Coil component and manufacturing method thereof
The coil component with a metal magnetic particle base and insulating oxide layer addresses magnetic property deterioration and short circuits, enhancing dielectric strength and oxidation resistance.
Patent Information
- Application Number
- JP2020216302
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-12-25
- Publication Date
- 2024-12-05
- Estimated Expiration
- 2040-12-25
AI Technical Summary
Conventional coil components face issues with magnetic property deterioration due to resin insulating coatings, which also lead to potential short circuits and oxidation when no coating is used, compromising dielectric strength and electrical characteristics.
A coil component design featuring a base body with metal magnetic particles, a buried coil conductor, and an insulating oxide layer containing metal element oxides, particularly with a higher zinc content, to enhance dielectric strength and oxidation resistance while minimizing magnetic property degradation.
The design provides excellent dielectric strength and oxidation resistance, suppressing short circuits and magnetic property deterioration, with the oxide layer ensuring effective insulation and protection against environmental factors.
Smart Images

Figure 0007594904000001 
Figure 0007594904000002 
Figure 0007594904000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a coil component and a method for manufacturing the same. [Background technology]
[0002] Conventional coil components include a base body made of a magnetic material and a coil conductor provided within the magnetic base body. In recent years, as circuits have become larger in current, soft magnetic metal materials that are less likely to cause magnetic saturation even when a large current flows through them have come to be used as materials for the base body of coil components.
[0003] An example of a conventional coil component is described in International Publication No. 2018 / 088264 (Patent Document 1). The coil component described in Patent Document 1 includes a base body containing metal magnetic particles made of a soft magnetic metal material, and a coil conductor embedded in the base body and coated with a polyimide resin.
[0004] Another example of a conventional coil component is described in JP 2019-153650 A (Patent Document 2). The coil component described in Patent Document 2 includes a base body containing metal magnetic particles made of a soft magnetic metal material, and a metal plate embedded in the base body. The metal plate in Patent Document 2 includes a base material layer made of a conductive metal, and a plating layer formed on one side of the base material layer. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] International Publication No. 2018 / 088264 [Patent Document 2] JP2019-153650A Summary of the Invention [Problem to be solved by the invention]
[0006] As described in Patent Document 1, the dielectric strength of the coil component is increased by covering the surface of the coil conductor with a resin material such as polyimide. In other words, the resin insulating coating provided on the surface of the coil conductor suppresses the occurrence of a short circuit between the coil conductor and the metal magnetic particles contained in the base. However, since the insulating coating is made of a non-magnetic resin, there is a problem that the magnetic properties (e.g., inductance) of the coil component are deteriorated by covering the surface of the coil conductor with the resin insulating coating. In Patent Document 1, the deterioration of the magnetic properties is suppressed by thinning the resin insulating coating to the extent that the dielectric strength does not decrease excessively, but the deterioration of the magnetic properties is unavoidable by the amount of the resin insulating coating provided on the surface of the coil conductor.
[0007] If the surface of the coil conductor is not covered with a resin insulating coating, the problem of deterioration of magnetic properties due to the insulating coating does not occur. However, if there is no resin insulating coating on the surface of the coil conductor, a short circuit is likely to occur between the coil conductor and the metal magnetic particles. In addition, if the gap between the coil conductor and the metal magnetic particles is not filled with a resin insulating coating, a gap will inevitably be generated between the coil conductor and the metal magnetic particles. For this reason, when the coil component is used, there is a problem that the oxidation of the coil conductor progresses due to oxygen present in the gap between the coil conductor and the metal magnetic particles, and the electrical properties of the coil component will deteriorate. In addition, there is also a problem that moisture penetrates into the gap between the coil conductor and the metal magnetic particles, and the moisture that penetrates into this gap advances the oxidation of the coil conductor.
[0008] An object of the present invention is to solve or alleviate at least a part of the above-mentioned problems, and more specifically, to provide a coil component that has excellent dielectric strength and oxidation resistance while suppressing deterioration of magnetic properties.
[0009] The object of the present invention other than the above will become clear throughout the entire description of the specification. The invention described in the claims may solve problems other than those grasped from the "Problem to be solved by the invention." [Means for solving the problem]
[0010] A coil component according to one or more embodiments of the present invention comprises a base including a plurality of metal magnetic particles each containing a metal element, a coil conductor mainly composed of copper having an embedded portion disposed inside the base and an exposed portion exposed to the outside of the base, and an insulating oxide layer covering the surface of the embedded portion and containing an oxide of the metal element contained in the plurality of metal magnetic particles and a copper element.
[0011] In one or more embodiments of the present invention, each of the plurality of metal magnetic particles contains a metal element having a greater ionization tendency than copper.
[0012] In one or more embodiments of the present invention, each of the plurality of metal magnetic particles has an oxide film on its surface, and is bonded to adjacent metal magnetic particles by the oxide film.
[0013] In one or more embodiments of the present invention, some of the metal magnetic particles are in contact with the coil conductor via the oxide layer and the oxide coating.
[0014] In one or more embodiments of the present invention, the oxide layer includes elemental zinc.
[0015] In one or more embodiments of the present invention, the oxide layer has a higher zinc element content than the oxide coating.
[0016] In one or more embodiments of the present invention, the atomic ratio of zinc in the oxide layer is 1.0 at % or more and 25 at %.
[0017] One or more embodiments of the present invention relate to a circuit board including any of the coil components described above.One or more embodiments of the present invention relate to an electronic device including the circuit board described above.
[0018] A method for manufacturing a coil component according to one or more embodiments of the present invention includes a preparation step of preparing an intermediate body including an element body including a plurality of metal magnetic particles and a conductor portion mainly composed of copper embedded in the element body, a first heating step of heating the intermediate body at a first temperature to form an oxide film including copper oxide so as to cover a surface of the conductor portion, and a second heating step of heating the intermediate body at a second temperature higher than the first temperature after heating at the first temperature to generate an oxide film including an oxide of a metal element included in each of the plurality of metal magnetic particles, thereby forming a base from the element body and forming an insulating oxide layer including the oxide and a copper element. In the second heating step, at least a part of the copper oxide included in the oxide film is reduced.
[0019] In the second heating step in one or more embodiments of the present invention, an oxide film is formed on each of the plurality of metal magnetic particles, and each of the plurality of metal magnetic particles is bonded to adjacent metal magnetic particles by the oxide film to form the base.
[0020] In one or a plurality of embodiments of the present invention, the conductor portion is covered with a thermally decomposable insulating coating, and the insulating coating is decomposed in the first heating step.
[0021] In one or more embodiments of the present invention, in the second heating step, the intermediate body is heated in an atmosphere having a lower oxygen concentration than in the first heating step.
[0022] In one or more embodiments of the present invention, the preparation step includes a step of applying a suspension containing zinc oxide to the surface of the conductor portion.
[0023] In one or more embodiments of the present invention, in the second heating step, the oxide layer is formed to include zinc oxide. Effect of the Invention
[0024] According to the invention disclosed in this specification, it is possible to provide a coil component that has excellent dielectric strength and oxidation resistance while suppressing deterioration of magnetic properties. [Brief description of the drawings]
[0025] [Figure 1] 1 is a perspective view of a coil component according to an embodiment of the present invention mounted on a mounting board. [Diagram 2] 2 is a cross-sectional view of the coil component shown in FIG. 1 taken along line II. [Diagram 3] 3 is an enlarged cross-sectional view showing a part of the cross section of FIG. 2 in an enlarged manner. [Figure 4] FIG. 4 is a flow diagram showing a manufacturing process of a coil component according to an embodiment of the present invention. [Diagram 5] FIG. 2 is a perspective view showing a schematic diagram of an intermediate product produced in a manufacturing process of a coil component according to one or more embodiments of the present invention. [Figure 6] 4 is an enlarged cross-sectional view showing a part of a cross section of an intermediate body before heating in a first heating step in a manufacturing process of a coil component according to an embodiment of the present invention. FIG. [Figure 7] 1 is an enlarged cross-sectional view showing a portion of a cross section of an intermediate body after being heated in a first heating step and before being heated in a second heating step in a manufacturing process of a coil component according to an embodiment of the present invention. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0026] Various embodiments of the present invention will be described below with reference to the drawings as appropriate. Note that components common to multiple drawings are given the same reference numerals throughout the multiple drawings. Please note that the drawings are not necessarily drawn to scale for the sake of convenience. The embodiments of the present invention described below do not limit the invention according to the claims. Elements described in the following embodiments are not necessarily essential to the solution of the invention.
[0027] A coil component 1 according to an embodiment of the present invention will be described with reference to Figs. 1 to 3. Fig. 1 is a perspective view of the coil component 1 mounted on a mounting substrate 2a, Fig. 2 is a cross-sectional view of the coil component 1 cut along line II, and Fig. 3 is an enlarged cross-sectional view of a part of the cross-section shown in Fig. 2. Each of Figs. 1 and 2 shows a W-axis, an L-axis, and a Z-axis that are orthogonal to each other. In this specification, unless otherwise understood in the context, the "length" direction, the "width" direction, and the "thickness" direction of the coil component 1 are respectively the "L-axis" direction, the "W-axis" direction, and the "T-axis" direction in Fig. 1. In this specification, the orientation and arrangement of the components of the coil component 1 may be described based on the L-axis, W-axis, and Z-axis directions.
[0028] The coil component 1 can be applied to inductors, transformers, filters, reactors, and various other coil components. The coil component 1 can also be applied to coupled inductors, choke coils, and various other magnetically coupled coil components. Applications of the coil component 1 are not limited to those explicitly described in this specification.
[0029] 1 and 3, the coil component 1 includes a base 10 made of a magnetic material, a coil conductor 25 provided on the base 10, and an oxide layer 60 provided between the coil conductor 25 and the base 10. The coil conductor 25 has an embedded portion 25a disposed inside the base 10, an exposed portion 25b extending from one end of the embedded portion 25a to the outside of the base 10, and an exposed portion 25c extending from the other end of the embedded portion 25a to the outside of the base 10.
[0030] The coil component 1 is mounted on a mounting board 2a. The mounting board 2a is provided with land portions 3a and 3b. The coil component 1 is mounted on the mounting board 2a by joining the exposed portion 25b of the coil conductor 25 to the land portion 3a and by joining the exposed portion 25c of the coil conductor 25 to the land portion 3b. In this manner, the circuit board 2 includes the coil component 1 and the mounting board 2a on which the coil component 1 is mounted. The circuit board 2 can include the coil component 1 and various electronic components other than the coil component 1.
[0031] The circuit board 2 can be mounted on various electronic devices. Examples of electronic devices in which the circuit board 2 can be mounted include smartphones, tablets, game consoles, automotive electrical components, servers, and various other electronic devices. The electronic devices in which the coil component 1 is mounted are not limited to those explicitly stated in this specification. The coil component 1 may be an internal component embedded inside the circuit board 2.
[0032] In the illustrated embodiment, the base 10 has a generally rectangular parallelepiped shape. The base 10 has a first main surface 10a, a main surface 10b, a first end surface 10c, a second end surface 10d, a first side surface 10e, and a second side surface 10f, and the six surfaces define the outer surface of the base 10. The first main surface 10a and the second main surface 10b face each other, the first end surface 10c and the second end surface 10d face each other, and the first side surface 10e and the second side surface 10f face each other. In FIG. 1, the first main surface 10a is located on the upper side of the main body 10, so the first main surface 10a may be referred to as the "upper surface". Similarly, the second main surface 10b may be referred to as the "lower surface". The magnetically coupled coil component 1 is disposed so that the second main surface 10b faces the mounting board 2a, so the second main surface 10b may be referred to as the "mounting surface". The up-down direction of the coil component 1 is referred to based on the up-down direction in Fig. 1. In this specification, unless otherwise understood in the context, the "length" direction, "width" direction, and "thickness" direction of the coil component 1 are respectively the "L-axis" direction, "W-axis" direction, and "T-axis" direction in Fig. 1. The L-axis, W-axis, and T-axis are perpendicular to each other.
[0033] In one or more embodiments of the present invention, the coil component 1 is formed so that the length dimension (dimension in the L axis direction) is 1.0 to 12.0 mm, the width dimension (dimension in the W axis direction) is 1.0 to 12.0 mm, and the height dimension (dimension in the T axis direction) is 1.0 to 6.0 mm. The coil component 1 may be formed so that the length dimension (dimension in the L axis direction) is 0.2 to 6.0 mm, the width dimension (dimension in the W axis direction) is 0.1 to 4.5 mm, and the height dimension (dimension in the T axis direction) is 0.1 to 4.0 mm. These dimensions are merely examples, and the coil component 1 to which the present invention can be applied may have any dimensions as long as they are not contrary to the spirit of the present invention.
[0034] The substrate 10 is made of a magnetic material. In one or more embodiments of the present invention, the substrate 10 includes a plurality of metal magnetic particles. The metal magnetic particles are particles or powders made of a soft magnetic metal material. The metal magnetic particles include a metal element having a greater ionization tendency than copper. The metal magnetic particles are, for example, powders of an Fe-Cr-Si alloy. Fe and Cr have a greater ionization tendency than copper (Cu). The soft magnetic metal material for the metal magnetic particles is not limited to an Fe-Cr-Si alloy. The soft magnetic metal material for the metal magnetic particles is, for example, (1) alloy Fe-Si-Al or Fe-Ni, (2) amorphous Fe-Si-Cr-BC or Fe-Si-B-Cr, or (3) particles of a mixed material thereof. When the metal magnetic particles are made of an alloy material, the Fe content in the metal magnetic particles may be 80 wt% or more and less than 97 wt%. When the metal magnetic particles are made of an amorphous material, the Fe content in the metal magnetic particles may be 72 wt% or more and less than 85 wt%. The total content of metal elements that are more easily oxidized than Si and copper in the metal magnetic particles may be 3 wt% or more, 8 wt% or more, or 10 wt% or more.
[0035] In one or more embodiments of the present invention, the particle size of the metal magnetic particles contained in the base 10 is distributed according to a predetermined particle size distribution. The metal magnetic particles have an average particle size of, for example, 1 μm or more and 10 μm or less. The average particle size of the metal magnetic particles contained in the base 10 is determined based on the particle size distribution obtained by cutting the base 10 along its thickness direction (T-axis direction) to expose a cross section, and taking an SEM photograph of the cross section at a magnification of 1000 times to 5000 times with a scanning electron microscope (SEM). For example, the 50% value of the particle size distribution obtained based on the SEM photograph can be set as the average particle size of the metal magnetic particles. The base 10 may be composed of one type of metal magnetic particles, or may be composed of two or more types of metal magnetic particles that are different from each other in terms of material and / or average particle size. When the base 10 is composed of two or more types of metal magnetic particles, the two or more types of metal magnetic particles may be composed of different soft magnetic metal materials. For example, the base 10 may be a mixed particle of metal magnetic particles made of an Fe-Cr-Si alloy and metal magnetic particles made of an Fe-Ni alloy. When the base 10 is composed of two or more kinds of metal magnetic particles, the two or more kinds of metal magnetic particles may have different average particle sizes. The fact that the base 10 contains mixed particles made of two or more kinds of metal magnetic particles with different average particle sizes can be confirmed by two or more peaks appearing in the particle size distribution created based on an SEM photograph.
[0036] The coil conductor 25 is mainly composed of copper. In this specification, the main component refers to the component with the highest content ratio on a mass basis. Therefore, the coil conductor 25 has the highest content ratio of copper on a mass basis. In order to reduce the electrical resistance, the content ratio of copper in the coil conductor 25 may be 90 wt% or more, 95 wt% or more, 99 wt% or more, or a higher content ratio than that. In addition to copper, the coil conductor 25 may contain Ni, Sn, Zn, and / or other elements. The coil conductor 25 is a conductor made of a metal with copper as the main component. The coil conductor 25 may be formed, for example, by bending a metal plate or a metal wire. The coil conductor 25 may be formed, for example, by sintering a paste with copper as the main component. In the illustrated embodiment, the exposed portion 25b of the coil conductor 25 extends from one end of the embedded portion 25a along the first end surface 10c of the base 10, and extends from the lower end of the first end surface 10c along the mounting surface 10b. The exposed portion 25c of the coil conductor 25 extends from the other end of the embedded portion 25a along the second end surface 10d of the base 10, and extends from the lower end of the second end surface 10d along the mounting surface 10b. Thus, the illustrated coil conductor 25 is bent at the boundaries between the embedded portion 25a and each of the exposed portions 25b and 25c, at a position corresponding to the lower end of the first end surface 10c, and at a position corresponding to the lower end of the second end surface 10d. The exposed portions 25b and 25c applicable to the present invention are not limited to the illustrated embodiment. The exposed portions 25b and 25c can have any shape and can be disposed at any position as long as they are exposed from the base 10. When the exposed portion 25b does not extend to the mounting surface 10b, the coil component 1 may include an external electrode (not shown) connected to the exposed portion 25b. As this external electrode, a known external electrode can be applied. The external electrodes are obtained, for example, by applying a conductive paste to the surface of the base body 10 to form a base electrode, and then forming one or more plating layers on the surface of the base electrode. Similarly, even if the exposed portion 25c does not extend to the mounting surface 10b, the coil component 1 can be provided with an external electrode (not shown) that is connected to the exposed portion 25c. The exposed portions 25b and 25c may function as external electrodes as they are.In this case, the exposed portions 25b and 25c are connected directly or indirectly to the conductive members of the mounting board 2 (for example, the lands 3a and 3b), respectively.
[0037] The shape of the coil conductor 25 applicable to the present invention is not limited to the shape shown in the figure. The embedded portion 25a of the coil conductor 25 may have a spiral shape. The embedded portion 25a having a spiral shape may extend in a spiral shape around an axis line that passes through the intersection of the diagonals of the first main surface 10a having a rectangular shape in a plan view and extends in a direction perpendicular to the first main surface 10a (T-axis direction). The shapes of the exposed portions 25b and 25c can also be modified from the shapes shown in the figures. In the illustrated coil conductor 25, the embedded portion 25a and the exposed portions 25b and 25c have the same cross-sectional shape. In the coil conductor 25, the embedded portion 25a may have a circular or elliptical cross-section. The coil conductor 25 may be a straight wire rod with a wire diameter of 1.5 mm. The exposed portions 25b and 25c may be formed by pressing such a wire rod. The exposed portions 25b and 25c may be formed to have a thickness in the range of, for example, 0.1 mm to 0.5 mm.
[0038] When the embedded portion 25a has a helical shape, the embedded portion 25a extends around the coil axis. The embedded portion 25a having a helical shape may be wound around the coil axis for a plurality of turns. The coil axis may be a virtual axis line extending along any one of the T-axis, the L-axis, or the W-axis. A part of the base 10 may be interposed between adjacent turns of the embedded portion 25a wound around the coil axis for a plurality of turns. An insulating material mainly composed of copper oxide may be interposed between adjacent turns of the embedded portion 25a wound around the coil axis for a plurality of turns.
[0039] Next, the microscopic structure near the boundary between the base 10 and the embedded portion 25a of the coil conductor 25 will be described with reference to FIG. 3. FIG. 3 is an enlarged cross-sectional view showing an area A of the cross section of the coil component 1 shown in FIG. 2. Area A is an area that straddles the embedded portion 25a of the coil conductor 25 and the base 10. In the example shown in FIG. 3, the base 10 contains two types of metal magnetic particles having different average particle sizes, specifically, a plurality of first metal magnetic particles 31 and a plurality of second metal magnetic particles 32 having an average particle size smaller than that of the first metal magnetic particles 31. The first metal magnetic particles 31 and the second metal magnetic particles 32 may be formed from the same soft magnetic metal material, or may be formed from different soft magnetic metal materials.
[0040] The surfaces of the metal magnetic particles contained in the substrate 10 are provided with insulating oxide films containing oxides of the metal elements contained in the metal magnetic particles. As shown in FIG. 3, the surfaces of the first metal magnetic particles 31 are provided with oxide films 41, and the surfaces of the second metal magnetic particles 32 are provided with oxide films 42. The oxide films on the surfaces of the metal magnetic particles contain oxides of Fe and other constituent elements of the metal magnetic particles. For example, when the metal magnetic particles are made of an Fe-Cr-Si alloy, the oxide films on the surfaces contain oxides of Fe, Cr, and Si. The first metal magnetic particles 31 are bonded to the adjacent first metal magnetic particles 31 or second metal magnetic particles 32 via the oxide films 41 and / or oxide films 42.
[0041] Between the embedded portion 25a of the coil conductor 25 and the first and second metal magnetic particles 31 and 32, an oxide layer 60 is disposed, covering the surface of the embedded portion 25a. The oxide layer 60 may be in contact with the embedded portion 25a. The oxide layer 60 is provided between the embedded portion 25a and the first and second metal magnetic particles 31 and 32 so as to close the space between the embedded portion 25a and the first and second metal magnetic particles 31 and 32. The oxide layer 60 is in contact with the first metal magnetic particle 31 via the oxide film 41, and is in contact with the second metal magnetic particle 32 via the oxide film 42. A gap may be present between the oxide layer 60 and the first metal magnetic particle 31 and / or the second metal magnetic particle 32.
[0042] As shown in the figure, the oxide layer 60 may cover the entire surface area of the embedded portion 25a. For example, the base 10 is cut along the T axis to expose a cross section, and SEM photographs of the cross section are taken at a magnification of 5000 times so that a part of the surface of the embedded portion 25a and the base 10 are included in the field of view at each of three points (which may be five or more points) arranged at equal intervals in the L axis direction. When the entire surface of the embedded portion 25a is covered with the oxide layer 60 in each of the taken SEM photographs, it can be determined that the oxide layer 60 covers the entire surface of the embedded portion 25a. In this way, the surface of the embedded portion 25a of the coil conductor 25 is covered with the oxide layer 60, and the oxide layer 60 blocks the space between the embedded portion 25a and the first metal magnetic particles 31 and the second metal magnetic particles 32, so that the atmosphere in the usage environment and moisture in the atmosphere can be prevented or suppressed from reaching the embedded portion 25a through the base 10 when the coil component 1 is used.
[0043] In one or more embodiments of the present invention, the oxide layer 60 contains an oxide of a metal element contained in at least one of the first metal magnetic particles 31 and the second metal magnetic particles 32. For example, when the first metal magnetic particles 31 and the second metal magnetic particles 32 are made of an Fe-Cr-Si alloy, the oxide layer 60 contains an oxide of at least one of Fe and Cr. Since the oxide layer 60 contains an oxide of a metal element contained in at least one of the first metal magnetic particles 31 and the second metal magnetic particles 32, the relative magnetic permeability of the oxide layer 60 is higher than the relative magnetic permeability of a conventional insulating coating made of a resin (for example, made of polyimide). The oxide layer 60 may contain an oxide of a constituent element (for example, Si) of the first metal magnetic particles 31 and the second metal magnetic particles 32 other than the metal element. When the base 10 is made of one type of metal magnetic particles, the oxide layer 60 contains at least one metal element of one or more types of metal elements contained in the metal magnetic particles. For example, when the substrate 10 includes one type of metal magnetic particles made of an Fe-Cr-Si alloy, the oxide layer 60 includes at least one of the Fe element and the Cr element. When the substrate 10 includes two or more types of metal magnetic particles, the oxide layer 60 includes at least one metal element out of one or more types of metal elements included in any of the two or more types of metal magnetic particles. For example, when the substrate 10 includes a first type of metal magnetic particles made of an Fe-Cr-Si alloy and a second type of metal magnetic particles made of an Fe-Ni alloy, the oxide layer 60 includes at least one of the Fe element, the Cr element, and the Ni element. t Includes.
[0044] In one or more embodiments of the present invention, the oxide layer 60 may contain elemental copper in addition to an oxide of a metal element contained in at least one of the first metal magnetic particles 31 and the second metal magnetic particles 32. The elemental copper may be present as copper oxide in the oxide layer.
[0045] In an SEM photograph of the cross section of the base 10 taken at a magnification of 5000 to 20000 times, the boundary between the oxide layer 60 and the embedded portion 25a of the coil conductor 25, and the boundary between the oxide layer 60 and the first metal magnetic particle 31 and the second metal magnetic particle 32 can be identified by the difference in brightness. It can be confirmed that the oxide layer 60 contains an oxide of a metal element contained in at least one of the first metal magnetic particle 31 and the second metal magnetic particle 32 by performing energy dispersive X-ray analysis (EDS) on the cross section of the base 10. Specifically, if it can be confirmed by EDS analysis of the cross section of the base 10 that the oxide layer 60 contains a metal element and an oxygen element contained in at least one of the first metal magnetic particle 31 and the second metal magnetic particle 32, it can be confirmed that the oxide layer 60 contains an oxide of a metal element contained in at least one of the first metal magnetic particle 31 and the second metal magnetic particle 32. When mapping data of each element obtained by EDS analysis of the cross section of the base 10 is reconstructed along a line (for example, a line extending along the T-axis direction) that crosses the oxide layer 60, the count number of the metal element contained in at least one of the first metal magnetic particles 31 and the second metal magnetic particles 32 in this scanning line may increase with distance from the embedded portion 25a (closer to the first metal magnetic particles 31 and the second metal magnetic particles 32). In other words, the detection intensity of the metal element contained in at least one of the first metal magnetic particles 31 and the second metal magnetic particles 32 may increase with distance from the embedded portion 25a. On the other hand, the detection intensity of copper in the same scanning line may increase with distance from the embedded portion 25a.
[0046] The oxide layer 60 has excellent insulating properties. The oxide layer 60 exhibits excellent insulating properties because it contains hematite, silicon dioxide, and / or other insulating oxides. The oxide layer 60 is, for example, 10 8 It has a high resistivity of Ω·cm or more. Since the surface of the embedded portion 25a of the coil conductor 25 is covered with the insulating oxide layer 60, it is possible to suppress the occurrence of short circuits between the coil conductor 25 and the first metal magnetic particles 31 and between the coil conductor 25 and the second metal magnetic particles 32. In other words, the coil device 1 has an excellent dielectric strength voltage.
[0047] As described above, when the embedded portion 25a has a spiral shape, a part of the base 10 may be interposed between adjacent turns of the embedded portion 25a. In this case, an oxide layer 60 is provided between the area of the base 10 interposed between the adjacent turns of the embedded portion 25a and the surface of the embedded portion 25a. Since the adjacent turns are thus separated by the insulating oxide layer 60, it is possible to suppress the occurrence of a short circuit between the portions constituting the different turns of the coil conductor 25. Therefore, the coil component 1 has an excellent dielectric strength voltage.
[0048] When embedded portion 25a has a spiral shape, an insulating material mainly composed of copper oxide may be interposed between adjacent turns of embedded portion 25a instead of substrate 10. This insulating material mainly composed of copper oxide can suppress the occurrence of short circuits between the portions constituting different turns of coil conductor 25.
[0049] In one or more embodiments of the present invention, the oxide layer 60 contains elemental zinc. The elemental zinc may be contained in the oxide layer 60 as zinc oxide. The oxide layer 60 contains elemental zinc at a ratio of, for example, 1.0 at% to 25 at%. The elemental zinc may also be contained in at least one of the oxide film 41 of the first metal magnetic particle 31 and the oxide film 42 of the second metal magnetic particle 32. In one or more embodiments, the content ratio (atomic ratio) of elemental zinc in the oxide layer 60 is higher than the content ratio (atomic ratio) of elemental zinc in the oxide film 41 and the content ratio (atomic ratio) of elemental zinc in the oxide film 42. By containing zinc oxide in the oxide layer 60, the oxide layer 60 can be made dense. This can further prevent oxygen and moisture in the air from reaching the embedded portion 25a during use of the coil component 1.
[0050] Next, an exemplary manufacturing method of the coil component 1 according to one embodiment of the present invention will be described with reference to Fig. 4 to Fig. 7. Fig. 4 is a flow diagram showing a manufacturing process of the coil component 1 according to one embodiment of the present invention. In the following description, it is assumed that the coil component 1 is manufactured by a compression molding method. The coil component 1 may be manufactured by any known method other than the compression molding method. For example, the coil component 1 may be manufactured by a sheet lamination method, a print lamination method, a thin film process method, or a slurry build method.
[0051] First, in step S1, an intermediate body 100 is produced. As described later, the intermediate body 100 is subjected to a heat treatment in a later process. This intermediate body 100 is shown in FIG. 5 as a schematic diagram. As shown in the figure, the intermediate body 100 has an element body 110 made of a magnetic material, and a conductor part mainly composed of copper, partly embedded in the element body 110. In the illustrated embodiment, the conductor part 125 is a metal plate mainly composed of copper. A resin insulating coating may or may not be provided on the surface of the conductor part 125. A suspension in which zinc oxide (ZnO) powder is dispersed in alcohol may be applied to the area of the surface of the conductor part 125 that is embedded in the element body 110. A copper wire may be used as the conductor part 125 instead of the above-mentioned copper plate material.
[0052] When producing the intermediate body 100, the conductor 125 is placed in a molding die, a metal magnetic paste containing metal magnetic particles is placed in the molding die in which the conductor 125 is placed, and a predetermined molding pressure (for example, 500 kN to 5000 kN) is applied to the metal magnetic paste in the molding die. This molds the metal magnetic paste into the element 110, and a part of the conductor 125 is embedded in the element 110. In one embodiment, the apparent density of the element 110 is 6.0 g / cm. 3 The molding pressure is adjusted so that the magnetic paste is obtained by kneading metal magnetic particles such as Fe-Cr-Si alloy powder with a binder resin and a solvent. The metal magnetic particles may contain a plurality of types of metal magnetic particles having different particle sizes. The binder resin is, for example, an acrylic resin or other known resin.
[0053] As described above, the coil component 1 can be manufactured by various methods other than the compression molding method. In step S1, the intermediate body 100 in which the conductor portion 125 mainly composed of copper is embedded in the base body 110 containing metal magnetic particles may be manufactured by a manufacturing method other than the compression molding method described above. The intermediate body 100 can be manufactured by, for example, a sheet lamination method. When manufacturing the intermediate body 100 by the sheet lamination method, first, a slurry obtained by kneading the metal magnetic particles and a thermally decomposable binder resin is kneaded, and then a binder resin is kneaded into a slurry (the binder resin is, for example, an acrylic resin or another known resin) by using various sheet forming machines such as a die coater type sheet forming machine. Magnetic Next, prepare multiple sheets of this material. magnetic material Through holes are formed at predetermined positions of the sheet using a laser processing machine or other processing machine, and a conductive paste containing copper as a conductive material is applied in a desired pattern to the magnetic sheet with the through holes formed therein, thereby obtaining a magnetic sheet with a conductor pattern formed thereon. At this time, the through holes formed in the magnetic sheet are filled with the conductive paste. The conductive paste is applied by, for example, a screen printing method. Next, the magnetic sheets with the conductor patterns formed thereon are stacked in a predetermined order, and are heated and pressed at, for example, 80° C. and 300 KN to obtain an intermediate body 100.
[0054] FIG. 6 shows an enlarged view of a part of a cross section of the intermediate body 100 produced in step S1 cut along the T axis. The area shown in FIG. 6 corresponds to area A in FIG. 2. As shown in FIG. 6, the element body 110 includes a plurality of first metal magnetic particles 31 and second metal magnetic particles 32 having an average particle size smaller than that of the first metal magnetic particles 31. A binder resin 45 is filled in the gaps between adjacent metal magnetic particles and between the conductor portion 125 and the metal magnetic particles. In the illustrated embodiment, the conductor portion 125 does not have a resin insulating coating, and is therefore in contact with the first metal magnetic particles 31 and the second metal magnetic particles 32 directly or via the binder resin 45. As described above, the surface of the conductor portion 125 may be covered with an insulating coating made of a thermally decomposable resin. In this case, the conductor portion 125 is in contact with the first metal magnetic particles 31 and the second metal magnetic particles 32 via a resin insulating coating, or via a resin insulating coating and the binder resin 45.
[0055] Next, in step S2, a first heating process is performed on the intermediate body 100 produced in step S1. Specifically, the intermediate body 100 is placed in a heating furnace and heated in the furnace in an air atmosphere at 250 to 350° C. for 30 to 120 minutes. This first heating process decomposes the binder resin 45, and also forms a copper oxide film 50 containing copper oxide on the surface of the portion of the conductor 125 that is embedded in the element body 110. If the surface of the conductor 125 is covered with an insulating coating made of a thermally decomposable resin, in the first heating process, the intermediate body 100 is heated to a temperature equal to or higher than the thermal decomposition temperature of the resin that constitutes the insulating coating on the surface of the conductor 125. Therefore, the insulating coating on the surface of the conductor 125 is thermally decomposed in the first heating process, and a copper oxide film 50 containing copper oxide is formed on the surface of the portion of the conductor 125 that is embedded in the element body 110. In this way, when the conductor 125 is covered with a resin insulating coating, the area around the conductor 125 where the resin insulating coating existed before the first heat treatment does not become a void, but is blocked by the copper oxide film 50. Since the first heat treatment is performed in an oxygen atmosphere, the oxidation of the copper contained in the conductor 125 is promoted in the first heat treatment, and the copper oxide film 50 is formed on the surface of the conductor 125 so as to block the voids created by the decomposition of the resin insulating coating and the binder resin 45.
[0056] The portion of the conductor 125 embedded in the element 110 may have a spiral shape. When the portion of the conductor 125 having an insulating coating on its surface embedded in the element 110 has a spiral shape, the insulating coating is thermally decomposed by the first heat treatment, and the space occupied by the insulating coating before the thermal decomposition is filled with copper oxide generated by oxidation of the copper contained in the conductor 125. In other words, when the conductor 125 having an insulating coating is embedded in the element 110, the copper oxide film 50 is also provided between adjacent turns of the conductor 125 having a spiral shape. The copper oxide film 50 interposed between the adjacent turns suppresses the occurrence of a short circuit between the adjacent turns of the conductor 125.
[0057] The main component of the copper oxide film 50 may be copper oxide (CuO). In this way, the element body 110 is degreased and the surface of the conductor portion 125 is oxidized by the first heating treatment. The heating conditions in the first heating treatment may be appropriately changed so that the thickness of the copper oxide film 50 is 0.1 μm or more. The heating conditions in the first heating treatment are set so that the metal magnetic particles contained in the element body 110 are not oxidized to form an oxide film on their surfaces. When the heating temperature in the first heating treatment is set to 250 to 350° C., the first metal magnetic particles 31 and the second metal magnetic particles 32 are made of a material that does not form an oxide film on its surface at the heating temperature in the first heating treatment.
[0058] When a zinc oxide (ZnO) suspension is applied to the surface of the conductor portion 125 in step S1, when a copper oxide film 50 is formed on the surface of the conductor portion 125, the zinc oxide that was present on the surface of the conductor portion 125 is incorporated into the copper oxide film 50.
[0059] FIG. 7 shows an enlarged view of a part of a cross section of the intermediate body 100 after the first heat treatment in step S2, cut along the T-axis. As shown in the figure, the binder resin is decomposed in the first heat treatment, and the gaps between adjacent metal magnetic particles in the region filled with the binder resin 45 before the first heat treatment become voids 55. On the other hand, the binder resin 45 filled between the conductor portion 125 and the metal magnetic particles is also decomposed, but the gaps between the conductor portion 125 and the metal magnetic particles do not become voids and are blocked by the copper oxide film 50. Since the first heat treatment is performed in an oxygen atmosphere, the oxidation of copper contained in the conductor portion 125 is promoted in the first heat treatment, and the copper oxide film 50 is formed on the surface of the conductor portion 125 so as to block the voids formed by the decomposition of the binder resin 45. The copper oxide film 50 may be formed so as to cover the entire region of the surface of the conductor portion 125 that is in contact with the element body 110.
[0060] Next, in step S3, a second heat treatment is performed on the intermediate body 100 that has been subjected to the first heat treatment. The second heat treatment is performed in a low-oxygen concentration atmosphere with a lower oxygen concentration than that of the first heat treatment at a higher temperature than that of the first heat treatment. The second heat treatment oxidizes each of the first metal magnetic particles 31 and the second metal magnetic particles 32 contained in the element body 110, and an oxide film 41 is formed on the surface of the first metal magnetic particle 31, and an oxide film 42 is formed on the surface of the second metal magnetic particle 32. Since the first metal magnetic particles 31 and the second metal magnetic particles 32 contain a metal element having a higher ionization tendency than copper, when an oxide of a metal element having a higher ionization tendency than copper is generated in the first metal magnetic particle 31 or the second metal magnetic particle 32 arranged in the vicinity of the copper oxide film 50, a part or all of the copper oxide contained in the copper oxide film 50 is reduced. Since the second heat treatment is performed in a low oxygen concentration atmosphere, the metal elements contained in the first metal magnetic grains 31 and the second metal magnetic grains 32 near the copper oxide film 50 inside the element body 110 take oxygen from the copper oxide to become oxides. In this way, in the second heat treatment, the copper oxide contained in the copper oxide film 50 is reduced, and the copper oxide film 50 becomes an oxide layer 60. Unlike the copper oxide film 50, the oxide layer 60 does not contain copper oxide as a main component. When only a portion of the copper oxide contained in the copper oxide film 50 is reduced by the second heat treatment, the oxide layer 60 contains the copper oxide that was contained in the copper oxide film 50. The oxide layer 60 contains an oxide of a metal element contained in at least one of the first metal magnetic grains 31 and the second metal magnetic grains 32. The oxide layer 60 may contain a copper element that existed as copper oxide before the second heat treatment.
[0061] As described above, when the portion of the conductor 125 having an insulating coating on its surface that is embedded in the element 110 has a spiral shape, the copper oxide film 50 is interposed between adjacent turns of the conductor 125 having this spiral shape. The copper oxide contained in the copper oxide film 50 interposed between adjacent turns of the conductor 125 having this spiral shape is less likely to be reduced by a metal element having a higher ionization tendency than the copper contained in the first metal magnetic particle 31 or the second metal magnetic particle 32 because of the large distance between the copper oxide film 50 and the first metal magnetic particle 31 or the second metal magnetic particle 32. Therefore, a relatively large amount of copper oxide remains in the region of the copper oxide film 50 interposed between adjacent turns of the conductor 125 having a spiral shape compared to other regions adjacent to the first metal magnetic particle 31 or the second metal magnetic particle 32. When a metal element (e.g., Fe or Cr) having a greater ionization tendency than copper contained in the first metal magnetic particle 31 or the second metal magnetic particle 32 migrates by thermal diffusion to between adjacent turns of the spiral conductor 125, the copper oxide present between the adjacent turns of the spiral conductor 125 can also be reduced by the metal element having a greater ionization tendency than copper. In other words, the copper oxide film 50 interposed between the adjacent turns of the spiral conductor 125 may be partially turned into an oxide layer 60 by the second heat treatment.
[0062] When a suspension of zinc oxide (ZnO) is applied to the surface of the conductor part 125 in step S1, the oxide layer 60 is formed so as to contain zinc oxide in addition to an oxide of a metal element contained in at least one of the first metal magnetic particles 31 and the second metal magnetic particles 32. This zinc oxide can densify the oxide layer 60 generated in the second heat treatment.
[0063] The second heat treatment is carried out, for example, for 30 to 120 minutes in a mixed atmosphere of nitrogen and oxygen at about 600 to 900° C. The oxygen concentration of the mixed atmosphere is set to 100 to 2000 ppm. Research by the present inventors has revealed that if the distance between the copper oxide film 50 and the surface of the element body 110 in the intermediate body 100 is 2 mm or more, the copper oxide contained in the 0.5 μm copper oxide film 50 can be entirely reduced by heating the intermediate body at a temperature of about 800° C. for 60 minutes in a mixed atmosphere of nitrogen and oxygen with an oxygen concentration of 2000 ppm.
[0064] When zinc oxide is contained in the copper oxide film 50, at least a part of the zinc oxide is reduced in the second heat treatment. Since the melting point of zinc is lower than the heating temperature in the second heat treatment, the reduced zinc melts in the second heat treatment. When there are gaps between the copper oxide film 50 and the metal magnetic particles 31 and / or the metal magnetic particles 32, the molten zinc can move to the gaps and fill at least a part of the gaps. This can reduce the gaps between the oxide layer 60 and the first metal magnetic particles 31 and / or the second metal magnetic particles 32 after the second heat treatment, so that the air or moisture in the air can be further prevented from reaching the embedded portion 25a when the coil component 1 is used.
[0065] Next, the coil conductor 25 is formed by bending the portion of the conductor 125 exposed from the base 10 along the surface of the base 10. The coil conductor 25 is formed by bending the conductor 125. The bent portions of the conductor 125 become the exposed portions 25b and 25c. When a copper wire is used instead of the conductor 125, the portion of the wire exposed from the base 10 is pressed into a plate shape, and the plate-shaped portion is bent to form the exposed portions 25b and 25c. In another embodiment of the present invention, the exposed portions 25b and 25c may be exposed to the outside of the base 10 from the mounting surface 10b. In this case, the exposed surfaces 25b and 25c can be connected to the lands 3a and 3b, respectively, without bending the conductor 125. In other words, the exposed surfaces 25b and 25c of the coil conductor 25 can function as external electrodes without bending the conductor 125.
[0066] The coil component 1 is produced in the above manner. The method for producing the coil component 1 may additionally include steps other than steps S1 to S3. For example, the base 10 produced by the heat treatment step is subjected to a polishing treatment such as barrel polishing as necessary. Some of the steps S1 to S3 may be performed in parallel or in a different order. For example, the bending process of the conductor portion 125 may be performed before the first heat treatment in step S2, or may be performed between steps S2 and S3. The method for producing the coil component 1 may also include steps other than steps S1 to S3. For example, an external electrode may be provided on the base 10 by a known method. The external electrode is electrically connected to a portion of the coil conductor 25 exposed from the base 10.
[0067] Next, the effects of the above-mentioned embodiment will be described. According to one or more embodiments of the present invention, since the surface of the embedded portion 25a of the coil conductor 25 is covered with the insulating oxide layer 60, no short circuit occurs between the coil conductor 25 and the metal magnetic particles (for example, the first metal magnetic particles 31 and the second metal magnetic particles 32) included in the base 10. In addition, since the surface of the embedded portion 25a of the coil conductor 25 is covered with the oxide layer 60 and the gap between the coil conductor 25 and the metal magnetic particles constituting the base 10 is filled with this oxide layer 60, it is possible to suppress the air or moisture in the air from passing through the base 10 and reaching the coil conductor 25. Furthermore, since the oxide layer 60 contains oxides of metal elements contained in the metal magnetic particles, the relative magnetic permeability of the oxide layer 60 is higher than that of a conventional resin insulating coating. Therefore, in the coil component 1, the oxide layer 60 provides excellent dielectric strength and oxidation resistance, and also suppresses deterioration of magnetic properties.
[0068] According to one or more embodiments of the present invention, the oxide layer 60 contains zinc oxide, thereby making the oxide layer 60 dense. This can further prevent the air and moisture in the air from reaching the coil conductor 25.
[0069] The dimensions, materials, and arrangement of each component described in this specification are not limited to those explicitly described in the embodiments, and each component can be modified to have any dimensions, materials, and arrangement that can be included in the scope of the present invention. In addition, components not explicitly described in this specification can be added to the described embodiments, and some of the components described in each embodiment can be omitted.
[0070] The designations "first," "second," "third," and the like in this specification are given to identify components, and do not necessarily limit the number, order, or content. Furthermore, numbers for identifying components are used in different contexts, and a number used in one context does not necessarily indicate the same configuration in another context. Furthermore, a component identified by a certain number does not prevent the component from also having the function of a component identified by another number. [Explanation of symbols]
[0071] 1 Coil parts 10 Base 25 Coil conductor 25a Buried part 25b, 25c Exposed part 31 First metal magnetic particles 32 Second metal magnetic particles 41, 42 Oxide film 45 Binder Resin 50 Copper oxide film 55 void 60 Oxide layer
Claims
1. A substrate including a plurality of metal magnetic particles each containing a metal element and having an oxide film on the surface thereof; a coil conductor mainly made of copper, the coil conductor having an embedded portion disposed inside the base and an exposed portion exposed to the outside of the base; an insulating oxide layer formed between the oxide film and the embedded portion, covering a surface of the embedded portion, and containing an oxide of the metal element contained in the plurality of metal magnetic particles and a copper element; A coil component comprising:
2. Each of the plurality of metal magnetic particles contains a metal element having a greater ionization tendency than copper. The coil component according to claim 1 .
3. Each of the plurality of metal magnetic grains is bonded to an adjacent metal magnetic grain by the oxide coating. The coil component according to claim 1 or 2.
4. a part of the plurality of metal magnetic particles is in contact with the coil conductor via the oxide layer and the oxide coating; The coil component according to claim 1 .
5. The oxide layer contains zinc element. The coil component according to claim 1 .
6. the zinc element content in the oxide layer is higher than the zinc element content in the oxide coating; The coil component according to claim 5 .
7. The atomic ratio of zinc in the oxide layer is 1.0 at% or more and 25 at% or less. The coil component according to claim 5 or 6.
8. A circuit board comprising the coil component according to claim 1 .
9. An electronic device comprising the circuit board according to claim 8.
10. a preparation step of preparing an intermediate body including an element body including a plurality of metal magnetic particles and a conductor portion mainly composed of copper embedded in the element body; a first heating step of heating the intermediate body at a first temperature to form an oxide film containing copper oxide so as to cover a surface of the conductor portion; a second heating step of heating the intermediate body at a second temperature higher than the first temperature after heating at the first temperature to generate an oxide film containing an oxide of a metal element contained in each of the plurality of metal magnetic particles, thereby forming a base body from the element body and forming an insulating oxide layer containing the oxide and a copper element; Equipped with the oxide layer is formed between the oxide film formed on the surfaces of the plurality of metal magnetic particles and a surface of the conductor portion; A manufacturing method for coil components.
11. In the second heating step, at least a portion of the copper oxide contained in the oxide film is reduced. The method for manufacturing a coil component according to claim 10.
12. In the second heating step, an oxide film is formed on each of the plurality of metal magnetic particles, and each of the plurality of metal magnetic particles is bonded to an adjacent metal magnetic particle by the oxide film to form the base. The method for manufacturing a coil component according to claim 10 or 11.
13. In the second heating step, the intermediate body is heated in an atmosphere having an oxygen concentration lower than that in the first heating step. The method for manufacturing the coil component according to claim 10 .
14. the conductor portion is covered with a thermally decomposable insulating coating, The insulating coating is decomposed in the first heating step. The method for manufacturing the coil component according to any one of claims 10 to 13.
15. The preparation step includes a step of applying a suspension containing zinc oxide to a surface of the conductor portion. The method for manufacturing the coil component according to any one of claims 10 to 14.
16. In the second heating step, the oxide layer is formed so as to contain zinc oxide. The method for manufacturing the coil component according to claim 15 .
Citation Information
Patent Citations
Coil component and manufacturing method of the same, coil component built-in substrate, and voltage adjustment module including the substrate
JP2015088753A
Surface mount inductor and manufacturing method thereof
JP2019153650A
Laminate inductor
WO2013099297A1
Inductance element and method for manufacturing same
WO2018088264A1