Method for manufacturing protective sheets for workpiece machining and individual workpiece sheets

TWI945384BActive Publication Date: 2026-11-11LINTEC CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
TW112104519
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-02-15
Filing Date
2023-02-09
Publication Date
2026-11-11
Estimated Expiration
2043-02-08

AI Technical Summary

Technical Problem

The use of adhesive tapes in LDBG (Laser Dicing Before Grinding) for semiconductor wafers leads to potential movement and contact between individualized workpieces, causing cracks and reducing yield due to the small kerf width and uneven application of shear force during grinding.

Method used

A protective sheet for workpiece processing with a base material and adhesive layer having a shear storage modulus of 40,000 Pa or more and a shear stress relaxation rate of 30% or more at 55°C, along with a buffer layer to alleviate stress and prevent collisions between workpiece fragments.

Benefits of technology

The protective sheet effectively reduces the occurrence of large cracks in workpieces during grinding, enhancing the yield and quality of individualized pieces by maintaining stability and minimizing collisions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

[Problem] To provide a protective sheet for workpiece processing that reduces the number of defective workpiece pieces after grinding, even when the workpiece is individually pieced by LDBG grinding. [Solution] A protective sheet for workpiece processing has a substrate and an adhesive layer disposed on one of the main surfaces of the substrate. The adhesive layer has a shear storage modulus of 40,000 Pa or more at 55°C, a shear stress relief rate of 30% or more after 1 second at 55°C, and an elongation of 2.5% or less when a tensile load is applied to the protective sheet at 23°C and the tensile load reaches 30 N / 15 mm.
Need to check novelty before this filing date? Find Prior Art

Description

Method for manufacturing protective sheets for workpiece machining and individual workpiece sheets This invention relates to a protective sheet for workpiece processing and a method for manufacturing individual workpiece pieces. In particular, it relates to a protective sheet for workpiece processing, and a method for manufacturing individual workpiece pieces using the protective sheet, which is suitable for methods of grinding the back side of a workpiece and individually processing the workpiece by means of stress, etc. With the miniaturization and multifunctionality of various electronic devices, the semiconductor chips mounted on them are also pursuing miniaturization and thinning. To achieve chip thinning, the thickness is typically adjusted by grinding the back side of the semiconductor wafer. Furthermore, to obtain thinner chips, a process called Dicing Before Grinding (DBG) can be used. In DBG, a dicing tool forms grooves of a predetermined depth on the surface of the wafer, and then grinding is performed from the back side, thus obtaining chips by individual wafer assembly. In DBG, because back-side grinding and individual wafer assembly can be performed simultaneously, thin chips can be manufactured efficiently. In the past, when grinding semiconductor wafers and other workpieces on the back side, or when manufacturing semiconductor wafers and other workpiece wafers using DBG, adhesive tape called a back grinding sheet was generally attached to the surface of the workpiece to protect the circuitry on the surface of the workpiece or to hold the workpiece and its wafers. As a back-side abrasive pad used in DBG, an adhesive tape is used, which has a substrate and an adhesive layer provided on one side of the substrate. As an example of such an adhesive tape, Patent Document 1 discloses an adhesive tape with a high Young's modulus substrate, an adhesive layer provided on one side of the substrate, and a buffer layer provided on the other side. In recent years, as a variation of the pre-dicing method, a method has been proposed that uses lasers to create modified regions inside the wafer, and then uses the stress from back-side grinding to wafer individualize the wafer. Hereinafter, this method is sometimes referred to as LDBG (Laser Dicing Before Grinding). In LDBG, since the modified region is used as a starting point to cut the wafer along the crystal direction, chipping is reduced more significantly than in pre-dicing methods that use a dicing blade. Furthermore, compared to DBG, which forms grooves of predetermined depth on the wafer surface using a dicing blade, LDBG does not involve cutting any area of ​​the wafer with a dicing blade; that is, the kerf width is extremely small, resulting in superior wafer yield. [Prior Art Documents] [Patent Documents] Patent document 1: Japanese Patent Application Publication No. 2015-183008. [The problem the invention aims to solve] However, when using the adhesive tape described in Patent Document 1 to wafer-like components via LDBG, slight movement and contact between the wafer-like components occur due to the cutting force applied to them. This results in cracks (accidental cracks) in the wafer-like components. The tendency to crack, as mentioned above, is also due to the extremely small kerf width. In particular, large cracks directly lead to defective wafer-like components, significantly impacting the yield. In view of this actual situation, the object of the present invention is to provide a protective sheet for workpiece processing, which can reduce the number of defective workpiece fragments after grinding, even when the workpiece is processed into individual fragments by LDBG grinding. [Means for solving the problem] The present invention is as follows. [1] A protective sheet for semiconductor processing, comprising a substrate and an adhesive layer disposed on one of the main surfaces of the substrate, wherein the shear storage modulus of the adhesive layer at 55°C is 40,000 Pa or more, the shear stress relief rate of the adhesive layer after 1 second at 55°C is 30% or more, and the elongation of the protective sheet for semiconductor processing is 2.5% or less when a tensile load is applied to the protective sheet for semiconductor processing at 23°C and the tensile load reaches 30 N / 15 mm. [2] As described in [1], a protective sheet for workpiece processing is provided on the main surface of the other side of the substrate, wherein a buffer layer is disposed. [3] The protective sheet for workpiece processing as described in [1] or [2], wherein the tensile stress relief rate of the protective sheet for workpiece processing after 1 minute at 23°C is less than 40%. [4] A protective sheet for workpiece processing as described in any one of [1] to [3], wherein the adhesive layer is composed of an energy-line hardening acrylic adhesive, wherein the acrylic adhesive comprises a polymer bonded to an energy-line hardening group and an energy-line hardening compound. [5] The protective sheet for workpiece processing as described in any one of [1] to [4] is used in the step of forming a workpiece sheet by grinding the back side of the workpiece in which a modified region is formed inside, and attaching it to the surface of the workpiece. [6] A method for manufacturing individual workpiece pieces includes the following steps: attaching a workpiece processing protective sheet as described in any one of [1] to [5] to the surface of a workpiece; forming a modified region inside the workpiece from the surface or back side of the workpiece; grinding the workpiece with the workpiece processing protective sheet attached to the surface and the modified region formed therein from the back side, and individually forming a plurality of workpiece pieces starting from the modified region; and peeling off the workpiece processing protective sheet from the individually formed workpiece. [Effects of the Invention] According to the present invention, a protective sheet for workpiece processing can be provided, which can reduce the number of defective workpiece pieces after grinding, even when the workpiece is individually pieced by LDBG grinding. [The form in which the invention is carried out] The present invention will now be described in detail using drawings based on specific embodiments. First, the main terms used in this specification will be explained. The workpiece refers to a plate-like body that is individually sheeted after the protective sheet for workpiece processing of this embodiment is attached. Examples of workpieces include circular (but including cases with an orientation flat) wafers, rectangular panel-level packages, and strips (short-film substrates) sealed with molded resin, among which wafers are preferred from the viewpoint of easily obtaining the effects of the present invention. Examples of wafers include semiconductor wafers such as silicon wafers, gallium arsenide wafers, silicon carbide wafers, gallium nitride wafers, and indium phosphide wafers, as well as insulator wafers such as glass wafers, lithium tantalate wafers, and lithium niobate wafers. Alternatively, it can be a reconstituted wafer formed from resin and semiconductors for fabricating fan-out packages, etc. From the viewpoint of easily obtaining the effects of the present invention, semiconductor wafers or insulator wafers are preferred, with semiconductor wafers being more preferred. The process of chipification of a workpiece refers to dividing a workpiece into individual chip-sized components based on circuit units. For example, if the workpiece is a wafer, the chip-sized component is a wafer; if the workpiece is a panel-level package or a strip-shaped (short-film-shaped substrate) sealed with molding resin, the chip-sized component is a semiconductor package. The "surface" of a workpiece refers to the surface where circuits, electrodes, etc., are formed, while the "back side" of a workpiece refers to the surface where circuits, etc., are not formed. As an electrode, it can be a convex electrode such as a bump. DBG (Drilling-by-Grinding) refers to a method of grinding a workpiece by creating grooves of a predetermined depth on its surface side and then grinding it from the back side. The grooves formed on the surface side of the workpiece can be created using methods such as blade dicing, laser cutting, and plasma cutting. In addition, LDBG is a variation of DBG, which refers to the method of creating a fragile modified region inside a workpiece (such as a wafer) using a laser, and using the stress during the grinding of the back side of the workpiece as a starting point to allow cracking to progress, thereby enabling the individualization of the workpiece. "Workpiece wafer group" refers to a plurality of workpiece wafers held on the workpiece processing protective sheet of the present invention after the workpiece has been wafered. These workpiece wafers, as a whole, have the same shape as the workpiece. Furthermore, "wafer group" refers to a plurality of wafers held on the workpiece processing protective sheet of the present invention after the workpiece has been wafered into a wafer. These wafers, as a whole, have the same shape as the wafer. "(Meth)acrylate" is used to distinguish between "acrylate" and "methacrylate", and other similar terms are used in the same way. "Energy rays" refer to ultraviolet rays, electron rays, etc., with ultraviolet rays being preferred. Unless otherwise specified, "weight average molecular weight" refers to the converted value of polystyrene determined by gel permeation chromatography (GPC). This method is used, for example, in a Tosoh high-speed GPC apparatus, the "HLC-8120GPC," connected sequentially to a high-speed column, the "TSK guard column H..." XL -H”, "TSK Gel GMH" XL "TSK Gel G2000 H" XL "(All of the above are from Tosoh Corporation) and the detector was used as a differential refractive index detector under the conditions of column temperature: 40°C and liquid delivery rate: 1.0 mL / min. A release sheet is a sheet that can be peeled off to support an adhesive layer. The term "sheet" is used in the context of thin films, without limitation on thickness. The mass ratios in the description of compositions such as adhesive layer compositions are based on the active ingredient (solid fraction) and, unless otherwise specified, do not include solvents. (1. Protective sheet for workpiece processing) As shown in FIG1A, the protective sheet 1 for workpiece processing in this embodiment has a substrate 10 and an adhesive layer 20 disposed on the substrate 10. In this embodiment, as shown in FIG2, the protective sheet 1 for workpiece processing is used to attach an adhesive layer to the main surface 20a of the surface 100a of the workpiece 100 (e.g., a wafer). The surface 100a of the workpiece 100 is a surface having circuits, electrodes, etc. The surface having circuits can be a surface exposing the circuits, or it can be a main surface for protecting the circuits formed on the circuits. In addition, protruding electrodes such as bumps can also be formed on the circuits. In this embodiment, a workpiece with a protective sheet for workpiece processing attached is individually sheeted into a plurality of workpiece sheet-like objects after being ground on its back side. While deepbed grinding (DBG) can be used as a method for sheet-forming the workpiece, the protective sheet 1 for workpiece processing in this embodiment is suitable for sheet-forming workpieces using LDBG. Specifically, after a modified region is formed inside the workpiece, the back side 100b of the main surface of the workpiece 100, on the surface 100a, is ground after the workpiece 100 is attached with a protective sheet 1 for workpiece processing to the surface 100a. As grinding progresses and the workpiece becomes thinner, shear forces and pressures from the modified zones formed within the workpiece cause cracks to form in these zones, which then propagate to both sides of the workpiece. This results in the formation of individual workpiece pieces. In LDBG-based piecemaking, since almost no area is cut from the workpiece, the distance (cut width) between adjacent workpiece pieces (a group of workpiece pieces) is very small. Furthermore, the individual workpieces can be individualized at different times; grinding can begin after a portion of the workpiece has started to be individualized, until the entire workpiece is individualized. Therefore, a grinding wheel can be used to continuously apply shear force to the individual workpiece pieces. Because the uneven surface of the grinding wheel rotates continuously while contacting the group of individual workpiece pieces, the same shear force is not applied to all individual workpiece pieces simultaneously; instead, a different shear force is applied to each individual workpiece piece. Therefore, in the direction parallel to the workpiece plane (i.e., the plane of the group of individual workpiece pieces), due to the separate movement of each individual workpiece piece and the small kerf width, the individual workpiece pieces may come into contact with each other. Such contact makes the individual workpiece pieces prone to cracking. In particular, large cracks associated with defective individual workpiece pieces are more likely to occur. The occurrence of such large cracks will lead to a decrease in the yield of individual workpiece pieces. When the thickness of the workpiece and its individual flakes after grinding is less than 20μm, the individual flakes are more fragile and more prone to large cracks than when the thickness is greater than 20μm. To address this problem, it was thought that a hard protective sheet for workpiece machining could be used to firmly hold the workpiece pieces in place to suppress movement during grinding. However, hardness alone is insufficient to resist shear forces; instead, shear stress caused by these forces makes the workpiece pieces more prone to colliding with each other, increasing the likelihood of cracks. Therefore, for example, a layer with high stress-relieving properties can be incorporated in addition to the substrate and adhesive layer to eliminate shear stress. However, a problem arises where such a layer cannot adequately eliminate shear stress. To address this problem, the inventors of this case conceived of imparting stress-relieving properties to the adhesive layer that is closest to and in contact with the workpiece. The adhesive layer is crucial for ensuring a tight bond between the workpiece and the protective sheet used for workpiece processing; the idea of ​​imparting stress-relieving properties to such an adhesive layer did not exist previously. The inventors of this case discovered that by maintaining the original function of the adhesive layer and simultaneously imparting stress relief to the adhesive layer as described later, the generation of large cracks associated with defective workpiece fragments can be suppressed. The following is a detailed description of the constituent elements of the protective sheet 1 for workpiece machining as shown in Figure 1A. (2. Substrate) The substrate is the rigid component responsible for the protective sheet used in workpiece processing. There are no particular restrictions on the substrate as long as it is made of a material capable of supporting the workpiece. For example, various resin films used as substrates for back-grinding tapes can be cited. By using such resin films, the workpiece can be held in place without damage even if its thickness decreases due to grinding. The substrate can consist of a single layer of resin film or multiple layers of resin film laminated together. (2.1 Material of Substrate) In this embodiment, the material used as the substrate may include, for example, polyesters such as polyethylene terephthalate, polyethylene naphthalate, polyethylene terephthalate, and fully aromatic polyesters, polyamide, polycarbonate, polyacetal, modified polyphenylene oxide, polyphenylene sulfide, polyurethane, polyetherketone, and biaxially stretched polypropylene. Among these, polyester is preferred, and polyethylene terephthalate is even more preferred. Since the thickness of the substrate affects the rigidity of the protective sheet for workpiece processing, it can be set according to the material of the substrate. For example, the thickness of the substrate can be set in a way that makes the physical properties of the protective sheet for workpiece processing fall within the range described later. In this embodiment, a substrate thickness of 25 μm or more and 200 μm or less is preferred, 35 μm or more and 150 μm or less is more preferred, and 40 μm or more and 150 μm or less is even more preferred. To improve the adhesion of the layer formed on the substrate, a bonding treatment such as corona treatment can be performed on at least one of the substrate's main surfaces. Furthermore, to further improve the adhesion of the layer formed on the substrate, an easy-adhesion layer can be formed on at least one of the substrate's main surfaces. (3. Adhesive layer) The adhesive layer is attached to the surface of the workpiece (i.e., the surface where circuits, electrodes, etc. are formed). The adhesive layer serves to protect the surface and support the workpiece until it is peeled off from this surface. The adhesive layer can consist of one layer (single layer) or multiple layers (two or more layers). When the adhesive layer has multiple layers, these multiple layers can be the same or different from each other, and there are no particular restrictions on the combination of the layers that make up these multiple layers. In this embodiment, the adhesive layer possesses the following physical properties, which can mitigate collisions between individual workpiece pieces. As a result, cracks in the workpiece pieces caused by collisions between them, particularly large cracks, can be suppressed. (3.1. Shear Storage Modulus of Adhesive Layer) In this embodiment, the shear storage modulus (G') of the adhesive layer at 55°C is 40,000 Pa or higher. During back-side grinding of the workpiece, heat is generated on the grinding surface, and this heat is also conducted to the adhesive layer. As a result, the temperature of the adhesive layer rises, for example, from 50°C to approximately 60°C. Since the shear storage modulus of the adhesive layer at 55°C is within the aforementioned range, a relatively hard adhesive layer can still be maintained during back-side grinding of the workpiece. Therefore, even if shear forces applied to the workpiece during back-side grinding are transmitted to the adhesive layer, deformation of the adhesive layer can be suppressed. As a result, the amount of movement of the workpiece fragments held by the adhesive layer is reduced, and collisions between the workpiece fragments are suppressed. The shear storage modulus of the adhesive layer at 55°C is preferably 45,000 Pa or higher, more preferably 50,000 Pa or higher, and even more preferably 55,000 Pa or higher. From the viewpoint of easily achieving both the numerical range of the shear storage modulus of the adhesive layer and the numerical range of the shear stress mitigation rate of the adhesive layer (described later), the shear storage modulus of the adhesive layer at 55°C is preferably below 200,000 Pa, more preferably below 150,000 Pa, and even more preferably below 100,000 Pa. The shear storage modulus of the adhesive layer at 55°C can be determined as follows: First, a test sample of a predetermined size is prepared, consisting of the material constituting the adhesive layer. Using a dynamic viscoelasticity measuring device, the test sample is torsionally subjected to shear strain within a predetermined temperature range and at a predetermined frequency, and the modulus of the test sample is measured. The shear storage modulus of the adhesive layer at 55°C is calculated from the measured modulus. Details of the measurement are described in the examples. (3.2. Shear Stress Relief Rate of Adhesive Layer) In this embodiment, the shear stress relief rate of the adhesive layer at 55°C after 1 second is 30% or more. When grinding a workpiece, starting from the initial splitting of individual workpiece pieces into multiple workpiece pieces, the shear force applied to each workpiece piece by the grinding wheel may be uneven between the connected state before splitting and the time point when the workpiece pieces are mixed after splitting. As mentioned above, although the high shear storage modulus of the adhesive layer can relatively suppress deformation of the adhesive layer due to shear force, workpiece pieces located in areas of temporarily high shear force among workpiece pieces with unevenly applied shear force may deform the adhesive layer. If the shear stress relief rate of the adhesive layer at 55°C is not suppressed within the above range, the time required to return to a normal state without deformation when the temporarily high shear force is no longer applied is short, and adjacent workpiece pieces are more likely to experience stronger collisions. However, by suppressing the shear stress relief rate of the adhesive layer at 55°C within the aforementioned range, even if the adhesive layer deforms due to temporarily high shear force, the time required for it to return to its normal, undeformed state after the shear stress is relieved in a short time and the temporarily high shear force is no longer applied is longer. Therefore, the acceleration of the workpiece fragments held by the adhesive layer can be suppressed, and stronger collisions between the workpiece fragments can be suppressed. The shear stress mitigation rate of the adhesive layer at 55℃ is preferably above 35%, and above 38% is even better. The upper limit of the shear stress relief rate of the adhesive layer at 55°C is not particularly limited, as long as it falls within the range where the effects of the present invention can be obtained. In this embodiment, from the viewpoint of considering other physical properties of the adhesive layer, the upper limit of the shear stress relief rate of the adhesive layer at 55°C is preferably 65%, and more preferably 60%. In this embodiment, the shear stress relief rate of the adhesive layer can be determined as follows: A test sample of a predetermined size is prepared, consisting of the material constituting the adhesive layer. Shear strain is applied to the test sample, which is torsionally heated to 55°C, using a dynamic viscoelasticity measuring device. In this embodiment, considering the short-term relief of shear stress, the shear stress relief rate is calculated from the shear stress after the strain is applied and the shear stress one second after the strain is applied. Details of the measurement are described in the examples. (3.3. Composition of the Adhesive Layer) There are no particular limitations as to whether the adhesive layer is composed of an adhesive that satisfies the above-described properties. In this embodiment, the adhesive layer is preferably formed of an energy-curing adhesive. Since the adhesive layer of the protective sheet for workpiece processing is formed of an energy-curing adhesive, it adheres to the workpiece with high adhesion when attached, and the adhesion can be reduced by irradiating the energy line when peeling it off. Therefore, the workpiece's circuitry can be appropriately protected, and damage to the workpiece's circuitry, electrodes, etc., and adhesion to the adhesive on the workpiece can be prevented when peeling off the protective sheet. As a composition for an adhesive layer constituting a line-curing adhesive, for example, a line-curing adhesive layer composition (hereinafter sometimes referred to as "X-type adhesive layer composition") may be used, which includes a non-line-curing adhesive resin (also referred to as "adhesive resin I") as the main component and includes a line-curing compound other than the adhesive resin as the main component. In addition, as a composition for an adhesive layer constituting an energy line curing adhesive, an energy line curing adhesive resin (hereinafter, sometimes referred to as "adhesive resin II") containing side chains in which unsaturated groups are introduced into a non-energy line curing adhesive resin may be used as the main component, and an energy line curing adhesive layer composition (hereinafter, sometimes referred to as "Y-type adhesive layer composition") may be used that does not contain energy line curing compounds other than adhesive resin. Furthermore, as a composition for an adhesive layer constituting an energy-line curing adhesive, a combination of type X and type Y can also be used, that is, an energy-line curing adhesive layer composition that includes an energy-line curing adhesive resin II as the main component and also includes an energy-line curing compound other than the adhesive resin (hereinafter, sometimes referred to as "XY type adhesive layer composition"). However, the adhesive layer can be formed from a non-energy-line-curable adhesive that does not harden even when irradiated with an energy line. The composition constituting the non-energy-line-curable adhesive layer contains at least a non-energy-line-curable adhesive resin I, but does not contain the aforementioned energy-line-curable adhesive resin II or the energy-line-curable compound. In this embodiment, to achieve the aforementioned physical properties of the adhesive layer, an XY-type adhesive layer composition is preferably used as the energy line curing adhesive. By using an XY-type composition, the polymer structure of the adhesive resin II contains a flowable energy line curing compound, making it easier to control stress relief without affecting the range of shear storage modulus. Furthermore, it becomes easier to achieve: sufficient adhesive properties before energy line curing, and sufficient reduction in peel strength to the workpiece after energy line curing. Furthermore, in the following description, "adhesive resin" refers to one or both of the aforementioned adhesive resin I and adhesive resin II. Specific examples of adhesive resins include acrylic resins, urethane resins, rubber resins, and silicone resins. In this embodiment, from the viewpoints of easily controlling the shear storage modulus and shear stress relief rate of the adhesive layer within the aforementioned ranges, and from the viewpoint of reducing costs, acrylic adhesives are preferred. The following is a more detailed explanation of acrylic adhesives using acrylic resins as adhesive resins. (3.3.1. Acrylic Polymers) Acrylic resins utilize acrylic polymers. Acrylic polymers are obtained by polymerizing monomers containing at least an alkyl methacrylate, and include constituent units derived from alkyl methacrylates. As alkyl methacrylates, the alkyl group may have 1 to 20 carbon atoms, and the alkyl group may be straight-chain or branched. Specific examples of alkyl methacrylates include methyl methacrylate, ethyl methacrylate, isopropyl methacrylate, n-propyl methacrylate, n-butyl methacrylate, 2-ethylhexyl methacrylate, n-octyl methacrylate, isooctyl methacrylate, nonyl methacrylate, decyl methacrylate, undecyl methacrylate, and dodecyl methacrylate. Alkyl methacrylates may be used alone or in combination of two or more. Furthermore, from the viewpoint of improving the adhesion of the adhesive layer and easily controlling the shear stress relief rate of the adhesive layer to the aforementioned range, acrylic polymers preferably contain alkyl (meth)acrylate constituents with 4 or more carbon atoms in the alkyl group. The number of carbon atoms in this alkyl (meth)acrylate is preferably 4 to 12, and more preferably 4 to 6. Moreover, alkyl acrylates with 4 or more carbon atoms in the alkyl group are preferably alkyl acrylates. Examples of such alkyl acrylates include n-butyl acrylate, 2-ethylhexyl acrylate, and dodecyl acrylate. The acrylic polymer contains alkyl methacrylates with 4 or more carbon atoms in the alkyl group, preferably 40 to 98 parts by mass, more preferably 45 to 95 parts by mass, and even more preferably 50 to 90 parts by mass relative to 100 parts by mass of the total amount of monomers constituting the acrylic polymer (hereinafter sometimes referred to as "total amount of monomers"). Acrylic polymers, except for those composed of alkyl (meth)acrylates with alkyl groups having 4 or more carbon atoms, are preferably copolymers containing monomeric units, from the perspectives of reducing paste residue in the adhesive layer, increasing adhesion, and easily controlling the shear storage modulus and shear stress relief rate of the adhesive layer to the aforementioned ranges. These monomers, when polymerized to form homopolymers, become polymers with higher glass transition temperatures (Tg). Specifically, when polymerizing to form homopolymers, monomers with a glass transition temperature of 50°C or higher are preferred, monomers with a glass transition temperature of 70°C or higher are more preferred, and monomers with a glass transition temperature of 90°C or higher but below 150°C are further preferred. The Tg of the homopolymer can be found in polymer data handbooks, adhesive handbooks, or polymer handbooks. Examples of such monomers include dimethacrylamide, methyl methacrylate, and acrylmorpholine. Among these, dimethacrylamide and methyl methacrylate are preferred, with dimethacrylamide being even more preferred. When an acrylic polymer forms a homopolymer, the content of monomers with a glass transition temperature of 50°C or higher is preferably 2 to 40 parts by mass relative to 100 parts by mass of the total monomers, more preferably 5 to 30 parts by mass, and even more preferably 8 to 25 parts by mass. In addition to the aforementioned constituent units, acrylic polymers are preferably composed of monomers containing functional groups. Examples of functional groups in monomers include hydroxyl, carboxyl, amino, and epoxy groups. These functionalized monomers can react with crosslinking agents (described later) to become crosslinking initiation points; and can react with substances containing unsaturated groups (described later) to introduce unsaturated groups into the side chains of the acrylic polymer. Examples of monomers containing functional groups include hydroxyl-containing monomers, carboxyl-containing monomers, amine-containing monomers, and epoxy-containing monomers. These can be used alone or in combination of two or more. Among these, the use of hydroxyl-containing monomers and carboxyl-containing monomers is preferred, with the use of hydroxyl-containing monomers being even better. Examples of hydroxyl-containing monomers include, for example, hydroxyalkyl esters of 2-hydroxyethyl acrylate, 2-hydroxyethyl methacrylate, 2-hydroxypropyl acrylate, 3-hydroxypropyl acrylate, 2-hydroxybutyl acrylate, 3-hydroxybutyl acrylate, 4-hydroxybutyl acrylate, etc.; and unsaturated alcohols such as vinyl alcohol and allyl alcohol. Examples of carboxyl-containing monomers include, for example, olefinic unsaturated monocarboxylic acids such as (meth)acrylic acid and crotonic acid; olefinic unsaturated dicarboxylic acids such as fumaric acid, itaconic acid, maleic acid, and citraconic acid and their anhydrides; and 2-carboxyethyl methacrylate. The content of functionalized monomers is preferably 1 to 35 parts by mass, more preferably 3 to 32 parts by mass, and even more preferably 6 to 30 parts by mass, relative to 100 parts by mass of the total monomers constituting the acrylic polymer. In addition to the above, acrylic polymers may also contain monomers that can copolymerize with the aforementioned acrylic monomers derived from styrene, α-methylstyrene, vinyltoluene, vinyl formate, vinyl acetate, acrylonitrile, etc. The aforementioned acrylic polymer can be used as a non-energy-line-curable adhesive resin I. Furthermore, as an energy-line-curable adhesive resin II, examples include those formed by reacting a substance having an energy-line-curable group (also called a substance containing an unsaturated group) with the functional groups of the aforementioned non-energy-line-curable acrylic polymer to form a bond. Substances containing unsaturated groups are those having both a substituent that can bond with the functional groups of acrylic polymers and a line-hardening group. Examples of line-hardening groups include (meth)acrylic, vinyl, allyl, and vinylbenzyl, but (meth)acrylic is preferred. Furthermore, examples of substituents that can bond with the functional groups of acrylic polymers and contain unsaturated groups include isocyanate groups and glycidyl groups. Therefore, examples of substances containing unsaturated groups include (meth)acryloxyethyl isocyanate, (meth)acrylic isocyanate, and (meth)acrylic glycidyl ester. Furthermore, it is preferable that the unsaturated group-containing substance reacts with a portion of the functional groups of the acrylic polymer. Specifically, it is preferable that 50-98 mol% of the functional groups of the acrylic polymer react with the unsaturated group-containing substance, and even more preferable that 55-93 mol% of the functional groups of the acrylic polymer react with the unsaturated group-containing substance. In this way, the energy line curable acrylic resin becomes easier to crosslink via a crosslinking agent because a portion of the functional groups do not react with the unsaturated group-containing substance. In addition, the weight average molecular weight (Mw) of the acrylic resin is preferably 300,000 to 1,600,000, more preferably 400,000 to 1,400,000, and even more preferably 500,000 to 1,200,000. (3.3.2. Energy-line curing compounds) The energy-line curing compounds contained in the compositions for X-type or XY-type adhesive layers are preferably monomers or oligomers that have unsaturated groups within their molecules and can be polymerized and cured by energy-line irradiation. Examples of such energy-line curing compounds include, for example, polyvalent (meth)acrylate monomers such as trimethylolpropane tri(meth)acrylate, neopentyl tert-methacrylate, neopentyl tert-methacrylate, dinepentyl tert-hexa(meth)acrylate, 1,4-butanediol di(meth)acrylate, and 1,6-hexanediol (meth)acrylate monomers; and oligomers such as ethyl carbamate (meth)acrylate, polyester (meth)acrylate, polyether (meth)acrylate, and epoxy (meth)acrylate. Among these, from the viewpoint of relatively high molecular weight and difficulty in reducing the shear storage modulus of the adhesive layer, ethyl carbamate (meth)acrylate oligomers are preferred. The molecular weight of the energy-line curing compound (weight average molecular weight in the case of oligomers) is preferably 100-12000, more preferably 200-10000, further preferably 400-8000, and especially preferably 600-6000. The content of the energy-curing compound in the X-type adhesive layer composition is preferably 40 to 200 parts by weight, more preferably 50 to 150 parts by weight, and even more preferably 60 to 90 parts by weight, relative to 100 parts by weight of the adhesive resin. On the other hand, the content of the energy-curing compound in the XY-type adhesive layer composition is preferably 4 to 90 parts by weight, more preferably 7 to 50 parts by weight, and even more preferably 9 to 25 parts by weight, relative to 100 parts by weight of the adhesive resin. By setting the content of the energy-curing compound within the above range, it is easier to control the shear stress relief rate of the adhesive layer. Furthermore, in the XY-type adhesive layer composition, since the adhesive resin is energy-curing, even if the content of the energy-curing compound is very low, the peel strength can be sufficiently reduced after energy beam irradiation. (3.3.3. Crosslinking Agent) From the viewpoint of more easily increasing the shear storage modulus of the adhesive layer, it is preferable for the adhesive layer composition to further contain a crosslinking agent. The crosslinking agent, for example, reacts with the functional groups of the adhesive resin, causing the resins to crosslink with each other. Examples of crosslinking agents include, for example, isocyanate crosslinking agents (crosslinking agents having isocyanate groups) such as toluene diisocyanate, hexamethylene diisocyanate, and xylene diisocyanate, and their adducts; epoxy crosslinking agents (crosslinking agents having glycidyl groups) such as ethylene glycol glycidyl ether; aziridine crosslinking agents (crosslinking agents having aziridine groups) such as hexa[1-(2-methyl)aziridinyl]triphosphate triazine; metal chelate crosslinking agents (crosslinking agents having metal chelate structures) such as aluminum chelates; and urate crosslinking agents (crosslinking agents having isocyanurate backbones). These crosslinking agents can be used alone or in combination of two or more. From the perspectives of improving the cohesiveness of the adhesive, reducing the paste residue when the adhesive layer is peeled off from individual workpieces, easily controlling the shear storage modulus of the adhesive layer to rise to the aforementioned range, and ease of use, isocyanate crosslinking agents are preferred. From the viewpoint of promoting the crosslinking reaction, the amount of crosslinking agent is preferably 0.01 to 10 parts by weight, more preferably 0.03 to 7 parts by weight, and even more preferably 0.05 to 4 parts by weight, relative to 100 parts by weight of the adhesive resin. (3.3.4. Photopolymerization Initiator) When the adhesive layer composition is energy-line curable, it is preferable that the adhesive layer composition further contains a photopolymerization initiator. By containing a photopolymerization initiator in the adhesive layer composition, the curing reaction can be fully carried out even when irradiated with relatively low-energy energy lines such as ultraviolet light. Examples of photopolymerization initiators include benzoin compounds, acetophenone compounds, phosphine oxide compounds, titanoceramsite compounds, thioxanthone compounds, and peroxides; and photosensitizers such as amines and quinones. Specifically, examples include α-hydroxycyclohexylphenyl ketone, benzoin, benzoin methyl ether, benzoin ethyl ether, benzoin isopropyl ether, benzyl diphenyl sulfide, benzyl dimethyl ketal, tetramethylthiuram monosulfide, azobisisobutyronitrile, dibenzyl, diacetyl, β-chloroanthraquinone, bis(2,4,6-trimethylbenzoyl)phenylphosphine oxide, and 2,4,6-trimethylbenzoyl diphenylphosphine oxide. These photopolymerization initiators can be used alone or in combination of two or more. The amount of photopolymerization initiator prepared relative to 100 parts by weight of adhesive resin is preferably 0.01 to 10 parts by weight, more preferably 0.03 to 5 parts by weight, and even more preferably 0.05 to 5 parts by weight. (3.3.5. Other Additives) Without impairing the effects of the present invention, the adhesive layer composition may also contain other additives. Examples of other additives include, for instance, antistatic agents, antioxidants, softeners (plasticizers), fillers, rust inhibitors, pigments, dyes, etc. When formulating these additives, the amount of additive is preferably 0.01 to 6 parts by weight relative to 100 parts by weight of the adhesive resin. (3.4. Glass Transition Temperature of Adhesive Layer) In this embodiment, the glass transition temperature (Tg) of the adhesive layer is preferably above -50°C and below 30°C. As described above, during back-side grinding, the workpiece (including the case of individual workpiece pieces) is heated to approximately 50-60°C by the grinding heat. Heating is not performed at the same rate across the entire surface of the workpiece; rather, depending on the grinding process, uneven temperatures may occur within the ground surface. With this heating, the adhesive layer directly adjacent to the workpiece is also heated to the same temperature. On the other hand, when the adhesive layer is composed of an adhesive resin, the physical properties of the adhesive resin tend to change significantly around the glass transition temperature of the adhesive resin. For example, if the glass transition temperature of the adhesive layer is greater than the range mentioned above, the properties of the adhesive layer are prone to change during back-side grinding. In particular, as mentioned above, if the workpiece temperature becomes uneven within the surface, the properties of the adhesive layer are also prone to become uneven within the surface. Accompanying this phenomenon, there is a tendency for cracks to form on individual parts of the workpiece. Therefore, during back-side grinding, in order to prevent significant changes in the properties of the adhesive layer, it is best to keep the glass transition temperature of the adhesive layer away from the temperature at which the adhesive layer is heated (50~60°C). Incidentally, as mentioned above, in this embodiment, with the aim of reducing paste residue in the adhesive layer and increasing adhesion, the adhesive layer composition preferably contains monomers with high glass transition temperatures of homopolymers. Therefore, even if the adhesive layer composition contains monomers with high glass transition temperatures of homopolymers, it is preferable to control the glass transition temperature of the adhesive layer within the aforementioned range. The glass transition temperature of the adhesive layer is preferably above -40°C, further preferably above -30°C, further preferably above -20°C, and especially preferably above -10°C. On the other hand, the glass transition temperature of the adhesive layer is preferably below 20°C, further preferably below 10°C, and especially preferably below 0°C. The glass transition temperature of the adhesive layer can be determined as follows. First, a test sample of a predetermined size is prepared, consisting of the material constituting the adhesive layer. Using a dynamic viscoelasticity measuring device, the test sample is torsionally applied to the sample at a predetermined frequency within a predetermined temperature range, and shear strain is applied. The storage modulus and loss modulus of the test sample are measured, and the loss tangent (tanδ) at each temperature is calculated. The peak temperature of the measured loss tangent is set as the glass transition temperature (Tg) of the adhesive layer. Details of the measurement are described in the examples. In this embodiment, the thickness of the adhesive layer is preferably less than 50 μm, more preferably less than 45 μm, and further preferably less than 40 μm. By keeping the thickness of the adhesive layer within the above range, the minute movement of the workpiece pieces caused by the pressure applied to the workpiece or the group of workpiece pieces during grinding can be suppressed. As a result, the probability of the workpiece pieces coming into contact with each other is reduced, and the crack initiation rate can be further suppressed. On the other hand, from the perspective of embedding circuits, electrodes, etc. formed on the workpiece into the adhesive layer, the thickness of the adhesive layer is preferably 10μm or more. In addition, the thickness of the adhesive layer refers to the total thickness of the adhesive layer. For example, the thickness of an adhesive layer composed of multiple layers refers to the total thickness of all the layers that make up the adhesive layer. (4. Physical properties of the protective sheet for workpiece processing) In this embodiment, in addition to the physical properties of the adhesive layer mentioned above, the physical properties of the protective sheet for workpiece processing are controlled as follows. (4.1. Elongation of the protective sheet for workpiece machining) In this embodiment, the elongation of the protective sheet for workpiece machining at 23°C is 2.5% or less. This elongation is the elongation when the tensile load first reaches 30 N / 15 mm after being stretched from both ends of the protective sheet for workpiece machining. This parameter assumes that the protective sheet for workpiece processing is applied under tension while being attached to the workpiece. The environment in which the protective sheet is attached to the workpiece is typically room temperature; therefore, the elongation of the protective sheet at 23°C is defined as the parameter. By ensuring that the elongation of the protective sheet for workpiece processing is within the aforementioned range at 23°C, the tensile stress caused by the tension applied during attachment of the protective sheet can suppress deformation of the protective sheet during back-side grinding. As a result, shift of the individual workpiece pieces caused by deformation of the protective sheet can be suppressed. For protective plates used in workpiece processing at 23°C, an elongation of less than 2.1% is preferred, less than 1.8% is even better, and less than 1.5% is even better. The elongation of the protective sheet used for machining workpieces at 23°C can be determined using a tensile testing apparatus. Details of the measurement are described in the examples. (4.2. Tensile stress mitigation rate of the protective sheet for workpiece machining) In this embodiment, the tensile stress mitigation rate of the protective sheet for workpiece machining at 23°C is preferably less than 40%. This tensile stress mitigation rate is calculated by taking the stress at both ends of the protective sheet for workpiece machining from the stress when the length before stretching is increased by 10%, and taking the stress one minute after the stretching is stopped when the stretching is stopped. With the tensile stress mitigation rate within the aforementioned range, the entire protective sheet for workpiece processing remains undeformed and is supported and fixed to the adsorption stage during back-side grinding. As a result, the amount of movement of the workpiece (a group of individual workpiece pieces) held on the protective sheet for workpiece processing can be suppressed, and cracks caused by collisions between the individual workpiece pieces can also be suppressed. For protective plates used in workpiece processing at 23°C, a tensile stress mitigation rate of 38% or less is preferred, 36% or less is even better, and 34% or less is exceptionally good. Furthermore, there is no particular limitation on the lower limit of the tensile stress relief rate of the protective sheet for workpiece processing at 23°C, but from the viewpoint of workpiece processing workability and cost, it is better to have a rate of 5% or more, and even better to have a rate of 10% or more. The tensile stress relief rate of a protective sheet used for machining workpieces at 23°C can be determined using a tensile testing apparatus. Details of the measurement are described in the examples. (5. Buffer Layer) In this embodiment, the protective sheet for workpiece processing is not limited to the configuration shown in FIG1A. Other layers may be provided as long as the effects of the present invention can be achieved. That is, as long as the configuration of disposing of the adhesive layer 20 on the substrate 10 is present, for example, other layers may be formed between the substrate 10 and the adhesive layer 20. In order to protect the adhesive layer 20 until the adhesive layer 20 is attached to the object to be bonded, a release tab may be disposed on the main surface 20a of the adhesive layer 20. In particular, in this embodiment, as shown in FIG1B, the protective sheet 1 for workpiece processing preferably has a buffer layer 30 in addition to the substrate 10 and the adhesive layer 20. The buffer layer 30 is formed on the main surface 10b opposite to the main surface 10a of the substrate on which the adhesive layer 20 is formed. In addition, the outermost layer of the protective sheet for workpiece processing shown in Figures 1A and 1B can also be formed to perform the desired function, as needed. Compared to the substrate, the buffer layer 30 is a soft layer, which can further alleviate the stress generated during back-side grinding of the workpiece and further prevent cracks from forming on the workpiece. In addition, when the workpiece with the workpiece processing protective sheet is attached is placed on the adsorption stage via the workpiece processing protective sheet during back-side grinding, it becomes easier to hold properly on the adsorption stage because it has a buffer layer as a constituent layer of the workpiece processing protective sheet. On the other hand, from the perspective of reducing raw material costs and reducing the risk of thickness variations during the manufacturing of protective sheets for workpiece processing due to increased thickness, it is preferable to have virtually no buffer layer 30. "Substantially not having" means that the buffer layer is completely absent or its thickness is less than 1 μm. The thickness of the buffer layer is preferably 1~100μm, more preferably 5~80μm, and even more preferably 10~60μm. By setting the thickness of the buffer layer within the above range, the buffer layer can appropriately alleviate the stress during back-side grinding. The buffer layer can be a layer formed by a buffer layer composition containing an energy line polymerizable compound, or it can be a polypropylene membrane, an ethylene-vinyl acetate copolymer membrane, an ionomer resin membrane, an ethylene-(meth)acrylic acid copolymer membrane, an ethylene-(meth)acrylic acid ester copolymer membrane, an LDPE membrane, an LLDPE membrane, etc. In addition, a substrate with a buffer layer can be obtained by laminating the buffer layer onto the substrate. (5.1 Buffer layer composition) A buffer layer composition containing an energy line polymerizable compound can be hardened by irradiation with an energy line. Furthermore, the buffer layer composition containing the energy line polymerizable compound is more specifically preferably composed of ethyl carbamate (meth)acrylate (d1), a polymerizable compound (d2) having an alicyclic or heterocyclic group having 6 to 20 ring atoms, and / or a multifunctional polymerizable compound (d3). In addition, the buffer layer composition may also contain a polymerizable compound (d4) having functional groups, besides the components (d1) to (d3) described above. Furthermore, the buffer layer composition may also contain a photopolymerization initiator, in addition to the components described above. Further, the buffer layer composition may also contain other additives, resin components, etc., without impairing the effects of the present invention. The following describes in detail the components contained in the composition for a buffer layer containing an energy line polymerizable compound. (5.1.1 Ethyl carbamate (meth)acrylate (d1)) Ethyl carbamate (meth)acrylate (d1) refers to a compound having at least a (meth)acrylic acid group and an ethyl carbamate bond, which has the property of being polymerized and hardened by energy beam irradiation. Ethyl carbamate (meth)acrylate (d1) is an oligomer or a polymer. The weight-average molecular weight (Mw) of component (d1) is preferably 1,000 to 100,000, more preferably 2,000 to 60,000, and even more preferably 3,000 to 20,000. Furthermore, the (meth)acrylic acid group (hereinafter also referred to as "functional group") in component (d1) can be monofunctional, difunctional, or trifunctional or more, but monofunctional or difunctional is preferred. Component (d1), for example, is obtained by reacting a hydroxyl-containing (meth)acrylate with a terminal isocyanate ethyl carbamate prepolymer obtained by reacting a polyol compound with a polyvalent isocyanate compound. Alternatively, component (d1) may be used alone or in combination of two or more. The content of component (d1) in the composition for the buffer layer is preferably 10 to 70 parts by mass, more preferably 20 to 60 parts by mass, and even more preferably 25 to 55 parts by mass, relative to 100 parts by mass of the composition for the buffer layer. (5.1.2. Polymerizable compound having an alicyclic or heterocyclic group having 6 to 20 ring atoms (d2)) Component (b2) is a polymerizable compound having an alicyclic or heterocyclic group having 6 to 20 ring atoms. More preferably, it is a compound having at least one (meth)acrylic group, and even more preferably, it is a compound having one (meth)acrylic group. By using component (d2), the film-forming properties of the obtained buffer layer composition can be improved. Furthermore, the definition of component (d2) overlaps with the definitions of components (d3) and (d4) described later, but the overlapping parts are also included in component (d3) or component (d4). For example, a compound having at least one (meth)acrylic acid group, forming an alicyclic or heterocyclic group with 6 to 20 ring atoms, a hydroxyl group, an epoxy group, an amide group, an amino group, etc., is included in the definitions of both component (d2) and component (d4), but in this invention, this compound is set to be included in component (d4). Specific examples of component (d2) include, for instance, alicyclic (meth)acrylates such as isoborneol (meth)acrylate; heterocyclic (meth)acrylates such as tetrahydrofurfuryl (meth)acrylate; and so on. Furthermore, component (d2) can be used alone or in combination of two or more. The content of component (d2) in the composition for the buffer layer is preferably 10 to 70 parts by weight, more preferably 20 to 60 parts by weight, and even more preferably 25 to 55 parts by weight, relative to 100 parts by weight of the composition for the buffer layer. (5.1.3. Multifunctional Polymerizable Compounds (d3)) Multifunctional polymerizable compounds refer to compounds having two or more energy-line hardening groups. Energy-line hardening groups are functional groups containing carbon-carbon double bonds, such as (meth)acryl, vinyl, allyl, and vinylbenzyl. Two or more energy-line hardening groups can also be combined. Through the reaction of the energy-line hardening groups in the multifunctional polymerizable compound with the (meth)acryl group in component (d1) and the reaction of the energy-line hardening groups in component (d3) with each other, a three-dimensional network structure (cross-linked structure) is formed. Using multifunctional polymerizable compounds, compared to using compounds containing only one energy-line hardening group, increases the cross-linked structure formed by energy line irradiation, exhibiting a unique viscoelasticity of the buffer layer and more easily mitigating stress during back-side grinding. Furthermore, the definition of component (d3) overlaps with the definition of component (d4) described later, but the overlapping portion is included in component (d3). For example, compounds containing functional groups such as hydroxyl, epoxy, amide, and amino groups, and having two or more (meth)acrylic acid groups, are included in the definitions of both component (d3) and component (d4), but in this invention, such compounds are designed to be included in component (d3). From the above perspective, the number of energy line hardening groups (functional groups) in multifunctional polymeric compounds is preferably 2 to 10, and even better if it is 3 to 6. In addition, the weight average molecular weight of component (d3) is preferably 30 to 40,000, more preferably 100 to 10,000, and even more preferably 200 to 1,000. Specific components (d3) include, for example, diethylene glycol di(meth)acrylate, ethylene glycol di(meth)acrylate, tetraethylene glycol di(meth)acrylate, neopentyl glycol di(meth)acrylate, 1,6-hexanediol di(meth)acrylate, trimethylolpropane tri(meth)acrylate, neopentyl tetra(meth)acrylate, neopentyl tetra(meth)acrylate, dinepentyl tetra(meth)acrylate, divinylbenzene, vinyl(meth)acrylate, divinyl adipate, N,N'-methylenebis(meth)acrylamide, etc. Among these, neopentyl glycol di(meth)acrylate and dinepentyl tetra(meth)acrylate are preferred. Furthermore, components (d3) can be used alone or in combination of two or more. The content of component (d3) in the composition for the buffer layer is preferably 2 to 40 parts by weight, more preferably 3 to 20 parts by weight, and even more preferably 5 to 15 parts by weight, relative to 100 parts by weight of the composition for the buffer layer. (5.1.4 Polymerizable compound with functional group (d4)) Component (d4) is a polymerizable compound containing functional groups such as hydroxyl, epoxy, amide, and amino groups. More preferably, it is a compound having at least one (meth)acrylic acid group, and even more preferably, it is a compound having one (meth)acrylic acid group. Component (d4) and component (d1) have good compatibility, and the viscosity of the composition for the buffer layer can be easily adjusted to an appropriate range. Furthermore, even when the buffer layer is made relatively thin, the buffering performance remains good. As a component (d4), examples include hydroxyl-containing (meth)acrylates, epoxy-containing compounds, amide-containing compounds, and amine-containing (meth)acrylates. Among these, hydroxyl-containing (meth)acrylates are preferred. To improve the film-forming properties of the buffer layer composition, the content of component (d4) in the buffer layer composition is preferably 5 to 40 parts by weight, more preferably 7 to 35 parts by weight, and even more preferably 10 to 30 parts by weight, relative to 100 parts by weight of the buffer layer composition. (5.1.5 Polymer compounds (d5) other than components (d1) to (d4)) The composition for forming the buffer layer may contain polymer compounds (d5) other than the above-mentioned components (d1) to (d4) without impairing the effects of the present invention. As a component (d5), for example, alkyl (meth)acrylates having alkyl groups having 1 to 20 carbon atoms; ethylene compounds, etc. The content of component (d5) in the composition for the buffer layer is preferably 0 to 20 parts by weight, more preferably 0 to 10 parts by weight, and even more preferably 0 to 5 parts by weight, relative to 100 parts by weight of the composition for the buffer layer. (5.1.6 Photopolymerization initiator) From the viewpoint of shortening the polymerization time caused by light irradiation or reducing the amount of light irradiation when forming the buffer layer, the composition for the buffer layer is preferably further containing a photopolymerization initiator. Examples of photopolymerization initiators include, for example, benzoin compounds, acetophenone compounds, phosphonium oxychloride compounds, titanoceramic compounds, thioxanthone compounds, peroxide compounds, and further, photosensitizers such as amines and quinones. More specifically, examples include, for instance, 1-hydroxycyclohexylphenyl ketone and 2-hydroxy-2-methyl-1-phenyl-propane-1-one. These photopolymerization initiators can be used alone or in combination of two or more. The content of the photopolymerization initiator in the composition for the buffer layer is preferably 0.05 to 15 parts by mass, more preferably 0.1 to 10 parts by mass, and even more preferably 0.3 to 5 parts by mass, relative to 100 parts by mass of the energy-line polymerizable compound. (5.1.7 Other Additives) Without impairing the effects of the present invention, the buffer layer composition may also contain other additives. Examples of other additives include, for instance, antistatic agents, antioxidants, softeners (plasticizers), fillers, rust inhibitors, pigments, dyes, etc. When these additives are formulated, the content of each additive in the buffer layer composition is preferably 0.01 to 6 parts by weight, more preferably 0.1 to 3 parts by weight, relative to 100 parts by weight of the energy-line polymerizable compound. A buffer layer formed from a buffer layer composition containing an energy-polymerizable compound can be obtained by polymerizing and hardening the aforementioned buffer layer composition by energy-ray irradiation. That is, this buffer layer is a product of a hardened buffer layer composition. (6. Method for manufacturing a protective sheet for workpiece machining) The method for manufacturing the protective sheet for workpiece machining according to this embodiment can be a known method. For example, a protective sheet for workpiece machining having a substrate and an adhesive layer formed on one of the main surfaces of the substrate can be manufactured in the following manner. First, as a composition for forming the adhesive layer, for example, a composition for forming the adhesive layer is prepared, or a composition for diluting the composition for forming the adhesive layer is prepared with a solvent (these two compositions are called "adhesive layer coating agents"). The prepared adhesive layer coating agent can be applied to the release surface of the release film and dried as needed to form an adhesive layer on the release film. Then, one main surface of the substrate can be bonded to the adhesive layer to obtain a protective sheet for workpiece processing with an adhesive layer formed on one main surface of the substrate. Alternatively, the prepared adhesive layer coating agent can be directly applied to one main surface of the substrate to form an adhesive layer. In addition, a protective sheet for workpiece processing can be manufactured in the following manner, having a substrate, an adhesive layer formed on the main surface of one side of the substrate, and a buffer layer formed on the main surface of the other side of the substrate. Similar to the above, an adhesive coating agent for forming the adhesive layer is prepared. Next, as a composition for forming the buffer layer, for example, a buffer layer composition constituting the buffer layer is prepared, or a composition of this buffer layer composition diluted with a solvent (these two compositions are referred to as "buffer layer coating agents"). The prepared buffer layer coating agent can be applied to the release surface of the release film, dried as needed, forming a coating film on the release film, and the buffer layer is formed by curing this coating film (e.g., irradiation with energy beams). Subsequently, one of the main surfaces of the substrate can be bonded to the buffer layer. If this buffer layer still has the property of being curable by energy beams, it can be further cured as needed (e.g., irradiation with energy beams). Furthermore, the prepared adhesive layer is applied to the release surface of the release film using a coating agent, and dried as needed to form an adhesive layer on the release film. Then, the main surface of the substrate without the buffer layer is bonded to the adhesive layer, resulting in a workpiece processing protective sheet with an adhesive layer formed on one main surface of the substrate and a buffer layer formed on the other main surface of the substrate. Alternatively, similar to the case of forming the adhesive layer described above, the buffer layer can be directly applied to one main surface of the substrate using a coating agent to form a buffer layer. (7. Method for manufacturing individual workpiece pieces) The protective sheet for workpiece processing of the present invention, as described above, is applicable to the method of individual workpieces using LDBG. As a non-limited example of the use of protective sheets for workpiece processing, the following describes in detail the manufacturing method of workpiece wafers (e.g., wafers) using LDBG. The method for manufacturing individual workpiece wafers specifically includes at least the following steps 1 to 4: Step 1: attaching the aforementioned workpiece processing protective sheet to the surface of the workpiece; Step 2: forming a modified region inside the workpiece from its surface or back side; Step 3: grinding the workpiece with the workpiece processing protective sheet attached to its surface and the modified region formed therein from the back side, using the modified region as a starting point, to wafer into a plurality of workpiece wafers; Step 4: peeling the workpiece processing protective sheet from the wafered workpiece (i.e., the plurality of workpiece wafers). The steps of the above method for manufacturing individual workpiece wafers will be described in detail below. In the description, a wafer is used as a specific example of a workpiece, and a wafer is used as a specific example of a workpiece wafer. (Step 1) In Step 1, an adhesive layer for the workpiece processing protective sheet of this embodiment is attached to the wafer surface. At this time, tension is applied to the workpiece processing protective sheet, but since the tensile stress relief rate of the workpiece processing protective sheet is within the aforementioned range, the workpiece processing protective sheet does not deform and is sufficiently fixed to the adsorption stage during back-side grinding. As a result, wafer movement during back-side grinding is suppressed, and crack formation is inhibited. This step can be performed after Step 2 described later, but from the viewpoint of reducing the risk of unintended wafer localization when attaching the workpiece processing protective sheet, it is preferable to perform it before Step 2. In addition, circuits are formed on the surface of the wafer. The formation of circuits on the wafer surface can be carried out by various methods, including the conventionally used methods such as etching and lift-off. The circuit can be exposed, or a circuit protection layer can be formed to protect the circuit. In addition, convex electrodes such as bumps and pillars can be formed in the circuit. (Step 2) In Step 2, a modified region is formed inside the wafer from the surface or back side of the wafer. The modified region formed in this step is the embrittled portion of the wafer. This modified region is prone to cracking due to the shear force and pressure applied to the wafer. Such cracking becomes the starting point for wafer dicing. That is, the modified region in step 2 is formed in step 3 (described later) along the dicing line where the wafer is diced into individual wafers. The modified region is formed by irradiation with a laser focused on the interior of the wafer. Therefore, the modified region is formed inside the wafer. Laser irradiation can be performed from either the surface or the back side of the wafer. Alternatively, in step 2, which is performed after step 1 and involves laser irradiation from the wafer surface, the wafer is irradiated with a laser via a workpiece protection sheet. A wafer with a protective sheet for workpiece processing attached and a modified region formed thereon is placed on an adsorption stage and held by the adsorption stage. At this time, the surface side of the wafer is adsorbed by the protective sheet for workpiece processing positioned on the adsorption stage side. (Step 3) After Step 1 and Step 2, grind the back side of the wafer on the adsorption stage to break down the wafer into multiple wafers. Here, back-side grinding can be performed with the grinding surface (back side of the wafer) reaching the remodeling region, but the grinding surface can also reach the remodeling region less strictly. That is, starting from the remodeling region, in order to obtain individual wafers of the divided wafer, grinding can be performed to a position close to the remodeling region. In addition, after grinding the back side with a grinding wheel, stress relief can also be achieved through dry polishing or other methods. The shape of the individual wafer can be square or rectangular, or other elongated shapes. Furthermore, the thickness of the individual wafer is not particularly limited, but is preferably around 5-100 μm, more preferably 10-45 μm. According to LDBG, the thickness of the individual wafer is easily set to less than 50 μm, more preferably 10-45 μm. Furthermore, the size of the individual wafer is not particularly limited. For example, the wafer area is preferably less than 600 mm². 2 Ideally, it should be less than 400mm. 2 Further, it is better if it is less than 120mm. 2 . By using the workpiece processing protective sheet of this embodiment, large cracks related to wafer defects can be reduced in the wafer after back-side grinding (step 3). (Step 4) Next, the protective film for workpiece processing is peeled off from the individual wafers (i.e., the wafer array). This step is performed, for example, by the following method. First, the adhesive layer of the protective sheet used for workpiece machining is formed from an energy line-cured adhesive, and is cured by irradiation with an energy line. For example, the irradiance of the energy line is 120~280mW / cm. 2 The light intensity of the energy line is 100~1000 mJ / cm. 2 Ideally, ultraviolet light is preferred as the energy source. Next, pick-up tape is attached to the back side of the wafer array, and its position and orientation are adjusted in a pick-up manner. At this time, the outer periphery of the wafer is also attached to the pick-up tape, fixing the outer edge of the pick-up tape to the frame. The pick-up tape can attach the wafer and the frame simultaneously, or it can attach them at different times. Next, the workpiece processing protective film is peeled off from the plurality of wafers held on the pick-up tape. Subsequently, a plurality of wafers are picked up from the pick-up tape. Next, the wafers are fixed onto a substrate for a device, and the device is manufactured. For example, if the wafers are semiconductors, the wafers are fixed onto a substrate for a semiconductor device, and a semiconductor device is manufactured. In addition, there are no particular limitations on the type of adhesive tape used, but for example, it can be an adhesive sheet having a substrate and an adhesive layer provided on one side of the substrate. The above description pertains to embodiments of the present invention, but the present invention is not limited to any of the above embodiments, and various modifications are possible within the scope of the present invention. [Examples] The invention will be described in more detail below using examples, but the invention is not limited to these examples. The measurement and evaluation methods of this embodiment are shown below. (Shear storage modulus of adhesive layer) In the examples and comparative examples described later, an adhesive layer composition was used to form an adhesive layer on a release film. By preparing a plurality of adhesive layers thus formed, the release film was peeled off, and the peel surfaces were laminated together to produce a laminate of adhesive layers with a thickness of 1 mm. The resulting adhesive layer laminate was stamped into a cylindrical shape with a diameter of 8 mm and used as a sample for determining the shear storage modulus. The shear storage modulus (G') of the adhesive layer was determined using an Anton Paar MCR302 rheometer. The sample was sandwiched between parallel plates at both ends along its thickness direction. Under conditions of -40 to 100°C, a heating rate of 3°C / min, a gap of 1 mm, a strain of 0.05 to 0.5%, and an angular frequency of 1 Hz, the sample was rotated along its thickness direction while a shear force was applied, and the shear storage modulus was measured. The shear storage modulus (G') at 55°C was calculated from the measured values. (Shear stress relief rate of the adhesive layer) A sample for measuring the shear stress relief rate was prepared in the same manner as the sample used to determine the shear storage modulus. The shear stress relief rate of the adhesive layer was measured using an Anton Paar MCR302 rheometer. The sample was heated and maintained at 55°C. With a gap of 1 mm and an angular frequency of 1 Hz, the sample was rotated along its thickness axis to apply shear stress. The stress at the instant (0 seconds) when the strain of the sample reaches 5% (angle 18°) was defined as A. 0, while maintaining a strain of 5%, let the stress generated after 1 second be A. At time 1, the shear stress mitigation rate is calculated from the following formula: Shear stress mitigation rate = {(A 0-A 1) / A 0}×100(%). (Glass transition temperature (Tg) of the adhesive layer) Samples for determining the glass transition temperature (Tg) were prepared in the same manner as those used for determining the shear storage modulus. The glass transition temperature of the adhesive layer was determined using an Anton Paar MCR302 rheometer. The sample was clamped between parallel plates at both ends along its thickness direction. Under the conditions of a measurement temperature of -40 to 100°C, a heating rate of 3°C / min, a gap of 1 mm, a strain of 0.05 to 0.5%, and an angular frequency of 1 Hz, the sample was rotated along its thickness direction while shear force was applied. The loss modulus was measured, and the loss tangent tanδ at each temperature was calculated using the loss modulus and the aforementioned shear storage modulus. From the table of tanδ values ​​obtained for each temperature, the peak temperature was identified and set as the glass transition temperature (Tg) of the adhesive layer. (Elongation and Tensile Stress Relief of Protective Sheets for Workpiece Machining) The protective sheets for workpiece machining prepared in the examples and comparative examples were cut into dimensions of 140 mm in length and 15 mm in width to obtain samples for measuring elongation and tensile stress relief. Using a universal tensile testing apparatus (SHIMADZU, Autograph AG-10kNIS), the samples were clamped 20 mm from both ends along their length (i.e., the initial distance between the clamps was 100 mm). While recording the tensile load, the samples were stretched along their length at a speed of 200 mm / min at 23°C. The elongation of the sample at the point when the tensile load first reached 30 N / 15 mm was measured. Furthermore, under the above conditions, the sample is stretched along its length, and the stretching is stopped at the point where the sample has been stretched by 10% (i.e., the distance between the clamps is 110 mm). The maximum stress from the point of stretching to the point of stopping is set as A (N / m). 2 ) Measure the stress B (N / m) 1 minute after stopping the stretching of the sample 2 ). From the measured values of stress A and B, calculate the tensile stress relaxation rate using the following formula. Tensile stress relaxation rate = {(A - B) / A} × 100 (%) (Crack generation rate) Using a back grinding tape laminator (manufactured by Lintec Corporation, RAD - 3510F / 12), attach the workpiece processing protective sheets produced in the examples and comparative examples to a silicon mirror wafer with a diameter of 300 mm and a thickness of 780 μm as the workpiece. The attachment temperature is 50°C. Then, use a dicing saw (manufactured by Disco Corporation, DFL7361) to perform dicing on the wafer to form a lattice - shaped modified area. The grid size is 10 mm × 10 mm. Next, use a back grinding device (manufactured by Disco Corporation, DGP8761) to perform grinding (including dry polishing) until the opposite side of the wafer surface with the modified area where the workpiece processing protective sheet is attached becomes 18 μm thick, and individualize the wafer into a plurality of chips as a chip group. After the grinding step, in order to easily observe the cracks generated in the chips, use a wafer mounter (RAD - 2510F / 12, manufactured by Lintec Corporation) to attach a dicing tape (manufactured by Lintect Corporation, D - 175D) to the chip group side surface of the chip group with the workpiece processing protective sheet attached (i.e., the ground surface), and a 12 - inch ring frame. Next, irradiate the workpiece processing protective sheet with an energy beam (ultraviolet ray) to peel off the workpiece processing protective sheet and expose the surface of the wafer (chip group). Use an infrared camera embedded in a dicing saw (manufactured by Disco Corporation, DFL7361) to observe and count the cracks on the chips from the wafer surface side. The observation range is set to a range with a radius of 145 mm from the center of the wafer (diameter is 290 mm). Based on the length of the observed cracks, classify as follows. .For one crack, if the longest length is less than 10 μm, it is defined as a small crack. .For one crack, if the longest length is 10 μm or more and less than 20 μm, it is defined as a medium crack. .For one crack, if the longest length is 20 μm or more, it is defined as a large crack. Using the classified crack types, calculate the crack score from the following formula. Crack score = 0 × number of small cracks + 1 × number of medium cracks + 10 × number of large cracks. In this example, when the crack score is 0 or more and 20 or less, it is judged as A; when the crack score is 21 or more and 40 or less, it is judged as B; when the crack score is 41 or more and 55 or less, it is judged as C; when the crack score is 56 or more, it is judged as D. Samples judged as A and B are qualified. (Example 1) (1) Substrate First, as a substrate, a PET film with two easy-to-adhere coating layers on both sides was prepared (thickness: 50 μm, Young's modulus at 23°C: 4000 MPa). (2) The adhesive layer is obtained by copolymerizing 52 parts by mass of n-butyl acrylate (BA), 20 parts by mass of dimethacrylamide (DMAA), and 28 parts by mass of 2-hydroxyethyl acrylate (HEA). The acrylic polymer is then reacted with 2-methacryloxyethyl isocyanate (MOI) in such a way that 90 hydroxyl equivalents are added to the total hydroxyl groups (100 equivalents) of the acrylic polymer to obtain an energy line hardening acrylic copolymer (Mw: approximately 750,000) (BA / DMAA / HEA(MOI)=52 / 20 / 28(90mol%)(A-1). In 100 parts by weight of this energy-line curable acrylic copolymer, 12 parts by weight of polyfunctional ethyl formate acrylate (manufactured by Mitsubishi Chemical Corporation, SHIKOH UT-4332), 1.07 parts by weight of isocyanate crosslinking agent (manufactured by TOSOH Corporation, CORONATE L), and 1.4 parts by weight of bis(2,4,6-trimethylbenzoyl)phenylphosphine oxide as a photopolymerization initiator are prepared. The mixture is diluted with methyl ethyl ketone to prepare a coating agent for an adhesive layer composition with a solids concentration of 34% by weight. (3) Buffer layer (modulation of the combination for forming the buffer layer) As an energy line polymerizable compound, 50 parts by weight of ethyl carbamate acrylate oligomer (manufactured by Sartomer, CN8888) (component d1), 40 parts by weight of isoborneol acrylate (IBXA) (component d2), and 10 parts by weight of neopentyl glycol diacrylate (component d3) were further mixed in, and 2.0 parts by weight of 2-hydroxy-2-methyl-1-phenyl-propane-1-one (manufactured by BASF, Omnirad 1173) as a photopolymerization initiator were further mixed in to prepare the composition for forming the buffer layer. The above-mentioned buffer layer forming composition is coated onto the silicone-treated surface of a release sheet (manufactured by Lintec, SP-PET381031, thickness: 38 μm) to form a coated film. Then, the coated film is irradiated with ultraviolet light to semi-cure the coated film, forming a semi-cure film with a buffer layer thickness of 30 μm. In addition, the aforementioned ultraviolet irradiation was performed using a belt conveyor type ultraviolet irradiation device (EYE GRAPHICS, ECS-401GX) and a high-pressure mercury lamp (EYE GRAPHICS, H04-L41), with a lamp height of 260mm, an output of 80W / cm, and an illuminance of 70mW / cm. 2 Irradiation dose 30mW / cm 2 The process is carried out under the following irradiation conditions. Then, the surface of the formed semi-cured film is bonded to the first coating layer of the substrate, and ultraviolet light is irradiated again from the release liner side of the semi-cured film to completely cure the semi-cured film and form a buffer layer with a thickness of 30 μm. (Fabrication of Protective Sheet for Workpiece Machining) On the silicone-treated surface of a release sheet (Lintec, SP-PET381031, thickness: 38 μm), the coating agent of the above-mentioned adhesive layer composition is applied and heated to dry, forming an adhesive layer with a thickness of 20 μm on the release sheet. The glass transition temperature (Tg) of the adhesive layer is 7.4 °C. Next, a protective sheet for workpiece processing is manufactured by attaching the adhesive layer of the release sheet with the aforementioned adhesive layer to the second coating layer of the PET film with the aforementioned two-sided coating layers. That is, the protective sheet for workpiece processing shown in FIG1B is manufactured. (Example 2) As an acrylic copolymer, except that the amount of isocyanate crosslinking agent (TOSOH Corporation, CORONATE L) added was changed to 0.27 parts by mass, a protective sheet for workpiece processing was obtained by the same method as in Example 1. The glass transition temperatures of the adhesive layer are shown in Table 1. An acrylic polymer obtained by copolymerizing 70 parts by mass of n-butyl acrylate (BA), 20 parts by mass of methyl methacrylate (MMA), and 10 parts by mass of 2-hydroxyethyl acrylate (HEA) was reacted with 2-methacryloxyethyl isocyanate (MOI) by adding 70 equivalent hydroxyl groups to the total hydroxyl groups (100 equivalents) of the acrylic polymer to obtain an energy line hardening acrylic copolymer (Mw: approximately 750,000) (BA / MMA / HEA(MOI) = 70 / 20 / 10 (70 mol%) (A-4). (Example 3) Except that the amount of isocyanate crosslinking agent (TOSOH, CORONATE L) added was changed to 0.54 parts by weight, a protective sheet for workpiece processing was obtained by the same method as in Example 2. The glass transition temperatures of the adhesive layer are shown in Table 1. (Example 4) Except that the amount of isocyanate crosslinking agent (TOSOH, CORONATE L) added was changed to 1.07 parts by weight, a protective sheet for workpiece processing was obtained by the same method as in Example 2. The glass transition temperatures of the adhesive layer are shown in Table 1. (Example 5) Using the acrylic copolymer obtained below, except that the amount of isocyanate crosslinking agent (TOSOH, CORONATE L) added was changed to 0.27 parts by mass, a protective sheet for workpiece processing was obtained by the same method as in Example 1. The glass transition temperatures of the adhesive layer are shown in Table 1. An acrylic polymer obtained by copolymerizing 80 parts by mass of n-butyl acrylate (BA), 10 parts by mass of methyl methacrylate (MMA), and 10 parts by mass of 2-hydroxyethyl acrylate (HEA) was reacted with 2-methacryloxyethyl isocyanate (MOI) by adding 70 hydroxyl equivalents to the total hydroxyl groups (100 equivalents) of the acrylic polymer to obtain an energy line hardening acrylic copolymer (Mw: approximately 750,000) (BA / MMA / HEA(MOI) = 80 / 10 / 10 (70 mol%) (A-3). (Example 6) Except for not forming a buffer layer, a protective sheet for workpiece processing was manufactured using the same method as in Example 1. The glass transition temperatures of the adhesive are shown in Table 1. (Example 7) Except for not forming a buffer layer, a protective sheet for workpiece processing was manufactured using the same method as in Example 2. The glass transition temperatures of the adhesive are shown in Table 1. (Example 8) Except for not forming a buffer layer, a protective sheet for workpiece processing was manufactured using the same method as in Example 3. The glass transition temperatures of the adhesive are shown in Table 1. (Example 9) Except for not forming a buffer layer, a protective sheet for workpiece processing was manufactured using the same method as in Example 4. The glass transition temperatures of the adhesive are shown in Table 1. (Example 10) Except that a buffer layer is not formed, a protective sheet for workpiece processing is manufactured using the same method as in Example 5. The glass transition temperatures of the adhesive are shown in Table 1. (Comparative Example 1) Using the acrylic copolymer obtained below, except that the amount of isocyanate crosslinking agent (TOSOH, CORONATE L) added was changed to 0.27 parts by mass, a protective sheet for workpiece processing was obtained by the same method as in Example 1. The glass transition temperatures of the adhesive layer are shown in Table 1. An acrylic polymer obtained by copolymerizing 90 parts by mass of n-butyl acrylate (BA) and 10 parts by mass of 2-hydroxyethyl acrylate (HEA) was reacted with 2-methacryloxyethyl isocyanate (MOI) by adding 70 hydroxyl equivalents to the total hydroxyl groups (100 equivalents) of the acrylic polymer to obtain an energy line hardening acrylic copolymer (Mw: approximately 750,000) (BA / HEA(MOI) = 90 / 10 (70 mol%) (A-2). (Comparative Example 2) As an acrylic copolymer, except for using the acrylic copolymer obtained below, a protective sheet for workpiece processing was obtained by the same method as in Example 1. The glass transition temperatures of the adhesive layer are shown in Table 1. An acrylic polymer obtained by copolymerizing 85 parts by mass of n-butyl acrylate (BA), 5 parts by mass of methyl methacrylate (MMA), and 10 parts by mass of 2-hydroxyethyl acrylate (HEA) was reacted with 2-methacryloxyethyl isocyanate (MOI) by adding 70 hydroxyl equivalents to the total hydroxyl groups (100 equivalents) of the acrylic polymer to obtain an energy line hardening acrylic copolymer (Mw: approximately 750,000) (BA / MMA / HEA(MOI) = 85 / 5 / 10 (70 mol%) (A-5). (Comparative Example 3) Except that the amount of isocyanate crosslinking agent (TOSOH Corporation, CORONATE L) added was changed to 4 parts by mass, a protective sheet for workpiece processing was obtained by the same method as in Comparative Example 1. The glass transition temperatures of the adhesive are shown in Table 1. (Comparative Example 4) Except for changing the thickness of the substrate to 20 μm, a protective sheet for workpiece processing was obtained using the same method as in Example 2. The glass transition temperatures of the adhesive are shown in Table 1. The obtained samples (Examples 1-10 and Comparative Examples 1-4) were subjected to the above-described measurements and evaluations. The results are shown in Table 1. [Table 1] Table 1 confirms that when the shear storage modulus and shear stress relief rate of the adhesive, and the elongation of the protective sheet for workpiece processing are within the above ranges, it is difficult to generate large cracks related to wafer defects (i.e., defective workpiece individualizations) even when using LDBG individual wafers. 1: Protective sheet for workpiece processing 10: Substrate 10a: Main surface 10b: Main surface 20: Adhesive layer 20a: Main surface 30: Buffer layer 100: Workpiece 100a: Surface 100b: Back side Figure 1A is a cross-sectional schematic diagram showing one example of the protective sheet for workpiece machining according to this embodiment. Figure 1B is a cross-sectional schematic diagram showing another example of the protective sheet for workpiece machining according to this embodiment. Figure 2 is a cross-sectional schematic diagram showing how the protective sheet for workpiece machining according to this embodiment is attached to a workpiece. 1: Protective sheet for workpiece machining 10: Substrate 20: Adhesive layer 20a: Main face

Claims

1. A protective sheet for workpiece processing, comprising a substrate and an adhesive layer disposed on a main surface of one of the substrates, wherein the shear storage modulus of the adhesive layer at 55°C is 40,000 Pa or more, the shear stress relief rate of the adhesive layer after 1 second at 55°C is 55.8% or more, and the elongation of the protective sheet for workpiece processing is 2.5% or less when a tensile load is applied to the protective sheet at 23°C and the tensile load reaches 30 N / 15 mm.

2. The protective sheet for workpiece processing as described in claim 1, wherein a buffer layer is disposed on the main surface of the other side of the aforementioned substrate.

3. The protective sheet for workpiece processing as described in claim 1 or 2, wherein the tensile stress relief rate of the aforementioned protective sheet for workpiece processing after 1 minute at 23°C is less than 40%.

4. The protective sheet for workpiece processing as described in claim 1 or 2, wherein the aforementioned adhesive layer is composed of an energy-line hardening acrylic adhesive, wherein the aforementioned acrylic adhesive comprises a polymer bonded to an energy-line hardening group and an energy-line hardening compound.

5. The protective sheet for workpiece processing as described in claim 1 or 2, wherein the workpiece is sheeted into a workpiece sheet by grinding the back side of the workpiece in which a modified region is formed inside, and is then attached to the surface of the workpiece.

6. A method for manufacturing individual workpiece pieces, comprising the following steps: attaching a workpiece processing protective sheet as described in any one of claims 1 to 5 to the surface of a workpiece; forming a modified region inside the workpiece from the surface or back side of the workpiece; grinding the workpiece with the workpiece processing protective sheet attached to the surface and the modified region formed thereon from the back side, and individually forming a plurality of individual workpiece pieces starting from the modified region; and peeling off the workpiece processing protective sheet from the individually formed workpiece.

Citation Information

Patent Citations

  • Warpage-inhibitive pressure-sensitive adhesive sheets for wafer grinding

    TW200809949A

  • Adhesive tape for semiconductor processing, and semiconductor device manufacturing method capable of suppressing chip cracking even when being used in laser dicing before grinding

    TW201918537A