Battery manufacturing method
By employing separators with a PVdF and inorganic particle surface layer, the method addresses miswinding issues, improving the productivity of battery manufacturing by ensuring stable winding and reducing separator discard rates.
Patent Information
- Application Number
- JP2021131374
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-08-11
- Publication Date
- 2024-12-04
- Estimated Expiration
- 2041-08-11
AI Technical Summary
The existing method for manufacturing electrode plate groups in non-aqueous secondary batteries results in high discard rates of separators due to miswinding, leading to reduced productivity.
A method for manufacturing batteries that involves using separators with a porous base material layer and a surface layer containing polyvinylidene fluoride (PVdF) and inorganic particles, which are wound around a core with a pressing mechanism to improve alignment and reduce misalignment.
This approach enhances the productivity of wound electrode bodies by effectively suppressing misalignment and enabling continuous production.
Smart Images

Figure 0007594508000001 
Figure 0007594508000002 
Figure 0007594508000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a battery. [Background technology]
[0002] JP 2009-193750 A discloses a method for manufacturing an electrode plate group for a non-aqueous secondary battery, in which strip-shaped positive and negative electrode plates are alternately stacked with two separators and wound into a spiral shape. In the manufacturing method disclosed in this publication, the leading end of the separator is pressed against and attracted to a winding core, and the positive and negative electrode plates are sandwiched and wound into a spiral shape. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2009-193750 A Summary of the Invention [Problem to be solved by the invention]
[0004] In such a manufacturing method, a separator having a base layer and a surface layer may be used as the separator used in the wound electrode body. Since such a separator having a base layer and a surface layer is expensive, reducing the number of separators that are disposed of due to misalignment of winding or the like can contribute to improving productivity. Therefore, the present inventors would like to improve productivity by eliminating problems such as misalignment of winding in a simpler way. [Means for solving the problem]
[0005] The method for manufacturing a battery disclosed herein is a method for manufacturing a battery including a wound electrode body, and includes the following steps. Step A: A step of adsorbing the first separator and the second separator onto the core in a stacked state. Step B: A step of winding the first separator and the second separator onto the core. Here, the first separator and the second separator each have a porous base material layer made of resin and a surface layer formed on at least one surface of the base material layer.
[0006] According to this manufacturing method, the productivity of the wound electrode body can be improved.
[0007] In each of the first and second separators, when the surface layers are formed on both sides of the substrate layer, the surface layers may have a three-dimensional network structure containing polyvinylidene fluoride (PVdF), the mass ratio of PVdF in the surface layers may be 10 mass% or more, and the surface layers may further contain inorganic particles in addition to PVdF.
[0008] When the surface layer of each of the first separator and the second separator is formed only on one side of the base layer, the surface layer may contain inorganic particles and a binder. The mass ratio of the inorganic particles in the surface layer may be 90 mass% or more. In step B, the first separator and the second separator may be wound around a core with the base layer of the first separator facing the base layer of the second separator.
[0009] In step B, the first separator and the second separator may be pressed with a jig having a plurality of protrusions formed on its surface. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a vertical sectional plan view of the battery 2. FIG. [Diagram 2] FIG. 2 is a schematic diagram of the wound electrode body 20. As shown in FIG. [Diagram 3] FIG. 3 is a schematic diagram of the winding machine 100. [Figure 4] FIG. 4 is a schematic diagram of the winding machine 100. [Diagram 5] FIG. 5 is a schematic diagram of the winding machine 100. [Figure 6] FIG. 6 is a schematic diagram of the winding machine 100. [Figure 7]FIG. 7 is a cross-sectional view that illustrates a schematic view of the winding core 140 disposed at the first position P1. [Figure 8] FIG. 8 is a schematic diagram of the winding core 140 and the separators 31 and 32. [Figure 9] FIG. 9 is a schematic diagram of the winding core 140 and the separators 31 and 32. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Hereinafter, an embodiment of the invention disclosed herein will be described. Of course, the embodiment described herein is not intended to limit the present invention in particular. The present invention is not limited to the embodiment described herein unless otherwise specified. Each drawing is drawn typically and does not necessarily reflect the actual product. In addition, the same reference numerals are appropriately assigned to members and parts that perform the same function, and duplicated explanations are omitted.
[0012] Fig. 1 is a vertical cross-sectional plan view of a battery 2. In Fig. 1, the wide surface on the front side of a battery case 10 is virtually removed, and the battery 2 is illustrated diagrammatically so that the inside of the battery case 10 can be seen. The battery 2 is one form of a battery manufactured by the manufacturing method disclosed herein, and a wound electrode body 20 is housed inside the battery case 10. The battery manufactured by the manufacturing method disclosed herein is not limited to the form shown in Fig. 1.
[0013] 《Battery 2》 The battery 2 shown in Fig. 1 is a horizontally elongated rectangular battery. As shown in Fig. 1, the battery 2 has a battery case 10, a wound electrode body 20, a positive electrode terminal 50, and a negative electrode terminal 60. The battery case 10 has an exterior body 11 and a sealing plate 12.
[0014] <Exterior body 11> The exterior body 11 is a bottomed rectangular case having a horizontally long rectangular storage space. The exterior body 11 mainly stores the wound electrode body 20. The exterior body 11 has a substantially rectangular bottom surface 11e, a pair of opposing wide surfaces 11a, 11b (not shown) along the long side of the bottom surface 11e, and a pair of opposing narrow surfaces 11c, 11d along the short side of the bottom surface 11e. An opening 11f for storing the wound electrode body 20 is formed on the surface opposite to the bottom surface 11e. A sealing plate 12 is attached to the opening 11f.
[0015] <Sealing plate 12> The sealing plate 12 is attached to the opening 11f of the battery case 10. The sealing plate 12 is made of a substantially rectangular plate material that can be attached to the opening 11f of the exterior body 11. The sealing plate 12 is a substantially rectangular plate material, and has an attachment hole for attaching the positive electrode terminal 50 formed on one side in the longitudinal direction, and attachment holes 12a and 12b for attaching the negative electrode terminal 60 formed on the opposite side.
[0016] A liquid injection hole 12c and a gas exhaust valve 12d are provided in the center of the sealing plate 12. The liquid injection hole 12c is a through hole provided for injecting a non-aqueous electrolyte into the battery case 10 after sealing. The liquid injection hole 12c is sealed by attaching a sealing member 12e after the non-aqueous electrolyte is injected. The gas exhaust valve 12d is a thin-walled portion designed to break (open) when a large amount of gas is generated inside the battery case 10, and to exhaust the gas.
[0017] The non-aqueous electrolyte can be any electrolyte used in conventional secondary batteries without any particular limitations. For example, the non-aqueous electrolyte is prepared by dissolving a supporting salt in a non-aqueous solvent. Examples of the non-aqueous solvent include carbonate-based solvents such as ethylene carbonate, dimethyl carbonate, and ethyl methyl carbonate. Examples of the supporting salt include fluorine-containing lithium salts such as LiPF6.
[0018] <Positive terminal 50, negative terminal 60> The positive electrode terminal 50 and the negative electrode terminal 60 are attached to the sealing plate 12. The wound electrode body 20 is housed in the exterior body 11 in a state where it is attached to the positive electrode terminal 50 and the negative electrode terminal 60. The positive electrode terminal 50 includes an external terminal 51, an axial member 52, an internal terminal 53, a current collecting member 54, a first insulator 71, a second insulator 72, and a gasket 73. The negative electrode terminal 60 includes an external terminal 61, an axial member 62, an internal terminal 63, a current collecting member 64, a first insulator 81, a second insulator 82, and a gasket 83. The first insulators 71, 81, the second insulators 72, 82, and the gaskets 73, 83 are each made of an insulating material. The first insulators 71, 81, and the second insulators 72, 82 are each made of a resin having a required rigidity. The gaskets 73 and 83 are members that are attached to the mounting holes 12a and 12b of the sealing plate 12, and have a required flexibility.
[0019] The shaft members 52, 62 of the positive electrode terminal 50 and the negative electrode terminal 60 are attached to the mounting holes 12a, 12b of the sealing plate 12 with gaskets 73, 83 interposed therebetween. The external terminals 51, 61 are attached to the outside of the sealing plate 12 with first insulators 71, 81 interposed therebetween. The external terminals 51, 61 have mounting holes and are attached to the outer axial ends of the shaft members 52, 62. The internal terminals 53, 63 are attached to the inside of the sealing plate 12 with second insulators 72, 82 interposed therebetween. The internal terminals 53, 63 have mounting holes and are attached to the inner axial ends of the shaft members 52, 62. The inner axial ends of the shaft members 52, 62 are crimped around the mounting holes of the internal terminals 53, 63. The current collecting members 54, 64 are attached to one end of the internal terminals 53, 63.
[0020] In this manner, the positive electrode terminal 50 and the negative electrode terminal 60 are attached to the sealing plate 12 in a state in which they are electrically insulated through the first insulators 71, 81, the second insulators 72, 82, and the gaskets 73, 83, and in a state in which airtightness is ensured. In addition, an electrical conduction path is formed by the external terminals 51, 61, the shaft members 52, 62, the internal terminals 53, 63, and the current collecting members 54, 64. The wound electrode body 20 is attached to the current collecting members 54, 64. The wound electrode body 20 is housed in the exterior body 11 in a state in which it is attached to the sealing plate 12 in this manner. A plurality of wound electrode bodies 20 may be attached to one sealing plate 12, and a plurality of wound electrode bodies 20 may be housed in one battery case 10.
[0021] <Wound electrode body 20> Fig. 2 is a schematic diagram of the wound electrode body 20. In Fig. 2, the wound electrode body 20 is illustrated in a state where one end is unfolded. For example, as shown in Fig. 2, the wound electrode body 20 is formed by stacking a long strip-shaped positive electrode plate 21, a first separator 31, a negative electrode plate 22, and a second separator 32 in order with their longitudinal directions aligned, and winding them around a winding axis WL set in the width direction.
[0022] The positive electrode plate 21 includes a positive electrode core 21a, a positive electrode active material layer 21b, a protective layer 21c, and a tab 21d. The positive electrode core 21a is a base material of the positive electrode plate 21. The positive electrode core 21a is formed of a predetermined metal foil (for example, aluminum foil). The positive electrode active material layer 21b is formed on the positive electrode core 21a with a constant width at one end in the width direction. A protective layer 21c is formed on both sides of the positive electrode plate 21 except for the part of the positive electrode core 21a where the positive electrode active material layer 21b is formed. Furthermore, a tab 21d protruding in the width direction is formed on the side of the positive electrode core 21a where the protective layer 21c is formed. The tab 21d protrudes partially with a predetermined width on the side where the protective layer 21c is formed, exposing the positive electrode core 21a.
[0023] The positive electrode active material layer 21b is a layer containing a positive electrode active material. In a lithium ion secondary battery, the positive electrode active material is, for example, a material that can release lithium ions during charging and absorb lithium ions during discharging, such as a lithium transition metal composite material. In general, various positive electrode active materials have been proposed other than lithium transition metal composite materials, and are not particularly limited. For example, a lithium transition metal composite oxide is preferable as the positive electrode active material. Among the lithium transition metal composite oxides, a lithium transition metal composite oxide containing at least one of the group consisting of nickel (Ni), cobalt (Co) and manganese (Mn) as a transition metal is particularly preferable. Specific examples include lithium nickel cobalt manganese composite oxide (NCM), lithium nickel composite oxide, lithium cobalt composite oxide, lithium manganese composite oxide, lithium nickel manganese composite oxide, lithium nickel cobalt aluminum composite oxide (NCA), and lithium iron nickel manganese composite oxide. Moreover, a suitable example of the lithium transition metal composite oxide that does not contain Ni, Co, or Mn is lithium iron phosphate composite oxide (LFP).
[0024] In this specification, the term "lithium nickel cobalt manganese composite oxide" refers to oxides containing additive elements in addition to the main constituent elements (Li, Ni, Co, Mn, O). Examples of such additive elements include transition metal elements and typical metal elements such as Mg, Ca, Al, Ti, V, Cr, Si, Y, Zr, Nb, Mo, Hf, Ta, W, Na, Fe, Zn, and Sn. The additive elements may also be semimetal elements such as B, C, Si, and P, or nonmetal elements such as S, F, Cl, Br, and I. The positive electrode active material layer 21b may contain additives other than the positive electrode active material. Examples of such additives include conductive materials and binders. Specific examples of conductive materials include carbon materials such as acetylene black (AB). Specific examples of binders include resin binders such as polyvinylidene fluoride (PVdF). When the entire solid content of the positive electrode active material layer 21b is taken as 100 mass %, the content of the positive electrode active material is generally 80 mass % or more, and typically 90 mass % or more.
[0025] The protective layer 21c is a layer configured to have low electrical conductivity. Such a protective layer 22c is provided in an area adjacent to the edge of the positive electrode active material layer 21b. When either of the separators 31, 32 is damaged, the positive electrode core 21a and the negative electrode active material layer 22b come into direct contact with each other, and an internal short circuit can be prevented. For example, a layer containing insulating ceramic particles is preferably formed in the protective layer 22c. Examples of such ceramic particles include inorganic oxides such as alumina (Al2O3), magnesia (MgO), silica (SiO2), and titania (TiO2), nitrides such as aluminum nitride and silicon nitride, metal hydroxides such as calcium hydroxide, magnesium hydroxide, and aluminum hydroxide, clay minerals such as mica, talc, boehmite, zeolite, apatite, and kaolin, and glass fibers. Considering insulation and heat resistance, alumina, boehmite, aluminum hydroxide, silica, and titania are preferable among the above. The protective layer 22c may contain a binder for fixing the ceramic particles to the surface of the positive electrode core 21a. Examples of such binders include resin binders such as polyvinylidene fluoride (PVdF). A small amount of conductive material (e.g., carbon material such as carbon black) may be added to the protective layer 22c. The conductive material may be added to impart slight conductivity. The amount of conductive material added may be adjusted to an amount that exhibits a required conductivity. The protective layer is not an essential component of the positive electrode plate. In other words, in the secondary battery disclosed herein, a positive electrode plate without a protective layer may also be used.
[0026] The negative electrode plate 22 includes a negative electrode core 22a, a negative electrode active material layer 22b, and a tab 22d. The negative electrode core 22a is a base material of the negative electrode plate 22. The negative electrode core 22a is formed of a predetermined metal foil (e.g., copper foil). The negative electrode active material layer 22b is formed on both sides of the negative electrode core 22a across approximately the entire width. The negative electrode core 22a is formed with a tab 22d that protrudes from one side in the width direction. The tab 22d protrudes partially by a predetermined width from one side in the width direction of the negative electrode core 22a.
[0027] The negative electrode active material layer 22b is a layer containing a negative electrode active material. The negative electrode active material is not particularly limited as long as it can reversibly absorb and release charge carriers in relation to the above-mentioned positive electrode active material. Examples of such negative electrode active materials include carbon materials and silicon-based materials. Examples of carbon materials that can be used include graphite, hard carbon, soft carbon, and amorphous carbon. Also, amorphous carbon-coated graphite, in which the surface of graphite is coated with amorphous carbon, can also be used. Examples of silicon-based materials include silicon and silicon oxide (silica). Also, the silicon-based material may contain other metal elements (e.g., alkaline earth metals) or their oxides. Also, the negative electrode active material layer 22b may contain additives other than the negative electrode active material. Examples of such additives include binders and thickeners. Specific examples of binders include rubber-based binders such as styrene butadiene rubber (SBR). Also, specific examples of thickeners include carboxymethyl cellulose (CMC). The content of the negative electrode active material is generally 30% by mass or more, typically 50% by mass or more, when the entire solid content of the negative electrode active material layer 22b is taken as 100% by mass. The negative electrode active material may account for 80% by mass or more, or may account for 90% by mass or more of the negative electrode active material layer 22b.
[0028] For example, the separators 31 and 32 are made of porous resin sheets through which electrolytes having required heat resistance can pass. Various separators 31 and 32 have been proposed, and are not particularly limited. A suitable example of the separators 31 and 32 is a separator including a porous base material layer made of a resin such as polyolefin resin (e.g., polyethylene (PE), polypropylene (PP)). A coating layer may be formed on one or both sides of the porous base material layer as appropriate. The coating layer may include a porous surface layer or an adhesive layer containing an insulating inorganic material. Since the porous surface layer has excellent heat resistance, it can suppress the shrinkage and damage of the separators 31 and 32 due to temperature rise. Examples of inorganic materials for the porous surface layer include ceramic particles such as alumina, boehmite, aluminum hydroxide, and titania. The porous surface layer also includes a binder that binds the ceramic particles. Resin binders such as polyvinylidene fluoride (PVdF) and acrylic resins can be used as the binder. The two separators 31 and 32 used in this embodiment may be made of the same material or different materials.
[0029] As shown in Fig. 2, the negative electrode active material layer 22b of the negative electrode plate 22 may cover the positive electrode active material layer 21b of the positive electrode plate 21 with the separators 31 and 32 interposed therebetween. The separators 31 and 32 may further cover the positive electrode active material layer 21b of the positive electrode plate 21 and the negative electrode active material layer 22b of the negative electrode plate 22. Although not shown, the lengths of the positive electrode plate 21, the negative electrode plate 22, and the separators 31 and 32 may be such that the separators 31 and 32>the negative electrode plate 22>the positive electrode plate 21. The width La of the positive electrode active material layer 21b, the width Ln of the negative electrode active material layer 22b, and the width Ls of the separators 31 and 32 are such that Ls>Ln>La. In the region where the positive electrode plate 21 and the negative electrode plate 22 overlap, the region where the positive electrode active material layer 21b is formed is covered with the negative electrode active material layer 22b. In addition, in the region where the negative electrode active material layer 22b overlaps with the positive electrode plate 21, a protective layer 22c is formed in a portion where the positive electrode active material layer 21b does not face.
[0030] As shown in FIG. 2, the tab 21d of the positive electrode plate 21 protrudes from one side of the separators 31 and 32 in the width direction. The positive electrode plate 21 is provided with a plurality of tabs 21d at a predetermined pitch in the longitudinal direction. The tab 22d of the negative electrode plate 22 protrudes from the separators 31 and 32 on the opposite side in the width direction. The negative electrode plate 22 is provided with a plurality of tabs 22d at a predetermined pitch in the longitudinal direction. The plurality of tabs 21d of the positive electrode plate 21 and the plurality of tabs 22d of the negative electrode plate 22 are provided at a predetermined pitch so as to be at approximately the same position after being wound around the wound electrode body 20. The tab 21d of the positive electrode plate 21 and the tab 22d of the negative electrode plate 22 may be formed at the stage when the positive electrode plate 21 and the negative electrode plate 22 are prepared, respectively. The tab 21d of the positive electrode plate 21 and the tab 22d of the negative electrode plate 22 may be cut out after the wound electrode body 20 is wound.
[0031] As shown in FIG. 1 and FIG. 2, the wound electrode body 20 is housed in the exterior body 11 through the opening 11f where the sealing plate 12 is attached. For this reason, the wound electrode body 20 has a flat shape to match the shape of the opening 11f. When the wound electrode body 20 is produced, it may be wound around a flat shaft. When the wound electrode body 20 is produced, it may be pressed flat after being wound around a cylindrical shaft. The wound electrode body 20 and the exterior body 11 are electrically insulated by a resin insulating sheet 90 arranged between the wound electrode body 20 and the exterior body 11. The insulating sheet 90 is a resin sheet and is folded into a box shape so as to wrap the wound electrode body 20. Note that FIG. 1 illustrates the insulating sheet 90 with the wide surface on the front side also removed.
[0032] "Winding machine 100" Next, the winding machine 100 will be described. Figures 3 to 6 are schematic diagrams of the winding machine 100. The winding machine 100 is an example of a winding machine that embodies the battery manufacturing method disclosed herein. Figures 3 to 6 each show a turret 120 portion of the winding machine 100 as viewed from a distance from the rotation axis C1 of the turret 120.
[0033] Fig. 3 shows a standby state when the winding machine 100 starts to newly wind the positive electrode plate 21 and the negative electrode plate 22. Fig. 4 shows a state in which the positive electrode plate 21 and the negative electrode plate 22 are newly wound on the winding machine 100. Fig. 5 shows a state in which the winding core 140 around which the positive electrode plate 21 and the negative electrode plate 22 are wound moves from the first position P1 to the second position P2. Fig. 6 shows a state in which the winding core 140 around which the positive electrode plate 21 and the negative electrode plate 22 are wound moves to the second position P2, the new winding core moves to the first position P1, and the separators 31 and 32 are cut off.
[0034] 3, the winding machine 100 is a device for winding the positive electrode plate 21, the negative electrode plate 22, and the separators 31, 32. The turret 120 is provided with a plurality of winding cores 140(1)-(3) around which the positive electrode plate 21, the negative electrode plate 22, and the separators 31, 32 are wound.
[0035] As shown in FIG. 3, the winding machine 100 includes movement paths k1-k4, a turret 120, a plurality of winding cores 140(1)-(3), a cutter 151, a press roller 152, a plurality of fixed rollers 161-163, a plurality of movable rollers 171-174, a first chuck 181, a second chuck 182, an index unit 185 provided on the turret 120, index rollers 186-188 provided on the index unit 185, a winding stop device 190, and a control device 200. The positive electrode plate 21, the negative electrode plate 22, and the separators 31 and 32 are prepared in a state of being wound on reels (not shown) or the like. Each component of the winding machine 100 has a required actuator as appropriate. The control device 200 is configured to control each component of the winding machine 100 so that a required operation is performed at a specified timing according to a preset program. The control device 200 may be embodied by a computer, such as a microcontroller, for example.
[0036] <Travel route k1~k4> The movement path k1 is a path along which the positive electrode plate 21 is fed from the reel toward the turret 120. The movement path k2 is a path along which the negative electrode plate 22 is fed from the reel toward the turret 120. The movement path k3 is a path along which the first separator 31 is fed from the reel toward the turret 120. The movement path k4 is a path along which the second separator 32 is fed from the reel toward the turret 120. The positive electrode plate 21, the negative electrode plate 22, the first separator 31, and the second separator 32 are each strip-shaped and fed along predetermined movement paths k1 to k4. The movement path k1 of the positive electrode plate 21 merges with the movement path k3 of the first separator 31 just before reaching the winding core 140 arranged at the first position P1. The movement path k1 of the negative electrode plate 22 merges with the movement path k4 of the second separator 32 just before reaching the winding core 140 disposed at the first position P1. On the movement paths k1 to k4, a dancer roll mechanism for removing slack in the positive electrode plate 21, negative electrode plate 22, first separator 31, and second separator 32 being fed, a tensioner for adjusting tension, and the like are appropriately disposed.
[0037] <Turret 120> The turret 120 is a rotating disk with a rotation axis set at the center C1. A plurality of (three in this embodiment) winding cores 140 are arranged on the turret 120. Each of the plurality of winding cores 140 is a substantially cylindrical shaft that can rotate independently. In this embodiment, the shafts of the plurality of winding cores 140 are arranged to be parallel to the central axis of the turret 120. The turret 120 is provided with three winding cores 140: a first winding core 140(1), a second winding core 140(2), and a third winding core 140(3). The first winding core 140(1), the second winding core 140(2), and the third winding core 140(3) are arranged at equal intervals in the circumferential direction around the central axis of the turret 120. The first winding core to the third winding core 140(1) to (3) are winding cores having the same configuration. Although not shown, the turret 120 is provided with a required actuator (for example, a servo motor) and rotates at an appropriate angle at an appropriate timing.
[0038] A first position P1, a second position P2, and a third position P3 are set in advance around the axis of the center C1 of the turret 120. In FIG. 3, the first winding core 140(1) is disposed at the first position P1, the third winding core 140(3) is disposed at the second position P2, and the second winding core 140(2) is disposed at the third position P3. The positions of the first winding core to the third winding core 140(1)-(3) are not fixed to the positions shown in FIG. 3. In this embodiment, the turret 120 rotates counterclockwise. The first winding core to the third winding core 140(1)-(3) also rotate counterclockwise. The first winding core to the third winding core 140(1)-(3) move in order from the first position P1 to the second position P2 to the third position P3 by the rotation of the turret 120. Although not shown in the figures, the first to third winding cores 140(1)-(3) are equipped with the necessary actuators (e.g., servo motors) and rotate at appropriate timing and speeds. Here, the first to third winding cores 140(1)-(3) are referred to as winding cores 140 when no particular distinction is made. Furthermore, when a distinction is made between the first to third winding cores 140(1)-(3), they are appropriately distinguished as winding core 140(1), winding core 140(2), and winding core 140(3).
[0039] <Core 140> FIG. 7 is a cross-sectional view showing the winding core 140 arranged at the first position P1. The winding core 140 is a substantially cylindrical member. FIG. 7 shows a view of the winding core 140 from the axial direction, and shows a state in which the first separator 31 and the second separator 32 are wound around the winding core 140 arranged at the first position P1 as shown in FIG. 3. The winding core 140 has a function of holding the separators 31 and 32 wound around the side circumferential surface as shown in FIG. 4. In this embodiment, the winding core 140 has a suction hole 141, a suction path 142, and a groove 143. The suction hole 141 is a hole for adsorbing the separators 31 and 32 wound around the side circumferential surface. The suction path 142 is a flow path formed inside the winding core 140 and connected to the suction hole 141. The suction path 142 is a flow path for forming a negative pressure in the suction hole 141. The suction path 142 may be configured to be connected to, for example, an externally installed vacuum line (not shown) as appropriate to generate negative pressure. The groove 143 is formed as a receiving portion onto which the blade of the cutter 151 is lowered when the separators 31, 32 are cut. In this embodiment, the groove 143 is formed on the outer circumferential surface of the winding core 140 along the axial direction of the winding core 140. Note that, in this embodiment, the winding core 140 has a substantially cylindrical shape, but when winding into a flat shape, a flat winding core may be used. In addition, the winding core may be a winding core divided along the radial direction, and the diameter of the winding core may be variable.
[0040] Cutter 151 The cutter 151 is a cutter that cuts the separators 31, 32. It is configured so that the blade 151a is pressed against the separators 31, 32 held by the winding core 140 arranged at the first position P1. In this embodiment, the cutter 151 is pushed out along a guide to a determined position so that the blade is pressed against the separators 31, 32 held by the winding core 140, and is retracted from the position. Although not shown, the cutter 151 is operated so as to operate at an appropriate timing by an actuator (for example, a cylinder mechanism). The blade 151a may be, for example, a serrated blade (a saw-like blade).
[0041] <Pressure roller 152> The pressing roller 152 is a roller that presses the separators 31, 32 against the winding core 140 arranged at the first position P1. The pressing roller 152 presses the separators 31, 32 against the winding core 140 arranged at the first position P1 while winding them up. The pressing roller 152 functions as a pressing tool that presses the separators 31, 32 against the winding core 140 arranged at the first position P1. In this embodiment, as shown in FIG. 7, the pressing roller 152 has a plurality of protrusions 152a formed on its outer circumferential surface. In this way, the roller 152 with the protrusions 152a presses the two separators 31, 32 against the winding core 140, and the force is locally concentrated by the protrusions 152a, so that the separators 31, 32 are strongly pressed against each other. For this reason, the separators 31, 32 are more suitably pressed against each other. The pressing roller 152 may be, for example, substantially cylindrical, and may have a knurled circumferential surface. The pressure roller 152 may be configured to press the separators 31, 32 against the winding core 140 arranged at the first position P1 with an appropriate pressure by a mechanism having a spring or the like built therein. Although not shown, the pressure roller 152 is moved by a guide and an actuator between a position where it is pressed against the separators 31, 32 wound around the winding core 140 arranged at the first position P1 (see FIG. 3) and a position where it is separated from the winding core 140 (see FIG. 5). The pressure roller 152 may be provided as a single cylindrical roller in the width direction of the winding core 140, or may be composed of multiple rollers arranged intermittently in the width direction of the winding core 140.
[0042] <Fixed roller 161, movable roller 171> The fixed roller 161 is provided at a position where the moving path k3 of the first separator 31 and the moving path k1 of the positive electrode plate 21 join together. The movable roller 171 is a roller that presses the first separator 31 against the fixed roller 161 to sandwich the first separator 31. The movable roller 171 moves in a predetermined direction by a guide and an actuator. The movement of the movable roller 171 is controlled by the control device 200. The movable roller 171 is configured to move to a position where the first separator 31 is pressed against the fixed roller 161 and a position where it is separated from the fixed roller 161. When the movable roller 171 sandwiches the first separator 31, it is preferable that the movable roller 171 is configured to sandwich the first separator 31 with a predetermined force by the action of a spring or the like. The first separator 31 is sandwiched between the fixed roller 161 and the movable roller 171 with an appropriate force, so that it is sent out toward the winding core 140 arranged at the first position P1 without slack.
[0043] <Fixed roller 162, movable roller 172> The fixed roller 162 is provided at a position where the moving path k4 of the second separator 32 and the moving path k2 of the negative electrode plate 22 join together. The movable roller 172 is a roller that presses the second separator 32 against the fixed roller 162 to sandwich the second separator 32. The movable roller 172 moves in a predetermined direction by a guide and an actuator. The movement of the movable roller 172 is controlled by the control device 200. The movable roller 172 is configured to move to a position where the second separator 32 is pressed against the fixed roller 162 and a position where it is separated from the fixed roller 162. When the movable roller 172 sandwiches the second separator 32, it is preferable that the movable roller 172 is configured to sandwich the second separator 32 with a predetermined force by the action of a spring or the like. The second separator 32 is fed toward the winding core 140 arranged at the first position P1 without slack by being sandwiched between the fixed roller 162 and the movable roller 172 with an appropriate force.
[0044] <Fixed roller 163> The fixed roller 163 is disposed at a predetermined position on the movement path k3 of the first separator 31, and is a roller for determining the movement path k3 of the first separator 31.
[0045] <First zipper 181> As shown in FIG. 3, the first chuck 181 is disposed before a pair of rollers 161, 171 that sandwich the first separator 31 in the moving path k1 along which the positive electrode plate 21 is sent out. The first chuck 181 is a member that grips the positive electrode plate 21. In this embodiment, the first chuck 181 includes a pair of gripping members. Although not shown, the first chuck 181 includes a cutter for cutting the positive electrode plate 21. Although not shown, the first chuck 181 operates at an appropriate timing by a guide and an actuator (for example, a cylinder mechanism). The operation of the first chuck 181 is configured to be controlled by the control device 200.
[0046] In the state shown in FIG. 3, the first separator 31 is held by the winding core 140 arranged at the first position P1 and extends along the movement path k3 while being sandwiched between the pair of rollers 161, 171. The first chuck 181 holds the positive electrode plate 21 just before the pair of rollers 161, 171. When the positive electrode plate 21 is wound around the winding core 140 arranged at the first position P1, as shown in FIG. 4, the first chuck 181 inserts the held positive electrode plate 21 between the pair of rollers 161, 171 and releases the positive electrode plate 21. As a result, the positive electrode plate 21 is pulled into the pair of rollers 161, 171 together with the first separator 31 and wound around the winding core 140 arranged at the first position P1. When the positive electrode plate 21 is fed out by a predetermined length, the winding around the winding core 140 stops. The positive electrode plate 21 is gripped by the first chuck 181 and cut between the first chuck 181 and the pair of rollers 161, 171. The first chuck 181 is configured to move appropriately between a predetermined position where the positive electrode plate 21 is gripped and a predetermined position where the positive electrode plate 21 is inserted between the pair of rollers 161, 171.
[0047] <Second zipper 182> As shown in FIG. 3, the second chuck 182 is disposed before the pair of rollers 162, 172 that sandwich the second separator 32 in the moving path k2 along which the negative electrode plate 22 is sent out. The second chuck 182 is a member that grips the negative electrode plate 22. In this embodiment, the second chuck 182 has a pair of gripping members. Although not shown, the second chuck 182 has a cutter for cutting the negative electrode plate 22. Although not shown, the second chuck 182 operates at an appropriate timing by a guide and an actuator (for example, a cylinder mechanism). The operation of the second chuck 182 is configured to be controlled by the control device 200.
[0048] In the state shown in FIG. 3, the second separator 32 is held by the winding core 140 arranged at the first position P1 and extends along the movement path k4 while being sandwiched between the pair of rollers 162, 172. The second chuck 182 holds the negative electrode plate 22 just before the pair of rollers 162, 172. When the negative electrode plate 22 is wound around the winding core 140 arranged at the first position P1, as shown in FIG. 4, the second chuck 182 inserts the held negative electrode plate 22 between the pair of rollers 162, 172 and releases the negative electrode plate 22. As a result, the negative electrode plate 22 is pulled into the pair of rollers 162, 172 together with the second separator 32 and wound around the winding core 140 arranged at the first position P1. As described above, when the positive electrode plate 21 is fed out by a predetermined length, the winding of the winding core 140 stops. In other words, when a predetermined length of the negative electrode plate 22 has been fed out, the winding of the winding core 140 stops. The negative electrode plate 22 is gripped by the second chuck 182 and cut between the second chuck 182 and the pair of rollers 162, 172. The second chuck 182 is configured to move appropriately between a predetermined position where the negative electrode plate 22 is gripped and a predetermined position where the negative electrode plate 22 is inserted between the pair of rollers 162, 172.
[0049] The positive electrode plate 21 and the negative electrode plate 22 may be inserted between a pair of rollers 161, 171 and between a pair of rollers 162, 172, for example, after the first separator 31 and the second separator 32 have been wound around the outer circumferential surface of the winding core 140 about once.
[0050] <Movable roller 173> The movable roller 173 is a roller for pressing the first separator 31 and the second separator 32 against the winding core 140 arranged at the first position P1 when the first separator 31 and the second separator 32 are cut, as shown in FIG. 6. The movable roller 173 moves in a predetermined direction by a guide and an actuator. The movement of the movable roller 173 is controlled by the control device 200. As shown in FIG. 6, the movable roller 173 is arranged at a position for pressing the first separator 31 and the second separator 32 against the winding core 140 arranged at the first position P1 when the first separator 31 and the second separator 32 are cut. At other times, the movable roller 173 moves to a position away from the winding core 140 arranged at the first position P1, as shown in FIG. 3. It is preferable that movable roller 173 is configured to sandwich first separator 31 with a predetermined force by the action of a spring or the like when pressing first separator 31 and second separator 32 against core 140.
[0051] As shown in FIG. 6, the cutter 151 is pressed against the winding core 140 arranged at the first position P1, thereby cutting the first separator 31 and the second separator 32. In this embodiment, as shown in FIG. 7, a groove 143 is provided on the outer peripheral surface of the winding core 140. When the cutter 151 is pressed against the winding core 140, the groove 143 provided on the outer peripheral surface of the winding core 140 is directed toward the position where the cutter 151 is pressed. With the groove 143 directed toward the cutter 151, the first separator 31 and the second separator 32 are pressed against the winding core 140 by the movable roller 173. As a result, the first separator 31 and the second separator 32 are adsorbed to the winding core 140. Furthermore, in this state, the cutter 151 is pressed against the first separator 31 and the second separator 32 held by the winding core 140. This cuts the first separator 31 and the second separator 32. In addition, because the blade of the cutter 151 enters the groove 143 of the winding core 140, the first separator 31 and the second separator 32 are cut more reliably and neatly, the winding core 140 is less likely to be scratched, and foreign matter is less likely to be generated.
[0052] <Movable roller 174> 6, the movable roller 174 is a roller for applying tension to the first separator 31 and the second separator 32 when the first separator 31 and the second separator 32 are cut off. The movable roller 174 is moved in a predetermined direction by a guide and an actuator. The movement of the movable roller 174 is controlled by the control device 200.
[0053] For example, as shown in FIG. 4, the positive electrode plate 21, the first separator 31, the negative electrode plate 22, and the second separator 32 are wound up in order by the winding core 140(1) arranged at the first position P1, while being stacked on top of each other. The winding core 140(1) on which the positive electrode plate 21, the first separator 31, the negative electrode plate 22, and the second separator 32 have been wound moves from the first position P1 to the second position P2, as shown in FIG. 5. At that time, another winding core 140(2) moves to the first position P1. Then, as shown in FIG. 6, the first separator 31 and the second separator 32 are attracted to the winding core 140(2) newly arranged at the first position P1, and the first separator 31 and the second separator 32 are held on the outer peripheral surface of the winding core 140(2). At this time, the first separator 31 and the second separator 32 wound around the winding core 140(1) arranged at the second position P2 are held in a connected state on the outer peripheral surface of the winding core 140(2) arranged at the first position P1.
[0054] The movable roller 174 is pushed out toward the first separator 31 and the second separator 32 at an appropriate timing when the winding core 140(1) moves from the first position P1 to the second position P2, and is pressed against the first separator 31 and the second separator 32 as shown in Fig. 6. The movable roller 174 sends out the first separator 31 and the second separator 32 without slack when the winding core 140(1) moves from the first position P1 to the second position P2. The movable roller 174 is retracted to a position away from the turret 120 except for this timing, as shown in Figs. 3 to 5.
[0055] <Index Unit 185> The index unit 185 is provided at the center of the turret 120. As described above, the three winding cores 140(1)-(3) are evenly arranged in the circumferential direction on the turret 120. The index unit 185 has a substantially equilateral triangular base that rotates together with the turret 120. Index rollers 186-188 are arranged at the vertices of the base, and the index rollers 186-188 are respectively arranged between the three winding cores 140(1)-(3).
[0056] When the winding core 140(1) on which the positive electrode plate 21, the first separator 31, the negative electrode plate 22, and the second separator 32 are wound moves from the first position P1 to the second position P2, the index roller 186 of the index rollers 186-188 arranged from the first position P1 to the second position P2 presses against the first separator 31 and the second separator 32 from the inner diameter side as shown in FIG. 6. The index roller 186 and the movable roller 174 feed the first separator 31 and the second separator 32 without slack between the first position P1 and the second position P2. At the timing shown in FIG. 6, the index roller 186 presses against the first separator 31 and the second separator 32 from the inner diameter side, but the index unit 185 rotates together with the rotation of the turret 120. For this reason, the index rollers 186 to 188 of the index unit 185 function in sequence as rollers that press against the first separator 31 and the second separator 32 from the inner diameter side when the winding core 140, on which the positive electrode plate 21, the first separator 31, the negative electrode plate 22, and the second separator 32 are wound, moves from the first position P1 to the second position P2.
[0057] <Winding device 190> For example, as shown in FIG. 6, the winding core 140(1) on which the positive electrode plate 21, the first separator 31, the negative electrode plate 22, and the second separator 32 have been wound moves to a second position P2 away from the first position P1. Then, after the separators 31 and 32 are cut, the cut separators 31 and 32 are wound up to the cut ends. The winding stop device 190 is disposed at the second position P2. The winding stop device 190 includes a pressure roller 191 and a tape application device 192. The pressure roller 191 is pressed against the outermost second separator 32 wound around the winding core 140(1) when the winding core 140 moved to the second position P2 winds up the cut positive electrode plate 21, the first separator 31, the negative electrode plate 22, and the second separator 32 to the cut ends. As a result, the cut positive electrode plate 21, first separator 31, negative electrode plate 22, and second separator 32 are each wound up without loosening. The tape application device 192 is a device that applies tape to fasten the cut end of the outermost second separator 32 or the first separator 31. This winding stop process may be performed, for example, in parallel with the process of winding the first separator 31, positive electrode plate 21, second separator 32, and negative electrode plate 22 around the winding core 140(2) newly arranged at the first position P1.
[0058] Further, in this embodiment, for example, as shown in FIG. 6, the winding machine 100 performs the winding stop process, and then the positive electrode plate 21, the first separator 31, the negative electrode plate 22, and the second separator 32 are newly wound around the winding core 140(2) arranged at the first position P1, and then the turret 120 rotates. The winding core 140(1) on which the winding stop process has been performed moves to the third position P3, the winding core 140(2) moves to the second position P2, and another winding core 140(3) is arranged at the first position P1. At this time, the first separator 31 and the second separator 32 wound around the winding core 140(2) arranged at the second position P2 are held in a connected state on the outer circumferential surface of the winding core 140(3) arranged at the first position P1. Then, after the separators 31 and 32 are cut, the winding stop process of the winding core 140(2) is performed at the second position P2. At the first position P1, the positive electrode plate 21, the first separator 31, the negative electrode plate 22, and the second separator 32 are newly wound around the winding core 140(3). At the third position P3, the wound body 20a is removed from the winding core 140(1) (see FIG. 3). After being removed, the wound body 20a is pressed flat and can be handled as the wound electrode body 20. In this manner, the winding cores 140(1)-(3) provided on the turret 120 move sequentially from the first position P1 to the third position P3. Then, the positive electrode plate 21, the first separator 31, the negative electrode plate 22, and the second separator 32 are continuously wound around the winding cores 140(1)-(3) in order.
[0059] Here, the winding machine 100 embodies the following steps A and B in the method for manufacturing a battery 2 including a wound electrode body 20. Step A: In step A, the first separator 31 and the second separator 32, which have been sent out along predetermined moving paths k1 to k4, are attracted to the winding core 140(1) arranged at the first position P1 in a stacked state (see FIG. 3). Step B: In step B, the first separator 31 and the second separator 32 that have been stacked and attracted in step A are wound around the winding core 140(1) (see FIG. 3). Here, the first separator 31 and the second separator 32 each have a base material layer 33 and a surface layer 34 formed on at least one surface of the base material layer 33. According to the manufacturing method disclosed herein, even when the first separator 31 and the second separator 32 each have the base material layer 33 and the surface layer 34, it is possible to effectively suppress the winding misalignment of each separator with respect to the winding core 140 by a simple method, and it becomes possible to produce a continuous wound electrode body 20. This improves productivity. The surface layer 34 may be provided on only one surface or both surfaces of the base layer 33. Below, a case where the surface layer 34 is formed on both surfaces of the base layer 33 and a case where the surface layer 34 is formed on only one surface of the base layer 33 will be described.
[0060] First, a case where the surface layers 34 are formed on both surfaces of the base layer 33 will be described. FIG. 8 is a schematic diagram of the winding machine 100 (more specifically, the winding core 140) and the separators 31 and 32. As shown in FIG. 8, the separators 31 and 32 each have a surface layer 34a formed on both sides of the base material layer 33. The base material layer 33 is typically made of a resin porous sheet (film). Examples of the porous sheet (film) include a polyolefin resin such as polyethylene (PE) or polypropylene (PP), a polyvinyl chloride resin, a polyvinyl acetate resin, a polyimide resin, a polyamide resin, and a cellulose resin. Among them, a porous sheet made of polyethylene (PE) is preferable because its shutdown temperature is sufficiently lower than the heat resistance temperature of the battery and it has an appropriate shutdown function. The base material layer 33 may be a single-layer structure made of a single material, or a laminate structure in which two or more types of resin porous sheets having different materials and properties (for example, average thickness, porosity, etc.) are laminated (for example, a structure in which PP is laminated on both sides of PE).
[0061] The average thickness of the base layer 33 is not particularly limited, but is usually 5 μm or more, typically 8 μm or more, for example 10 μm or more. On the other hand, the thickness of the base layer 33 is usually 40 μm or less, for example 30 μm or less, for example 25 μm or less. Although not particularly limited, the porosity of the base layer 33 is about 30 to 60%.
[0062] When the surface layers 34 are formed on both sides of the base layer 33, the surface layer 34a is a layer with a three-dimensional mesh structure containing PVdF. The surface layer 34a typically has a structure (three-dimensional mesh structure) formed by randomly laminating a plurality of fibrous PVdF aggregates so as to have a large number of pores (voids). When the surface layers 34 having such a three-dimensional mesh structure contact each other, it is possible to suitably suppress the occurrence of static electricity and the displacement of the separators 31 and 32. In addition, it is possible to suppress the displacement of each separator with respect to the winding core 140 due to such static electricity. This suppresses the occurrence of defects at the start of winding the separator, and allows the wound electrode body 20 to be continuously manufactured. That is, according to the above configuration, even when the separator has the base layer 33 and the surface layers 34 on both sides of the base layer 33, it is possible to effectively suppress the displacement of the separators 31 and 32 with respect to the winding core 140 by a simple method, thereby improving productivity.
[0063] The surface layer 34a has many pores formed by the PVdF constituting the surface layer 34a. The porosity of the surface layer 34a is preferably higher than that of the base layer 33, and is typically 40% or more, for example, about 50 to 70%. The average thickness of the surface layer 34a is not particularly limited, but may be, for example, 0.1 μm to 5 μm, or 0.5 μm to 3 μm. The surface layer 34a having such an average thickness and porosity is easily sucked into the suction holes 141, and the winding core 140 can favorably adsorb the separators 31 and 32.
[0064] The surface layer 34a contains at least PVdF as a resin component constituting the three-dimensional network structure. More preferably, the surface layer 34a contains 10% by mass or more of PVdF when the surface layer 34a is taken as 100% by mass. According to the knowledge of the present inventors, the surface layer 34a can function as an adhesive layer having appropriate adhesiveness by containing 10% by mass or more of PVdF. This more suitably suppresses the winding deviation of the separators 31 and 32 with respect to the winding core 140. From this viewpoint, the mass ratio of PVdF contained in the surface layer 34a is preferably 10% by mass or more, more preferably 15% by mass or more, and even more preferably 20% by mass or more when the surface layer 34a is taken as 100% by mass. The upper limit of the mass ratio of PVdF contained in the surface layer 34a is not particularly limited, but may be, for example, 50% by mass or less, 45% by mass or less, or 40% by mass or less. By setting the PVdF content in the surface layer 34a within the above range, a three-dimensional mesh structure with uniform properties (e.g., pore distribution and average thickness) can be formed. This makes it easier for static electricity to be generated in the separators 31 and 32, and prevents the separators 31 and 32 from being misaligned with respect to the winding core 140.
[0065] The surface layer 34a may contain one or more other resin components in addition to the PVdF, as long as the effect of the present invention is not significantly impaired. Such other resin components are not particularly limited, but are preferably resins that do not dissolve in a non-aqueous electrolyte and do not inhibit the insertion and removal of charge carriers (e.g., lithium ions). Examples of other resin components contained in the surface layer 34a include fluorine-based resins such as polytetrafluoroethylene (PTFE); acrylic resins such as polymethylmethacrylate (PMMA), polyacrylonitrile (PAN), and polyvinyl alcohol (PVA); polyester resins such as polyethylene terephthalate; polyamide resins; and polyimide resins. When the surface layer 34a contains other resin components other than PVdF, the ratio of the other resin components is, for example, preferably 45 mass % or less of the total resin components contained in the surface layer 34a, and more preferably 30 mass % or less.
[0066] In order to improve the strength of the surface layer 34a, the surface layer 34a preferably contains one or more types of inorganic particles in addition to the PVdF. The inorganic particles may be made of any of the inorganic materials exemplified as those that may be contained in the separators 31 and 32. Among these, alumina, boehmite, silica, and titania are preferably used, which are stable in quality, inexpensive, and easily available. The inorganic particles are preferably arranged (i.e., dispersed) approximately uniformly in the three-dimensional mesh structure formed of the resin such as the PVdF described above. This makes it easier for the separators 31 and 32 to generate more suitable static electricity, eliminates winding misalignment with the winding core 140, and makes it easier for the winding core 140 to adsorb the separators 31 and 32.
[0067] The properties of the inorganic particles are not particularly limited. For example, the aspect ratio may be 1 or more and 5 or less (typically 2 or less, preferably 1.5 or less). Here, the aspect ratio refers to the ratio of the length of the longest side to the length of the shortest side of the inorganic particles. The average particle size of the inorganic particles is not particularly limited, but may be 0.01 μm or more (e.g., 0.05 μm or more, typically 0.1 μm or more) and 10 μm or less (e.g., 5 μm or less, typically 3 μm or less) in consideration of dispersibility, etc. In this specification, the term "average particle size" refers to a particle size (D50, also called the median diameter) corresponding to a cumulative frequency of 50 volume % from the fine particle side with a small particle size in a volume-based particle size distribution based on a general laser diffraction / light scattering method.
[0068] The mass ratio of the inorganic particles contained in the surface layer 34a is preferably 50% by mass or more, more preferably 60% by mass or more, and even more preferably 70% by mass or more, when the surface layer 34a is taken as 100% by mass. The upper limit of the mass ratio of the inorganic particles contained in the surface layer 34a is not particularly limited, but may be, for example, 90% by mass or less, 85% by mass or less, or 80% by mass or less.
[0069] The surface layer 34a may contain materials other than the above-mentioned resin components and inorganic particles, so long as the effects of the present invention are not significantly impaired. Examples of such materials include various additives such as oxidation stabilizers. In a preferred embodiment, when the surface layer 34a is taken as 100 mass%, the total mass ratio of the resin components (PVdF and other resin components) and inorganic particles contained in the surface layer 34a is approximately 90 mass% (e.g., 95 mass% or more). The surface layer 34a may be substantially composed of only the resin components and inorganic particles.
[0070] Next, a case where the surface layer 34 is formed on only one surface of the base layer 33 will be described. FIG. 9 is a schematic diagram of the winding machine 100 (more specifically, the winding core 140) and the separators 31 and 32. As shown in FIG. 9, the surface layer 34b is formed only on one side of the base material layer 33 of the first separator 31 and the second separator 32. In this case, the base material layer 33 of the first separator 31 and the base material layer 33 of the second separator 32 may be arranged in an opposing direction. According to the findings of the present inventors, the separators are more easily pressed together when the base material layers 33 are opposed to each other than when the surface layers 34b are opposed to each other, so that misalignment is less likely to occur, and the winding core 140 can suitably wind up the first separator 31 and the second separator 32. According to the above configuration, even when the separator has the base layer 33 and the surface layer 34 on only one side of the base layer 33, it is possible to suppress miswinding of the separators 31, 32 with respect to the winding core 140 by a simple method, and to produce a wound electrode body 20 with a stable shape. This makes it possible to improve productivity.
[0071] When the surface layer 34 is formed only on one side of the base layer 33, the surface layer 34b contains inorganic particles and a binder. The inorganic particles may be the same as those exemplified as those that may be contained in the surface layer 34a. When the surface layer 34 is formed on one side of the base layer 33, the surface layer 34b is preferably a porous insulating layer having heat resistance. For example, the surface layer 34b may have a porous structure that allows charge carriers to pass through and has heat resistance to a shutdown temperature (typically 80 to 140°C). Therefore, inorganic particles having such heat resistance and insulating properties are particularly preferable. Specifically, alumina, boehmite, and magnesia are preferably used. These have high melting points and can exhibit excellent heat resistance. The mass ratio of the inorganic particles contained in the surface layer 34b is preferably 90 mass% or more, and more preferably 95 mass% or more, when the surface layer 34b is 100 mass%. The upper limit of the mass proportion of the inorganic particles contained in the surface layer 34b is not particularly limited, but may be, for example, 99 mass % or less, or 98 mass % or less.
[0072] The binder contained in the surface layer 34b may be one of the resin components exemplified as those that may be contained in the surface layer 34a, or two or more of them may be mixed in an appropriate ratio and used. Among them, acrylic resins are preferred because they have suitable adhesive properties and are electrochemically stable, and therefore can exhibit high shape retention.
[0073] When the surface layer 34 is formed on only one surface of the base layer 33, the three-dimensional mesh structure as described above does not need to be formed in the surface layer 34b. That is, the binder only needs to be contained to an extent that it can bind the inorganic particles. From this viewpoint, the mass ratio of the inorganic particles contained in the surface layer 34b may be, for example, 1 mass% or more and 10 mass% or less, or 2 mass% or more and 8 mass% or less.
[0074] The average thickness of the surface layer 34b is not particularly limited, and may be, for example, 0.1 μm to 5 μm, or 0.5 μm to 3 μm. The surface layer 34b having such an average thickness is easily sucked into the suction holes 141, and the winding core 140 can favorably adsorb the separators 31 and 32.
[0075] The surface layer 34b may contain materials other than the inorganic particles and binder as long as the effects of the present invention are not significantly impaired. Examples of such materials include various additives such as oxidation stabilizers. In a preferred embodiment, when the surface layer 34b is taken as 100 mass%, the total mass ratio of the inorganic particles and binder contained in the surface layer 34b is approximately 90 mass% (e.g., 95 mass% or more). The surface layer 34b may be substantially composed of only the inorganic particles and binder.
[0076] Hereinafter, matters common to the first separator 31 and the second separator 32 in which the surface layer 34 is formed on both sides of the base material layer 33 and in which the surface layer 34 is formed on only one side will be described.
[0077] The separators 31, 32 are preferably configured to be pressed by a pressure roller 152 when being wound around the winding core 140 (see FIG. 7). In particular, the pressure roller 152 is preferably formed with a plurality of protrusions 152a on its outer circumferential surface. The surface layer 34 can exhibit adhesiveness by being pressed by the pressure roller 152. This further suppresses the winding misalignment of the separators 31, 32 with respect to the winding core 140.
[0078] The width Ls (see FIG. 2) of the first separator 31 and the second separator 32 is preferably 25 cm or more, and more preferably 30 cm or more. By making the width Ls of the first separator 31 and the second separator 32 relatively large, the adhesion area with the winding core 140 is increased, and the area that can be attracted by the suction holes 141 is also increased. This makes it possible to prevent the separators 31 and 32 from shifting from the winding core 140, and to produce a wound electrode body 20 with a more stable shape.
[0079] According to the above-described configuration, even when each of the first separator 31 and the second separator 32 has a base material layer 33 and a surface layer formed on at least one side of the base material layer 33, steps A and B are performed in a state in which misalignment of each separator with respect to the winding core 140 is effectively suppressed. That is, a wound electrode body 20 with a more stable shape (high quality) can be continuously manufactured by a simple method, and improved productivity is achieved.
[0080] In addition, after the first separator 31 and the second separator 32 are wound around the outer peripheral surface of the winding core 140 by about one revolution in process B, the positive electrode plate 21 and the negative electrode plate 22 are preferably inserted between a pair of rollers 161, 171 and a pair of rollers 162, 172, respectively, and wound (see Figure 6).
[0081] The battery manufacturing method disclosed herein and the winding machine 100 embodying the battery manufacturing method have been described above. The winding machine 100 is merely one form of a winding machine embodying the battery manufacturing method, and unless otherwise specified, the winding machine embodying the battery manufacturing method is not limited to the above-mentioned form. For example, in the above-mentioned embodiment, three winding cores 140 are provided on the turret 120 and are configured to move simultaneously by the rotation of the turret 120. The turret 120 may further be provided with multiple winding cores and configured to perform multiple processes in parallel at multiple positions. Also, unless otherwise specified, the multiple winding cores may not be provided on the turret and may be configured to move independently. Also, even if the steps of the battery manufacturing method described above are performed in parallel, the start timing may be simultaneous or may be appropriately shifted.
[0082] Furthermore, although a cylindrical pressing roller 152 has been exemplified as the pressing jig, the pressing jig may be a member that presses the first separator 31 and the second separator 32 against the winding core 140 disposed at the first position P1, and is not necessarily limited to the form of a roller.
[0083] The invention disclosed herein has been described in various ways. Unless otherwise specified, the embodiments described herein do not limit the present invention. Furthermore, the embodiments of the invention disclosed herein can be modified in various ways, and each component or each process described herein can be omitted or combined as appropriate, unless a particular problem occurs. [Explanation of symbols]
[0084] 10 Battery case 11 Exterior body 12 Sealing plate 20 Wound electrode body 20a Winding body 21 Positive electrode plate 22 Negative plate 31 Separator (first separator) 32 Separator (second separator) 33 Base material layer 34 Surface layer 34a Surface layer 34b Surface layer 50 Positive terminal 60 Negative terminal 100 Winding Machine 120 Turret 140 Roll core 141 Suction hole 142 Suction Path 143 Groove 151 Cutter 151a blade 152 Lola 152a protrusion 161~163 Fixed roller 171~174 Movable roller 181 First Chuck 182 Second Chuck 185 Index Unit 186~188 Index roller 190 Winding stop device 191 Lola 192 Tape application device 200 Control device k1~k4 Travel route P1 1st position P2 2nd position P3 3rd position WL Winding shaft
Claims
1. A method for manufacturing a battery including a wound electrode assembly in which a first separator, a negative electrode plate, a second separator, and a positive electrode plate are wound, comprising the steps of: A step A of adsorbing the first separator and the second separator in a stacked state onto a winding core; A step B of winding the first separator and the second separator around the winding core; having each of the first separator and the second separator has a porous base layer made of resin and a surface layer formed on at least one surface of the base layer; In the step B, the first separator and the second separator are pressed against the winding core by a jig having a plurality of protrusions formed on a surface thereof.
2. A method for manufacturing a battery including a wound electrode assembly in which a first separator, a negative electrode plate, a second separator, and a positive electrode plate are wound, comprising the steps of: A step A of adsorbing the first separator and the second separator in a stacked state onto a winding core; A step B of winding the first separator and the second separator around the winding core; having each of the first separator and the second separator has a porous base layer made of resin and a surface layer formed on at least one surface of the base layer; a surface layer of the first separator and a surface layer of the second separator are each an adhesive layer; In the step B, the first separator and the second separator are wound around the winding core at least one turn without supplying the negative electrode plate and the positive electrode plate to the winding core, and then the negative electrode plate and the positive electrode plate are supplied to the winding core to wind the first separator, the negative electrode plate, the second separator, and the positive electrode plate around the winding core; In the step B, the first separator and the second separator are pressed with a jig having a plurality of protrusions formed on a surface thereof. How batteries are manufactured.
3. A method for manufacturing a battery including a wound electrode assembly in which a first separator, a negative electrode plate, a second separator, and a positive electrode plate are wound, comprising the steps of: A step A of adsorbing the first separator and the second separator in a stacked state onto a winding core; A step B of winding the first separator and the second separator around the winding core; having each of the first separator and the second separator has a porous base layer made of resin and a surface layer formed on at least one surface of the base layer; a surface layer of the first separator and a surface layer of the second separator are each an adhesive layer; A plurality of suction holes are provided on an outer peripheral surface of the winding core and are arranged in a circumferential direction of the winding core, In the step A, the first separator is attracted to the winding core through the plurality of suction holes, In the step B, the first separator and the second separator are pressed with a jig having a plurality of protrusions formed on a surface thereof.
4. 4. The method for manufacturing a battery according to claim 3, wherein in the step B, the first separator and the second separator are wound around the winding core for at least one turn without supplying the negative electrode plate and the positive electrode plate to the winding core, and then the negative electrode plate and the positive electrode plate are supplied to the winding core to wind the first separator, the negative electrode plate, the second separator, and the positive electrode plate around the winding core.
5. A method for manufacturing a battery including a wound electrode assembly in which a first separator, a negative electrode plate, a second separator, and a positive electrode plate are wound, comprising the steps of: A step A of adsorbing the first separator and the second separator in a stacked state onto a winding core; A step B of winding the first separator and the second separator around the winding core; having each of the first separator and the second separator has a porous base layer made of resin and a surface layer formed on at least one surface of the base layer; The surface layer has a three-dimensional network structure containing polyvinylidene fluoride (PVdF), a surface layer of the first separator and a surface layer of the second separator are each an adhesive layer; In the step A, the first separator and the second separator are disposed on the winding core such that the surface layer of the first separator and the surface layer of the second separator are in contact with each other, In the step B, the first separator and the second separator are pressed with a jig having a plurality of protrusions formed on a surface thereof.
6. The first separator and the second separator each have a surface layer formed on both surfaces of the base material layer, The method for manufacturing a battery according to claim 1 , wherein the surface layer is a three-dimensional network structure containing polyvinylidene fluoride (PVdF).
7. 7. The method for producing a battery according to claim 5, wherein a mass percentage of PVdF in the surface layer of each of the first separator and the second separator is 10 mass% or more.
8. The method for manufacturing a battery according to claim 5 , wherein the surface layer of each of the first separator and the second separator contains inorganic particles.
9. The first separator and the second separator each have a surface layer formed on only one surface of the base material layer, the surface layer includes inorganic particles and a binder; The mass ratio of the inorganic particles in the surface layer is 90 mass% or more, In the step B, the first separator and the second separator are wound around the core such that a base material layer of the first separator and a base material layer of the second separator face each other. A method for producing the battery according to any one of claims 1 to 3.
10. The method for manufacturing a battery according to claim 1 , wherein the first separator and the second separator each have a width of 25 cm or more.
Citation Information
Patent Citations
JP1972-044040A
Winding device for polypropylene film
JP1992350050A
Manufacturing method for flat electrode
JP2003068350A
Method of manufacturing electrode group for nonaqueous secondary battery, electrode group for nonaqueous secondary battery and nonaqueous secondary battery using the same
JP2009193750A
Separator and battery
JP2011138761A