Heteroleptic yttrium precursor for thin film formation and method for forming thin film using the same
The heteroligand yttrium precursor compound addresses non-uniformity and defects in ALD by ensuring consistent vapor pressure and improved heat transfer, resulting in uniform thin films with reduced process time.
Patent Information
- Application Number
- KR1020250102354
- Authority / Receiving Office
- KR · KR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2025-07-28
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2045-07-28
AI Technical Summary
Existing yttrium oxide thin film deposition methods, particularly atomic layer deposition (ALD), suffer from non-stoichiometric defects and oxygen vacancies due to high-temperature sublimation of solid precursors, leading to non-uniform thin films and incomplete vaporization, which are exacerbated by the use of solid-state precursors.
Development of a heteroligand yttrium precursor compound, specifically cyclopentadienyl-based and formamidinate-based ligands, which are liquid at low melting points, ensuring consistent vapor pressure and improved heat transfer, facilitating uniform thin film deposition through processes like ALD and CVD.
The heteroligand yttrium precursor provides uniform thin films with consistent thickness and improved vaporization rates, reducing process time and enhancing film uniformity by maintaining stable vapor pressure, thus overcoming the limitations of solid precursors.
Smart Images

Figure 112025085544052-PAT00001 
Figure 112025085544052-PAT00002 
Figure 112025085544052-PAT00003
Abstract
Description
Technology Field
[0001] The present invention relates to a heteroligand yttrium precursor compound for thin film formation and a method for forming a thin film using the same, according to embodiments of the present invention. Background Technology
[0002] Precursors for thin film formation consist of a central metal atom and a ligand. Since chemical properties such as reactivity, phase (e.g., liquid, solid), thermal stability, volatility, and heat resistance vary depending on the structure of the ligand, precursors with various types of ligands are being developed in consideration of these factors.
[0003] Recently, yttrium oxide (Y2O3) has garnered significant attention as an alternative to silicon oxide (SiO2) in nanoscale semiconductor electronic devices due to its excellent material properties, such as high dielectric constant or refractive index. Nano-thick yttrium oxide (Y2O3) films are being fabricated using methods such as sputtering chemical vapor deposition and atomic layer deposition (ALD). In particular, atomic layer deposition of yttrium oxide is becoming increasingly important because there are limitations to methods such as chemical vapor deposition (CVD) or sputtering for achieving a uniform coating of yttrium oxide that exhibits plasma and chemical resistance characteristics on semiconductor manufacturing equipment components with complex three-dimensional microstructures.
[0004] In the ALD oxide fabrication process, thin films grow through unique surface reactions between vaporized precursors and oxidizers. For yttrium oxide (Y2O3) thin films, the entire ALD cycle for single-layer growth consists of four stages: pulses of the Y2O3 precursor, purging with an inert gas, pulses of the oxidizer, and purging with an inert gas. By adjusting the number of cycles, a film of the desired thickness is obtained. Yttrium oxide (Y2O3) thin films formed by ALD using solid precursors suffer from problems such as non-stoichiometric defects and oxygen vacancies. These phenomena are related to the high-temperature environment required for proper sublimation when using solid-state precursors, as well as the presence of incompletely sublimated particles within various components of the ALD equipment.
[0005] In the case of solid precursors, heat transfer for vaporization is not uniform compared to the liquid phase, which can affect thin film thickness due to fluctuations in precursor vapor pressure; therefore, the development of yttrium precursors with heteroligands is underway to obtain precursors that become liquid upon heating due to a low melting point or a liquid phase. The problem to be solved
[0006] Accordingly, the present invention provides a novel heteroligand yttrium precursor for thin film formation to solve the above problems. According to one embodiment, the heteroligand yttrium precursor is a cyclopentadienyl-based ligand (e.g., R 1 -Cp) and formamidinate-based ligands (e.g., R 2 -N-CH=NR 3 ) or guandinate-based ligands (e.g., R 2 -NC(NR a R b )=NR 3 It may include ).
[0007] According to one embodiment, the present invention provides a yttrium precursor source for forming a thin film comprising the heteroligand yttrium precursor of the present invention.
[0008] According to one embodiment, the present invention provides a thin film deposition process using a yttrium precursor source for forming a thin film comprising the heteroligand yttrium precursor of the present invention.
[0009] However, the problems that the present invention aims to solve are not limited to those mentioned above, and other unmentioned problems will be clearly understood by those skilled in the art from the description below. means of solving the problem
[0010] According to one embodiment, the yttrium precursor compound of the present invention may be a yttrium precursor compound represented by the following chemical formula 1.
[0011] [Chemical Formula 1]
[0012]
[0013] (R in Chemical Formula 1 above 1 is hydrogen, a straight-chain or branched-chain alkyl group having 1 to 20 carbon atoms, and R 2 and R 3 It is selected from straight-chain or branched-chain alkyl groups having 1 to 20 carbon atoms, and
[0014] R 4 is hydrogen or -N(R a )(R b )(here, R a and R b Each is selected from hydrogen and alkyl groups having 1 to 3 carbon atoms.)
[0015] According to one embodiment, R in Formula 1 1 is hydrogen, a straight-chain or branched-chain alkyl group having 1 to 10 carbon atoms, and R 2 and R 3 It may be selected from straight-chain or branched-chain alkyl groups having 1 to 10 carbon atoms.
[0016] According to one embodiment, the R 1 It may be hydrogen, methyl, ethyl, propyl, or iso-propyl.
[0017] According to one embodiment, the R 2 and R 3 Each may be selected from ethyl, propyl, iso-propyl, tert-butyl, and sec-butyl.
[0018] According to one embodiment, the yttrium precursor compound is R in Formula 1. 2 and R 3 This may have the same ligand or different asymmetric ligands.
[0019] According to one embodiment, the R 4 is hydrogen, or -N(R a )(R b )(here, R a and R b Each may be hydrogen and an alkyl group having 1 to 3 carbon atoms.
[0020] According to one embodiment, the yttrium precursor compound may be selected from the following formulas 1-1 and 1-2.
[0021] [Chemical Formula 1-1]
[0022]
[0023] (R in the above chemical formula 1-1 1 is hydrogen, a straight-chain or branched-chain alkyl group having 1 to 10 carbon atoms, and R 2 and R 3 The groups are identical or different from each other and are selected from straight-chain or branched-chain alkyl groups having 1 to 10 carbon atoms.)
[0024] [Chemical Formula 1-2]
[0025]
[0026] (R in Chemical Formula 1-2 1It is hydrogen, a straight-chain or branched-chain alkyl group having 1 to 10 carbon atoms, and
[0027] R 2 and R 3 The groups are identical or different from each other and are selected from straight-chain or branched-chain alkyl groups having 1 to 10 carbon atoms.).
[0028] According to one embodiment, the yttrium source for forming a thin film of the present invention may comprise an yttrium precursor compound according to embodiments of the present invention.
[0029] According to one embodiment, the yttrium precursor compound may be in liquid, powder, or crystal form.
[0030] According to one embodiment, the source may be for an Atomic Layer Deposition (ALD) or Chemical Vapor Deposition (CVD) process.
[0031] A method for forming an yttrium-containing deposited film according to one embodiment of the present invention may include the step of forming an yttrium-containing deposited film on a substrate by introducing an yttrium source for thin film formation according to embodiments of the present invention.
[0032] According to one embodiment, the step of forming the yttrium-containing deposited film may utilize atomic layer deposition (ALD) or chemical vapor deposition (CVD), and the process temperature of the atomic layer deposition may be 100°C to 500°C.
[0033] According to one embodiment, the deposited film may be a yttrium film, a yttrium oxide film, a yttrium carbide film, or a yttrium nitride film. Effects of the invention
[0034] The present invention provides a novel heteroleptic yttrium precursor compound for thin film deposition. The heteroleptic yttrium precursor compound of the present invention has improved volatility and vapor pressure homeostasis, enabling the formation of a uniform deposited film and providing an opportunity to repeatedly obtain thin films of a desired thickness.
[0035] The present invention can provide a thin film deposition process using the heteroligand yttrium precursor of the present invention. Specific details for implementing the invention
[0036] Embodiments of the present invention will be described in detail below with reference to the attached drawings. In describing the present invention, specific descriptions of related known functions or configurations will be omitted if it is determined that such detailed descriptions may unnecessarily obscure the essence of the present invention. Furthermore, the terms used in this specification are used to appropriately express preferred embodiments of the present invention, and these may vary depending on the intentions of the user or operator, or the conventions of the field to which the present invention belongs. Accordingly, the definitions of these terms should be based on the content throughout this specification. Identical reference numerals in each drawing indicate identical components.
[0037] Throughout the specification, when it is stated that a component is located "on" another component, this includes not only cases where a component is in contact with another component, but also cases where another component exists between the two components.
[0038] Throughout the specification, when a part is described as "including" a certain component, this means that it does not exclude other components but may include additional components.
[0039] In this document, each of the phrases such as “A or B,” “at least one of A and B,” “at least one of A or B,” “A, B or C,” “at least one of A, B and C,” and “at least one of A, B, or C” may include any one of the items listed together in the corresponding phrase, or all possible combinations thereof. Terms such as “first,” “second,” or “first” or “second” may be used simply to distinguish a component from another component and do not limit the components in any other aspect (e.g., importance or order).
[0040] Hereinafter, the yttrium precursor compound of the present invention and its applications will be described in detail with reference to the embodiments and drawings. However, the present invention is not limited to these embodiments and drawings.
[0041] According to one embodiment, the yttrium precursor compound of the present invention is an organometallic or metal-organic molecule formed by the combination of a metal (Y; yttrium) represented by the following Chemical Formula 1 and an organic compound (ligand), and may be a heterooleptic yttrium precursor compound in which two or more ligands are coordinated to a single central metal. For example, a cyclopentadienyl-based ligand (e.g., R 1 -Cp) and formamidinate-based ligands (e.g., R 2 -N-CH=NR 3 ); or guandinate-based ligands (e.g., R 2 -NC(NR a R b )=NR 3 It may include ).
[0042] [Chemical Formula 1]
[0043]
[0044] According to one embodiment, R in Formula 1 1 Silver can be selected from hydrogen and straight-chain or branched-chain alkyl groups having 1 to 20 carbon atoms. Preferably, the alkyl group may be a straight-chain or branched-chain alkyl group having 1 to 10 carbon atoms; 1 to 5 carbon atoms; or 1 to 4 carbon atoms. For example, R 1 It may be hydrogen, methyl, ethyl, n-propyl, iso-propyl, n-butyl, iso-butyl, tert-butyl, or sec-butyl.
[0045] According to one embodiment, R in Formula 1 2 and R 3 The alkyl group may be selected from straight-chain or branched-chain alkyl groups having 1 to 20 carbon atoms. Preferably, the alkyl group may be a straight-chain or branched alkyl group having 1 to 15 carbon atoms; 1 to 10 carbon atoms; 1 to 5 carbon atoms; or 1 to 4 carbon atoms. For example, the R 2 and R 3 It can be selected from ethyl, n-propyl, iso-propyl, n-butyl, iso-butyl, tert-butyl, and sec-butyl.
[0046] According to one embodiment, R in Formula 1 2 and R 3These can be identical or different. If different, they can provide yttrium precursor compounds having asymmetric ligands. The introduction of such asymmetric ligands can improve the volatility and vapor pressure homeostasis of yttrium precursor compounds. For example, the introduction of asymmetric ligands can increase the probability of synthesizing yttrium precursors that have a low melting point and become liquid at the precursor heating temperature, or liquid phases that are suitable for creating a constant vapor pressure. Furthermore, in thin film deposition processes (e.g., ALD), heat transfer is more effectively transferred to the entire yttrium precursor within the canister compared to the solid-phase precursor, resulting in a higher vaporization rate of the precursor. Consequently, the increased amount of precursor resulting from the relatively higher vapor pressure compared to the solid phase during deposition provides an opportunity to reduce the precursor pulsing time or surface exposure time, which can lead to a reduction in process time. Additionally, the high vapor pressure of the precursor can provide a uniform thin film over a wide area. In other words, 1) increasing vaporization is advantageous for obtaining a high vapor pressure of the precursor and can help improve the uniformity of the thin film. 2) Liquid precursors have excellent constancy of vapor pressure, so they can be advantageous for repeatedly obtaining thin films of a uniform thickness. 3) Precursors containing formamidinate can provide higher volatility compared to precursors containing acetamide, which has methyl instead of hydrogen. For example, heterooleptic precursors include cyclopentadienyl; and ligands of asymmetric formamidinate or guandinate, and can increase volatility by lowering the molecular weight.
[0047] According to one embodiment, in the above formula 1, R 4 Silver hydrogen or -NRa R b It may be. Preferably -N(R a )(R b R in ) a and R b The groups are identical or different from each other and may be selected from hydrogen; and straight-chain or branched-chain alkyl groups having 1 to 5 carbon atoms; 1 to 3 carbon atoms; or 1 to 2 carbon atoms. Preferably, R a and R b Each can be selected from hydrogen and straight-chain or branched-chain alkyl groups having 1 to 3 carbon atoms. More preferably, it can be selected from straight-chain or branched-chain alkyl groups having 1 to 3 carbon atoms; or alkyl groups having 1 to 2 carbon atoms.
[0048] According to one embodiment, the yttrium precursor compound may be selected from Formula 1-1 and Formula 1-2.
[0049] [Chemical Formula 1-1]
[0051]
[0052] [Chemical Formula 1-2]
[0053]
[0054] According to one embodiment, R in Formula 1-1 and Formula 1-2 1 is hydrogen, a straight-chain or branched-chain alkyl group having 1 to 20 carbon atoms, and preferably, the alkyl group may be a straight-chain or branched-chain alkyl group having 1 to 10 carbon atoms; 1 to 5 carbon atoms; or 1 to 4 carbon atoms. For example, the R 1 It may be hydrogen, methyl, ethyl, n-propyl, iso-propyl, n-butyl, iso-butyl, tert-butyl, or sec-butyl.
[0055] According to one embodiment, R in Formula 1-1 and Formula 1-2 2 and R 3The alkyl group may be selected from straight-chain or branched-chain alkyl groups having 1 to 20 carbon atoms. Preferably, the alkyl group may be a straight-chain or branched-chain alkyl group having 1 to 15 carbon atoms; 1 to 10 carbon atoms; 1 to 5 carbon atoms; or 1 to 4 carbon atoms. For example, the R 2 and R 3 Each can be selected from ethyl, n-propyl, iso-propyl, n-butyl, iso-butyl, tert-butyl, and sec-butyl. The above R 2 and R 3 They may be different or identical to each other. Preferably, the above R 2 and R 3 These can form different asymmetric ligands.
[0056] According to one embodiment, R in Formula 1-1 and Formula 1-2 2 and R 3 These are different from each other, and this can provide yttrium precursor compounds having asymmetric ligands. The introduction of these asymmetric ligands can improve the volatility of the yttrium precursor compounds. This increases the vaporization of yttrium precursor compounds (e.g., liquid or solid) during a thin film deposition process (e.g., ALD), and shortens the precursor injection time (e.g., shortening the atomic layer deposition process time) by increasing the number of gaseous precursors capable of surface reactions due to the increased vapor pressure during deposition, thereby providing a uniform and high-quality deposited film.
[0057] According to one embodiment, the compound of Formula 1 may be synthesized by utilizing a reaction process known in the art of the present invention according to Scheme 1 or 2 below. The solvents (THF and pentane) presented in Scheme 1 and Scheme 2 may be changed to suitable solvents to achieve the objectives of the present invention. The compounds thereof may be identified using methods for confirming structure and physical properties known in the art of the present invention. For example, 11H NMR, TGA, DSC, mass spectrometry, elemental analysis, etc., may be used, but are not specifically mentioned in this document.
[0058] [Scheme 1]
[0059]
[0060] (R in Scheme 1 1 , R 2 , R 3 and R 4 is as described in the above Chemical Formula 1, Chemical Formula 1-1, and Chemical Formula 1-2.)
[0061] [Scheme 2]
[0062]
[0063] (R in Scheme 2 1 , R 2 , R 3 and R 4 is as described in the above Chemical Formula 1, Chemical Formula 1-1, and Chemical Formula 1-2.)
[0064] According to one embodiment, the present invention may provide a yttrium source for thin film formation comprising the yttrium precursor compound of the present invention. The yttrium source may further comprise a source material required depending on the composition of the yttrium-containing thin film. The yttrium source may utilize a liquid and / or solid yttrium precursor compound. For example, the solid may be in the form of a powder or a crystalline solid. For example, a liquid precursor (e.g., a heteroligand precursor) may induce the formation of a stable precursor vapor pressure.
[0065] According to one embodiment, the yttrium source for thin film formation can be applied to a thin film formation process by an atomic layer deposition (ALD) process. The yttrium source can be supplied into a process chamber in the form of a precursor gas by vaporizing a precursor.
[0066] According to one embodiment, the present invention provides a method for forming an yttrium-containing deposited film, which may include the step of forming an yttrium-containing deposited film on a substrate by introducing an yttrium source for thin film formation according to the present invention. The step may utilize at least one deposition process among a vapor deposition process and an atomic layer deposition (ALD) process. The vapor deposition process may be chemical vapor deposition (CVD), etc.
[0067] The above deposition process (e.g., CVD or ALD) may include a process of vaporizing the yttrium source for thin film formation according to the present invention and supplying it into a chamber, wherein the yttrium precursor molecules supplied into the chamber react with the surface of a substrate to form a surface reaction product layer. Additionally, in the case of chemical vapor deposition (CVD), the precursor and the reactant may be supplied simultaneously into the chamber to cause a reaction to occur in the gas phase, thereby obtaining a desired thin film. Furthermore, depending on the desired thin film, the process may further include a process of reacting the precursor surface reaction product layer with a reactant or co-precursor.
[0068] According to one embodiment, in the deposition process (e.g., CVD or ALD), the thin film formation process (e.g., temperature, etc.) may be appropriately selected according to the desired thin film or source, for example, the process temperature (e.g., deposition temperature) may be above room temperature; 100°C to 500°C; 100°C to 400°C; 100°C to 300°C; 100°C to 200°C; or 100°C to 150°C (Celsius). The carrier gas of the precursor source may be an inert gas such as argon (Ar), nitrogen (N2), or helium (He). In addition, the above inert gas can be used as a purging gas to remove excess precursors and reactants, along with their surface reaction byproducts, after precursor pulsing and reactant or co-precursor pulsing in the case of atomic layer deposition.
[0069] According to one embodiment, the deposited film may be an yttrium film, a yttrium oxide film, or a yttrium nitride film, but is not limited thereto.
[0070] According to one embodiment, the reactant may be at least one of carbon, hydrocarbon (CH4, C2H2), nitrogen (N2), ammonia (NH3), hydrazine (N2H4), nitrous oxide (N2O), oxygen (O2), water vapor (H2O), ozone (O3), hydrogen peroxide (H2O2), silane, hydrogen (H), and diborane (B2H6), but is not limited thereto.
[0071] Although the embodiments have been described above with reference to limited examples and drawings, those skilled in the art can make various modifications and variations from the description above. For example, suitable results may be achieved even if the described techniques are performed in a different order than described, and / or the described components are combined or assembled in a form different from described, or replaced or substituted by other components or equivalents. Therefore, other implementations, other embodiments, and equivalents to the claims below are also within the scope of the claims.
Claims
Claim 1 Yttrium precursor compound represented by the following chemical formula 1: [Chemical Formula 1] (R in Chemical Formula 1 above 1 is hydrogen, a straight-chain or branched-chain alkyl group having 1 to 20 carbon atoms, and R 2 and R 3 Silver is selected from straight-chain or branched-chain alkyl groups having 1 to 20 carbon atoms, and R 4 is hydrogen or -N(R a )(R b )(here, R a and R b Each is selected from hydrogen and alkyl groups having 1 to 3 carbon atoms.) Claim 2 In claim 1, R in the above chemical formula 1 1 is hydrogen, a straight-chain or branched-chain alkyl group having 1 to 10 carbon atoms, and R 2 and R 3 Yttrium precursor compound selected from straight-chain or branched-chain alkyl groups having 1 to 10 carbon atoms. Claim 3 In paragraph 1, the above R 1 Yttrium precursor compound that is hydrogen, methyl, ethyl, propyl, or iso-propyl. Claim 4 In paragraph 1, the above R 2 and R 3 yttrium precursor compounds, each selected from ethyl, propyl, iso-propyl, tert-butyl, and sec-butyl. Claim 5 In claim 1, the yttrium precursor compound is R in Formula 1. 2 and R 3 Yttrium precursor compounds having identical ligands or different asymmetric ligands. Claim 6 In paragraph 1, the above R 4 is hydrogen, or -N(R a )(R b )(here, R a and R b yttrium precursor compounds, each being hydrogen and an alkyl group having 1 to 3 carbon atoms. Claim 7 In claim 1, the yttrium precursor compound is selected from the following Chemical Formula 1-1 and Chemical Formula 1-2, yttrium precursor compound: [Chemical Formula 1-1] (R in the above chemical formula 1-1 1 is hydrogen, a straight-chain or branched-chain alkyl group having 1 to 10 carbon atoms, and R 2 and R 3 The groups are identical or different from each other and are selected from straight-chain or branched-chain alkyl groups having 1 to 10 carbon atoms.)[Chemical Formula 1-2] (R in Chemical Formula 1-2 1 is hydrogen, a straight-chain or branched-chain alkyl group having 1 to 10 carbon atoms, and R 2 and R 3 The groups are identical or different from each other and are selected from straight-chain or branched-chain alkyl groups having 1 to 10 carbon atoms.). Claim 8 A yttrium source for thin film formation comprising the yttrium precursor compound of claim 1. Claim 9 In claim 8, the yttrium source for thin film formation is in the form of a liquid, powder, or crystal, wherein the yttrium precursor compound is a liquid, powder, or crystal. Claim 10 In claim 8, the above source is a yttrium source for thin film formation, which is for an Atomic Layer Deposition (ALD) or Chemical Vapor Deposition (CVD) process. Claim 11 A method for forming an yttrium-containing deposited film, comprising the step of introducing an yttrium source for thin film formation according to claim 8 to form an yttrium-containing deposited film on a substrate. Claim 12 A method for forming a yttrium-containing deposited film according to claim 11, wherein the step of forming the yttrium-containing deposited film utilizes Atomic Layer Deposition (ALD) or Chemical Vapor Deposition (CVD), and the process temperature of the deposition is 100°C to 500°C. Claim 13 A method for forming a yttrium-containing deposited film according to claim 11, wherein the deposited film is a yttrium film, a yttrium oxide film, a yttrium carbide film, or a yttrium nitride film.
Citation Information
Patent Citations
Metal complexes with n-aminoamidinate ligands
KR1020140015404A
Precursor comprisi ng for yttrium or actinoid containg thin film, deposition method of film and semiconductor device of the same
KR1020240038327A
Multisubstituted cyclopentadienyl rare-earth complexes as precursors for vapor-phase thin film deposition processes
KR1020250054807A
In-situ formation of non-volatile lanthanide thin film precursors and use in ALD and CVD
US10643838B2