Technical Problem

Current precision filtration filters in semiconductor, liquid crystal, food, and medical fields face challenges in capturing fine particles due to increasing miniaturization and stringent safety requirements, with existing filters lacking sufficient accuracy and reliability for particles smaller than 0.5 μm.

Method used

A porous membrane laminate with polytetrafluoroethylene (PTFE) as the main component, featuring an average flow pore diameter of 75 nm or less and a narrow pore diameter distribution, ensuring effective particle capture and filtration accuracy by minimizing pore size variation and enhancing mechanical strength through support membrane lamination.

Benefits of technology

The porous membrane laminate demonstrates excellent fine particle trapping performance and improved filtration accuracy, suitable for high-integrity applications in semiconductor, liquid crystal, food, and medical fields, ensuring reliable removal of minute foreign substances.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

A porous membrane according to the present disclosure is composed mainly of polytetrafluoroethylene, wherein the mean flow pore size E is 75 nm or less, and the pore size difference G-E between the maximum pore size G and the mean flow pore size E is not more than 20 nm.
Need to check novelty before this filing date? Find Prior Art

Description

Porous membrane and porous membrane laminate

[0001] The present disclosure relates to a porous membrane and a porous membrane laminate. This application claims priority to Japanese Patent Application No. 2022-007435, filed on January 20, 2022. The entire contents of the Japanese patent application are incorporated herein by reference.

[0002] Porous films using polytetrafluoroethylene have the properties of polytetrafluoroethylene, such as high heat resistance, chemical stability, weather resistance, non-flammability, high strength, non-stickiness, and low friction coefficient, as well as the properties of flexibility, dispersion medium permeability, particle capture, and low dielectric constant due to porosity.Therefore, porous films mainly composed of polytetrafluoroethylene are widely used as precision filtration filters for dispersion mediums and gases in the fields of semiconductors, liquid crystals, and food and medical care.In the prior art, as a filtration filter, a porous film laminate has been proposed in recent years, using a porous film mainly composed of PTFE, which can capture fine particles with a particle diameter of less than 0.1 μm (see JP 2010-94579 A).

[0003] JP 2010-94579 A

[0004] A porous membrane according to one embodiment of the present disclosure is a porous membrane primarily composed of polytetrafluoroethylene, having a mean flow pore size E of 75 nm or less, and a pore size difference (G-E) between the maximum pore size G and the mean flow pore size E of 20 nm or less.

[0005] FIG. 1 is a schematic partial cross-sectional view showing a porous membrane according to an embodiment of the present disclosure. FIG. 2 is a schematic partial cross-sectional view showing an example of a porous membrane stack according to an embodiment of the present disclosure. FIG. 3 is a schematic partial cross-sectional view showing another example of a porous membrane stack according to an embodiment of the present disclosure. FIG. 4 is a cross-sectional image of the porous membrane stack of Test No. 1 taken using a scanning electron microscope. FIG. 5 is a cross-sectional image of the porous membrane stack of Test No. 2 taken using a scanning electron microscope. FIG. 6 is a cross-sectional image of the porous membrane stack of Test No. 3 taken using a scanning electron microscope. FIG. 7 is a cross-sectional image of the porous membrane stack of Test No. 4 taken using a scanning electron microscope. FIG. 8 is a schematic partial cross-sectional view showing another example of a porous membrane stack according to an embodiment of the present disclosure. FIG. 9 is a schematic partial cross-sectional view showing another example of a porous membrane stack according to an embodiment of the present disclosure. FIG. 10 is a schematic partial cross-sectional view showing another example of a porous membrane stack according to an embodiment of the present disclosure. Fig. 11 is a schematic partial cross-sectional view showing another example of a porous membrane stack according to an embodiment of the present disclosure. Fig. 12 is a schematic partial cross-sectional view showing another example of a porous membrane stack according to an embodiment of the present disclosure. Fig. 13 is a schematic partial cross-sectional view showing another example of a porous membrane stack according to an embodiment of the present disclosure. Fig. 14 is a schematic partial cross-sectional view showing another example of a porous membrane stack according to an embodiment of the present disclosure. Fig. 15 is a schematic partial cross-sectional view showing another example of a porous membrane stack according to an embodiment of the present disclosure. Fig. 16 is a schematic partial cross-sectional view showing another example of a porous membrane stack according to an embodiment of the present disclosure.

[0006] [Problem to be Solved by the Present Disclosure] In the fields described above, further technological innovation and increasing requirements have led to a demand for higher performance microfiltration filters. Specifically, in the semiconductor and liquid crystal fields, integration levels have been increasing year by year, and photoresists have been miniaturized to the 0.5 μm range or less. Therefore, a microfiltration filter that can reliably capture such fine particles is needed. These microfiltration filters are mainly used as filters for treating the outside air in clean rooms, filters for chemical solutions, etc., and their performance also affects product yield. Furthermore, in the food and medical fields, due to the recent increase in safety awareness, there is a strong demand for the ability to remove minute foreign matter.

[0007] The present disclosure has been made in light of the above circumstances, and has an object to provide a porous membrane that has excellent fine particle capture performance.

[0008] [Effects of the Present Disclosure] According to the present disclosure, a porous membrane having excellent particle trapping performance can be provided.

[0009] [Description of Embodiments of the Present Disclosure] First, embodiments of the present disclosure will be listed and described.

[0010] (1) A porous membrane according to one embodiment of the present disclosure is a porous membrane primarily composed of polytetrafluoroethylene, having a mean flow pore size E of 75 nm or less, and a pore size difference G-E between the maximum pore size G and the mean flow pore size E of 20 nm or less.

[0011] The porous membrane is mainly composed of polytetrafluoroethylene (hereinafter also referred to as PTFE), and the gaps between the polytetrafluoroethylene particles form the pore size. Since the upper limit of the mean flow pore size of the porous membrane is 75 nm, fine particles tend to collide with the fibers, and the porous membrane has excellent fine particle capture performance. Furthermore, since the difference G-E between the maximum pore size G and the mean flow pore size E of the porous membrane (hereinafter also referred to as pore size difference) is 20 nm or less, the pore size variation is small, and the accuracy of the filtration process is improved. The "main component" refers to the component with the largest content in terms of mass, for example, a component with a content of 90 mass% or more, preferably 95 mass% or more.

[0012] (2) In the above (1), the porous membrane preferably has a pore size difference of 15 nm or less between the maximum pore size G and the mean flow pore size E. By having the pore size difference between the maximum pore size G and the mean flow pore size E of the porous membrane be 15 nm or less, the pore size variation can be further reduced, and the accuracy of the filtration process can be improved.

[0013] (3) In the above (1) or (2), the porous membrane preferably has a pore size difference ratio {(G−E) / E}×100 (hereinafter also referred to as pore size ratio) of 35% or less, where the pore size difference is between the maximum pore size G and the mean flow pore size E relative to the mean flow pore size E. When the pore size ratio of the porous membrane is 35% or less, the pore size variation can be further reduced, and the accuracy of the filtration process can be improved.

[0014] As will be described later, the "mean flow pore size," "pore size difference (G-E)," and "pore size ratio {(G-E) / E} x 100" can be calculated from the pore size distribution measured with a pore diameter distribution measuring device (for example, a Perm Porometer "CFP-1500A" manufactured by PMI) in accordance with ASTM F316-03 and JIS-K3832 (1990) using propylene and 1,1,2,3,3,3-hexahydrofluoric acid oxide having a surface tension of 15.9 mN / m as reagents.

[0015] (4) A porous membrane stack according to another aspect of the present disclosure includes one or more of the porous membranes described in (1) to (3) above, and preferably has a mean flow pore size K of 75 nm or less, and a pore size difference J-K between the maximum pore size J and the mean flow pore size K of 20 nm or less. Because the porous membrane stack includes the porous membrane, it has excellent fine particle capture performance and is suitable as a microfiltration filter. Since the upper limit of the mean flow pore size of the porous membrane stack is 75 nm, fine particles are more likely to collide with the fibers, and the porous membrane stack has excellent fine particle capture performance. Furthermore, since the mean flow pore size K of the porous membrane stack is 75 nm or less and the pore size difference J-K between the maximum pore size J and the mean flow pore size K is 20 nm or less, pore size variation is small, resulting in improved filtration accuracy.

[0016] (5) In the above (4), the porous membrane stack preferably has a pore size difference ratio {(J−K) / K}×100 of 35% or less, where {(J−K) / K} is the difference between the maximum pore size J and the mean flow pore size K relative to the mean flow pore size K. When the pore size ratio of the porous membrane stack is 35% or less, the variation in pore size can be reduced, and the accuracy of the filtration process of the porous membrane stack can be further improved.

[0017] (6) In the above (4) or (5), it is preferable that the porous membrane laminate comprises one or more porous support membranes whose main component is polytetrafluoroethylene, and the support membranes are laminated on one or both sides of the porous membrane. By comprising one or more porous support membranes whose main component is polytetrafluoroethylene, the support membranes function as protective materials for the porous membranes, and the porous membrane laminate can improve its capture performance while increasing its mechanical strength and lifespan. Furthermore, by using polytetrafluoroethylene as the main component of the support membrane, it is possible to improve its heat resistance, chemical stability, etc.

[0018] (7) In the above (6), the support membrane preferably has a mean flow pore size of 200 nm or less. By having the mean flow pore size of the support membrane be 200 nm or less, the particle capture performance of the porous membrane stack can be further improved.

[0019] (8) In the above (6) or (7), it is preferable that the porous membrane stack comprises a plurality of the porous membranes and a plurality of the support membranes, the porous membranes and the support membranes are alternately stacked, and the support membranes are stacked at both ends. In the porous membrane stack, the porous membranes and the support membranes are alternately stacked, and the support membranes are stacked at both ends, thereby further improving the capture performance, mechanical strength, and lifespan of the porous membrane stack.

[0020] (9) In any of the above (4) to (8), the mean flow pore size K of the porous membrane stack is preferably 60 nm or less. By setting the mean flow pore size K of the porous membrane stack to 60 nm or less, the fine particle capture performance of the porous membrane stack can be further improved.

[0021] [Details of the embodiment of the present disclosure] Preferred embodiments of the present disclosure will now be described with reference to the drawings.

[0022] <Porous membrane> Figure 1 is a schematic partial cross-sectional view showing a porous membrane according to one embodiment of the present disclosure. The porous membrane 1 is composed of a biaxially stretched porous membrane mainly composed of polytetrafluoroethylene. This biaxially stretched porous membrane is made porous by stretching the surface of a sheet mainly composed of PTFE in two perpendicular directions. The porous membrane 1 allows the filtrate to permeate in the thickness direction while preventing the permeation of fine impurities.

[0023] The PTFE powder preferably has a high molecular weight. By using a high molecular weight PTFE powder, excessive pore expansion and tearing of the sheet can be prevented during stretching, while promoting the growth of the fibrous skeleton. In addition, nodules in the sheet can be reduced, allowing the formation of a porous film with densely packed micropores.

[0024] The PTFE powder preferably has a high molecular weight. By using a high molecular weight PTFE powder, the growth of the fibrous skeleton can be promoted while preventing excessive expansion of the pores and rupture of the membrane during stretching. In addition, the number of nodes in the membrane can be reduced, and a porous membrane with densely formed micropores can be formed.

[0025] The lower limit of the number average molecular weight of the PTFE powder forming the porous membrane 1 is preferably 12 million, more preferably 20 million. On the other hand, the upper limit of the number average molecular weight of the PTFE powder forming the porous membrane 1 is preferably 50 million, more preferably 40 million. If the number average molecular weight of the PTFE powder forming the porous membrane 1 is less than the above lower limit, the pore size of the porous membrane 1 may become large, and the accuracy of the filtration process may decrease. On the other hand, if the number average molecular weight of the PTFE powder forming the porous membrane 1 exceeds the above upper limit, it may be difficult to form the membrane. Note that the "number average molecular weight" is calculated from the specific gravity of the molded product, but since the molecular weight of PTFE varies greatly depending on the measurement method and is difficult to measure accurately, it may not fall within the above range depending on the measurement method.

[0026] The lower limit of the average thickness of the porous membrane 1 is preferably 2 μm, more preferably 5 μm. On the other hand, the upper limit of the average thickness of the porous membrane 1 is preferably 50 μm, more preferably 40 μm. If the average thickness is less than the lower limit, the strength of the porous membrane 1 may be insufficient. On the other hand, if the average thickness exceeds the upper limit, the porous membrane 1 may become unnecessarily thick, which may increase the pressure loss when the filtrate is passed through. When the average thickness of the porous membrane 1 is within the above range, the strength of the porous membrane 1 and the filtration treatment efficiency can both be achieved. The "average thickness" refers to the average value of thicknesses at any 10 points, and is measured using a standard digital thickness gauge.

[0027] The upper limit of the mean flow pore diameter E of the porous membrane 1 is 75 nm or less, more preferably 70.0 nm or less. When the upper limit of the mean flow pore diameter E of the porous membrane 1 is 75 nm or less, the porous membrane 1 has excellent microparticle capture performance. On the other hand, the lower limit of the mean flow pore diameter of the porous membrane 1 is preferably 25.0 nm or more, more preferably 35.0 nm or more. If the mean flow pore diameter E of the porous membrane 1 is less than the lower limit, the pressure loss of the porous membrane 1 may increase. The mean flow pore diameter E of the porous membrane 1 can be adjusted by selecting, for example, the molecular weight of the raw material PTFE, the difference between the onset temperature and the end set temperature of the peak in the range of 300 ° C. or more and 360 ° C. or less of the melting curve of the first run in thermal analysis by a differential scanning calorimeter (DSC), the stretching ratio, etc. The mean flow pore diameter E of the porous membrane 1 is preferably 25.0 nm or more and 75 nm or less, more preferably 35.0 nm or more and 70.0 nm or less.

[0028] The upper limit of the pore size difference G-E between the maximum pore size G and the mean flow pore size E of the porous membrane 1 is 20 nm or less, and may be 15 nm or less. When the pore size difference of the porous membrane 1 is 20 nm or less, the pore size variation of the laminate is small, and the accuracy of the filtration process can be improved. The pore size ratio of the porous membrane 1 can be adjusted by selecting, for example, the molecular weight of the raw material PTFE, the difference between the onset temperature and the end set temperature of the peak in the range of 300 ° C. to 360 ° C. of the melting curve of the first run in thermal analysis by a differential scanning calorimeter (DSC), the stretching speed, etc.

[0029] The upper limit of the ratio of the difference between the maximum pore size G and the mean flow pore size E of the porous membrane 1, {(G-E) / E} x 100 (pore size ratio), may be 35% or less, or may be 20% or less. By making the pore size ratio of the porous membrane 1 35% or less, the pore size variation can be further reduced, and the accuracy of the filtration process can be improved. The lower limit of the pore size ratio can be 10% or more, or 15% or more. The pore size ratio can be 10% or more and 35% or less, or 10% or more and 20% or less. The pore size ratio of the porous membrane 1 can be adjusted by selecting, for example, the molecular weight of the raw material PTFE, the difference between the onset temperature and the end set temperature of the peak in the range of 300 ° C. to 360 ° C. in the melting curve of the first run in thermal analysis by a differential scanning calorimeter (DSC) of the raw material, the stretching speed, etc.

[0030] The upper limit of the Gurley second of the porous membrane 1 is preferably 100 seconds, more preferably 80 seconds. If the Gurley second exceeds the upper limit, the filtration efficiency of the porous membrane 1 may decrease. On the other hand, the lower limit of the Gurley second is preferably 1 second, more preferably 3 seconds. If the Gurley second is less than the lower limit, the pore size of the porous membrane 1 may become too large, which may decrease the ability to capture fine particles. "Gurley second" is measured in accordance with JIS-P8117 (2009) and is the number of times that the porous membrane 1 can capture fine particles. 3 The air flows at an average pressure difference of 1.22 kPa and is 6.42 cm 2 This means the time it takes for a sample to pass through.

[0031] The upper limit of the porosity of the porous membrane 1 is preferably 90%, more preferably 85%. On the other hand, the lower limit of the porosity of the porous membrane 1 is preferably 40%, more preferably 50%. If the porosity of the porous membrane 1 exceeds 90%, the porous membrane 1 may not be able to capture enough fine particles. On the other hand, if the porosity of the porous membrane 1 is less than 40%, the pressure loss of the porous membrane 1 may increase. Note that "porosity" refers to the ratio of the total volume of pores to the volume of an object, and can be determined by measuring the density of the object in accordance with ASTM-D-792.

[0032] In addition to PTFE, the porous membrane 1 may contain other fluororesins or additives within a range that does not impair the desired effects of the present disclosure.

[0033] [Method for manufacturing porous membrane] One embodiment of the method for manufacturing the porous membrane will be described. The method for manufacturing the porous membrane comprises the steps of molding a mixture of PTFE powder and liquid lubricant, and stretching the molded body.

[0034] (Molding process) In the molding process, a mixture of PTFE powder produced by emulsion polymerization or the like and a liquid lubricant is extrusion molded to produce a sheet-shaped molded body. The raw material PTFE particles are powders made of fine PTFE particles. Examples of PTFE powders include PTFE fine powders made by emulsion polymerization and PTFE molding powders made by suspension polymerization, which are powders made of fine PTFE particles.

[0035] As the liquid lubricant, various lubricants conventionally used in the extrusion method can be used. Examples of the liquid lubricant include petroleum solvents such as solvent naphtha and white oil, hydrocarbon oils such as undecane, aromatic hydrocarbons such as toluene and xylol, alcohols, ketones, esters, silicone oil, fluorochlorocarbon oil, solutions of polymers such as polyisobutylene and polyisoprene dissolved in these solvents, and water or aqueous solutions containing surfactants. These can be used alone or in combination of two or more. However, from the viewpoint of uniform mixing, it is preferable to use a liquid lubricant of a single component.

[0036] The lower limit of the amount of the liquid lubricant mixed with 100 parts by mass of PTFE powder is preferably 10 parts by mass, more preferably 16 parts by mass.On the other hand, the upper limit of the amount of the liquid lubricant mixed is preferably 40 parts by mass, more preferably 25 parts by mass.If the amount of the liquid lubricant mixed is less than the lower limit, it may be difficult to extrude.On the other hand, if the amount of the liquid lubricant mixed is more than the upper limit, it may be difficult to carry out the compression molding described below.

[0037] In addition to the liquid lubricant, the material for forming the porous film may contain other additives depending on the purpose. Examples of other additives include pigments for coloring, inorganic fillers such as carbon black, graphite, silica powder, glass powder, glass fiber, silicates and carbonates, metal powder, metal oxide powder, metal sulfide powder, etc., for improving wear resistance, preventing low-temperature flow, and facilitating pore formation. In addition, in order to help form a porous structure, substances that can be removed or decomposed by heating, extraction, dissolution, etc., such as ammonium chloride, sodium chloride, plastics other than PTFE, rubber, etc., may be blended in the form of powder or solution.

[0038] In this process, the PTFE powder and the liquid lubricant are first mixed and then compressed into a block using a compression molding machine. Next, this block is extruded into a sheet at room temperature (e.g., 25°C) or higher and 50°C or lower at a speed of, for example, 10 mm / min to 30 mm / min. This sheet is then rolled using a calender roll or the like to obtain a PTFE sheet with an average thickness of 250 μm to 350 μm.

[0039] The porous film has excellent permeability for liquid lubricants, and the extrusion pressure during production is reduced.

[0040] The liquid lubricant contained in this PTFE sheet may be removed after stretching the sheet, but is preferably removed before stretching. The liquid lubricant can be removed by heating, extraction, dissolution, etc. When heating, the liquid lubricant can be removed, for example, by rolling the PTFE sheet with a heated roll at 130°C or higher and 220°C or lower. When using a liquid lubricant with a relatively high boiling point, such as silicone oil or fluorochlorocarbon oil, removal by extraction is preferred.

[0041] (Stretching step) In this step, the PTFE sheet, which is a molded body, is biaxially stretched. This step allows pores to be formed, and a porous membrane can be obtained. In this step, the PTFE sheet is stretched sequentially in the longitudinal direction (flow direction) and the transverse direction (width direction) perpendicular to the longitudinal direction, to obtain a biaxially stretched porous membrane.

[0042] The PTFE sheet is preferably stretched at a high temperature to densify the porous structure. The lower limit of the stretching temperature is preferably 60°C, more preferably 120°C. On the other hand, the upper limit of the stretching temperature is preferably 300°C, more preferably 280°C. If the stretching temperature is below the lower limit, the pore size may become too large. On the other hand, if the stretching temperature is above the upper limit, the pore size may become too small.

[0043] Furthermore, it is preferable that the biaxially stretched porous membrane is heat-set after stretching. By performing heat-setting, the main shrinkage of the biaxially stretched porous membrane can be prevented and the porous structure can be more reliably maintained. As a specific method of heat-setting, for example, a method can be used in which both ends of the biaxially stretched porous membrane are fixed and kept at a temperature of 200°C or higher and 500°C or lower for 0.1 minutes or longer and 20 minutes or shorter. In addition, when stretching is performed in multiple stages, it is preferable to perform heat-setting after each stage.

[0044] The structure of the manufactured porous membrane is as described above, so a duplicated description will be omitted.

[0045] The porous membrane has excellent particle capturing performance and can therefore be suitably used as a filter or the like that requires high accuracy in filtration processing.

[0046] <Porous membrane stack> The porous membrane stack includes one or more of the porous membranes described above. Because the porous membrane stack includes the porous membrane, it has excellent fine particle capture performance and is suitable as a microfiltration filter.

[0047] The upper limit of the mean flow pore diameter K of the porous membrane stack is preferably 75 nm or less, more preferably 60 nm or less, and even more preferably 55 nm or less. By setting the upper limit of the mean flow pore diameter K of the porous membrane stack to 75 nm or less, the fine particle capture performance of the porous membrane stack can be further improved. On the other hand, the lower limit of the mean flow pore diameter K of the porous membrane stack is preferably 25 nm or more, more preferably 30 nm or more. If the mean flow pore diameter K of the porous membrane stack is less than the lower limit, the pressure loss of the porous membrane stack may increase. The mean flow pore diameter K of the porous membrane stack is preferably 25 nm or more and 75 nm or less, more preferably 25 nm or more and 60 nm or less, and even more preferably 30 nm or more and 55 nm or less.

[0048] The upper limit of the pore size difference J-K between the maximum pore size J and the mean flow pore size K in the porous membrane stack is preferably 20 nm or less, and more preferably 18 nm or less. When the difference J-K between the maximum pore size J and the mean flow pore size K of the porous membrane stack is 20 nm or less, the fine particle capture performance of the porous membrane stack can be further improved. The lower limit of the pore size difference J-K can be 17 nm or more, or 15 nm or more. The pore size difference J-K can be 17 nm or more and 20 nm or less, or 15 nm or more and 18 nm or less.

[0049] The upper limit of the ratio of the difference between the maximum pore size J and the mean flow pore size K to the mean flow pore size K in the porous membrane stack, {(J-K) / K} x 100 (pore size ratio), is preferably 35% or less, and more preferably 33% or less. Having a pore size ratio of 35% or less in the porous membrane stack reduces pore size variation and further improves the accuracy of the filtration process of the porous membrane stack. The lower limit of the pore size ratio can be 20% or more, or 23% or more. The pore size ratio can be 20% or more to 35% or less, or 23% or more to 33% or less.

[0050] The upper limit of the Gurley seconds of the porous membrane laminate is preferably 75 seconds, more preferably 70 seconds, and even more preferably 65 seconds.On the other hand, the lower limit of the Gurley seconds of the porous membrane laminate is preferably (1) seconds.If the Gurley seconds of the porous membrane laminate exceed 75 seconds, the filtration cost of the porous membrane laminate may not be sufficiently reduced.On the other hand, if the Gurley seconds of the porous membrane laminate are less than the above lower limit, the pore size of the porous membrane laminate may become too large, which may reduce the ability to capture fine particles.

[0051] The porous membrane stack preferably comprises one or more porous support membranes, the support membranes being laminated on one or both sides of the porous membrane. By laminating the support membranes on one or both sides of the porous membrane, the support membranes function as protective materials for the porous membrane, thereby improving the capture performance of the porous membrane stack while increasing the mechanical strength and lifespan of the porous membrane stack. The support membranes are preferably composed primarily of polytetrafluoroethylene. By using polytetrafluoroethylene as the main component of the support membrane, heat resistance, chemical stability, etc. can be improved.

[0052] The upper limit of the mean flow pore diameter of the support membrane is preferably 200 nm or less, more preferably 180 nm or less. If the mean flow pore diameter of the support membrane exceeds 3000 nm, the strength of the support membrane 2 may be insufficient. On the other hand, the lower limit of the mean flow pore diameter of the support membrane is preferably 80 nm or more, more preferably 100 nm or more. If the mean flow pore diameter of the support membrane is less than the lower limit, the pressure loss of the porous membrane stack may increase. The mean flow pore diameter of the support membrane is preferably 80 nm or more and 200 nm or less, more preferably 100 nm or more and 180 nm or less.

[0053] The upper limit of the average thickness of the support membrane is preferably 20 μm, more preferably 15 μm. On the other hand, the lower limit of the average thickness of the support membrane is preferably 2 μm, more preferably 5 μm. If the average thickness of the support membrane exceeds the upper limit, the pressure loss of the porous membrane stack may increase. On the other hand, if the average thickness of the support membrane 2 is less than the lower limit, the strength of the porous membrane stack may be insufficient.

[0054] 2 is a schematic partial cross-sectional view showing a porous membrane laminate according to an embodiment of the present disclosure. The porous membrane laminate 10 shown in FIG. 2 comprises a porous membrane 1 and a porous support membrane 2 laminated on one side of the porous membrane 1. The phrase "the porous membrane laminate 10 comprises a porous membrane 1 and a porous support membrane 2 laminated on one side of the porous membrane 1" can be rephrased as "the porous membrane laminate 10 comprises a first porous membrane 1 made of the porous membrane 1 and a first support membrane 2 mainly composed of polytetrafluoroethylene, with the first porous membrane 1 disposed on one main surface of the first support membrane 2." The porous membrane laminate 10 comprises a porous support membrane 2 laminated on one side of the porous membrane 1, and the porous membrane 1 is supported by the support membrane 2, thereby improving mechanical strength and suppressing filter clogging.

[0055] The porous membrane stack may have a three-layer structure, for example, a pair of support membranes disposed as the outermost layers and a porous membrane disposed between the pair of support membranes, for a total of three layers. The porous membrane stack may also have a structure of four or more layers.

[0056] The porous membrane stack preferably comprises a plurality of the porous membranes and a plurality of the support membranes, the porous membranes and the support membranes being alternately stacked, and the support membranes being stacked at both ends. In the porous membrane stack, the porous membranes and the support membranes are alternately stacked, and the support membranes are stacked at both ends, thereby further improving the capture performance, mechanical strength, and lifespan of the porous membrane stack.

[0057] When the porous membrane stack has, for example, a five-layer structure, it is preferable that the porous membrane stack includes a plurality of the porous membranes and a plurality of the support membranes, the porous membranes and the support membranes are alternately stacked, and the support membranes are stacked at both ends. Figure 3 is a schematic partial cross-sectional view showing a porous membrane stack according to another embodiment of the present disclosure. The porous membrane stack 20 shown in Figure 3 has a five-layer structure in which two layers of porous membranes 1 are stacked between a pair of support membranes 2 in the outermost layers, and a support membrane 2 is further stacked between this pair of porous membranes 1. In addition, "the porous membrane stack 20 has a five-layer structure in which two layers of porous membranes 1 are laminated between a pair of support membranes 2 of the outermost layers, and a support membrane 2 is further laminated between this pair of porous membranes 1" can be rephrased as "the porous membrane stack 20 is composed of a first porous membrane 1 consisting of the porous membrane 1, a second porous membrane 1 consisting of the porous membrane 1, a first support membrane 2 mainly composed of polytetrafluoroethylene, a second support membrane 2 mainly composed of polytetrafluoroethylene, and a third support membrane 2 mainly composed of polytetrafluoroethylene, and is configured such that the first porous membrane 1, the second support membrane 2, the second porous membrane 1, and the third support membrane 2 are arranged in the above order on one main surface of the first support membrane 2." In this way, by alternately stacking the porous membranes 1 and the support membranes 2 and stacking the support membranes 2 at both ends, the capture performance, mechanical strength, and lifespan of the porous membrane stack 20 can be further improved. Here, the first porous membrane 1 and the second porous membrane 1 may have the same configuration or different configurations, and the first support membrane 2, the second support membrane 2, and the third support membrane 2 may have the same configuration or different configurations.

[0058] For example, as shown in Fig. 8, the porous membrane stack 10 can be composed of a first porous membrane 1 made of the porous membrane 1 and a second porous membrane 1 made of the porous membrane 1, with the second porous membrane 1 disposed on one main surface of the first porous membrane 1. This can improve the mechanical strength of the porous membrane stack 10 and the particle capture performance (probability of particle capture by fibers). Note that the first porous membrane 1 and the second porous membrane 1 may have the same configuration or different configurations.

[0059] 9, the porous membrane stack 20 can be made of a first porous membrane 1 made of the porous membrane 1, a first support membrane 2 mainly composed of polytetrafluoroethylene, and a second support membrane 2 mainly composed of polytetrafluoroethylene, with the first porous membrane 1 and the second support membrane 2 being arranged in the above order on one main surface of the first support membrane 2. This improves the mechanical strength of the porous membrane stack 20, suppresses filter clogging, and prevents deterioration of particle capture performance due to external damage. Note that the first support membrane 2 and the second support membrane 2 may have the same configuration or different configurations.

[0060] 10, the porous membrane stack 20 can be composed of a first porous membrane 1 made of the porous membrane 1, a second porous membrane 1 made of the porous membrane 1, and a first support membrane 2 mainly composed of polytetrafluoroethylene, and the first porous membrane 1 and the second porous membrane 1 can be arranged in the above order on one main surface of the first support membrane 2. This improves the mechanical strength of the porous membrane stack 20, suppresses filter clogging, and improves the particle capture performance (probability of particle capture by fibers). Note that the first porous membrane 1 and the second porous membrane 1 can be the same configuration or different configurations.

[0061] 11, the porous membrane stack 20 can be composed of a first porous membrane 1 made of the porous membrane 1, a second porous membrane 1 made of the porous membrane 1, a first support membrane 2 mainly composed of polytetrafluoroethylene, and a second support membrane 2 mainly composed of polytetrafluoroethylene, with the first porous membrane 1, the second porous membrane 1, and the second support membrane 2 being arranged in the above order on one main surface of the first support membrane 2. This improves the mechanical strength of the porous membrane stack 20, suppresses filter clogging, improves the particle capture performance (probability of particle capture by fibers), and suppresses a decrease in particle capture performance due to external damage. Note that the first porous membrane 1 and the second porous membrane 1 may have the same configuration or different configurations. The first support membrane 2 and the second support membrane 2 may have the same configuration or different configurations.

[0062] 12, the porous membrane stack 20 comprises a first porous membrane 1 made of the porous membrane 1, a second porous membrane 1 made of the porous membrane 1, a third porous membrane 1 made of the porous membrane 1, and a first support membrane 2 mainly composed of polytetrafluoroethylene, and the first porous membrane 1, the second porous membrane 1, and the third porous membrane 1 are arranged in the above order on one main surface of the first support membrane 2. This improves the mechanical strength of the porous membrane stack 20, suppresses filter clogging, and improves the particle capture performance (probability of particle capture by fibers). Note that the first porous membrane 1, the second porous membrane 1, and the third porous membrane 1 may each have the same configuration or different configurations.

[0063] 13, the porous membrane stack 20 can be made of a first porous membrane 1 made of the porous membrane 1, a second porous membrane 1 made of the porous membrane 1, a third porous membrane 1 made of the porous membrane 1, a first support membrane 2 mainly made of polytetrafluoroethylene, and a second support membrane 2 mainly made of polytetrafluoroethylene, and can be made by arranging the first porous membrane 1, the second porous membrane 1, the third porous membrane 1, and the second support membrane 2 in the above order on one main surface of the first support membrane 2. This improves the mechanical strength of the porous membrane stack 20, suppresses filter clogging, improves the particle capture performance (probability of particle capture by fibers), and suppresses a decrease in particle capture performance due to external damage. Here, the first porous membrane 1, the second porous membrane 1, and the third porous membrane 1 may have the same configuration or different configurations, and the first support membrane 2 and the second support membrane 2 may have the same configuration or different configurations.

[0064] 14, the porous membrane stack 20 can be made of a first porous membrane 1 made of the porous membrane 1, a first support membrane 2 mainly made of polytetrafluoroethylene, a second support membrane 2 mainly made of polytetrafluoroethylene, a third support membrane 2 mainly made of polytetrafluoroethylene, and a fourth support membrane 2 mainly made of polytetrafluoroethylene, and can be made by arranging the second support membrane 2, the first porous membrane 1, the third support membrane 2, and the fourth support membrane 2 in the above order on one main surface of the first support membrane 2. This can improve the mechanical strength of the porous membrane stack 20, suppress clogging of the filtration, and suppress a decrease in particle capture performance due to external damage. Here, the first support film 2, the second support film 2, the third support film 2, and the fourth support film 2 may have the same configuration or different configurations.

[0065] 15, the porous membrane stack 20 may be composed of a first porous membrane 1 made of the porous membrane 1, a second porous membrane 1 made of the porous membrane 1, a third porous membrane 1 made of the porous membrane 1, a first support membrane 2 mainly made of polytetrafluoroethylene, a second support membrane 2 mainly made of polytetrafluoroethylene, a third support membrane 2 mainly made of polytetrafluoroethylene, and a fourth support membrane 2 mainly made of polytetrafluoroethylene, and may be composed of the first porous membrane 1, the second support membrane 2, the second porous membrane 1, the third support membrane 2, the third porous membrane 1, and the fourth support membrane 2 arranged in the above order on one main surface of the first support membrane 2. This improves the mechanical strength of the porous membrane stack 20, suppresses clogging of the filtration, and suppresses deterioration of particle capture performance due to external damage. Here, the first porous membrane 1, the second porous membrane 1, and the third porous membrane 1 may each have the same configuration or different configurations, and the first support membrane 2, the second support membrane 2, the third support membrane 2, and the fourth support membrane 2 may each have the same configuration or different configurations.

[0066] 16, the porous membrane stack 20 may be composed of a first porous membrane 1 made of the porous membrane 1, a second porous membrane 1 made of the porous membrane 1, a third porous membrane 1 made of the porous membrane 1, a fourth porous membrane 1 made of the porous membrane 1, a fifth porous membrane 1 made of the porous membrane 1, a first support membrane 2 mainly made of polytetrafluoroethylene, and a second support membrane 2 mainly made of polytetrafluoroethylene, and may be composed of the first porous membrane 1, the second porous membrane 1, the third porous membrane 1, the fourth porous membrane 1, the fifth porous membrane 1, and the second support membrane 2 arranged in the above order on one main surface of the first support membrane 2. This improves the mechanical strength of the porous membrane stack 20, suppresses filter clogging, improves the particle capture performance (probability of particle capture by fibers), and suppresses a decrease in particle capture performance due to external damage. Note that the first porous membrane 1, the second porous membrane 1, the third porous membrane 1, the fourth porous membrane 1, and the fifth porous membrane 1 may each have the same configuration or different configurations. Furthermore, the first support membrane 2 and the second support membrane 2 may have the same configuration or different configurations.

[0067] [Method for manufacturing a porous membrane stack] An embodiment of a method for manufacturing a porous membrane stack, for example, when the porous membrane stack includes the porous membrane and a support membrane, will be described. The method for manufacturing a porous membrane stack includes a step of stacking porous membranes.

[0068] (Laminating Step) In this step, the porous membrane is laminated on, for example, one surface of a support membrane, and then heated to form a porous membrane laminate.

[0069] Examples of methods for laminating the porous membrane onto the support membrane include a method of fusing by heating, and a method of adhering using an adhesive or pressure sensitive adhesive.

[0070] As the method of fusing by heating, specifically, first, the porous membrane is laminated on one side of a support membrane, for example, and this laminate is heated to heat-seal each layer at the boundary and integrate them, thereby obtaining a porous membrane laminate.The lower limit of this heating temperature is preferably 327°C, which is the glass transition point of PTFE, and more preferably 360°C.On the other hand, the upper limit of heating temperature is preferably 400°C.If the heating temperature is less than 327°C, the heat fusion of each layer may be insufficient.On the other hand, if the heating temperature is more than 400°C, each layer may be deformed.In addition, the heating time is preferably 0.5 minutes or more and 3 minutes or less.

[0071] In the method of bonding using an adhesive or pressure-sensitive adhesive, the adhesive or pressure-sensitive adhesive is preferably a solvent-soluble or thermoplastic fluororesin or fluororubber from the viewpoint of heat resistance, chemical resistance, etc.

[0072] (Hydrophilic treatment) The porous membrane laminate obtained as described above may be subjected to hydrophilic treatment. This hydrophilic treatment is to impregnate the porous membrane laminate with a hydrophilic material and crosslink it. This hydrophilic material can be polyvinyl alcohol (PVA), ethylene vinyl alcohol copolymer (EVOH), acrylate resin, etc. Among these, PVA is preferred because it is easily adsorbed on the surface of PTFE fibers and can be impregnated uniformly.

[0073] Specifically, the hydrophilization treatment can be performed, for example, by the following procedure. First, the porous membrane laminate is immersed in isopropyl alcohol (IPA) for 0.25 to 2 minutes, and then immersed in a PVA aqueous solution with a concentration of 0.5 to 0.8% by weight for 5 to 10 minutes. The porous membrane laminate is then immersed in pure water for 2 to 5 minutes, and crosslinking is then performed by adding a crosslinking agent or irradiating with an electron beam. After this crosslinking, the porous membrane laminate is washed with pure water and dried at room temperature (25°C) to 80°C, thereby hydrophilizing the surface of the porous membrane laminate. The crosslinking agent used can be, for example, one that forms glutaraldehyde crosslinking, terephthalaldehyde crosslinking, or the like. The electron beam can be, for example, 6 Mrad.

[0074] The porous membrane laminate, which includes one or more porous membranes, has excellent particle capture performance and is therefore suitable as a precision filter for dispersion media and gases used in applications such as cleaning, stripping, and chemical supply in the semiconductor, liquid crystal, and food and medical fields.

[0075] [Other Embodiments] The embodiments disclosed herein should be considered to be illustrative in all respects and not restrictive. The scope of the present invention is not limited to the configurations of the above-described embodiments, but is defined by the claims, and is intended to include all modifications within the meaning and scope of the claims.

[0076] [Appendix 1] A porous membrane mainly composed of polytetrafluoroethylene, having a mean flow pore size E of 75 nm or less, and a pore size difference G-E between the maximum pore size G and the mean flow pore size E of 20 nm or less.

[0077] [Appendix 2] The porous membrane according to Appendix 1, wherein the pore size difference between the maximum pore size G and the mean flow pore size E is 15 nm or less.

[0078] [Appendix 3] The porous membrane according to appendix 1 or appendix 2, wherein the ratio of the pore size difference between the maximum pore size G and the mean flow pore size E to the mean flow pore size E {(G−E) / E}×100 is 35% or less.

[0079] [Appendix 4] A porous membrane stack comprising one or more porous membranes according to any one of appendices 1 to 3, wherein the porous membrane stack has a mean flow pore size K of 75 nm or less, and a pore size difference J-K between the maximum pore size J and the mean flow pore size K is 20 nm or less.

[0080] [Appendix 5] The porous membrane stack according to appendix 4, wherein the ratio of the pore size difference between the maximum pore size J and the mean flow pore size K to the mean flow pore size K {(J−K) / K}×100 is 35% or less.

[0081] [Appendix 6] The porous membrane laminate according to appendix 4 or appendix 5, comprising one or more porous support membranes whose main component is polytetrafluoroethylene, wherein the support membranes are laminated on one or both sides of the porous membrane.

[0082] [Appendix 7] The porous membrane stack according to Appendix 6, wherein the support membrane has a mean flow pore size of 200 nm or less.

[0083] [Appendix 8] The porous membrane stack according to appendix 6 or appendix 7, comprising a plurality of the porous membranes and a plurality of the support membranes, wherein the porous membranes and the support membranes are alternately stacked, and the support membranes are stacked on both ends.

[0084] [Supplementary Note 9] The porous membrane stack according to any one of Supplementary Notes 4 to 8, wherein the mean flow pore size K is 60 nm or less.

[0085] [Appendix 10] A porous membrane stack comprising a first porous membrane comprising the porous membrane described in any one of Appendices 1 to 3, and a second porous membrane comprising the porous membrane described in any one of Appendices 1 to 3, wherein the second porous membrane is disposed on one main surface of the first porous membrane.

[0086] [Appendix 11] A porous membrane laminate comprising a first porous membrane comprising the porous membrane according to any one of Appendices 1 to 3, a first support membrane mainly composed of polytetrafluoroethylene, and a second support membrane mainly composed of polytetrafluoroethylene, wherein the first porous membrane and the second support membrane are arranged in the above order on one main surface of the first support membrane.

[0087] [Appendix 12] A porous membrane laminate comprising: a first porous membrane comprising the porous membrane described in any one of Appendices 1 to 3; a second porous membrane comprising the porous membrane described in any one of Appendices 1 to 3; and a first support membrane mainly composed of polytetrafluoroethylene, wherein the first porous membrane and the second porous membrane are arranged in the above order on one main surface of the first support membrane.

[0088] [Supplementary Note 13] A porous membrane laminate comprising: a first porous membrane comprising the porous membrane described in any one of Supplementary Note 1 to Supplementary Note 3; a second porous membrane comprising the porous membrane described in any one of Supplementary Note 1 to Supplementary Note 3; a first support membrane mainly composed of polytetrafluoroethylene; and a second support membrane mainly composed of polytetrafluoroethylene, wherein the first porous membrane, the second porous membrane, and the second support membrane are arranged in the aforementioned order on one main surface of the first support membrane.

[0089] [Appendix 14] A porous membrane laminate comprising: a first porous membrane comprising the porous membrane described in any one of Appendices 1 to 3; a second porous membrane comprising the porous membrane described in any one of Appendices 1 to 3; a third porous membrane comprising the porous membrane described in any one of Appendices 1 to 3; and a first support membrane mainly composed of polytetrafluoroethylene, wherein the first porous membrane, the second porous membrane, and the third porous membrane are arranged in the aforementioned order on one main surface of the first support membrane.

[0090] [Appendix 15] A porous membrane laminate comprising: a first porous membrane comprising the porous membrane described in any one of Appendices 1 to 3; a second porous membrane comprising the porous membrane described in any one of Appendices 1 to 3; a first support membrane mainly composed of polytetrafluoroethylene; a second support membrane mainly composed of polytetrafluoroethylene; and a third support membrane mainly composed of polytetrafluoroethylene, wherein the first porous membrane, the second support membrane, the second porous membrane, and the third support membrane are arranged in the aforementioned order on one main surface of the first support membrane.

[0091] [Appendix 16] A porous membrane laminate comprising: a first porous membrane comprising the porous membrane described in any one of Appendices 1 to 3; a second porous membrane comprising the porous membrane described in any one of Appendices 1 to 3; a third porous membrane comprising the porous membrane described in any one of Appendices 1 to 3; a first support membrane mainly composed of polytetrafluoroethylene; and a second support membrane mainly composed of polytetrafluoroethylene, wherein the first porous membrane, the second porous membrane, the third porous membrane, and the second support membrane are arranged in the aforementioned order on one main surface of the first support membrane.

[0092] [Appendix 17] A porous membrane laminate comprising a first porous membrane comprising the porous membrane according to any one of Appendices 1 to 3, a first support membrane mainly composed of polytetrafluoroethylene, a second support membrane mainly composed of polytetrafluoroethylene, a third support membrane mainly composed of polytetrafluoroethylene, and a fourth support membrane mainly composed of polytetrafluoroethylene, wherein the second support membrane, the first porous membrane, the third support membrane, and the fourth support membrane are arranged in the aforementioned order on one main surface of the first support membrane.

[0093] [Appendix 18] A porous membrane laminate comprising: a first porous membrane comprising the porous membrane described in any one of Appendices 1 to 3; a second porous membrane comprising the porous membrane described in any one of Appendices 1 to 3; a third porous membrane comprising the porous membrane described in any one of Appendices 1 to 3; a first support membrane mainly composed of polytetrafluoroethylene; a second support membrane mainly composed of polytetrafluoroethylene; a third support membrane mainly composed of polytetrafluoroethylene; and a fourth support membrane mainly composed of polytetrafluoroethylene, wherein the first porous membrane, the second support membrane, the second porous membrane, the third support membrane, the third porous membrane, and the fourth support membrane are arranged in the aforementioned order on one main surface of the first support membrane.

[0094] [Supplementary Note 19] A porous membrane laminate comprising: a first porous membrane comprising the porous membrane described in any one of Supplementary Notes 1 to 3; a second porous membrane comprising the porous membrane described in any one of Supplementary Notes 1 to 3; a third porous membrane comprising the porous membrane described in any one of Supplementary Notes 1 to 3; a fourth porous membrane comprising the porous membrane described in any one of Supplementary Notes 1 to 3; a fifth porous membrane comprising the porous membrane described in any one of Supplementary Notes 1 to 3; a first support membrane mainly composed of polytetrafluoroethylene; and a second support membrane mainly composed of polytetrafluoroethylene, wherein the first porous membrane, the second porous membrane, the third porous membrane, the fourth porous membrane, the fifth porous membrane, and the second support membrane are arranged in the aforementioned order on one main surface of the first support membrane.

[0095] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these examples.

[0096] <Porous membrane laminate> [Test No. 1 and Test No. 2] (Molding process) PTFE fine powder A (second heat of fusion 15.8 J / g, molecular weight approximately 28 million) shown in Table 1 was used as the raw material powder. The PTFE fine powder A used here is a powder obtained by drying and granulating a material (emulsion polymerization product) consisting of PTFE particles (primary particles) produced by emulsion polymerization of tetrafluoroethylene. The specific gravity of PTFE fine powder A and the results of differential scanning calorimetry analysis using a differential scanning calorimeter (Shimadzu Corporation "DSC-60A") are shown in Table 1. The differential scanning calorimetry analysis using a differential scanning calorimeter was performed using the method described above.

[0097] 100 parts by mass of PTFE fine powder was kneaded with 18 parts by mass of solvent naphtha (Idemitsu Oil Co., Ltd.'s "Supersol FP-25", boiling point: 50°C to 180°C) as a liquid lubricant. The kneaded material was then placed in a molding machine and compression molded to obtain a block-shaped molded product. The block-shaped molded product was then continuously extruded into a sheet, passed through a rolling mill, and then passed through a heated roll (130°C to 220°C) to remove the liquid lubricant, and wound up on a roll to form a PTFE sheet with an average thickness of 320 μm. The film was then stretched 4 times in the machine direction (machine direction) at a roll temperature of 250°C to 280°C. The film was then gripped at both ends in the width direction with a chuck, and stretched 25 times in the transverse direction, which is perpendicular to the machine direction, in a 150°C atmosphere. The film was then heat-set by holding it at 285°C for 0.25 to 1 minute. This stretching resulted in porous membranes with a thickness of 7 μm, Test No. 1 and Test No. 2. The stretched sheet was passed through a heating furnace at 360° C. and sintered for 1.5 minutes, to obtain porous membranes, Test No. 1 and Test No. 2.

[0098] Next, PTFE fine powder (second heat of fusion 26.0 J / g, molecular weight approximately 5 million) was used as the raw material powder, and a PTFE sheet was prepared according to the following procedure, which served as a support film. Next, 100 parts by mass of PTFE fine powder was mixed with 23 parts by mass of solvent naphtha (Idemitsu Oil Co., Ltd.'s "Supersol FP-25") as a liquid lubricant. Next, the kneaded product was placed in a molding machine and compression molded to obtain a block-shaped molded product. Next, the block-shaped molded product was continuously extruded into a sheet, passed through a rolling roller, and then passed through a heated roll (130 ° C to 220 ° C) to remove the liquid lubricant, and wound up on a roll to form a PTFE sheet with an average thickness of 320 μm. Next, the roll temperature was 250 ° C to 280 ° C, and the stretched product was stretched 3.5 times in the longitudinal direction (flow direction). Next, both ends of the longitudinally stretched film were gripped with chucks in the width direction, and the film was stretched 23 times in the transverse direction, which is the direction perpendicular to the machine direction, in an atmosphere of 150°C. The film was then held at 285°C for 0.25 to 1 minute for heat setting. The stretched sheet was then passed through a heating furnace at 360°C and sintered for 1.5 minutes. This resulted in a support membrane with an average thickness of 8 μm, a maximum pore size of 235 nm, a mean flow pore size of 194 nm, a pore size ratio of 21.1%, and a Gurley time of 13 seconds.

[0099] Next, as shown in Figure 3, two layers of support membrane, two layers of porous membrane disposed between this pair of support membrane, and one layer of support membrane laminated between this pair of porous membrane, Test No. 1 and Test No. 2 porous membrane laminates were prepared. In the step of laminating the porous membrane of Test No. 1 and Test No. 2 on the support membrane, the porous membrane and support membrane of Test No. 1 and Test No. 2 were laminated, respectively, and heated at 370 ° C for 100 seconds, and the boundaries of each layer were heat-sealed and integrated. The average thickness of the porous membrane laminate of Test No. 1 was 34 μm. The average thickness of the porous membrane laminate of Test No. 2 was 36 μm.

[0100] [Test No. 3] Use PTFE fine powder B (second heat of fusion 17.0 J / g, molecular weight about 23 million) as raw material powder, have specific gravity and differential scanning calorimetry analysis result shown in table 1, knead with 100 mass parts of PTFE fine powder and 16 mass parts of solvent naphtha as liquid lubricant, and make longitudinal stretching 6 times, and make transverse stretching 25 times, except that, by the same process as No. 1 porous film laminate, obtain the porous film laminate of test No. 3 with an average thickness of 45 μ m.

[0101] [Test No. 4] Use PTFE fine powder C (second heat of fusion 16.8J / g, molecular weight about 22 million) as raw material powder, have specific gravity and differential scanning calorimetry analysis result shown in table 1, knead with 100 mass parts of PTFE fine powder and 16 mass parts of solvent naphtha as liquid lubricant, and make longitudinal stretching 4 times stretching ratio, transverse stretching 21 times stretching ratio, except that, by the same process as No. 1 porous membrane laminate, obtain the porous membrane laminate of test No. 4 with average thickness of 31 μ m.

[0102] <Evaluation> [Thermal analysis of raw materials using a differential scanning calorimeter] Differential scanning calorimetry was performed using a differential scanning calorimeter according to the following method. The sample was heated from room temperature to 380°C at a rate of 10°C / min (Pattern 1 (1st Run)), then cooled from 380°C to 100°C at a rate of -1°C / min (Pattern 2), and then heated from 100°C to 380°C at a rate of 10°C / min (Pattern 3 (2nd Run)). The endotherm obtained by integrating the 48°C section from the endset temperature of the peak in the range of 300°C to 360°C in the melting curve of Pattern 1 was defined as the first heat of fusion. Similarly to the first heat of fusion, the endotherm obtained by integrating the 48°C section from the endset temperature of the peak in the range of 300°C to 360°C in the melting curve of Pattern 3 was defined as the second heat of fusion.

[0103] [Pore size difference and pore size ratio] The pore size ratios of the porous membranes and porous membrane laminates of Test No. 1 to Test No. 4 were calculated by the following procedure. First, for the porous membranes and porous membrane laminates of Test No. 1 to Test No. 4, in accordance with ASTM F316-03 and JIS-K3832 (1990), propylene, 1,1,2,3,3,3-hexahydrofluoric acid oxide (PMI "GALWICK") with a surface tension of 15.9 mN / m was used as a reagent, and the pore size distribution was measured with a pore size distribution measuring instrument (PMI Perm Porometer "CFP-1500A"). Then, the maximum pore size [nm] and the mean flow pore size [nm] were determined from the pore size distribution, and the pore size difference and pore size ratio were calculated using the following formula. The larger the pore size ratio, the greater the variation in the pore size of the porous membrane. Pore ​​diameter difference of porous membrane [nm] = Maximum pore diameter G - Average flow pore diameter E Pore diameter difference of porous membrane laminate [nm] = Maximum pore diameter J - Average flow pore diameter K Pore diameter ratio of porous membrane [%] = {(G-E) / E}×100 Pore diameter ratio of porous membrane laminate [%] = {(J-K) / K}×100

[0104] [Gurley seconds] The Gurley seconds [seconds] of the porous membranes and porous membrane laminates of Test No. 1 to Test No. 4 were measured by the method described above.

[0105] [Polystyrene Particle Capture Rate] The polystyrene particle capture rates [%] of the porous membrane laminates of Test No. 1 to Test No. 4 were measured by passing an aqueous solution of 0.1% octoxynol (Dow Chemical Company's "Triton X-100") containing 12 ppb of Thermo Fisher Scientific polystyrene particles G40 (nominal diameter 0.04 μm) through the porous membrane laminate, and collecting the filtrate after 500 ml of the solution had passed through the porous membrane laminate. The concentration of polystyrene particles in the filtrate was calculated from the fluorescence intensity of the polystyrene particle filtrate measured using a spectrofluorometer (Shimadzu Corporation's "Spectrofluorophotometer RF-6000"). The particle retention rate was then calculated using the following formula: Particle retention rate [%] = {([Concentration of polystyrene particles in the feed solution] - [Concentration of polystyrene particles in the filtrate]) / [Concentration of polystyrene particles in the feed solution]} x 100

[0106] The evaluation results of the mean flow pore size, pore size ratio, Gurley seconds, and polystyrene particle capture rate of the porous membrane laminate of Test No. 1 to Test No. 4 are shown in Table 1. Also, Fig. 4 shows a surface image of the porous membrane of Test No. 1 photographed using a scanning electron microscope, Fig. 5 shows a surface image of the porous membrane of Test No. 2 photographed using a scanning electron microscope, and Fig. 6 shows a surface image of the porous membrane of Test No. 3 photographed using a scanning electron microscope. Fig. 7 shows a surface image of the porous membrane of Test No. 4 photographed using a scanning electron microscope.

[0107]

[0108] As shown in Table 1, the porous membrane laminates of Test No. 1 and Test No. 2, which have porous membranes with a mean flow pore size E of 75 nm or less and a difference between the maximum pore size G and the mean flow pore size E (pore size difference G-E) of 20 nm or less, had superior polystyrene particle capture rates compared to the porous membrane laminate of Test No. 3, which has a porous membrane with a mean flow pore size E of more than 75 nm, and the porous membrane laminate of Test No. 4, which has a porous membrane with a pore size difference G-E of more than 20 nm. Furthermore, as shown in Figures 4 to 6, the porous membranes of Test No. 1 and Test No. 2 have smaller gaps between the fibers in cross-section and smaller gap size variations than the porous membranes of Test No. 3 and Test No. 4. This is thought to be due to the pore size difference G-E of the porous membranes of Test No. 1 and Test No. 2 being narrower than the porous membranes of Test No. 3 and Test No. 4.

[0109] The above results demonstrate that the porous membrane laminate including the porous membrane has excellent particle capture performance, and therefore can be suitably used as a filter or the like that requires high-precision filtration performance.

[0110] 1 porous membrane, 2 support membrane, 10, 20 porous membrane stack.

Claims

1. A porous membrane mainly composed of polytetrafluoroethylene, The mean flow pore size E is 75 nm or less; A porous membrane having a pore size difference G-E between the maximum pore size G and the mean flow pore size E of 20 nm or less.

2. 2. The porous membrane of claim 1, wherein the pore size difference between the maximum pore size G and the mean flow pore size E is 15 nm or less.

3. The porous membrane according to claim 1, wherein the ratio of the pore size difference between the maximum pore size G and the mean flow pore size E to the mean flow pore size E {(G-E) / E} x 100 is 35% or less.

4. The porous membrane according to claim 1 or 2 is provided. The mean flow pore size K is 75 nm or less; A porous membrane stack, in which the pore size difference J-K between the maximum pore size J and the mean flow pore size K is 20 nm or less.

5. 5. The porous membrane stack according to claim 4, wherein the ratio of the pore size difference between the maximum pore size J and the mean flow pore size K to the mean flow pore size K, {(J-K) / K} x 100, is 35% or less.

6. One or more porous support membranes made mainly of polytetrafluoroethylene; The porous membrane stack according to claim 4 , wherein the support membrane is laminated on one or both sides of the porous membrane.

7. 7. The porous membrane stack according to claim 6, wherein the support membrane has a mean flow pore size of 200 nm or less.

8. A plurality of the porous membranes and a plurality of the support membranes are provided, 7. The porous membrane stack according to claim 6, wherein the porous membranes and the support membranes are stacked alternately, and the support membranes are stacked on both ends.

9. The porous membrane stack according to claim 4, wherein the mean flow pore size K is 60 nm or less.