Abstract
Claims
1. A method for manufacturing an environmentally friendly substrate, comprising the following steps: mixing 15-25 parts by weight of dry pulp with 200-300 parts by weight of water, squeezing out the water to form wet pulp, and refining the wet pulp into shredded pulp (A); drying water bamboo shoot husks, grinding them into water bamboo shoot husk powder, and taking 15-25 parts by weight of the water bamboo shoot husk powder (B); mixing 15-25 parts by weight of glutinous rice flour with 55-65 parts by weight of water and heating and cooking to form glutinous rice glue (C); mixing the aforementioned glutinous rice glue with 15-25 parts by weight of baking soda to form baking soda glutinous rice glue (D); and mixing and stirring the aforementioned shredded pulp, water bamboo shoot husk powder, and baking soda glutinous rice glue to form a mixture to obtain an environmentally friendly substrate (E).
2. The method for manufacturing an environmentally friendly substrate as described in claim 1, wherein, The environmentally friendly substrate is molded into a soft blank, and then the soft blank is dried and shaped to obtain the finished product.
3. The method for manufacturing an environmentally friendly substrate as described in claim 2, wherein, The method involves painting or coloring the finished product.
4. The method for manufacturing an environmentally friendly substrate as described in claim 3, wherein, This method uses laser engraving to paint or color.
5. The method for manufacturing an environmentally friendly substrate as described in claim 1, wherein, In step (A), the wet pulp comprises 20 parts by weight of dry pulp and 260 parts by weight of water.
6. The method for manufacturing an environmentally friendly substrate as described in claim 1, wherein, In step (B), 20 parts by weight of water bamboo shoot husk powder with a size of 0.5mm-1.0mm are used.
7. The method for manufacturing an environmentally friendly substrate as described in claim 6, wherein, The size of the water bamboo shoot husk powder is 0.7mm.
8. The method for manufacturing an environmentally friendly substrate as described in claim 1, wherein, In step (C), the glutinous rice glue contains 20 parts by weight of glutinous rice flour and 60 parts by weight of water.
9. The method for manufacturing an environmentally friendly substrate as described in claim 1, wherein, In step (D), 20 parts by weight of baking soda are used.
10. The method for manufacturing an environmentally friendly substrate as described in claim 1, wherein, In step (A), the wet pulp is refined by using a juicer to break the wet pulp into shredded pulp.