Method for manufacturing deposition mask and method for manufacturing display device
Patent Information
- Application Number
- JP2023562617
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-11-10
- Filing Date
- 2022-11-10
- Publication Date
- 2024-10-09
- Estimated Expiration
- 2042-11-10
AI Technical Summary
Existing vapor deposition masks face issues with relative positional accuracy between mask bodies due to positioning errors during manufacturing, which affect the precision of pattern regions.
A method for manufacturing a vapor deposition mask involving patterning, bonding, and processing steps to form separation grooves, ensuring high relative positional accuracy of pattern regions, using a support substrate with controlled thermal expansion and alignment marks for precise alignment.
The method enhances the relative positional accuracy of pattern regions, enabling precise vapor deposition processes suitable for manufacturing display devices with small pixel sizes, maintaining alignment even under temperature changes.
Description
Technical Field
[0001] The present invention relates to a method for manufacturing a vapor deposition mask of and a method for manufacturing a display device. and
Background Art
[0002] Patent Document 1 discloses a vapor deposition mask having a frame body having a plurality of openings and a plurality of mask bodies respectively disposed in the plurality of openings. Here, one mask body is joined to each of the individual openings via a metal layer. In such a configuration, it is necessary to position the mask bodies with respect to each of the plurality of openings, and a positioning error may occur between the plurality of mask bodies.
Prior Art Documents
Patent Documents
[0003]
Patent Document 1
Summary of the Invention
[0004] The present invention provides a technique advantageous for improving the relative positional accuracy of a plurality of pattern regions in a vapor deposition mask.
[0005] A first aspect of the present invention relates to a method for manufacturing a vapor deposition mask, the method for manufacturing the vapor deposition mask including: a patterning step of patterning a mask substrate so that a plurality of pattern regions are formed on the mask substrate; after the patterning step, a bonding step of bonding the mask substrate and a support substrate to form a laminate; after the bonding step, and a processing step of processing the mask substrate so that the plurality of pattern regions in the laminate a are separated from each other. separation groove is formed
[0006] The second aspect of the present invention relates to a method for manufacturing a display device. The method for manufacturing the display device includes a vapor deposition step of performing vapor deposition on a substrate using a vapor deposition mask manufactured by the method for manufacturing the vapor deposition mask, and a processing step of processing the substrate that has undergone the vapor deposition step to obtain a display device.
[0007] one of the inventions disclosed in this specification The aspect relates to a vapor deposition mask. The vapor deposition mask includes a support substrate having a plurality of first openings and a plurality of second openings, a plurality of masks supported by the support substrate, and a plurality of members supported by the support substrate. Each mask includes a pattern region exposed through any one of the plurality of first openings, and each member includes an alignment mark exposed through any one of the plurality of second openings.
Brief Description of the Drawings
[0008]
Figure 1A
Figure 1B
Figure 1C
Figure 1D
Figure 1E
Figure 1F
Figure 1G
Figure 1H
Figure 2
Figure 3
Figure 4
Mode for Carrying Out the Invention
[0009] Hereinafter, embodiments will be described in detail with reference to the accompanying drawings. It should be noted that the following embodiments do not limit the invention according to the claims. Although a plurality of features are described in the embodiments, not all of these plurality of features are essential to the invention, and the plurality of features may be arbitrarily combined. Further, in the accompanying drawings, the same or similar configurations are denoted by the same reference numerals, and duplicate explanations are omitted.
[0010] Hereinafter, a method for manufacturing a vapor deposition mask according to an embodiment will be exemplarily described with reference to FIGS. 1A to 1H. Note that FIGS. 1A to 1H are schematic cross-sectional views of the structure to be described. First, the patterning process will be described with reference to FIGS. 1A to 1D. In the patterning process, the mask substrate 110 can be patterned so that a plurality of pattern regions are defined or formed on the mask substrate 110. FIG. 1A schematically shows the coating process. In the coating process, a photoresist can be coated on the mask substrate 110, whereby a photoresist film RF is formed. The mask substrate 110 can be, for example, a silicon substrate or a glass substrate.
[0011] FIG. 1B schematically shows a transfer process and a development process that can be performed after the coating process. In the transfer process, the pattern of the original plate can be sequentially transferred to a plurality of pattern formation regions PFR of the photoresist film RF using an exposure apparatus such as a stepper or a scanner. Also, in the transfer process, alignment marks can be transferred to a plurality of alignment mark regions AA of the photoresist film RF in the exposure apparatus. The alignment marks may be transferred simultaneously with the pattern of the original plate. In the transfer process, while the substrate stage on which the mask substrate 110 on which the photoresist film RF is formed is loaded is driven under the coordinate system of the exposure apparatus, the pattern of the original plate can be sequentially transferred to a plurality of pattern formation regions PFR. Also, in the transfer process, while the substrate stage is driven under the coordinate system of the exposure apparatus, a plurality of alignment marks can be transferred to a plurality of alignment mark regions AA. Therefore, for each of the plurality of pattern formation regions PFR, the pattern of the original plate is transferred according to the positioning accuracy of the substrate stage of the exposure apparatus, and for each of the plurality of alignment mark regions AA, alignment marks can be transferred according to the positioning accuracy of the substrate stage of the exposure apparatus. Thus, the relative positional accuracy of the plurality of patterns transferred to each of the plurality of pattern formation regions PFR and the alignment marks transferred to each of the plurality of alignment mark regions AA becomes high according to the positioning accuracy of the substrate stage. In the development process, a resist pattern RP can be formed by developing the photoresist film RF that has undergone the transfer process.
[0012] FIG. 1C schematically shows an etching process that can be performed after the development process. In the etching process, by etching the mask substrate 110 through the openings of the resist pattern RP, a plurality of pattern regions PR each including a plurality of grooves 13 and a plurality of alignment marks 12 can be formed. Since the plurality of pattern regions PR and the plurality of alignment marks 12 are those onto which the resist pattern RP is transferred, the relative positional accuracy of the plurality of pattern regions PR and the plurality of alignment marks 12 is high according to the positioning accuracy of the substrate stage of the exposure apparatus. In the etching process, a plurality of grooves 13 can be formed in the mask substrate 110 so that through holes are not formed in the mask substrate 110. In this case, a thinning process described later is performed. However, in the etching process, a plurality of grooves 13 may be formed in the mask substrate 110 so that through holes are formed in the mask substrate 110.
[0013] FIG. 1D schematically shows a resist stripping process that can be performed after the etching process. In the resist stripping process, the resist film RF can be stripped.
[0014] FIGS. 1E and 1F schematically show a bonding process. The bonding process can be performed after the patterning process. The patterning for forming the plurality of pattern regions PR described above is performed on the first surface S1 of the mask substrate 110, and in the bonding process, the support substrate 120 can be bonded to the side of the first surface S1 of the mask substrate 110. In the bonding process, the mask substrate 110 that has undergone the patterning process and a separately prepared support substrate 120 can be bonded to form a laminate ST. Here, in order to improve the bonding strength between the mask substrate 110 and the support substrate 120, before the bonding process, metal films 131 and 132 are formed on the mask substrate 110 and the support substrate 120, respectively, and in the bonding process, the metal film 131 and the metal film 132 may be bonded. In the bonding process, the mask substrate 110 and the support substrate 120 can be bonded, for example, by atomic diffusion bonding. In the bonding process, the mask substrate 110 and the support substrate 120 can be aligned using the alignment marks 12 formed on the mask substrate 110.
[0015] The support substrate 120 preferably has a sufficiently low coefficient of linear thermal expansion. The coefficient of linear thermal expansion of the support substrate 120 is, for example, smaller than that of the mask substrate 110. The coefficient of linear thermal expansion of the support substrate 120 is composed of, for example, an alloy containing nickel and cobalt, and the coefficient of linear thermal expansion is, for example, 0.5x10 -6 ( / °C) or less. The support substrate 120 can be composed of, for example, Invar. The support substrate 120 may be composed of a ceramic composite material containing amorphous silicon and titanium or crystalline silicon, and the coefficient of linear thermal expansion can be 0.5x10 -6 ( / °C) or less.
[0016] In one example, the support substrate 120 can be composed of, for example, a 32Ni-5Co alloy. In this case, the coefficient of linear thermal expansion is 0.2x10 -6 ( / °C), and when the temperature of the vapor deposition mask rises by 30°C, the amount of expansion per 100 mm is 0.2x10 -6 ( / °C) × 30 (°C) × 100 (mm) = 0.0006 mm = 0.6 μm. That is, vapor deposition can be performed with sufficient positional accuracy even in the manufacture of an OLED panel with a pixel size of 10 μm or less.
[0017] The support substrate 120 may have a plurality of first openings OP1 for exposing the plurality of pattern regions PR in the laminate ST, respectively, and a plurality of second openings OP2 for observing the plurality of alignment marks 12. The plurality of pattern regions PR are exposed through the plurality of first openings OP1, and the plurality of alignment marks 12 can be exposed through the plurality of second openings OP2.
[0018] The bonding process is carried out without heating or cooling. From another perspective, the bonding process can be carried out within a temperature range of 7°C or higher and 39°C or lower. Such conditions are advantageous for keeping the warpage of the laminate ST or the vapor deposition mask after the bonding process within an allowable range.
[0019] FIG. 1G schematically shows a thinning process. The thinning process can be carried out between the bonding process and the processing process described later. In the thinning process, the mask substrate 110 can be thinned so that a plurality of grooves 13 change into a plurality of through holes. In the thinning process, for example, the mask substrate 110 can be thinned by grinding or etching the second surface S2 (the surface opposite to the first surface S1) of the mask substrate 110.
[0020] FIG. 1H schematically shows a processing process. In the processing process, the mask substrate 110 can be processed so that a plurality of pattern regions PR (masks) in the laminate ST and a plurality of members 16 each including an alignment mark 12 are separated from each other. More specifically, in the processing process, separation grooves 15 can be formed between the plurality of pattern regions PR and the plurality of members 16 so that the plurality of pattern regions PR (masks) and the plurality of members 16 are separated from each other. Thereby, the vapor deposition mask M is completed. The separation grooves 15 make it difficult for the support substrate 120 to be affected by the deformation of the plurality of pattern regions PR due to temperature change, and also make it difficult for the plurality of pattern regions PR to be affected by the deformation of the support substrate 120 due to temperature change. After the separation process, the plurality of pattern regions PR separated from each other are supported by the support substrate 120. The width of the separation groove 15 (the width in a direction orthogonal to the direction in which the region between the adjacent pattern regions PR along the edge of the pattern region PR extends) is preferably larger than the width of the plurality of grooves 13 (the width in the above direction).
[0021] The vapor deposition mask M that can be connected as described above is suitable for manufacturing a display device. A method for manufacturing such a display device can include a vapor deposition step of performing vapor deposition on a substrate using the vapor deposition mask M, and a processing step of processing the substrate that has undergone the vapor deposition step to obtain a display device. In the vapor deposition step, for example, an organic EL light-emitting material can be vapor-deposited on the substrate through a plurality of through holes of the vapor deposition mask.
[0022] In one example, the thickness of the mask substrate 110 before the thinning process is 775 μm, and the thickness of the mask substrate 110 after the thinning process is 30 μm. In this case, in the patterning process, for example, a plurality of grooves 13 can be formed to have a depth that is 10% more than the thickness of the mask substrate 110 after the thinning process (that is, 30 μm × (100 + 10) / 100 = 33 μm).
[0023] In one example, before the bonding process is carried out, in a vacuum chamber with a vacuum pressure of 1x10 -4 Pa or less, a metal film 131, 132 such as titanium can be formed on the mask substrate 110 and the support substrate 120 by sputtering or evaporation. The thickness of the metal films 131, 132 can be, for example, in the range of 0.3 to 5 nm.
[0024] The mask substrate 110 and the support substrate 120 are typically composed of different materials from each other. In one example, the mask substrate 110 is made of silicon, and the support substrate 120 is made of an alloy of 32Ni - 5Co. In this case, the linear expansion coefficient of the mask substrate 110 is 2.6x10 -6 ( / ℃), and the linear expansion coefficient of the support substrate 120 is 0.2x10 -6 ( / ℃). Also, in one example, the size of the pattern region PR after the processing step can be 25.4 mm x 25.4 mm. In this example, the difference in the amount of expansion between the mask substrate 110 and the support substrate 120 per 1℃ increase in temperature is (2.6x10 -6 - 0.2x10 -6 ) × 1 × 25.4 = 0.00006096 mm = 0.061 μm. For a deposition mask used in the manufacture of an OLED panel with a pixel size of 10 μm or less, it is desirable to keep the difference in the amount of expansion within 1 μm, which is 10% of its pixel size. In the case of this example, 10x10 -3 ×0.1÷(0.061x10 -3) It is desirable to set the temperature difference at 16.4 °C. Therefore, if the set temperature in a general clean room is 23 °C, 23 ± 16.4 °C, that is, 7 to 39 °C is the temperature suitable for the bonding process. The greater the difference between the temperature during the bonding process and the temperature after the bonding process, the greater the warpage amount of the laminate ST or the vapor deposition mask M after the bonding process, making it impossible to maintain a constant distance between the pattern region PR and the wafer or to bring the two into contact. Therefore, the bonding process is preferably carried out within the range of 7 to 39 °C.
[0025] FIG. 2 shows a schematic plan view of the vapor deposition mask M manufactured by the above manufacturing method as viewed from the support substrate 120 side. FIG. 3 shows a schematic plan view of the vapor deposition mask M as viewed from the pattern region PR side. The vapor deposition mask M may include a support substrate 120 having a plurality of first openings OP1 and a plurality of second openings OP2, a plurality of pattern regions PR (masks) supported by the support substrate 120, and a plurality of members 16 supported by the support substrate. Each pattern region PR (mask) may include a pattern region PR exposed through any of the plurality of first openings OP1. All or part of the plurality of members 16 may include alignment marks 12 exposed through any of the plurality of second openings OP2.
[0026] Metal films 131, 132 (see FIG. 1H) may be disposed between the support substrate 120 and the pattern region PR (mask), and between the support substrate 120 and the plurality of members 16. The support substrate 120 is made of, for example, an alloy containing nickel and cobalt, and may have a linear expansion coefficient of 0.5x10 -6 ( / °C) or less. The plurality of pattern regions PR (masks) may be, for example, a silicon substrate or a glass substrate.
[0027] As schematically shown in FIG. 4, the plurality of pattern regions PR (masks) are aligned with respect to a lattice L defined by a plurality of alignment marks 12 provided on the plurality of members 16 respectively. The number of the plurality of members 16 is less than the number of the plurality of pattern regions PR (masks).
[0028] The invention is not limited to the above embodiments, and various changes and modifications are possible without departing from the spirit and scope of the invention. Therefore, claims are attached to disclose the scope of the invention.
Claims
1. a patterning step of patterning the mask substrate so that a plurality of pattern regions are formed on the mask substrate; a bonding step of bonding the mask substrate and a support substrate to form a laminate; a processing step of processing the mask substrate such that the plurality of pattern regions in the laminate are separated from each other; A method for producing a deposition mask comprising the steps of:
2. The bonding step is carried out without heating or cooling. The method for producing a deposition mask according to claim 1 .
3. The bonding step is carried out at a temperature ranging from 7° C. to 39° C. The method for producing a deposition mask according to claim 1 .
4. In the patterning step, a plurality of grooves are formed in the mask substrate so that no through holes are formed in the mask substrate, a thinning step of thinning the mask substrate so that the plurality of grooves are changed into a plurality of through holes is carried out between the bonding step and the processing step; The method for producing a deposition mask according to claim 1 .
5. The bonding step is performed after the patterning step. The method for producing a deposition mask according to claim 1 .
6. The support substrate is made of an alloy containing nickel and cobalt and has a linear expansion coefficient of 0.5×10 -6 ( / °C) or less, The method for producing a deposition mask according to claim 1 .
7. The support substrate is made of a ceramic composite material containing amorphous silicon and titanium or crystalline silicon, and has a linear expansion coefficient of 0.5×10 -6 ( / °C) or less, The method for producing a deposition mask according to claim 1 .
8. The mask substrate is a silicon substrate or a glass substrate. The method for producing a deposition mask according to claim 1 .
9. In the patterning step, an alignment mark is formed on the mask substrate, In the bonding step, the mask substrate and the support substrate are aligned using the alignment mark. The method for producing a deposition mask according to claim 1 .
10. the supporting substrate has a plurality of first openings for exposing the plurality of pattern regions in the laminate, respectively, and a second opening for observing the alignment mark; The method for producing a deposition mask according to claim 9 .
11. patterning to form the plurality of pattern areas is performed on a first surface of the mask substrate; In the bonding step, the support substrate is bonded to the first surface side of the mask substrate. The method for producing a deposition mask according to claim 1 .
12. In the bonding step, the first surface side of the mask substrate and the supporting substrate are bonded via a metal film. The method for producing a deposition mask according to claim 11 .
13. The bonding step bonds the mask substrate and the support substrate by atomic diffusion bonding. The method for producing a deposition mask according to claim 1 .
14. The patterning step includes: a coating step of coating a photoresist on the mask substrate to form a photoresist film; a transfer step of sequentially transferring a pattern of an original onto a plurality of pattern forming regions of the photoresist film using an exposure device; a developing step of developing the photoresist film to form a resist pattern; an etching step of forming the plurality of pattern areas by etching the mask substrate through openings in the resist pattern; The method for producing a deposition mask according to claim 1 , further comprising:
15. The processing step includes a step of forming a separation groove by which the plurality of pattern regions are separated from each other. The method for manufacturing a deposition mask according to claim 1 .
16. The processing step includes a step of forming a separation groove by which the plurality of pattern regions are separated from each other, The width of the separation groove is greater than the width of the plurality of grooves. The method for producing a deposition mask according to claim 4 .
17. a deposition step of performing deposition on a substrate using the deposition mask manufactured by the manufacturing method according to any one of claims 1 to 13; a processing step of processing the substrate that has been subjected to the deposition step to obtain a display device; A method for manufacturing a display device comprising the steps of: