Hydrogen production from hydrocarbons

The method of sublimating metal salts with hydrocarbons efficiently produces hydrogen gas, addressing inefficiencies and emissions of traditional methods by using a process that forms hydrogen and carbon without water or carbon dioxide.

JP7948623B2Active Publication Date: 2026-11-11JOHNS HOPKINS UNIVERSITY
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2023541079
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-01-07
Filing Date
2022-01-07
Publication Date
2026-11-11
Estimated Expiration
2042-01-07

AI Technical Summary

Technical Problem

Existing methods for producing hydrogen, such as steam methane reforming and electrolysis, are inefficient in terms of energy use and produce significant carbon dioxide emissions, and require large amounts of water.

Method used

A method involving the sublimation of metal salts with hydrocarbons to produce hydrogen gas, using a process that includes sublimating a metal salt containing a metal and a halide, contacting it with a gas-phase hydrocarbon to form elemental metal, carbon, and hydrogen halide, and then thermally decomposing the hydrocarbon to produce additional hydrogen gas.

Benefits of technology

This process is more energy-efficient than steam methane reforming and electrolysis, does not require water as a reactant, and produces high-purity carbon byproducts without carbon dioxide emissions, while also avoiding carbon tar accumulation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007948623000002
    Figure 0007948623000002
  • Figure 0007948623000003
    Figure 0007948623000003
  • Figure 0007948623000004
    Figure 0007948623000004
Patent Text Reader

Abstract

A method of producing hydrogen includes sublimating a metal salt comprising a metal and a halide to produce a gas-phase metal salt comprising the metal and the halide, and contacting the gas-phase metal salt with a gas-phase hydrocarbon to produce a hydrogen halide comprising the metal in elemental form, carbon in elemental form, hydrogen gas, and the halide.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] [Cross-reference with related applications] This application claims the interests of U.S. Patent Application No. 63 / 134,796, filed on 7 January 2021, entitled “Production of Hydrogen from Hydrocarbons,” which is incorporated herein by reference in its entirety.

[0002] [Research or development sponsored by the federal government] This invention was developed with government support under Contract DE-AR00001019, granted by the Energy Advanced Research Projects Office, a part of the U.S. Department of Energy. The government has certain rights to this invention.

[0003] This invention relates to a method and system for producing hydrogen from hydrocarbons. [Background technology]

[0004] Hydrogen is typically produced by steam methane reforming or electrolysis. In steam methane reforming, natural gas is reacted with water at high temperature and pressure to produce hydrogen and carbon monoxide. Additional hydrogen can be obtained by reacting carbon monoxide with water to produce hydrogen and carbon dioxide. Electrolysis uses an electrochemical reaction to break down water into hydrogen and oxygen. Steam methane reforming is used to produce over 95% of the total hydrogen, but it requires large amounts of water and produces millions of tons of carbon dioxide annually. Electrolysis is less cost-effective than steam methane reforming and requires large amounts of water as well as electricity. [Overview of the Initiative] [Problems that the invention aims to solve]

[0005] This disclosure generally relates to systems and methods for producing hydrogen from hydrocarbons. Embodiments include systems and methods for the reduction of gas-phase metal halides using gas-phase hydrocarbons, yielding carbon elements, hydrogen halides, and metals, and for the reoxidation of metals using hydrogen halides, yielding hydrogen gas and metal halides. The reduced metal halides and carbon catalyze the thermal decomposition of gas-phase hydrocarbons, yielding additional carbon elements and hydrogen gas.

[0006] The disclosed inventive concept includes those defined in the attached claims, but it should be understood that the inventive concept may also be defined according to the following embodiments.

[0007] In addition to the embodiments of the attached claims and the embodiments described above, the following numbered embodiments are also innovative. [Means for solving the problem]

[0008] Embodiment 1 is a reaction method, The steps include sublimating a metal salt containing a metal and a halide to produce a gas-phase metal salt containing the metal and the halide, and The method comprises the step of contacting the gas-phase metal salt with a gas-phase hydrocarbon to produce a metal in elemental form, carbon in elemental form, hydrogen gas, and a hydrogen halide containing the halide.

[0009] Embodiment 2 is a method according to Embodiment 1, wherein the contact occurs at a temperature in the range of about 800°C to about 1300°C, or between about 850°C and about 1300°C.

[0010] Embodiment 3 is a method according to Embodiment 1 or 2, wherein the metal comprises one or more of magnesium, calcium, manganese, iron, cobalt, nickel, and copper.

[0011] Embodiment 4 is the method according to any one of Embodiments 1 to 3, wherein the halide comprises one or more of fluoride, chloride, bromide, and iodide.

[0012] Embodiment 5 is the method according to any one of Embodiments 1 to 4, wherein the gaseous hydrocarbon comprises natural gas.

[0013] Embodiment 6 is the method according to any one of Embodiments 1 to 5, wherein the gaseous hydrocarbon comprises one or more of methane, ethane, propane, butane, pentane, hexane, heptane, octane, and nonane, or any isomer thereof.

[0014] Embodiment 7 is the method according to any one of Embodiments 1 to 6, wherein the sublimation step occurs at a pressure in the range between about 0.01 MPa (0.1 bar) and about 5 MPa (50 bar).

[0015] Embodiment 8 is the method according to any one of Embodiments 1 to 7, wherein the contacting step occurs at a pressure in the range between about 0.01 MPa (0.1 bar) and about 5 MPa (50 bar).

[0016] Embodiment 9 is the method according to any one of Embodiments 1 to 8, further comprising the step of thermally decomposing a gaseous hydrocarbon to produce carbon and hydrogen gas.

[0017] Embodiment 10 is the method according to Embodiment 9, wherein the contacting step comprises the step of reducing the metal in the gaseous metal salt using the gaseous hydrocarbon.

[0018] Embodiment 11 is the method according to Embodiment 9 or 10, wherein the pyrolysis step is catalyzed by a metal.

[0019] Embodiment 12 is a method according to any one of Embodiments 9 to 11, wherein the heat for pyrolysis is supplied by electricity.

[0020] Embodiment 13 is a method according to any one of Embodiments 1 to 12, further comprising the step of contacting a metal with a hydrogen halide to produce a gaseous metal salt and hydrogen gas.

[0021] Embodiment 14 is the method according to Embodiment 13, further comprising the step of heating the hydrogen halide before contacting the metal with the hydrogen halide.

[0022] Embodiment 15 is a method according to Embodiment 14, wherein the step of heating the hydrogen halide includes the step of heating the hydrogen halide to a temperature of at least 1000°C.

[0023] Embodiment 16 is a method according to Embodiment 14 or 15, wherein the step of contacting a metal with a high-temperature hydrogen halide to produce a metal salt occurs in an adiabatic reactor.

[0024] Embodiment 17 is a method according to any one of Embodiments 13 to 16, further comprising the step of condensing a metal salt to produce a solid-phase metal salt.

[0025] Embodiment 18 is a method according to Embodiment 17, wherein the solid-phase metal salt is in the form of particles, and the particles are at least partially coated with carbon.

[0026] Embodiment 19 is the method according to Embodiment 18, further comprising the step of contacting a metal salt with hydrogen chloride having a temperature of at least 1000°C to produce a gaseous metal halide and particulate carbon material.

[0027] Embodiment 20 is a method according to Embodiment 19, wherein the particulate carbon material comprises a large number of hollow carbon particles.

[0028] Embodiment 21 is a method according to Embodiment 20, wherein the hollow carbon particles have a diameter in the range of approximately 200 nm to approximately 300 nm.

[0029] Embodiment 22 is a method according to Embodiment 21, wherein the particulate carbon material contains less than 100 ppm by weight of metal.

[0030] Embodiment 23 is a method according to any one of Embodiments 1 to 22, wherein the halide is a chloride and the metal is nickel.

[0031] Embodiment 24 is a method according to any one of Embodiments 1 to 23, wherein the hydrocarbon is methane.

[0032] Embodiment 25 is a method according to any one of Embodiments 1 to 24, wherein the sublimation step occurs prior to contact.

[0033] Embodiment 26 is a method according to any one of Embodiments 1 to 25, wherein the sublimation step includes advancing the metal salt toward the reaction zone of the reactor together with the gaseous hydrocarbon.

[0034] Embodiment 27 is the method according to Embodiment 26, further comprising the step of heating the reaction zone to a temperature in the range of about 800°C and about 1300°C.

[0035] Embodiment 28 is a method in which the step of heating the reaction zone is achieved using electricity, in the method of Embodiment 26 or 27.

[0036] Embodiment 29 is a method in which electricity is used to generate radiant heat, in the same manner as described in Embodiment 28.

[0037] Embodiment 30 is a method according to Embodiment 29, wherein the radiant heat is supplied by an electric furnace or an induction heating element.

[0038] Embodiment 31 is a method according to any one of Embodiments 1 to 30, wherein the sublimation step and the contact step occur simultaneously in the reaction zone of the reactor.

[0039] Embodiment 32 is a method according to any one of Embodiments 1 to 31, wherein the metal salt is anhydrous.

[0040] Embodiment 33 is a method for generating hydrogen gas, The steps include bringing a gaseous metal halide into contact with a gaseous hydrocarbon, A step of decomposing metal halides and hydrocarbons to produce gaseous products containing hydrogen and hydrogen halides, and solid products containing metals and carbon, The steps include separating hydrogen from hydrogen halide, and The steps include: bringing hydrogen halide into contact with a metal to produce a gaseous metal halide; This method includes [something].

[0041] Embodiment 34 is the method according to Embodiment 33, further comprising the step of contacting a metal with hydrogen halide and then cooling the gaseous metal halide to produce a solid-phase metal halide.

[0042] Embodiment 35 is the method according to Embodiment 34, further comprising the step of heating a solid-phase metal halide to produce a gaseous metal halide.

[0043] Embodiment 36 is the method according to Embodiment 35, further comprising the step of contacting a gas-phase metal halide with a gas-phase hydrocarbon.

[0044] Embodiment 37 is a method according to any one of Embodiments 33 to 36, further comprising the step of separating a gaseous product from a solid product.

[0045] Embodiment 38 is a method according to any one of Embodiments 33 to 37, further comprising the step of heating the hydrogen halide to a temperature of at least about 1000°C before contacting the hydrogen halide with the metal.

[0046] Embodiment 39 is a method according to any one of Embodiments 33 to 38, further comprising the step of contacting a solid product with hydrogen halide to produce gaseous metal halide and carbon.

[0047] Embodiment 40 is the method according to Embodiment 39, further comprising the step of condensing a metal halide to produce a solid mixture containing a metal halide and carbon.

[0048] Embodiment 41 is a method according to Embodiment 40, wherein the solid mixture comprises particles of a metal halide coated with a portion of carbon.

[0049] Embodiment 42 is the method according to Embodiment 41, further comprising the step of contacting a solid mixture with hydrogen chloride having a temperature of at least 1000°C to produce gaseous metal halides and particulate carbon materials.

[0050] Embodiment 43 is a method according to Embodiment 42, wherein the particulate carbon material comprises a large number of hollow carbon particles.

[0051] Embodiment 44 is a method according to Embodiment 43, wherein the hollow carbon particles have a diameter in the range of approximately 200 nm to approximately 300 nm.

[0052] Embodiment 45 is a method according to Embodiment 44, wherein the particulate carbon material contains less than 100 ppm by weight of metal.

[0053] Embodiment 46 is a hydrogen generation system, A first reactor configured to react gaseous reactants, A heat exchanger configured to receive a mixture of gaseous and solid reaction products from a first reactor, A separator configured to receive the gas outflow from the heat exchanger and to supply a gas inflow to the heat exchanger, A second reactor configured to react the solid inflow from the heat exchanger with the gas inflow, A condenser configured to condense the reaction products from the second reactor, A third reactor is configured to receive solid products from a condenser, evaporate the solid products to produce gaseous products, and supply the gaseous products to the first reactor, It is a system that includes [this feature].

[0054] Embodiment 47 is a system in which, in the system described in Embodiment 46, the first reactor, the second reactor, or both are configured to operate at temperatures in the range of about 800°C and about 1200°C.

[0055] Embodiment 48 is a system in which the second reactor is an adiabatic reactor, in the system described in Embodiment 46 or 47.

[0056] Embodiment 49 is a system in which, in any one of Embodiments 46 to 48, the third reactor is configured to separate the solid product components from the condenser.

[0057] Embodiment 50 is a system according to any one of Embodiments 46 to 49, further comprising an additional separator configured to remove hydrogen from the gas inflow from the heat exchanger.

[0058] The systems and methods described herein are advantageously more energy-efficient than steam methane reforming and far more energy-efficient than electrolysis. These systems and methods can be powered by electricity, do not contain water as a reactant, do not produce carbon dioxide as a product, and produce high-purity carbon byproducts. In addition, these systems and methods produce free-flowing carbon element powder without accumulating carbon tar products on the surface of the high-temperature pyrolysis reactor.

[0059] Details of one or more embodiments of the subject matter of this disclosure are described in the accompanying drawings and specification. Other features, aspects, and advantages of the subject matter will become apparent from the specification, drawings, and claims. [Brief explanation of the drawing]

[0060] [Figure 1] This flowchart illustrates the reaction scheme for the sublimation of metal salts, the reaction of gas-phase metal salts with hydrocarbons, and the thermal decomposition of hydrocarbons that produce hydrogen gas. [Figure 2] This is a schematic diagram of a reactor configured to carry out the reaction shown in Figure 1. [Figure 3] This figure shows methane decomposition in a reactor similar to the one shown in Figure 2, as a function of temperature. [Figure 4A] This is an image of nickel chloride before sublimation in the reaction scheme shown in Figure 1. [Figure 4B] Figure 1 shows an image of nickel chloride after partial consumption in the reaction scheme. [Figure 4C] Figure 1 shows an image of nickel chloride after partial consumption in the reaction scheme. [Figure 5] This flowchart shows the reaction scheme for oxidizing the metal generated in the reaction scheme of Figure 1 with concentrated hydrogen halide to produce hydrogen gas and the metal salt shown in Figure 1. [Figure 6] This is a flowchart showing the operation in the generation of hydrogen gas according to the embodiments described herein. [Figure 7]This is an exemplary process flow diagram for hydrogen gas production according to embodiments described herein. [Figure 8] This is a schematic diagram of a unit for separating nickel chloride from solid carbon and evaporating the nickel chloride. [Figure 9A] This is a transmission electron microscope image of carbon-coated nickel particles before nickel chloride is regenerated and evaporated in a heater. [Figure 9B] This is a transmission electron microscope image of hollow carbon particles produced after the regeneration and evaporation of nickel chloride from the material shown in Figure 9A. [Figure 9C] Figure 9A shows scanning electron microscope images at 10,000x magnification of hollow carbon particles produced after the regeneration and evaporation of nickel chloride from the material. [Figure 9D] This is a scanning electron microscope image at 50,000x magnification of hollow carbon particles produced after the regeneration and evaporation of nickel chloride from the material shown in Figure 9A. [Modes for carrying out the invention]

[0061] Figure 1 is a flowchart representing reaction scheme 100 for sublimation of a metal salt, reaction of a gas-phase metal salt with a gas-phase hydrocarbon, and thermal decomposition of the hydrocarbon producing hydrogen gas. In the example shown in Figure 1, the metal salt is nickel chloride and the gas-phase hydrocarbon is methane. However, in some embodiments, the metal includes one or more alkaline earth metals and transition metals such as magnesium, calcium, manganese, iron, cobalt, nickel, and copper, and the metal salt is a metal halide including one or more fluorides, chlorides, bromides, and iodides. In some embodiments, the gas-phase hydrocarbon includes one or more methane, ethane, propane, butane, pentane, hexane, heptane, octane, and nonane or any isomers thereof. In some embodiments, the gas-phase hydrocarbon includes natural gas.

[0062] In reaction 102, a metal salt is sublimated to produce a gas-phase metal salt. The metal salt is typically a metal halide in an anhydrous powder form. Reaction 102 is endothermic and occurs under temperature and pressure conditions selected to sublimate the metal salt. In reaction 104, the gas-phase metal salt reacts with a gas-phase hydrocarbon to produce the metal in elemental form, the carbon in elemental form, and a gas-phase hydrogen halide. In some cases, reaction 102 is initiated by blowing the metal salt together with the gas-phase hydrocarbon towards a heated reaction zone in the reactor. The reduction of the metal chloride in reaction 104 is exothermic and occurs in the absence of a catalyst under temperature and pressure conditions selected to reduce the metal in the metal salt and decompose the hydrocarbon by contacting the gas-phase metal salt with the gas-phase hydrocarbon. In some embodiments, reaction 102 occurs before reaction 104. In some embodiments, reactions 102 and 104 occur simultaneously. In some embodiments, reaction 106 occurs simultaneously with reactions 102 and 104. In one embodiment, in reaction 106, which occurs in the absence of a metal salt (i.e., after the metal salt is consumed in reaction 104, an excess hydrocarbon is present), the hydrocarbon decomposes to produce carbon and hydrogen gas. Reaction 106 is endothermic itself and occurs under temperature and pressure conditions selected to thermally decompose the hydrocarbon in the presence of metallic and elemental forms of carbon capable of acting as a catalyst. Reaction 106 proceeds until the reactants cool to a temperature at which thermal decomposition kinetically stops, typically about 850°C.

[0063] Figure 2 shows a portion of reactor 200 configured to carry out reactions 102, 104, and 106 of reaction scheme 100. The metal salt is supplied to reactor 200 through inlet 202 (e.g., in the form of anhydrous powder). The gaseous hydrocarbon is supplied to reactor 200 through inlet 204 and passes through distributor 206. The gaseous hydrocarbon can be mixed with an inert gas (e.g., argon). The gaseous hydrocarbon comes into contact with the metal salt in mixing zone 208, and the mixture advances to reaction zone 210. In one embodiment, reaction zone 210 includes a fluidized bed. Electricity is used to generate radiant heat within reaction zone 210, for example, using an electric furnace or high-frequency induction heating. The reaction zone 210 can be maintained at a temperature in the range of about 800°C to about 1300°C, and at an appropriate corresponding pressure selected for the completion of reactions 102 and 104. In some embodiments, reactor 200 includes an insulating material 212. As shown in Figure 2, reaction zone 210 includes a high-frequency coil 214 and a heating element 216. Reactions 102 and 104 may occur simultaneously in reaction zone 210. Reaction 106 occurs in outlet zone 218. The thermal decomposition of hydrocarbons in outlet zone 218 typically occurs at temperatures in the range of about 800°C to about 1300°C (e.g., between about 850°C and about 1300°C, or above about 850°C), and at appropriate corresponding pressures selected for the complete thermal decomposition of the available hydrocarbons. The thermal decomposition results in the cooling of the reaction products in outlet zone 218. In some embodiments, the reaction products exit the reactor at about 850°C.

[0064] For example, as shown in Figure 1, the metal salt is anhydrous nickel chloride in powder form, and the hydrocarbon is methane. Reaction 102 is carried out under temperature and pressure conditions selected to sublimate the nickel chloride (e.g., between about 750°C and about 1300°C, or about 1100°C, and an appropriate corresponding pressure in the range between about 0.01 MPa (0.1 bar) and about 5 MPa (50 bar)). Reaction 102 is endothermic and requires an energy inflow of about 213 kJ per mole of methane, given that the reactants are preheated to 400°C. In reaction 104, methane reacts with gaseous nickel chloride at temperatures in the range of about 800°C and about 1300°C (e.g., between about 850°C and about 1300°C, or about 1100°C), producing nickel, carbon, and hydrogen chloride. Reaction 104 can be carried out at a suitable corresponding pressure in the range between approximately 0.01 MPa (0.1 bar) and approximately 5 MPa (50 bar). Reaction 104 is slightly exothermic, releasing approximately 6 kJ of energy per mole of methane supplied to reaction 104. In reaction 106, unreacted methane is thermally decomposed, producing carbon and hydrogen gases. Reaction 106 is endothermic, cooling the product flow from 1100°C to 850°C. In some embodiments, the reduction of nickel in reaction 104 and the thermal decomposition of methane in reaction 106 occur simultaneously.

[0065] In the example shown in Figure 1, if reaction 102 occurs before reaction 104, then 0.5 moles of methane per mole of nickel chloride are decomposed in reaction 104, and 1.2 moles of methane per mole of nickel chloride are decomposed in reaction 106, resulting in a methane-to-nickel chloride molar ratio of 5:3.

[0066] Figure 3 is similar to the one described for Figure 2, but shows the methane decomposition by reduction of nickel chloride according to nickel chloride reduction reaction 104 in a reactor packed with a stationary nickel chloride plug, as a function of temperature. The reactor column length was 28 cm, and the methane-to-argon ratio (standard cubic centimeters / min) was 80:20. As seen in Figure 3, the initial conversion rate of methane to hydrogen chloride is temperature-dependent. The conversion rate increases until about half of the nickel chloride is consumed. Above about 850°C, the conversion of methane to hydrochloric acid is almost complete (e.g., about 100%). The conversion does not decrease even when the nickel chloride is consumed (i.e., when the reactor volume is almost empty). In other experiments, it has been observed that reaction 104 proceeds at about 10 times the rate of reaction 106.

[0067] Figure 4A is a scanning electron microscope (SEM) image of anhydrous nickel chloride powder 400 before sublimation in reaction 102. Figures 4B and 4C are low-magnification and high-magnification SEM images of nickel chloride after approximately half has been consumed in reaction 104, respectively. Figure 4B shows nickel chloride flakes 402, and Figure 4C shows nickel element particles 404 and carbon element flakes 406.

[0068] Figure 5 is a flowchart representing reaction scheme 500 for oxidizing the metal produced in reaction 104 of Figure 1 with concentrated hydrogen halide to produce hydrogen gas and the metal salt of Figure 1. Reaction scheme 500 typically occurs in solution. Examples of suitable solvents include water, alcohols (e.g., methanol, ethanol), other organic and inorganic solvents (e.g., dimethyl sulfoxide, thionyl chloride), or any mixture thereof. As in Figure 1, the metal salt is nickel chloride and the halide is a chloride. However, other metals and halides described for Figure 1 can also be selected to undergo the corresponding reactions in Figure 5.

[0069] In reaction scheme 500, the metal and carbon solids from reaction 104, and the carbon solid from reaction 106, if present, are mixed with a mixture containing the solvent and the hydrogen halide from reaction 104. In some embodiments, the products of reactions 104 and 106 are cooled (for example, to a temperature in the range of about 25°C and about 200°C) before initiating reaction 502 by contacting them with the hydrogen halide and solvent at a corresponding appropriate pressure (e.g., a pressure in the range of about 0.01 MPa (0.1 bar) and about 2 MPa (20 bar)). In one embodiment, the metal and carbon solids are supplied to a heated mixture containing the solvent and hydrogen halide. The hydrogen halide and metal react to produce hydrogen gas and metal salts dissolved in the solvent, which can almost deplete the hydrogen halide upon completion of the reaction. Generally, carbon does not react with the hydrogen halide and can therefore be removed by filtration in reaction zone 504. In some embodiments, the metal salt can be recovered from the solvent by sedimentation that occurs when the solution is re-acidified in zone 506 with the gaseous product of reaction 104. The settled metal salt is removed from the solvent by filtration in zone 508. The metal salt is typically solvated, but can also be brought into contact with gases from reactions 104 and 106 to produce anhydrous metal salt, gaseous hydrogen halide, and vaporized water along with hydrogen. The anhydrous metal salt can be supplied as a reactant in reaction 102 in reaction scheme 100, and the gas can be supplied to reaction zone 506. Hydrogen gas can be collected from reactions 502 and 106 (through zone 506).

[0070] In the example shown in Figure 5, nickel and carbon solids from reactions 104 and 106, along with gaseous hydrochloric acid from reaction 104, are mixed in solution, and according to reaction 502, nickel chloride and hydrogen gas are produced along with the carbon solid. Nickel and gaseous hydrochloric acid are typically cooled to a temperature in the range of about 25°C to about 200°C before reaction 502 begins. In 504, the carbon solid is filtered from the product mixture of reaction 502. In 506, nickel chloride hydrate settles by acidifying the remaining product mixture from reaction 502 with the gaseous products of reactions 104 and 106. In 508, the nickel chloride hydrate is separated from the aqueous hydrochloric acid, and the regenerated hydrochloric acid can be supplied to reaction 502. Nickel chloride hydrate can be dried by contacting it with the gases (hydrochloric acid and hydrogen) from reactions 104 and 106, and together with hydrogen, anhydrous nickel chloride, gaseous hydrochloric acid, and vaporized water (from the hydrate) can be produced. Anhydrous nickel chloride can be supplied to reaction 102 of reaction scheme 100, and the gas can be supplied to reaction zone 506. Hydrogen gas can be collected from reactions 502 and 106 (through zone 506).

[0071] Figure 6 is a flowchart illustrating the operations in an exemplary process 600 for hydrogen production according to the embodiments described herein. In process 600, M n+ X n represents a metal halide, where M is an alkaline earth metal (e.g., magnesium or calcium) or a transition metal (e.g., manganese, iron, cobalt, nickel, or copper), and X is a halogen (e.g., fluorine, chlorine, bromine, or iodine), and M n+ X n n is electrically neutral and is an integer. In some embodiments, the gaseous hydrocarbon includes one or more of methane, ethane, propane, butane, pentane, hexane, heptane, octane, and nonane or any isomers thereof. In some embodiments, the gaseous hydrocarbon includes natural gas. In one embodiment of process 600, M is nickel, X is chlorine, the hydrocarbon is methane, and n=2.

[0072] In 602, hydrocarbons are M n+ X n (g) is thermally decomposed in the presence of (g), producing gaseous and solid products. The molar ratio of hydrocarbons to metal halides is typically in the range of about 0.5 to about 25, and the residence time is typically in the range of about 0.1 seconds to about 20 seconds. Thermal decomposition typically occurs in a reactor at temperatures in the range of about 1000°C to about 1200°C. The gaseous product is a mixture containing hydrogen gas (H2) and hydrogen halides (HX), with H2 typically in the range of about 92 mol% to about 96 mol% and HCl typically in the range of about 4% to about 8%. The solid product is a mixture containing metal (M) and elemental form of carbon (C).

[0073] In 604, the gaseous and solid products are separated. In some embodiments, the products from 602 are cooled before separation in 604. In one embodiment, the products are fed into a heat exchanger (e.g., a regenerating heat exchanger) where the heat from the products is transferred to another flow (e.g., HX) in process 600.

[0074] In 606, the solid product from 604 reacts with HX (e.g., recycled from other flows in process 600 and / or heated by other flows in process 600, as discussed for 604) to produce a product mixture. The molar ratio of HX to M is typically in the range of about 1:1 to about 100:1. The reactor may be an adiabatic reactor. The reaction typically takes place in a reactor at temperatures in the range of about 900°C to about 1200°C. In some cases, the product is H2 + HX + M n+ X ncomprises (g)+C, HX contains a small amount of H₂ (e.g., less than about 5 mol%, or less than about 3 mol%), such that the total amount of H₂+HX comprises up to 4 mol% H₂ and at least 95 mol% HX. In some cases, the small amount of H₂ is removed from HX before reacting the solid product from 604 with HX, such that HX is substantially pure (with a purity of >99 mol% or >99.9 mol%).

[0075] At 608, the product mixture from 606 is cooled, and M n+ X n A solid product comprising a mixture of (s)+C and a gaseous product comprising a mixture of H₂+HX are produced, and the total amount of H₂+HX comprises up to 4% H₂ and at least 95 mol% HX. Cooling can be accomplished with a flash cooler that injects the gas stream into a vessel at a lower pressure to reduce its temperature. Cooling can also be accomplished using a heat exchanger. In some cases, the solid product is separated at 608, and M n+ X n A stream of (s) and a stream of C are produced. That is, M n+ X n No further downstream processing (e.g., processing at 612 to 616) is required to separate and C. At 610, the solid product and the gaseous product from 608 are separated. In one embodiment, the separation is accomplished using a ceramic candle filter.

[0076] At 612, the solid product from 610 is heated in a furnace to M n+ X n evaporate (s), thereby producing M n+ X n a mixture comprising (g)+C. At 614, C is removed from the 612 mixture. At 616, M from the 612 mixture n+ X n (g) is recycled to 602.

[0077] At 618, HX and H2 are separated from 610, resulting in a stream of HX and a stream of H2 products. In one embodiment, HX and H2 are separated by contacting a gaseous mixture with aqueous HX to capture the HX, leaving substantially pure H2 (e.g., >99% or >99.9% purity) as a stream of primary hydrogen products. At 620, the stream of HX from 618 is supplied to 606. At 622, the stream of H2 products from 618 exits process 600 as nearly pure hydrogen (e.g., >99 mol% or >99.9 mol% purity).

[0078] At 624, HX and H2 are separated from 604, resulting in a flow of HX and a flow of H2 products. At 626, HX from 624 is supplied to 606. At 628, the H2 products from 624 exit process 600.

[0079] In some embodiments, operations can be added to or omitted from process 600. In some embodiments, the order of operations in process 600 can be changed. In one embodiment, the solid product is separated in 608 or 610, M n+ X n A flow of (s) and a flow of C occur. That is, M n+ X n Further downstream processing (e.g., processing in 612-616) is not necessary to separate C, and M n+ X n And C is M n+ X n It separates as a solid before it evaporates.

[0080] Figure 7 is a process flow diagram representing an exemplary system 700 for performing hydrogen production according to process 600, where the molar ratio of methane to metal halide is approximately 0.5:1 to approximately 25:1. In the example described for Figure 7, the metal halide is nickel chloride and the gaseous hydrocarbon is methane (or natural gas). However, as discussed with respect to process 600, other metal halides and hydrocarbons can be used in a system similar to system 700. System 700 includes a hydrocarbon decomposition zone 702, a heat exchange zone 704, H2 separation zones 706, 706′, and a metal halide regeneration zone 708, which are described in more detail below. In Figure 7, solid flows are shown as solid lines. Unheated (or "low temperature") flows are shown as dotted lines. Heated (or "high temperature") flows are shown as dashed lines.

[0081] Flow 710 (CH4) is supplied to heater 712, producing flow 714 (CH4). Flow 716 (NiCl2(s)) is supplied to heater 718, producing flow 720 (NiCl2(g)). Flows 714 (CH4) and 720 (NiCl2(s)) are supplied to reactor 722 in a CH4:NiCl2 molar ratio in the range of approximately 10:1 to approximately 20:1 (e.g., approximately 13:1 to approximately 17:1 or approximately 14:1 to approximately 16:1). 2+ The gas-phase exothermic reduction and endothermic thermal decomposition of CH4 occur in reactor 722, as shown in equations 1 and 2. CH4+2NiCl2(g)→2Ni+C+4HCl ΔH°=-147kJ / mol CH4(1) CH4→C+2H2ΔH°=75kJ / mol CH4(2) [Examples]

[0082] Table 1 lists the CH4:NiCl2 molar ratio and the CH4 conversion rate to carbon according to formulas 1 and 2 for Examples 1 to 19. The CH4:NiCl2 molar ratio ranges from approximately 1 to approximately 20, the residence time ranges from approximately 5 seconds to approximately 20 seconds, and the CH4 conversion rate ranges from approximately 10% to approximately 100%. The residence time for Example 19 (conversion rate 95 mol%, CH4:NiCl2 molar ratio 6.08) was approximately 16 seconds. The residence time for Example 13 (conversion rate 88%, CH4:NiCl2 molar ratio 15.43) was approximately 8 seconds.

[0083] [Table 1]

[0084] From reactor 722, flow 724 (H2 + HCl + Ni + C) is supplied to heat exchange zone 704, where flow 724 is cooled by flow 726 (recycled HCl) in heat exchanger 728. Heat exchanger 728 may be a reheating heat exchanger. In heat exchanger 728, flow 726 cools flow 724 to a temperature in the range of about 150°C to about 250°C (e.g., about 200°C). In one embodiment, heat exchanger 728 is a multi-tube exchanger, and flow 724 is supplied to the tube side. Flow 730 (C + H2 + HCl + Ni) is supplied to filter 732, where the gaseous product (H2 + HCl) is separated from the solid product (C + Ni). In one embodiment, filter 732 is a candle filter.

[0085] Flow 734 (H2 + HCl) is fed to separator 736 in H2 separation zone 706, producing flow 738 (H2) and flow 740 (HCl). In one embodiment, separator 736 operates by spraying aqueous HCl (e.g., 20 wt% HCl at 25°C) onto flow 734 to capture HCl from flow 734. Flow 738 (nearly pure H2) exits system 700 from separator 736. Flow 740 (aqueous HCl) can be distilled (e.g., by pressure swing distillation) to produce anhydrous HCl. Flow 738 (purity >99.9 mol%) is the flow of primary hydrogen products. Flow 740 (HCl) is returned to heat exchanger 728 in flow 726.

[0086] From filter 732, flow 742 (Ni+C) is supplied to reactor 744 in the metal halide regeneration zone 708. Reactor 744 can be an adiabatic reactor or a heated reactor. The particle diameters of the Ni and C solids are typically in the range of about 0.1 μm to about 1 μm (e.g., about 0.1 μm to about 0.5 μm, or about 0.2 μm to about 0.4 μm). From heat exchanger 728, flow 746 (HCl) is supplied to heater 748. Flow 746 may contain a small amount (e.g., less than about 5%) of H2. From heater 748, flow 750 (HCl) is supplied to reactor 744 in an HCl:Ni molar ratio in the range of about 5:1 to about 50:1. In reactor 744, Ni reacts with HCl to produce NiCl2(g), as shown in Equation 3. Ni+2HCl→NiCl2(g)+H2ΔH°=110kJ / mol Ni (3) The HCl in flow 750 heats the solid from flow 742 to a temperature in reactor 744 in the range of approximately 1000°C to 1200°C, thereby promoting the formation of NiCl2(g) in reactor 744. In one embodiment, reactor 744 has a downflow design and receives co-feeds of HCl and Ni+C solid (e.g., simultaneous gas-solid flow in an adiabatic reactor with high-temperature HCl gas). The residence time in reactor 744 is typically in the range of approximately 5 seconds to approximately 30 seconds (e.g., approximately 10 seconds).

[0087] In some cases, flow 746 (and therefore flow 750) contains a small amount (e.g., less than about 5%) of H2. A corresponding molar amount of chlorine gas is added to flow 750 via flow 756. The chlorine gas reacts with the H2 in flow 750 to form excess HCl gas. This excess HCl gas is removed via flow 750′, leaving 750 as a flow of pure HCl (e.g., >99 mol% or >99.9 mol% purity). Flow 750′ is fed to separator 752 in the H2 separation zone 706′. In some embodiments, separator 752 is a chlorine-alkali electrolytic cell that produces pure hydrogen (flow 754) and chlorine (flow 756) from the HCl flow (flow 750′). Flow 754 (>99.9 mol% H2) can exit system 700 and mix with the primary hydrogen product flow 738 (>99.9 mol% H2).

[0088] From reactor 744, flow 758 (H2 + HCl + NiCl2(g) + C) enters condenser 760, where NiCl2(g) condenses to produce NiCl2(s). The heat from condenser 760 can be used to generate steam that powers H2 separation in one or both of the H2 separation zones 706 and 706'. Flow 762 (H2 + HCl + NiCl2(s) + C) enters filter 764, where solid products are separated from gaseous products. In one embodiment, filter 764 is a ceramic candle filter. Flow 766 (H2 + HCl) is mixed with flow 740 (HCl) and recycled to heat exchanger 728 in flow 726 (HCl). Flow 768 (NiCl2(s) + C) is recycled to heater 718 in hydrocarbon decomposition zone 702, where NiCl2(s) evaporates to produce NiCl2(g). Flow 770(C) exits the heater 718 as a solid carbon. In some cases, the heat from flow 770 is supplied to the heater 712 to heat flow 710, and flow 772(C) exits the system 700 as a cooled solid carbon.

[0089] Figure 8 is a schematic diagram showing the heater 718. The flow 716 (C + NiCl2(s)) enters the heater 718 through the inlet 802. Heat is supplied to evaporate the solid NiCl2, and it exits the heater 718 through the outlet 804 as NiCl2(g). The carbon bed 806 moving downwards is contacted by the heating element 808 and exits the heater 718 through the outlet 810 by gravity. In some cases, the carbon is contacted by a separating gas (e.g., a flow of HCl at a temperature in the range of approximately 900°C to approximately 1200°C) near the outlet 810, and residual NiCl2(g) is removed from the carbon. As the HCl flows over the mixture, the HCl replaces the gaseous NiCl2 in the solid, so that little or no NiCl2 is removed along with the solid carbon. The carbon exits the heater 718 as homogeneous hollow carbon particles with a diameter between approximately 225 nm and 275 nm (for example, between approximately 240 nm and 260 nm, or 250 nm).

[0090] Figure 9A is a transmission electron microscope image of carbon-coated nickel particles 900 before regeneration and evaporation of nickel chloride in heater 718. Figure 9B is a transmission electron microscope image of hollow carbon particles 902 produced after regeneration and evaporation of nickel chloride from the material in Figure 9A. Figures 9C and 9D are scanning electron microscope images of hollow carbon particles 902 (containing nickel particles 904) produced after regeneration and evaporation of nickel chloride from the material in Figure 9A, at 10,000x and 50,000x magnification, respectively. Elemental analysis shows that the total metal content of carbon is less than 100 ppm. Toxicity elution (TCLP) shows that the elutable nickel is less than 300 ppb.

[0091] In some embodiments, components of the system 700 (e.g., heaters, heat exchangers, filters) can be rearranged or removed. Other components may be added. One or more flows within the system 700 can be mixed, removed, or rerouted. Operating parameters may be modified to achieve desired results, such as hydrogen conversion rate or flow purity.

[0092] This disclosure includes details of many specific embodiments, which should not be construed as limitations on the scope of the subject matter or the scope of what is claimed, but rather as descriptions of features that may be specific to a particular embodiment. Certain features described in this disclosure in the context of a separate embodiment may also be performed in combination in a single embodiment. Conversely, various features described in the context of a single embodiment may also be performed individually or in any suitable subordinate combination in multiple embodiments. Furthermore, while the features described herein are described as acting in a particular combination, and may even be initially claimed as such, one or more features of a claimed combination may, in some cases, be removed from the combination, and the claimed combination may cover a subordinate combination or a variation of a subordinate combination.

[0093] Specific embodiments of the subject matter are described. Other embodiments, modifications, and rearrangements of the described embodiments are within the following claims, as will be apparent to those skilled in the art. Although the operations are shown in a specific order in the drawings or claims, this should not be understood as requiring that such operations be performed in a specific or sequential order shown, or that all illustrated operations be performed, in order to achieve the desired result (some operations may be considered optional).

[0094] Therefore, the exemplary embodiments described above do not define or limit this disclosure. Other modifications, substitutions, and alterations are also possible without departing from the spirit and scope of this disclosure.

Claims

1. A reaction method, A sublimation step of sublimating a metal salt containing a metal and a halide to produce a gas-phase metal salt containing the metal and the halide, The step includes contacting the aforementioned gas-phase metal salt with a gas-phase hydrocarbon, The aforementioned contact step is, A step of reducing the gas-phase metal salt using the gas-phase hydrocarbon to produce hydrogen halide containing the metal in elemental form, carbon in elemental form, and the halide, A method comprising the step of decomposing the gaseous hydrocarbon to produce elemental forms of carbon and hydrogen gas.

2. The method according to claim 1, wherein the contact step occurs at a temperature in the range of about 800°C to about 1300°C, or between about 850°C and about 1300°C.

3. The method according to claim 1, wherein the metal comprises one or more of magnesium, calcium, manganese, iron, cobalt, nickel, and copper.

4. The method according to claim 1, wherein the halogenated material comprises one or more of fluorides, chlorides, bromides, and iodides.

5. The method according to claim 1, wherein the gaseous hydrocarbon includes natural gas.

6. The method according to claim 1, wherein the gaseous hydrocarbon comprises one or more of methane, ethane, propane, butane, pentane, hexane, heptane, octane, and nonane, or any isomers thereof.

7. The method according to claim 1, wherein the sublimation step is carried out at a pressure in the range of about 0.01 MPa (0.1 bar) and about 5 MPa (50 bar).

8. The method according to claim 1, wherein the contact step occurs at a pressure in the range of about 0.01 MPa (0.1 bar) and about 5 MPa (50 bar).

9. A method according to claim 1, further comprising a pyrolysis step of pyrolyzing the gaseous hydrocarbon to produce the carbon and hydrogen gases.

10. The method according to claim 9, wherein the pyrolysis step is catalyzed by the metal.

11. The method according to claim 9, wherein the heat for thermal decomposition is supplied by electricity.

12. A method according to claim 1, further comprising the step of contacting the metal with the hydrogen halide to produce a gaseous metal salt and hydrogen gas.

13. A method according to claim 12, further comprising the step of heating the hydrogen halide before contacting the metal with the hydrogen halide.

14. The method according to claim 13, wherein the step of heating the hydrogen halide comprises the step of heating the hydrogen halide to a temperature of at least 1000°C.

15. The method according to claim 13, wherein the step of contacting the metal with the hydrogen halide at a high temperature to produce the metal salt is carried out in an adiabatic reactor.

16. A method according to claim 12, further comprising the step of condensing the metal salt to produce a solid phase of the metal salt.

17. The method according to claim 16, wherein the solid phase of the metal salt is in the form of particles, and the particles are at least partially coated with carbon.

18. A method according to claim 17, further comprising the step of contacting the metal salt with hydrogen chloride having a temperature of at least 1000°C to produce a gaseous metal halide and particulate carbon material.

19. The method according to claim 18, wherein the particulate carbon material comprises a large number of hollow carbon particles.

20. The method according to claim 19, wherein the hollow carbon particles have a diameter in the range of about 200 nm to about 300 nm.

21. The method according to claim 20, wherein the particulate carbon material contains less than 100 ppm by weight of metal.

22. The method according to claim 1, wherein the halide is a chloride and the metal is nickel.

23. The method according to claim 1, wherein the gaseous hydrocarbon comprises methane.

24. The method according to claim 1, wherein the sublimation step occurs prior to the contact step.

25. A method according to claim 1, wherein the sublimation step includes advancing the metal salt toward the reaction zone of the reactor together with the gaseous hydrocarbon.

26. A method according to claim 25, further comprising the step of heating the reaction zone to a temperature in the range of about 800°C and about 1300°C.

27. The method according to claim 26, wherein the step of heating the reaction zone is achieved using electricity.

28. A method according to claim 27, wherein the power is used to generate radiant heat.

29. The method according to claim 28, wherein the radiant heat is supplied by an electric furnace or an induction heating element.

30. The method according to claim 1, wherein the sublimation step and the contact step occur simultaneously in the reaction zone of the reactor.

31. The method according to claim 1, wherein the metal salt is anhydrous.

32. A method for generating hydrogen gas, A contact step involves contacting a gaseous metal halide with a gaseous hydrocarbon to produce gaseous products containing hydrogen and hydrogen halides, as well as solid products containing metal and carbon. The steps of separating the hydrogen from the hydrogen halide, and The steps include bringing the hydrogen halide into contact with the metal to generate the gaseous metal halide, Includes, The aforementioned contact step is, A step of reducing the metal halide using the hydrocarbon to produce hydrogen halide containing the metal in elemental form, carbon in elemental form, and a halide; A method comprising the step of decomposing the hydrocarbon to produce carbon and hydrogen in elemental forms.

33. A method according to claim 32, further comprising the step of contacting the hydrogen halide with a metal, and then cooling the gaseous metal halide to produce a solid-phase metal halide.

34. A method according to claim 33, further comprising the step of heating the solid-phase metal halide to produce the gas-phase metal halide.

35. A method according to claim 34, further comprising the step of contacting the gas-phase metal halide with the gas-phase hydrocarbon.

36. A method according to claim 32, further comprising the step of separating the gaseous product from the solid product.

37. A method according to claim 32, further comprising the step of heating the hydrogen halide to a temperature of at least about 1000°C before contacting the hydrogen halide with the metal.

38. A method according to claim 32, further comprising the step of contacting the solid product with the hydrogen halide to produce the gas phase metal halide and the carbon.

39. A method according to claim 38, further comprising the step of condensing the metal halide to produce a solid mixture containing the metal halide and the carbon.

40. The method according to claim 39, wherein the solid mixture comprises particles of the metal halide coated with a portion of the carbon.

41. A method according to claim 40, further comprising the step of contacting the solid mixture with hydrogen chloride having a temperature of at least 1000°C to produce the gas phase metal halide and particulate carbon material.

42. The method according to claim 41, wherein the particulate carbon material comprises a large number of hollow carbon particles.

43. The method according to claim 42, wherein the hollow carbon particles have a diameter in the range of about 200 nm to about 300 nm.

44. The method according to claim 43, wherein the particulate carbon material contains less than 100 ppm by weight of the metal.

45. A hydrogen generation system, A first reactor configured to react gaseous reactants, A heat exchanger configured to receive a mixture of gas and solid reaction products from the first reactor and to supply solid and gas inflows to the second reactor, The second reactor is configured to react the solid inflow from the heat exchanger with the gas inflow, A separator configured to receive the gas outflow from the heat exchanger and to supply a gas inflow to the heat exchanger, A condenser configured to condense the reaction product from the second reactor, A third reactor is configured to receive solid products from the cooler, evaporate the solid products to produce gaseous products, and supply the gaseous products to the first reactor, A system equipped with these features.

46. A system according to claim 45, wherein the first reactor, the second reactor, or both are configured to operate at temperatures in the range of about 800°C and about 1200°C.

47. The system according to claim 45, wherein the second reactor is an adiabatic reactor.

48. The system according to claim 45, wherein the third reactor is configured to separate the components of the solid product from the condenser.

49. A system according to claim 45, further comprising an additional separator configured to remove hydrogen from the gas inflow from the heat exchanger.

Citation Information

Patent Citations

  • Method of carbon dioxide-free hydrogen production from hydrocarbon decomposition over metal salts

    US20170240421A1

  • Processes for producing hydrogen from hydrocarbon feed sources

    WO2008157047A1

  • Hydrogen generation

    WO2013111015A1

  • A process for producing hydrogen and graphitic carbon from hydrocarbons

    WO2016154666A1

  • Process for the production of hydrogen

    WO2018141911A1