Method for manufacturing microporous polyolefin resin sheet and device for manufacturing microporous polyolefin resin sheet

JPWO2022168546A5Active Publication Date: 2024-10-04TORAY INDUSTRIES INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2022508806
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2022-01-12
Filing Date
2022-01-12
Publication Date
2024-10-04
Estimated Expiration
2042-01-12

AI Technical Summary

Technical Problem

Current methods for producing microporous polyolefin resin sheets fail to prevent droplet scattering onto casting equipment and sheet materials due to airflow in the vacuum chamber, leading to defects and tearing of the sheets.

Method used

The method involves optimizing the distances and ratios of the exhaust nozzle openings to the sheet material, using a sealing material to close the gap between the decompression chamber and casting device, and adjusting the suction width to suppress airflow and droplet scattering, ensuring stable sheet production.

Benefits of technology

This approach effectively reduces droplet scattering and sheet defects, enabling the stable manufacture of high-quality microporous polyolefin resin sheets by maintaining a controlled vacuum environment and preventing airflow disruptions.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The present invention provides a method and a device for manufacturing a microporous polyolefin resin sheet with which it is possible to manufacture a high-quality sheet in a stable manner. This method for manufacturing a microporous polyolefin resin sheet is a method for manufacturing a sheet in which a sheet material containing a polyolefin resin and a diluent is discharged from a discharge port of a mouthpiece towards a cast device, and in a decompression chamber, the space between the sheet material and the cast device is covered, air is suctioned, and the sheet material is brought into intimate contact with the cast device. The suctioning of the air in the decompression chamber is performed from exhaust nozzles disposed on the outer side relative to the two width-direction edge sides of the sheet material so that opening parts face each other; and the relationships Y1 / H ≤ 0.13 and 0.25 ≤ Y2 / H ≤ 0.75 are satisfied, where H represents the shortest distance from the discharge port of the mouthpiece to the outer peripheral surface of the cast device, Y1 represents the shortest distance from the upper edge side of the opening parts to an edge part of the sheet material, and Y2 represents the shortest distance from the lower edge of the opening parts to an edge part of the sheet material.
Need to check novelty before this filing date? Find Prior Art

Description

Method for producing microporous polyolefin resin sheet and apparatus for producing microporous polyolefin resin sheet

[0001] The present invention relates to a method and an apparatus for producing a microporous polyolefin resin sheet.

[0002] First, a typical method for producing a microporous polyolefin resin sheet will be described. Fig. 6 is a schematic diagram of a typical apparatus for producing a microporous polyolefin resin sheet. The apparatus shown in Fig. 6 includes a die 1 having a discharge port 5 for discharging a sheet material 3 containing a polyolefin resin and a diluent; a casting device 2 that cools and solidifies the sheet material 3 discharged from the discharge port 5 while conveying it; and a decompression chamber 4 disposed upstream of the discharge port 5 in the sheet conveyance direction, covering a space 13 between the sheet material 3 and the casting device 2, and drawing air to form a decompressed space. A known sheet production method involves discharging the sheet material 3 from the discharge port 5 of the die 1 toward the casting device 2, drawing air from the space 13 through openings 9 of exhaust nozzles 12 disposed outward from both ends of the sheet material 3 in the sheet width direction, thereby bringing the sheet material 3 into close contact with the casting device 2, and cooling and solidifying the sheet material 3 while conveying it through the casting device 2. In addition, in general, in order to prevent contact between the casting device 2 and the decompression chamber 4 while suppressing the inflow of outside air, a small gap is formed between the casting device 2 and the side wall 4a of the decompression chamber 4 that covers the surface perpendicular to the sheet width direction of the space 13.

[0003] Incidentally, Patent Document 1 discloses a resin sheet manufacturing apparatus as a technology for improving sheet quality. Patent Document 1 discloses a resin sheet manufacturing apparatus equipped with a shielding plate near the edge of the sheet material for the purpose of suppressing thickness unevenness due to membrane vibration of the sheet material. FIG. 7 is a schematic view of the resin sheet manufacturing apparatus of Patent Document 1 observed from the vertical top. As shown in FIG. 7, in the manufacturing apparatus of Patent Document 1, the rectifying effect of the shielding plate 6 suppresses the formation of vortices at the edge of the sheet material 3, suppressing membrane vibration of the sheet material and reducing thickness unevenness of the resin sheet.

[0004] Japanese Patent Application Publication No. 10-180847

[0005] With the recent increase in resin sheet production, there is a strong demand for increasing the discharge rate of sheet material and extending the continuous film production time. However, increasing the discharge rate of sheet material and extending the continuous film production time also increases the chances that low-molecular-weight components in the sheet material, diluents, and gases derived from additives will adhere to the nozzle of the die and liquefy (hereinafter referred to as droplets). When these droplets adhere to the casting equipment or sheet material due to the airflow in the decompression chamber, they can cause defects or tearing in the sheet. However, no methods have been proposed to prevent droplet scattering or to suppress it.

[0006] Therefore, the present invention provides a method and apparatus for producing a microporous polyolefin resin sheet that can stably produce high-quality sheets by suppressing the scattering of droplets onto the casting device or sheet material due to airflow generated in the decompression chamber.

[0007] The present invention, which solves the above-mentioned problems, provides a method for producing a microporous polyolefin resin sheet, comprising: discharging a sheet material containing a polyolefin resin and a diluent from a discharge port of a die toward a casting device; covering the space between the sheet material and the casting device with a decompression chamber located upstream of the discharge port in the sheet conveyance direction; sucking air from the decompression chamber to create a decompressed space; bringing the sheet material into close contact with the casting device; and cooling and solidifying the sheet material while conveying it with the casting device; wherein the air is sucked from the decompression chamber using exhaust nozzles located so that their openings face outward from both widthwise ends of the sheet material; and wherein, where H is the shortest distance from the discharge port of the die to the outer peripheral surface of the casting device, Y1 is the shortest distance from the upper end of the opening to the end of the sheet material, and Y2 is the shortest distance from the lower end of the opening to the end of the sheet material, the relationships Y1 / H≦0.13 and 0.25≦Y2 / H≦0.75.

[0008] In the method for producing a microporous polyolefin resin sheet of the present invention, it is preferable that the suction width L1, which is the horizontal distance from the edge of the sheet material 3 at the upper end of the exhaust nozzle opening to the upstream end in the sheet conveying direction when observed from the outside in the sheet width direction, is L1 / H≦0.38. In the method for producing a microporous polyolefin resin sheet of the present invention, it is preferable that the sealing gap, which is the gap located directly below the exhaust nozzle opening, among the gaps between the side walls of the decompression chamber perpendicular to the sheet width direction and the casting device is physically sealed with a sealing material. In the method for producing a microporous polyolefin resin sheet of the present invention, it is preferable that the sealing material is an elastic material and is pressed against the casting device to seal the sealing gap. In the method for producing a microporous polyolefin resin sheet of the present invention, it is preferable that the sealing material is pressed against the decompression chamber with a pressing member to fix it.

[0009] Furthermore, the present invention provides a microporous polyolefin resin sheet manufacturing apparatus that solves the above-mentioned problems, comprising: a die having a discharge port for discharging a sheet material containing a polyolefin resin and a diluent; a casting device that cools and solidifies the sheet material discharged from the discharge port while transporting it; and a decompression chamber that is arranged upstream of the discharge port in the sheet transport direction, covers the space between the sheet material and the casting device, and draws air into the decompression space. The decompression chamber is arranged outside both ends of the sheet material in the width direction so that exhaust nozzles that draw air from the decompression chamber face each other, and is arranged so that Y1 / H≦0.13 and 0.25≦Y2 / H≦0.75, where H is the shortest distance from the discharge port of the die to the outer peripheral surface of the casting device, Y1 is the shortest distance from the upper end of the exhaust nozzle opening to the edge of the sheet material, and Y2 is the shortest distance from the lower end of the exhaust nozzle opening to the edge of the sheet material.

[0010] In the apparatus for producing a microporous polyolefin resin sheet of the present invention, the die, the casting device, and the exhaust nozzle are preferably arranged so that the suction width L1, which is the horizontal distance from the edge of the sheet material 3 at the upper end of the opening of the exhaust nozzle to the upstream end in the sheet conveying direction when observed from the outside in the sheet width direction, satisfies L1 / H≦0.38. In addition, the apparatus for producing a microporous polyolefin resin sheet of the present invention preferably includes a sealant that physically closes a seal gap, which is a gap located directly below the opening, among gaps formed between the side wall of the decompression chamber perpendicular to the sheet width direction and the casting device.

[0011] In the apparatus for producing a microporous polyolefin resin sheet of the present invention, the sealing material is preferably an elastic material that is pressed against the casting device to close the sealing gap, and the apparatus for producing a microporous polyolefin resin sheet of the present invention preferably includes a pressing member that presses and fixes the sealing material against the decompression chamber.

[0012] According to the polyolefin resin sheet manufacturing method and manufacturing apparatus of the present invention, high-quality sheets can be stably manufactured by suppressing the scattering of droplets onto the casting device or sheet material due to the air flow in the decompression chamber.

[0013] 5A is a schematic diagram of an embodiment of the microporous polyolefin resin sheet manufacturing apparatus of the present invention, observed from downstream in the sheet conveying direction. It is a partially enlarged cross-sectional view perpendicular to the vertical direction along line X-X in FIG. 1. It is a diagram showing a state in which Y1 / H is increased from the state in FIG. 2. It is a schematic diagram of an embodiment of the microporous polyolefin resin sheet manufacturing apparatus of the present invention, observed from the sheet width direction. It is a diagram explaining the sealing material and pressing member arranged between the casting device and the decompression chamber of the microporous polyolefin resin sheet manufacturing apparatus of FIG. 1. It is a vertical cross-sectional view taken along line Y-Y in FIG. 5A. It is a vertical cross-sectional view taken along line Z-Z in FIG. It is a graph showing the shortest distance from the opening to the edge of the sheet material in each example and each comparative example. It is a schematic diagram of a general microporous polyolefin resin sheet manufacturing apparatus. It is a schematic diagram of the resin sheet manufacturing apparatus of Patent Document 1, observed from the vertical top.

[0014] [Terminology] The meanings of each term in the present invention are explained below. "Sheet material" refers to the material that constitutes the sheet. Examples of sheet materials include polyolefin solution resins prepared by mixing a polyolefin resin, such as polyethylene, polypropylene, polystyrene, or polymethylpentene, with a diluent and then heating and melting the mixture. The diluent is not particularly limited as long as it can be mixed or dissolved in the polyolefin resin. Materials that are miscible with the polyolefin in the melt-kneaded state but solid at room temperature may also be used. Examples of such solid diluents include stearyl alcohol, ceryl alcohol, and paraffin wax. To prevent unevenness during stretching and to allow for subsequent application, the diluent is preferably liquid at room temperature. Examples of liquid diluents include aliphatic, cycloaliphatic, or aromatic hydrocarbons such as nonane, decane, decalin, paraxylene, undecane, dodecane, and liquid paraffin, as well as mineral oil fractions with corresponding boiling points, and phthalate esters that are liquid at room temperature, such as dibutyl phthalate and dioctyl phthalate. Liquid paraffin is even more preferable for obtaining a stable gel-like sheet. The viscosity of the liquid diluent is preferably 20 to 200 cSt at 40°C. The blending ratio of the polyolefin resin and the diluent is preferably 10 to 50% by mass of the polyolefin resin and 50 to 90% by mass of the diluent, with the total of the polyolefin resin and the diluent being 100% by mass, from the viewpoint of improving the moldability of the extrudate. The uniform melt-kneading process for the sheet material is not particularly limited, but examples include a calender, various mixers, and an extruder equipped with a screw.

[0015] A "casting device" refers to a device that transports sheet material discharged from the nozzle of a die downstream while cooling and solidifying it by tightly adhering it to the die. The form is not particularly limited, but examples include rolls and belts. The "width direction" refers to the direction that corresponds to the width direction of the sheet material when it is formed into a sheet by the die. The "sheet transport direction" refers to the direction in which the casting device transports the sheet. The downstream side is the transport destination, and the opposite is the upstream side. A "reduced pressure space" refers to the space formed between the sheet material and the casting device, which is covered by a reduced pressure chamber and maintains a negative pressure. A "reduced pressure chamber" refers to a device that covers the space between the sheet material and the casting device and reduces the pressure to bring the sheet material into close contact with the casting device. Typically, the pressure within the reduced pressure chamber is between -1500 Pa and -50 Pa relative to atmospheric pressure. The pressure within the reduced pressure chamber may also be controlled according to the film production conditions. An "opening" refers to a portion of the exhaust nozzle that draws air from inside the reduced pressure chamber. The shape of the opening is not particularly limited, but examples include square, rectangular, trapezoidal, circular, and elliptical shapes. The opening may be subjected to a surface treatment such as nickel plating, chrome plating, or zinc plating. The suction power source is not particularly limited, but examples include a blower and a vacuum pump. The "side wall" refers to the side surface of the decompression chamber perpendicular to the sheet width direction.

[0016] Next, the polyolefin resin sheet manufacturing apparatus and manufacturing method of the present invention will be described in detail with reference to the drawings. However, the present invention is not limited to the embodiments described here. Note that components having the same uses and functions as those in the prior art may be designated by the same reference numerals.

[0017] Referring to FIG. 1 , the influence of the dimensions of the opening 9 of the exhaust nozzle 12 of the decompression chamber 4 on the airflow within the decompression chamber 4 will be described. FIG. 1 is a schematic diagram of one embodiment of the polyolefin resin sheet manufacturing apparatus of the present invention, observed from upstream in the sheet conveyance direction. In the figure, symbols Y1 and Y2 represent the shortest distances from the opening 9 to the edge of the sheet material 3, with Y1 representing the shortest distance at the upper end of the opening 9 and Y2 representing the shortest distance at the lower end of the opening 9. Symbol H represents the shortest distance from the discharge port 5 of the die 1 to the outer peripheral surface of the casting device 2. The length of H is determined by the film-forming conditions. However, if the opening 9 is small, clogging due to droplets or the like can cause unstable suction. Therefore, from the viewpoint of ensuring a sufficient height from the upper end to the lower end of the opening 9, H is preferably 10 mm or more, more preferably 30 mm or more. After extensive research, the present inventors have found that Y1 / H and Y2 / H, which are obtained by normalizing Y1 and Y2 with H, affect the airflow within the decompression chamber 4 and ultimately cause droplets to scatter within the decompression chamber 4.

[0018] The pressure and airflow near the edge of the sheet material 3 will be described with reference to Figures 2 and 3. Figure 2 is a partially enlarged cross-sectional view perpendicular to the vertical direction along line X-X in Figure 1, showing the pressure near the edge of the sheet material 3 using contour lines. Figure 3 is a contour line showing the pressure near the edge of the sheet material 3 when the distance Y1 is longer than in the state shown in Figure 2 (when H is the same and Y1 / H is larger). Here, specific numerical values ​​of the pressure will be given to accurately convey the gist of the present invention, but these values ​​are merely examples and do not limit the scope of the present invention.

[0019] 2, the pressure at each location is assumed to be atmospheric pressure near the end (point A) of the sheet material 3 on the downstream side in the sheet conveying direction, (atmospheric pressure -300) Pa near the end (point B) of the sheet material 3 on the inside side of the decompression chamber 4, (atmospheric pressure -600) Pa downstream (point C) of the opening 9, and (atmospheric pressure -400) Pa near the end (point D) of the sheet material 3 on the exhaust nozzle 12 side. In this case, the pressure contours are as shown in FIG. 2, and according to the Navier-Stokes equation, air has the property of flowing from high pressure to low pressure, so most of the air flows to point C, where the pressure is lower than point A, like air flow 8a, that is, to the opening 9 of the exhaust nozzle 12.

[0020] If the distance Y1 is longer and Y1 / H is larger than in the state shown in Figure 2, the pressure gradient from point A to point C becomes gentler, and the pressure at point D becomes higher than in the state shown in Figure 2, to (atmospheric pressure - 200) Pa. This results in a pressure distribution as shown in Figure 3, and some air flows from point A through point D to point B, where the pressure is lower, as airflow 8b, i.e., into decompression chamber 4. This airflow 8b scatters droplets 7 near the discharge port 5 of die 1 into the main body of decompression chamber 4, where they adhere to the casting device 2 and sheet material 3, causing defects or tearing in the sheet.

[0021] Furthermore, if the shortest distance Y2 from the lower end of the opening 9 to the edge of the sheet material 3 is small, or the shortest distance H from the discharge port 5 of the die 1 to the outer peripheral surface of the casting device 2 is large, and Y2 / H is too small, the decompression chamber 4 becomes more airtight, the pressure inside the decompression chamber 4 becomes lower than the pressure near the end of the sheet material 3 on the exhaust nozzle 12 side, and an airflow 8b flows into the decompression chamber 4 from the downstream side in the sheet conveyance direction, via the edge of the sheet material 3, as in the case of Figure 3. On the other hand, if the shortest distance Y2 from the lower end of the opening 9 to the edge of the sheet material 3 is large, or the shortest distance H from the discharge port 5 of the die 1 to the outer peripheral surface of the casting device 2 is small, and Y2 / H is too large, a vortex is generated near the edge of the sheet material 3, and the turbulent pressure and airflow cause the droplets 7 to scatter.

[0022] As a result of further experiments and theoretical calculations, the inventors have found that by satisfying Y1 / H≦0.13 and 0.25≦Y2 / H≦0.75, the pressure at point B is stably higher than that at point D as shown in Figure 2, eliminating airflow within the decompression chamber 4, preventing droplets 7 from scattering into the main body of the decompression chamber 4, and suppressing adhesion of droplets 7 to the casting apparatus 2 and sheet material 3. More preferably, Y1 / H≦0.05.

[0023] In order to achieve Y1 / H≦0.13 and 0.25≦Y2 / H≦0.75, it is possible to design the decompression chamber 4 taking into consideration the amount of sheet material 3 discharged from the nozzle 1, the shortest distance H from the discharge outlet 5 of the nozzle 1 to the outer peripheral surface of the casting device 2, the amount of suction from the exhaust nozzle 12, etc., but it is preferable to make the side wall 4a of the decompression chamber 4 perpendicular to the sheet width direction movable in the width direction of the sheet material 3 and adjust Y1 and Y2.

[0024] Please refer to FIG. 4. FIG. 4 is a schematic diagram of one embodiment of the polyolefin resin sheet manufacturing apparatus of the present invention, observed from the sheet width direction. In reality, the sheet material 3 is obscured by the decompression chamber 4, but FIG. 4 illustrates the sheet material 3 as being observable through the decompression chamber 4 for easier understanding of the present invention. The suction width L1 in the figure is the horizontal distance from the edge of the sheet material 3 at the upper end of the opening 9 of the exhaust nozzle 12 to the upstream end in the sheet conveyance direction, as observed from the outside in the sheet width direction. In the polyolefin resin sheet manufacturing method of the present invention, it is preferable to set L1 / H≦0.38. Even if L1 / H is greater than 0.38, the effects of the present invention can be achieved by setting Y1, Y2, and H within the above-mentioned ranges. However, by setting L1 / H to 0.38 or less, the amount of air suctioned from within the main body of the decompression chamber 4 is reduced, and the pressure inside the decompression chamber 4 can be increased, thereby suppressing the airflow from the downstream side in the sheet conveyance direction through the edge of the sheet material 3 into the decompression chamber 4. 1 and 4, the pressure in the main body of the decompression chamber 4 is not reduced by a vacuum pump or the like from the main body of the decompression chamber 4, and the space 13 within the main body of the decompression chamber 4 is made into a reduced pressure space only by the exhaust nozzle 12, but the inside of the main body of the decompression chamber 4 may also be reduced by a vacuum pump. To adjust Y1 and Y2, it is preferable to reduce the pressure in the main body of the decompression chamber 4 only by the exhaust nozzle 12, without reducing the pressure by a vacuum pump or the like.

[0025] Referring again to Figure 1, the seal gap 14 in the figure is the gap between the side wall 4a of the vacuum chamber 4 perpendicular to the sheet width direction and the casting device 2, and is located directly below the opening 9 of the exhaust nozzle 12. As shown in Figure 1, in the method for producing a polyolefin resin sheet of the present invention, it is preferable to close the seal gap 14 with a seal material 10. Although the effects of the present invention can be obtained without this seal material 10, providing the seal material 10 eliminates airflow that would flow through the seal gap 14 and disrupt the pressure balance near the edge of the sheet material 3, thereby suppressing the scattering of droplets 7 into the vacuum chamber. The material of the seal material 10 is not particularly limited, but examples include resin, rubber, and ceramics.

[0026] Furthermore, in the method for producing a polyolefin resin sheet of the present invention, it is preferable that the sealing material 10 is an elastic material, and that the sealing material 10 is pressed against the casting device 2 to close the sealing gap 14. By pressing the elastic sealing material 10 against the casting device 2, the sealing material 10 is deformed by the compressive load, and even small gaps with the casting device 2 can be prevented. More preferably, the sealing material 10 is a non-conductive, porous resin or rubber that does not impart conductivity to the product even if wear powder is mixed into the product. Furthermore, the hardness of the sealing material 10 is preferably Shore E10 to 35, which can impart sealing properties under low load. More preferably, it is Shore E25 to 35, which minimizes distortion due to friction with the casting device 2.

[0027] The method for fastening the sealing material 10 is not particularly limited, and examples include a method of directly fastening the sealing material 10 to the sidewall 4a with multiple bolts. However, care must be taken when fastening the sealing material 10, as friction with the casting device 2 can cause distortion or misalignment, preventing the sealing function from being fully realized. If the sealing material 10 is directly fastened with bolts, the fastening may be insufficient, for example, in a narrow gap between the exhaust nozzle 12 and the casting device 2, resulting in distortion or misalignment of the sealing material 10. Therefore, in the polyolefin resin sheet manufacturing method of the present invention, it is preferable to fasten the sealing material 10 to the decompression chamber 4 using a presser member 11. Figures 5A to 5C are diagrams illustrating the sealing material 10 and presser member 11 arranged between the casting device 2 and the decompression chamber 4 of the microporous polyolefin resin sheet manufacturing apparatus of Figure 1. As shown in Figures 5A to 5C, the sealing material 10 is preferably fastened with bolts 15 via the presser member 11. Even in a narrow gap between the exhaust nozzle 12 and the casting device 2 where a bolt 15 cannot be placed, as shown in FIG. 5B , the sealing material 10 is fixed over the entire surface that contacts the pressing member 11, thereby suppressing distortion and misalignment, and allowing the sealing material 10 to stably seal the sealing gap 14. The shape of the pressing member 11 is not particularly limited, and an L-shaped plate that also covers the top of the sealing material 10 as shown in FIGS. 5A and 5C is preferred, but a flat plate may also be used. Furthermore, the frictional force of the contact surface with the sealing material 10 may be increased to prevent misalignment of the sealing material 10. For example, protrusions may be provided, the surface roughness may be increased, or an adhesive may be applied.

[0028] Below, we present examples of polyolefin resin sheet production using the polyolefin resin sheet production method of the present invention. [Example 1] A polyolefin resin sheet was actually produced using the polyolefin resin sheet production method, and the results of evaluating defects due to droplet scattering are described. Specific sheet production conditions and defect evaluation methods in this embodiment are as follows. (1) Sheet Material: High-density polyethylene (HDPE): viscosity 1000 Pa·s. Here, viscosity was measured at a shear rate of 100 / s and a temperature of 200°C according to the method of JIS K7117-2. Liquid paraffin (LP): kinematic viscosity 50 cSt (at 40°C). The blend ratio of HDPE to LP was HDPE:LP = 30:70 by mass. (2) Extrusion: The sheet material was extruded using an extruder at a flow rate of 250 kg / h, passed through a gear pump and a filter, and then fed to a die. The temperature of the device up to the die was 220°C. (3) Die: The sheet material was discharged from a 500 mm wide discharge port with a 2 mm gap and formed into a sheet. The amount of LP volatilization from the discharged sheet was measured and found to be approximately 100 g / h. (4) Casting Device: The sheet was brought into close contact with a sheet forming roll rotating at a temperature of 35°C and a speed of 10 m / min, and then cooled and solidified. The die's discharge port was installed directly above the center of the sheet forming roll, at a position where the shortest distance H from the die's discharge port to the outer peripheral surface of the sheet forming roll was 40 mm. (5) Decompression Chamber: The decompression chamber was installed upstream of the die's discharge port in the conveying direction and was shaped to cover the space between the sheet material discharged from the discharge port and the casting device. Exhaust nozzles were arranged opposite each other on the wall surfaces at both ends of the decompression chamber, and the opening of the exhaust nozzle was rectangular with the long side in the horizontal direction, with the long side being 70 mm and the short side being 32 mm. When the die was set under film-forming conditions, the distance from the die outlet to the upper end of the opening was 3 mm, and the distance from the lower end of the opening to the sheet forming roll was 5 mm. In this state, the inside of the decompression chamber was evacuated to −600 Pa from atmospheric pressure using a blower connected to the opening.The decompression chamber was equipped with a mechanism for adjusting the position of the wall surfaces at both ends, and while the sheet material was being discharged from the nozzle of the die, the adjustments were made so that Y1 was 4 mm (Y1 / H = 0.1), Y2 was 20 mm (Y2 / H = 0.5), and L1 was 16 mm (L1 / H = 0.4). The decompression chamber was also positioned so that the seal gap was 1 mm. (6) Defect Detection Device Using the inspection device MaxEye. Impact (Hutec Co., Ltd.), the number of defects caused by droplet scattering was counted on the sheet (width 423 mm, length 100 m) collected under the above conditions. The number of defects was 5.

[0029] Examples 2 to 6, Comparative Examples 1 to 5 Sheets were collected in the same manner as in Example 1, except that the dimensions were changed as shown in Table 1, and the number of defects was inspected.

[0030] Example 7 Sheets were collected in the same manner as in Example 1, except that a sealing material (polytetrafluoroethylene, Shore hardness D55) was fixed to a decompression chamber with bolts to physically seal the seal gap, and the number of defects was inspected.

[0031] [Example 8] Sheets were collected in the same manner as in Example 7, except that the sealing material was made of elastic silicone sponge rubber (Shore hardness E30), the sealing material was pressed against a casting device and fixed to a decompression chamber with bolts, and the sealing gap was sealed, and the number of defects was inspected.

[0032] [Example 9] Sheets were collected and inspected for the number of defects in the same manner as in Example 8, except that the sealing material was pressed and fixed to the decompression chamber using a pressing member (a flat plate made of SUS304 and having a thickness of 2 mm). The manufacturing conditions and the number of defects that occurred in the sheets for Examples 1 to 6 and Comparative Examples 1 to 5 are summarized in Tables 1 and 2, respectively.

[0033]

[0034]

[0035] [Evaluation Results] The relationship between Y1 / H and Y2 / H in each Example and Comparative Example will be described with reference to FIG. 6. FIG. 6 is a graph showing the positions of Y1 / H and Y2 / H for each Example and Comparative Example, with Y1 / H on the vertical axis and Y2 / H on the horizontal axis. Here, ◯ indicates Examples 1 to 5, × indicates Comparative Examples 1 to 5, and the dotted line indicates the range satisfying the conditions "Y1 / H≦0.13" and "0.25≦Y2 / H≦0.75." As shown in FIG. 6 and Table 1, in Examples 1 to 5, which satisfied the conditions "Y1 / H≦0.13" and "0.25≦Y2 / H≦0.75," the pressure in the decompression chamber was higher than that at the edge of the sheet material, suppressing the airflow in the decompression chamber, resulting in a small number of defects (4 to 5). On the other hand, as shown in FIG. 6 and Table 2, Comparative Examples 1 to 5, which did not satisfy the condition "Y1 / H≦0.13" or "0.25≦Y2 / H≦0.75," had a high number of defects, ranging from 10 to 13. Furthermore, in Example 6, which satisfied the condition "L1 / H≦0.38," the small L1 further suppressed the airflow flowing into the decompression chamber, resulting in a number of defects of three, fewer than in Examples 1 to 5. Furthermore, in Example 7, in which the sealing gap was blocked with a sealing material, there was no airflow that would flow through the gap and disrupt the pressure balance near the edge of the sheet material, resulting in a number of defects of two, fewer than in Examples 1 to 5. In Example 8, in which the sealing material was an elastic material and was pressed against the casting device to block the sealing gap, even small gaps with the casting device could be prevented, resulting in a number of defects of one, fewer than in Example 7. In Example 9, in which the sealing material was pressed and fixed to the decompression chamber with a pressing member, distortion and displacement of the sealing material were suppressed, and the number of defects was 0, which was fewer than in Example 8.

[0036] The present invention is not limited to a manufacturing apparatus and manufacturing method for a microporous polyolefin resin sheet, but can also be applied to a manufacturing apparatus and manufacturing method for a solution resin sheet, die coating, etc., but the scope of application is not limited to these.

[0037] REFERENCE SIGNS LIST 1 die 2 casting device 3 sheet material 4 reduced pressure chamber 4a side wall 5 discharge port 6 shielding plate 7 droplets 8a, 8b air flow 9 opening 10 sealing material 11 pressing member 12 exhaust nozzle 13 space 14 sealing gap 15 bolt

Claims

1. A method for manufacturing a sheet, comprising: discharging a sheet material containing a polyolefin resin and a diluent from a discharge port of a die toward a casting device; covering a space between the sheet material and the casting device with a decompression chamber disposed upstream of the discharge port in the sheet conveyance direction; sucking air in the decompression chamber to form a decompressed space, and bringing the sheet material into close contact with the casting device; cooling and solidifying the sheet material while conveying it with the casting device, wherein the sucking of the air in the decompression chamber is performed from exhaust nozzles arranged such that openings face outward from both ends in the width direction of the sheet material, and when the shortest distance from the discharge port of the die to the outer peripheral surface of the casting device is H, the shortest distance from the upper end side of the opening to the end of the sheet material is Y1, and the shortest distance from the lower end side of the opening to the end of the sheet material is Y2, Y1 / H ≤ 0.13 and 0.25 ≤ Y2 / H ≤ 0.

75. A method for manufacturing a microporous polyolefin resin sheet.

2. The method for manufacturing a microporous polyolefin resin sheet according to claim 1, wherein a suction width L1, which is the horizontal distance from the end of the sheet material 3 at the upper end of the opening of the exhaust nozzle to the upstream end in the sheet conveyance direction, as observed from the outside in the sheet width direction, satisfies L1 / H ≤ 0.

38.

3. The method for manufacturing a microporous polyolefin resin sheet according to claim 1 or 2, wherein a seal gap, which is a gap between a side wall perpendicular to the sheet width direction of the decompression chamber and the casting device and is located directly below the opening of the exhaust nozzle, is physically blocked with a sealing material.

4. The method for manufacturing a microporous polyolefin resin sheet according to claim 3, wherein the sealing material is an elastic body, and the sealing gap is blocked by pressing the sealing material against the casting device.

5. The method for manufacturing a microporous polyolefin resin sheet according to claim 4, wherein the sealing material is pressed against the decompression chamber with a pressing member and fixed.

6. A manufacturing apparatus for a microporous polyolefin resin sheet, comprising: a die having a discharge port for discharging a sheet material containing a polyolefin resin and a diluent; a casting device for cooling and solidifying the sheet material discharged from the discharge port while conveying it; and a decompression chamber disposed upstream of the discharge port in the sheet conveying direction, covering the space between the sheet material and the casting device, and sucking air to form a decompression space. The decompression chamber is arranged such that exhaust nozzles for sucking air in the decompression chamber are disposed outside both end portions in the width direction of the sheet material with their openings facing each other. When the shortest distance from the discharge port of the die to the outer peripheral surface of the casting device is H, the shortest distance from the upper end side of the opening of the exhaust nozzle to the end portion of the sheet material is Y1, and the shortest distance from the lower end side of the opening of the exhaust nozzle to the end portion of the sheet material is Y2, Y1 / H ≤ 0.13 and 0.25 ≤ Y2 / H ≤ 0.

75. The die, the casting device, and the exhaust nozzle are arranged accordingly.

7. The manufacturing apparatus for a microporous polyolefin resin sheet according to claim 6, wherein the exhaust nozzle is arranged such that the suction width L1, which is the horizontal distance from the end portion of the sheet material 3 at the upper end of the opening of the exhaust nozzle to the upstream end in the sheet conveying direction as observed from the outside in the sheet width direction, satisfies L1 / H ≤ 0.

38.

8. The manufacturing apparatus for a microporous polyolefin resin sheet according to claim 6 or 7, further comprising a sealing material for physically blocking a seal gap, which is a gap located directly below the opening of the exhaust nozzle, among the gaps between the side wall perpendicular to the sheet width direction of the decompression chamber and the casting device.

9. The manufacturing apparatus for a microporous polyolefin resin sheet according to claim 8, wherein the sealing material is an elastic body and is pressed against the casting device.

10. The manufacturing apparatus for a microporous polyolefin resin sheet according to claim 9, further comprising a pressing member for pressing and fixing the sealing material to the decompression chamber.

11. The manufacturing apparatus for a microporous polyolefin resin sheet according to any one of claims 8 to 10, wherein the side wall is movable in the width direction of the sheet material.