Membrane electrode structure for fuel cell and method for manufacturing membrane electrode structure for fuel cell
The membrane electrode assembly for fuel cells addresses the challenge of adhesive quality inspection and electrolyte membrane protection by using a frame with orthogonal inner edges and ultraviolet curable adhesives, ensuring reliable sealing and durability.
Patent Information
- Application Number
- PCT/JP2024/007295
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-30
- Filing Date
- 2024-02-28
- Publication Date
- 2024-10-03
AI Technical Summary
The existing membrane electrode structure for fuel cells makes it difficult to check the quality of the adhesive from the outside, and substances that cause electrolyte membrane deterioration can penetrate, affecting the assembly's reliability and durability.
The membrane electrode assembly features a frame with inner edges extending orthogonally, allowing for the application and curing of ultraviolet curable adhesives between the gas diffusion layers and the electrolyte membrane, ensuring proper sealing and preventing moisture ingress, while enabling easy inspection of adhesion quality.
This configuration allows for effective sealing, prevents electrolyte membrane deterioration, and enhances the durability and reliability of the fuel cell assembly by using ultraviolet curable adhesives that cure below a predetermined temperature, reducing thermal stress and deformation.
Smart Images

Figure JP2024007295_03102024_PF_FP_ABST
Abstract
Description
Membrane electrode assembly for fuel cell and method for manufacturing membrane electrode assembly for fuel cell
[0001] The present invention relates to a membrane electrode assembly for a fuel cell and a method for manufacturing a membrane electrode assembly for a fuel cell.
[0002] In recent years, technological developments have been made in fuel cells that contribute to energy efficiency in order to ensure that more people have access to affordable, reliable, sustainable, and advanced energy. As a technology related to membrane electrode assemblies used in this type of fuel cell, a membrane electrode assembly is known in which a pair of frames are laminated on both sides of an electrolyte membrane, a pair of gas diffusion layers are further laminated on the outside of the frames, and an adhesive is filled between the electrolyte membrane and the pair of frames (see, for example, Patent Document 1).
[0003] JP 2017-182894 A
[0004] However, in the configuration described in Patent Document 1, since the adhesive is filled inside the frame and the gas diffusion layer, it is difficult to check from the outside whether the adhesive is good or bad.
[0005] One aspect of the present invention is a membrane electrode structure for a fuel cell, comprising: a membrane electrode assembly constructed by stacking, in a first direction, an electrolyte membrane, a first gas diffusion electrode layer disposed along one side of the electrolyte membrane, and a second gas diffusion electrode layer disposed along the other side of the electrolyte membrane; and a frame member extending in a second direction perpendicular to the first direction and having an inner edge portion forming an opening in which the membrane electrode assembly is disposed, wherein the first gas diffusion electrode layer has a first gas diffusion layer to which a first reactant gas is supplied, and a first electrode catalyst layer disposed between the electrolyte membrane and the first gas diffusion layer, and the second gas diffusion electrode layer has a second gas diffusion layer to which a second reactant gas is supplied, and a second electrode catalyst layer disposed between the electrolyte membrane and the second gas diffusion layer. The fuel cell membrane electrode structure further includes a first sealing portion, the first sealing portion being a constituent material of an adhesive, and configured to seal between a first surface, which is the surface on one side in a first direction of the inner edge portion of the frame member, and a first side end face, which is the end face in a second direction of the first gas diffusion layer; and a second sealing portion, the second sealing portion being a constituent material of an adhesive, and configured to seal between a second surface, which is the surface on the other side in the first direction of the inner edge portion of the frame member, and a second side end face, which is the end face in the second direction of the second gas diffusion layer.
[0006] Another aspect of the present invention is a method for manufacturing a membrane electrode assembly for a fuel cell, which includes a membrane electrode assembly constructed by stacking, in a first direction, an electrolyte membrane, a first gas diffusion electrode layer disposed along one side of the electrolyte membrane, and a second gas diffusion electrode layer disposed along the other side of the electrolyte membrane, and a frame member extending in a second direction perpendicular to the first direction and having an inner edge portion forming an opening in which the membrane electrode assembly is disposed, wherein a first electrode catalyst layer and a first gas diffusion layer included in the first gas diffusion electrode layer are disposed on one side of the inner edge portion of the frame member in the first direction, and a second gas diffusion electrode layer and a first electrode catalyst layer and a second gas diffusion electrode layer are disposed on the other side of the inner edge portion of the frame member in the first direction. the second electrode catalyst layer, the second electrode catalyst layer, the electrolyte membrane, the inner edge of the frame member, the first electrode catalyst layer, and the first gas diffusion layer in order so as to arrange the second electrode catalyst layer and the second gas diffusion layer included therein; an application step of applying an adhesive to seal between a first surface which is the surface on one side in a first direction of the inner edge of the frame member and a first side end face which is the end face in a second direction of the first gas diffusion layer, and to apply the adhesive to seal between a second surface which is the surface on the other side in the first direction of the inner edge of the frame member and a second side end face which is the end face in the second direction of the second gas diffusion layer; and a curing step of curing the adhesive applied in the application step.
[0007] According to the present invention, it is possible to easily check from the outside whether the adhesiveness is good or bad, while preventing substances that may cause deterioration of the electrolyte membrane from penetrating into the interior.
[0008] 1 is a perspective view schematically showing the overall configuration of a fuel cell stack including a fuel cell membrane electrode assembly according to an embodiment of the present invention. A cross-sectional view taken along line II-II in FIG. 1. A front view showing the schematic configuration of a fuel cell membrane electrode assembly included in the fuel cell stack of FIG. 1. A cross-sectional view taken along line IV-IV in FIG. 3. A diagram illustrating a stacking process included in a manufacturing method of a fuel cell membrane electrode assembly according to an embodiment of the present invention. A diagram illustrating a coating process included in a manufacturing method of a fuel cell membrane electrode assembly according to an embodiment of the present invention. A diagram illustrating a curing process included in a manufacturing method of a fuel cell membrane electrode assembly according to an embodiment of the present invention. A diagram showing the relationship between the integrated amount of light irradiated to an ultraviolet-curing adhesive and the temperature of a frame.
[0009] Hereinafter, an embodiment of the present invention will be described with reference to Figures 1 to 6. A fuel cell membrane electrode assembly according to an embodiment of the present invention constitutes a power generation cell included in a fuel cell stack, which is the main body of the fuel cell. The fuel cell is mounted, for example, in a vehicle and generates electric power to drive the vehicle. First, the overall configuration of a fuel cell stack will be described in brief. A fuel cell stack may also be simply called a fuel cell.
[0010] FIG. 1 is a perspective view showing a schematic overall configuration of a fuel cell stack 100 according to an embodiment of the present invention. Hereinafter, for convenience, three mutually orthogonal axial directions as shown in the figure are defined as the front-rear direction, the left-right direction, and the up-down direction, and the configuration of each part will be described according to these definitions. These directions are not necessarily the same as the front-rear direction, the left-right direction, and the up-down direction of a vehicle. For example, the front-rear direction in FIG. 1 may be the front-rear direction, the left-right direction, or the up-down direction of a vehicle.
[0011] As shown in FIG. 1 , a fuel cell stack 100 includes a cell stack 101 formed by stacking a plurality of power-generating cells 1 in the front-rear direction, and end units 102 disposed at both front and rear ends of the cell stack 101. The overall structure has a generally rectangular parallelepiped shape. The cell stack 101 has a longer left-right length than a longer vertical length. For convenience, FIG. 1 shows only a single power-generating cell 1. The power-generating cell 1 includes a unitized electrode assembly (UEA) 2 having a membrane electrode assembly including an electrolyte membrane and electrodes, and a pair of front and rear separators 3, 3 disposed on both the front and rear sides of the unitized electrode assembly 2 and sandwiching the unitized electrode assembly 2 between them. The unitized electrode assemblies 2 and the separators 3 are alternately disposed in the front-rear direction. Although not shown, a generally box-shaped case with open front and rear faces is disposed around the cell stack 101. The front end surface of the case and the front end unit 102, and the rear end surface of the case and the rear end unit 102 are fastened together by bolts.
[0012] Fig. 2 is a cross-sectional view (a cross-sectional view taken along line II-II in Fig. 1) of a portion of the cell stack 101. As shown in Fig. 2, the separator 3 has a front plate 31 and a rear plate 32, which are a pair of front and rear thin metal plates having a corrugated cross section. The outer peripheral edges of the front plate 31 and the rear plate 32 are joined together by welding or the like to form the separator 3. The separator 3 is made of a conductive material with excellent corrosion resistance, such as stainless steel, titanium, or a titanium alloy.
[0013] A cooling flow path PAw through which a coolant flows is formed inside the separator 3 surrounded by the front plate 31 and the rear plate 32, and the flow of the coolant cools the power generation surface of the power generation cell 1. Water, for example, can be used as the coolant. The surfaces (front and rear surfaces) of the separator 3 facing the integrated electrode assembly 2 are formed unevenly by press molding or the like to form gas flow paths between the separator 3 and the integrated electrode assembly 2. More specifically, the front plate 31 and the rear plate 32 each have rib portions 301 that protrude toward the front and rear integrated electrode assemblies 2, and recesses 302 that are continuous with the rib portions 301 and are formed in a concave shape.
[0014] The rear rib portion 301 abuts against the front surface 2a of the integrated electrode assembly 2, and the front rib portion 301 abuts against the rear surface 2b of the integrated electrode assembly 2. A compressive load F is applied to the cell stack 101 in the front-to-rear direction when assembling the fuel cell stack 100, and in this state the case and the front and rear end units 102 are fastened together. After assembly of the fuel cell stack 100 is complete, this compressive load F is maintained. Therefore, a predetermined surface pressure due to the compressive load F acts on the integrated electrode assembly 2 in the front-to-rear direction via the rib portion 301.
[0015] An anode flow path PAa through which a fuel gas flows is formed by a recess 302 between the front surface 2a of the integrated electrode assembly 2 and the rear plate 32 of the separator 3 facing this front surface 2a. A cathode flow path PAc through which an oxidizer gas flows is formed by the recess 302 between the rear surface 2b of the integrated electrode assembly 2 and the front plate 31 of the separator 3 facing this rear surface 2b. For example, hydrogen gas containing hydrogen can be used as the fuel gas, and air containing oxygen can be used as the oxidizer gas.
[0016] Fig. 3 is a front view showing a schematic configuration of an integrated electrode assembly 2 serving as a membrane electrode structure. As shown in Fig. 3, the integrated electrode assembly 2 has a substantially rectangular membrane electrode assembly (MEA) 20 and a frame 21 that supports the membrane electrode assembly 20. As shown in the detailed view of portion A in Fig. 2, the membrane electrode assembly 20 has an electrolyte membrane 23, an anode electrode 24 provided on a front surface 231 of the electrolyte membrane 23, and a cathode electrode 25 provided on a rear surface 232 of the electrolyte membrane 23.
[0017] The electrolyte membrane 23 is, for example, a solid polymer electrolyte membrane, and a thin film of a perfluorosulfonic acid polymer containing water can be used. The electrolyte membrane 23 is not limited to a fluorine-based electrolyte membrane, and a hydrocarbon-based electrolyte membrane can also be used.
[0018] The anode 24 is formed on the front surface 231 of the electrolyte membrane 23 and includes an electrode catalyst layer 241 that serves as a reaction field for the electrode reaction, and a gas diffusion layer 242 that is provided on the front surface of the electrode catalyst layer 241 and diffuses and supplies a fuel gas. An intermediate layer (base layer) may be provided between the electrode catalyst layer 241 and the gas diffusion layer 242. The cathode 25 is formed on the rear surface 232 of the electrolyte membrane 23 and includes an electrode catalyst layer 251 that serves as a reaction field for the electrode reaction, and a gas diffusion layer 252 that is provided on the rear surface of the electrode catalyst layer 251 and diffuses and supplies an oxidant gas. An intermediate layer (base layer) may be provided between the electrode catalyst layer 251 and the gas diffusion layer 252.
[0019] The electrode catalyst layers 241, 251 contain a catalytic metal that promotes the electrochemical reaction between hydrogen contained in the fuel gas and oxygen contained in the oxidant gas, a proton-conductive electrolyte (e.g., ionomer), and electron-conductive carbon particles. The gas diffusion layers 242, 252 are made of a gas-permeable conductive material, such as a porous carbon material. The gas diffusion layers 242, 252 are primarily composed of carbon and fluorine, and therefore have water-repellent properties.
[0020] At the anode electrode 24, the fuel gas (hydrogen) supplied via the anode flow path PAa is ionized by the action of a catalyst and passes through the electrolyte membrane 23 to move toward the cathode electrode. The electrons generated at this time pass through an external circuit and are extracted as electrical energy. At the cathode electrode 25, the oxidant gas (oxygen) supplied via the cathode flow path PAc reacts with the hydrogen ions introduced from the anode electrode 24 and the electrons transferred from the anode electrode 24 to produce water. The produced water provides an appropriate humidity to the electrolyte membrane 23, and excess water is discharged to the outside of the integrated electrode assembly 2 along the gas flow.
[0021] The frame 21 in Figure 3 is a thin, generally rectangular plate with a thickness of approximately 0.05 to 0.1 mm, and can be made of insulating resin, rubber, or the like. Examples of materials that can be used include PEN (polyethylene naphthalate) and PPS (polyphenylene sulfide). In particular, in this embodiment, PPS is used as the material for the frame 21. When PEN is used while immersed in water, hydrolysis occurs, and its strength decreases over time. In contrast, PPS has high hydrolysis resistance and shows almost no decrease in strength over time.
[0022] A substantially rectangular opening 210 is provided in the center of the frame 21, and the membrane electrode assembly 20 is provided so as to cover the entire opening 210. The frame 21 has a substantially rectangular outer edge 221 and a substantially rectangular inner edge 222 inside the outer edge 221. The outer edge 221 refers to the outer edge of the frame 21 and its surrounding area, and the inner edge 222 refers to the inner edge of the frame 21 (the edge of the opening 210) and its surrounding area. A frame-shaped adhesive portion 40 is provided around the opening 210 by applying an adhesive.
[0023] 3 is a center point passing through the middle in the vertical and horizontal directions of the opening 210. On the left side of the opening 210 in the frame 21, three through-holes 201 to 203 that penetrate the frame 21 in the front-to-rear direction are opened in a line up in the vertical direction, and on the right side of the opening 210, three through-holes 204 to 206 that penetrate the frame 21 in the front-to-rear direction are opened in a line up in the vertical direction.
[0024] As shown in FIG. 1 , the front and rear separators 3 of the integrated electrode assembly 2 are provided with through-holes 311 to 316 that penetrate the separators 3 in the front-rear direction at positions corresponding to the through-holes 201 to 206 in the frame 21. The through-holes 311 to 316 are connected to the through-holes 201 to 206 in the frame 21, respectively. These mutually connected through-holes 201 to 206 and 311 to 316 collectively form flow paths PA1 to PA6 (indicated by arrows for convenience) that penetrate the cell stack 101 and extend in the front-rear direction. The flow paths PA1 to PA6 are sometimes called manifolds. The flow paths PA1 to PA6 are connected to a manifold external to the fuel cell stack 100.
[0025] Flow path PA1 (solid arrow) extending forward via through-holes 201 and 311 is a fuel gas supply flow path. Flow path PA6 (solid arrow) extending rearward via through-holes 206 and 316 is a fuel gas discharge flow path. The fuel gas supply flow path PA1 and the fuel gas discharge flow path PA6 are connected to an anode flow path PAa ( FIG. 2 ) provided opposite the front surface of the membrane electrode assembly 20, and as shown by the solid arrows, fuel gas flows to the right through the anode flow path PAa via the fuel gas supply flow path PA1 and the fuel gas discharge flow path PA6. Communication between the anode flow path PAa and the other flow paths PA2 to PA5 is blocked via a seal (not shown).
[0026] A flow path PA4 (dotted arrow) extending forward via the through-holes 204 and 314 is an oxidant gas supply flow path. A flow path PA3 (dotted arrow) extending rearward via the through-holes 203 and 313 is an oxidant gas discharge flow path. The oxidant gas supply flow path PA4 and the oxidant gas discharge flow path PA3 are connected to a cathode flow path PAc ( FIG. 2 ) provided opposite the rear surface of the membrane electrode assembly 20. As shown by the dotted arrows, the oxidant gas flows leftward through the cathode flow path PAc via the oxidant gas supply flow path PA4 and the oxidant gas discharge flow path PA3. Communication between the cathode flow path PAc and the other flow paths PA1, PA2, PA5, and PA6 is blocked by a seal (not shown).
[0027] A flow path PA5 (indicated by a dashed-dotted arrow) extending forward through through-holes 205 and 315 is a coolant supply flow path. A flow path PA2 (indicated by a dashed-dotted arrow) extending rearward through through-holes 202 and 312 is a coolant discharge flow path. The coolant supply flow path PA5 and the coolant discharge flow path PA2 communicate with a cooling flow path PAw ( FIG. 2 ) provided inside the separator 3, and the coolant flows through the cooling flow path PAw via the coolant supply flow path PA5 and the coolant discharge flow path PA2. Communication between the cooling flow path PAw and the other flow paths PA1, PA3, PA4, and PA6 is blocked by a seal (not shown).
[0028] End units 102, arranged on both the front and rear sides of the cell stack 101, each have a terminal plate 4, an insulating plate 5, and an end plate 6. The rear end unit 102 has a plurality of through holes 102a to 102f that penetrate the end unit 102 in the front-to-rear direction. The through hole 102a is opened on an extension of the fuel gas supply channel PA1 and communicates with the fuel gas supply channel PA1. The through hole 102b is opened on an extension of the coolant discharge channel PA2 and communicates with the coolant discharge channel PA2. The through hole 102c is opened on an extension of the oxidant gas discharge channel PA3 and communicates with the oxidant gas discharge channel PA3. The through hole 102d is opened on an extension of the oxidant gas supply channel PA4 and communicates with the oxidant gas supply channel PA4. The through hole 102e is opened on an extension of the coolant supply channel PA5 and communicates with the coolant supply channel PA5. The through-hole 102f is opened on an extension of the fuel gas discharge passage PA6 and communicates with the fuel gas discharge passage PA6.
[0029] More specifically, a fuel gas tank storing high-pressure fuel gas is connected to the through-hole 102a via an ejector, an injector, etc., and the fuel gas is supplied to the fuel cell stack 100 via the through-hole 102a. The fuel gas is discharged from the through-hole 102f. A compressor for supplying oxidant gas is connected to the through-hole 102d, and the oxidant gas compressed by the compressor is supplied to the fuel cell stack 100 via the through-hole 102d. The oxidant gas is discharged from the through-hole 102c. A pump for supplying a cooling medium is connected to the through-hole 102e, and the cooling medium is supplied to the fuel cell stack 100 via the through-hole 102e. The cooling medium is discharged from the through-hole 102b. The discharged cooling medium is cooled by heat exchange in the radiator and is supplied again to the fuel cell stack 100 via the through-hole 102e.
[0030] The above is a schematic configuration of the fuel cell stack 100. Next, a description will be given of the characteristic configuration of the integrated electrode assembly 2 as a membrane electrode structure for a fuel cell according to this embodiment. The integrated electrode assembly 2 according to this embodiment is characterized by the configuration of the periphery of the opening 210 of the frame 21.
[0031] Figure 4 is a cross-sectional view taken along line IV-IV in Figure 3, showing the configuration around the inner edge 222 on the left side of the frame 21. The configuration around the inner edge 222 is the same around the entire periphery of the inner edge 222 along the opening 210. Hereinafter, the rightward direction in Figure 4, i.e., the direction toward the center point P in Figure 3 (toward the center), will be referred to as the inner direction or inward, and the rightward side in Figure 4 will be referred to as the inside. Furthermore, the leftward direction in Figure 4, i.e., the direction toward the outer edge 221 in Figure 3, will be referred to as the outer direction or outward, and the leftward direction in Figure 4 will be referred to as the outside.
[0032] As shown in Figure 4, the electrode catalyst layer 251 and gas diffusion layer 252 that constitute the cathode electrode 25, and the electrolyte membrane 23 are configured to be flat in the left-right direction toward their left end faces 251a, 252a, and 23a (outer end faces). The left end face 251a of the electrode catalyst layer 251, the left end face 252a of the gas diffusion layer 252, and the left end face 23a of the electrolyte membrane 23 are located at the same position in the left-right direction. The rear end face 252b of the gas diffusion layer 252 corresponds to the rear end face of the integrated electrode assembly 2. The corner where the left end face 252a and the rear end face 252b of the gas diffusion layer 252 intersect is the trailing edge point P3.
[0033] The electrode catalyst layer 241 and gas diffusion layer 242 constituting the anode electrode 24 bend forward near their left end surfaces 241a, 242a (outer end surfaces) by an amount corresponding to the thickness of the frame 21 provided on the front surface of the electrolyte membrane 23. Therefore, the anode-side electrode catalyst layer 241 is spaced from the front surface 231 of the electrolyte membrane 23 near the left end surface 241a. The rear surface 232 of the electrolyte membrane 23 remains bonded to the cathode-side electrode catalyst layer 251 over the entire left-right direction. The left end surface 241a of the electrode catalyst layer 241 and the left end surface 242a of the gas diffusion layer 242 are located at the same position in the left-right direction. The front end surface 242b of the gas diffusion layer 242 corresponds to the front end surface of the integrated electrode assembly 2. The corner where the left end surface 242a and the front end surface 242b of the gas diffusion layer 242 intersect is the leading edge point P2.
[0034] The frame 21 is a frame-shaped member made of PPS and is flat in the left-right direction up to an opening 210 at its right end. The frame 21 has a front surface 211 and a rear surface 212. An adhesive layer 213, where an adhesive is applied, is provided on the rear surface 212 of the frame 21 up to the opening 210. The rear surface 212 of the inner edge portion 222 of the frame 21 and the electrolyte membrane 23 are joined via the adhesive layer 213. An electrode catalyst layer 241 of the anode 24 is laminated on the front surface 211 of the inner edge portion 222 of the frame 21.
[0035] At the intersection between the front surface 211 of the frame 21 and the left end surface 242a of the gas diffusion layer 242 of the anode electrode 24, an adhesive portion 40 (front adhesive portion 41) made of an adhesive is provided from the front surface 211 to the left end surface 242a. On the left end surface 242a of the gas diffusion layer 242, the front end of the front adhesive portion 41 is located forward of the left end surface 241a of the electrode catalyst layer 241 and within a range not exceeding a leading edge point P2 of the gas diffusion layer 242. Therefore, although the front end of the front adhesive portion 41 coincides with the leading edge point P2 in FIG. 4 , the front end of the front adhesive portion 41 may be located rearward of the leading edge point P2.
[0036] At the intersection between the rear surface 212 of the frame 21 and the left end surface 252a of the gas diffusion layer 252 of the cathode electrode 25, an adhesive portion 40 (rear adhesive portion 42) made of an adhesive is provided from the rear surface 212 to the left end surface 252a. On the left end surface 252a of the gas diffusion layer 252, the rear end portion of the rear adhesive portion 42 is located rearward of the left end surface 251a of the electrode catalyst layer 251 and within a range not exceeding a trailing edge point P3 of the gas diffusion layer 252. Therefore, although the rear end portion of the rear adhesive portion 42 coincides with the trailing edge point P3 in FIG. 4 , the rear end portion of the rear adhesive portion 42 may be located forward of the trailing edge point P3.
[0037] An ultraviolet-curable adhesive that hardens when exposed to ultraviolet light is used for the front and rear adhesive portions 40. For example, an ultraviolet-curable adhesive made of an olefin resin is used. Examples of such ultraviolet-curable adhesives include those manufactured by ThreeBond Co., Ltd. under the trade names "UV-Curable Olefin Resin TB3175 and TB3178" and those manufactured by Toagosei Co., Ltd. under the trade name "Aronix UVX-6654." Using these adhesives increases the hardening speed, thereby shortening the time required to manufacture the integrated electrode assembly 2.
[0038] Furthermore, a rapid temperature rise in the frame 21 during UV irradiation can be suppressed, thereby suppressing deformation of the frame 21, such as warping or undulation. In other words, in this embodiment, the frame 21 is formed using PPS as a constituent material. PPS has high hydrolysis resistance but a higher thermal shrinkage rate than PEN. Therefore, if the heat input during adhesive curing is large, the frame may deform due to thermal stress, potentially preventing sufficient sealing performance between the frame and the separators 3 ( FIG. 1 ) before and after it. For example, if a thermosetting adhesive is used, deformation of the frame 21 becomes a problem. In contrast, UV-curable adhesives have a smaller heat input than thermosetting adhesives, so deformation of the frame 21 due to thermal stress is suppressed, ensuring sufficient sealing performance.
[0039] Separators 3 are disposed on both the front and rear sides of the frame 21. An anode flow path PAa is formed between the front surface 211 of the frame 21 and the rear plate 32 (FIG. 2) of the separator 3. A cathode flow path PAc is formed between the rear surface 212 of the frame 21 and the front plate 31 (FIG. 2) of the separator 3. Because the separator 3 contains iron as a component, water produced by the electrochemical reaction between the fuel gas and the oxidant gas and condensed water accumulates in the anode flow path PAa and the cathode flow path PAc, and iron ions may elute into this accumulated water.
[0040] Because eluted iron ions can cause deterioration of the electrolyte membrane 23, it is necessary to configure the electrolyte membrane 23 so that moisture containing iron ions does not penetrate into the electrolyte membrane 23. Therefore, it is preferable to prevent the electrolyte membrane 23 from being exposed to the flow paths PAa and PAc. Furthermore, the electrode catalyst layers 241 and 251 contain an electrolyte such as an ionomer, which serves as a path for moisture to penetrate. Therefore, it is also preferable to prevent the electrode catalyst layers 241 and 251 from being exposed to the flow paths PAa and PAc.
[0041] In this regard, in the present embodiment, a front adhesive portion 41 is provided from the front surface 211 of the frame 21 to the left end surface 242a of the gas diffusion layer 242 of the anode electrode 24, and a rear adhesive portion 42 is provided from the rear surface 212 of the frame 21 to the left end surface 252a of the gas diffusion layer 252 of the cathode electrode 25. As a result, the electrolyte membrane 23 and the electrode catalyst layers 241, 251 are not exposed to the flow paths PAa, PAc on the front and rear sides of the frame 21. This blocks the path of moisture penetration leading to the electrolyte membrane 23, preventing moisture containing iron ions from penetrating the electrolyte membrane 23. As a result, deterioration of the electrolyte membrane 23 can be suppressed, and the durability of the integrated electrode assembly 2 is improved.
[0042] A method for manufacturing a fuel cell membrane electrode structure according to an embodiment of the present invention will be described with reference to Figures 5A to 5C. In Figures 5A to 5C, the thickness of each part is emphasized. When manufacturing an integrated electrode assembly 2 as a fuel cell membrane electrode structure, first, as shown in Figure 5A, a cathode electrode 25, an electrolyte membrane 23, a frame 21, and an anode electrode 24 are stacked in this order (stacking step).
[0043] More specifically, the anode 24 is formed by applying an electrode catalyst layer 241 to a gas diffusion layer 242, and the cathode 25 is formed by applying an electrode catalyst layer 251 to a gas diffusion layer 252. Next, the electrolyte membrane 23 is bonded to the upper surface of the electrode catalyst layer 251 of the cathode 25. Next, the frame 21 is bonded to the upper surface of the electrolyte membrane 23 via an adhesive layer 213. Next, the electrode catalyst layer 241 of the anode 24 is bonded to the upper surface of the electrolyte membrane 23 through the opening 210 of the frame 21, and the outer edge of the electrode catalyst layer 241 is laminated on the upper surface of the inner edge portion 222 of the frame 21. This forms a laminate 2A before adhesive is applied. The frame 21 is made of PPS (polyphenylene sulfide).
[0044] Next, an adhesive is applied to seal the gaps between the inner edge 222 of the frame 21, the electrolyte membrane 23, and the cathode 25, and between the inner edge 222 of the frame 21 and the anode 24 (application process). More specifically, as shown in FIG. 5B , the stack 2A obtained in the lamination process is placed on a stage 400. Then, an ultraviolet-curable adhesive is applied using a dispenser 401 to the intersection of one surface of the inner edge 222 of the frame 21 (front surface 211 in FIG. 4 ) and the outer end face of the anode 24 (left end faces 241 a, 242 a in FIG. 4 ), all around the inner edge 222 (adhesive portion 40). That is, the adhesive is applied in a substantially rectangular shape along the opening 210 of the frame 21, as shown in FIG. 3 .
[0045] In this case, the adhesive is applied so as to cover at least the entire outer end surface of the electrode catalyst layer 241. In other words, the adhesive is applied so as to extend beyond the outer end surface (left end surface 241a in FIG. 4 ) of the electrode catalyst layer 241 and reach the outer end surface (left end surface 242a in FIG. 4 ) of the gas diffusion layer 242. However, the amount of adhesive applied is adjusted so that, when the adhesive hardens, the adhesive portion 40 does not extend beyond the leading edge point P2 in FIG. 4 and reach the front end surface 242b of the gas diffusion layer 242.
[0046] Similarly, a dispenser 401 is used to apply an ultraviolet-curable adhesive to the other surface of the inner edge portion 222 of the frame 21 (rear surface 212 in FIG. 4 ) at the intersection with the outer end surfaces of the electrolyte membrane 23 and the cathode electrode 25 (left end surfaces 23 a, 251 a, 252 a in FIG. 4 ). The adhesive is applied so as to cover at least the entire outer end surfaces of the electrolyte membrane 23 and the electrode catalyst layer 251. In other words, the adhesive is applied so as to extend beyond the outer end surface of the electrode catalyst layer 251 (left end surface 251 a in FIG. 4 ) and reach the outer end surface of the gas diffusion layer 252 (left end surface 252 a in FIG. 4 ). However, the amount of adhesive applied is adjusted so that, when the adhesive hardens, the adhesive portion 40 does not extend beyond the trailing edge point P3 in FIG. 4 and reach the rear end surface 252 b of the gas diffusion layer 252.
[0047] Next, as shown in Fig. 5C, ultraviolet rays are irradiated from an ultraviolet irradiating unit 402 onto the adhesive portion 40 of the laminate 2A to which the adhesive has been applied in the application step, thereby curing the adhesive portion 40 (curing step). The hatched area AR10 in Fig. 5C is the irradiation range of ultraviolet rays irradiated from the ultraviolet irradiating unit 402, and this irradiation range includes the entire adhesive portion 40. This allows the entire adhesive portion 40 to be cured at once, resulting in high work efficiency.
[0048] Because the frame 21 is made of PPS, which has a relatively high thermal shrinkage rate, the illuminance and integrated light amount of the ultraviolet light are set during the curing process so as to prevent deformation such as warping or undulation of the frame 21 due to thermal shrinkage. Figure 6 is a diagram showing the relationship between the integrated light amount J of the ultraviolet light and the temperature (frame temperature) T of the frame 21. Characteristic f1 (solid line) is the characteristic obtained under a first illuminance W1 (e.g., 230 mW / cm2), and characteristic f2 (dotted line) is the characteristic obtained under a second illuminance W2 (e.g., 450 mW / cm2) that is higher than the first illuminance W1.
[0049] As is clear from characteristics f1 and f2, the lower the illuminance and the smaller the integrated light amount J, which is the integrated value of illuminance and time, the lower the temperature T of the frame 21. If the temperature at which the frame 21 begins to soften (softening temperature) or the temperature obtained by adding a predetermined margin to the softening temperature is defined as the predetermined temperature Ta, in this embodiment, the illuminance W and the integrated light amount J are set so that the temperature of the frame 21 during the hardening process is equal to or lower than the predetermined temperature Ta. This makes it possible to suppress deformation of the frame 21. The predetermined temperature Ta is, for example, 60°C. If the temperature of the adhesive is low, it takes a long time for the adhesive to harden. Therefore, considering work efficiency, it is preferable that the temperature of the frame 21 be equal to or higher than the predetermined temperature (for example, 40°C) and equal to or lower than the predetermined temperature Ta.
[0050] The ultraviolet irradiation unit 402 is integrally provided with the conveyor 403. In the curing process, as shown in FIG. 5C , a nitrogen-filled space SP10 (inert gas) is formed above the conveyor 403. The stage 400 is then moved into this space SP10, and the adhesive is cured by irradiating it with ultraviolet light in the nitrogen atmosphere. That is, the ultraviolet-curable adhesive is cured under a nitrogen purge. This reduces the oxygen concentration in the space SP10, making it easy to reduce the integrated light intensity J. As a result, the temperature of the frame 21 during the curing process can be limited to a predetermined temperature Ta or lower while suppressing a decrease in ultraviolet irradiance. Therefore, the adhesive can be cured in a short time while suppressing deformation of the frame 21, thereby improving work efficiency.
[0051] Furthermore, when ultraviolet light is irradiated under nitrogen purging, the energy at which a substance adheres to the surface of the adhesive portion 40 (surface adhesion energy) can be reduced compared to when ultraviolet light is irradiated under conditions other than nitrogen purging. Surface adhesion energy corresponds to viscosity, and if the surface adhesion energy of the adhesive portion 40 is high, water is likely to remain on the surface of the adhesive portion 40, which may impair power generation stability. In contrast, by irradiating ultraviolet light under nitrogen purging to reduce the surface adhesion energy of the adhesive portion 40, water does not remain on the surface of the adhesive portion 40, and power generation stability can be ensured.
[0052] The present embodiment provides the following advantageous effects. (1) The integrated electrode assembly 2 as a membrane electrode structure for a fuel cell includes a membrane electrode assembly 20 formed by stacking, in the front-rear direction, an electrolyte membrane 23, an anode electrode 24 disposed along a front surface 231 of the electrolyte membrane 23, and a cathode electrode 25 disposed along a rear surface 232 of the electrolyte membrane 23, and a frame 21 extending in the up-down and left-right directions and having an inner edge 222 that forms an opening 210 in which the membrane electrode assembly 20 is disposed ( FIGS. 2 and 3 ). The anode electrode 24 includes a gas diffusion layer 242 to which fuel gas is supplied and an electrode catalyst layer 241 disposed between the electrolyte membrane 23 and the gas diffusion layer 242, and the cathode electrode 25 includes a gas diffusion layer 252 to which oxidant gas is supplied and an electrode catalyst layer 251 disposed between the electrolyte membrane 23 and the gas diffusion layer 252 ( FIG. 2 ). The integrated electrode assembly 2 further includes a front adhesive portion 41 made of an adhesive and arranged to seal the gap between the front surface 211 of the inner edge portion 222 of the frame 21 and the outer end surface (left end surface 242 a) of the gas diffusion layer 242, and a rear adhesive portion 42 made of an adhesive and arranged to seal the gap between the rear surface 212 of the inner edge portion 222 of the frame 21 and the outer end surface (left end surface 252 a) of the gas diffusion layer 252 ( FIG. 4 ).
[0053] With this configuration, the outer end surfaces of the electrolyte membrane 23 and the electrode catalyst layers 241, 251 are covered by the front adhesive portion 41 and the rear adhesive portion 42 without being exposed to the flow paths PAa, PAc. As a result, not only the electrolyte membrane 23 but also the electrode catalyst layers 241, 251, which could serve as a path for moisture, are blocked from the flow paths PAa, PAc, preventing moisture containing iron ions eluted from the separator 3 from reaching the electrolyte membrane 23 via the electrode catalyst layers 241, 251. As a result, deterioration of the electrolyte membrane 23 is suppressed, and a longer lifespan of the electrolyte membrane 23 can be achieved. Furthermore, because the adhesive portion 40 is not exposed to the flow paths PAa, PAc, the quality of the adhesion at the adhesive portion 40 can be easily confirmed from the outside.
[0054] (2) The adhesives constituting the front adhesive portion 41 and the rear adhesive portion 42 are both ultraviolet-curing adhesives. The frame 21 is made of polyphenylene sulfide (PPS). By using PPS, which has high hydrolysis resistance, the frame 21 can have a long lifespan. Furthermore, by using an ultraviolet-curing adhesive, the temperature of the frame 21 can be easily kept below a predetermined temperature Ta when the adhesive cures. As a result, deformation of PPS, which has a high thermal shrinkage rate, can be suppressed, ensuring sufficient sealing performance at the connection between the frame 21 and the separator 3.
[0055] (3) The front adhesive portion 41 is provided from the front surface 211 to the left end surface 242a of the frame 21 within a range not exceeding a leading edge point P2 of the outer end surface (left end surface 242a) of the gas diffusion layer 242, and the rear adhesive portion 42 is provided from the rear surface 212 to the left end surface 252a of the frame 21 within a range not exceeding a trailing edge point P3 of the outer end surface (left end surface 252a) of the gas diffusion layer 252 ( FIG. 4 ). If the adhesive portion 40 exceeds the leading edge point P2 of the gas diffusion layer 242 or the trailing edge point P3 of the gas diffusion layer 252, the end surface of the separator 3 and the end surfaces 242b, 252b of the gas diffusion layers 242, 252 will not be in uniform contact with each other, which may result in variations in the stacking state of the cell stack 101. In response to this, by limiting the thickness of the adhesive portion 40 in the front-to-rear direction so that it does not exceed the leading edge point P2 or the trailing edge point P3, it is possible to suppress variations in the stacking state of the cell stack 101.
[0056] (4) In a method for manufacturing a membrane electrode structure for a fuel cell as a manufacturing method for manufacturing the above-described integrated electrode assembly 2, the gas diffusion layer 252, the electrode catalyst layer 241, the gas diffusion layer 242 included in the anode electrode 24 are arranged on the front surface 211 side of the inner edge portion 222 of the frame 21, and the electrolyte membrane 23, and the electrode catalyst layer 251 and the gas diffusion layer 252 included in the cathode electrode 25 are arranged on the rear surface 212 side of the inner edge portion 222 of the frame 21. The method includes a lamination step of sequentially laminating the electrode catalyst layer 241, the electrode catalyst layer 242, and the gas diffusion layer 242; a coating step of applying adhesive to seal the gap between the front surface 211 of the inner edge portion 222 of the frame 21 and the outer end surface (left end surface 242a) of the gas diffusion layer 242, and also to seal the gap between the rear surface 212 of the inner edge portion 222 of the frame 21 and the outer end surface (left end surface 252a) of the gas diffusion layer 252; and a curing step of curing the adhesive of the adhesive portion 40 applied in the coating step (FIGS. 5A to 5C). This prevents moisture containing iron ions, which can cause deterioration of the electrolyte membrane 23, from reaching the electrolyte membrane 23. Furthermore, the adhesive strength of the adhesive portion 40 can be easily confirmed from the outside.
[0057] (5) The frame 21 is made of polyphenylene sulfide. The curing process includes curing the adhesive at a predetermined temperature Ta or lower, which corresponds to the softening temperature of the frame 21 (FIG. 6). This allows the frame 21 to have a long life while suppressing deformation of the frame 21.
[0058] (6) The adhesive applied in the application step is an ultraviolet-curable adhesive. The curing step involves irradiating the adhesive portion 40 with ultraviolet light so that the temperature of the frame 21 is equal to or lower than a predetermined temperature Ta ( FIG. 5C ). This makes it easy to prevent deformation of the frame 21 when the adhesive is cured.
[0059] (7) The curing step includes curing the adhesive at the adhesive joint 40 under a nitrogen atmosphere ( FIG. 5C ). This shortens the time required for the adhesive to harden, thereby improving the work efficiency when manufacturing the integrated electrode assembly 2. In addition, the surface adhesion energy of the adhesive joint 40 is reduced, ensuring stable power generation.
[0060] The above embodiment can be modified in various ways. Some modifications will be described below. In the above embodiment, the anode 24 is disposed as a first gas diffusion electrode layer along the front surface 231 (one surface) of the electrolyte membrane 23, and the cathode 25 is disposed as a second gas diffusion electrode layer along the rear surface 232 (the other surface). More specifically, the anode 24, which has a gas diffusion layer 242 (first gas diffusion layer) and an electrode catalyst layer 241 (first electrode catalyst layer) to which a fuel gas (first reactant gas) is supplied, and the cathode 25, which has a gas diffusion layer 252 (second gas diffusion layer) and an electrode catalyst layer 251 (second electrode catalyst layer) to which an oxidant gas (second reactant gas) is supplied, are disposed on both sides of the electrolyte membrane 23. However, the configuration of the membrane electrode assembly 20 is not limited to this.
[0061] In the above embodiment, the frame 21 extends in a left-right direction (second direction) perpendicular to the front-rear direction (first direction), which is the stacking direction of the membrane electrode assemblies 20. However, the extending direction of the frame member is not limited to the above. In the above embodiment, the front adhesive portion 41 (first sealing portion) is provided to seal the gap between the front surface 211 (first surface) of the inner edge portion 222 of the frame 21 and the left end surface 242 a (first side end surface) of the gas diffusion layer 242, and the rear adhesive portion 42 (second sealing portion) is provided to seal the gap between the rear surface 212 (second surface) of the inner edge portion 222 of the frame 21 and the left end surface 252 a (second side end surface) of the gas diffusion layer 252. More specifically, the front adhesive portion 41 is provided within a range not exceeding a front edge point P2 (outer edge), which is a corner on the front side (one side in the first direction) of the left end face 242a, and the rear adhesive portion 42 is provided within a range not exceeding a rear edge point P3 (outer edge), which is a corner on the rear side (the other side in the first direction) of the left end face 252a. In this case, an ultraviolet-curable adhesive such as olefin resin is used, but other ultraviolet-curable adhesives can also be used.
[0062] In the above embodiment, as the curing process, a space SP10 with a nitrogen atmosphere is formed below the ultraviolet irradiation section 402, and ultraviolet rays are irradiated onto the entire adhesive section 40 in the nitrogen atmosphere, but the configuration of the device that performs the curing process is not limited to this.
[0063] In the above embodiment, an example of applying the fuel cell stack 100 to a vehicle has been described, but a fuel cell stack having a fuel cell membrane electrode structure of the present invention can also be applied to moving bodies other than vehicles, such as aircraft and ships, robots, and various industrial machines.
[0064] The above description is merely an example, and the present invention is not limited to the above-described embodiment and modifications as long as the features of the present invention are not impaired. One or more of the above-described embodiment and modifications can be arbitrarily combined, and modifications can also be combined with each other.
[0065] 1 Power generation cell, 2 Integrated electrode assembly, 21 Frame, 23 Electrolyte membrane, 23a Left end surface, 24 Anode electrode, 25 Cathode electrode, 40 Adhesive portion, 41 Front adhesive portion, 42 Rear adhesive portion, 100 Fuel cell stack, 210 Opening, 211 Front surface, 212 Rear surface, 222 Inner edge portion, 241, 251 Electrode catalyst layer, 241a, 251a Left end surface, 242, 252 Gas diffusion layer, 252a Left end surface, P2 Leading edge point, P3 Trailing edge point, PAa Anode flow path, PAc Cathode flow path
Claims
1. A membrane electrode assembly for a fuel cell comprising: a membrane electrode assembly constructed by stacking in a first direction an electrolyte membrane, a first gas diffusion electrode layer disposed along one side of the electrolyte membrane, and a second gas diffusion electrode layer disposed along the other side of the electrolyte membrane; and a frame member extending in a second direction perpendicular to the first direction and having an inner edge portion forming an opening in which the membrane electrode assembly is disposed, wherein the first gas diffusion electrode layer comprises a first gas diffusion layer to which a first reactant gas is supplied, and a first electrode catalyst layer disposed between the electrolyte membrane and the first gas diffusion layer, and the second gas diffusion electrode layer comprises a second gas diffusion layer to which a second reactant gas is supplied, and a second electrode catalyst layer disposed between the electrolyte membrane and the second gas diffusion layer, and the membrane electrode assembly for a fuel cell comprises: a first sealing portion made of an adhesive and provided to seal between a first surface which is a surface on one side in the first direction of the inner edge portion of the frame member and a first side end face which is an end face in the second direction of the first gas diffusion layer, a second sealing portion, the second sealing portion being made of an adhesive and provided to seal between a second surface, which is the surface on the other side in the first direction of the inner edge portion of the frame member, and a second side end face, which is the end face in the second direction of the second gas diffusion layer.
2. A membrane electrode structure for a fuel cell as described in claim 1, characterized in that the adhesive of the first sealing portion and the adhesive of the second sealing portion are each an ultraviolet curing adhesive, and the frame member is made of polyphenylene sulfide as a constituent material.
3. A membrane electrode structure for a fuel cell as described in claim 1 or 2, characterized in that the first sealing portion is provided from the first surface to the first side end face within a range not exceeding the outer edge of one side of the first direction of the first side end face, and the second sealing portion is provided from the second surface to the second side end face within a range not exceeding the outer edge of the other side of the second side end face in the first direction.
4. A method for producing a membrane electrode assembly for a fuel cell, comprising: a membrane electrode assembly constructed by stacking, in a first direction, an electrolyte membrane, a first gas diffusion electrode layer disposed along one side of the electrolyte membrane, and a second gas diffusion electrode layer disposed along the other side of the electrolyte membrane; and a frame member extending in a second direction perpendicular to the first direction and having an inner edge portion forming an opening in which the membrane electrode assembly is disposed, the method comprising the steps of: stacking the second gas diffusion layer, the second electrode catalyst layer, the electrolyte membrane, the inner edge portion of the frame member, the first electrode catalyst layer, and the first gas diffusion layer in order such that the first electrode catalyst layer and the first gas diffusion layer contained in the first gas diffusion electrode layer are disposed on one side of the inner edge portion of the frame member in the first direction, and the electrolyte membrane and the second electrode catalyst layer and the second gas diffusion layer contained in the second gas diffusion electrode layer are disposed on the other side of the inner edge portion of the frame member in the first direction; a coating step of coating an adhesive so as to seal between a first surface, which is a surface on one side in the first direction of the inner edge portion of the frame member, and a first side end face, which is an end face in the second direction of the first gas diffusion layer, and also coating an adhesive so as to seal between a second surface, which is a surface on the other side in the first direction of the inner edge portion of the frame member, and a second side end face, which is an end face in the second direction of the second gas diffusion layer; and a curing step of curing the adhesive applied in the coating step.
5. A method for manufacturing a membrane electrode structure for a fuel cell as described in claim 4, characterized in that the frame member is made of polyphenylene sulfide as a constituent material, and the hardening process includes hardening the adhesive at a predetermined temperature or lower corresponding to the softening temperature of the frame member.
6. A method for manufacturing a membrane electrode structure for a fuel cell as described in claim 5, wherein the adhesive applied in the application process is an ultraviolet-curing adhesive, and the curing process includes irradiating the adhesive with ultraviolet light so that the temperature of the frame member becomes equal to or lower than the predetermined temperature.
7. A method for producing a membrane electrode assembly for a fuel cell according to any one of claims 4 to 6, characterized in that the curing step includes curing the adhesive under a nitrogen atmosphere.
Citation Information
Patent Citations
Fuel cell frame
JP1979161516U
Method for manufacturing membrane electrode gas diffusion layer assembly sheet
JP2020087669A
Fuel cell
JP2020198199A
MEA with resin frame and manufacturing method thereof
JP2022151538A
Cited By
Frame-mounted membrane electrode structure and method for manufacturing the same
JP2026160420A
Frame-mounted membrane electrode structure and method for manufacturing the same
JP7949091B2