Dry mask pack and preparing method thereof

A dry mask pack with high elasticity and friction nonwoven fabric ensures effective adhesion and even distribution of cosmetic ingredients, addressing adhesion issues and improving user experience.

KR103045195B1Active Publication Date: 2026-11-06IMINE LABS CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
KR1020230165701
Authority / Receiving Office
KR · KR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-11-24
Publication Date
2026-11-06
Estimated Expiration
2043-11-24

AI Technical Summary

Technical Problem

Existing mask packs suffer from poor adhesion to the skin, particularly around areas like the nose, cheeks, and eyes, and often result in uneven distribution and absorption of cosmetic ingredients due to their thinness and lack of elasticity and friction.

Method used

A dry mask pack using a nonwoven fabric with high elasticity (100-220% in MD and 100-240% in CD direction) and high friction (4.0-6.0) is coated with a cosmetic composition having a moisture content of 10 wt% or less, ensuring effective adhesion and even distribution.

Benefits of technology

The mask pack adheres closely to the skin, providing uniform application of moisturizing and soothing effects without dripping, enhancing user convenience and effectiveness.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 112023131710417-PAT00001_ABST
    Figure 112023131710417-PAT00001_ABST
Patent Text Reader

Abstract

The present invention relates to a dry mask pack and a method for manufacturing the same, comprising: a nonwoven fabric; and a cosmetic composition dry-coated on at least a portion of the surface of the nonwoven fabric; wherein the elongation of the nonwoven fabric is 100-220% in the MD direction and 100-240% in the CD direction. Since the nonwoven fabric has high elasticity and high friction characteristics, it is possible to deform and adhere to the contours of the skin, thereby providing the advantage of being able to apply a mask pack customized to an individual's face shape. Furthermore, since it is a dry mask pack, the cosmetic composition does not flow, making it convenient to handle and use.
Need to check novelty before this filing date? Find Prior Art

Description

Technology Field

[0001] The present invention relates to a dry mask pack and a method for manufacturing the same, and more specifically, to a dry mask pack and a method for manufacturing the same in which the adhesion of the mask pack is significantly enhanced by using a fabric with excellent elasticity and friction. Background Technology

[0003] The skin is the largest organ of the human body and a vital organ responsible for various roles, including protection, barrier function, temperature regulation, excretion, and respiration. However, due to various external environmental factors such as strong ultraviolet rays, fine dust, and excessive use of air conditioners and heaters, as well as internal factors like aging, stress, and nutritional deficiencies, skin cells are damaged and cell proliferation does not occur properly. Consequently, not only are the aforementioned functions of the skin not effectively performed, but cosmetic problems such as wrinkles, loss of elasticity, and keratinization also arise.

[0004] This problem can be resolved by appropriately controlling the oil and moisture content and their ratio in the skin's epidermal layer, and various cosmetic products for this purpose are available on the market.

[0005] Typically, cosmetic products are applied by spreading the composition directly onto the skin using hands or various beauty tools and gently patting it to aid absorption. However, this method presents several problems: the amount of active ingredients actually absorbed into the skin area where moisturizing, whitening, or soothing effects are desired is small, resulting in a long waiting period to achieve results; and some of the cosmetic composition is absorbed into the hands or the tools used for application, leading to a decrease in the actual amount of product used.

[0006] On the other hand, mask packs are used by applying a fabric impregnated or coated with a medicinal solution to the target area of ​​the skin and maintaining that contact for a certain period of time. This allows for effective and intensive skin care in a short period, offering the advantage of faster and more certain results.

[0007] Mask packs generally utilize thin non-woven fabrics; while their thinness allows for adjustment of the fabric's placement and shape to conform to the skin, particularly the facial contours, the inherent characteristics of the material result in poor skin adhesion. Furthermore, if highly concentrated beauty ingredients come into contact with the skin initially, there is a high likelihood of causing skin irritation.

[0008] Accordingly, there is a demand for new mask packs that utilize fabrics and cosmetic compositions capable of enhancing skin adhesion. Prior art literature

[0010] Registered Patent No. 10-2060699 (Registered Dec. 23, 2019) The problem to be solved

[0011] The present invention aims to provide a dry mask pack with significantly improved adhesion by using a fabric with excellent elasticity and friction, and a method for manufacturing the same. means of solving the problem

[0013] One embodiment of the present invention for achieving the above-described purpose relates to a dry mask pack comprising: a nonwoven fabric; and a cosmetic composition dry-coated on at least a portion of the surface of the nonwoven fabric; wherein the elongation of the nonwoven fabric is 100 to 220% in the MD direction and 100 to 240% in the CD direction, and the moisture content of the dry-coated cosmetic composition is 10 wt% or less.

[0014] The tensile strength of the above nonwoven fabric is 0.2~3 kg f It can be / cm.

[0015] The above cosmetic composition can be gravure coated on at least a portion of the surface of a nonwoven fabric and then dried.

[0016] The above cosmetic composition may be of a cream type or an oil type, and the cream type cosmetic composition may include a moisturizer, an emulsifier, an oil, an antioxidant, an additive, and purified water, and the oil type cosmetic composition may include an oil, a thickener, an antioxidant, and an additive.

[0017] Another embodiment of the present invention relates to a method for manufacturing a dry mask pack, comprising: a fabric laminate preparation step of preparing a fabric laminate by laminating a nonwoven fabric with an elongation of 100-220% in the MD direction and 100-240% in the CD direction with a release liner; a coating step of supplying the fabric laminate to a roller to gravure-coat a cosmetic composition onto at least a portion of the surface of the nonwoven fabric; and a drying step of drying the nonwoven fabric coated with the cosmetic composition so that the moisture content of the cosmetic composition is 10 wt% or less.

[0018] The above drying step may be a step of hot air drying at 80 to 150°C. Effects of the invention

[0020] The dry mask pack of the present invention has excellent elasticity and friction, allowing it to adhere closely to the skin. Therefore, the mask pack can adhere even to areas where it typically does not adhere well, such as around the nose, the outer edges of the cheeks, and around the eyes, thereby offering the advantage of evenly applying moisturizing, nourishing, and soothing effects to the entire skin.

[0021] In addition, since it is a dry type mask pack rather than a wet type, the cosmetic composition does not drip when the mask pack is taken out of the pouch or applied to the skin, making it easier to use. Brief explanation of the drawing

[0023] FIG. 1 is a photograph of a dry mask pack according to one embodiment of the present invention. Specific details for implementing the invention

[0024] Before describing the preferred embodiments of the present invention in detail below, it should be noted that the terms and words used in this specification and claims should not be interpreted as being limited to their ordinary or dictionary meanings, but should be interpreted in a meaning and concept consistent with the technical spirit of the present invention.

[0025] Throughout this specification, when a part is described as “comprising” a certain component, it means that, unless specifically stated otherwise, it does not exclude other components but may include additional components.

[0026] Throughout this specification, “%” used to indicate the concentration of a specific substance means (weight / weight)% for solid / solid, (weight / volume)% for solid / liquid, and (volume / volume)% for liquid / liquid, unless otherwise noted.

[0027] In each step, identification codes are used for convenience of explanation and do not describe the order of the steps; unless the context clearly indicates a specific order, the steps may be performed differently from the specified order. That is, the steps may be performed in the same order as specified, substantially simultaneously, or in the reverse order.

[0028] Hereinafter, embodiments of the present invention are examined. However, the scope of the present invention is not limited to the following preferred embodiments, and those skilled in the art may implement various modified forms of the contents described herein within the scope of the present invention.

[0029] The present invention relates to a dry mask pack and a method for manufacturing the same. The dry mask pack of the present invention has excellent elasticity and friction, allowing it to adhere closely to the skin. Accordingly, the mask pack can adhere even to locations where it does not typically adhere well, such as around the nose, the outer edges of the cheeks, and around the eyes, thereby providing the advantage of evenly applying moisturizing, nourishing, and soothing effects to the entire skin.

[0030] In addition, since it is a dry type mask pack rather than a wet type, the cosmetic composition does not drip when the mask pack is taken out of the pouch or applied to the skin, making it more convenient to use.

[0031] First, one embodiment of the present invention relates to a dry mask pack, wherein the dry mask pack comprises: a nonwoven fabric; and a cosmetic composition dry-coated on at least a portion of the surface of the nonwoven fabric. At this time, the elongation of the nonwoven fabric may be 100 to 220% in the MD (Machine Direction) direction and 100 to 240% in the CD (Cross Direction) direction.

[0032] The above nonwoven fabric is a fabric with high elasticity and high friction characteristics. Due to its high elongation properties, the fabric can be stretched to conform to the contours of the skin. Since the fabric, once conformed to the contours of the skin, adheres closely to the skin due to its high friction properties, no wrinkles or gaps occur during use, it can provide a sense of adhesion and usability that is significantly different from conventional mask packs.

[0033] Specifically, unlike nonwoven fabrics that typically have an elongation rate of 25–80%, it is desirable for the above nonwoven fabric to have high elasticity characteristics of 100–220% in the MD direction and 100–240% in the CD direction. Specifically, it is even more desirable for it to have high elasticity characteristics of 100–200% in the MD direction and 100–200% in the CD direction. When high elasticity characteristics are present in both the MD and CD directions, a mask pack made of such fabric can be stretched in four directions to conform to the contours of the skin when attached to the skin.

[0034] In addition, while the existing nonwoven fabric has a friction coefficient of 0.01 to 0.10 and a friction force of 0.05 to 0.20 N, the nonwoven fabric used in the present invention has a friction coefficient of 4.0 to 6.0 and a friction force of 9.0 to 12.0 N, and it is desirable to have a higher friction force compared to the general nonwoven fabric.

[0035] The above nonwoven fabric may include thermoplastic polyester and has a tensile strength of 0.2 to 3 kg f / cm or 0.2~2.5 kg f It has a lower thickness than general nonwoven fabric at / cm and has a soft touch.

[0036] In addition, to ensure the mask pack adheres more effectively to the skin, guarantee convenience during use, and minimize the amount of cosmetic composition absorbed by the non-woven fabric that is not delivered to the skin (loss amount), the basis weight of the non-woven fabric is 50 to 70 g / m² 2 It may be, and the thickness may be 0.2 to 0.4 mm. In addition, the nonwoven fabric may be an embossed fabric, and may provide a comfortable user experience by having excellent breathability with an air permeability of 1,300 mm / s or more.

[0037] The mask pack according to the present embodiment is a dry mask pack, which can be formed by gravure coating a cosmetic composition on at least a portion of the surface of a nonwoven fabric and then drying it. The gravure coating can be performed on the entire surface of the mask pack, or it is possible to coat only a portion to form a specific image, character, pattern, etc. For example, the gravure coating can be performed to form a pattern such as that shown in FIG. 1. In addition, by adjusting the depth of the intaglio or relief of the coated cosmetic composition, the coated cosmetic composition can be formed to have different coating thicknesses depending on the area of ​​the nonwoven fabric.

[0038] In conventional mask packs, the degree of cosmetic absorption varies by area of ​​the skin, so parts of the mask pack dry out after a certain amount of time has passed. In these areas, there was a problem where moisture was lost from the skin due to the mask pack, causing dryness or a tight sensation. However, the mask pack according to one embodiment of the present invention prevents specific areas of the mask pack from drying out first by forming a thicker layer of cosmetic composition in areas that dry out easily, thereby enhancing the user experience and the moisturizing and soothing effects of the mask pack.

[0039] The above cosmetic composition is applied to the skin to provide effects such as moisturizing and soothing, and the cosmetic composition may include a cream-type cosmetic composition or an oil-type cosmetic composition. The moisture content of the cosmetic composition included in the dry mask pack may be 10 wt% or less. Here, moisture content refers to the moisture content of the cosmetic composition included in the dry mask pack, which is the final product.

[0040] In particular, if the moisture content of the dry mask pack exceeds the above range, the mask packs stick together and cause inconvenience during use, but if the moisture content is below the above range, the mask packs do not stick together and are convenient to use, so it is desirable to adjust the moisture content of the dry mask pack to 10 wt% or less, preferably 8 wt% or less.

[0041] A cream-type cosmetic composition may include a moisturizer, an emulsifier, an oil, an antioxidant, an additive, and purified water. Specifically, it may include 20 to 35 wt% of a moisturizer, 3 to 5 wt% of an emulsifier, 25 to 40 wt% of an oil, 0.1 to 1 wt% of an antioxidant, 0.01 to 3 wt% of an additive, and the remainder being purified water.

[0042] Moisturizers are added to provide a moisturizing effect to the skin. Examples of moisturizers may be used, but are not limited to polyols such as glycerin, butylene glycol, dipropylene glycol, methylpropanediol, and propanediol.

[0043] Emulsifiers are added to uniformly mix oily components, such as oil, with aqueous components. Examples include polyglyceryl-6 stearate, polyglyceryl-6 behenate, C14-22 alcohol, C12-20 alkylglucoside, glyceryl stearate, sorbitan stearate, sodium surpectin, etc., but are not limited thereto.

[0044] Oil is added to form a film on the skin surface to prevent moisture evaporation, and can be added without special restrictions, such as ester oils or general moisturizing oils.

[0045] Ester oils may include, for example, at least one of caprylic / capric triglycerides, cetyl ethylhexanoate, polyglyceryl-2 triisostearate, diisostearyl malate, hydrogenated ethylhexyl oliveate, caprylic / capric / succinic triglycerides, and jojoba esters, but are not limited thereto, and general moisturizing oils may include at least one of sunflower seed oil, shea butter, hydrogenated polydecene, and hydrogenated poly(C6-14 olefin), but are not limited thereto.

[0046] Antioxidants are added to prevent oxidation and denaturation of cosmetic compositions and may include at least one of tocopherol, tocopheryl acetate, pentaerythrityl tetra-di-t-butylhydroxyhydrocinnamate, and octadecyl-di-t-butyl-4-hydroxyhydrocinnamate, but are not limited thereto.

[0047] Additives are added to improve the physical and chemical properties of a cosmetic composition, such as its appearance, color, odor, shelf life, and stability. Examples include pigments, chelating agents, preservatives, fragrances, and pH adjusters. In addition to these, various other additives may be included to improve the properties of the cosmetic composition.

[0048] The oil-type cosmetic composition may include oil, a thickener, an antioxidant, and an additive, and specifically, may include 85 to 95 wt% oil, 0.1 to 2 wt% thickener, 0.01 to 5 wt% antioxidant, and 3 to 10 wt% additive.

[0049] Oil is added to form a film on the surface of the skin to prevent moisture evaporation, and it is desirable to include both ester oil and general moisturizing oil. Specifically, the oil may contain 80 to 95 wt% ester oil and 5 to 20 wt% general moisturizing oil.

[0050] Ester oils may include, for example, at least one of caprylic / capric triglycerides, cetyl ethylhexanoate, polyglyceryl-2 triisostearate, diisostearyl malate, hydrogenated ethylhexyl oliveate, caprylic / capric / succinic triglycerides, and jojoba esters, but are not limited thereto, and general moisturizing oils may include at least one of sunflower seed oil, shea butter, hydrogenated polydecene, and hydrogenated poly(C6-14 olefin), but are not limited thereto.

[0051] Thickeners are added to compensate for the low viscosity characteristic of oil-type cosmetic compositions, and can improve the viscosity of oil-type cosmetic compositions. As for the thickener, any oil-based thickener that can be used in cosmetic compositions, such as hydrogenated palm oil, hydrogenated rapeseed oil, hydrogenated olive oil, cetyl palmitate, sorbitan palmitate, sorbitan oliveate, sucrose laurate, and dextrin palmitate, can be used without particular limitation.

[0052] Antioxidants are added to prevent oxidation and denaturation of cosmetic compositions and may include at least one of tocopherol, tocopheryl acetate, pentaerythrityl tetra-di-t-butylhydroxyhydrocinnamate, and octadecyl-di-t-butyl-4-hydroxyhydrocinnamate, but are not limited thereto.

[0053] Additives are added to improve the physical and chemical properties of a cosmetic composition, such as its appearance, color, odor, shelf life, and stability. Examples include pigments, chelating agents, preservatives, fragrances, and pH adjusters. In addition to these, various other additives may be included to improve the properties of the cosmetic composition.

[0055] Meanwhile, another embodiment of the present invention relates to a method for manufacturing a dry mask pack. Since the dry mask pack according to the previously described embodiment can be manufactured according to this embodiment, some overlapping details are omitted.

[0056] The method for manufacturing a dry mask pack according to the present embodiment comprises: a fabric laminate preparation step of preparing a fabric laminate by laminating a nonwoven fabric with an elongation of 100-220% in the MD direction and 100-240% in the CD direction with a release liner; a coating step of supplying the fabric laminate to a roller to gravure-coat a cosmetic composition onto at least a portion of the surface of the nonwoven fabric; and a drying step of drying the nonwoven fabric coated with the cosmetic composition.

[0057] The above fabric preparation step is a fabric laminate preparation step in which a nonwoven fabric with an elongation of 100–220% in the MD direction and 100–240% in the CD direction is laminated with a release liner to prepare a fabric laminate. Specifically, it is a step of preparing a fabric laminate by laminating a nonwoven fabric onto a release liner film so that a cosmetic composition can be coated onto the nonwoven fabric in a subsequent step.

[0058] The above nonwoven fabric is a fabric with high elasticity and high friction characteristics. Due to its high elongation properties, the fabric can be stretched to conform to the contours of the skin. Since the fabric, once conformed to the contours of the skin, adheres closely to the skin due to its high friction properties, no wrinkles or gaps occur during use, it can provide a sense of adhesion and usability that is significantly different from conventional mask packs.

[0059] Specifically, it is preferable that the nonwoven fabric has high elasticity characteristics of 100–220% in the MD direction and 100–240% in the CD direction, and it is even more preferable that the coefficient of friction be in the range of 4.0–6.0 and the frictional force be in the range of 9.0–12.0 N. In addition, including thermoplastic polyester, 0.2–3 kg fIt has a low tensile strength of / cm. In addition, it has the advantage of being soft to the touch.

[0060] In addition, to ensure the mask pack adheres more effectively to the skin, guarantee convenience during use, and minimize the amount of cosmetic composition absorbed by the non-woven fabric that is not delivered to the skin (loss amount), the basis weight of the non-woven fabric is 50 to 70 g / m² 2 It can be, and the thickness can be 0.2 to 0.4 mm.

[0061] Due to the high elasticity of these nonwoven fabrics, applying them to general mask pack manufacturing processes such as coating or immersion can lead to fabric damage or difficulties in controlling the fabric. Furthermore, because the nonwoven fabric exhibits poor slip properties due to high friction and elongation, transporting it alone on rollers or conveyor belts can cause problems such as the fabric sticking to the rollers or belts, partial adhesion resulting in wrinkles, or the roll-shaped fabric failing to unravel easily. Therefore, it is advisable not to apply the nonwoven fabric alone to the process, but rather to prepare it as a laminated structure laminated with release paper first, and then apply it to subsequent processes.

[0062] Here, a polymer film can be used as the release liner, and the type of polymer used is not particularly limited.

[0063] The above coating step is a step of feeding the fabric laminate to a roller to gravure-coat a cosmetic composition onto at least a portion of the surface of the nonwoven fabric.

[0064] Gravure coating is a coating technique in which a cosmetic composition is transferred to the surface of a nonwoven fabric by contacting a copper plate loaded with a cosmetic composition with the surface of the nonwoven fabric. By using this coating method, changes in the nonwoven fabric due to the coating process are minimized, thereby preventing damage to the nonwoven fabric with high elasticity and high friction characteristics during coating.

[0065] At this time, the intaglio depth of the surface of the gravure plate formed to support the cosmetic composition may be 70 to 130 μm. If the intaglio depth is less than the above range, the amount of cosmetic composition supported on the plate is small, making it difficult to transfer the cosmetic composition onto the nonwoven fabric; if it exceeds the above range, the amount of cosmetic composition supported is large, causing the cosmetic composition to flow down during the movement of the plate, and consequently, it may be difficult to uniformly control the amount of transferred cosmetic composition.

[0066] In addition, the depth of the engraving formed on the copper plate may be uniformly formed throughout, or the depth in at least one area may be formed differently from other areas. For example, the copper plate depth in areas that dry quickly when a mask pack is applied, such as the cheeks, philtrum, and chin, may be formed to 110㎛, while the copper plate depth in the remaining areas may be formed to 90㎛. In this case, since the amount of cosmetic composition loaded on the cheeks, philtrum, and chin areas of the final dry mask pack is greater, the phenomenon of only specific areas drying quickly when the mask pack is applied is prevented, thereby further improving the usability and effectiveness of the mask pack. Furthermore, there is an advantage in that various visual effects can be provided due to the difference in coating amount.

[0067] The coating amount of the cosmetic composition coated onto the non-woven fabric through this step is 40–100 g / m² 2 , preferably 40~80 g / m² 2 It may be. If the coating amount is less than the above range, the effect of using the mask pack is reduced, and if it exceeds the above range, the degree of enhancement of the effect by using the mask pack is minimal, but productivity decreases due to an increase in the amount of cosmetic composition used and drying time during the manufacturing process, so it is desirable to control the coating amount within the above-mentioned range.

[0068] In the above coating step, the movement speed of the fabric laminate may be 2 to 20 m / min. This is because if the movement speed of the fabric laminate is below the above range, there is a problem of reduced productivity due to the movement speed being too slow, and if it exceeds the above range, the tension applied to the nonwoven fabric increases, which may cause problems such as the nonwoven fabric having high elasticity wrinkling or tearing.

[0069] The viscosity of the cosmetic composition used in the coating process may be 2,000 to 10,000 cP. If the viscosity is below the above range, there is a large amount of loss of the cosmetic composition before drying due to excessive flowability, and if the viscosity exceeds the above range, the transfer from the roll to the nonwoven fabric is not easily achieved when applied to the gravure coating process, so it is desirable to use a cosmetic composition with the above-mentioned viscosity.

[0070] In addition, the hardness of the cosmetic composition may be 0.001 to 0.08 kg, and within this range, the phase stability and shape stability of the cosmetic composition are ensured, so it can be easily applied to the gravure coating process.

[0071] The cosmetic composition used in this step is the same as that described in the previous embodiment, so a redundant description is omitted.

[0072] The above drying step is a step of drying a nonwoven fabric coated with a cosmetic composition. Through this step, the moisture content of the cosmetic composition coated on the nonwoven fabric is dried to about 10 wt% or less, so that a dry mask pack can be manufactured in which the cosmetic composition is not visible to the naked eye or drips down.

[0073] Specifically, the cosmetic composition can be dried so that its moisture content is 10 wt% or less.

[0074] At this stage, drying may be performed using hot air drying at 80 to 150°C, and the drying time is not specifically limited. If the temperature during hot air drying is too low outside the above range, the time required to dry the cosmetic composition to the point where it does not run off becomes excessively long, which reduces productivity. If the drying temperature exceeds the above range, problems such as the cosmetic composition drying unevenly, forming wrinkles, or the nonwoven fabric being damaged by heat may occur. Therefore, it is desirable to perform hot air drying at the above-mentioned temperature.

[0075] The dry mask pack formed through these steps can be packaged in a pouch through a packaging step, and a perforation step may be performed prior to packaging, and if necessary, a step of removing the release liner may be performed.

[0076] Hereinafter, the specific operation and effects of the present invention will be explained through an embodiment of the present invention. However, this is presented as a preferred example of the present invention, and the scope of the rights of the present invention is not limited according to the embodiment.

[0078] [Preparation Example]

[0079] First, a cosmetic composition in the form of a cream was prepared in which 100g of purified water, 78.5g of glycerin, 36.1g of butylene glycol, 15.4g of polyglyceryl-6 stearate as an emulsifier, 96.2g of caprylic / capric triglyceride, 37.7g of hydrogenated polydecene, 1.8g of tocopheryl acetate as an antioxidant, and 0.15g of disodium EDTA as a metal ion chelating agent were uniformly dispersed.

[0080] Next, basis weight 60 g / m² 2 , thickness 0.34 mm, MD direction elongation 163%, CD direction elongation 156%, coefficient of kinetic friction 5.43, kinetic friction force 10.64 N, MD direction tensile strength 0.28 kg f / cm, tensile strength in CD direction 0.44 kg fA thermoplastic polyester nonwoven fabric with a thickness of / cm was prepared.

[0081] Next, the above nonwoven fabric was laminated with a release liner film to prepare a fabric laminate roll, which was installed in a gravure coating device, and a coating bath was filled with the above cosmetic composition and gravure coating was performed on the nonwoven fabric. At this time, a gravure plate with a depth of 120 μm was used for the coating.

[0082] A nonwoven fabric coated with a cosmetic composition was placed in a drying device and dried with hot air at 110°C to produce a dry mask pack with a moisture content of approximately 4.5 wt%. The dry mask pack was perforated to produce a mask pack equipped with perforations for the eyes, nose, and mouth, as well as cut lines for ear loops. The mask pack produced in this way was photographed and is shown in Fig. 1.

[0084] [Experimental Example 1]

[0085] A dry mask pack was manufactured using the same method as the manufacturing example, but with the movement speed of the laminated fabric varied during the coating step. The coating amount of each dry mask pack was measured and recorded in Table 1. The shape deformation (tearing, wrinkles, folding, etc.) of the nonwoven fabric was visually observed and the results were also recorded in Table 1. "○" was used when there was no shape deformation of the nonwoven fabric, and "×" was used when there was shape deformation.

[0086] Movement speed (m / s) Coating amount (g / m²) 2 ) Fabric appearance 2 45.3±0.8 ○ 6 53.1±1.0 ○ 10 59.8±1.1 ○ 14 64.1±1.1 ○ 17 71.9±1.5 ○ 20 77.9±2.6 ○ 24 83.7±3.1 ×

[0087] Referring to the experimental results in Table 1 above, it was found that as the moving speed of the fabric laminate increased, the amount of coating decreased slightly and the variation in the amount of coating of individual mask packs increased. In particular, when the speed exceeded 20 m / min, it was found that the nonwoven fabric lacked resistance to tension, causing problems such as wrinkling or folding of the nonwoven fabric. Therefore, based on the results of this experiment, it was confirmed that the moving speed of the fabric laminate should be 2 to 20 m / s to ensure the quality of the mask pack.

[0089] [Experimental Example 2]

[0090] A dry mask pack was prepared using the same method as the preparation example, but during the drying step, the drying temperature was varied and drying was carried out for 5, 15, and 30 minutes, and the moisture content was measured.

[0091] In addition, when individual mask packs were folded and unfolded after drying for 15 minutes, they were evaluated as good if the folded surfaces did not stick together and poor if they stuck together, and this was recorded in Table 2. Additionally, the appearance of each mask pack was visually inspected, and it was evaluated as good if there was no deformation of the nonwoven fabric and poor if deformation occurred.

[0092] Drying temperature (°C) Moisture content (wt%) Whether to attach to each other when overlapping appearance Dry for 5 minutes Dry for 15 minutes Dry for 30 minutes 60 15.21 15.21 14.58 error Good 70 13.48 12.96 11.79 error Good 80 9.66 8.56 6.40 Good Good 100 8.56 6.88 5.69 Good Good 120 8.48 6.80 5.30 Good Good 150 5.83 4.74 3.96 Good Good 170 3.10 Measurement and observation impossible due to fabric damage

[0093] Experimental results confirmed that when the drying temperature is between 80 and 150°C, the moisture content is dried to 10 wt% or less, and workability and usability are ensured as the fabric does not stick together when overlapped, and no deformation of the nonwoven fabric occurs due to heat. On the other hand, when the drying temperature is below 80°C, the moisture content remains high, exceeding 10 wt% even after drying for 30 minutes, and problems with mutual adhesion occur when overlapped, and when the temperature is 170°C, the fabric is damaged if dried for more than 5 minutes.

[0094] Therefore, as a result of this experiment, it was confirmed that it is desirable to control the moisture content of the dry mask pack to 10 wt% or less in order to secure workability and productivity during the manufacture of the dry mask pack and to ensure more convenient use. In addition, it was confirmed that the drying temperature required to ensure productivity and quality is 80 to 150℃.

Claims

Claim 1 In a mask pack in which a cosmetic composition is impregnated into a nonwoven fabric, the elongation of the nonwoven fabric in the MD (Machine Direction) direction is 100–220%, the elongation in the CD (Cross Direction) direction is 100–240%, the tensile strength is 0.2–3 kgf / cm, the coefficient of friction is 4.0–6.0, and the frictional force is 9.0–12.0 N, and the cosmetic composition is applied at a rate of 45–80 g / m² to at least a portion of the surface of the nonwoven fabric. 2 A dry mask pack characterized by being gravure coated in an amount and then dried at 80 to 150°C for 5 to 30 minutes, such that the moisture content of the coated cosmetic composition is 3.96 to 9.66 wt%. Claim 2 delete Claim 3 delete Claim 4 A dry mask pack according to claim 1, wherein the cosmetic composition may be of a cream type or an oil type, and the cream type cosmetic composition comprises a moisturizer, an emulsifier, an oil, an antioxidant, an additive, and purified water, and the oil type cosmetic composition comprises an oil, a thickener, an antioxidant, and an additive. Claim 5 A method for manufacturing a mask pack impregnated with a cosmetic composition, comprising: a step of preparing a fabric laminate by laminating a nonwoven fabric having a tensile strength of 0.2 to 3 kgf / cm, a coefficient of friction of 4.0 to 6.0, and a frictional force of 9.0 to 12.0 N, and an elongation of 100 to 220% in the MD direction and 100 to 240% in the CD direction, and a release liner; and a step of supplying the fabric laminate to a roller to apply a cosmetic composition at a rate of 45 to 80 g / m² to at least a portion of the surface of the nonwoven fabric. 2 A method for manufacturing a dry mask pack, comprising: a coating step of gravure coating in an amount of; and a drying step of hot-air drying a nonwoven fabric coated with a cosmetic composition at 80 to 150°C for 5 to 30 minutes so that the moisture content of the cosmetic composition becomes 3.96 to 9.66 wt%. Claim 6 delete

Citation Information

Patent Citations

  • Fabric base for sheet containing liquid cosmetic

    JP2014101320A

  • Cosmetic sheet and manufacturing apparatus thereof

    KR1020230121443A