Charging roll for electrophotographic apparatuses

The charging roll for electrophotographic equipment, featuring a specific composition of rubber and fluororesin layers, addresses the challenge of balancing charging performance and substance generation, achieving effective and environmentally friendly charging while maintaining image quality.

WO2024203189A1PCT designated stage expired Publication Date: 2024-10-03SUMITOMO RIKO CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/009201
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-29
Filing Date
2024-03-09
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Charging rolls for electrophotographic equipment face challenges in achieving optimal charging performance without generating harmful substances like ozone and NOx, which leads to environmental and image deterioration, either due to insufficient charging or excessive discharge.

Method used

A charging roll configuration with an elastic layer containing non-polar rubber, polar rubber, and carbon black, and a surface layer made of fluororesin and (meth)acrylic resin, optimized to reduce discharge while maintaining effective charge transfer and image quality, by controlling dielectric constants and resistance values within specific ranges.

Benefits of technology

This configuration reduces harmful substance generation, ensures efficient charging performance even with reduced discharge, and enhances the durability and uniformity of the charging roll, preventing image deterioration and environmental impact.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JPOXMLDOC01-APPB-T000001
    Figure JPOXMLDOC01-APPB-T000001
  • Figure JPOXMLDOC01-APPB-T000002
    Figure JPOXMLDOC01-APPB-T000002
  • Figure 00000029_0000
    Figure 00000029_0000
Patent Text Reader

Abstract

Provided is a charging roll for electrophotographic apparatuses, which has excellent electrification properties even with a small electric discharge amount. A charging roll 10 for electrophotographic apparatuses comprises: a shaft body 12; an elastic body layer 14 formed on the outer circumferential surface of the shaft body 12; and a surface layer 16 formed on the outer circumferential surface of the elastic body layer 14. The elastic body layer 14 contains a non-polar rubber, a polar rubber, and carbon black, and has a relative dielectric constant of 7-29 and a resistance value of 6.0×104-5.0×106 Ω. The surface layer 16 contains a fluorine resin and a (meth)acrylic resin, and has a relative dielectric constant of 10-22 and a resistance value of 1.2×104-8.8×105 Ω.
Need to check novelty before this filing date? Find Prior Art

Description

Charging rolls for electrophotographic equipment

[0001] The present invention relates to a charging roll for electrophotographic equipment, which is suitably used in electrophotographic equipment such as copying machines, printers, and facsimiles that employ an electrophotographic system.

[0002] A known configuration of a charging roll for an electrophotographic device includes a shaft formed of a core metal or the like, an elastic layer formed on the outer circumferential surface of the shaft, and a surface layer formed on the outer circumferential surface of the elastic layer. The elastic layer is made of a rubber material such as isoprene rubber, and the surface layer is made of a resin material such as acrylic resin.

[0003] Japanese Patent Application Laid-Open No. 2003-140442

[0004] The charging rolls of electrophotographic devices often employ a charging system that charges the photoconductor by discharging electricity from the charging roll to the photoconductor, but if the amount of discharge is increased in order to sufficiently charge the photoconductor, harmful substances such as ozone and NOx are generated in large amounts, which may cause environmental degradation and image degradation.On the other hand, if the amount of discharge is too small, the amount of charge is insufficient, which may cause image degradation.

[0005] The problem to be solved by the present invention is to provide a charging roll for electrophotographic equipment which has excellent charging properties even when the amount of discharge is small.

[0006] The charging roll for an electrophotographic device according to the present invention comprises a shaft, an elastic layer formed on the outer peripheral surface of the shaft, and a surface layer formed on the outer peripheral surface of the elastic layer, wherein the elastic layer contains a non-polar rubber, a polar rubber, and carbon black, and has a relative dielectric constant of 7 or more and 29 or less, and a resistance value of 6.0×10 4 Ω or more 5.0×10 6 Ω or less, and the surface layer contains a fluororesin and a (meth)acrylic resin, has a relative dielectric constant of 10 or more and 22 or less, and a resistance value of 1.2 × 10 4 Ω or more 8.8×10 5 It is less than Ω.

[0007] The area ratio of the non-polar rubber to the polar rubber on the surface of the elastic layer may be non-polar rubber:polar rubber = 9:1 to 7:3. The non-polar rubber may be isoprene rubber or natural rubber, and the polar rubber may be nitrile rubber or hydrin rubber. The carbon black may have an average particle diameter of 36 nm to 80 nm, and a product of DBP absorption and specific surface area of ​​1728 to 5445. The carbon black content may be 15 parts by mass to 50 parts by mass per 100 parts by mass of the non-polar rubber and the polar rubber combined. The elastic layer may be composed of a composition that does not contain an ion conductive agent. The content ratio of the fluororesin to the (meth)acrylic resin may be fluororesin:(meth)acrylic resin = 9.5:0.5 to 7:3 by mass. The fluororesin may have a relative dielectric constant of 8 to 10 and a volume resistivity of 1.0 x 10 13 Ω・cm or more 1.0×10 14 The resistance may be Ω·cm or less. The fluororesin may be polyvinylidene fluoride. The difference in volume resistivity between the fluororesin and the (meth)acrylic resin may be 0.2 log Ω or less. The fluororesin may have an indentation Young's modulus of 0.65 GPa to 0.75 GPa and an elastic recovery of 40% to 50%, and the (meth)acrylic resin may have an indentation Young's modulus of 0.65 GPa to 0.75 GPa and an elastic recovery of 45% to 50%. The difference in indentation Young's modulus between the fluororesin and the (meth)acrylic resin may be 0.1 GPa or less and an elastic recovery of 5% or less. The tensile strength of the fluororesin may be 28 MPa to 40 MPa. The difference in relative dielectric constant between the fluororesin and the (meth)acrylic resin may be 2 or less. The surface layer may further contain roughness-forming particles. The roughness-forming particles may be porous particles.

[0008] (1) A charging roll for an electrophotographic device according to the present invention comprises a shaft, an elastic layer formed on the outer peripheral surface of the shaft, and a surface layer formed on the outer peripheral surface of the elastic layer, wherein the elastic layer contains a non-polar rubber, a polar rubber, and carbon black, and has a relative dielectric constant of 7 or more and 29 or less, and a resistance value of 6.0×10 4 Ω or more 5.0×10 6Ω or less, and the surface layer contains a fluororesin and a (meth)acrylic resin, has a relative dielectric constant of 10 or more and 22 or less, and a resistance value of 1.2 × 10 4 Ω or more 8.8×10 5 It is less than Ω.

[0009] (2) In the above (1), the area ratio of the non-polar rubber to the polar rubber on the surface of the elastic layer is preferably non-polar rubber:polar rubber=9:1 to 7:3.

[0010] (3) In the above (1) or (2), the non-polar rubber may be isoprene rubber or natural rubber, and the polar rubber may be nitrile rubber or hydrin rubber.

[0011] (4) In any one of (1) to (3) above, the carbon black may have an average particle size of 36 nm or more and 80 nm or less, and a product of DBP absorption and specific surface area of ​​1728 or more and 5445 or less.

[0012] (5) In any one of (1) to (4) above, the content of the carbon black may be 15 parts by mass or more and 50 parts by mass or less per 100 parts by mass of the total of the non-polar rubber and the polar rubber.

[0013] (6) In any one of the above (1) to (5), the elastic layer may be made of a composition that does not contain an ion conductive agent.

[0014] (7) In any one of (1) to (6) above, the content ratio of the fluororesin to the (meth)acrylic resin may be, in mass ratio, fluororesin:(meth)acrylic resin=9.5:0.5 to 7:3.

[0015] (8) In any one of the above (1) to (7), the fluororesin has a relative dielectric constant of 8 to 10 and a volume resistivity of 1.0 × 10 13 Ω・cm or more 1.0×10 14 It is preferable that the resistivity is Ω·cm or less.

[0016] (9) In any one of the above (1) to (8), the fluororesin may be polyvinylidene fluoride.

[0017] (10) In any one of (1) to (9) above, the difference in volume resistivity between the fluororesin and the (meth)acrylic resin may be 0.2 log Ω or less.

[0018] (11) In any one of (1) to (10) above, the fluororesin may have an indentation Young's modulus of 0.65 GPa or more and 0.75 GPa or less and an elastic recovery rate of 40% or more and 50% or less, and the (meth)acrylic resin may have an indentation Young's modulus of 0.65 GPa or more and 0.75 GPa or less and an elastic recovery rate of 45% or more and 50% or less.

[0019] (12) In any one of (1) to (11) above, the difference in indentation Young's modulus between the fluororesin and the (meth)acrylic resin may be 0.1 GPa or less, and the difference in elastic recovery may be 5% or less.

[0020] (13) In any one of (1) to (12) above, the fluororesin may have a tensile strength of 28 MPa or more and 40 MPa or less.

[0021] (14) In any one of (1) to (13) above, the difference in relative dielectric constant between the fluororesin and the (meth)acrylic resin may be 2 or less.

[0022] (15) In any one of the above (1) to (14), the surface layer may further contain particles for providing roughness.

[0023] (16) In the above (15), the roughness-imparting particles may be porous particles.

[0024] In the charging roll for electrophotographic equipment according to the present invention, the elastic layer contains non-polar rubber, polar rubber, and carbon black, and has a relative dielectric constant of 7 or more and 29 or less, and a resistance value of 6.0×10 4 Ω or more 5.0×10 6 Ω or less, the surface layer contains a fluororesin and a (meth)acrylic resin, the relative dielectric constant is 10 or more and 22 or less, and the resistance is 1.2 × 10 4 Ω or more 8.8×10 5Since the resistance is Ω or less, the amount of discharge from the charging roll to the photosensitive member is reduced, suppressing the generation of harmful substances such as ozone and NOx, thereby preventing environmental degradation and image deterioration. Furthermore, the above-mentioned configuration facilitates charge transfer at the grounded portion of the charging roll and the photosensitive member, and the photosensitive member can be charged to the desired charge amount by injecting charge from the charging roll into the photosensitive member. This results in excellent charging performance even with a small amount of discharge.

[0025] Here, when the area ratio of the non-polar rubber to the polar rubber on the surface of the elastic layer is non-polar rubber:polar rubber=9:1 to 7:3, the relative dielectric constant of the elastic layer is easily within a specific range.

[0026] When the non-polar rubber is isoprene rubber or natural rubber and the polar rubber is nitrile rubber or hydrin rubber, the relative dielectric constant of the elastic layer is easily kept within a specific range.

[0027] When the carbon black has an average particle size of 36 nm or more and 80 nm or less and a product of DBP absorption and specific surface area of ​​1728 or more and 5445 or less, it is easy to make the carbon black have a desired dielectric constant, thereby making the relative dielectric constant of the elastic layer fall within a specific range.

[0028] When the content of the carbon black is 15 parts by mass or more and 50 parts by mass or less relative to 100 parts by mass of the total of the non-polar rubber and the polar rubber, the resistance value and relative dielectric constant of the elastic layer are easily kept within a specific range.

[0029] When the elastic layer is made of a composition that does not contain an ionic conductive agent, the relative dielectric constant of the elastic layer does not increase too much, and it is easy to keep the relative dielectric constant of the elastic layer within a specific range.

[0030] When the content ratio of the fluororesin to the (meth)acrylic resin is fluororesin:(meth)acrylic resin=9.5:0.5 to 7:3 by mass, the relative dielectric constant of the surface layer is easily kept within a specific range.

[0031] The fluororesin has a relative dielectric constant of 8 to 10 and a volume resistivity of 1.0×10 13 Ω・cm or more 1.0×10 14When the resistivity is Ω·cm or less, the fluororesin has a relatively high dielectric constant and low resistance, so that the surface layer can be easily made to have a high dielectric constant and low resistance, and the electrostatic chargeability effect of the fluororesin can also be easily maintained.

[0032] When the fluororesin is polyvinylidene fluoride, it has a relatively high dielectric constant and low resistance, so that the surface layer can be easily made to have a high dielectric constant and low resistance, and the electrostatic property of the fluororesin can be easily maintained.

[0033] When the difference in volume resistivity between the fluororesin and the (meth)acrylic resin is 0.2 log Ω or less, the unevenness of charge injection from the charging roll to the photosensitive member is reduced.

[0034] Furthermore, when the fluororesin has an indentation Young's modulus of 0.65 GPa or more and 0.75 GPa or less and an elastic recovery rate of 40% or more and 50% or less, and the (meth)acrylic resin has an indentation Young's modulus of 0.65 GPa or more and 0.75 GPa or less and an elastic recovery rate of 45% or more and 50% or less, deformation of the charging roll in response to the pressure received from the photosensitive member during rotation becomes uniform, and local stress concentration is less likely to occur.

[0035] When the difference in indentation Young's modulus between the fluororesin and the (meth)acrylic resin is 0.1 GPa or less and the difference in elastic recovery rate is 5% or less, cracking of the surface layer due to physical stress from the photoreceptor is easily suppressed, thereby improving durability.

[0036] When the tensile strength of the fluororesin is 28 MPa or more and 40 MPa or less, the strength of the surface layer is improved, and the durability is improved.

[0037] When the difference in relative permittivity between the fluororesin and the (meth)acrylic resin is 2 or less, unevenness in discharge from the charging roll to the photosensitive member is reduced.

[0038] Furthermore, if the surface layer further contains roughness-forming particles, a suitable discharge space can be formed between the photoreceptor and the charging roll. In this case, if the roughness-forming particles are porous particles, the binder resin in the surface layer and the roughness-forming particles are more closely integrated, making the surface layer less likely to crack. In addition, the resistance can be integrated, making the injected charge uniform.

[0039] 1A is a schematic view of the appearance of a charging roll for an electrophotographic apparatus according to one embodiment of the present invention, and FIG. 1B is a cross-sectional view taken along line AA thereof.

[0040] The charging roll for electrophotographic equipment (hereinafter, sometimes simply referred to as the charging roll) according to the present invention will be described in detail. Fig. 1 is a schematic diagram of the appearance of the charging roll for electrophotographic equipment according to one embodiment of the present invention (a) and a cross-sectional view of the same taken along line A-A (b).

[0041] The charge roll 10 includes a shaft 12, an elastic layer 14 formed on the outer peripheral surface of the shaft 12, and a surface layer 16 formed on the outer peripheral surface of the elastic layer 14. The elastic layer 14 is a layer (base layer) that forms the base of the charge roll 10. The surface layer 16 is a layer that appears on the surface of the charge roll 10.

[0042] The shaft 12 is not particularly limited as long as it is electrically conductive. Specific examples include a solid or hollow core made of metal such as iron, stainless steel, or aluminum. The surface of the shaft 12 may be coated with an adhesive, primer, or the like, as needed. That is, the elastic layer 14 may be bonded to the shaft 12 via an adhesive layer (primer layer). The adhesive, primer, or the like may be made electrically conductive as needed.

[0043] The elastic layer 14 contains non-polar rubber, polar rubber, and carbon black, and has a relative dielectric constant of 7 or more and 29 or less, and a resistance value of 6.0×10 4 Ω or more 5.0×10 6 It is less than Ω.

[0044] Examples of non-polar rubbers for the elastic layer 14 include isoprene rubber (IR), hydrogenated isoprene rubber, natural rubber (NR), butadiene rubber (BR), styrene-butadiene rubber (SBR), butyl rubber (IIR), ethylene-propylene rubber (EPM), ethylene-propylene-diene terpolymer rubber (EPDM), and silicone rubber (Q). These may be used alone or in combination of two or more as the non-polar rubber for the elastic layer 14. Of these, isoprene rubber and natural rubber are preferred from the viewpoints of high resistance and excellent effect as a dielectric phase.

[0045] Examples of polar rubbers for the elastic layer 14 include nitrile rubber (NBR), hydrin rubber, urethane rubber (U), acrylic rubber (a copolymer of acrylic acid ester and 2-chloroethyl vinyl ether, ACM), and chloroprene rubber (CR). Examples of hydrin rubbers include epichlorohydrin homopolymer (CO), epichlorohydrin-ethylene oxide binary copolymer (ECO), epichlorohydrin-allyl glycidyl ether binary copolymer (GCO), and epichlorohydrin-ethylene oxide-allyl glycidyl ether terpolymer (GECO). These may be used alone as the polar rubber for the elastic layer 14, or two or more types may be used in combination. Of these, nitrile rubber (NBR) and hydrin rubber are preferred from the viewpoints of lower resistance and higher dielectric constant.

[0046] As a combination of non-polar rubber and polar rubber, it is preferable that the non-polar rubber is isoprene rubber or natural rubber and the polar rubber is nitrile rubber or hydrin rubber, from the viewpoint of making it easier to keep the relative dielectric constant of the elastic layer 14 within a specific range.

[0047] The content ratio of the non-polar rubber to the polar rubber depends on the mixing method, but from the viewpoint of making it easier to set the area ratio of the non-polar rubber to the polar rubber within a specific range on the surface of the elastic layer 14, the mass ratio of the non-polar rubber to the polar rubber is preferably 8:2 to 6:4, and more preferably 8:2 to 7:3.

[0048] The area ratio of the non-polar rubber to the polar rubber on the surface of the elastic layer 14 is preferably non-polar rubber:polar rubber=9:1 to 7:3. This makes it easier to keep the relative dielectric constant of the elastic layer 14 within a specific range. From this perspective, the area ratio is more preferably non-polar rubber:polar rubber=9:1 to 8:2.

[0049] The carbon black in the elastic layer 14 contributes to adjusting the resistance and dielectric constant of the elastic layer 14. From the viewpoint of easily keeping the resistance and dielectric constant of the elastic layer 14 within a specific range, the carbon black in the elastic layer 14 preferably has an average particle diameter of 36 nm to 80 nm and a product of DBP absorption (oil absorption) and specific surface area of ​​1728 to 5445. The product of DBP absorption and specific surface area is related to the amount of functional groups, such as carbonyl groups and hydroxyl groups, in the carbon black, and is therefore related to the resistance and dielectric constant of the carbon black. The average particle diameter of the carbon black is expressed as the arithmetic mean diameter determined by observing the carbon black with an electron microscope. The DBP absorption of the carbon black is calculated from the amount of DBP (dibutyl phthalate) absorbed by 100 g of carbon black in accordance with JIS K6221. The specific surface area of ​​the carbon black is a value measured by the BET method.

[0050] The carbon black in the elastic layer 14 has a good balance between the resistance value and the relative dielectric constant, and the DBP absorption amount is set to 69 cm 3 / 100g or more 121cm 3 The carbon black in the elastic layer 14 has a good contact area with the rubber, and therefore has a high tolerance for variations in the amount of addition, making it easy to control the target resistance value and dielectric constant. 2 / g or more 58m 2 / g or less is preferred.

[0051] In the elastic layer 14, the content of carbon black is preferably 15 to 50 parts by mass, more preferably 20 to 45 parts by mass, and even more preferably 25 to 40 parts by mass, per 100 parts by mass of the total of the non-polar rubber and the polar rubber, from the viewpoint of making it easier to keep the resistance value and the relative dielectric constant of the elastic layer 14 within a specific range, more preferably 20 to 45 parts by mass, and even more preferably 25 to 40 parts by mass.

[0052] The elastic layer 14 is preferably made of a composition that does not contain an ionic conductive agent. When the elastic layer 14 is made of a composition that does not contain an ionic conductive agent, the relative dielectric constant of the elastic layer 14 does not increase too much, and it is easy to keep the relative dielectric constant of the elastic layer 14 within a specific range.

[0053] If necessary, various additives may be added appropriately to the elastic layer 14. Examples of the additives include a lubricant, a vulcanization accelerator, an antioxidant, a light stabilizer, a viscosity modifier, a processing aid, a flame retardant, a plasticizer, a foaming agent, a filler, a dispersant, an antifoaming agent, a pigment, and a mold release agent.

[0054] The thickness of the elastic layer 14 is not particularly limited, and may be set appropriately within the range of 0.1 to 10 mm depending on the application.

[0055] The surface layer 16 contains a fluororesin and a (meth)acrylic resin, has a relative dielectric constant of 10 or more and 22 or less, and a resistance value of 1.2×10 4 Ω or more 8.8×10 5 It is less than Ω.

[0056] The fluororesin preferably has a relatively high dielectric constant and low resistance. The relative dielectric constant of the fluororesin is preferably 8 or more and 10 or less. The volume resistivity of the fluororesin is preferably 1.0×10 13 Ω・cm or more 1.0×10 14 When the dielectric constant and volume resistivity of the fluororesin are within the above ranges, the fluororesin has a relatively high dielectric constant and low resistance, making it easy to achieve a high dielectric constant and low resistance for the surface layer 16. In this case, the electrostatic chargeability effect of the fluororesin can also be easily maintained.

[0057] The fluororesin is preferably polyvinylidene fluoride. Since polyvinylidene fluoride has a relatively high dielectric constant and low resistance, it is easy to make the surface layer high in dielectric constant and low in resistance. In this case, the electrostatic chargeability effect of the fluororesin can be easily maintained.

[0058] Here, if the relative permittivity of the fluororesin is set to be greater than the above range, the relative permittivity of the surface layer 16 can be set to a desired value even when the fluororesin is used alone. However, in order to set the relative permittivity of the fluororesin to be greater than the above range, the fluororesin needs to be modified. Because the effect of using the fluororesin is reduced by modification, it is difficult to set the relative permittivity of the surface layer 16 to a desired value when the fluororesin is used alone. Therefore, in order to set the relative permittivity of the surface layer 16 to a desired value, a (meth)acrylic resin is used together with the fluororesin. Note that if the resin component of the surface layer 16 is a (meth)acrylic resin alone, the relative permittivity is too high, making it difficult to set the relative permittivity of the surface layer 16 to a desired value.

[0059] The (meth)acrylic resin is a resin selected from an acrylic resin and a methacrylic resin. Examples of the (meth)acrylic resin include a (meth)acrylate polymer (homopolymer or copolymer). The (meth)acrylate may be either monofunctional or polyfunctional.

[0060] Examples of monofunctional (meth)acrylates include alkyl (meth)acrylates such as methyl (meth)acrylate, ethyl (meth)acrylate, propyl (meth)acrylate, butyl (meth)acrylate, isoamyl (meth)acrylate, 2-ethylhexyl (meth)acrylate, lauryl (meth)acrylate, and stearyl (meth)acrylate; cycloalkyl (meth)acrylates such as cyclohexyl (meth)acrylate; 2-hydroxyethyl (meth)acrylate, 2-hydroxypropyl (meth)acrylate, and 3-chloro-2-hydroxypropyl (meth)acrylate. alkoxyalkyl (meth)acrylates such as methoxyethyl (meth)acrylate, ethoxyethyl (meth)acrylate, and butoxyethyl (meth)acrylate; phenoxyalkyl (meth)acrylates such as phenoxyethyl acrylate and nonylphenoxyethyl (meth)acrylate; and alkoxyalkylene glycol (meth)acrylates such as ethoxydiethylene glycol (meth)acrylate, methoxytriethylene glycol (meth)acrylate, and methoxydipropylene glycol (meth)acrylate.

[0061] Examples of polyfunctional (meth)acrylates include alkyl diol di(meth)acrylates such as 1,9-nonanediol di(meth)acrylate, polyethylene glycol di(meth)acrylates such as diethylene glycol di(meth)acrylate, polypropylene glycol di(meth)acrylates such as dipropylene glycol di(meth)acrylate, trimethylolpropane tri(meth)acrylate, pentaerythritol tri(meth)acrylate, pentaerythritol tetra(meth)acrylate, glycerol tri(meth)acrylate, and polyvalent (meth)acrylates obtained by addition reaction of ethylene glycol diglycidyl ether with a compound having an ethylenically unsaturated bond and active hydrogen, such as an unsaturated carboxylic acid or an unsaturated alcohol, polyvalent (meth)acrylates obtained by addition reaction of an unsaturated epoxy compound such as glycidyl (meth)acrylate with a compound having active hydrogen, such as a carboxylic acid or an amine, polyvalent (meth)acrylamides such as methylenebis(meth)acrylamide, and polyvalent vinyl compounds such as divinylbenzene.

[0062] The (meth)acrylic resin is more preferably a methacrylic resin from the viewpoints of the relative dielectric constant, volume resistivity, indentation Young's modulus, elastic recovery rate, etc. Furthermore, the (meth)acrylic resin is more preferably an alkyl (meth)acrylate or a cycloalkyl (meth)acrylate from the viewpoints of the relative dielectric constant, volume resistivity, indentation Young's modulus, elastic recovery rate, etc.

[0063] The content ratio of the fluororesin to the (meth)acrylic resin is preferably fluororesin:(meth)acrylic resin=9.5:0.5 to 7:3 by mass, which makes it easier to keep the relative dielectric constant of the surface layer 16 within a specific range. The content ratio is more preferably fluororesin:(meth)acrylic resin=9:1 to 7:3, and even more preferably fluororesin:(meth)acrylic resin=8:2 to 7:3.

[0064] The difference in relative permittivity between the fluororesin and the (meth)acrylic resin is preferably 2 or less, thereby reducing unevenness in discharge from the charging roll 10 to the photoconductor. The difference in volume resistivity between the fluororesin and the (meth)acrylic resin is preferably 0.2 log Ω or less, thereby reducing unevenness in charge injection from the charging roll 10 to the photoconductor.

[0065] Here, it is preferable that the fluororesin have an indentation Young's modulus of 0.65 GPa or more and 0.75 GPa or less and an elastic recovery rate of 40% or more and 50% or less, and the (meth)acrylic resin have an indentation Young's modulus of 0.65 GPa or more and 0.75 GPa or less and an elastic recovery rate of 45% or more and 50% or less. This ensures uniform deformation of the charging roll 10 in response to pressure from the photoreceptor during rotation, reducing the likelihood of localized stress concentration. Furthermore, it is preferable that the difference in indentation Young's modulus between the fluororesin and the (meth)acrylic resin be 0.1 GPa or less and the difference in elastic recovery rate be 5% or less. This effectively prevents cracking of the surface layer 16 due to physical stress from the photoreceptor, improving durability. The indentation Young's modulus can be measured from a sheet sample using a microindentation hardness tester. The elastic recovery rate can be measured from a sheet sample using a tensile tester.

[0066] The fluororesin preferably has a tensile strength of 28 MPa or more and 40 MPa or less, which improves the strength and durability of the surface layer 16. The tensile strength of the fluororesin can be measured by measuring the elongation at break of a sheet sample using a tensile tester.

[0067] The surface layer 16 may contain roughness-forming particles. The roughness-forming particles are particles for imparting roughness to the surface of the surface layer 16. In other words, the roughness particles are particles for imparting irregularities to the surface of the surface layer 16. The surface irregularities of the surface layer 16 form a discharge space between the photoreceptor and the charging roll 10.

[0068] The roughness-forming particles may be resin particles, inorganic particles, or the like. The roughness-forming particles may be solid particles or porous particles. When the roughness-forming particles are porous particles, the roughness-forming particles are more closely integrated with the fluororesin or (meth)acrylic resin that is the binder resin of the surface layer 16, making the surface layer 16 less likely to crack. Furthermore, the resistance can be integrated, making it possible to uniformly inject electric charges.

[0069] Examples of materials for the roughness-forming particles include urethane resin, polyamide resin, (meth)acrylic resin, (meth)acrylic silicone resin, silicone-grafted (meth)acrylic polymer, (meth)acrylic-grafted silicone polymer, urethane rubber, silica, etc. Among these, (meth)acrylic resin is more preferred from the viewpoints of affinity with and integration with the binder resin of the surface layer 16.

[0070] The size of the roughness-forming particles is not particularly limited, but from the viewpoint of easily ensuring uniform charging properties, an average particle diameter of 3.0 μm or more and 50 μm or less is preferable. An average particle diameter of 5.0 μm or more and 30 μm or less is more preferable. The average particle diameter of the roughness-forming particles is expressed as the average of 20 arbitrary points when the surface of the surface layer 16 is observed with a laser microscope, and the diameter of the roughness-forming particles visible during surface observation is taken as the particle size.

[0071] The content of the roughness-forming particles in the surface layer 16 is not particularly limited, but from the viewpoint of easily ensuring uniform charging properties, it is preferably 3 parts by mass or more and 50 parts by mass or less, more preferably 5 parts by mass or more and 30 parts by mass or less, relative to 100 parts by mass of the binder resin in the surface layer 16.

[0072] Various additives may be added to the surface layer 16 as needed.

[0073] The thickness of the surface layer 16 is not particularly limited, and may be set in the range of 0.1 to 3.0 μm. The thickness of the surface layer 16 can be measured by observing the cross section using a laser microscope (such as Keyence's "VK-9510"). For example, the distance from the surface of the elastic layer 14 to the surface of the surface layer 16 can be measured at five arbitrary positions, and the thickness can be expressed as the average.

[0074] The charging roll 10 can be produced by forming an elastic layer 14 on the outer peripheral surface of a shaft, and then forming a surface layer 16 on the outer peripheral surface of the elastic layer 14 .

[0075] The elastic layer 14 can be formed, for example, as follows: First, the shaft 12 is placed coaxially in the hollow portion of a roll molding die, an uncrosslinked elastic layer-forming composition is injected, heated and cured (crosslinked), and then demolded, or the uncrosslinked elastic layer-forming composition is extruded onto the surface of the shaft 12 to form the elastic layer 14 on the outer periphery of the shaft.

[0076] A surface layer forming composition is used to form the surface layer 16. The surface layer forming composition contains the above-mentioned main material and other additives that may be added as needed.

[0077] The surface layer forming composition may contain an appropriate solvent, such as an organic solvent such as methyl ethyl ketone, toluene, acetone, ethyl acetate, butyl acetate, methyl isobutyl ketone (MIBK), THF, or DMF, or a water-soluble solvent such as methanol or ethanol, in order to adjust the viscosity, for example.

[0078] The surface layer 16 can be formed by a method such as coating a surface layer-forming composition onto the outer peripheral surface of the elastic layer 14. As the coating method, various coating methods such as roll coating, dipping, and spray coating can be applied. The coated surface layer 16 may be subjected to ultraviolet irradiation or heat treatment, if necessary.

[0079] In the charging roll 10 having the above configuration, the elastic layer 14 contains non-polar rubber, polar rubber, and carbon black, and has a relative dielectric constant of 7 or more and 29 or less, and a resistance value of 6.0×10 4Ω or more 5.0×10 6 Ω or less, the surface layer 16 contains a fluororesin and a (meth)acrylic resin, has a relative dielectric constant of 10 or more and 22 or less, and has a resistance value of 1.2 × 10 4 Ω or more 8.8×10 5 Ω or less. As a result, the amount of discharge from the charging roll 10 to the photosensitive member is reduced, suppressing the generation of harmful substances such as ozone and NOx, thereby preventing environmental degradation and image deterioration. Furthermore, the above-mentioned configuration facilitates charge transfer between the charging roll 10 and the grounded portion of the photosensitive member, and by injecting charge from the charging roll 10 into the photosensitive member, the photosensitive member can be charged to the desired charge amount. This results in excellent charging performance even with a small amount of discharge.

[0080] If the dielectric constant of the surface layer 16 or the elastic layer 14 is too high above a specific range, too much charge is accumulated, making it difficult for charge to transfer from the charging roll 10 to the photosensitive member at the contact point. On the other hand, if this dielectric constant is too low below the specific range, discharge from the charging roll 10 to the photosensitive member increases, resulting in the generation of large amounts of harmful substances such as ozone and NOx. Furthermore, if the resistance value of the surface layer 16 or the elastic layer 14 is too high above the specific range, it makes it difficult for charge to transfer from the charging roll 10 to the photosensitive member at the contact point. On the other hand, if this resistance value is too low below the specific range, discharge from the charging roll 10 to the photosensitive member increases, resulting in the generation of large amounts of harmful substances such as ozone and NOx.

[0081] From the above viewpoint, the relative dielectric constant of the elastic layer 14 is more preferably 10 or more, more preferably 15 or more, and is also 25 or less, more preferably 20 or less. The resistance value of the elastic layer 14 is more preferably 8.0×10 4 Ω or more, 1.0×10 5 Ω or more. Also, 1.0 × 10 6 Ω or less, 5.0×10 5 Ω or less. Similarly, the relative dielectric constant of the surface layer 16 is more preferably 12 or more, more preferably 14 or more, and 20 or less, more preferably 18 or less. The resistance value of the surface layer 16 is more preferably 2.0×10 4 Ω or more, 5.0×10 4 Ω or more. 5 Ω or less, 5.0×10 5It is less than Ω.

[0082] To achieve the dielectric constant and resistivity of the elastic layer 14 within the above ranges, it is recommended to use a non-polar rubber as a base and a small amount of polar rubber, and to select the carbon black accordingly. A suitable combination of non-polar rubber and polar rubber can be selected from those listed above. Because non-polar rubber and polar rubber have low compatibility, the surface area ratio is important for the content ratio. By setting the area ratio within the above specific range, it is easy to achieve the dielectric constant of the elastic layer 14 within the specific range. The average particle size and the product of DBP absorption and specific surface area are important factors for carbon black, and it is particularly recommended to select an appropriate value for the product of DBP absorption and specific surface area, which serves as an indicator of the dielectric constant of carbon black.

[0083] To achieve the dielectric constant and resistivity of the surface layer 16 within the above ranges, it is recommended to select a fluororesin with a relatively high dielectric constant and low resistance as a base, and to use a small amount of (meth)acrylic resin, which has a higher dielectric constant than the fluororesin. The fluororesin preferably has the above-specified dielectric constant and volume resistivity. By setting the content ratio of the fluororesin and the (meth)acrylic resin within the above-specified range, it is easy to achieve the dielectric constant of the surface layer 16 within the specified range. By selecting a fluororesin and a (meth)acrylic resin with similar indentation Young's modulus and elastic recovery rate, cracking of the surface layer 16 due to physical stress from the photoreceptor is suppressed, improving durability.

[0084] The present invention will be described in detail below using examples and comparative examples.

[0085] (Examples 1 to 7, Comparative Examples 1 to 10) <Preparation of composition for forming elastic layer> A polar rubber, a non-polar rubber, and carbon black were blended in the blending ratios (parts by mass) shown in the table, and a peroxide crosslinking agent, a vulcanization aid, and a catalyst were also blended. These were then stirred and mixed using a stirrer to prepare a composition for forming an elastic layer.

[0086] <Preparation of elastic layer> A core metal (diameter 8 mm) was set in a molding die (pipe-shaped), and the composition for forming the elastic layer was poured into it. After heating at 180°C for 30 minutes, the die was cooled and demolded, and an elastic layer having a thickness of 1.9 mm was molded around the outer periphery of the core metal.

[0087] <Preparation of Composition for Forming Surface Layer> A fluororesin, a (meth)acrylic resin, carbon black, and particles for forming roughness were blended in the blending ratios (parts by mass) shown in the table, diluted with methyl ethyl ketone (MEK), and mixed and stirred at a predetermined stirring speed to prepare a composition for forming a surface layer.

[0088] <Preparation of Surface Layer> While continuing to stir the surface layer-forming composition, the composition was roll-coated on the outer periphery of the elastic layer and subjected to heat treatment to form a surface layer having a thickness of 1.0 μm on the outer periphery of the elastic layer, thereby preparing a charging roll.

[0089] The following materials were prepared as materials for the elastic layer-forming composition. (Polar rubbers) Polar rubber <1> (NBR): "Nipol 1041" manufactured by Nippon Zeon Polar rubber <2> (ECO): "Hydrin H1100" manufactured by Nippon Zeon Polar rubber <3> (CR): "Denka Chloroprene DCR-107" manufactured by Denka (Non-polar rubbers) Non-polar rubber <1> (IR): "Nipol IR2200" manufactured by Nippon Zeon Non-polar rubber <2> (NR): "GW540N" manufactured by Maxell Kureha Non-polar rubber <3> (BR): "UBEPOL BR130B" manufactured by UBE Elastomers (Carbon black) Carbon black <1>: "Mitsubishi Carbon Black #25" manufactured by Mitsubishi Chemical, average particle size 47 nm, oil absorption (DBP absorption) 69 cm 3 / 100g, specific surface area 55m 2 / g Carbon black <2>: Mitsubishi Chemical "Mitsubishi Carbon Black #20", average particle size 50 nm, oil absorption (DBP absorption) 121 cm 3 / 100g, specific surface area 45m 2 / g Carbon black <3>: Tokai Carbon "TOKABLACK#7270SB", average particle size 36 nm, oil absorption (DBP absorption) 62 cm 3 / 100g, specific surface area 58m 2 / g Carbon black <4>: "Diablack G" manufactured by Mitsubishi Chemical, average particle size 80 nm, oil absorption (DBP absorption) 84 cm 3 / 100g, specific surface area 28m 2 / g Carbon black <5>: "HTC#SSRF" manufactured by Nippon Steel Carbon, average particle size 68 nm, oil absorption (DBP absorption) 72 cm3 / 100g, specific surface area 24m 2 / g Carbon black <6>: Asahi #70L manufactured by Asahi Carbon, average particle size 25 nm, oil absorption (DBP absorption) 85 cm 3 / 100g, specific surface area 75m 2 / g

[0090] The following materials were prepared as the surface layer forming composition: (Fluororesin) Fluororesin <1> (PVDF): "Kynar 711" manufactured by Arkema, volume resistivity 1.0×10 14 Ω cm, relative dielectric constant 8, indentation Young's modulus 0.65 GPa, elastic recovery rate 40% Fluorocarbon resin <2> (PVDF): Arkema "Kynar HSV900", volume resistivity 1.0 x 10 13 Ω cm, relative dielectric constant 10, indentation Young's modulus 0.75 GPa, elastic recovery rate 50% Fluororesin <3> (PTFE + PFA): Daikin Industries "Neoflon PFA AP-230AS", volume resistivity 1.4 x 10 13 Ω cm, relative dielectric constant 8.2, indentation Young's modulus 0.71 GPa, elastic recovery rate 48% Fluorine resin <4> (PVDF): Kureha "KF Polymer #1000", volume resistivity 2.1 x 10 14 Ω cm, relative dielectric constant 7.6, indentation Young's modulus 0.72 GPa, elastic recovery 40% ((meth)acrylic resin) - (meth)acrylic resin <1> (PMMA): "DIANAL BR107" manufactured by Mitsubishi Chemical, relative dielectric constant 10, indentation Young's modulus 0.65 GPa, elastic recovery 50% - (meth)acrylic resin <2> (PMMA): "ACRYPET IRH50001" manufactured by Mitsubishi Chemical, relative dielectric constant 11, indentation Young's modulus 0.75 GPa, elastic recovery 40% (carbon black) - Carbon black: "9027BLACK" manufactured by Tokushiki (particle for forming roughness) - Particle for forming roughness <1> (PMMA): "TECHPOLYMER MBP-8" manufactured by Sekisui Chemical, average particle size 8 μm, porous particle Roughness forming particles <2> (PMMA): "Chemisnow MZ-8HN" manufactured by Soken Chemical & Engineering, average particle size 8 μm, solid particles

[0091] (Method of preparing samples) Resin (fluororesin or acrylic resin) was added to a mixed solvent of acetone and water (9:1) to a concentration of 5 wt %, dissolved by stirring with a blade for 24 hours, cast in an environment of 28°C x 60% RH, and then baked at 100°C for 30 minutes to prepare measurement samples (sheet-shaped) made of each resin.

[0092] (Method for Measuring Physical Properties of Samples) (Volume Resistivity) The volume resistivity of the obtained sheet-like sample was measured in accordance with JIS K7194 using a resistance meter RM3545 manufactured by HIOKI and a four-point probe RM9010-01 manufactured by HIOKI.

[0093] (Dielectric Constant) The obtained sheet sample was measured in accordance with JIS C2138 by applying 10 kHz using a Precision LCR Meter E4980A (manufactured by Agilent Technologies).

[0094] (Indentation Young's Modulus) The indentation Young's modulus of the obtained sheet sample was measured based on the nanoindentation method using an ultra-microindentation hardness tester (nanoindentation tester: ENT-1100a manufactured by Elionik Co., Ltd.).

[0095] (Elastic Recovery Rate) The elastic recovery rate of the obtained sheet-like sample was measured in accordance with JIS K6251 using a tensile tester (AE-F Strograph manufactured by Toyo Seiki Seisakusho, Ltd.).

[0096] (Tensile Strength) The elongation at break of the obtained sheet-like sample was measured in accordance with JIS K6251 using a tensile tester (AE-F Strograph manufactured by Toyo Seiki Seisakusho, Ltd.).

[0097] (Relative dielectric constant of elastic layer) The elastic layer before the formation of the surface layer was cut into a sample piece of 1 cm × 1 cm × 0.3 cm, and the obtained sheet-like sample was measured in accordance with JIS C2138 by applying 10 kHz using a precision LCR meter E4980A (manufactured by Agilent Technologies).

[0098] (Dielectric Constant of Surface Layer) A measurement sample (sheet-shaped) made of the surface layer-forming composition was prepared by casting the surface layer-forming composition in an environment of 28°C x 60% RH and then baking it at 100°C for 30 minutes. The obtained sheet-shaped sample was measured by applying 10 kHz using a precision LCR meter E4980A (manufactured by Agilent Technologies) in accordance with JIS C2138.

[0099] (Resistance Value of Elastic Layer) The elastic layer before the formation of the surface layer was cut into a sample piece of 1 cm × 1 cm × 0.3 cm, and the resistance value of the obtained sheet-like sample was measured in accordance with JIS K7194 using a HIOKI resistance meter RM3545 and a HIOKI four-point probe RM9010-01.

[0100] (Resistance Value of Surface Layer) A measurement sample (sheet-shaped) made of the surface layer-forming composition was prepared by casting the surface layer-forming composition in an environment of 28°C x 60% RH and then baking it for 30 minutes at 100°C. The resistance value of the obtained sheet-shaped sample was measured in accordance with JIS K7194 using a HIOKI resistance meter RM3545 and a HIOKI four-point probe RM9010-01.

[0101] (Rubber Surface Existence Area Ratio) The elastic layer before the surface layer was formed was cut into a sample piece of 11 cm × 1 cm × 0.3 cm, stained by Os staining, and then observed under a scanning electron microscope at a magnification of 2000. The areas occupied by the rubber were measured, as dark and light colored areas indicated the presence of rubber.

[0102] (Evaluation / Judgment Method) The produced charging roll was attached to a unit (black) of an actual machine ("IM C8000" manufactured by RICOH), and images were output at 25% density halftone in an environment of 10°C x 10% RH, and evaluation was performed after 1 million sheets were printed.

[0103] (Black and white dots): Charging property (amount of discharge) Images with no white or black dots were rated as very good (◎), images with a few dots but with a low density and within the acceptable range were rated as good (○), and images with many dots and a high density were rated as unacceptable (×).

[0104] (Fogging): Charging property (charge amount) Images with no fogging were rated as very good (◎), images with a few spots of fogging but with a low density and within the acceptable range were rated as good (○), and images with many spots of fogging and with a high density were rated as unacceptable (×).

[0105] (Unevenness): Stain resistance: Images with no unevenness were rated as very good "◎", images with slight unevenness but within the acceptable range were rated as good "◯", and images with strong unevenness were rated as unacceptable "×".

[0106] (Cracks): Durability: A roll with no cracks on the surface was rated as very good (⊚), and a roll with a few cracks that did not affect the image was rated as good (◯).

[0107]

[0108]

[0109] In Comparative Example 1, the area ratio of the polar rubber on the surface of the elastic layer is too small, and the relative dielectric constant of the elastic layer is too low. As a result, the amount of discharge is too high, resulting in image deterioration due to black and white dots. In Comparative Example 3, the area ratio of the polar rubber on the surface of the elastic layer is too large, and the relative dielectric constant of the elastic layer is too high. As a result, charging is insufficient, resulting in image deterioration due to fogging. In Comparative Example 2, the carbon black content of the elastic layer is low, and the resistance value of the elastic layer is too high. As a result, charging is insufficient, resulting in image deterioration due to fogging. In Comparative Example 4, the carbon black content of the elastic layer is high, and the resistance value of the elastic layer is too low. As a result, charging is too high, resulting in image deterioration due to black and white dots.

[0110] In Comparative Example 5, the content of fluororesin in the surface layer is too high, resulting in a low dielectric constant for the surface layer. This results in an excessive amount of discharge, causing image degradation due to black and white dots. In Comparative Example 7, the content of fluororesin in the surface layer is too low, resulting in a high dielectric constant for the surface layer. This results in insufficient charging, causing image degradation due to fogging. In Comparative Example 6, the content of carbon black in the surface layer is too low, resulting in a high resistance value for the surface layer. This results in insufficient charging, causing image degradation due to fogging. In Comparative Example 8, the content of carbon black in the surface layer is too high, resulting in a low resistance value for the surface layer. This results in an excessive amount of discharge, causing image degradation due to black and white dots.

[0111] In Comparative Example 9, the product of the oil absorption amount and the specific surface area of ​​the carbon black in the elastic layer is large, and the relative dielectric constant of the elastic layer is too large. As a result, insufficient charging occurs, resulting in image deterioration due to fog. In addition, the resistance value of the elastic layer is too small. As a result, the amount of discharge becomes too large, resulting in image deterioration due to black and white dots. In Comparative Example 10, the relative dielectric constant of the fluororesin in the surface layer is small at 7.6, which is too small. As a result, the amount of discharge becomes too large, resulting in image deterioration due to black and white dots. In addition, the volume resistivity is 2.1 x 10 14 The surface layer has a high resistance of Ω·cm, which causes insufficient charging and leads to image deterioration due to fogging.

[0112] In contrast, in the example, the elastic layer contains non-polar rubber, polar rubber, and carbon black, and has a relative dielectric constant of 7 or more and 29 or less, and a resistance value of 6.0 × 10 4 Ω or more 5.0×10 6 Ω or less, the surface layer contains a fluororesin and a (meth)acrylic resin, the relative dielectric constant is 10 or more and 22 or less, and the resistance is 1.2 × 10 4 Ω or more 8.8×10 5 Ω or less. This reduces the amount of discharge, preventing image degradation due to black and white dots. Furthermore, the above configuration facilitates charge transfer, resulting in excellent charging performance even with a reduced amount of discharge. This also prevents image degradation due to fogging caused by insufficient charging.

[0113] Although the embodiments and examples of the present invention have been described above, the present invention is not limited to the above embodiments and examples, and various modifications are possible within the scope of the invention.

[0114] 10 charging roll 12 shaft body 14 elastic layer 16 surface layer

Claims

1. A coil comprising a shaft body, an elastic layer formed on the outer peripheral surface of the shaft body, and a surface layer formed on the outer peripheral surface of the elastic layer, wherein the elastic layer contains non-polar rubber, polar rubber, and carbon black, and has a relative dielectric constant of 7 to 29 and a resistance value of 6.0 x 10 4 Ω or more 5.0×10 6 The surface layer contains a fluororesin and a (meth)acrylic resin, has a relative dielectric constant of 10 to 22, and has a resistance of 1.2×10 4 Ω or more 8.8×10 5 Ω or less for electrophotographic equipment.

2. The charging roll for electrophotographic equipment according to claim 1, wherein the area ratio of said non-polar rubber to said polar rubber on the surface of said elastic layer is non-polar rubber:polar rubber=9:1 to 7:

3.

3. The charging roll for an electrophotographic device according to claim 1 or 2, wherein the non-polar rubber is isoprene rubber or natural rubber, and the polar rubber is nitrile rubber or hydrin rubber.

4. The charging roll for an electrophotographic device according to any one of claims 1 to 3, wherein the carbon black has an average particle size of 36 nm or more and 80 nm or less, and a product of DBP absorption amount and specific surface area of ​​1,728 or more and 5,445 or less.

5. A charging roll for an electrophotographic device according to any one of claims 1 to 4, wherein the content of the carbon black is 15 parts by mass or more and 50 parts by mass or less per 100 parts by mass of the total of the non-polar rubber and the polar rubber.

6. The charging roll for electrophotographic equipment according to any one of claims 1 to 5, wherein the elastic layer is made of a composition that does not contain an ion conductive agent.

7. The charging roll for electrophotographic equipment according to any one of claims 1 to 6, wherein a content ratio of the fluororesin to the (meth)acrylic resin, in terms of mass ratio, is fluororesin:(meth)acrylic resin=9.5:0.5 to 7:

3.

8. The fluororesin has a relative dielectric constant of 8 to 10 and a volume resistivity of 1.0 x 10 13 Ω・cm or more 1.0×10 14 The charging roll for an electrophotographic apparatus according to claim 1 , wherein the surface roughness is Ω·cm or less.

9. The charging roll for an electrophotographic device according to any one of claims 1 to 8, wherein the fluororesin is polyvinylidene fluoride.

10. The charging roll for electrophotographic equipment according to any one of claims 1 to 9, wherein the difference in volume resistivity between the fluororesin and the (meth)acrylic resin is 0.2 log Ω or less.

11. A charging roll for electrophotographic equipment according to any one of claims 1 to 10, wherein the fluororesin has an indentation Young's modulus of 0.65 GPa or more and 0.75 GPa or less and an elastic recovery rate of 40% or more and 50% or less, and the (meth)acrylic resin has an indentation Young's modulus of 0.65 GPa or more and 0.75 GPa or less and an elastic recovery rate of 45% or more and 50% or less.

12. The charging roll for electrophotographic equipment according to any one of claims 1 to 11, wherein the difference in indentation Young's modulus between said fluororesin and said (meth)acrylic resin is 0.1 GPa or less, and the difference in elastic recovery rate between said fluororesin and said (meth)acrylic resin is 5% or less.

13. The charging roll for electrophotographic equipment according to any one of claims 1 to 12, wherein the tensile strength of the fluororesin is 28 MPa or more and 40 MPa or less.

14. The charging roll for electrophotographic equipment according to any one of claims 1 to 13, wherein the difference in relative dielectric constant between the fluororesin and the (meth)acrylic resin is 2 or less.

15. The charging roll for an electrophotographic device according to any one of claims 1 to 14, wherein the surface layer further contains particles for providing roughness.

16. The charge roll for an electrophotographic device according to claim 15, wherein said roughness-forming particles are porous particles.

Citation Information

Patent Citations

  • Charging member and charging device

    JP2003140442A

  • Charging roll and method of producing the same

    JP2010266844A

  • Conductive member for electrophotographic apparatus

    JP2012047871A