Carbon fiber intermediate substrate treatment agent
A treatment agent with low molecular weight monool compounds enhances resin permeability and bonding in carbon fiber composites, addressing impregnation issues and improving composite strength.
Patent Information
- Application Number
- JP2020163648
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-10-10
- Filing Date
- 2020-09-29
- Publication Date
- 2024-11-27
- Estimated Expiration
- 2040-09-29
AI Technical Summary
The use of thermoplastic resins as matrix resins in carbon fiber composite materials results in poor impregnation, leading to voids and reduced strength due to insufficient permeability and bonding between carbon fibers and the resin.
A treatment agent for carbon fiber intermediate base materials containing a monool compound with a molecular weight of 2000 or less is applied to increase resin permeability and bonding, using compounds like aliphatic and aromatic monools and their alkylene oxide adducts, along with surfactants and polyester resins to enhance impregnation and strength.
The treatment agent significantly improves the permeability of thermoplastic resins into carbon fiber materials, resulting in high-strength composite materials with enhanced bonding and reduced voids.
Smart Images

Figure 0007590843000001
Abstract
Description
[Technical field]
[0001] The present invention relates to a treating agent for carbon fiber intermediate substrates. [Background technology]
[0002] Composite materials of various matrix resins and carbon fiber intermediate substrates are widely used in fields such as sports equipment, leisure goods, and aircraft. Thermosetting resins such as epoxy resins, vinyl ester resins, and unsaturated polyester resins have long been used as matrix resins, but in recent years, thermoplastic resins have also been used because of their heat resistance and the shortening of processing time. However, when a thermoplastic resin is used as a matrix resin, there are problems such as poor impregnation of the thermoplastic resin into the carbon fiber intermediate substrate and the occurrence of many voids in the composite material, which reduces the strength of the composite material. To address this issue, for example, when the carbon fiber intermediate substrate is a carbon fiber bundle, measures have been taken such as a method in which the carbon fiber bundle is first spread and then impregnated with a thermoplastic resin (e.g., Patent Document 1).
[0003] However, the impregnation of the highly viscous thermoplastic resin by simply going through the fiber-opening process as in Patent Document 1 is not sufficient, and the strength of the composite material is still low. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2005-29912 A Summary of the Invention [Problem to be solved by the invention]
[0005] An object of the present invention is to provide a treating agent for carbon fiber intermediate substrates that can produce high-strength carbon fiber composite materials. [Means for solving the problem]
[0006] The present inventors have conducted extensive research to solve the above problems, and have arrived at the present invention. That is, the present invention is a treatment agent for carbon fiber intermediate substrates, which contains a monol compound (A) having a chemical formula weight or number average molecular weight of 2000 or less. Effect of the Invention
[0007] The treating agent for carbon fiber intermediate substrates of the present invention has the effect of making it possible to produce carbon fiber composite materials with high strength. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] The treating agent for carbon fiber intermediate substrates of the present invention contains a monol compound (A) having a chemical formula weight or number average molecular weight of 2,000 or less.
[0009] The carbon fiber intermediate substrate treating agent of the present invention is a treating agent for enhancing the permeability of a matrix resin into a carbon fiber intermediate substrate, and is different from carbon fiber sizing agents (carbon fiber sizing agents) used to bundle carbon fibers and adjust the adhesion between the carbon fibers and the matrix resin in a composite material. In the present invention, the carbon fiber intermediate substrate means a substrate composed of a plurality of carbon fibers before impregnation with a matrix resin, and examples thereof include carbon fiber bundles {short fiber bundles (chopped yarns, etc.)}, carbon fiber fabrics (unidirectional carbon fiber fabrics, two-dimensional carbon fiber fabrics, three-dimensional carbon fiber fabrics, etc.), carbon fiber knitting, carbon fiber nonwoven fabrics (felt, mats, papers, etc.), and carbon fiber cloths. By treating with the carbon fiber intermediate substrate treating agent of the present invention, a film of the monol compound (A) is formed on the carbon fiber surface of the carbon fiber intermediate substrate composed of a plurality of carbon fibers, which enhances the lubrication between the carbon fibers of the matrix resin, and enhances the permeability of the matrix resin into the carbon fiber intermediate substrate (between the carbon fibers).
[0010] In the present invention, the monol compound (A) is a compound having a chemical formula weight or number average molecular weight of 2,000 or less. As the monol compound (A), a compound having one hydroxyl group other than a phenolic hydroxyl group (a hydroxyl group directly bonded to an aromatic ring) is preferred from the viewpoints of permeability into the matrix resin and strength of the composite material. Examples of the monol compound (A) include an aliphatic monol (A1), an alkylene oxide (hereinafter abbreviated as AO) adduct (A2) of the aliphatic monol (A1), and a monol compound having an aromatic ring (A3). The monol compound (A) may be used alone or in combination of two or more kinds.
[0011] Examples of the aliphatic monool (A1) include saturated linear aliphatic monoalcohols having 10 to 34 carbon atoms (hereinafter abbreviated as C) (n-decanol, lauryl alcohol, myristyl alcohol, cetyl alcohol, stearyl alcohol, behenyl alcohol, montanyl alcohol, etc.), unsaturated linear aliphatic monoalcohols having 10 to 34 carbon atoms (palmitoleyl alcohol, oleyl alcohol, elaidyl alcohol, linoleyl alcohol, linolenyl alcohol, etc.), saturated branched aliphatic monoalcohols having 10 to 34 carbon atoms (isostearyl alcohol, etc.), unsaturated branched aliphatic monoalcohols having 4 to 34 carbon atoms (methylvinylcarbinol, 3-methyl-6-hexen-2-ol, 4-propyl-8-octadecen-1-ol, etc.), and alicyclic monoalcohols having 5 to 34 carbon atoms (cyclopentanol, cyclohexanol, cyclooctadecanol, 2-methylcyclohexanol, etc.).
[0012] Examples of the AO adduct (A2) of an aliphatic monol include those obtained by adding AO to the above aliphatic monol (A1). AO includes those having C2 to C4, such as ethylene oxide (hereinafter abbreviated as EO), 1,2-propylene oxide (hereinafter abbreviated as PO), 1,3-propylene oxide, and 1,2-, 1,3-, or 1,4-butylene oxide (hereinafter abbreviated as BO), etc. Two or more of these AOs may be used in combination, and when two or more of them are used in combination, the bonding mode may be any of block addition, random addition, and combinations of these. Of these, EO is preferred from the viewpoints of the permeability of the matrix resin and the ease of handling of the carbon fiber intermediate substrate treating agent. The number of moles of AO added is preferably 2 to 40, and more preferably 2 to 20, from the viewpoints of the permeability of the matrix resin and the handleability of the treatment agent for carbon fiber intermediate substrates.
[0013] Examples of the monol compound (A3) having an aromatic ring include araliphatic monols (A31), AO adducts of araliphatic monols (A32), and AO adducts of aromatic monols (A33).
[0014] Examples of the aromatic aliphatic monool (A31) include C7 to C34 aromatic aliphatic monools (benzyl alcohol, diphenylmethanol, diphenylethanol, triphenylcarbinol, cinnamyl alcohol, etc.).
[0015] Examples of the AO adduct of the aromatic aliphatic monol (A32) include those obtained by adding AO to the above (A31). The AO includes those having C2 to C4, such as EO, PO, 1,3-propylene oxide, and BO. Two or more of these AO may be used in combination, and in the case of using two or more of them in combination, the bonding mode may be any of block addition, random addition, and a combination of these. Of these, EO is preferred from the viewpoints of the permeability of the matrix resin and the ease of handling of the carbon fiber intermediate substrate treating agent. The number of moles of AO added is preferably 2 to 43, and more preferably 2 to 20, from the viewpoints of the permeability of the matrix resin and the handleability of the treating agent for carbon fiber intermediate substrates.
[0016] In the AO adduct of aromatic monol (A33), examples of the aromatic monol include phenol, phenolic compounds having a carboxyl group (2-hydroxybenzoic acid, 4-hydroxybenzoic acid, 2,6-dicarboxyphenol, etc.), alkylphenols having an alkyl group of C1 to C20 (cresol, butylphenol, octylphenol, nonylphenol, etc.), arylphenols (phenylphenol, etc.), arylalkyl (C1 to C15) phenols (including those with C13 to C45, such as benzylphenol, phenylethylphenol, phenylpropylphenol, cumylphenol, etc.), alkyl (C1 to C20) arylphenols (C ... and the like. Examples of condensed polycyclic phenols include those with a carbon number of from 10 to 63, such as methylphenylphenol, ethylphenylphenol, propylphenylphenol, methylbenzylphenol, ethylbenzylphenol, and propylbenzylphenol, condensed polycyclic phenols (including those with a carbon number of from 10 to 20, such as naphthol and anthranol), condensed polycyclic phenolic compounds having a carboxyl group (6-hydroxy-2-naphthalenecarboxylic acid, etc.), and styrenated products thereof (including those with a carbon number of from 14 to 87, such as styrenated phenol, styrenated nonylphenol, styrenated phenylphenol, styrenated benzylphenol, and styrenated cumylphenol).
[0017] In the AO adduct of aromatic monol (A33), AO includes those having C2 to C4, such as EO, PO, 1,3-propylene oxide, and BO. Among these AO, EO is preferred from the viewpoints of permeability of the matrix resin and ease of handling of the carbon fiber intermediate substrate treatment agent. The number of moles of AO added is preferably 2 to 43, and more preferably 2 to 30, from the viewpoints of the permeability of the matrix resin and the handleability of the treating agent for carbon fiber intermediate substrates.
[0018] As the monol compound (A), from the viewpoint of the permeability of the matrix resin and the strength of the composite material, a monol compound (A3) having an aromatic ring is preferred, an AO adduct of an aromatic monol (A33) is more preferred, an AO adduct of at least one aromatic monol selected from the group consisting of cumylphenol, naphthol, anthrol, styrenated phenol, styrenated cresol, styrenated cumylphenol, and styrenated naphthol is next more preferred, and an EO adduct of at least one aromatic monol selected from the group consisting of cumylphenol, naphthol, anthrol, styrenated phenol, styrenated cresol, styrenated cumylphenol, and styrenated naphthol is particularly preferred.
[0019] The weight proportion of EO units in the monol compound (A) (number of EO units × 44 / chemical formula weight or number average molecular weight) is preferably 10 to 95% by weight, more preferably 20 to 80% by weight, from the viewpoints of the permeability of the matrix resin and the handleability of the treatment agent for carbon fiber intermediate substrates.
[0020] The HLB of the monol compound (A) is preferably 2 to 19, and more preferably 4 to 18, from the viewpoints of the permeability of the matrix resin and the handleability of the treating agent for carbon fiber intermediate substrates. The HLB value is an index showing the balance between hydrophilicity and lipophilicity, and can be calculated from the ratio of the molecular weight of a compound to the molecular weight of the hydrophilic group portion using the Griffin method described on page 142 of "Introduction to Surfactants" [published by Sanyo Chemical Industries, Ltd. in 2007, written by Takehiko Fujimoto], using the following formula: HLB = 20 x molecular weight of hydrophilic group part of compound / chemical formula weight or number average molecular weight of compound The HLB of the monol compound (A) can be increased, for example, by increasing the content of EO units in the molecule.
[0021] In the present invention, the weight loss rate of the monool compound (A) at 300°C is preferably 50% by weight or less, more preferably 40% by weight or less, and particularly preferably 30% by weight or less, from the viewpoints of the permeability of the matrix resin and the strength of the composite material. The weight loss rate at 300°C is measured using TG-DTA. Specifically, a "TG / DTA6200" (Seiko Instruments Inc.) is used to heat about 10 mg of a sample from 30°C to 500°C at 20°C / min, and the TG curve is analyzed to calculate the weight loss rate at 300°C based on the weight of the sample used in the measurement (measurement atmosphere: nitrogen at 200 ml / min, sample container: aluminum pan). The weight loss rate at 300° C. can be adjusted by the molecular weight and the aromatic ring content per molecular weight. The larger the molecular weight and the higher the aromatic ring content per molecular weight, the lower the weight loss rate at 300°C. The weight loss rate at 300°C is, for example, cumylphenol EO 6 mole adduct (10 wt%), cumylphenol EO 30 mole adduct (1 wt%), styrenated (2.75 moles) phenol EO 4 mole adduct (4 wt%), styrenated (2.75 moles) phenol EO 5 mole adduct (4 wt%), styrenated (2 moles) phenol EO 17 mole adduct (1.5 wt%), styrenated (1.1 moles) phenol EO 5 mole adduct (12 wt%), styrenated (2 moles) cresol EO 10 mole adduct (3 wt%), styrenated Styrenated (1 mol) cumylphenol EO 5 mol adduct (5 wt%), styrenated (1 mol) cumylphenol EO 10 mol adduct (3 wt%), styrenated (1 mol) cumylphenol EO 25 mol adduct (1 wt%), β-naphthol EO 7 mol adduct (10 wt%), β-naphthol EO 20 mol adduct (1 wt%), styrenated (1 mol) β-naphthol EO 10 mol adduct (10 wt%), anthrol EO 10 mol adduct (3 wt%) and 4-(2-hydroxyethoxy)benzoic acid DBU salt (33 wt%).
[0022] The monol compound (A) is a compound having a chemical formula weight or number average molecular weight of 2000 or less, and from the viewpoints of the permeability of the matrix resin and the strength of the composite material, it is preferably 1500 or less, more preferably 1000 or less. From the same viewpoint, the lower limit is preferably 100 or more, more preferably 200 or more. The number average molecular weight is measured by gel permeation chromatography (hereinafter, abbreviated as GPC). The GPC conditions used for measuring the number average molecular weight of the monol compound (A) are, for example, as follows. Model: HLC-8220GPC (Tosoh Corporation liquid chromatograph) Column: TSK gel Super H4000 +TSK gel Super H3000 +TSK gel Super H2000 (both manufactured by Tosoh Corporation) Column temperature: 40℃ Detector: RI (Refractive Index) Solvent: Tetrahydrofuran Flow rate: 0.6ml / min Sample concentration: 0.25% by weight Injection volume: 10μl Standard: Polystyrene (manufactured by Tosoh Corporation; TSK STANDARD POLYSTYRENE
[0023] The treating agent for a carbon fiber intermediate substrate preferably further contains a surfactant (B). The surfactant (B) may be a nonionic surfactant (B1) other than the monol compound (A), an anionic surfactant (B2), a cationic surfactant (B3), an amphoteric surfactant (B4), etc. The surfactant (B) may be used alone or in combination of two or more kinds. As the surfactant (B), from the viewpoint of strength when made into a composite material (molded article), the nonionic surfactant (B1), the anionic surfactant (B2), and a combination of these are preferred.
[0024] The nonionic surfactant (B1) other than the monol compound (A) can be used without any particular limitation, and examples thereof include those having an alkyl group of C7 to 24 (B11) and those having an aralkyl group of C7 to 24 (B12).
[0025] Examples of (B11) include AO adducts (number of moles added = 43 to 100) of C7-24 monoalcohols having a number average molecular weight exceeding 2000 {preferably the following saturated or unsaturated aliphatic alcohols as the monoalcohols, specifically an EO 60 mole adduct of dodecyl alcohol, etc.} and esters of diols {(poly)oxyalkylenes ((poly)oxyethylene, (poly)oxypropylene, (poly)oxybutylene, etc.) and fatty acids (C7-24) {preferably the following saturated or unsaturated fatty acids as the fatty acids, specifically polyethylene glycol monostearate, etc.}, fatty acid (C7-24) esters of polyhydric (trihydric to decahydric or higher) alcohols {fatty acids Examples of the fatty acid include the following saturated or unsaturated fatty acids, which are preferably glycerin monostearate and sorbitan monolaurate, etc.}, fatty acid (C7-24) esters of AO (alkylene group has 2-4 carbon atoms) adducts (number of moles added = 1-100) of polyhydric alcohols {the fatty acid includes the following saturated or unsaturated fatty acids, which are preferably sorbitan monolaurate (poly)oxyethylene (average number of moles added = 1-100), etc.}, and amidations of fatty acids (C7-24) and alkanolamines (C1-10) {coconut oil fatty acid monoethanolamide, 1:1 type coconut oil fatty acid diethanolamide, and 1:1 type lauric acid diethanolamide, etc.}.
[0026] In (B12), the aralkyl group includes an aralkyl group in which one hydrogen atom of a C1-18 alkyl group is substituted with an aryl group (including C6-18 aryl groups such as phenyl, benzyl, tolyl, and xyl), such as a benzyl group, a phenylethyl group, and a phenylpropyl group. Specific examples of (B12) include those having a chemical formula weight or number average molecular weight of more than 2000, such as AO adducts of styrenated products (C14-62) of phenols (phenol, cumylphenol, cresol, etc.) [AO adducts of styrenated phenol (C14-62), AO adducts of styrenated cumylphenol, and AO adducts of styrenated cresol (C15-61), etc.] and AO adducts of C7-32 alkylphenols.
[0027] Among the nonionic surfactants (B1) other than the monol compound (A), from the viewpoint of the strength of the composite material, AO adducts of C7-24 saturated or unsaturated aliphatic alcohols and those having a C7-24 aralkyl group (B12) are preferred, and more preferred are AO adducts of C7-12 saturated or unsaturated aliphatic alcohols and AO adducts of styrenated phenols.
[0028] The anionic surfactant (B2) includes those having at least one selected from the group consisting of a carboxyl group, a sulfate ester group, a sulfonic acid group, and a phosphate ester group as an anionic group, and specifically includes those having a carboxyl group as an anionic group {carboxylate (B21) having a C7-24 saturated or unsaturated aliphatic group}, those having a sulfate ester group as an anionic group {sulfate (B22) having a C7-24 saturated or unsaturated aliphatic group or a C7-62 aralkyl group}, and sulfuric acid surfactants other than (B22). neutral salts of oxidized oils (B23); neutral salts of sulfates of unsaturated fatty acid alkyl (C1-22) esters other than (B22) (B24); neutral salts of sulfates of C12-18 olefins (B25)}, those having a sulfonic acid group as the anionic group {sulfonate salts having a C12-18 saturated or unsaturated aliphatic group or a C7-62 aralkyl group (B26)}, and those having a phosphate ester group as the anionic group {phosphate ester salts having a C7-60 alkyl group or a C14-66 aralkyl group (B27)}.
[0029] (B21) includes C7-24 saturated fatty acids (caprylic acid, pelargonic acid, capric acid, lauric acid, myristic acid, pentadecylic acid, palmitic acid, margaric acid, stearic acid, arachidic acid, henicosylic acid, behenic acid, lignoceric acid, cerotic acid, montanic acid, etc.), C7-24 unsaturated fatty acids (myristoleic acid, palmitoleic acid, sapienic acid, oleic acid, vaccenic acid, gadoleic acid, eicosenoic acid, erucic acid, etc.), , nervonic acid, linoleic acid, eicosadienoic acid, docosadienoic acid, linolenic acid, pinolenic acid, eleostearic acid, mead acid, eicosatrienoic acid, stearidonic acid, arachidonic acid, and eicosatetraenoic acid, etc.), C7-24 saturated or unsaturated aliphatic alcohols (octanol, nonanol, decanol, undecyl alcohol, lauryl alcohol, tridecyl alcohol, myristyl alcohol, pentadecyl alcohol, cetearyl alcohol, glyceryl alcohol, glyceryl stearate ... Examples of the ammonium salt or amine salt of a compound having a carboxyl group include carboxymethylated products of alkoxylated alcohols such as alkoxylated alcohols (e.g., ethyl ether, palmitoleyl alcohol, heptadecanol, stearyl alcohol, isostearyl alcohol, elaidyl alcohol, oleyl alcohol, linoleyl alcohol, elaidolinoleyl alcohol, linolenyl alcohol, elaidolinolenyl alcohol, ricinoleyl alcohol, nonadecyl alcohol, arachidyl alcohol, heneicosanol, behenyl alcohol, erucyl alcohol, lignoceryl alcohol, ceryl alcohol, heptacosanol, and montanyl alcohol), and carboxymethylated products of AO (including C2-4, ethylene oxide, propylene oxide, and butylene oxide, the same applies below) adducts (number of moles added = 1-20) of the above-mentioned C7-24 saturated or unsaturated aliphatic alcohols.
[0030] Examples of (B22) include ammonium salts or amine salts of compounds having a sulfate group, such as sulfate esters of the above-mentioned C7-24 saturated or unsaturated aliphatic alcohols, sulfate esters of AO adducts (number of moles added=1 to 10) of the above-mentioned C7-24 saturated or unsaturated aliphatic alcohols, sulfate esters of alkylphenols having a C3-13 alkyl group (n-propylphenol, i-propylphenol, n-butylphenol, sec-butylphenol, t-butylphenol, n-hexylphenol, 2-ethylhexylphenol, n-octylphenol, n-nonylphenol, etc.), sulfate esters of AO adducts (number of moles added=1 to 20) of the above-mentioned alkylphenols, and sulfate esters of AO adducts (number of moles added=1 to 20) of arylalkylphenols {styrenated phenols (C14-62), styrenated cumylphenol, styrenated cresol (C15-61), etc.}.
[0031] (B23) may be exemplified by sulfides of natural unsaturated fats and oils (castor oil, olive oil, soybean oil, herring oil, etc.) or unsaturated waxes (sperm whale oil, etc.) neutralized with ammonia or amines.
[0032] Examples of (B24) include esters of the above unsaturated fatty acids with C1-4 alcohols (such as methanol and ethanol), which are sulfonated at their unsaturated bonds and neutralized with ammonia or an amine.
[0033] Examples of (B25) include C12-18 olefins (dodecene, tridecene, tetradecene, pentadecene, hexadecene, octadecene, and the like) in which unsaturated bonds are sulfated and neutralized with ammonia or an amine.
[0034] Examples of (B26) include ammonium salts or amine salts of compounds having a sulfonic acid group, such as alkylbenzenesulfonic acids having a C1 to 20 alkyl group (methylbenzenesulfonic acid, ethylbenzenesulfonic acid, propylbenzenesulfonic acid, butylbenzenesulfonic acid, pentylbenzenesulfonic acid, hexylbenzenesulfonic acid, dimethylbenzenesulfonic acid, dipropylbenzenesulfonic acid, etc.), alkylnaphthalenesulfonic acids having a C1 to 20 alkyl group, diesters of sulfosuccinic acid and C4 to 20 alcohols (dioctyl sulfosuccinic acid, etc.), α-olefinsulfonic acids having C12 to 18, and Igepone T-type sulfonic acid.
[0035] Examples of (B27) include ammonium salts or amine salts of compounds having a phosphate group, such as the phosphate esters of saturated or unsaturated aliphatic alcohols, the phosphate esters of AO adducts of saturated or unsaturated aliphatic alcohols (number of moles added = 1 to 20), the phosphate esters of alkylphenols having C3 to 13 alkyl groups, and the phosphate esters of AO adducts of alkylphenols having C3 to 13 alkyl groups (number of moles added = 1 to 20).
[0036] In (B2), from the viewpoint of the strength of the composite material (molded article), the salt is preferably a salt other than an alkali metal salt, more preferably an ammonium salt and / or an amine salt, and particularly preferably a tertiary monoamine. The amines include monoamines having a C1-20 alkyl group which may be partially substituted with a hydroxyl group, and C1-20 polyamines. Specific examples of amines include primary monoamines (methylamine, ethylamine, propylamine, butylamine, pentylamine, hexylamine, heptylamine, octylamine, nonylamine, decylamine, dodecylamine, tridecylamine, tetradecylamine, pentadecylamine, hexadecylamine, heptadecylamine, octadecylamine, nonadecylamine, icosylamine, monoethanolamine, monoethanolamine, and monopropanolamine), secondary monoamines (dimethylamine, diethylamine, dipropylamine, dibutylamine, dipentylamine, dihexylamine, diheptylamine, dioctylamine, dinonylamine, didecylamine, didodecylamine, ditridecylamine, ditetradecylamine, dipentadecylamine, dihexadecylamine, diheptadecylamine, dioctadecylamine, dinodecylamine, diicosylamine, amines, methylethylamine, dimethanolamine, diethanolamine, etc.), tertiary monoamines (trimethylamine, triethylamine, tripropylamine, tributylamine, tripentylamine, trihexylamine, triheptylamine, trioctylamine, trinonylamine, tridecylamine, tridodecylamine, tritridecylamine, tritetradecylamine, tripentadecylamine, trihexadecylamine, triheptadecylamine, trioctadecylamine, trinonadecylamine, triicosylamine, dimethylethylamine, methyldimethanolamine, methyldiethanolamine, ethyldiethanolamine, triethanolamine, etc.), polyamines {C2 to 20 acyclic polyamines (ethylenediamine, diethylenetriamine, etc.), C4 to 20 cyclic polyamines (diazabicycloundecene, diazabicyclononene, etc.), etc.}.
[0037] Of (B2), from the viewpoint of the strength of the composite material, sulfate ester salts (B22) having a C7-24 saturated or unsaturated aliphatic group or a C7-62 aralkyl group are preferred, and sulfate ester salts of AO adducts of C7-24 saturated or unsaturated aliphatic alcohols are more preferred.
[0038] From the viewpoint of the strength of the composite material, (B2) is preferably an ammonium salt or amine salt of a sulfate ester having a C7-24 saturated or unsaturated aliphatic group or a C7-62 aralkyl group, and more preferably an ammonium salt or amine salt of a sulfate ester of an AO adduct of a C7-24 saturated or unsaturated aliphatic alcohol.
[0039] The weight ratio ((A) / (B)) of the monol compound (A) to the surfactant (B) in the carbon fiber intermediate substrate treating agent of the present invention is preferably 80 / 20 to 99 / 1, more preferably 90 / 10 to 99 / 1, from the viewpoints of the permeability of the matrix resin and the strength of the composite material.
[0040] It is preferable that the treating agent for carbon fiber intermediate substrates further contains a polyester resin (C). The polyester resin (C) may be used alone or in combination of two or more kinds. The polyester resin (C) preferably has an HLB of 4-18, more preferably 5-17, from the viewpoints of the permeability of the matrix resin and the strength of the composite material.
[0041] The viscosity of the polyester resin (C) at 30° C. is preferably from 10 to 1,000,000 Pa·s, and more preferably from 20 to 500,000 Pa·s, from the viewpoints of the permeability of the matrix resin and the strength of the composite material.
[0042] In the present invention, the viscosity of the polyester resin (C) is a complex viscosity, which can be measured, for example, by a viscoelasticity measuring device (for example, ARES manufactured by Rheometric Scientific Co., Ltd.) The measurement conditions are shown below. <Measurement conditions for viscosity of polyester resin (C)> Sample fixture: 25mm diameter disk Gap distance: 0.25mm Distortion: 1% Frequency: 1Hz Temperature: 30℃
[0043] The polyester resin (C) is preferably a condensation polymer of a dicarboxylic acid (a1) and / or a dicarboxylic anhydride (a2) with a diol (b).
[0044] Examples of the dicarboxylic acid (a1) include acyclic saturated dicarboxylic acids, acyclic unsaturated dicarboxylic acids, alicyclic dicarboxylic acids, dimer acids, and aromatic dicarboxylic acids. Examples of the chain saturated dicarboxylic acid include C2 to C22 linear or branched chain saturated dicarboxylic acids (oxalic acid, malonic acid, succinic acid, glutaric acid, methylsuccinic acid, ethylsuccinic acid, dimethylmalonic acid, α-methylglutaric acid, β-methylglutaric acid, 2,4-diethylglutaric acid, isopropylmalonic acid, adipic acid, pimelic acid, suberic acid, azelaic acid, sebacic acid, decanedicarboxylic acid, undecanedicarboxylic acid, dodecanedicarboxylic acid, tridecanedicarboxylic acid, tetradecanedicarboxylic acid, hexadecanedicarboxylic acid, octadecanedicarboxylic acid, icosanedicarboxylic acid, decylsuccinic acid, dodecylsuccinic acid, and octadecylsuccinic acid, etc.). Examples of the chain unsaturated dicarboxylic acid include C4 to C22 linear or branched chain unsaturated dicarboxylic acids (maleic acid, fumaric acid, citraconic acid, mesaconic acid, dodecenylsuccinic acid, pentadecenylsuccinic acid, octadecenylsuccinic acid, etc.). Examples of the alicyclic dicarboxylic acid include C7 to C14 alicyclic dicarboxylic acids (1,3- or 1,2-cyclopentanedicarboxylic acid, 1,2-, 1,3- or 1,4-cyclohexanedicarboxylic acid, 1,2-, 1,3- or 1,4-cyclohexanediacetic acid, and dicyclohexyl-4,4'-dicarboxylic acid). Examples of dimer acids include dimers of C8 to C24 chain unsaturated carboxylic acids (oleic acid, linoleic acid, linolenic acid, etc.). Examples of aromatic dicarboxylic acids include C8 to C14 aromatic dicarboxylic acids (terephthalic acid, isophthalic acid, phthalic acid, phenylmalonic acid, phenylsuccinic acid, β-phenylglutaric acid, α-phenyladipic acid, β-phenyladipic acid, biphenyl-2,2'- and 4,4'-dicarboxylic acid, naphthalenedicarboxylic acid, sodium 5-sulfoisophthalate, and potassium 5-sulfoisophthalate).
[0045] The dicarboxylic anhydride (a2) is an anhydride of the above dicarboxylic acid (a1), and examples thereof include succinic anhydride, maleic anhydride, and phthalic anhydride.
[0046] The dicarboxylic acid (a1) and the dicarboxylic anhydride (a2) may be used alone or in combination of two or more. Among these, from the viewpoint of the strength of the composite material, chain saturated dicarboxylic acid and aromatic dicarboxylic acid are preferred, more preferred are oxalic acid, malonic acid, succinic acid, adipic acid, sebacic acid, terephthalic acid, isophthalic acid, phthalic acid and combination of two or more of these, and particularly preferred are adipic acid, terephthalic acid, isophthalic acid and combination of two or more of these.
[0047] Examples of the diol (b) include aliphatic alkanediols and AO adducts thereof, alicyclic diols and AO adducts thereof, AO adducts of primary amines, and AO adducts of aromatic ring-containing dihydric phenols.
[0048] Examples of the aliphatic alkanediol include those having 2 to 16 carbon atoms, such as ethylene glycol, 1,2-propylene glycol, 1,3-propylene glycol, 1,4-butanediol, 1,6-hexanediol, octanediol, decanediol, dodecanediol, hexadecanediol, neopentyl glycol, and 2,2-diethyl-1,3-propanediol. The AO adduct of the aliphatic alkanediol may be a compound in which a C2-4 AO is added to the above diol. Examples of the C2-4 AO include EO, PO, 1,3-propylene oxide, and BO. Two or more of these AOs may be used in combination, and when two or more of them are used in combination, the bonding mode may be any of block addition, random addition, and combinations of these. The number of moles of AO added per molecule of the aliphatic alkanediol is preferably 1 to 120 moles from the viewpoint of the strength of the composite material.
[0049] Examples of the alicyclic diol include those having C4 to C16, 1,4-cyclohexanediol, 1,4-cyclohexanedimethanol, and hydrogenated bisphenol A. Examples of the AO adducts of the alicyclic diol include compounds in which C2 to C4 AO are added to the above diols.
[0050] Examples of the primary amine in the AO adduct of a primary amine include C1 to C22 primary amines, methylamine, ethylamine, propylamine, butylamine, octylamine, decylamine, and dodecylamine. Examples of AO adducts of primary amines include compounds in which C2-4 AO is added to the above amines.
[0051] Examples of the aromatic ring-containing dihydric phenol in the AO adduct of the aromatic ring-containing dihydric phenol include bisphenol A, bisphenol S, cresol, and hydroquinone. Examples of AO adducts of aromatic ring-containing dihydric phenols include compounds in which C2-4 AO is added to the above phenols.
[0052] Of the diols (b), from the viewpoint of ease of handling of the treatment agent for carbon fiber intermediate substrates, preferred is at least one selected from the group consisting of aliphatic alkanediols, AO adducts of aliphatic alkanediols, AO adducts of alicyclic diols, AO adducts of primary amines, and AO adducts of aromatic ring-containing dihydric phenols, and more preferred is at least one selected from the group consisting of aliphatic alkanediols, AO adducts of aliphatic alkanediols, and AO adducts of aromatic ring-containing dihydric phenols.
[0053] The polyester resin (C) may be produced, for example, by adding a dicarboxylic acid (a1) and / or a dicarboxylic anhydride (a2) and a diol (b) in a predetermined molar ratio, and distilling off water under stirring at a reaction temperature of 100 to 250° C. and a pressure of −0.1 to 1.2 MPa. Diol (b) may be further added to the reaction mixture to cause the reaction.
[0054] When producing polyester resin (C), it is preferable to add a catalyst in an amount of 0.05 to 0.5% by weight based on the weight of polyester resin (C). Examples of the catalyst include paratoluenesulfonic acid, dibutyltin oxide, tetraisopropoxy titanate, and potassium oxalate titanate. From the viewpoints of reactivity and environmental impact, tetraisopropoxy titanate and potassium oxalate titanate are preferred, and potassium oxalate titanate is more preferred.
[0055] The weight ratio ((A) / (C)) of the monol compound (A) to the polyester resin (C) in the treatment agent for carbon fiber intermediate substrate of the present invention is preferably 60 / 40 to 99 / 1, more preferably 80 / 20 to 99 / 1, from the viewpoints of the permeability of the matrix resin and the strength of the composite material.
[0056] The weight ratio of the monool compound (A) in the evaporation residue (which also applies to the evaporation residues below) when the carbon fiber intermediate substrate treatment agent is heated at 105°C according to JIS K0067 (1992) is preferably 100% by weight from the viewpoint of the permeability of the matrix resin. When (B) and / or (C) are contained, from the viewpoint of the permeability of the matrix resin and the strength of the composite material, the upper limit of the weight ratio of the monool compound (A) in the evaporation residue of the treatment agent for carbon fiber intermediate substrates is preferably less than 100% by weight, more preferably 99.99% by weight or less, next more preferably 99.98% by weight or less, particularly preferably 99.95% by weight or less, and most preferably 99.9% by weight or less. The lower limit is preferably 60% by weight or more, more preferably 70% by weight or more, next more preferably 80% by weight or more, and particularly preferably 90% by weight or more.
[0057] The weight ratio of the surfactant (B) in the evaporation residue of the treating agent for carbon fiber intermediate substrate of the present invention is preferably 0.01 to 20% by weight, more preferably 0.05 to 10% by weight, from the viewpoints of the permeability of the matrix resin and the strength of the composite material. The weight ratio of the polyester resin (C) in the evaporation residue of the treating agent for carbon fiber intermediate substrate of the present invention is preferably 0.01 to 20% by weight, more preferably 0.05 to 10% by weight, from the viewpoints of the permeability of the matrix resin and the strength of the composite material.
[0058] The carbon fiber intermediate substrate treating agent is preferably diluted or dispersed in an aqueous medium to be in the form of an aqueous solution, aqueous emulsion or aqueous suspension, and then used to treat the carbon fiber intermediate substrate. When the carbon fiber intermediate substrate treatment agent is diluted and dispersed in an aqueous medium, it is easy to adjust the amount of solids contained in the carbon fiber intermediate substrate to be adhered to the carbon fiber intermediate substrate, so that a fiber intermediate substrate having even greater strength when made into a composite material can be obtained. As the aqueous medium, known aqueous media can be used, and specific examples thereof include water and hydrophilic organic solvents [C1-4 monohydric alcohols (methanol, ethanol, isopropanol, etc.), C3-6 ketones (acetone, ethyl methyl ketone, methyl isobutyl ketone, etc.), C2-6 glycols (ethylene glycol, propylene glycol, diethylene glycol, triethylene glycol, etc.) and their monoalkyl (C1-2) ethers, dimethylformamide, and C3-5 alkyl acetates (methyl acetate, ethyl acetate, etc.)]. These may be used in combination of two or more kinds. Among these, water is preferred from the viewpoint of safety and the like.
[0059] The content of the monol compound (A) in the treatment agent for carbon fiber intermediate substrates of the present invention when treating the carbon fiber intermediate substrate is preferably 0.1 to 20% by weight, more preferably 0.5 to 10% by weight, from the viewpoint of ensuring an appropriate amount of adhesion of the treatment agent when treating the carbon fiber intermediate substrate.
[0060] The concentration of the treatment liquid when treating with the treatment agent for carbon fiber intermediate substrates of the present invention (evaporation residue of the treatment agent for carbon fiber intermediate substrates) is preferably 0.1 to 20% by weight, more preferably 0.5 to 10% by weight, from the viewpoint of ensuring an appropriate amount of treatment agent adhered when treating the carbon fiber intermediate substrate.
[0061] There are no limitations on the mixing equipment, dissolving equipment, and emulsifying / dispersing equipment used when producing a treatment agent for carbon fiber intermediate substrates, and any of the following can be used: agitator blades (blade shape: paddle type, three-stage paddle, etc.), Nauta mixer, ribbon mixer, conical blender, mortar mixer, universal mixer (Universal Mixer Agitator 5DM-L, manufactured by San-Ei Manufacturing Co., Ltd., etc.), and Henschel mixer.
[0062] The carbon fiber intermediate substrate to be treated with the carbon fiber intermediate substrate treating agent of the present invention is one composed of a plurality of carbon fibers and means one prior to impregnation with a matrix resin, and examples thereof include carbon fiber bundles {short fiber bundles (chopped yarn, etc.)}, carbon fiber fabrics (unidirectional carbon fiber fabrics, two-dimensional carbon fiber fabrics, three-dimensional carbon fiber fabrics, four- or more dimensional carbon fiber fabrics, etc.), carbon fiber knitted fabrics, carbon fiber nonwoven fabrics (felt, mat, paper, etc.), and carbon fiber cloth.
[0063] The diameter of the carbon fibers is not particularly limited, but from the viewpoint of handling of the carbon fibers, it is preferably 4 to 20 μm, and more preferably 5 to 10 μm.
[0064] Examples of the treatment method include immersing the carbon fiber intermediate substrate in the treatment agent for carbon fiber intermediate substrates of the present invention (immersion method), or spraying the treatment agent for carbon fiber intermediate substrates of the present invention onto the carbon fiber intermediate substrate (spray method, etc.). The amount (wt%) of the evaporation residue contained in the carbon fiber intermediate substrate treatment agent adhered to the carbon fiber intermediate substrate is preferably 0.1 to 10 wt%, more preferably 1 to 5 wt%, based on the weight of the untreated carbon fiber intermediate substrate. When in this range, the strength of the composite material (molded product) is further improved. When a carbon fiber intermediate substrate is immersed in the carbon fiber intermediate substrate treatment agent of the present invention, the amount of evaporation residue contained in the carbon fiber intermediate substrate treatment agent is preferably 0.5 to 10 parts by weight, more preferably 1 to 5 parts by weight, per 100 parts by weight of the untreated carbon fiber intermediate substrate, from the viewpoint of permeability between the carbon fibers of the carbon fiber intermediate substrate. When the carbon fiber intermediate substrate treatment agent of the present invention is sprayed onto a carbon fiber intermediate substrate, the amount of evaporation residue contained in the carbon fiber intermediate substrate treatment agent is preferably 0.5 to 10 parts by weight, more preferably 1 to 5 parts by weight, per 100 parts by weight of the untreated carbon fiber intermediate substrate, from the viewpoint of permeability between the carbon fibers of the carbon fiber intermediate substrate. The drying temperature is preferably from 50 to 250°C, more preferably from 100 to 200°C, from the viewpoint of process time. From the viewpoint of removing the solvent, the drying time is preferably 1 to 30 minutes, and more preferably 2 to 20 minutes.
[0065] The carbon fiber intermediate substrate treated with the treating agent for carbon fiber intermediate substrates of the present invention is preferably used as a composite material in combination with a thermoplastic resin as a matrix resin. Examples of thermoplastic resins include polyethylene, polypropylene, polyethylene terephthalate, polybutylene terephthalate, polyamide, polystyrene, polyethersulfone, acrylonitrile-styrene resin, acrylonitrile-butadiene-styrene resin, acrylic resin, polycarbonate, polyetherimide, polyetheretherketone, polyacetal, polyphenylene oxide, and polyphenylene sulfide. Among these, polyethylene terephthalate, polybutylene terephthalate and polycarbonate are preferred from the viewpoint of the strength of the composite material.
[0066] From the viewpoint of the strength of the composite material, the weight ratio of the matrix resin to the carbon fiber intermediate substrate (matrix resin / carbon fiber intermediate substrate) in the composite material is preferably 10 / 90 to 90 / 10, more preferably 20 / 80 to 70 / 30, and particularly preferably 30 / 70 to 60 / 40.
[0067] The composite material can be produced by using the carbon fiber intermediate substrate treated with the carbon fiber intermediate substrate treating agent of the present invention, for example, by impregnating a carbon fiber intermediate substrate (woven fabric, knitted fabric, nonwoven fabric, etc.) treated with the carbon fiber intermediate substrate treating agent with the thermoplastic resin that has been heat-melted (melting temperature: 100 to 400°C) and molding the same, or by introducing a carbon fiber intermediate substrate (chopped fiber) treated with the carbon fiber intermediate substrate treating agent into the molten thermoplastic resin, kneading, and injection molding the same. EXAMPLES
[0068] The present invention will be further described below with reference to examples and comparative examples, but the present invention is not limited thereto. In the following descriptions, unless otherwise specified, % means % by weight and parts means parts by weight. In addition, In the above, Examples 1 to 15 and 24 are Reference Examples 1 to 16, respectively.
[0069] <Production Example 1> Cumylphenol EO 6 mole adduct (A-1) In a pressure-resistant reaction vessel equipped with a stirrer, a heating / cooling device, and a dropping bomb, 212 parts (1 mol) of cumylphenol "PCP" [manufactured by Mitsui Chemical Fine Co., Ltd.] and 0.5 parts of potassium hydroxide were put in, replaced with nitrogen, sealed, heated to 100°C, and dehydrated under reduced pressure for 1 hour. The temperature was raised to 160°C, and 264 parts (6 mol) of EO were dropped over 3 hours while adjusting the pressure to 0.5 MPaG or less, and then aged at 160°C for 3 hours. Next, after cooling to 70°C, 10 parts of an adsorption treatment agent "Kyoward 600" [manufactured by Kyowa Chemical Industry Co., Ltd.] were put in, and the mixture was stirred and treated at 70°C for 1 hour, and the adsorption treatment agent was filtered to obtain cumylphenol EO 6 mol adduct (A-1). {The number average molecular weight of (A-1) is 480, and HLB=11.1}
[0070] <Production Example 2> Cumylphenol EO 30 mole adduct (A-2) A cumylphenol EO 30-mol adduct (A-2) was obtained in the same manner as in Production Example 1, except that "EO 264 parts (6 mol parts)" was changed to "EO 1320 parts (30 mol parts)". {The number average molecular weight of (A-2) was 1530, and HLB=17.2}
[0071] <Production Example 3> Styrenated (2.75 mol) phenol EO 5 mol adduct (A-3) 94 parts (1 mol) of phenol and 5 parts of Lewis acid catalyst "Galleon Earth" [Mizusawa Chemical Industry Co., Ltd.] were charged into a reaction vessel equipped with a stirrer, a heating and cooling device, and a dropping bomb. The system was replaced with nitrogen gas while stirring, and the temperature was raised to 90°C. 286 parts (2.75 mol) of styrene were dropped at the same temperature over 5 hours, and the reaction was continued for another 5 hours at the same temperature. After cooling the product to 50°C, the catalyst was filtered off to obtain a 2.75 mol styrene adduct of phenol {styrenated (2.75 mol) phenol}. Next, 380 parts (1 mol) of the obtained styrenated (2.75 mol) phenol and 0.5 parts of potassium hydroxide were put into a pressure-resistant reaction vessel equipped with a stirrer, a heating / cooling device, and a dropping bomb, and after replacing with nitrogen, the vessel was sealed, heated to 100°C, and dehydrated under reduced pressure for 1 hour. The vessel was heated to 160°C, and 220 parts (5 mol) of EO were dropped over 3 hours while adjusting the pressure to 0.5 MPaG or less, and then aged at 160°C for 3 hours. Next, after cooling to 70°C, 10 parts of the adsorption treatment agent "Kyoward 600" [manufactured by Kyowa Chemical Industry Co., Ltd.] were put in, and the mixture was stirred and treated at 70°C for 1 hour, and the adsorption treatment agent was filtered to obtain styrenated (2.75 mol) phenol EO 5 mol adduct (A-3). {The number average molecular weight of (A-3) is 600, HLB=7.3}
[0072] <Production Example 4> Styrenated (1.1 mol) phenol EO 5 mol adduct (A-4) In Production Example 3, "286 parts (2.75 mol parts) of styrene" was changed to "114.4 parts (1.1 mol parts) of styrene", "380 parts (1 mol parts) of styrenated (2.75 mol) phenol" was changed to "208.4 parts (1 mol parts) of styrenated (1.1 mol) phenol", and "220 parts (5 mol parts) of EO" was changed to "264 parts (6 mol parts) of EO", but the same procedure as in Production Example 3 was followed to obtain styrenated (1.1 mol) phenol EO 6 mol adduct (A-4). {The number average molecular weight of (A-4) is 470, and HLB=11.2}
[0073] <Production Example 5> Styrenated (2 moles) phenol EO 17 moles adduct (A-5) In Production Example 3, "286 parts (2.75 mol parts) of styrene" was changed to "208 parts (2 mol parts) of styrene", "380 parts (1 mol part) of styrenated (2.75 mol) phenol" was changed to "302 parts (1 mol part) of styrenated (2 mol) phenol", and "220 parts (5 mol parts) of EO" was changed to "748 parts (17 mol parts) of EO", but the same procedure as in Production Example 3 was followed to obtain styrenated (2 mol) phenol EO 17 mol adduct (A-5). {The number average molecular weight of (A-5) is 1050, HLB=14.2}
[0074] <Production Example 6> Styrenated (2.75 mol) phenol EO 4 mol adduct (A-6) A styrenated (2.75 mol) phenol EO 4 mol adduct (A-6) was obtained in the same manner as in Production Example 3, except that "EO 220 parts (5 mol parts)" was changed to "EO 176 parts (4 mol parts)". {The number average molecular weight of (A-6) is 550, HLB = 6.3}
[0075] <Production Example 7> Styrenated (2 moles) cresol EO 10 moles adduct (A-7) In Production Example 3, "phenol 94 parts (1 mol)" was changed to "cresol "metacresol" [Honshu Chemical Industry Co., Ltd.] 108 parts (1 mol)", "styrene 286 parts (2.75 mol)" was changed to "styrene 208 parts (2 mol)", "styrenated (2.75 mol) phenol 380 parts (1 mol)" was changed to "styrenated (2 mol) cresol 316 parts (1 mol)", and "EO 220 parts (5 mol)" was changed to "EO 440 parts (10 mol)". The same procedure as in Production Example 3 was used to obtain styrenated (2 mol) cresol EO 10 mol adduct (A-7). {The number average molecular weight of (A-7) is 756, HLB = 11.6}
[0076] <Production Example 8> Styrenated (1 mol) cumylphenol EO 5 mol adduct (A-8) In Production Example 3, "phenol 94 parts (1 mol)" was changed to "cumylphenol "PCP" [manufactured by Mitsui Chemicals Fine Co., Ltd.] 212 parts (1 mol)", "styrene 286 parts (2.75 mol)" was changed to "styrene 104 parts (1 mol)", and "styrenated (2.75 mol) phenol 380 parts (1 mol)" was changed to "styrenated (1 mol) cumylphenol 316 parts (1 mol)". The same procedure as in Production Example 3 was used to obtain styrenated (1 mol) cumylphenol EO 5 mol adduct (A-8). {The number average molecular weight of (A-8) is 540, HLB = 8.2}
[0077] <Production Example 9> Styrenated (1 mol) cumylphenol EO 10 mol adduct (A-9) In Production Example 3, "phenol 94 parts (1 mol)" was changed to "cumylphenol "PCP" [Mitsui Chemicals Fine Co., Ltd.] 212 parts (1 mol)", "styrene 286 parts (2.75 mol)" was changed to "styrene 104 parts (1 mol)", "styrenated (2.75 mol) phenol 380 parts (1 mol)" was changed to "styrenated (1 mol) cumylphenol 316 parts (1 mol)", and "EO 220 parts (5 mol)" was changed to "EO 440 parts (10 mol)". The same procedure as in Production Example 3 was used to obtain styrenated (1 mol) cumylphenol EO 10 mol adduct (A-9). {Number average molecular weight of (A-9) is 760, HLB = 11.6}
[0078] <Production Example 10> Styrenated (1 mol) cumylphenol EO 25 mol adduct (A-10) In Production Example 3, "phenol 94 parts (1 mol)" was changed to "cumylphenol "PCP" [Mitsui Chemicals Fine Co., Ltd.] 212 parts (1 mol)", "styrene 286 parts (2.75 mol)" was changed to "styrene 104 parts (1 mol)", "styrenated (2.75 mol) phenol 380 parts (1 mol)" was changed to "styrenated (1 mol) cumylphenol 316 parts (1 mol)", and "EO 220 parts (5 mol)" was changed to "EO 1100 parts (25 mol)". The same procedure as in Production Example 3 was used to obtain styrenated (1 mol) cumylphenol EO 25 mol adduct (A-10). {Number average molecular weight of (A-10) is 1420, HLB = 15.5}
[0079] <Production Example 11> β-Naphthol EO 7 mole adduct (A-11) In Production Example 1, 212 parts (1 mol) of cumylphenol "PCP" [manufactured by Mitsui Fine Chemicals, Inc.] was replaced with 144 parts (1 mol) of β-naphthol "β-naphthol" [manufactured by Mitsui Fine Chemicals, Inc.], and 264 parts (6 mol) of EO was replaced with 308 parts (7 mol) of EO, in the same manner as in Production Example 1 to obtain β-naphthol EO 7 mol adduct (A-11). {The number average molecular weight of (A-11) is 450, and HLB=13.6}
[0080] <Production Example 12> β-Naphthol EO 20 mole adduct (A-12) In Production Example 1, 212 parts (1 mol) of cumylphenol "PCP" [manufactured by Mitsui Fine Chemicals, Inc.] was replaced with 144 parts (1 mol) of β-naphthol "β-naphthol" [manufactured by Mitsui Fine Chemicals, Inc.], and 264 parts (6 mol) of EO was replaced with 880 parts (20 mol) of EO. The procedure was the same as in Production Example 1, except that β-naphthol EO 20 mol adduct (A-12) was obtained. {The number average molecular weight of (A-12) is 1020, and HLB=17.2}
[0081] <Production Example 13> Styrenated (1 mol) naphthol EO 10 mol adduct (A-13) In Production Example 3, "phenol 94 parts (1 mol)" was changed to "β-naphthol 144 parts (1 mol)", "styrene 286 parts (2.75 mol)" was changed to "styrene 104 parts (1 mol)", "styrenated (2.75 mol) phenol 380 parts (1 mol)" was changed to "styrenated (1 mol) naphthol 248 parts (1 mol)", and "EO 220 parts (5 mol)" was changed to "EO 440 parts (10 mol)". The same procedure as in Production Example 3 was used to obtain styrenated (1 mol) naphthol EO 10 mol adduct (A-13). {The number average molecular weight of (A-13) is 690, HLB = 12.8}
[0082] <Production Example 14> Anthrol EO 10 mole adduct (A-14) In Production Example 1, 212 parts (1 mol) of cumylphenol "PCP" [Mitsui Fine Chemicals Co., Ltd.] was replaced with 194 parts (1 mol) of 9-anthrol [Fujifilm Wako Pure Chemical Industries, Ltd.], and 264 parts (6 mol) of EO was replaced with 440 parts (10 mol) of EO. An anthrol EO 10 mol adduct (A-14) was obtained in the same manner as in Production Example 1. {The number average molecular weight of (A-14) is 640, and HLB=13.9}
[0083] <Production Example 15> 4-(2-hydroxyethoxy)benzoic acid DBU salt (A-15) 182 parts (1 mol) of 4-(2-hydroxyethoxy)benzoic acid "HE-POB" [Ueno Pharmaceutical Co., Ltd.] and 334 parts of water were charged into a reaction vessel, and 152 parts (1 mol) of diazabicycloundecene "DBU" [San-Apro Co., Ltd.] was added dropwise under stirring to obtain a 50% by weight aqueous solution of 4-(2-hydroxyethoxy)benzoic acid DBU salt (A-15). {The molecular weight of (A-15) is 334}
[0084] <Comparative Preparation Example 1> Phenol EO 55 mole adduct (A'-2) A phenol-EO 55-mol adduct (A'-2) was obtained in the same manner as in Production Example 1, except that in Production Example 1, 212 parts (1 mol) of cumylphenol "PCP" [manufactured by Mitsui Fine Chemicals, Inc.] was changed to 94 parts (1 mol) of phenol, and 64 parts (6 mol) of EO was changed to 420 parts (55 mol) of EO. {The number average molecular weight of (A'-2) is 2420, and HLB is 19.3.}
[0085] <Production Example 16> Polyoxyethylene (4.5 mol) lauryl ether acetate diethanolamine salt (B-3) In a beaker in a reaction vessel equipped with a thermometer, a stirrer, and a nitrogen gas inlet tube, 44.2 parts by weight (0.1 parts by mole) of polyoxyethylene (4.5 mol) lauryl ether acetic acid [Viewlite LCA-25NH, manufactured by Sanyo Chemical Industries, Ltd.] and 50 ml of methanol were placed, and 10.5 parts by weight (0.1 parts by mole) of diethanolamine was added dropwise with stirring. The mixture was neutralized by stirring for 2 hours, and the methanol was removed under reduced pressure at 60°C to obtain polyoxyethylene (4.5 mol) lauryl ether acetic acid diethanolamine salt (B-3).
[0086] <Production Example 17> Triethanolamine laurate (B-6) In a reaction vessel equipped with a thermometer, a stirrer, and a nitrogen gas inlet tube, 200 parts by weight (1 part by mole) of lauric acid (Lunac L-98, manufactured by Kao Corporation) and 200 ml of tetrahydrofuran (hereinafter, abbreviated as THF) were placed in a beaker, and 149 parts by weight (1 part by mole) of triethanolamine was added dropwise with stirring. The mixture was neutralized by stirring for 2 hours, and the THF was removed at 80°C under reduced pressure to obtain triethanolamine laurate (B-6).
[0087] <Production Example 18> Decanol EO 55 mole adduct (B-7) In Production Example 1, 212 parts (1 mol) of cumylphenol "PCP" [manufactured by Mitsui Fine Chemicals, Inc.] was replaced with 158 parts (1 mol) of "decanol" [manufactured by KH Neochem Co., Ltd.], and 64 parts (6 mol) of EO2 was replaced with 420 parts (55 mol) of EO2, but the procedure was the same as in Production Example 1 to obtain a decanol EO 55 mol adduct (B-7). {The number average molecular weight of (B-7) is 2580, and HLB=18.8}
[0088] <Production Example 19> Polyester resin (C-1) 316 parts by weight (1 mol) of bisphenol A EO 2 mol adduct "Newpol BPE-20" [manufactured by Sanyo Chemical Industries, Ltd.], 142 parts by weight (0.86 mol) of terephthalic acid (a11) and 3 parts by weight of potassium oxalate titanate were reacted in a glass reaction vessel at 230°C for 15 hours while reducing the pressure to 0.001 MPa and distilling off water. 263 parts by weight (0.26 mol) of polyethylene glycol (b11) "PEG-1000" [manufactured by Sanyo Chemical Industries, Ltd.] was further added to the reaction mixture and reacted at 150°C and normal pressure for 2 hours to obtain 690 parts by weight of polyester resin (C-1). {The viscosity (complex viscosity) of (C-1) at 30°C is 100 Pa·s, HLB=8.8}
[0089] <Production Example 20> Polyester resin (C-2) 803 parts by weight of polyester resin (C-2) was obtained in the same manner as in Production Example 19, except that 142 parts by weight (0.86 parts by mole) of terephthalic acid (a11) was changed to 163 parts by weight (0.98 parts by mole), and 263 parts by weight (0.26 parts by mole) of polyethylene glycol (b11) "PEG-1000" [manufactured by Sanyo Chemical Industries, Ltd.] was changed to 359 parts by weight (0.04 parts by mole) of polyethylene glycol (b12) "PEG-10000" [manufactured by Sanyo Chemical Industries, Ltd.]. {The viscosity (complex viscosity) of (C-2) at 30°C was 800,000 Pa·s, HLB=9.8}
[0090] <Examples 1 to 24 and Comparative Examples 1 to 2> The raw materials were mixed in the amounts by weight shown in Table 1 to obtain the carbon fiber intermediate substrate treating agents (X-1) to (X-24) of the present invention and the comparative carbon fiber intermediate substrate treating agents (X'-1) to (X'-2).
[0091] [Table 1]
[0092] The chemical compositions of the raw materials with the symbols shown in Table 1 are as follows: The blending amounts (parts by weight) in Table 1 are listed as pure amounts. (A-1) to (A-15): Obtained in Production Examples 1 to 15 (A'-1): EO 18 mole adduct of bisphenol A [number average molecular weight 1020, trade name "Newpol BPE-180", manufactured by Sanyo Chemical Industries, Ltd.] (A'-2): Obtained in Comparative Production Example 1 (B-1): 30% by weight aqueous solution of polyoxyethylene (4 mol) lauryl ether sulfate triethanolamine [product name "Sandet ET", manufactured by Sanyo Chemical Industries, Ltd.] (B-2): 40% by weight aqueous solution of alkyl (C12, 13) triethanolamine sulfate (product name "Sandet LTD", manufactured by Sanyo Chemical Industries, Ltd.) (B-3): Obtained in Production Example 16 (B-4): Polyoxyethylene polycyclic phenyl ether sulfate ammonium salt [product name "Newcol 707SF", manufactured by Nippon Nyukazai Co., Ltd.] (B-5): Polyoxyalkylene alkenyl ether ammonium sulfate [product name "Latemul PD-140", manufactured by Kao Corporation] (B-6) to (B-7): Obtained in Production Examples 17 to 18 (C-1) to (C-2): Obtained in Production Examples 19 to 20
[0093] The carbon fiber intermediate substrates were treated with the carbon fiber intermediate substrate treating agents of the Examples and Comparative Examples, and the strength of the composite material and the permeability of the matrix resin were evaluated by the following evaluation methods. The results are shown in Table 1.
[0094] <Manufacturing of carbon fiber intermediate materials> The carbon fiber intermediate substrate treating agents (X-1) to (X-24) obtained in Examples 1 to 24 and the comparative carbon fiber intermediate substrate treating agents (X'-1) to (X'-2) were dissolved and dispersed in water so that the evaporation residue was 2% by weight. A carbon fiber fabric (product name "EC3C", manufactured by Taiwan Plastics) was immersed in the solution, passed through nip rolls so that the evaporation residue (adhesion amount) was 2% by weight relative to the carbon fiber fabric, and impregnated with the treating agent. The fabric was then dried with hot air at 200°C for 3 minutes to obtain a carbon fiber intermediate substrate (carbon fiber fabric) treated with the treating agent.
[0095] <Strength of composite materials> Both sides of the carbon fiber intermediate substrate (carbon fiber fabric) treated with the obtained treatment agent were laminated with a polycarbonate resin film "Technoloy C000" [Sumitomo Chemical Co., Ltd.] and compressed at 270°C and a pressure of 2 MPa for 3 minutes to obtain a carbon fiber composite material with a thickness of 250 μm (carbon fiber volume content of 50%). The flexural modulus and flexural strength of the obtained carbon fiber composite material were measured in accordance with JIS K7074.
[0096] <Matrix resin permeability> (1) Both sides of the carbon fiber intermediate substrate (carbon fiber fabric) treated with the obtained treatment agent were laminated with a polycarbonate resin film "Technoloy C000" [Sumitomo Chemical Co., Ltd.] and compressed at 270°C and a pressure of 2 MPa for 1.5 minutes to obtain a carbon fiber composite material with a thickness of 250 μm (carbon fiber volume content: 50% by weight). (2) The obtained carbon fiber composite material was cut, and the cross section perpendicular to the fiber direction was examined using an optical microscope. (3) The cross-sectional image (magnification 900x) was printed out on paper, and the resin-impregnated and non-impregnated parts were cut out. Each piece of paper was weighed and the impregnation rate was calculated using the following formula. Matrix resin permeability (%) = (weight of part impregnated with resin) / [(weight of part impregnated with resin)+(weight of part not impregnated with resin)]×100
[0097] From the results in Table 1, it can be seen that the carbon fiber fabrics treated with the carbon fiber intermediate substrate treating agent of the present invention in Examples 1 to 24 are permeated with the matrix resin by 85% or more in a short time of 1.5 minutes, and penetrate almost to the center, so that the matrix resin has high permeability. It can be seen that the carbon fiber composite material using the carbon fiber fabrics treated with the carbon fiber intermediate substrate treating agent of the present invention has high flexural modulus and flexural strength, and excellent molded body strength. [Industrial Applicability]
[0098] The treating agent for carbon fiber intermediate substrates of the present invention is useful as a treating agent for enhancing the permeability of matrix resins in carbon fiber intermediate substrates such as carbon fiber bundles {short fiber bundles (chopped yarn, etc.)}, carbon fiber fabrics (unidirectional carbon fiber fabrics, two-dimensional carbon fiber fabrics, three-dimensional carbon fiber fabrics, four- or more dimensional carbon fiber fabrics, etc.), carbon fiber knitted fabrics, carbon fiber nonwoven fabrics (felt, mat, paper, etc.), and carbon fiber cloth.
Claims
[Claim 1] A treatment agent for carbon fiber intermediate substrates, comprising a monol compound (A) having a chemical formula weight or number average molecular weight of 2000 or less, the monol compound (A) is an ethylene oxide adduct of an aromatic monol, and the aromatic monol is at least one selected from the group consisting of cumylphenol, naphthol, anthrol, styrenated phenol, styrenated cresol, styrenated cumylphenol, and styrenated naphthol; the ethylene oxide adduct of the aromatic monool has an ethylene oxide addition mole number of 6 to 43; The composition further comprises a surfactant (B), the surfactant (B) being at least one selected from the group consisting of a nonionic surfactant (B12) having an aralkyl group having 7 to 24 carbon atoms, a carboxylate (B21) having a saturated or unsaturated aliphatic group having 7 to 24 carbon atoms, a sulfate (B22) having a saturated or unsaturated aliphatic group having 7 to 24 carbon atoms or an aralkyl group having 7 to 62 carbon atoms, and a sulfonate (B26) having a saturated or unsaturated aliphatic group having 12 to 18 carbon atoms or an aralkyl group having 7 to 62 carbon atoms, the weight ratio ((A) / (B)) of the monool compound (A) to the surfactant (B) is 80 / 20 to 99 / 1; A carbon fiber intermediate substrate treating agent, in which the weight ratio of the monool compound (A) in the evaporation residue according to JIS K0067 (1992) for carbon fiber intermediate substrate treating agents is 80% by weight or more and less than 100%.
Citation Information
Patent Citations
Carbonizable substance for coating of carbon yarn and treatment of carbon yarn using the same substance
JP1992209872A
Method for producing opened fiber sheet, method for producing thermoplastic resin-impregnated prepreg sheet with the same as reinforcing base, and production machine for the opened fiber sheet, and thermoplastic rein impregnator for the opened fiber sheet
JP2005029912A
JPP6556968B