Laminating system, insert injection system including laminating process, laminating method, and insert injection method including laminating process
The laminating system with film-type adhesive and dedicated equipment enhances adhesion between SUS metal sheets and plastic resin, addressing labor costs and environmental issues in vehicle window molding by automating adhesive application and improving bonding strength.
Patent Information
- Application Number
- PCT/KR2023/003978
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-02
- Filing Date
- 2023-03-24
- Publication Date
- 2024-12-05
AI Technical Summary
The existing manual application of solvent-based adhesives for bonding metal sheets to plastic resin in vehicle window molding is labor-intensive and detrimental to the working environment, leading to high labor costs and environmental concerns.
A laminating system and method using a film-type adhesive and dedicated equipment to improve adhesion between SUS metal sheets and plastic resin, involving unwinding, heating, adhesive application, secondary heating, protective tape attachment, and winding, integrated with an insert injection process for enhanced bonding.
This approach significantly increases adhesive strength, reduces labor costs, and improves the working environment by automating the adhesive application process, resulting in improved product quality and reduced odors and pollution.
Smart Images

Figure KR2023003978_05122024_PF_FP_ABST
Abstract
Description
Insert injection molding system including a laminating system and a laminating process, laminating method, and insert injection molding method including a laminating process
[0001] The present invention relates to an insert injection molding system including a laminating system and a laminating process, a laminating method, and an insert injection molding method including a laminating process, and more particularly, to an insert injection molding system including a designed laminating system and a laminating process, which are implemented to improve the adhesion between a metal sheet made of SUS material, which is a raw material of an injection molded product, and a plastic resin when manufacturing an injection molded product, such as a window molding of a vehicle, and a laminating method, and an insert injection molding method including a laminating process.
[0002]
[0003] Typically, vehicle window moldings are manufactured using an insert injection process. The molding is manufactured by press-molding a metal sheet (SUS material), manually applying a solvent-based bond to one side, and then injecting plastic resin into the bonded side.
[0004] In the insert injection process, an adhesive application process is required to bond the metal sheet and plastic resin. However, manpower was invested to apply a solvent-based adhesive to the back of the metal sheet, which had problems such as excessive labor costs and a worsening work environment.
[0005] Meanwhile, the background technology described above is technical information that the inventor possessed for the purpose of deriving the present invention or acquired in the process of deriving the present invention, and cannot necessarily be said to be publicly known technology disclosed to the general public prior to the application for the present invention.
[0006]
[0007] One aspect of the present invention provides an insert injection system including a laminating system and a laminating process, which are implemented to improve the adhesive strength between a metal sheet made of SUS material, which is a raw material for an injection molded product, and a plastic resin when manufacturing an injection molded product, such as a window molding of a vehicle, by introducing a film-type adhesive and a dedicated adhesive facility, and an insert injection system including a laminating method and a laminating process.
[0008] The technical problems of the present invention are not limited to the technical problems mentioned above, and other technical problems not mentioned will be clearly understood by those skilled in the art from the description below.
[0009]
[0010] A laminating system according to one embodiment of the present invention comprises: an unwinding unit for continuously supplying a metal sheet made of SUS material wound in a roll shape while rotating and unwinding the metal sheet; a first heating chamber unit for heating the metal sheet continuously delivered from the unwinding unit to a preset temperature; a film bond adhesive unit for continuously moving the metal sheet heated by the first heating chamber unit and the film-type bond between first and second adhesive rollers that are closely arranged and rotated in the vertical direction while continuously adhering the film-type bond to one surface of the moving metal sheet; a second heating chamber unit for heating the metal sheet to which the film-type bond delivered from the film bond adhesive unit is adhered to at a preset temperature so as to strengthen the adhesion between the film-type bond and the metal sheet; a protection tape attaching unit for attaching an SPV protection tape to the other surface of the metal sheet to which the film-type bond is not adhered; And it includes a winding unit that receives the metal sheet to which the film-type bond and the SPV protective tape are attached and winds it into a roll shape.
[0011] An insert injection system including a laminating process according to one embodiment of the present invention may include: a material receiving unit for receiving a metal sheet made of SUS material; a laminating system for bonding a film-type bond to one surface of the metal sheet prepared in the material receiving unit through a laminating process; a press unit for performing press molding on the metal sheet to which the film-type bond is bonded to manufacture a molded article; a first injection molding unit for performing primary injection molding by injecting a plastic resin onto one surface of the molded article to which the film-type bond is attached to manufacture an injection molded article; a second injection molding unit for performing secondary injection molding by injecting a plastic resin onto one or both surfaces of the injection molded article to reinforce rigidity of the injection molded article; and a processing unit for receiving the molded article from the second injection molding unit and performing a post-injection process.
[0012] A laminating method according to one embodiment of the present invention comprises: an unwinding step of continuously supplying a metal sheet made of SUS material wound in a roll shape from an unwinding unit while rotating and unwinding the metal sheet; a first heating step of heating the metal sheet continuously delivered from the unwinding unit to a preset temperature in a first heating chamber unit; a film bond bonding step of continuously moving the metal sheet heated by the first heating chamber unit and the film-type bond between a first bonding roller and a second bonding roller which are closely arranged vertically and rotatably driven in a film bond bonding unit while continuously adhering the film-type bond to one surface of the moving metal sheet; a second heating step of heating the metal sheet to which the film-type bond delivered from the film bond bonding unit is adhered to at a preset temperature in a second heating chamber unit so as to strengthen the adhesion between the film-type bond and the metal sheet; It includes a protection tape attachment step of attaching an SPV protection tape to the other surface of the metal sheet to which the film-type bond is not attached in a protection tape attachment section; and a winding step of receiving the metal sheet to which the film-type bond and the SPV protection tape are attached in a winding section and winding it in a roll shape.
[0013] An insert injection molding method including a laminating process according to one embodiment of the present invention comprises: a material receiving step of receiving a metal sheet made of SUS material; a laminating step of bonding a film-type bond to one surface of the metal sheet prepared in the material receiving step through a laminating process; a pressing step of performing press molding on the metal sheet to which the film-type bond is bonded to manufacture a molded article; a first injection molding step of injecting a plastic resin into one surface of the molded article to which the film-type bond is attached and performing primary injection molding to manufacture an injection molded article; a second injection molding step of injecting a plastic resin into one surface or both surfaces of the injection molded article to perform secondary injection molding so as to reinforce rigidity of the injection molded article; and a processing step of receiving the molded article manufactured by the second injection molding step and performing a post-injection process.
[0014]
[0015] According to one aspect of the present invention described above, when manufacturing injection molded products such as window moldings for vehicles, the adhesive strength between the metal sheet made of SUS material, which is the raw material of the injection molded product, and the plastic resin is improved through the introduction of a film-type adhesive and adhesive-only equipment, while at the same time providing the effects of reducing labor costs due to manual work by workers and improving the workplace environment (specific odor / contamination of solvent-type bonds, etc.).
[0016] The effects of the present invention are not limited to the effects mentioned above, and various effects may be included within a range apparent to those skilled in the art from the contents described below.
[0017]
[0018] FIG. 1 is a flowchart illustrating an insert injection method including a laminating process according to one embodiment of the present invention.
[0019] FIG. 2 is a schematic diagram illustrating the configuration of an insert injection system including a laminating process according to one embodiment of the present invention.
[0020] FIG. 3 is a drawing showing the product evaluation results of an injection molded product manufactured by an insert injection method including a laminating process according to one embodiment of the present invention.
[0021] Figure 4 is a flowchart illustrating a laminating method according to one embodiment of the present invention.
[0022] Figure 5 is a drawing showing the laminating system of Figure 3.
[0023] FIG. 6 is a schematic diagram illustrating the configuration of an insert injection system including a laminating process according to another embodiment of the present invention.
[0024] Figure 7 is a drawing showing a second air blower according to the present invention.
[0025]
[0026] The following detailed description of the present invention refers to the accompanying drawings, which illustrate specific embodiments in which the present invention may be practiced. These embodiments are described in sufficient detail to enable those skilled in the art to practice the present invention. It should be understood that the various embodiments of the present invention, while different from each other, are not necessarily mutually exclusive. For example, specific shapes, structures, and characteristics described herein may be implemented in other embodiments without departing from the spirit and scope of the present invention. Furthermore, it should be understood that the positions or arrangements of individual components within each disclosed embodiment may be modified without departing from the spirit and scope of the present invention. Accordingly, the following detailed description is not intended to be limiting, and the scope of the present invention is defined only by the appended claims, along with the full scope of equivalents to which such claims are entitled, if properly described. Like reference numerals in the drawings designate the same or similar functionality throughout the several aspects.
[0027] Hereinafter, preferred embodiments of the present invention will be described in more detail with reference to the drawings.
[0028] FIG. 1 is a flowchart illustrating an insert injection method including a laminating process according to one embodiment of the present invention.
[0029] Referring to FIG. 1, an insert injection method including a laminating process according to one embodiment of the present invention first receives a metal sheet (S1) made of SUS material from a material receiving section (10) (S10).
[0030] In the material receipt step (S10), a film-type bond (S2) is bonded to one side of the prepared metal plate (S1) through a laminating process (S20).
[0031] A molded product is manufactured by performing press molding on a metal sheet (S1) to which a film-type bond (S2) is bonded in a laminating system (20) (S30).
[0032] A plastic resin is injected into one side of a molded product to which a film-type bond (S2) is attached in a press section (30) to perform primary injection molding to produce an injection molded product (S40).
[0033] In order to reinforce the rigidity of the injection molded product, a plastic resin is injected into one or both sides of the injection molded product in the first injection molding section (40) to perform secondary injection molding (S50).
[0034] In the second injection molding section (50), the molded product manufactured by the second injection molding step (S50) is received from the processing section (60) and a post-injection process is performed (S60).
[0035] An insert injection method including a laminating process according to an embodiment of the present invention having steps as described above is performed using an insert injection system (1) including a laminating process according to an embodiment of the present invention described below in FIG. 2.
[0036] Referring to FIG. 2, an insert injection system (1) including a laminating process according to one embodiment of the present invention includes a material receiving section (10), a laminating system (20), a press section (30), a first injection molding section (40), a second injection molding section (50), and a processing operation section (60).
[0037] The material receiving section (10) receives a metal sheet (S1) made of SUS430 (0.4T).
[0038] The laminating system (20) adheres a film-type bond (S2) to one side of a metal sheet (S1) prepared in the material receiving section (10) through a laminating process.
[0039] The press section (30) performs press forming on a metal sheet (S1) to which a film-type bond (S2) is bonded to manufacture a molded product.
[0040] The first injection molding section (40) performs primary injection molding by injecting plastic resin into one surface of a molded product to which a film-type bond (S2) is attached, thereby producing an injection product.
[0041] The second injection molding section (50) performs secondary injection molding by injecting plastic resin into one or both sides of the injection molded product to reinforce the rigidity of the injection molded product.
[0042] The processing work unit (60) receives the molded product from the second injection molding unit (50) and performs post-injection processing (e.g., burr removal or defective product selection, etc.).
[0043] An insert injection method including a laminating process according to an embodiment of the present invention having a configuration as described above was confirmed to have a higher average strength standard of '7.21 kgf' than when an injection-molded product is manufactured using a conventional solvent-type bond as shown in FIG. 3 by using a laminating system (20), and it was confirmed that an adhesive strength increase effect of about 1.8 times was generated.
[0044] Accordingly, the insert injection molding method including the laminating process according to one embodiment of the present invention having the configuration described above can improve the adhesive strength between the metal sheet of SUS material, which is the raw material of the injection molded product, and the plastic resin when manufacturing the injection molded product, such as the window molding of a vehicle, by introducing a film-type adhesive and adhesive-only equipment, while providing the effects of reducing labor costs due to manual work by the worker and improving the workplace environment (specific smell / contamination of solvent-type bond, etc.).
[0045] Classification Number of people (persons) Amount (month) Effect amount (month) Effect amount (year) Note Existing solvent type 45135,000,000 won 128,000,000 won 1,536,000,000 won MOLD'G Applicable to all items Changed film type 26,000,000 won Equipment maintenance cost 1,000,000 won
[0046] In addition, the insert injection method including the laminating process according to one embodiment of the present invention having the configuration described above can not only improve the ease of material management, minimize the bond odor, and improve the uniformity of the quality of the injection-molded product, but can also have various advantages in terms of personnel, cost, etc. as indicated in Table 1 above.
[0047]
[0048] Figure 4 is a flowchart illustrating a laminating method according to one embodiment of the present invention.
[0049] Referring to FIG. 4, a laminating method according to one embodiment of the present invention, that is, a laminating step (S20) according to one embodiment of the present invention of FIG. 1, first, continuously supplies a metal sheet (S1) while rotating and unwinding a metal sheet (S1) wound in a roll shape from an unwinding unit (100) (S100).
[0050] A metal sheet (S1) continuously transmitted from a discharge unit (100) is heated to a preset temperature in a first heating chamber unit (200) (S200).
[0051] In one embodiment, the first heating step (S200) may heat the metal plate (S1) by heating the temperature of the internal space of the first heating chamber (200) through which the metal plate (S1) moves to 220 to 260°C.
[0052] A metal sheet (S1) heated by a first heating chamber (200) and a film-type bond (S2) are continuously moved between a first bonding roller (R1) and a second bonding roller (R2) that are arranged in close contact in the vertical direction in a film bond bonding section (300) and are driven to rotate, and the film-type bond (S2) is continuously bonded to one surface of the moving metal sheet (S1) (S300).
[0053] In order to strengthen the adhesion between the film-type bond (S2) and the metal plate (S1), the metal plate (S1) to which the film-type bond (S2) is adhered, which is transferred from the film bond adhesive portion (300), is heated to a preset temperature in the second heating chamber portion (400) (S400).
[0054] In one embodiment, the second heating step (S400) may heat the metal plate (S1) to which the film-type bond (S2) is bonded by heating the temperature of the internal space of the second heating chamber (400) through which the metal plate (S1) is moved to 230 to 270°C.
[0055] In the protective tape attachment section (500), the SPV protective tape (S3) is attached to the other surface of the metal plate (S1) to which the film-type bond (S2) is not attached (S500).
[0056] A metal sheet (S1) to which a film-type bond (S2) and an SPV protective tape (S3) are attached is received from a winding unit (600) and wound into a roll shape (S600).
[0057] The laminating method (S20) according to one embodiment of the present invention having the steps described above may further include a defect detection step (S700) of detecting whether there is a defect in the bonding surface of the metal sheet (S1) and the film-type bond (S2) using a vision inspection in a defect detection unit (900) as illustrated in FIG. 6.
[0058] The laminating method (S20) according to one embodiment of the present invention having the steps as described above may further include a defective section notification step (S700) in which, when a defect is determined to have occurred in the defective section detection step (S700) (in the case of “Yes” in S700 of FIG. 4) and an adhesive defect is notified from the defective section detection unit (900), the defective section notification unit (1000) as shown in FIG. 6 reads the section where the adhesive defect has occurred and then requests the worker to cut and discard the read adhesive defect section or remove the adhesive defect section.
[0059] The laminating method (S20) according to one embodiment of the present invention having the steps described above may further include a cooling step (not shown in the drawing for convenience of explanation) of cooling a metal sheet (S1) to which a film-type bond (S2) transferred from a second heating chamber unit (400) is adhered in a cooling unit (700) and then transferring the metal sheet to a protective tape attachment unit (500).
[0060] The laminating method (S20) according to one embodiment of the present invention having the steps described above may further include a roller overheating prevention step (not shown in the drawing for convenience of explanation) of blowing cold air from a roller overheating prevention unit (800) installed at the front end of the film bond bonding unit (300) toward a metal sheet (S1) fed into the film bond bonding unit (300) to prevent the film-type bond (S2) from sticking to the first adhesive roller (R1) or the second adhesive roller (R2) as the first adhesive roller (R1) or the second adhesive roller (R2) is heated.
[0061]
[0062] A laminating method (S20) according to one embodiment of the present invention having steps as described above is performed using a laminating system (20) according to one embodiment of the present invention.
[0063] Referring to FIG. 5, the laminating system (20) includes a winding unit (100), a first heating chamber unit (200), a film bond adhesive unit (300), a second heating chamber unit (400), a protective tape attachment unit (500), and a winding unit (600).
[0064] The roll-up unit (100) continuously supplies the metal sheet (S1) to the first heating chamber unit (200) while rotating and unwinding the metal sheet (S1) wound in a roll shape.
[0065] In one embodiment, the supply unit (100) supplies the metal sheet (S1) at a linear speed of 1.8 M / MIN, and can control the linear speed of the metal sheet (S1) at a speed of 20 sec±5 sec when accelerating, 20 sec±5 sec when decelerating, and 5 sec±1 sec when stopping.
[0066] The first heating chamber (200) heats the metal sheet (S1) continuously delivered from the discharge unit (100) to a preset temperature.
[0067] In one embodiment, the first heating chamber unit (200) can heat the metal plate (S1) by heating the temperature of the internal space in which the metal plate (S1) moves to 220 to 260°C, preferably 240°C.
[0068] The film bond adhesive unit (300) continuously moves a metal sheet (S1) heated by a first heating chamber unit (200) and a film-type bond (S2) continuously supplied from a film supply device (M1) between a first adhesive roller (R1) and a second adhesive roller (R2) that are arranged in close contact in the vertical direction and rotated, and continuously bonds the film-type bond (S2) to one surface of the moving metal sheet (S1).
[0069] In one embodiment, the film bond adhesive portion (300) preferably sets the pressing force between the first adhesive roller (R1) and the second adhesive roller (R2) to 8 ± 1 kgf / cm2 so that the adhesion of the metal sheet (S1) and the film-type bond (S2) can be efficiently achieved.
[0070] The second heating chamber section (400) heats the metal sheet (S1) to which the film-type bond (S2) transferred from the film bond adhesive section (300) is adhered, to a preset temperature so as to strengthen the adhesion between the film-type bond (S2) and the metal sheet (S1).
[0071] In one embodiment, the second heating chamber unit (400) can heat the metal plate (S1) to which the film-type bond (S2) is bonded by heating the temperature of the internal space in which the metal plate (S1) moves to 230 to 270°C, preferably 250°C.
[0072] The protective tape attachment section (500) attaches the SPV protective tape (S3) continuously supplied from the protective tape supply device (M2) to the other surface of the metal sheet (S1) to which the film-type bond (S2) is not adhered.
[0073] At this time, the SPV protection tape (S3) covers the exterior surface of the final injection molded product (e.g., vehicle molding, etc.) and serves as a protective film.
[0074] In one embodiment, the protective tape attachment portion (500) preferably sets the pressure between the third adhesive roller (R3) and the fourth adhesive roller (R4) to 8 ± 1 kgf / cm2 so that the attachment of the metal plate (S1) and the SPV protective tape (S3) can be efficiently performed.
[0075] The winding unit (600) receives a metal sheet (S1) to which a film-type bond (S2) and an SPV protective tape (S3) are attached and winds it into a roll shape.
[0076] A laminating system (20) having a configuration as described above may further include a cooling unit (700).
[0077] The cooling unit (700) cools the metal sheet (S1) to which the film-type bond (S2) transferred from the second heating chamber unit (400) is attached and then transfers it to the protective tape attachment unit (500).
[0078] In one embodiment, the cooling unit (700) can cool the metal sheet (S1) to which the film-type bond (S2) is bonded to room temperature (e.g., in the range of 20±5°C) by natural cooling or forced cooling using a blower.
[0079] At this time, the film-type bond (S2) can be cooled to room temperature by the cooling unit (700) to become adhesive-free.
[0080] A laminating system (20) having a configuration as described above may further include a roller overheat prevention unit (800).
[0081] The roller overheat prevention unit (800) is installed in the internal space of the film bond bonding unit (300) or at the front end of the film bond bonding unit (300) as illustrated in FIG. 6, and can blow cold air in the direction of the metal sheet (S1) fed into the film bond bonding unit (300) so as to prevent the film-shaped bond (S2) from sticking to the first bonding roller (R1) or the second bonding roller (R2) as the first bonding roller (R1) or the second bonding roller (R2) is heated.
[0082] In one embodiment, the film bond adhesive (300) may be provided with a first air blower (A1) that blows heated compressed air to the adhesive surface of the metal sheet (S1) before the film-type bond (S2) is adhered to the metal sheet (S1) to remove foreign substances such as dust from the adhesive surface of the metal sheet (S1).
[0083] Here, it is preferable that the first air blower (A1) blows air heated to about 200°C to prevent cooling of the metal plate (S1).
[0084] In one embodiment, the protective tape attachment unit (500) may be provided with a second air blower (A2) that sprays compressed air onto the attachment surface of the metal plate (S1) to remove foreign substances such as dust from the attachment surface of the metal plate (S1) before the SPV protective tape (S3) is attached to the metal plate (S1).
[0085] A laminating system (20) having a configuration as described above may further include a defect detection unit (900) and a defect section notification unit (1000).
[0086] The defect detection unit (900) detects whether there is a defect in the bonding surface of the metal sheet (S1) and the film-type bond (S2) using vision inspection, and then transmits the occurrence of a defect to the defect section notification unit (1000).
[0087] The defective section notification unit (1000) divides the metal sheet (S1) supplied from the release unit (100) into sections by a preset length (e.g., 1 m, etc.), and when a defective bond is notified from the defective detection unit (900), the section where the defective bond has occurred is read, and then the section where the defective bond has been read is cut using a personal terminal (1100-1) or a management terminal (1100-2) used by the worker, and then the section is discarded or the defective bond section is removed.
[0088] Accordingly, the worker can improve the quality of the product by cutting and discarding the section where a defect has occurred or removing the section with poor adhesion, which is notified by the defective section notification unit (1000).
[0089]
[0090] The embodiments described above are provided for illustrative purposes only, and those skilled in the art will readily appreciate that the embodiments described above can be readily modified into other specific forms without altering the technical concepts or essential characteristics of the embodiments described above. Therefore, the embodiments described above should be understood as illustrative in all respects and not restrictive. For example, components described as being single may be implemented in a distributed manner, and similarly, components described as being distributed may be implemented in a combined manner.
[0091]
[0092] The scope of protection sought through this specification is indicated by the claims described below rather than the detailed description above, and should be interpreted to include all changes or modifications derived from the meaning and scope of the claims and their equivalent concepts.
Claims
1. A roll-up unit that continuously supplies a metal sheet made of SUS material while rotating and unwinding the metal sheet wound in a roll shape; A first heating chamber unit that heats the metal sheet continuously transmitted from the above-mentioned discharge unit to a preset temperature; A film bond bonding unit that continuously moves the metal sheet heated by the first heating chamber unit and the film-type bond between the first and second bonding rollers that are closely arranged in the vertical direction and rotated, and continuously bonds the film-type bond to one surface of the moving metal sheet; A second heating chamber unit that heats the metal sheet to which the film-type bond is bonded, which is transferred from the film bond bonding unit, to a preset temperature so as to strengthen the bonding between the film-type bond and the metal sheet; A protective tape attachment portion that attaches SPV protective tape to the other surface of the metal sheet to which the film-type bond is not adhered; and A laminating system comprising a winding unit that receives the metal sheet to which the film-type bond and the SPV protective tape are attached and winds it into a roll shape.
2. In paragraph 1, A laminating system further comprising a cooling unit that cools the metal sheet to which the film-type bond is adhered and transferred from the second heating chamber unit and then transfers it to the protective tape attachment unit.
3. In paragraph 1, The above first heating chamber part, A laminating system that heats the metal plate by heating the temperature of the internal space through which the metal plate moves to 220 to 260°C.
4. In paragraph 1, The above second heating chamber part, A laminating system that heats the metal sheet to which the film-type bond is bonded by heating the temperature of the internal space through which the metal sheet moves to 230 to 270°C.
5. In paragraph 1, A laminating system further comprising a roller overheat prevention unit installed at the front end of the film bond bonding portion to blow cold air in the direction of the metal sheet being fed into the film bond bonding portion so as to prevent the film-type bond from sticking to the first adhesive roller or the second adhesive roller as the first adhesive roller or the second adhesive roller is heated.
6. In paragraph 1, The above film bond adhesive portion, A laminating system comprising a first air blower for removing foreign substances from the bonding surface of the metal sheet by spraying heated compressed air onto the bonding surface of the metal sheet before the film-type bond is bonded to the metal sheet.
7. In paragraph 1, The above protective tape attachment part is, A laminating system comprising a second air blower for removing foreign substances from the attachment surface of the metal sheet by blowing compressed air to the attachment surface of the metal sheet before the SPV protective tape is attached to the metal sheet.
8. In paragraph 1, A laminating system further comprising a defect detection unit that detects whether there is a defect in the bonding surface of the metal sheet and the film-type bond using a vision inspection.
9. In paragraph 8, A laminating system further comprising a defective section notification unit that divides the metal sheet supplied from the above-mentioned release unit into preset length units and sets the section, and when a defective bonding is notified from the defective detection unit, reads the section where the defective bonding has occurred and requests the worker to cut and discard the section of the defective bonding or remove the section of the defective bonding.
10. Material receiving department for receiving metal sheets made of SUS material; A laminating system that adheres a film-type bond to one side of the metal sheet prepared in the above material receiving section through a laminating process; A press section for manufacturing a molded product by performing press molding on the metal sheet to which the film-type bond is bonded; A first injection molding unit that performs primary injection molding by injecting plastic resin into one surface of the molded product to which the film-type bond is attached to produce an injection product; A second injection molding unit that performs secondary injection molding by injecting plastic resin into one or both sides of the injection molded product to reinforce the rigidity of the injection molded product; and An insert injection system including a laminating process, comprising a processing work section that receives the molded product from the second injection molding section and performs a post-injection process.
11. A rolling step for continuously supplying a metal sheet made of SUS material wound in a roll shape from a rolling section while rotating the metal sheet; A first heating step of heating the metal sheet continuously delivered from the above-mentioned discharge unit to a preset temperature in a first heating chamber unit; A film bond bonding step of continuously moving the metal sheet heated by the first heating chamber unit and the film-type bond between the first bonding roller and the second bonding roller, which are arranged in close contact in the vertical direction in the film bond bonding unit and are rotatably driven, while continuously bonding the film-type bond to one surface of the moving metal sheet; A second heating step of heating the metal sheet to which the film-type bond is bonded, which is transferred from the film bond adhesive portion, at a preset temperature in a second heating chamber portion so as to strengthen the bonding between the film-type bond and the metal sheet; A protective tape attachment step of attaching an SPV protective tape to the other surface of the metal sheet to which the film-type bond is not adhered in the protective tape attachment portion; and A laminating method, comprising a winding step of receiving the metal sheet to which the film-type bond and the SPV protective tape are attached from a winding unit and winding it into a roll shape.
12. In paragraph 11, A laminating method further comprising a cooling step of cooling the metal sheet to which the film-type bond transferred from the second heating chamber section is adhered in a cooling section and then transferring the metal sheet to the protective tape attachment section.
13. In paragraph 11, The above first heating step is, A laminating method for heating the metal sheet by heating the temperature of the internal space of the first heating chamber section through which the metal sheet moves to 220 to 260°C.
14. In paragraph 11, The second heating step is, A laminating method in which the temperature of the internal space of the second heating chamber section through which the metal sheet is moved is heated to 230 to 270°C to heat the metal sheet to which the film-type bond is bonded.
15. In paragraph 11, A laminating method further comprising a roller overheating prevention step of blowing cold air from a roller overheating prevention unit installed at the front end of the film bond bonding unit in the direction of the metal sheet being fed into the film bond bonding unit to prevent the film-type bond from sticking to the first adhesive roller or the second adhesive roller as the first adhesive roller or the second adhesive roller is heated.
16. In paragraph 11, The above film bond adhesive portion, A laminating method comprising a first air blower for removing foreign substances from the bonding surface of the metal sheet by spraying heated compressed air onto the bonding surface of the metal sheet before the film-type bond is bonded to the metal sheet.
17. In paragraph 11, The above protective tape attachment part is, A laminating method comprising a second air blower for removing foreign substances from the attachment surface of the metal sheet by blowing compressed air to the attachment surface of the metal sheet before the SPV protective tape is attached to the metal sheet.
18. In paragraph 11, A laminating method further comprising a defect detection step of detecting whether there is a defect in the bonding surface of the metal sheet and the film-type bond using a vision inspection in a defect detection unit.
19. In paragraph 18, A laminating method further comprising a defective section notification step in which, when a defective bonding is notified from the above-mentioned defective detection unit, the defective section notification unit reads the section where the defective bonding has occurred and then requests the worker to cut and discard the section of the defective bonding or remove the section of the defective bonding.
20. Material receiving stage for receiving metal sheets made of SUS material; A laminating step of bonding a film-type bond to one side of the metal sheet prepared in the material receiving step through a laminating process; A press step for manufacturing a molded product by performing press molding on the metal sheet to which the film-type bond is adhered; A first injection molding step of producing an injection molded product by performing primary injection molding by injecting a plastic resin into one surface of the molded product to which the film-type bond is attached; A second injection molding step of performing secondary injection molding by injecting plastic resin into one or both sides of the injection molded product to reinforce the rigidity of the injection molded product; and An insert injection molding method including a laminating process, comprising a processing step of receiving the molded product manufactured by the second injection molding step and performing a post-injection process.