Display device and method for manufacturing the same

The display device's innovative substrate design with a groove and support films addresses bending stress issues, improving durability and reducing manufacturing costs by facilitating easier bending and minimizing the non-display area.

KR103044465B1Active Publication Date: 2026-11-06SAMSUNG DISPLAY CO LTD

Patent Information

Application Number
KR1020220032525
Authority / Receiving Office
KR · KR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-03-16
Publication Date
2026-11-06
Estimated Expiration
2042-03-16

AI Technical Summary

Technical Problem

Flexible flat-panel displays are prone to defects during manufacturing due to bending stress, leading to increased costs and reduced lifespan, and there is a need to reduce the non-display region and bending stress.

Method used

A display device design featuring a substrate with a concave groove in the bending area, supported by support films with acute angled edges, and a bending protection layer to minimize bending stress and reduce the substrate's thickness in the bending region.

Benefits of technology

The design allows for easier bending of the substrate, reducing the radius of curvature and minimizing the non-display area, thereby enhancing durability and reducing manufacturing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 112022028208895-PAT00003_ABST
    Figure 112022028208895-PAT00003_ABST
Patent Text Reader

Abstract

The present invention relates to a display device capable of reducing the area of ​​a non-display region and bending stress. A display device according to one embodiment comprises: a substrate including a first flat region, a second flat region, and a bending region disposed between the first flat region and the second flat region and having a predetermined radius of curvature; a display unit that overlaps with the first flat region of the substrate and is disposed on one surface of the substrate to display an image; a first support film disposed on the other surface of the substrate that overlaps with the first flat region and overlaps with the first flat region; and a second support film disposed on the other surface of the substrate with the first support film and the bending region in between and overlapping with the second flat region, wherein the substrate includes a concave groove in the thickness direction of the substrate in the bending region, and the first support film includes a first flat portion that overlaps with the first flat region and a first bending portion that overlaps with the bending region and has a first inclination angle of an acute angle with respect to the other surface of the substrate.
Need to check novelty before this filing date? Find Prior Art

Description

Technology Field

[0001] The present invention relates to a display device and a method for manufacturing the same. Background Technology

[0002] Recently, various flat-panel display devices have been researched and developed. Flat-panel displays are thin and lightweight, which is expanding their range of applications. In addition, as flat-panel displays have recently become flexible, they are becoming more portable, and the range of applications is also increasing.

[0003] Flexible flat panel displays can be bent or folded, which is advantageous for reducing the size of the display or improving visibility from various angles. However, because the display is thin, defects can easily occur during the manufacturing process, manufacturing costs are high, and the lifespan of the display may be reduced due to stress caused by bending. The problem to be solved

[0004] The problem that the present invention aims to solve is to provide a display device capable of reducing the area of ​​the non-display region and bending stress.

[0005] The problems of the present invention are not limited to those mentioned above, and other unmentioned technical problems will be clearly understood by those skilled in the art from the description below. means of solving the problem

[0006] A display device according to one embodiment for solving the above problem comprises: a substrate including a first flat area, a second flat area, and a bending area disposed between the first flat area and the second flat area and having a predetermined radius of curvature; a display unit that overlaps with the first flat area of ​​the substrate and is disposed on one surface of the substrate to display an image; a first support film disposed on the other surface of the substrate that overlaps with the one surface of the substrate and overlaps with the first flat area; and a second support film disposed on the other surface of the substrate with the first support film and the bending area in between and overlaps with the second flat area, wherein the substrate includes a concave groove in the thickness direction of the substrate in the bending area, and the first support film includes a first flat portion that overlaps with the first flat area and a first bending portion that overlaps with the bending area and has a first angle of inclination of an acute angle with respect to the other surface of the substrate.

[0007] The above-mentioned first bending part can be bent to a predetermined first curvature.

[0008] The second support film may include a flat portion that overlaps with the second flat region and a second bending portion that overlaps with the bending region and has a second inclination angle of acute angle with respect to the other surface of the substrate.

[0009] The above second bending part can be bent to a predetermined second curvature.

[0010] The above substrate includes a first substrate, a first barrier layer, a second substrate, and a second barrier layer arranged sequentially, wherein the first barrier layer is located on one surface of the first substrate, and the first support film and the second support film are located on the other surface of the first substrate, and the groove may be formed in the first substrate.

[0011] The above groove may have a thickness thinner than the thickness of the first substrate.

[0012] The above groove has a thickness equal to the thickness of the first substrate, and the first barrier layer can be exposed by the groove.

[0013] The first barrier layer may include an inorganic material.

[0014] The above inorganic material may include at least one of a metal oxide, silicon oxide, and silicon nitride.

[0015] The above substrate may include an organic material.

[0016] The above substrate may contain polyimide, polyethylene napthalate, polyethyleneterephthalate (PET), polyarylate, polycarbonate, polyetherimide (PEI), or polyethersulfone.

[0017] The first substrate may be thicker than the thickness of the second substrate.

[0018] The above groove may have one end aligned with one end of the first bending part.

[0019] The above groove may have one end aligned with one end of the first bending part and the other end aligned with one end of the second bending part.

[0020] The display device further includes an optical member disposed on the display portion and a bending protection layer that covers a bending region of the substrate and contacts one side of the optical member.

[0021] The bending protection layer may become thinner from the side of the optical member toward the bending region, and may have a constant thickness in the bending region.

[0022] An embodiment of a display device for solving the above problem comprises the steps of: preparing a display panel including a substrate in which a first flat region, a bending region, and a second flat region are defined along a first direction, and a display member disposed in the first flat region of the substrate; combining a first support film, a second support film, and an optical member with the display panel; forming a bending protection layer in the bending region of the substrate; combining a window member on the optical member of the substrate; forming a first bending portion by laser patterning that overlaps the bending region and has an acute angle of inclination on one side of the first support film, and forming a groove in the bending region of the substrate by laser patterning; and bending the bending region of the substrate and the first bending portion of the first support film, wherein the groove may be concave in the thickness direction of the substrate.

[0023] The step of forming by the laser patterning above may further form a second bending portion having an acute angle of inclination on one side of the second support film by laser patterning.

[0024] The first bending part above may overlap with the bending area.

[0025] The second bending part above may overlap with the bending area.

[0026] The step of forming the bending protection layer above can be formed such that the thickness of the bending protection layer becomes thinner from the side of the optical member toward the bending region, and remains constant in the bending region.

[0027] A display device of another embodiment for solving the above problem comprises: a display panel including a display area and a non-display area; a circuit board including a first planar area disposed in the non-display area and a second bending area extending from the first planar area and having a predetermined curvature; and a display driving circuit attached to the circuit board, wherein the circuit board may have a concave groove in the thickness direction on the other surface that overlaps with one surface disposed on the display panel.

[0028] The above circuit board includes an insulating film defining the shape of the circuit board; a wiring layer disposed between the insulating film and the display panel; and an insulating layer covering at least a portion of the wiring layer, and the groove may be formed on the insulating film.

[0029] The above insulating layer may not overlap with the above groove.

[0030] The above groove can be formed over the entire bending area of ​​the circuit board with a width equal to the width of the bending area.

[0031] The above grooves are provided in multiple numbers, and at least one groove may have one end that overlaps with the boundary between the planar area and the bending area.

[0032] The above display device may further include a filler material that fills the space defined by the side of the display panel and the other side of the circuit board.

[0033] The above filler can come into contact with the wiring layer in the bending area.

[0034] Specific details of other embodiments are included in the detailed description and drawings. Effects of the invention

[0036] According to a display device according to one embodiment, the thickness of the substrate in the bending area is reduced by a groove or opening disposed in the bending area of ​​the substrate, thereby reducing the radius of curvature and preventing an increase in the non-display area, and the size of the display device can be effectively reduced because the substrate can be easily bent.

[0037] In addition, according to one embodiment of the display device, one side of the support film supporting the substrate includes an edge portion having an acute angle inclined surface, so that the edge portion supports the substrate bending region and can reduce the bending stress applied to the substrate by bending.

[0038] The effects according to the embodiments are not limited to those exemplified above, and a wider variety of effects are included in this specification. Brief explanation of the drawing

[0039] FIG. 1 is a perspective view schematically showing a part of a display device according to one embodiment. FIG. 2 is a cross-sectional view of a part of a display device in an unfolded state according to one embodiment. FIG. 3 is a cross-sectional view of a part of a display device in a bent state according to one embodiment. FIG. 4 is a cross-sectional view of a part of a display device in an unfolded state according to another embodiment. FIG. 5 is a cross-sectional view of a part of a display device in a bent state according to another embodiment. FIG. 6 is an enlarged view of the substrate of FIG. 2 according to one embodiment. FIG. 7 is an enlarged view of the substrate of FIG. 2 according to another embodiment. FIG. 8 is a side view of a display device according to one embodiment. FIG. 9 is a detailed side view of a display device according to one embodiment. FIG. 10 is a flowchart of a method for manufacturing a display device according to one embodiment. FIGS. 11 to 15 are cross-sectional views of the process steps of a method for manufacturing a display device according to one embodiment. FIG. 16 is a side view of a display device according to another embodiment of the present invention. FIG. 17 is a side view of a display device according to another embodiment of the present invention. FIG. 18 is a perspective view showing a display device according to one embodiment. FIG. 19 is a plan view showing a display device according to one embodiment. FIG. 20 is a side view of a circuit board in an unfolded state according to one embodiment. FIG. 21 is a side view of a display device according to one embodiment. FIG. 22 is a side view of a circuit board in an unfolded state according to another embodiment. FIG. 23 is a side view of a display device according to another embodiment. FIG. 24 is a side view of a display device according to another embodiment. Specific details for implementing the invention

[0040] The advantages and features of the present invention and the methods for achieving them will become clear by referring to the embodiments described below in detail together with the accompanying drawings. However, the present invention is not limited to the embodiments disclosed below but may be implemented in various different forms. These embodiments are provided merely to ensure that the disclosure of the present invention is complete and to fully inform those skilled in the art of the scope of the invention, and the present invention is defined only by the scope of the claims.

[0041] When elements or layers are referred to as being "on" another element or layer, this includes cases where another layer or element is interposed directly on or in the middle of another element. Throughout the specification, the same reference numerals refer to the same components. Shapes, sizes, ratios, angles, numbers, etc., disclosed in the drawings for describing embodiments are exemplary and therefore the invention is not limited to the depicted details.

[0042] Although terms such as "first," "second," etc., are used to describe various components, it goes without saying that these components are not limited by these terms. These terms are used merely to distinguish one component from another. Therefore, it goes without saying that the first component mentioned below may also be the second component within the technical scope of the present invention.

[0043] The features of each of the various embodiments of the present invention may be combined or combined with one another, either partially or wholly, and may technically enable various interlocking and operation. Each embodiment may be implemented independently of one another or may be implemented together in an associated relationship.

[0044] FIG. 1 is a perspective view schematically showing a part of a display device according to one embodiment, FIG. 2 is a cross-sectional view of a part of a display device according to one embodiment in an unfolded state, and FIG. 3 is a cross-sectional view of a part of a display device according to one embodiment in a bent state.

[0045] Referring to FIGS. 1 to 3, a display device (10) according to one embodiment may be applied to portable electronic devices such as a mobile phone, a smartphone, a tablet PC, a mobile communication terminal, an electronic notebook, an e-book, a PMP (portable multimedia player), a navigation system, a UMPC (Ultra Mobile PC), etc. Alternatively, a display device (10) according to one embodiment may be applied to a television, a laptop, a monitor, an advertising board, or a display unit of the Internet of Things (IOT). Alternatively, a display device (10) according to one embodiment may be applied to a wearable device such as a smart watch, a watch phone, a glasses-type display, and a head-mounted display (HMD). Alternatively, a display device (10) according to one embodiment may be applied to a center information display (CID) placed on the instrument panel of a vehicle, the center fascia of a vehicle, the dashboard of a vehicle, a room mirror display replacing the side mirror of a vehicle, or a display placed on the back of the front seat as entertainment for the rear seat of a vehicle.

[0046] A display device (10) according to one embodiment may be a light-emitting display device such as an organic light-emitting display device using an organic light-emitting diode, a quantum dot light-emitting display device including a quantum dot light-emitting layer, an inorganic light-emitting display device including an inorganic semiconductor, and a micro light-emitting display device using a micro or nano light-emitting diode (micro LED or nano LED). Hereinafter, the display device (10) according to one embodiment has been described mainly as being an organic light-emitting display device, but the present invention is not limited thereto.

[0047] In the display device according to the present embodiment, as shown in FIG. 1, a part of the substrate (100), which is part of the display device (10), is bent, so that a part of the display device has a bent shape similar to the substrate (100).

[0048] As illustrated in FIG. 1, the substrate (100) provided by the display device (10) according to the present embodiment has a first flat area (1FA), a bending area (BA), and a second flat area (2FA). The first flat area (1FA) is formed as a rectangular plane having a long side in a first direction (X-axis direction) and a short side in a second direction (Y-axis direction) that intersects the first direction (X-axis direction). The bending area (BA) is located between the first flat area (1FA) and the second flat area (2FA) in the first direction (X-axis direction).

[0049] As shown in FIG. 1, the substrate (100) is bent in a bending region (BA) around a bending axis (BAX) extended in a second direction (+y direction), and in this case, the second flat region (2FA) is placed on the lower surface of the first flat region (1FA), so that the second flat region (2FA) can overlap with the first flat region (1FA) in a third direction (Z-axis direction), which is the thickness direction of the substrate (100).

[0050] The bending area (BA) may be an area defined by a first boundary (BL1) adjacent to the first flat area (1FA) in the first direction (X-axis direction) and a second boundary (BL2) spaced apart from the first boundary (BL1) in the first direction (X-axis direction). The bending area (BA) may be an area that is bent with a predetermined radius of curvature when the display device (10) is bent in one direction. In this case, the radius of curvature of the display device (10) may be defined as the radius of a generally circular shape formed when the bending area (BA) is bent.

[0051] The display device (10) may include a display area (DA) for displaying an image and a non-display area (NDA) placed around the display area (DA).

[0052] The display area (DA) includes multiple pixels and can emit light generated from each pixel in a display direction. For example, the display direction may be a third direction (Z-axis direction).

[0053] A non-display area (NDA) may be arranged adjacent to a display area (DA) in the first direction (X-axis direction). Signal wiring or driving circuits for applying a signal to a display unit (400) described later may be arranged in the non-display area (NDA). The non-display area (NDA) may further include a bending area (BA). The bending area (BA) may be included within the non-display area (NDA). A bending axis (BAX) may be located on the non-display area (NDA) of the first flat area (1FA).

[0054] In the drawing, the boundary of the bending area (BA) is depicted as not overlapping with the boundary of the display area (DA) and the non-display area (NDA); however, this is not limited thereto, and it is understood that the boundary of the bending area (BA) adjacent to the display area (DA) may overlap with the boundary of the display area (DA) and the non-display area (NDA).

[0055] The substrate (100) may include a first substrate (110) and a second substrate (130) disposed on the first substrate (110) in a second direction (+y direction).

[0056] The first substrate (110) and the second substrate (130) can be formed from a flexible material capable of bending, folding, rolling, etc., and as an optional embodiment, the first substrate (110) and the second substrate (130) can be formed from an organic material. For example, the first substrate (110) and the second substrate (130) may include an organic material with excellent heat resistance and durability, such as polyimide, polyethylenenapthalate, polyethyleneterephthalate (PET), polyarylate, polycarbonate, polyetherimide (PEI), or polyethersulfone.

[0057] The first substrate (110) may have a thickness (t1) greater than the thickness (t2) of the second substrate (130). In a non-limiting example, the first substrate (110) may have a thickness (t1) of about 6 to 13 μm, preferably a thickness (t1) of 6 to 10 μm. The second substrate (130) may have a thickness (t2) of about 1 to 6 μm, preferably a thickness (t2) of 3 to 6 μm.

[0058] As illustrated in FIG. 2, the first substrate (110) may have a groove (100a) corresponding to a bending region (BA). The groove (100a) has a concave shape in the third direction (Z-axis), which is the thickness direction of the first substrate (110). Additionally, the groove (100a) has a depth (t3) that is thinner than or equal to the thickness (t1) of the first substrate (110) in the third direction (Z-axis) of the first substrate (110).

[0059] For convenience of explanation, the surface on the substrate (100) where the display part (400), which will be described later, is placed is referred to as one surface.

[0060] The display device (10) may further include a support film (210, 220) disposed on the other side of the substrate (100) that overlaps with one side of the substrate (100). The support film (210, 220) is disposed on one side of the first substrate (100) in the opposite direction of the second substrate (130).

[0061] The support film (210, 220) can prevent the substrate (100) from bending due to external force or mitigate the degree of bending. The support film (210, 220) can maintain the substrate (100) in a relatively flat state even when external force is applied.

[0062] The support film (210, 220) may include a material having rigidity or semi-rigidity. Specifically, the support film (500) may be made of a metal material such as stainless steel (SUS) or aluminum, or a polymer such as polymethyl methacrylate (PMMA), polycarbonate (PC), polyvinyl alcohol (PVA), acrylonitrile-butadiene-styrene (ABS), or polyethylene terephthalate (PET).

[0063] The support film (210, 220) includes a first support film (210) and a second support film (220) separated from each other in a first direction (X-axis direction 1). The thicknesses of the first support film (210) and the second support film (220) may be the same, but are not limited thereto.

[0064] The first support film (210) includes an edge portion (210-e) having a predetermined angle of inclination on a first side facing the second support film (220). The angle of inclination has an acute angle of inclination with respect to the other side of the substrate (100), and may be an acute angle of 1° to 89°, and preferably may be in the range of 20° to 70°. In other words, the edge portion (210-e) of the first support film (210) is formed to be inclined with respect to the thickness direction (Z direction), and the thickness becomes thinner as it moves toward the bending region (BA) direction relative to the bending axis (BAX). That is, the thickness of the edge portion (210-e) of the first support film (210) becomes thinner as it moves toward the outer edge of the first support film (210).

[0065] One end of the edge portion (210-e) can be aligned with one end of the groove (100a) of the substrate (100).

[0066] The edge portion (210-e) may include a flat portion (210-ef) that overlaps with the first flat area and a bending portion (210-eb) that overlaps with the bending area. When the display device (10) is bent in one direction, the bending portion (210-eb) of the first support film (210) is bent with a predetermined radius of curvature.

[0067] The flat portion (210-ef) of the edge portion (210-e) overlaps with the first flat region (1FA) of the substrate (100), and the bending portion (210-eb) of the edge portion (210-e) overlaps with the bending region (BA) of the substrate (100).

[0068] The bending portion (210-eb) of the edge portion (210-e) can be aligned with one end of the groove (100a) of the substrate (100).

[0069] The second support film (220) may have a straight side facing the first support film (210). That is, the angle of inclination of the side of the second support film (220) may be approximately 90 degrees.

[0071] FIG. 4 is a cross-sectional view of a part of a display device in an unfolded state according to another embodiment, and FIG. 5 is a cross-sectional view of a part of a display device in a bent state according to another embodiment.

[0072] The display device (11) described with reference to FIGS. 4 and 5 differs from the display device (10) described with reference to FIGS. 1 to 3 only in the second support film (221) and the groove (100b), so a detailed description of the same components and structure is omitted.

[0073] As illustrated in FIGS. 4 and 5, the support films (210, 221) comprise a first support film (210) and a second support film (221) separated from each other in a first direction (X-axis direction 1). The thicknesses of the first support film (210) and the second support film (221) may be the same, but are not limited thereto. The first support film (210) and the second support film (221) may be arranged to partially overlap with the bending region (BA).

[0074] The first support film (210) includes an edge portion (210-e) having an angle of inclination on a first side facing the first support film (210).

[0075] The edge portion (210-e) of the first support film (210) is formed at an angle with respect to the thickness direction (Z direction), and the thickness becomes thinner as it moves toward the bending region (BA) direction relative to the bending axis (BAX1). That is, the edge portion (210-e) of the first support film (210) becomes thinner as it moves toward the outer edge of the first support film (210).

[0076] One end of the edge portion (210-e) can be aligned with one end of the groove (100a) of the substrate (100).

[0077] The edge portion (210-e) may include a flat portion (210-ef) and a bending portion (210-eb). The bending portion (210-eb) of the edge portion (210-e) is bent with a first curvature when the display device (11) is bent in one direction. The flat portion (210-ef) of the edge portion (210-e) overlaps with the first flat region (1FA) of the substrate (100), and the bending portion (210-eb) of the edge portion (210-e) overlaps with the bending region (BA) of the substrate (100). The bending portion (210-eb) has a first acute angle of inclination with respect to the other surface of the substrate (100) (the surface on which the first support film (210) is placed).

[0078] The second support film (221) includes an edge portion (221-e) having an angle of inclination on a first side facing the first support film (210). The edge portion (221-e) of the second support film (221) is formed to be inclined with respect to the thickness direction (Z direction), and its thickness decreases as it moves toward the bending region (BA) direction relative to the bending axis (BAX2). That is, the edge portion (221-e) of the second support film (221) becomes thinner as it moves toward the outer edge of the second support film (221).

[0079] One end of the edge portion (221-e) can be aligned with one end of the groove (100a) of the substrate (100).

[0080] The edge portion (221-e) may include a flat portion (221-ef) and a bending portion (221-eb). The edge portion (221-e) is bent with a second curvature when the display device (11) is bent in one direction. It has a second angle of inclination that is acute with respect to the other side of the substrate (100) (the side on which the first support film (210) is placed).

[0081] The flat portion (221-ef) of the edge portion (221-e) overlaps with the first flat region (1FA) of the substrate (100), and the bending portion (221-eb) of the edge portion (210-e) overlaps with the bending region (BA) of the substrate (100).

[0082] The home (100b) has one end aligned with one end of the bending portion (210-eb) and the other end aligned with one end of the bending portion (221-eb).

[0083] FIG. 6 is an enlarged view of the substrate of FIG. 2 according to one embodiment, and FIG. 7 is an enlarged view of the substrate of FIG. 2 according to another embodiment.

[0084] Referring to FIG. 6, the substrate (100) may include a first substrate (110), a first barrier layer (120), a second substrate (130), and a second barrier layer (140) in a second direction (+y direction). A second substrate (130) is disposed on the first substrate (110), and a first barrier layer (120) is disposed between the first substrate (110) and the second substrate (130). A second barrier layer (140) is disposed on the second substrate (130).

[0085] The first barrier layer (120) is a film for protecting the first substrate (110), which is vulnerable to moisture permeability, and is disposed on the first substrate (110). The first barrier layer (120) includes an inorganic material. The inorganic material includes at least one of a metal oxide, a silicon oxide, and a silicon nitride. Additionally, the first barrier layer (120) may be composed of a plurality of inorganic films that are alternately stacked. For example, the barrier layer (BR) may be formed as a multilayer film in which one or more inorganic films selected from a silicon nitride layer, a silicon oxynitride layer, a silicon oxide layer, a titanium oxide layer, and an aluminum oxide layer are alternately stacked.

[0086] The second barrier layer (140) is a film for protecting the second substrate (130), which is vulnerable to moisture permeability, and is disposed on the second substrate (130). The second barrier layer (140) may be composed of a plurality of inorganic films that are alternately stacked. For example, the barrier layer (BR) may be formed as a multilayer film in which one or more inorganic films selected from a silicon nitride layer, a silicon oxynitride layer, a silicon oxide layer, a titanium oxide layer, and an aluminum oxide layer are alternately stacked.

[0087] As illustrated in FIG. 6, the first substrate (110) is provided with a groove (100a-1) corresponding to a bending region (BA). The groove (100a-1) has a concave shape in the third direction (Z-axis), which is the thickness direction of the first substrate (110). Additionally, the groove (100a-1) has a depth (t3) that is thinner than or equal to the thickness (t1) of the first substrate (110) in the third direction (Z-axis) of the first substrate (110).

[0088] As illustrated in FIG. 7, when the groove (100a-2) has a depth (t3) equal to the thickness (t1) of the first substrate (110) in the third direction (Z-axis) of the first substrate (110), the groove (100a-2) is opened. When the groove (100a-2) of the first substrate (110) is opened, the first barrier layer (BR) is exposed through the groove (100a-2).

[0089] FIG. 8 is a side view of a display device according to one embodiment.

[0090] Referring to FIG. 8, the display device (10) may include a display portion (400), an optical member (500), and a window member (800) on a substrate (100) described in one embodiment of FIG. 3. The display device (10) may further include a cover film (300).

[0091] The display portion (400) includes a thin film transistor layer (TFTL), a light-emitting element layer (EML), and an encapsulation layer (TFEL).

[0092] A thin film transistor layer (TFTL) can be placed in a display area (DA) and a non-display area (NDA) of a substrate (100). The thin film transistor layer (TFTL) includes thin film transistors.

[0093] The light-emitting element layer (EML) may be disposed on the thin-film transistor layer (TFTL). The light-emitting element layer (EML) may be disposed on the display area (DA). The light-emitting element layer (EML) includes light-emitting elements disposed on the light-emitting parts.

[0094] The encapsulation layer (TFEL) may be disposed on the light-emitting element layer (EML). The encapsulation layer (TFEL) may be disposed in the display area (DA) and non-display area (NDA) of the main area (MA). The encapsulation layer (TFEL) comprises at least one inorganic film and at least one organic film for encapsulating the light-emitting element layer.

[0095] A touch sensing unit (not shown) may be disposed on the encapsulation layer (TFEL). The touch sensing unit includes a plurality of touch electrodes driven by a capacitive method to detect a user's touch. The touch sensing unit includes a plurality of touch wirings connecting the plurality of touch electrodes and the plurality of touch pads.

[0096] A window member (800) is positioned on a substrate (100) on which a display unit (400) is located, and protects the display panel from external impacts and scratches. When viewed as a planar structure, the window member (800) may include a light-transmitting area (TA) and a light-blocking area (BLA). The light-transmitting area (TA) is an area through which light is transmitted, and an image provided by the display panel can be provided to the user by passing through the light-transmitting area (TA). The light-blocking area (BLA) may be an area that blocks light transmission. In some embodiments, the light-blocking area (BLA) may be located around the light-transmitting area (TA) and may surround the light-transmitting area (TA). In some embodiments, the light-transmitting area (TA) may overlap with the display area (DA), and the light-blocking area (BLA) may overlap with the non-display area (NDA). That is, the light-blocking area (BLA) may cover the non-display area (NDA).

[0097] The window member (800) may include a window (810) and a light-blocking member (820) when viewed as a laminated structure.

[0098] The window (810) may be made of a material including glass, sapphire, plastic, etc.

[0099] A light-blocking member (820) may be located on one side of a window (810) facing a display unit (400). The light-blocking member (820) may define a light-blocking area (BLA) of the window member (800). In some embodiments, the light-blocking member (820) may be made of a colored organic layer and may be formed on one side of the window (810) by a coating method or a printing method. Alternatively, in another embodiment, the light-blocking member (820) may be formed on a base layer such as a separate transparent film, and the base layer on which the light-blocking member (820) is formed may be attached to one side of the window (810).

[0100] A bonding layer (600) may be positioned between a window member (800) and a display structure (DS) including a display portion (400) to bond the window member (800) and the display structure (DS). Here, the display structure (DS) includes a substrate (100), a display portion (400), and an optical member (500). The bonding layer (600) may be formed to fill the entire space between the light-transmitting area (TA) of the window member (800) and the display structure (DS). In some embodiments, the bonding layer (600) may be formed to further fill a portion of the space between the light-blocking area (BLA) of the window member (800) and the display structure (DS).

[0101] The bonding layer (600) may be made of ultraviolet light-curing resin, and in some embodiments, the bonding layer (600) may be made of optical clear resin (OCR). The bonding layer (600) is initially applied to the window member (800) in a liquid or paste state and may be cured by ultraviolet light (UV) after the display structure (DS) is laminated.

[0102] The bonding layer (600) can come into contact with one side of the window (810) among the window members (800).

[0103] The window (810) may be an inorganic material such as glass, or an organic material such as plastic or polymer. To prevent a decrease in the visibility of the image due to external light reflection, an optical member (500) may be additionally placed between the display unit (400) and the window (810).

[0104] When an optical member (500) is placed between the display unit (400) and the window (810), the bonding layer (600) may further contact the upper surface of the optical member (500).

[0105] The bonding layer (600) may initially be in a liquid or paste state, and some spreading may occur when the display structure (DS) and the window member (800) are bonded. Accordingly, the bonding layer (600) may come into further contact with one side of the light-blocking member (820) and may come into further contact with the side of the optical member (500).

[0106] The optical member (500) can cover the display area (DA) of the substrate (100) and cover a part of the non-display area (NDA), for example (fan-out area (not shown)).

[0107] The bending protection layer (700) may be disposed on the first flat region (1FA) and the bending region (BA) of the second substrate (130) where the optical member (500) is not disposed. Additionally, the bending protection layer (700) may be disposed on a part of the second flat region (2FA) adjacent to the bending region (BA) of the second substrate (130).

[0108] The bending protection layer (700) can be formed such that the thickness in the bending region (BA) is thinner than the thickness in the first flat region (1FA).

[0109] The bending protection layer (700) may become thinner as it goes from the side of the optical member (500) toward the bending region (BA), and the thickness within the bending region (BA) may be constant.

[0110] The bending protection layer (700) is located on the side of the optical member (500), but the bending protection layer (700) or its constituent material may not be located on the upper surface (one side on the window side) of the optical member (500). In the drawing, an example is shown where the height of the upper surface of the bending protection layer (700) is the same as the height of the upper surface of the optical member (500) so that the bending protection layer (700) completely covers the side of the optical member (500), but the height of the upper surface of the optical member (500) may be lower so that a portion of the upper side of the optical member (500) is exposed.

[0111] The display device (10) may further include a filler (not shown) in the groove of the substrate (100) and in the space between the first support film (210) and the second support film (220). The filler (not shown) may be formed by injecting a liquid or paste-like substance into the groove and in the space between the first support film (210) and the second support film (220) and curing it. The filler (not shown) may be provided with a substance having adhesive properties, and as it is cured by ultraviolet (UV) light or heat, it may prevent or minimize deformation of the substrate (100) by a restoring force that attempts to restore the substrate (100) to its state before bending.

[0112] The cover film (300) is placed on the lower surface of the first support film (210). The cover film (300) can be placed between the first support film (210) and the second support film (220) in a third direction (Z-axis direction) while the substrate (100) is bent.

[0113] The cover film (300) may be formed from a film having excellent flexibility, insulation, and heat resistance properties, and may be formed from, for example, polyimide, but is not limited thereto.

[0114] The cover film (300) can be non-overlapping with the edge portion (210-e) of the first support film (210).

[0115] FIG. 9 is a detailed side view of a display device according to one embodiment. Since FIG. 9 is a side view of a display device for showing the display portion (400) of FIG. 8 in detail, the description of the same components is omitted.

[0116] Referring to FIG. 9, the substrate (100) includes a plurality of first substrates (110) and second substrates (130), and a barrier film (120, 140) may be disposed on each substrate (110, 130).

[0117] The active layer (ACT), source electrode (S), and drain electrode (D) of a thin-film transistor (ST) may be disposed on the barrier film (140). The active layer (ACT) of the thin-film transistor (ST) includes polycrystalline silicon, single-crystal silicon, low-temperature polycrystalline silicon, amorphous silicon, or oxide semiconductor. The active layer (ACT) that overlaps with the gate electrode (G) in the third direction (Z-axis direction), which is the thickness direction of the substrate (100), may be defined as a channel region. The source electrode (S) and drain electrode (D) are regions that do not overlap with the gate electrode (G) in the third direction (Z-axis direction), and may have conductivity by doping silicon semiconductor or oxide semiconductor with ions or impurities.

[0118] A gate insulating film (413) may be disposed on the active layer (ACT), source electrode (S), and drain electrode (D) of the thin-film transistor (ST). The gate insulating film (413) may be formed of an inorganic film, for example, a silicon nitride layer, a silicon oxynitride layer, a silicon oxide layer, a titanium oxide layer, or an aluminum oxide layer.

[0119] A gate electrode (G) of a thin-film transistor (ST) may be disposed on the gate insulating film (413). The gate electrode (G) may overlap with the active layer (ACT) in a third direction (Z-axis direction). The gate electrode (G) may be formed as a single layer or a multilayer made of any one of molybdenum (Mo), aluminum (Al), chromium (Cr), gold (Au), titanium (Ti), nickel (Ni), neodymium (Nd), and copper (Cu), or an alloy thereof.

[0120] A first interlayer insulating film (414-1) may be disposed on the gate electrode (G) of a thin-film transistor (ST). The first interlayer insulating film (414-1) may be formed of an inorganic film, for example, a silicon nitride layer, a silicon oxynitride layer, a silicon oxide layer, a titanium oxide layer, or an aluminum oxide layer. The first interlayer insulating film (414-1) may be formed of a plurality of inorganic films.

[0121] A capacitor electrode (CAE) may be disposed on the first interlayer insulating film (414-1). The capacitor electrode (CAE) may overlap with the gate electrode (G1) of the first thin-film transistor (ST1) in the third direction (Z-axis direction). Since the first interlayer insulating film (414-1) has a predetermined dielectric constant, a capacitor may be formed by the capacitor electrode (CAE), the gate electrode (G1), and the first interlayer insulating film (141) disposed between them. The capacitor electrode (CAE) may be formed as a single layer or a multilayer made of any one of molybdenum (Mo), aluminum (Al), chromium (Cr), gold (Au), titanium (Ti), nickel (Ni), neodymium (Nd), and copper (Cu), or an alloy thereof.

[0122] A second interlayer insulating film (414-2) may be disposed on the capacitor electrode (CAE). The second interlayer insulating film (414-2) may be formed of an inorganic film, for example, a silicon nitride layer, a silicon oxynitride layer, a silicon oxide layer, a titanium oxide layer, or an aluminum oxide layer. The second interlayer insulating film (414-2) may be formed of a plurality of inorganic films.

[0123] A first anode connection electrode (ANDE1) may be disposed on the second interlayer insulating film (414-2). The first anode connection electrode (ANDE1) may be connected to the drain electrode (D) of the thin-film transistor (ST) through a first connection contact hole (ANCT) penetrating the gate insulating film (413), the first interlayer insulating film (414-1), and the second interlayer insulating film (414-2). The first anode connection electrode (ANDE) may be formed as a single layer or a multilayer made of any one of molybdenum (Mo), aluminum (Al), chromium (Cr), gold (Au), titanium (Ti), nickel (Ni), neodymium (Nd), and copper (Cu), or an alloy thereof.

[0124] A first flattening film (416) for flattening the step difference caused by the thin-film transistor (ST1) may be disposed on the first anode connection electrode (ANDE1). The first flattening film (416) may be formed from an organic film such as an acrylic resin, an epoxy resin, a phenolic resin, a polyamide resin, or a polyimide resin.

[0125] A second anode connecting electrode (ANDE2) may be disposed on the first flattening film (416). The second anode connecting electrode (ANDE2) may be connected to the first anode connecting electrode (ANDE1) through a second connecting contact hole (ANCT2) that penetrates the first flattening film (416). The second anode connecting electrode (ANDE2) may be formed as a single layer or a multilayer made of any one of molybdenum (Mo), aluminum (Al), chromium (Cr), gold (Au), titanium (Ti), nickel (Ni), neodymium (Nd), and copper (Cu), or an alloy thereof.

[0126] A second planarization film (418) may be disposed on the second anode connection electrode (ANDE2). The second planarization film (418) may be formed from an organic film such as an acrylic resin, an epoxy resin, a phenolic resin, a polyamide resin, or a polyimide resin.

[0127] Light-emitting elements (LELs) and a bank (419) may be disposed on the second planarization film (418). Each of the light-emitting elements (LELs) includes a pixel electrode (171), a light-emitting layer (172), and a common electrode (173).

[0128] The pixel electrode (171) can be placed on the second flattening film (418). The pixel electrode (171) can be connected to the second anode connecting electrode (ANDE2) through a third connecting contact hole (ANCT3) that penetrates the second flattening film (418).

[0129] In a top emission structure that emits light in the direction of a common electrode (173) based on a light-emitting layer (172), the pixel electrode (171) can be formed of a highly reflective metallic material such as a stacked structure of aluminum and titanium (Ti / Al / Ti), a stacked structure of aluminum and ITO (Indium Tin Oxide) (ITO / Al / ITO), an APC alloy, and a stacked structure of APC alloy and ITO (ITO / APC / ITO). The APC alloy is an alloy of silver (Ag), palladium (Pd), and copper (Cu).

[0130] Bank (419) may be formed to partition the pixel electrode (171) on the second planarization film (418) to define the first light-emitting part (RE), the second light-emitting part (GE), and the third light-emitting part (BE). Bank (419) may be positioned to cover the edges of the pixel electrode (171). Bank (419) may be formed from an organic film such as acrylic resin, epoxy resin, phenolic resin, polyamide resin, or polyimide resin.

[0131] Each of the first light-emitting part (RE), the second light-emitting part (GE), and the third light-emitting part (BE) represents a region in which a pixel electrode (171), a light-emitting layer (172), and a common electrode (173) are sequentially stacked, and a hole from the pixel electrode (171) and an electron from the common electrode (173) combine with each other in the light-emitting layer (172) to produce light.

[0132] A light-emitting layer (172) may be disposed on the pixel electrode (171) and the bank (419). The light-emitting layer (172) may include an organic material and emit a predetermined color. For example, the light-emitting layer (172) includes a hole transporting layer, an organic material layer, and an electron transporting layer.

[0133] A common electrode (173) may be disposed on the light-emitting layer (172). The common electrode (173) may be disposed to cover the light-emitting layer (172). The common electrode (173) may be a common layer formed commonly on the first light-emitting part (RE), the second light-emitting part (GE), and the third light-emitting part (BE). A capping layer may be formed on the common electrode (173).

[0134] In the upper light-emitting structure, the common electrode (173) can be formed from a transparent conductive material (TCO) such as ITO or IZO that can transmit light, or a semi-transmissive conductive material such as magnesium (Mg), silver (Ag), or an alloy of magnesium (Mg) and silver (Ag). When the common electrode (173) is formed from a semi-transmissive conductive material, the light emission efficiency can be increased by the micro cavity.

[0135] An encapsulation layer (TFEL) may be disposed on the common electrode (173). The encapsulation layer (TFEL) includes at least one inorganic film to prevent oxygen or moisture from penetrating the light-emitting element layer (EML). Additionally, the encapsulation layer (TFEL) includes at least one organic film to protect the light-emitting element layer (EML) from foreign substances such as dust. For example, the encapsulation layer (TFEL) includes a first encapsulation inorganic film (TFE1), an encapsulation organic film (TFE2), and a second encapsulation inorganic film (TFE3).

[0136] A first encapsulating inorganic film (TFE1) may be disposed on a common electrode (173), an encapsulating organic film (TFE2) may be disposed on the first encapsulating inorganic film (TFE1), and a second encapsulating inorganic film (TFE3) may be disposed on the encapsulating organic film (TFE2). The first encapsulating inorganic film (TFE1) and the second encapsulating inorganic film (TFE3) may be formed as a multilayer film in which one or more inorganic films selected from a silicon nitride layer, a silicon oxynitride layer, a silicon oxide layer, a titanium oxide layer, and an aluminum oxide layer are alternately stacked. The encapsulating organic film (TFE2) may be an organic film such as an acrylic resin, an epoxy resin, a phenolic resin, a polyamide resin, or a polyimide resin.

[0137] As revealed by the manufacturing method of the display device below, one side of the support film (210) includes an edge portion (210-e) having an acute angle slope, and the edge portion (210-e) supports the bending region of the substrate (100) so as to reduce the bending stress applied to the substrate (100) by bending.

[0138] The method for manufacturing a display device is described below.

[0139] FIG. 10 is a flowchart of a method for manufacturing a display device according to one embodiment, and FIGS. 11 to 15 are cross-sectional views of process steps of a method for manufacturing a display device according to one embodiment. A detailed description of a configuration identical to that described with reference to FIGS. 1 to 9 is omitted.

[0140] First, as shown in FIG. 10, components of the display device are prepared (S10).

[0141] The components of the display device include a substrate (100) in which a first flat area (1FA), a bending area (BA), and a second flat area (2FA) are defined along a first direction, and a display panel including a display portion (400) disposed in the first flat area (1FA) of the substrate (100). Additionally, it may further include a first support film (210), a second support film (220), an optical member (500), and a window member (800).

[0142] Here, the substrate (100) may be a substrate in which a first planar region, a second planar region, and a bending region are defined as shown in FIG. 1.

[0143] Next, as illustrated in FIGS. 10 and 11, a first support film (210), a second support film (220), and an optical member (500) are combined with a prepared display panel (S20).

[0144] Here, the carrier substrate (C) can serve to support the components from below when combining the components. The carrier substrate (C) may be composed of a rigid material. For example, the carrier substrate (C) may include silicon oxide (SiO2). Furthermore, the carrier substrate (C) may include not only silicon oxide (SiO2) but also a small amount of impurities. The impurities may include aluminum (Al), potassium (K), or sodium (Na). In particular, potassium and sodium may each be included in the carrier substrate (C) in the form of cations. The impurities in the carrier substrate (C) may be a factor causing electrostatic attraction with the substrate (100). In the process of peeling the carrier substrate (C) from the substrate (100) described later, the carrier substrate (C) may reduce the electrostatic attraction, specifically the dipole moment, between the carrier substrate (C) and the substrate (100), thereby increasing the ease of peeling.

[0145] The first support film (210) and the second support film (220) are spaced apart and disposed on one side of the substrate (100), and the display portion (400) is disposed on the other side of the substrate (100). An optical member (500) is disposed on the display portion (400). Each member may further include a bonding layer by further disposing of an adhesive member (OCA).

[0146] It can be positioned between the first support film (210) and the substrate (100), between the second support film (220) and the substrate (100), and between the substrate (100) and the optical member (500). An upper member and a lower member are joined together with one adhesive member (OCA) as the center (lamination process).

[0147] A substrate (100) comprises a first substrate (110) and a second substrate (130), a first barrier layer (120) is formed on the first substrate (110), the second substrate (130) is placed on the first barrier layer (120), and a second barrier layer (140) is formed on the second substrate (130).

[0148] The first barrier layer (120) can be formed on one side of the first substrate (110) using plasma enhanced chemical vapor deposition (PECVD) to form the constituent material of the first barrier layer (120). Additionally, the second barrier layer (140) can be formed on one side of the second substrate (130) using plasma enhanced chemical vapor deposition (PECVD) to form the constituent material of the second barrier layer (140). A thin film transistor layer (TFTL), a light-emitting element layer (EML), and an encapsulation layer (TFEL) are formed on the second barrier layer (140).

[0149] Next, an optical member (500) can be bonded to the encapsulation layer (TFEL).

[0150] Next, as illustrated in FIGS. 10 and 12, a bending protection layer (700) is formed in the bending region (BA) of the substrate (100) (S30). The bending protection layer (700) may be formed to cover the entire bending region (BA) starting from the side of the optical member (500). The bending protection layer (700) may be formed such that its thickness decreases as it moves from the side of the optical member (500) toward the bending region (BA). Additionally, the bending protection layer (700) may have a constant thickness within the bending region (BA). The bending protection layer (700) may be formed by printing or laminating a solder resist or a coverlay film.

[0151] Next, as shown in FIGS. 10 and 13, a window member (800) is attached to a display structure (DS), and the display structure (DS) is separated from the carrier substrate (C) (S40).

[0152] For example, an optical clear resin (OCR) in a liquid or paste state is initially applied onto a window member (800) and laminated onto the top of an optical member (500) of a display structure (DS). Subsequently, the window (800) can be bonded onto the display structure (DS) by curing the optical clear resin (OCR) with ultraviolet light (UV).

[0153] As another example, a film-type binder (OCA (Optically Clear Adhesive) such as double-sided tape) is placed on an optical member (500), and a window member (800) is placed on the placed binder, thereby allowing the window (800) to be bonded to a display structure (DS).

[0154] As described with reference to FIG. 11, the carrier substrate (C) can be easily peeled off from the substrate (100), which is the bottom of the display structure (DS), by electrostatic attraction.

[0155] Next, as shown in FIGS. 10 and 14, the edge portion (210-e) of the first support film (210) and the groove of the substrate (100) are formed through laser patterning (S50).

[0156] Laser patterning is a process of forming a desired pattern using a laser source (LS), and the laser source (LS) may include a CO2 laser, an excimer laser, a fiber laser, etc.

[0157] An edge portion (210-e) of the support film (210) is formed by irradiating a laser onto an imaginary line connecting a point (P1) on the lower surface (opposite side to the direction of the display portion (400)) of the first support film (210), located at the bending axis (BAX) of the first support film (210), to a point (P2) on one end of the upper surface (one side to the direction of the display portion (400)) of the first support film (210) in the direction of the second support film (220) (xz direction). By such laser irradiation, the first support film (210) forms an edge portion (210-e) having a predetermined angle of inclination on the first side facing the second support film (220).

[0158] Here, the edge portion (210-e) formed in the bending area is called the first bending portion (210-eb).

[0159] A groove (100a) is formed in the first substrate (110) by considering the depth of the groove formed in the first substrate (100) with respect to the laser irradiation time. The width (length in the first direction (X-axis direction)) and width (length in the second direction (Y-axis direction)) of the groove may match the width and width of the bending area. That is, the groove may be formed over the entire bending area.

[0160] The first barrier layer (120 in FIG. 6) formed on the first substrate (110) is formed of an inorganic material, and the depth of the groove on the substrate (100) is equal to or smaller than the thickness in the third direction (Z-axis direction) of the first substrate (110). When the depth of the groove is equal to the thickness in the third direction (Z-axis direction) of the first substrate (110), an opening is formed. The first barrier layer (120) is exposed through the opening (100a) thus formed.

[0161] Next, as shown in FIGS. 10 and 15, the edge portion of the first support film (210) and the bending area of ​​the substrate (10) are bent around the bending axis (BAX) of the substrate (10) (S60).

[0162] At this time, a filling material (900) can be filled into the space formed by the separation of the first support film (210) and the second support film (220), and into the space formed by the edge portion (210-e) and the groove of the substrate (100).

[0163] After this, the edge portion (210-e) of the first support film (210) and the bending area of ​​the substrate (100) can be bent. When resin is filled, after bending the edge portion of the first support film (210) and the bending area of ​​the substrate (100), a step of curing by ultraviolet (UV) light or heat must be performed. As the filler (900) is cured, the deformation of the substrate (100) can be prevented or minimized by the restoring force that attempts to restore the bent substrate (100) to its state before bending.

[0164] FIG. 16 is a side view of a display device according to another embodiment of the present invention.

[0165] Since the display device (12) of FIG. 16 differs from the display device (10) shown in FIG. 8 only in the width (length in the first direction) of the groove (100a-3), a detailed description of the same components and structure is omitted.

[0166] The display device (12) includes a substrate (101), and the substrate (101) includes a first substrate (111) and a second substrate (131).

[0167] A second substrate (131) may be disposed on one side of the first substrate (111), and a first barrier layer (not shown) may be disposed between the first substrate (111) and the second substrate (131).

[0168] A first support film (211) and a second support film (220) may be disposed on the other side of the first substrate (111).

[0169] A first support film (211) has a first substrate (111) disposed on one surface and includes a first bending portion (211-eb) that overlaps with a bending region (BA) and has an acute angle of inclination with respect to the other surface that overlaps with the first surface. The first bending portion is bent with a predetermined first curvature.

[0170] A concave groove (100a-3) may be formed on the other side of the first substrate (111) in the third direction (Z-axis), which is the thickness direction. The concave groove (100a) may have one end aligned with one end of the first bending portion (211-eb) of the first support film (211), and the width from one end of the groove (100a) to the opposite end may be smaller than the thickness of the first support film (211).

[0171] In another variation, the first substrate (211) may include a plurality of concave grooves. Each of the plurality of concave grooves may be spaced apart from each other in the bending area. Each of the plurality of concave grooves may have the same depth, width, and height as the groove (100a-3), but is not limited thereto.

[0172] FIG. 17 is a side view of a display device according to another embodiment of the present invention.

[0173] The display device (13) of FIG. 17 is a modified example in which the substrate (102) does not include a groove compared to the display device (11) shown in FIG. 5.

[0174] As illustrated in FIG. 17, the display device (13) includes a substrate (102), the substrate (102) includes a first substrate (112) and a second substrate (132), and the first substrate (112) does not include a groove in the bending region. In this case, the bending stress in the bending region may be increased compared to FIG. 5.

[0175] FIG. 18 is a perspective view showing a display device according to one embodiment. FIG. 19 is a plan view showing a display device according to one embodiment, FIG. 20 is a side view of a circuit board in an unfolded state according to one embodiment, and FIG. 21 is a side view of a display device according to one embodiment.

[0176] Referring to FIGS. 18 and 19, the display device (20) may be a light-emitting display device such as an organic light-emitting display device using an organic light-emitting diode, a quantum dot light-emitting display device including a quantum dot light-emitting layer, an inorganic light-emitting display device including an inorganic semiconductor, and a micro light-emitting display device using a micro or nano light-emitting diode (micro LED or nano LED). Hereinafter, the display device (20) has been described with an organic light-emitting display device, but the present invention is not limited thereto.

[0177] The display device (20) includes a display panel (1000), a circuit board (1200), and a display driving circuit (1300).

[0178] The display panel (100) may be formed as a rectangular plane having a long side in a first direction (X-axis direction) and a short side in a second direction (Y-axis direction) that intersects the first direction (X-axis direction). The corner where the long side in the first direction (X-axis direction) and the short side in the second direction (Y-axis direction) meet may be formed rounded to have a predetermined curvature or formed at a right angle. The planar shape of the display panel (100) is not limited to a rectangle and may be formed as other polygons, circles, or ellipses. The display panel (1000) may be formed flat, but is not limited thereto. For example, the display panel (1000) may include curved surfaces formed at the left and right ends that have a constant curvature or a changing curvature. In addition, the display panel (1000) may be formed flexibly so that it can be bent, curved, folded, or rolled.

[0179] A display panel (1000) may include a display area (DA) for displaying an image and a non-display area (NDA) placed around the display area (DA). Alternatively, the display panel (1000) may include a display area (DA) and a non-display area (NDA).

[0180] The display area (DA) may occupy most of the area of ​​the display panel (100). The display area (DA) may be placed in the center of the display panel (100). Pixels may be placed in the display area (DA) to display an image.

[0181] The non-display area (NDA) may be positioned adjacent to the display area (DA). The non-display area (NDA) may be an outer area of ​​the display area (DA). The non-display area (NDA) may be positioned to surround the display area (DA). The non-display area (NDA) may be an edge area of ​​the display panel (100).

[0182] Display pads (DPs) may be placed in the non-display area (NDA) to be connected to circuit boards (300). The display pads (DPs) may be placed on one side edge of the display panel (100). For example, the display pads (DPs) may be placed on the lower side edge of the display panel (1000).

[0183] Circuit boards (1200) may be placed on display pads (DPs) positioned on one side edge of the display panel (100). The circuit boards (1200) may be attached to the display pads (DPs) using a low-resistance, high-reliability material such as an anisotropic conductive film or SAP (Self Assembly Anisotropic Conductive Paste). As a result, the circuit boards (1200) may be electrically connected to the signal wiring of the display panel (1000). The display panel (1000) may receive data voltages, power voltages, scan timing signals, etc., through the circuit boards (1200). The circuit boards (1200) may be flexible printed circuit boards, printed circuit boards, or flexible films such as chip-on-film.

[0184] The display driving circuits (1300) can generate data voltages, power voltages, scan timing signals, etc. The display driving circuits (1300) can supply data voltages, power voltages, scan timing signals, etc. to the display panel (1000) through the circuit boards (1200).

[0185] Each of the display driving circuits (1300) can be formed as an integrated circuit (IC) and attached to a circuit board (1200). Alternatively, the display driving circuits (1300) can be attached to a display panel (1000) using a COG (chip on glass) method, a COP (chip on plastic) method, or an ultrasonic bonding method.

[0186] As illustrated in FIGS. 20 and 21, the display device (20) may further include a cover panel (1400) and a filler (1500).

[0187] The cover panel (1400) can perform functions such as heat dissipation, electromagnetic shielding, pattern visibility prevention, grounding, cushioning, strength reinforcement, and / or digitizing. The cover panel (40) may include a functional layer having at least one of the functions described above. The functional layer may be provided in various forms such as a layer, membrane, film, sheet, plate, panel, etc. The cover panel (40) may include one or more functional layers. For example, the cover panel (40) may include a cushioning sheet, a graphite sheet, and a copper sheet sequentially stacked from top to bottom.

[0188] The cover panel (1400) can overlap with the display panel (30) in the thickness direction, which is the third direction (Z-axis direction). The cover panel (1400) can be attached to the lower surface of the display panel (1000).

[0189] The circuit board (1200) may be bent in the direction of the back of the display panel (1000) to cover the side of the display panel (1000) and may have an extended area that partially overlaps with the bottom surface of the display panel (1000). However, this is illustrated as an example and is not limited to any one embodiment.

[0190] The circuit board (1200) may include an insulating film (1210), a wiring layer (1220), and an insulating layer (1230). The insulating film (1210) defines the shape of the circuit board (1200) and may be a base layer on which the wiring layer (1220) is placed. The insulating film (1210) may have flexibility.

[0191] The insulating film (1210) has a first flat area (1FA), a bending area (BA), and a second flat area (2FA).

[0192] The insulating film (1210) may have a groove (1210-OP) in the bending region (BA). The groove (1210-OP) has a concave shape in the third direction (Z-axis direction), which is the thickness direction of the insulating film (1210). Additionally, the groove (1210-OP) has a depth (t31) that is thinner than the thickness (t11) of the insulating film (1210) in the third direction (Z-axis direction) of the insulating film (1210). Thus, the insulating film (1210) has a thickness (t21) in the bending region that is thinner than the thickness (t11) in the first flat region (1FA) of the insulating film (1210). The groove (1210-OP) can cover the bending region (BA).

[0193] A wiring layer (1220) is disposed on one side of an insulating film (1210). The wiring layer (1220) may include a plurality of signal wires. The signal wires may be electrically connected to a display panel (100) or a display driving circuit (1300).

[0194] An insulating layer (1230) is placed on one side of an insulating film (1210) to cover a wiring layer (1220). A portion of the wiring layer (1220) may be exposed by the insulating layer (1230). The insulating layer (1230) does not overlap with the bending area (BA) of the insulating film (1210). Additionally, the insulating layer (1230) does not overlap with the groove. The wiring layer (1220) may come into contact with a filler (1500) in the bending area (BA).

[0195] The filler (1500) can be formed by injecting and curing a liquid or paste-like substance into the space formed by the side of the display panel (1000) and the bottom surface of the circuit board (1300) in the bent state of the circuit board (1300). The filler (1500) may be provided with a substance having adhesive properties, and as it is cured by ultraviolet (UV) light or heat, it can prevent or minimize deformation of the circuit board (1300) by a restoring force that attempts to restore the circuit board (1300) to its state before bending.

[0196] FIG. 22 is a side view of a circuit board in an unfolded state according to another embodiment, and FIG. 23 is a side view of a display device according to another embodiment. FIG. 24 is a side view of a display device according to yet another embodiment.

[0197] FIGS. 22 and FIGS. 23 show a circuit board (1200) in the display device (20) described with reference to FIGS. 20 and FIGS. 21 that is folded without being bent from the side of the display panel (1000). The focus is on explaining this difference, and a detailed description of the same components is omitted.

[0198] The circuit board (1201) may include an insulating film (1211), a wiring layer (1220), and an insulating layer (1220). The insulating film (1210) defines the shape of the circuit board (1200) and may be a base layer on which the wiring layer (1220) is placed. The insulating film (1210) may have flexibility.

[0199] The insulating film (1211) has a first flat area (1FA), a bending area (BA), and a second flat area (2FA).

[0200] As illustrated in FIG. 23, a plurality of grooves (1211-OP1, 1211-OP2) may be formed at both ends of the second direction of the bending area (BA). For example, the first groove (1211-OP1) may be formed at the boundary point where the first planar area (1FA) and the bending area (BA) meet, and the second groove (1211-OP2) may be formed at the boundary point where the second planar area (2FA) and the bending area (BA) meet.

[0201] A plurality of grooves (1211-OP1, 1211-OP2) may be provided in the bending region (BA). The grooves (1211-OP1, 1211-OP2) have a concave shape in the third direction (Z-axis), which is the thickness direction of the insulating film (1210). Additionally, the grooves (1210-OP) have a depth (t31) that is thinner than the thickness (t11) of the insulating film (1211) in the third direction (Z-axis) of the insulating film (1211). Therefore, the insulating film (1211) has a thickness (t21) in the bending region (BA) that is thinner than the thickness (t11) in the first flat region (1FA) of the insulating film (1211). The grooves (1210-OP) can cover the bending region (BA).

[0202] FIG. 24 is a perspective view showing a display device with a circuit board in a bent state according to one embodiment.

[0203] According to one embodiment, a groove can be formed in the circuit board to control the bending area. Thus, as shown in FIG. 23, when the display device includes a plurality of circuit boards (1200-1, 1200-2, 1200-3), the bent plurality of circuit boards can be easily aligned with the alignment axis (AL).

[0204] Although embodiments of the present invention have been described above with reference to the attached drawings, those skilled in the art will understand that the present invention may be implemented in other specific forms without changing the technical concept or essential features thereof. Therefore, the embodiments described above should be understood as illustrative in all respects and not restrictive. Explanation of the symbols

[0205] 10, 11, 12, 13, 20: Display device 100: Display panel 100, 101, 102 : Substrate 210: 1st support film 220: 2nd support film 400 : Display unit 1FA: First planar region BA: Bending area 2FA: Second planar region

Claims

Claim 1 A substrate comprising a first flat area, a second flat area, and a bending area disposed between the first flat area and the second flat area and having a predetermined radius of curvature; a display unit that overlaps with the first flat area of ​​the substrate and is disposed on one surface of the substrate to display an image; a first support film disposed on the other surface of the substrate that overlaps with the one surface of the substrate and overlaps with the first flat area; and a second support film disposed on the other surface of the substrate with the first support film and the bending area in between and overlapping with the second flat area, wherein the substrate comprises a concave groove in the thickness direction of the substrate in the bending area, and the first support film comprises a first flat portion that overlaps with the first flat area and a first bending portion that overlaps with the bending area and has a first inclination angle of an acute angle with respect to the other surface of the substrate, and one end of the groove is aligned with one end of the first bending portion within the bending area. Claim 2 In claim 1, the first bending part is a display device that is bent to a predetermined first curvature. Claim 3 A display device according to claim 2, wherein the second support film comprises a second flat portion that overlaps with the second flat area and a second bending portion that overlaps with the bending area and has a second inclination angle of acute angle with respect to the other surface of the substrate. Claim 4 In claim 3, the second bending part is a display device that is bent to a predetermined second curvature. Claim 5 In claim 3, the other end of the groove is a display device aligned with one end of the second bending part within the bending area. Claim 6 A display device according to claim 1, wherein the substrate comprises a first substrate, a first barrier layer, a second substrate, and a second barrier layer arranged sequentially, wherein the first barrier layer is located on one surface of the first substrate, and the first support film and the second support film are located on the other surface of the first substrate, and the groove is formed on the first substrate. Claim 7 In claim 6, the groove is a display device having a thickness thinner than the thickness of the first substrate. Claim 8 In claim 6, the groove has a thickness equal to the thickness of the first substrate, and the first barrier layer is exposed by the groove. Claim 9 In claim 6, the first barrier layer is a display device comprising an inorganic material. Claim 10 In claim 9, the inorganic material comprises at least one of a metal oxide, a silicon oxide, and a silicon nitride. Claim 11 In claim 9, the substrate is a display device comprising an organic material. Claim 12 In claim 11, the substrate is a display device containing polyimide, polyethylene napthalate, polyethyleneterephthalate (PET), polyarylate, polycarbonate, polyetherimide (PEI), or polyethersulfone. Claim 13 In claim 6, the first substrate is a display device that is thicker than the thickness of the second substrate. Claim 14 delete Claim 15 A display device according to claim 1, further comprising: an optical member disposed on the display portion; and a bending protection layer covering a bending region of the substrate and in contact with one side of the optical member, wherein the thickness of the bending protection layer decreases from the side of the optical member toward the bending region and is formed to have a constant thickness in the bending region. Claim 16 A step of preparing a display panel comprising a substrate in which, while the substrate is unfolded, a first flat area, a bending area, and a second flat area are sequentially arranged such that a bending area is interposed between a first flat area and a second flat area along a first direction, and a display portion disposed in the first flat area of ​​the substrate; a step of, for a first surface and a second surface that face each other as the substrate is bent, attaching a first support film on an area corresponding to the first surface and attaching a second support film on an area corresponding to the second surface, and attaching an optical member to one surface of the display portion located on the first surface side; a step of forming a bending protection layer in the bending area of ​​the substrate; a step of attaching a window member to the optical member of the substrate; a step of forming a first bending portion by laser patterning that overlaps the bending area and has an acute angle of inclination on one side of the first support film, and forming a groove in the bending area of ​​the substrate by laser patterning. A method for manufacturing a display device, comprising the step of bending a bending region of the substrate and a first bending portion of the first support film, wherein the groove is concave in the thickness direction of the substrate and one end of the groove is aligned with one end of the first bending portion within the bending region. Claim 17 In claim 16, the step of forming by the laser patterning further forms a second bending portion having an acute angle of inclination on one side of the second support film by laser patterning. Claim 18 In claim 16, the above first bending part is a method for manufacturing a display device that overlaps with the above bending area. Claim 19 In claim 17, the method for manufacturing a display device in which the second bending part overlaps with the bending area. Claim 20 In claim 16, the step of forming the bending protection layer is a method for manufacturing a display device in which the thickness of the bending protection layer becomes thinner from the side of the optical member toward the bending region and is formed to be constant in the bending region. Claim 21 A display device comprising: a display panel including a display area and a non-display area; a circuit board including a first planar area disposed in the non-display area and a second bending area extending from the first planar area and having a predetermined curvature; and a display driving circuit attached to the circuit board; wherein the circuit board includes a groove concave in the bending area in the thickness direction on a other surface that overlaps with a surface disposed on the display panel; an insulating film defining the shape of the circuit board; a wiring layer disposed between the insulating film and the display panel; and an insulating layer covering at least a portion of the wiring layer, wherein the insulating layer does not overlap with the groove. Claim 22 In claim 21, the above groove is a display device formed on the insulating film. Claim 23 delete Claim 24 In claim 21, the above groove is formed over the entire bending area of ​​the circuit board with a width equal to the width of the bending area and a width equal to the width of the bending area. Claim 25 A display device according to claim 21, wherein the grooves are provided in plurality, and at least one groove has one end that overlaps with the boundary between the planar area and the bending area. Claim 26 A display device according to claim 22, further comprising a filler material that fills the space defined by the side of the display panel and the other side of the circuit board. Claim 27 In Clause 26, the above filler is a display device that contacts the wiring layer in the bending area.

Citation Information

Patent Citations

  • Display substrate and display device

    CN113066832A

  • Flexible display device with gate-in-panel circuit

    KR1020170095809A

  • Display device and manufacturing method thereof

    KR1020200099223A

  • Display panel and manufacturing method thereof

    US20210408405A1

Cited By

  • Method and apparatus for detecting fine residual disease by using tumor information

    WO2025041917A1