Electrolyte printed membrane and its manufacturing method

The electrolyte membrane uses a printing method to hold liquid electrolytes between insulating particles, ensuring precise patterns and stable operation with a simple sealing structure, addressing the challenges of pattern precision and conductivity in existing technologies.

JP7591808B2Active Publication Date: 2024-11-29NATIONAL INSTITUTE OF ADVANCED INDUSTRIAL SCIENCE & TECHNOLOGY
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2020179003
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-10-26
Publication Date
2024-11-29
Estimated Expiration
2040-10-26

AI Technical Summary

Technical Problem

Existing methods for forming electrolyte membranes using liquid electrolytes face challenges in achieving precise patterns and maintaining high ionic conductivity while simplifying the sealing structure, as solidification reduces conductivity and complicates sealing.

Method used

An electrolyte membrane formed using a printing method where a liquid electrolyte with ion conductivity is held between insulating particles by capillary force, fixed in shape on a substrate, allowing for a simple sealing structure.

Benefits of technology

Enables precise patterns and stable operation over a long period with a simple sealing structure, maintaining high ionic conductivity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007591808000001
    Figure 0007591808000001
  • Figure 0007591808000002
    Figure 0007591808000002
  • Figure 0007591808000003
    Figure 0007591808000003
Patent Text Reader

Abstract

To provide an electrolyte membrane that allows a precise pattern to be obtained using an inexpensive printing method, allows stable operation for a long time even with a simple sealing structure and is composed of ionic liquid, and a method for producing the same.SOLUTION: An electrolyte membrane can be formed using a printing method and includes a liquid electrolyte 2 having ionic conductivity that is held among insulation particles 3 by capillary action and fixed in shape on a substrate. The electrolyte membrane is formed on the substrate by transferring the ink given to a blanket 11 onto the substrate to be patterned. The ink is a solvent mixture 6 containing the liquid electrolyte 2 having ionic conductivity mixed in a dispersion solvent 4 with the insulation particles 3. The ink is given to the blanket by patterning to cause the dispersion solvent to be selectively absorbed onto the blanket and then transferred onto the substrate to produce an electrolyte membrane.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an electrolyte membrane that can be formed using a printing method and a method for producing the same. [Background technology]

[0002] It is necessary to form an electrolyte film on a substrate in order to manufacture planar electric double-layer capacitors (micro-supercapacitors), gate films for thin-film transistors that can be driven at low voltages, lithium-ion secondary batteries, etc. Here, when a liquid electrolyte is used for the electrolyte film, a cheaper manufacturing method can be used compared to vacuum film formation processes such as printing methods, but problems have been pointed out, such as the fact that it is more susceptible to deterioration than solid electrolytes, requiring strict sealing, and it is also difficult to laminate new functional layers on top of it.

[0003] For example, Patent Document 1 discloses a method for manufacturing an electrochemical cell in which a three-layer structure film of MnO2 cathode electrode film-gel electrolyte film-Zn anode electrode film is printed on a nickel substrate and then dried. Here, the electrode uses a slurry of active electrode material particles, and the gel electrolyte film uses an electrolyte consisting of a polymer network such as polyvinyl alcohol (PVA) absorbed with an ionic liquid. The gel electrolyte film acts as a physical and electronic separator between the cathode and anode electrodes, and by combining an ionic liquid, which is an organic salt with a low melting point, with the polymer network, the gel electrolyte film does not evaporate or leak even under long-term use, and does not require expensive and complicated sealed packaging.

[0004] So far, methods for forming an electrolyte membrane have been proposed, such as mixing a liquid electrolyte with a polymer network such as PVA as described above, and polymerizing and solidifying an ionic liquid, which is a liquid electrolyte. In all of these methods, the electrolyte is liquid when patterned onto a substrate, and it is difficult to form a precise pattern due to wetting or repelling the substrate, but as described above, a simple and inexpensive manufacturing method such as a printing method can be used. In addition, solidification can simplify the sealing structure. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2018-49833 A Summary of the Invention [Problem to be solved by the invention]

[0006] Generally, when a liquid electrolyte with ion conductivity is solidified, the ion conductivity is significantly reduced. Therefore, by using an ionic liquid with low vapor pressure in the electrolyte membrane without solidifying it, it is expected that the ion conductivity will not be reduced and high ion conductivity can be maintained even with a simple sealing structure, allowing stable operation for a long period of time.

[0007] The present invention has been made in consideration of the above-mentioned circumstances, and an object of the present invention is to provide an electrolyte membrane made of an ionic liquid that can be patterned precisely using an inexpensive printing method and that can operate stably for a long period of time even with a simple sealing structure, and a method for manufacturing the same. [Means for solving the problem]

[0008] The electrolyte membrane according to the present invention is an electrolyte membrane that can be formed by a printing method, and is characterized in that an ionically conductive liquid electrolyte is held between insulating particles by capillary force and fixed in shape on a substrate.

[0009] These features allow precise patterns to be obtained using inexpensive printing methods, and the liquid electrolyte is held between the insulating particles by capillary force and fixed in shape on the substrate, making it possible to operate stably for long periods of time even with a simple sealing structure.

[0010] In the above-mentioned invention, the liquid electrolyte may be an ionic liquid. According to this feature, by using an ionic liquid having a low vapor pressure as the liquid electrolyte, it becomes possible to operate stably for a long period of time even with a simple sealing structure.

[0011] In the above-mentioned invention, the liquid electrolyte may be a lithium salt solution such as lithium chloride, lithium nitrate, lithium bis(trifluoromethanesulfonyl)imide, lithium hexafluorophosphate, etc. According to this feature, as a component of a lithium ion secondary battery, it can operate stably for a long period of time even with a simple sealing structure.

[0012] In the above-mentioned invention, the liquid electrolyte may be a solution made of tetraethylammonium tetrafluoroborate. With this feature, as a member of an electric double layer capacitor, it can operate stably for a long period of time even with a simple sealing structure.

[0013] In the above-mentioned invention, the insulating particles may have an average cross-sectional diameter of 0.1 μm or less and a volume fraction of 50% or more. With this feature, the liquid electrolyte can be capillary condensed between the insulating particles to reliably fix the shape on the substrate, and even with a simple sealing structure, it is possible to operate stably for a long period of time.

[0014] In addition, a manufacturing method according to the present invention is a method for forming a patterned electrolyte membrane on a substrate by transferring an ink applied to a blanket onto the substrate, the ink containing an ionically conductive liquid electrolyte mixed with insulating particles in a dispersion solvent, the ink being applied to the blanket in a pattern to cause the dispersion solvent to be selectively absorbed into the blanket, and then transferred to the substrate, and the liquid electrolyte is subjected to capillary condensation between the insulating particles to fix the shape on the substrate.

[0015] These features make it possible to obtain precise patterns using inexpensive printing methods, and also to cause capillary condensation of the liquid electrolyte between the insulating particles to fix the shape on the substrate, thereby obtaining an electrolyte membrane that can operate stably for a long period of time even with a simple sealing structure.

[0016] In the above-mentioned invention, the blanket may have a faster absorption rate of the dispersion solvent than the liquid electrolyte. The blanket may be made of silicone rubber. With this feature, a more precise pattern can be obtained using an inexpensive printing method, and the liquid electrolyte can be capillary condensed between insulating particles to reliably fix the shape on the substrate, thereby obtaining an electrolyte membrane that can stably operate for a long period of time even with a simple sealing structure.

[0017] In the above-mentioned invention, the ink may further contain a polymer having a gel-forming ability. With this feature, a more precise pattern can be obtained using an inexpensive printing method, and the liquid electrolyte can be reliably fixed in shape on the substrate to obtain an electrolyte membrane that can operate stably for a long period of time even with a simple sealing structure.

[0018] In the above-mentioned invention, the insulating particles may have an average cross-sectional diameter of 0.1 μm or less, and may be added to the ink so as to be fixed in shape on the substrate and to constitute 50% or more by volume. This feature makes it possible to obtain a more precise pattern using an inexpensive printing method, and to reliably fix the shape of the liquid electrolyte on the substrate, thereby obtaining an electrolyte membrane that can stably operate for a long period of time even with a simple sealing structure. [Brief description of the drawings]

[0019] [Figure 1] 1 is a cross-sectional view of an electrolyte membrane according to an example of the present invention. [Diagram 2] FIG. 2 is an explanatory diagram of the process of reverse offset printing. [Diagram 3] FIG. 1 shows the change in ink on a blanket. [Figure 4] 1 is a table showing the ink formulations used in the production tests. [Diagram 5] 13 is a table showing other ink formulations used in production testing. [Figure 6] 1 is a photograph showing the appearance of an electrolyte membrane produced in a production test. [Figure 7] FIG. 2 is a cross-sectional view of an electric double layer capacitor manufactured in a manufacturing test. [Figure 8] 1 is a graph showing the change in potential over time during constant current charging of an electric double layer capacitor. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0020] One embodiment of the present invention will be described with reference to FIG.

[0021] As shown in Fig. 1, the electrolyte membrane 1 can be formed by a printing method, and an ionically conductive liquid electrolyte 2 is capillary condensed between insulating particles 3 and fixed in shape on a substrate 9. In other words, the insulating particles 3 form narrow gaps between each other, and the liquid electrolyte 2 is held between the insulating particles 3 by capillary force, resulting in the vapor pressure of the liquid electrolyte 2 being apparently lower than the bulk vapor pressure. Therefore, even with a simple sealing structure, the liquid electrolyte 2 can be kept in the electrolyte membrane 1 for a long period of time, enabling it to function as a stable electrolyte.

[0022] It is preferable that the liquid electrolyte 2 is an ionic liquid having a low vapor pressure, since this allows the liquid electrolyte 2 to be retained within the electrolyte membrane 1 for a longer period of time.

[0023] The liquid electrolyte 2 may be a solution in which a salt is dissolved in a solvent. For example, lithium salts such as lithium chloride, lithium nitrate, lithium bis(trifluoromethanesulfonyl)imide, and lithium hexafluorophosphate can be suitably used as such salts. When such lithium salts are used, they show high solubility in the solvent, and the electrolyte membrane 1 can be used as a member of a lithium ion battery. For example, tetraethylammonium tetrafluoroborate can be suitably used as a salt used in the liquid electrolyte 2. When such salts are used, an electrolyte with high electrochemical stability and high electrical conductivity can be obtained, and the electrolyte membrane 1 can be used as a member of an electric double layer capacitor. Details of the solvent used in the liquid electrolyte 2 will be described later.

[0024] The insulating particles 3 are used to fix the shape of the liquid electrolyte 2. Therefore, there is no limitation on the composition as long as the insulating particles are insulating. For example, insulating oxide particles such as silica, zirconia, alumina, clay minerals, and barium titanate can be suitably used as the insulating particles 3. On the other hand, it is preferable that the insulating particles 3 reliably fix the shape of the liquid electrolyte 2 by the gaps between the insulating particles 3 through capillary condensation, and can be precisely patterned. For example, it is preferable that the insulating particles have an average cross-sectional diameter of 0.1 μm or less, and are contained in the electrolyte membrane 1 at a volume ratio of 50% or more.

[0025] As described above, the electrolyte membrane 1 can be formed by using a printing method. Meanwhile, as described above, the insulating particles 3 are arranged so as to narrow the gaps between the particles, i.e., to make the particles denser, in order to fix the shape of the liquid electrolyte 2 by capillary condensation. In other words, the electrolyte membrane 1 has poor fluidity. In general, it is difficult to print such a paste-like material with poor fluidity in a uniform thickness, making the printing itself difficult.

[0026] A method for producing such an electrolyte membrane 1 by printing will be described with reference to FIGS.

[0027] 2, the electrolyte membrane 1 can be manufactured by offset printing, such as gravure offset printing, reverse offset printing, adhesion contrast printing, etc. Here, reverse offset printing will be taken as an example for explanation.

[0028] 2(a), ink 13 is applied to a blanket 11 by an ink coater 12 (coating step). The ink 13 contains an ion-conductive liquid electrolyte 2 mixed with insulating particles 3 in a dispersion solvent.

[0029] Next, as shown in FIG. 2(b), the ink 13 on the blanket 11 is brought into contact with a cliché 14 to remove a portion of the ink 13, thereby performing patterning (OFF process).

[0030] Finally, as shown in FIG. 2(c), the ink 13 patterned on the blanket 11 is transferred onto the substrate 9 (SET process).

[0031] As described above, the ink 13 is patterned by reverse offset printing and transferred onto the substrate 9, but the ink 13 needs to have a suitable fluidity in the coating process. Therefore, as described above, the ink 13 contains a dispersion solvent. On the other hand, in the electrolyte membrane 1 after the ink 13 is transferred in the SET process, the liquid electrolyte 2 must be able to be fixed in shape by capillary condensation as described above, and it is preferable to reduce the fluidity. Therefore, the dispersion solvent of the ink 13 is selectively absorbed into the blanket before it is transferred to the substrate 9. This gives the ink 13 the fluidity required for application in the coating process, and the dispersion solvent is reduced by the time of the SET process, so that the ink 13 can have the function of fixing the shape required for the electrolyte membrane 1 after transfer. For such selective absorption into the blanket 11, it is preferable that the absorption speed of the dispersion solvent into the blanket 11 is greater than the absorption speed of the liquid electrolyte 2.

[0032] In detail, as shown in FIG. 3(a), the ink 13 to be applied to the blanket 11 contains a dispersion solvent 4 so as to have the fluidity required for application to the blanket 11. The ink 13 is preferably a mixture of the dispersion solvent 4 and the liquid electrolyte 2, in which the insulating particles 3 are uniformly dispersed. The volume ratio of the content of the liquid electrolyte 2 to the content of the insulating particles 3 is preferably within a range of 0.5 to 1. This volume ratio is determined so as to reliably fix the shape of the obtained electrolyte membrane 1. If the content of the liquid electrolyte 2 is too high, the obtained electrolyte membrane 1 is given fluidity, and the shape fixation by the insulating particles 3 cannot be sufficiently obtained. On the other hand, if the content of the liquid electrolyte 2 is too low, sufficient ion conductivity cannot be obtained, and furthermore, transfer from the blanket 11 becomes difficult. In addition, the viscosity of the liquid electrolyte 2 is preferably 10 mPa·s or less from the viewpoint of ion conductivity.

[0033] As shown in FIG. 3(b), the dispersion solvent 4 is selectively absorbed by the blanket 11 from the ink 13 before the SET process. That is, the blanket 11 is made of a material capable of absorbing the dispersion solvent 4, and for example, silicone rubber can be preferably used. A representative example of silicone rubber is polydimethylsiloxane. As the dispersion solvent 4, a material that is easily absorbed by the blanket 11 and easily evaporates at room temperature is preferable, and for example, propylene glycol monomethyl ether acetate (PGMEA), propylene glycol monomethyl ether (PGME), ethylene glycol diethyl ether, methyl ethyl ketone, methyl isobutyl ketone, cyclohexanone, ethyl acetate, isopropyl acetate, diethyl carbonate, methyl propyl carbonate, isopropyl alcohol, ethanol, and butanol can be preferably used.

[0034] Furthermore, as shown in FIG. 3( c ), almost no dispersion solvent 4 remains due to absorption into the blanket 11 and evaporation, and the ink 13 can be transferred to the substrate 9 to obtain a patterned electrolyte membrane 1 .

[0035] In this way, the dispersion solvent 4 can be reduced to almost nothing, and can be used without affecting the resulting electrolyte membrane 1. Meanwhile, the content of the dispersion solvent 4 affects the viscosity of the ink 13 to be applied, and determines the fluidity. The content of the dispersion solvent 4 can be appropriately determined according to the printing method including application and the thickness of the electrolyte membrane 1 to be obtained, so as to adjust the viscosity. For example, in the ink 13, the content of the dispersion solvent 4 relative to the content of the insulating particles 3 is desirably 5 to 20 v / v %.

[0036] The ink 13 may contain known ink additives such as a dispersant for improving the dispersibility of the insulating particles 3, a surfactant for improving the wettability to the substrate 9, a polymer assistant for adjusting the viscosity of the ink 13, and a binder resin for improving the binding between the insulating particles 3 and the substrate 9. In order to improve the dispersion stability of the insulating particles 3, a mixture of multiple solvents may be used as the dispersion solvent 4. Furthermore, in order to further improve the shape fixation of the liquid electrolyte 2, a polymer having a gel forming ability such as polyvinyl alcohol, polyvinylidene fluoride, or polymethyl methacrylate may be added.

[0037] As described above, the dispersion solvent 4 is selectively absorbed into the blanket 11 from the ink 13. For this reason, when a salt solution is used as the liquid electrolyte 2, it is preferable that the solution and its solvent have a low absorption rate into the blanket 11. It is desirable that the solvent is liquid at room temperature, has a low viscosity, a high dielectric constant, a high boiling point, and is electrochemically stable. When silicone rubber is used as the blanket 11, examples of solvents having a low absorption rate include alkyl carbonate solvents such as ethylene carbonate and propylene carbonate, lactone solvents such as gamma butyrolactone and valerolactone, lactam solvents such as 1-methyl-2-pyrrolidone, polyhydric alcohol solvents such as ethylene glycol and 1,3-propanediol, amide solvents such as dimethylformamide and dimethylacetamide, nitrile solvents such as acetonitrile and adiponitrile, and water. The salt concentration of the liquid electrolyte 2 may be set to a range that completely dissolves the salt and increases the ion conductivity, and is generally within the range of 0.5 to 2M.

[0038] The absorption rate of the solvent used for the liquid electrolyte 2 into the blanket 11 can be estimated from the weight change of the material of the blanket 11 with respect to the time of immersion in the solvent. In general, the absorption rate can be reduced as the polarity of the solvent increases and the molecular weight of the solvent increases. Solvents with high polarity generally tend to exhibit a high dielectric constant, which is desirable from the viewpoints of both the ionic conductivity of the liquid electrolyte 2 and the transferability from the blanket 11.

[0039] On the other hand, as described above, an ionic liquid may also be suitably used as the liquid electrolyte 2. An ionic liquid is liquid at room temperature, has low viscosity, exhibits ionic conductivity, and has a high boiling point (i.e., has a low vapor pressure at room temperature), and therefore can be used as is as the liquid electrolyte 2 without adding a solvent. Note that, in order to further improve the shape fixation of the liquid electrolyte 2, a reactive ionic liquid that polymerizes by a polymerization reaction may also be used.

[0040] [Manufacturing test] Next, the results of actually producing an electrolyte membrane will be described with reference to FIGS.

[0041] As shown in FIG. 4, the electrolyte membrane 1 was produced by reverse offset printing using the inks of each composition of samples 1 to 5, which were patterned into a comb-tooth shape. As the dispersion solvent, 0.5 g and 1.4 g of the above-mentioned PGMEA and PGME were mixed, respectively. As the insulating particles, 0.6 g of SiO2 nanoparticles with an average cross-sectional diameter of 10 to 15 nm were mixed. As the liquid electrolyte, a solution in which a salt made of lithium chloride (sample 1) or lithium nitrate (samples 2 to 4) was dissolved in a solvent was mixed in the amount shown in the figure for samples 1 to 4, and an ionic liquid was mixed in the amount shown in the figure for samples 4 and 5. Note that N-methyl-2-pyrrolidone (NMP) was used as the solvent, and 1-butyl-1-methylpyrrolidinium bis(trifluoromethylsulfonyl)amine anion (BMP-TFSI) was used as the ionic liquid. In addition, 0.002 g of a surfactant was mixed in each sample.

[0042] Furthermore, as shown in FIG. 5, electrolyte membranes 1 were similarly manufactured using the inks of each composition of samples 6 to 8. As the dispersion solvent, in addition to the above-mentioned PGMEA or PGME, cyclohexanone, isopropyl alcohol, and ethylene glycol were further blended in the amounts shown in the figure. As the insulating particles, 0.15 g of SiO2 nanoparticles similar to those described above were blended. As the liquid electrolyte, a solution in which tetraethylammonium tetrafluoroborate was dissolved in a solvent was blended in the amount shown in the figure. Propylene carbonate was used as the solvent. No ionic liquid was used in samples 6 to 8. In addition, 0.001 g of a surfactant was blended in each sample.

[0043] Figures 6(a) and (b) show the external appearance of the electrolyte membranes of sample 1 and sample 4, respectively, as representative examples. All samples, including the other samples (2, 3, 5, 6, 7, and 8), were successfully printed, and precisely patterned electrolyte membranes were obtained. Furthermore, even after leaving the electrolyte membranes for two weeks in an open-air atmosphere at a temperature of 23°C and a relative humidity of 50%, no precipitation of ionic salts was observed on the surface of the electrolyte membrane, and it was determined that the shape of the liquid electrolyte was fixed by capillary condensation.

[0044] As shown in Fig. 7, an electric double layer capacitor 20 was produced using the ink of sample 1, and the charging characteristics were measured. A pair of flat carbon electrodes 8 were provided at a distance from each other on a glass substrate 9, and a patterned electrolyte membrane 1 was formed by printing from above so as to cover both electrodes.

[0045] As shown in Figure 8, the electric double layer capacitor was charged at a constant current (10nA, 20nA, 30nA, 40nA) and the time change in the potential difference between the electrodes was measured. It was confirmed that the potential difference increased more quickly as the current was increased.

[0046] As described above, an electrolyte membrane in which an ion-conductive liquid electrolyte is capillary condensed between insulating particles and fixed in shape on a substrate can be formed using a printing method. This makes it possible to obtain precise patterns using an inexpensive printing method, and to create an electrolyte membrane that can operate stably for a long period of time even with a simple sealing structure.

[0047] Although the exemplary embodiment and modified examples based thereon according to the present invention have been described above, the present invention is not necessarily limited thereto. Those skilled in the art will be able to find various alternative embodiments without departing from the scope of the appended claims. [Explanation of symbols]

[0048] 1 Electrolyte membrane 2 Liquid electrolyte 3. Insulating particles 9 Substrate 11 Blanket

Claims

1. An electrolyte printed film formed on a substrate, An electrolyte printed membrane, characterized in that an ionically conductive liquid electrolyte is held between condensed insulating particles by capillary force and its shape is fixed on the substrate.

2. 2. The electrolyte printed membrane according to claim 1, wherein the liquid electrolyte is an ionic liquid.

3. 2. The electrolyte printed membrane according to claim 1, wherein the liquid electrolyte is a lithium salt solution of lithium chloride, lithium nitrate, lithium bis(trifluoromethanesulfonyl)imide, or lithium hexafluorophosphate.

4. 2. The electrolyte printed membrane according to claim 1, wherein the liquid electrolyte is a solution containing tetraethylammonium tetrafluoroborate as a supporting salt.

5. 2. The electrolyte printed membrane according to claim 1, wherein the insulating particles have an average cross-sectional diameter of 0.1 μm or less and a volume fraction of the insulating particles of 50% or more.

6. A method for manufacturing an electrolyte printed film, comprising the steps of: transferring an ink applied to a blanket onto a substrate to form a patterned electrolyte film on the substrate, the method comprising the steps of: The ink contains an ionically conductive liquid electrolyte mixed with insulating particles in a dispersion solvent, A method for manufacturing an electrolyte printed membrane, comprising: providing the ink in a pattern onto the blanket, selectively absorbing the dispersion solvent into the blanket to condense the insulating particles, and then transferring the ink onto the substrate; and holding a non-polymer liquid electrolyte between the condensed insulating particles by capillary force to fix the shape on the substrate.

7. 7. The method for producing an electrolyte printed membrane according to claim 6, wherein the blanket absorbs the dispersion solvent at a rate faster than the liquid electrolyte.

8. 8. The method for producing an electrolyte printed membrane according to claim 7, wherein the blanket is made of silicone rubber.

9. 9. The method for producing an electrolyte printed membrane according to claim 6, wherein the ink further contains a polymer having a gel-forming ability.

10. The method for manufacturing an electrolyte printing membrane according to any one of claims 6 to 9, characterized in that the insulating particles have an average cross-sectional diameter of 0.1 μm or less, are fixed in shape on the substrate, and are added to the ink so as to account for 50% or more by volume.

Citation Information

Patent Citations

  • Gel-type electrolyte and lithium battery

    JP2001229966A

  • Electrolyte and secondary battery using the same

    JP2010135129A

  • Colloidal electrolyte composition

    JP2014512434A

  • Ionic gel electrolyte, energy storage devices, and methods of manufacture thereof

    JP2018049833A

  • Electrolyte for lithium secondary battery and lithium secondary battery containing same

    JP2019522875A