Silicon carbide sintered body and heat dissipation components

TWI946200BActive Publication Date: 2026-11-11MARUWA
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
TW114146773
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Priority Date
2025-09-12
Filing Date
2025-11-28
Publication Date
2026-11-11
Estimated Expiration
2045-11-27

Smart Images

  • Figure TWG2TB001920952_001
    Figure TWG2TB001920952_001
  • Figure TWG2TB001920952_002
    Figure TWG2TB001920952_002
  • Figure TWG2TB001920952_003
    Figure TWG2TB001920952_003
Patent Text Reader

Abstract

One embodiment of the present invention provides a silicon carbide sintered body comprising: sintered silicon carbide particles and a scandium compound; a thermal conductivity of 275 W / m·K or higher; and a free carbon content of 0.1% by weight or less. The volume resistivity of the aforementioned silicon carbide sintered body is 5.0 Ω·cm or higher. In the aforementioned silicon carbide sintered body, the main crystalline phase of the silicon carbide particles may be composed of a 4H crystal structure. According to one embodiment of the present invention, a silicon carbide sintered body with high thermal conductivity and high resistivity can be provided.
Need to check novelty before this filing date? Find Prior Art

Claims

1. A silicon carbide sintered body, comprising: sintered silicon carbide particles and scandium compounds; containing nitrogen of less than 300 ppm by weight; and containing free carbon of less than 0.1% by weight.

2. The silicon carbide sintered body as described in claim 1, wherein, The volume resistivity is above 5.0 Ω·cm.

3. The silicon carbide sintered body as described in claim 1, wherein, The main crystalline phase of the silicon carbide particles consists of a 4H crystal structure.

4. The silicon carbide sintered body as described in claim 1, wherein, After the surface of the silicon carbide sintered body is ground, the arithmetic mean of the major axis diameter of the silicon carbide particles in any region of the ground surface is greater than 10 μm.

5. The silicon carbide sintered body as described in claim 1, wherein, After the surface of the silicon carbide sintered body is ground, the area-weighted average of the major axis diameter of the silicon carbide particles in any region of the ground surface is greater than 30 μm.

6. The silicon carbide sintered body as described in claim 1, wherein, After the surface of the silicon carbide sintered body is ground, the maximum value of the major axis diameter of the silicon carbide particles in any region of the ground surface is 70 μm or more.

7. The silicon carbide sintered body as described in claim 1, wherein, After the surface of the aforementioned silicon carbide sintered body is ground, the arithmetic mean of the particle area of ​​the aforementioned silicon carbide particles in any region of the ground surface is 50 μm2 or more.

8. The silicon carbide sintered body as described in claim 1, wherein, After the surface of the aforementioned silicon carbide sintered body is ground, the area-weighted average of the particle areas of the aforementioned silicon carbide particles in any region of the ground surface is greater than 300 μm2.

9. The silicon carbide sintered body as described in claim 1, wherein, After the surface of the aforementioned silicon carbide sintered body is ground, the maximum particle area of ​​the aforementioned silicon carbide particles in any region of the ground surface is greater than 1000 μm2.

10. A heat dissipation component using a silicon carbide sintered body as described in any one of claims 1 to 9.

Citation Information

Patent Citations

  • Sintered sic

    JP1992270173A

  • POLYCRYSTAL SiC SINTERED COMPACT PRODUCTION OF THE SAME AND PRODUCT OBTAINED BY APPLYING THE SAME

    JP2001080964A