protective film coating process is performed. That is, the deposition film containing chlorine (Cl) that has accumulated inside the chamber 100 during or after the cleaning process is coated with a protective film to prevent a reaction between the deposition film and moisture. This makes it possible to prevent the generation of hydrogen chloride (HCl), which is a corrosive substance, and to prevent the inside of the chamber 100 from being corroded, i.e., damaged.

[0142] After the protective film is coated, a seasoning process may be further performed inside the chamber 100. When the seasoning process is performed, the inside of the chamber 100 is created in an atmosphere substantially the same as that during the subsequent deposition process, and elements that act as impurities during the deposition process can be reduced, thereby improving thin film characteristics. In addition, the performance of elements, for example, thin film transistors, is improved, and the occurrence of performance variations is reduced. [Industrial Applicability]

[0143] According to an embodiment of the present invention, it is possible to suppress the reaction of the parts exposed to corrosion with moisture after the cleaning process, and therefore it is possible to prevent or suppress the generation of corrosive substances, such as hydrogen chloride (HCl), and to suppress the corrosion, i.e., damage, of the inside of the chamber.

Claims

1. A chamber stabilization process is performed by removing the substrate from the chamber after the thin film deposition process and processing the inside of the chamber; The chamber stabilization step includes: a cleaning process in which a cleaning gas is injected into the chamber to etch and clean by-products generated during the thin film deposition process; a coating step of injecting a gas containing at least one of aluminum (Al), zirconium (Zr) and hafnium (Hf) as a first coating gas into the chamber to form a protective film on the inner wall of the chamber and on at least one surface of a component disposed inside the chamber; Including, The coating step includes: injecting a first coating gas into the chamber; injecting a purge gas into the chamber; injecting a second coating gas containing oxygen (O) into the chamber; generating a plasma within the chamber after the second coating gas injection is terminated; A method for cleaning a chamber, comprising:

2. 2. The method of claim 1, wherein the cleaning gas includes at least one of chlorine (Cl) and hydrogen (H).

3. The method of claim 1 , wherein the cleaning step includes the step of generating a plasma inside the chamber.

4. The chamber cleaning method of claim 1 , wherein the protective film formed by the coating step comprises a metal oxide film.

5. 5. The method of claim 4, wherein the protective film includes at least one of aluminum oxide, zirconium oxide, and hafnium oxide.

6. 5. The method of claim 4, wherein the protective film is formed to a thickness of 100 Å or more.

7. the chamber stabilization step includes a seasoning step performed after the coating step, The method of claim 1 , wherein the seasoning step includes a step of injecting a deposition gas used in a deposition step.

8. 8. The method of claim 7, wherein the seasoning thin film deposited on the inside of the chamber has a thickness of 100 Å or more.

9. 8. The chamber cleaning method of claim 7, wherein the thin film deposited on the substrate by the deposition process is a metal oxide film.

10. 10. The method of claim 9, wherein the metal oxide film deposited on the substrate by the deposition process is an active layer of a thin film transistor.

11. When forming the active layer in the vapor deposition process, 11. The chamber cleaning method according to claim 10, wherein the electrode is formed by doping zinc oxide (ZnO) with at least one of indium (In) and gallium (Ga).

Citation Information

Patent Citations

  • Methods for monitoring the status of system components

    JP2007507887A

  • Atomic layer deposition of protective coatings for semiconductor process chamber components

    JP2017199907A

  • A chemical vapor deposition apparatus and cleaning method of chemical vapor deposition

    KR101232904B1