Casting Equipment

The implementation of a sprue opening/closing plate with annular grooves and inert gas supply in the casting apparatus addresses impurity and oxidation issues, enhancing casting quality and efficiency by preventing leakage and contamination.

JP7589581B2Active Publication Date: 2024-11-26UBE MASCH CORP LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2021024821
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-02-19
Publication Date
2024-11-26
Estimated Expiration
2041-02-19

AI Technical Summary

Technical Problem

Existing vertical casting apparatuses face issues with impurities mixing with molten metal due to exposure to air, leading to oxidation and contamination, which results in casting defects, and the automatic opening/closing devices used to prevent this face challenges with leakage and deformation under pressure.

Method used

A sprue opening/closing plate with annular grooves and an inert gas supply system is implemented to prevent foreign matter entry and molten metal leakage, ensuring stable casting quality by capturing leaked metal and preventing oxidation.

Benefits of technology

The solution effectively prevents foreign matter contamination and oxidation, stabilizes the casting process, and reduces defects, thereby improving casting quality and cycle efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007589581000001
    Figure 0007589581000001
  • Figure 0007589581000002
    Figure 0007589581000002
  • Figure 0007589581000003
    Figure 0007589581000003
Patent Text Reader

Abstract

To suppress occurrence of defective casting caused by molten metal leakage and foreign substance contamination into a hot-water supply pipe, in a casting molding machine for filling molten metal in a holding furnace into a mold cavity through the hot-water supply pipe.SOLUTION: A casting apparatus capable of shortening a casting molding cycle, and obtaining stably a high quality casting, includes a sprue opening / closing plate provided with an annular groove aiming at opening / closing of the sprue, and at prevention of molten metal leakage and foreign substance contamination so as to enclose a spout for allowing communication between the sprue and a hot-water supply pipe, on a connection part between the sprue of a mold cavity and the hot-water supply pipe.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a casting apparatus that fills a molten metal in a holding furnace into a die cavity at low pressure via a molten metal supply pipe. [Background technology]

[0002] As a casting apparatus for filling the mold cavity of a casting mold with molten metal such as aluminum alloy at low pressure to obtain a casting product, for example, a vertical casting apparatus is generally used in which a holding furnace for holding the molten metal and a casting mold are arranged vertically, the holding furnace and the casting mold are connected by a hot water supply pipe, and the molten metal is filled into the mold cavity through the hot water supply pipe. Using this vertical casting apparatus, casting molding is repeated until the planned number of casting products are obtained. There are three methods for filling the mold cavity with molten metal: a piston method that mechanically pushes out the molten metal in the hot water supply pipe, a pressurization method that uses a sealed holding furnace and sends compressed air or other pressurized gas to push up the molten metal in the hot water supply pipe, and a suction method that reduces the pressure inside the mold cavity and sucks up the molten metal in the hot water supply pipe. After filling with the molten metal, the molten metal is pressurized while solidifying to obtain a casting product. The pressurization of the molten metal can be appropriately selected from a variety of means, such as increasing the pressure of the molten metal in the supply pipe and refilling the molten metal from the sprue, or closing the sprue with a seal pin or the like machined into the casting mold and pressurizing the molten metal with a pressurizing mechanism.

[0003] In the case of a vertical casting machine, the lower part of the supply pipe is immersed in the molten metal in the holding furnace, and the upper part is open. Therefore, there is a risk that impurities such as casting burrs and release agents may get into the supply pipe during any of the following steps: during the product removal process in which the casting mold is opened to remove the casting, during the air blow cleaning process to remove molten metal residues remaining in the mold cavity, and during the release agent application process in which a release agent is applied to the mold cavity, the gate, etc. in preparation for the next shot of casting. As a result, the molten metal mixed with impurities is filled into the mold cavity, causing casting defects due to the inclusion of foreign matter. In addition, when the pipe is exposed to the atmosphere, the molten metal in the pipe is exposed to air, which causes the molten metal to oxidize and produce oxides that can lead to contamination. Furthermore, the surface temperature of the molten metal also drops. As a result, the molten metal in the pipe becomes a mixture of oxides and solidified molten metal. If the molten metal is filled into the mold cavity in this state, it will cause casting defects due to contamination.

[0004] In order to prevent contamination by foreign objects, it has been proposed to provide a lid that covers the top surface of the hot water supply pipe, and to attach and remove the lid from the hot water supply pipe depending on the timing of casting. This work is very dangerous if done manually because it is done in a narrow space close to the high-temperature molten metal. For this reason, the work is often automated, for example, by using a product transport robot used in the product removal process or a separate transport robot. Note that the process of attaching and removing the lid from the top surface of the hot water supply pipe is required in addition to the casting process, unnecessarily lengthening the casting cycle.

[0005] Therefore, as shown in Patent Documents 1 and 2, by providing an automatic opening and closing device between the hot water pipe and the sprue of the mold cavity, which opens and closes the top of the hot water pipe and removes impurities from the molten metal inside the hot water pipe, it is possible to reduce casting defects caused by foreign matter contamination and shorten the casting molding cycle. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] JP 2010-167430 A [Patent Document 2] JP 2008-213034 A Summary of the Invention [Problem to be solved by the invention]

[0007] The automatic opening and closing device of the means shown in Patent Document 1 and Patent Document 2 includes a closing section, a by-product capture gap section, and an opening section. After closing the casting mold, the automatic opening and closing device is positioned in the by-product capture gap section, and the molten metal in the hot water supply pipe is filled into the by-product capture gap section. This allows the molten metal with a lot of impurities on the upper surface of the hot water supply pipe to be removed. Next, the automatic opening and closing device is slid to the opening position to forcibly cut the molten metal, and only clean molten metal from which impurities have been removed can be filled into the mold cavity. Furthermore, after filling the mold cavity with molten metal, the automatic opening and closing device is slid to the closing section position to seal the mold cavity, and then the molten metal in the mold cavity is pressurized by a pressurizing mechanism or the like incorporated in the casting mold and cooled and solidified.

[0008] Here, the automatic opening and closing device has a gap necessary for sliding. Therefore, if the automatic opening and closing device is slid while the molten metal with low melt viscosity is pressed against it, there is a high possibility that the molten metal will enter this gap and leak out, and it becomes difficult to maintain stable casting quality due to a decrease or fluctuation in the amount of molten metal to be filled. In addition, it is possible that the molten metal inserted into the gap will solidify and the automatic opening and closing device will not move. Furthermore, it is possible that the molten metal solidified material inserted and solidified will fall off and mix with the molten metal, causing casting defects such as foreign matter contamination. In addition, the pressure force from the pressurizing mechanism is also strongly applied to the automatic opening and closing device, so there is a concern that it may deform or break down. If it were to withstand the pressure force, the automatic opening and closing device would be enlarged, leading to the coarsening of the entire casting device. Although the supply of inert gas to the holding furnace is shown, there is no supply of inert gas to the hot water supply pipe, and the generation of oxides in the molten metal has not been prevented.

[0009] The present invention has been made in consideration of the above problems, and relates to a casting device that aims to shorten the casting molding cycle and stably produce high-quality castings by providing a gate opening and closing plate that can completely prevent foreign matter from entering the molten metal pipe and the leakage of molten metal. [Means for solving the problem]

[0010] The casting apparatus of the present invention comprises a casting mold for forming a mold cavity, a holding furnace for holding molten metal, a hot water supply pipe connecting the holding furnace to the mold cavity, and a casting apparatus for filling the molten metal into the mold cavity via the hot water supply pipe, wherein a gate opening and closing plate for opening and closing the gate is provided at the connection between the gate of the mold cavity and the hot water supply pipe, and the gate opening and closing plate is provided with a pouring spout that connects the gate and the hot water supply pipe when the gate is in an open position, and a groove-shaped annular recessed groove surrounding the pouring spout.

[0011] In the casting apparatus according to the present invention, the annular groove may be arranged in a plurality of rows.

[0012] In the casting apparatus according to the present invention, a cleaning space for cleaning the annular groove may be provided, and when the gate opening / closing plate is in a closed position, the annular groove may be accommodated in the cleaning space.

[0013] In the casting apparatus according to the present invention, an inert gas supply hole for supplying an inert gas into the molten metal pipe may be provided, and when the sprue opening and closing plate is in the closed position, the inert gas supply hole may be connected to the molten metal pipe.

[0014] In the casting apparatus of the present invention, the inert gas may be nitrogen gas separated from air. Effect of the Invention

[0015] According to the present invention, it is possible to provide a casting device that can completely prevent the intrusion of foreign matter into the molten metal supply pipe and the leakage of molten metal, improves casting defects caused by the intrusion of foreign matter, molten metal oxides, etc., improves variations in casting quality caused by molten metal leakage, and shortens the casting molding cycle. [Brief description of the drawings]

[0016] [Figure 1] 1 is a conceptual diagram of a casting device according to the present invention. [Diagram 2] FIG. 4 is a detailed view of a gate opening / closing plate according to the present invention. [Diagram 3]FIG. 4 is an enlarged view of the annular groove of the gate opening / closing plate according to the present invention. [Figure 4] 1 is a diagram showing an example of a molding process using a casting apparatus according to the present invention. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0017] Preferred embodiments for carrying out the present invention will be described below with reference to the drawings. Note that the following embodiments do not limit the inventions according to the claims. Furthermore, not all of the combinations of features described in the embodiments are necessarily essential to the means of solving the problems of the inventions according to the claims. Furthermore, in the present embodiments, the scales and dimensions of each component may be exaggerated, and some components may be omitted.

[0018] [Casting equipment] First, the casting apparatus according to the present embodiment will be described with reference to FIG. 1 includes a molten metal storage unit 10, a casting mold 20, a molten metal supply pipe 30, and a gate opening / closing plate 40. Molten metal 14 in the molten metal storage unit 10 is injected into a mold cavity 26 of the casting mold 20 via the molten metal supply pipe 30 to form a casting. In FIG. 1, the molten metal storage section 10 and the casting mold 20 are arranged vertically in a straight line, but they may be arranged at an angle between the horizontal and vertical directions, or in a two-dimensional arrangement combining an inclined direction and a vertical direction.

[0019] The molten metal storage section 10 includes a pressurization adjustment chamber 12, a holding furnace 13, and a pressurization control device 15. The holding furnace 13 heats and holds the molten metal 14 at a predetermined temperature inside, and is stored in the pressurization adjustment chamber 12. The pressurization control device 15 is used to introduce pressurized gas into the pressurization adjustment chamber 12, and the air pressure in the pressurization adjustment chamber 12 increases, thereby pushing down the molten metal 14 in the holding furnace 13, and the molten metal 14 rises in the molten metal supply pipe 30, and the molten metal 14 is filled in the mold cavity 26. The pressurization control device 15 is also used to exhaust the pressurized gas in the pressurization adjustment chamber 12 and reduce the air pressure in the pressurization adjustment chamber 12, thereby allowing the molten metal 14 in the molten metal supply pipe 30 to be pulled down. In this way, the pressurization control device 15 is used to control the increase and decrease in air pressure in the pressurization adjustment chamber 12 by introducing and exhausting the pressurized gas, thereby allowing the molten metal 14 to be freely controlled in the molten metal supply pipe 30, and allowing the molten metal 14 to be filled in the mold cavity 26. In particular, since the pressure state in the pressure adjustment chamber 12 by the introduction of the pressurized gas directly relates to the filling state of the molten metal 14 in the mold cavity 26, it is desirable to precisely control the pressure state in multiple stages according to the type of molten metal 14 and the shape of the mold cavity 26. Although compressed air may be used as the pressurized gas, it is preferable to use an inert gas such as nitrogen or argon in order to prevent oxidation of the molten metal 14.

[0020] Although the molten metal storage section 10 in Fig. 1 includes only the holding furnace 13, a melting furnace (not shown) for producing the molten metal 14 by melting an aluminum alloy or the like may be provided separately. In this case, it is preferable to connect the melting furnace and the holding furnace 13, and continuously supply the molten metal 14 from the melting furnace to the holding furnace 13, thereby maintaining the height of the surface of the molten metal 14 in the holding furnace 13 constant. In addition, although the molten metal 14 in the molten metal supply pipe 30 is controlled by introducing and discharging pressurized gas into the pressure adjustment chamber 12, for example, a plunger that can move back and forth within the molten metal supply pipe 30 may be provided, and the molten metal 14 in the molten metal supply pipe 30 may be controlled by the direction and distance of the plunger.

[0021] The casting mold 20 comprises a fixed mold 24 attached to a fixed platen 22 and a movable mold 25 attached to a movable platen 23, and the movable platen 23 and the movable mold 25 are opened and closed in the vertical direction by a mold clamping device (not shown). A mold cavity 26 is formed by clamping the fixed mold 24 and the movable mold 25. The mold cavity 26 is provided with a sprue 27 for filling the molten metal 14, and the sprue 27 is connected to a molten metal supply pipe 30.

[0022] The lower surface of the molten metal supply pipe 30 is immersed in the molten metal 14 in the holding furnace 13, and the upper surface thereof penetrates the fixed platen 22 and is connected to the gate 27 of the fixed mold 24. The molten metal supply pipe 30 has a hollow shape, and as the molten metal 14 flows inside the molten metal supply pipe 30, the molten metal 14 in the holding furnace 13 is filled into the mold cavity 26 via the molten metal supply pipe 30 and the gate 27. In FIG. 1, the molten metal supply pipe 30 has a straight shape connecting the molten metal 14 in the holding furnace 13 and the gate 27, but it may have a bent or curved shape such as an L-shape or a U-shape.

[0023] [Gate opening and closing plate] Next, the gate opening and closing plate according to this embodiment will be described with reference to Figs. First, as shown in FIG. 1, the gate opening / closing plate 40 is provided between the gate 27 and the hot water supply pipe 30, and the gate 27 and the hot water supply pipe 30 are opened and closed by the gate opening / closing plate drive device 42 according to the casting process. The opening and closing positions of the gate opening / closing plate 40 are defined as an open position OP where the gate 27 and the hot water supply pipe 30 are open, and a closed position CL where the gate 27 and the hot water supply pipe 30 are closed. In FIG. 1, the gate 27 is provided in the fixed mold 24, so the gate opening / closing plate 40 is also stored in the fixed mold 24. However, this is not limited to this, and for example, an auxiliary structure for storing the gate opening / closing plate 40 may be provided between the fixed platen 22 and the fixed mold 24. Furthermore, the gate opening / closing plate 40 may be provided on an inclined surface close to the gate 27 side as long as it is provided between the gate 27 and the hot water supply pipe 30. Conversely, it may be provided on an inclined surface close to the hot water supply pipe 30 side. For example, when the pressure holding process is performed using a pressure mechanism or the like incorporated in the casting mold 20 described later, since the gate 27 is also closed simultaneously by the pressure mechanism or the like, it is preferable to provide the gate opening / closing plate 40 on the molten metal pipe 30 side so as not to interfere.

[0024] The gate opening and closing plate 40 will be described in detail with reference to Fig. 2. Fig. 2(a) is a plan view of the gate opening and closing plate 40 (viewed from A in Fig. 1), and Fig. 2(b) is a BB cross-sectional view of the gate opening and closing plate 40. When the gate opening / closing plate 40 is in the open position OP, the pouring gate 47 penetrating the gate in the cross-sectional direction connects the gate 27 and the molten metal supply pipe 30, enabling the molten metal 14 to be filled into the mold cavity 26. When the gate opening / closing plate 40 is in the closed position CL, the top side of the molten metal supply pipe 30 is closed, and the gate 27 and the molten metal supply pipe 30 are cut off.

[0025] Here, in order for the gate opening / closing plate 40 to open and close between the open position OP and the closed position CL, it is necessary to provide an appropriate gap between the gate opening / closing plate 40 and the fixed mold 24 that houses the gate opening / closing plate 40. The molten metal 14, which has a low melt viscosity, easily leaks out from this gap. Therefore, one annular groove (48a, 48c) is provided on each of the upper and lower surfaces of the gate opening / closing plate 40 so as to surround the pouring gate 47. The molten metal 14 leaking out from the gap can be reliably captured as molten metal scum by the annular grooves (48a, 48c), and the leakage of the molten metal 14 can be stopped. In addition, it is possible to prevent the leaked molten metal scum from entering the molten metal supply pipe 30, and thus it is possible to prevent casting defects caused by the inclusion of foreign matter.

[0026] Further, as shown in FIG. 2, another annular groove (48b, 48d) is added outside the annular groove (48a, 48c) to arrange the annular grooves in multiple rows. The multiple rows of annular grooves further enhance the effect of capturing the leaked molten metal 14. For example, even if the inner annular groove (48a, 48c) is filled with the leaked molten metal 14, the overflowing molten metal 14 can be captured by the outer annular groove (48b, 48d). For this reason, it is preferable to provide multiple rows of annular grooves within the range of the size of the gate opening / closing plate 40. The interval between the multiple rows and the depth and width of the annular groove are appropriately designed based on the size of the gate opening / closing plate 40 and the capturing efficiency of the molten metal 14.

[0027] In addition, the arrangement of multiple rows of these annular grooves can also be expected to enhance the sealing performance and suppress the leakage of the molten metal 14. The sealing effect will be described with reference to FIG. 3. FIG. 3 is an enlarged cross-sectional view of a part of the annular groove. The symbols (A1, B1) in the figure represent the volume of the gap between the fixed die 24 and the gate opening / closing plate 40, and the symbols (A2, B2) represent the volume of the annular grooves (48a, 48b). The respective volume ratios are A1 < A2 and B1 < B2. Also, the symbols (P0 to P4) represent the pressure of the molten metal 14 at each part. Assume that the molten metal 14 leaks from the pouring gate 47 into the gap A1 and then from the gap A1 into the annular groove 48a. At this time, the pressure of the molten metal 14 is P0 = P1 > P2. This is the result of the pressure relaxation effect caused by the sudden expansion of the volume (from A1 to A2) (this effect is called the labyrinth effect). As a result, the pressure of the molten metal 14 that has leaked into the annular groove 48a is low and does not have the pressure necessary to leak out already, so the leakage of the molten metal 14 can be stopped.

[0028] Arranging the annular grooves in multiple rows aims to further enhance the labyrinth effect. For example, if the pressure of the molten metal 14 that has leaked into the annular groove 48a does not drop completely, it is conceivable that the molten metal 14 leaks out from the gap B1 to the outside. In this case, the pressure of the molten metal 14 is P2 = P3 > P4, and in the outer annular groove 48b, a further pressure drop can be obtained to reliably stop the leakage. As a result, the amount of molten metal filled into the mold cavity 26 becomes stable, and casting defects caused by fluctuations in the molten metal can be avoided. In addition, the mixing of solidified matter of the leaked molten metal can be reliably prevented, and high-quality castings without foreign matter defects and the like can be stably obtained. Also, regarding the number of rows, intervals, sizes, etc. of the annular grooves, it is preferable to be appropriately designed from both aspects of the capturing effect of the leaked molten metal 14 and the suppression of the leakage of the molten metal 14 using the labyrinth effect.

[0029] Also, the gate plate 40 may be provided with a temperature control mechanism for heating and cooling, and a means for either heating or cooling the entire gate plate 40 or locally the pouring gate 47 and the annular groove may be provided. In this case, the gate plate 40 expands or contracts according to the linear expansion coefficient by heating or cooling, and the gap between the fixed mold 23 and the gate plate 40 can be adjusted. As a result, the amount of molten metal 14 leaking from the gate plate 40 can be reduced, and the effect of reliably avoiding a problem in which the gate plate 40 cannot be opened or closed due to leakage of molten metal can be obtained.

[0030] 2, the gate opening / closing plate 40 is provided with an inert gas supply hole 49. When the gate opening / closing plate 40 is in the closed position CL, an outlet 49a of the inert gas supply hole 49 is located directly above the hot water supply pipe 30 (broken line in FIG. 2(a)). An inlet 49b of the inert gas supply hole 49 is connected to an inert gas supply device (not shown), and while the gate opening / closing plate 40 is in the closed position CL, an inert gas such as nitrogen is supplied into the hot water supply pipe 30 to prevent oxidation of the molten metal 14 in the hot water supply pipe 30. This reliably prevents foreign matter defects caused by entrapment of oxides of the molten metal, etc.

[0031] In addition, when nitrogen gas is selected, for example, nitrogen gas separated by a separator that separates nitrogen gas from air can be used. In this case, there is no need for storage equipment such as nitrogen cylinders, and high-concentration nitrogen gas can be obtained by simply connecting factory air to the separator, which contributes greatly to cost reduction. As the separator, commercially available ones such as separation membrane type and PSA (Pressure Swing Adsorption) type can be used. Furthermore, by sending the nitrogen gas separated by the separator to the pressurization control device 15, it is also possible to use it as the pressurized gas in the pressurization adjustment chamber 12.

[0032] [Casting] Next, casting using the casting apparatus according to this embodiment will be described with reference to FIGS. First, the casting mold 20 is clamped by a mold clamping device (not shown) to form the mold cavity 26. After that, the gate opening and closing plate 40 is opened by the gate opening and closing drive device 42 and fixed in the open position OP, and the gate 27, pouring gate 47, and molten metal supply pipe 30 are brought into communication with each other (the state shown in FIG. 1). Here, the gate plate 40 is fixed in the open position OP after the mold cavity 26 is formed by clamping the casting mold 20, but the gate plate 40 may be opened at the same time as the mold is clamped, or the gate plate 40 may be fixed in the open position OP first and then the mold cavity 26 may be formed by clamping. An appropriate selection should be made in consideration of the balance with the casting molding cycle, including a transfer process for transferring the cast product to a post-process such as casting deburring. At this point, the molten metal 14 has not yet reached the gate plate 40, so the molten metal 14 will not leak out from the gap between the gate plate 40 and the fixed mold 24.

[0033] Next, using the pressurized gas control device 15, a pressurizable gas such as nitrogen gas is introduced into the pressurized adjustment chamber 12, and the air pressure in the pressurized adjustment chamber is controlled to raise the molten metal 14 in the molten metal supply pipe 30 and fill the molten metal 14 into the mold cavity 26 through the pouring port 47 and the pouring port 27. Here, since disturbance in the flow of the molten metal 14 during the filling process can cause casting defects such as voids due to entrapment of air, etc., it is desirable to precisely control the filling speed of the molten metal 14 in multiple stages according to the shape of the mold cavity 26. For example, when the pressure of the pressurized gas changes by 1 KPa, the surface of the molten metal 14 in the molten metal supply pipe 30 changes from a density of 2500 kg / m 3 If so, the change will be about 25 mm, and this is utilized to adjust the filling speed of the molten metal 14 by adjusting the pressure of the pressurized gas. The pressure range of the pressurized gas is about 0 to 200 KPa, preferably about 10 to 80 KPa. A casting device with a filling speed of about 10 kPa at maximum is preferable. As shown in FIG. 1, the pressurization adjustment chamber 12 may be pre-pressurized by the pressurized gas control device 15, and the molten metal 14 in the molten metal supply pipe 30 may be raised in advance to the vicinity of the gate opening and closing plate 40, with the aim of shortening the cycle of casting.

[0034] When the filling process of the molten metal 14 into the mold cavity 26 is completed, the process proceeds to a pressure holding process in which a pressure holding is applied to the molten metal 14 to compensate for solidification shrinkage caused by cooling of the molten metal 14. For example, the pressure of the pressurized gas is set to a high pressure within the range of 0 to 200 KPa, and the pressure holding is applied to the molten metal 14 in the mold cavity 26 from the hot water supply pipe 30. Alternatively, the pressure holding is directly applied to the molten metal 14 in the mold cavity 26 using a pressurizing mechanism (not shown) or the like incorporated in the casting mold 20. If necessary, both the pressurized gas and the pressurizing mechanism may be used. In the pressure holding process using the pressurized gas, the pressure holding is relatively low, so the amount of leakage of the molten metal 14 from the gate opening and closing plate 40 is small. In the pressure holding process using the pressurizing mechanism, the pressure can be made higher than in the case of the pressurized gas, and the amount of leakage of the molten metal 14 from the gate opening and closing plate 40 is large. Therefore, when using a pressurizing mechanism, the amount of molten metal 14 leaking from the gate opening / closing plate 40 during the pressure holding step can be reduced by, for example, using a pressure pin or the like that pressurizes the molten metal 14 in the mold cavity 26 while closing the gate 27. This is also expected to have the effect of preventing damage to the gate opening / closing plate 40.

[0035] After the pressure-holding step, the pressurized gas is exhausted using the pressurized gas control device 15 to lower the air pressure in the pressure adjustment chamber 12, and the level of the molten metal 14 in the molten metal supply pipe 30 is lowered, and the process proceeds to a preparation step for the casting molding of the next shot. In the case of the pressure-holding step using the pressurizing mechanism of the casting mold 20, after the gate 27 is closed by the pressure pin or the like, the step of lowering the air pressure in the pressure adjustment chamber 12 to lower the level of the molten metal 14 in the molten metal supply pipe 30 and the step of applying the holding pressure by the pressure pin or the like may be performed simultaneously. In addition, a separate pipeline or the like capable of supplying an inert gas or the like may be provided at a position close to the molten metal supply pipe 30 on the lower side of the gate opening / closing plate 40, and the inert gas or the like may be supplied from an inert gas supply device (not shown) through the pipeline into the molten metal supply pipe 30 to lower the level of the molten metal 14 in the molten metal supply pipe 30. In this case, it is preferable to perform the step of lowering the air pressure in the pressure adjustment chamber 12 at the same time.

[0036] Here, the amount of leakage of molten metal 14 from the gate opening / closing plate 40 can be significantly reduced from the start of filling the mold cavity 26 with the molten metal 14 to the descent of the molten metal 14 in the feed pipe 30 after the gate 27 is closed, but it will not be completely reduced to zero as long as there is a gap. The annular groove provided to surround the pouring gate 47 is effective in reducing to zero casting defects caused by the leakage of molten metal 14. The molten metal 14 leaking from the gap is captured by the annular grooves (48a, 48c), and the labyrinth effect reduces the leakage of molten metal 14. This reduces the amount of casting defects caused by the leakage of molten metal 14.

[0037] Outside the annular grooves (48a, 48c), multiple rows of outer annular grooves (48b, 48d) are arranged to further enhance the labyrinth effect. This ensures that the leakage of the molten metal 14 is stopped, and that casting defects caused by the leakage of the molten metal are prevented. If there is room in the size of the gate opening and closing plate 40, it is preferable to add further annular grooves.

[0038] Furthermore, the leaked molten metal 14 is reliably captured within the annular groove. Even when the gate opening / closing plate 40 is opened and closed in accordance with the casting cycle, the solidified molten metal (molten metal scum) of the leaked molten metal 14 remains within the annular groove and does not scatter outside. This reliably prevents casting defects caused by molten metal scum mixing with the molten metal 14 in the molten metal supply pipe 30. It also prevents interruptions to casting due to breakdowns in the casting device, such as molten metal scum clogging gaps and impairing the opening and closing operation of the gate opening / closing plate 40, and maintains high productivity. These improvements are further enhanced by arranging the annular grooves in multiple rows, ensuring a stable supply of high-quality castings.

[0039] After the pressure-holding process of the molten metal 14 in the mold cavity 26 is completed, the casting mold 20 is opened by a mold clamping device (not shown), and the casting M is removed from the mold cavity 26 by a removal device (not shown). The casting M is then transferred by a transfer robot (not shown) to a post-process for removing burrs, etc. At the same time, a mold release agent is applied to the mold cavity 26 and the gate 27 by a mold release agent application device (not shown), and the process proceeds to the next shot casting molding. During the period from the opening of the casting mold 20 to the process of applying the mold release agent, foreign matter such as casting burrs and mold release agent may enter the molten metal pipe 30 through the gate 27 and mix with the molten metal 14, causing serious casting defects due to foreign matter defects. Therefore, simultaneously with or before the opening of the casting mold 20, the gate opening and closing plate 40 is closed by the gate opening and closing drive device 42 and fixed in the closed position CL, and the top surface of the molten metal pipe 30 is closed (the state shown in FIG. 2). This reliably prevents foreign matter from entering the molten metal pipe 30, and reliably avoids casting defects caused by foreign matter.

[0040] When the gate plate 40 is in the closed position CL, the pouring gate 47 and the multiple annular grooves (48a, 48b, 48c, 48d) of the gate plate 40 are located in a cleaning space 44 provided in a fixed mold or a simple structure that houses the gate plate 40, and the molten metal residue trapped in the annular groove is removed by spraying air or the like from the cleaning nozzle 43. This makes it even more certain to prevent foreign matter from entering the mold. By using a mechanical cleaning tool such as a rotating brush in combination with the spraying of air or the like, the removal efficiency of the molten metal residue can be increased. The removed molten metal residue is captured by a suction device or the like (not shown) to thoroughly prevent it from scattering. This cleaning process does not affect the casting cycle, as it is performed within the preparation process for the next shot.

[0041] Furthermore, when the gate opening / closing plate 40 is in the closed position CL, an inert gas such as nitrogen gas is supplied from an inert gas supply device (not shown) through an inert gas supply hole 49 into the molten metal pipe 30, sealing the inside of the molten metal pipe 30 with the inert gas. This prevents the molten metal 14 in the molten metal pipe 30 from deteriorating due to oxidation, and avoids the inclusion of foreign matter such as oxides. At the same time, the level of the molten metal 14 in the molten metal pipe 30 is forcibly lowered to mix with the molten metal 14 in the holding furnace 13, stabilizing the temperature of the molten metal 14 in the next shot and stabilizing the casting quality. It should be noted that the supply of inert gas into the molten metal pipe 30 can be achieved, for example, by providing an inert gas supply line between the gate opening / closing plate 40 and the molten metal pipe 30 and supplying the inert gas into the molten metal pipe 30 through this line. However, since the line is located in a position where it comes into contact with the molten metal 14 during the casting operation, the possibility cannot be denied that the line will be blocked by the molten metal 14. Even if the line is blocked, the supply of inert gas into the molten metal pipe 30 is not prevented, since the inert gas supply hole 49 is not located in a position where it comes into contact with the molten metal 14.

[0042] In supplying the inert gas to the hot water supply pipe 30, for example, nitrogen gas separated by a separator that separates nitrogen gas from air can be used. In this case, no storage equipment such as nitrogen cylinders is required, and high-concentration nitrogen gas can be obtained by simply connecting factory air to the separator, which contributes greatly to cost reduction. Furthermore, by sending the nitrogen gas separated by the separator to the pressurization control device 15, it can also be used as the pressurized gas in the pressurization adjustment chamber 12.

[0043] [Variations] Although the preferred embodiments of the present invention have been described above, the technical scope of the present invention is not limited to the scope described in the above-mentioned embodiments. Various modifications and improvements can be made to the above-mentioned embodiments.

[0044] In the above-described embodiment, the present invention is described as being applied to a casting apparatus based on a vertical low-pressure casting machine that fills a mold cavity with molten metal such as an aluminum alloy. However, the present invention is not limited to this, and may be applied to, for example, a casting apparatus based on a horizontal die-casting machine, or a casting apparatus based on a semi-solidified casting apparatus that pressurizes and injects a metal alloy in a semi-solidified state to fill the mold cavity.

[0045] In the above embodiment, the present invention is described as being applied to a casting apparatus based on a low-pressure casting method in which molten metal is filled into a mold cavity at low pressure, but the present invention is not limited to this, and may be applied to a casting apparatus based on a vacuum casting method in which molten metal is filled by vacuum suctioning the mold cavity. In this case, the inside of the mold cavity can be suctioned to a high vacuum, and furthermore, inadvertent suction of molten metal into the mold cavity (a casting defect called "first-flow") can be prevented. [Explanation of symbols]

[0046] 100 Casting Equipment 10 Molten metal storage section 12 Pressure adjustment chamber 13 Holding furnace 14 Molten metal 15 Pressure control device 20 Casting mold 24 Fixed mold 25 Movable mold 26 Mold Cavity 27 Spout 30 Hot water pipe 40 Gate opening and closing plate 42 Gate opening and closing plate drive device 43 Cleaning nozzle 44 Cleaning space 47 Pouring spout 48a~48d Circular groove 49 Inert gas supply hole

Claims

1. A casting apparatus including a casting mold for forming a mold cavity, a holding furnace for holding molten metal, a molten metal supply pipe connecting the holding furnace and the mold cavity, and a casting apparatus for filling the molten metal into the mold cavity through the molten metal supply pipe, A sprue opening / closing plate for opening and closing the sprue is provided at a connection between the sprue of the mold cavity and the molten metal supply pipe, and the sprue opening / closing plate is provided with a pouring sprue that communicates the sprue with the molten metal supply pipe when the sprue is in an open position, and a groove-shaped annular recessed groove that surrounds the pouring sprue; a sliding surface between the annular groove of the gate opening / closing plate and the pouring gate and between the casting mold and the gate opening / closing plate; A casting apparatus comprising an air blowing means for blowing air into the annular groove.

2. 2. The casting apparatus of claim 1, wherein the molten metal is filled into the mold cavity by gas pressure.

3. 3. The casting apparatus according to claim 1, wherein the annular groove is formed on a surface of the gate plate facing the casting mold.

4. A cleaning space for cleaning the annular groove is provided, and when the gate opening / closing plate is in a closed position, 4. The casting apparatus according to claim 1, wherein the annular groove is accommodated in the cleaning space.

Citation Information

Patent Citations

  • JP1981012559U

  • printer

    JP1990024183A

  • Pressure casting equipment

    JP1994039258U

  • Pressurized casting apparatus

    JP1994114525A

  • Device for blowing inert gas

    JP1995051833A