Resin molded body and method for manufacturing same
Patent Information
- Application Number
- PCT/JP2024/010282
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-31
- Filing Date
- 2024-03-15
- Publication Date
- 2024-10-03
Smart Images

Figure 000001 
Figure 000002 
Figure 000003
Abstract
Description
Resin molded body and its manufacturing method
[0001] The present invention relates to a resin molded article and a method for producing the same.
[0002] Conventionally, thermosetting resins have generally been used as matrix resins for composite materials. However, due to issues such as storage stability, toughness, and working environment, the use of thermoplastic resins as matrix resins has been considered in recent years. Among thermoplastic resins, for example, polyphenylene ether resins have excellent physical properties such as heat resistance, mechanical strength, electrical properties, dimensional stability, and water resistance, but have a high melt viscosity. Therefore, polyphenylene ether resins have the disadvantage of lower fluidity during molding compared to resins with lower melt viscosity, and polyphenylene ether resins have poor moldability. Furthermore, the impregnation of inorganic fibers with thermoplastic resins is greatly affected by the arrangement of the inorganic fibers when impregnating them with the thermoplastic resin.
[0003] In order to overcome the above drawbacks, for example, Patent Document 1 discloses a manufacturing method in which glass fibers are kneaded into a polyphenylene ether resin, and specifies that the ratio of the fiber length to the diameter of the glass fibers to be kneaded be within a predetermined range. However, Patent Document 1 assumes that the glass fibers contained in the resin after kneading are extremely short in length, and only short fibers are used, and is not a manufacturing method for a resin molded product that assumes the use of long fibers or continuous fibers.
[0004] Patent Document 2 discloses a molding material in which polyphenylene ether is attached and integrated to a group of unidirectionally oriented reinforcing fibers, and a crystalline thermoplastic resin is further attached and integrated to cover the polyphenylene ether. However, Patent Document 2 is premised on the use of a crystalline thermoplastic resin in addition to the polyphenylene ether resin, and the molding material of Patent Document 2 is not a polyphenylene ether resin alone integrated with a group of reinforcing fibers.
[0005] Patent Document 3 discloses a reinforcing fiber substrate used in a composite material formed by impregnating a laminated reinforcing fiber substrate with a matrix resin. However, Patent Document 3 only discloses a reinforcing fiber substrate in the form of a woven fabric, and uses a polyethersulfone resin in combination with an epoxy resin, which is a thermosetting resin, and does not disclose a reinforcing fiber substrate using, as a main component, a polyphenylene ether resin, which has a higher melt viscosity than polyethersulfone resin.
[0006] Japanese Patent Laid-Open No. 06-122771 Japanese Patent Laid-Open No. 2006-8939 Japanese Patent Laid-Open No. 2005-213469
[0007] As in Patent Document 2, it is known that, in order to improve the moldability of polyphenylene ether resins, a resin other than polyphenylene ether resin is alloyed with the polyphenylene ether resin to enhance the moldability. However, because a resin having lower heat resistance than the polyphenylene ether resin is alloyed with the polyphenylene ether resin, there is a problem in that when molding is performed using the alloyed resin, the heat resistance of the resulting resin molded body is reduced. On the other hand, it is difficult to impregnate a thermoplastic resin with a high melt viscosity between fibers (especially between long fibers) without modifying it by converting it into a polymer alloy, and even when molding is performed using the polyphenylene ether resin alone, the physical properties of the resulting resin molded body are poor.
[0008] The present invention has been made to solve the above-mentioned problems, and aims to obtain a resin molded article having excellent physical properties by improving the impregnation of inorganic fibers with a thermoplastic resin, even though the resin molded article uses, as a main component, a polyphenylene ether resin, which is a thermoplastic resin with a high melt viscosity.
[0009] As a result of intensive research to solve the above problems, the present inventors have found that even when a polyphenylene ether resin, which is a thermoplastic resin with a high melt viscosity, is used as a main component, by laminating a plurality of inorganic fiber layers with a thermoplastic resin interposed between the inorganic fiber layers, the impregnation of the thermoplastic resin into the inorganic fibers can be improved, and a resin molded product with excellent physical properties can be obtained.
[0010] That is, the present invention has the following features. [1] A resin molded product in which a plurality of inorganic fiber layers are laminated via a thermoplastic resin, wherein the content of polyphenylene ether resin in the thermoplastic resin is 90% by mass or more. [2] The resin molded product according to [1], wherein the volume content of the inorganic fibers is 30 to 85% by volume. [3] The resin molded product according to [1] or [2], wherein the resin molded product is used for electrical and electronic devices, building materials, or automobiles. [4] A method for producing a resin molded product containing inorganic fibers and a thermoplastic resin, comprising: a first step of alternately laminating inorganic fiber layers and a thermoplastic resin film to obtain a laminate; and a second step of heating the laminate to melt the thermoplastic resin and then press-molding the laminate, wherein the content of polyphenylene ether resin in the thermoplastic resin is 90% by mass or more. [5] The method for producing a resin molded product according to [4], wherein the thermoplastic resin film has an average thickness of 30 μm to 250 μm. [6] The method for producing a resin molded body according to [4] or [5], wherein the volume content of the inorganic fibers in the resin molded body is 30 to 85 volume %. [7] The method for producing a resin molded body according to any one of [4] to [6], wherein further cooling is performed after the press molding, and the melting, press molding, and cooling are performed under a pressure of 2 MPa or more. [8] The method for producing a resin molded body according to any one of [4] to [7], wherein in the second step, the thermoplastic resin is melted at a temperature 20°C or higher than the glass transition temperature of the thermoplastic resin.
[0011] Even when a polyphenylene ether resin, which is a thermoplastic resin with a high melt viscosity, is used as the main component, by laminating multiple inorganic fiber layers with a thermoplastic resin between the inorganic fiber layers, the impregnation of the thermoplastic resin into the inorganic fibers can be improved, and a resin molded product with excellent physical properties can be obtained.
[0012] The resin molded article of the present invention has a plurality of inorganic fiber layers laminated together with a thermoplastic resin interposed therebetween, and the content of polyphenylene ether resin in the thermoplastic resin is 90 mass% or more. Although the thermoplastic resin of the present invention is mainly composed of polyphenylene ether resin, which has a very high melt viscosity among resins, the presence of the thermoplastic resin between the inorganic fiber layers can enhance the impregnation of the thermoplastic resin into the inorganic fibers, thereby producing a resin molded article with excellent physical properties.
[0013] The polyphenylene ether resin has a glass transition temperature of about 210 to 220°C and has excellent heat resistance and flame retardancy. -1 Preferably, the polyphenylene ether resin has a melt viscosity of 1000 Pa s or more at a temperature of 330° C., more preferably 1500 Pa s or more, even more preferably 2000 Pa s or more, and particularly preferably 2500 Pa s or more. The upper limit of the melt viscosity is not particularly limited, and is, for example, 6000 Pa s or less.
[0014] It is preferable that the polyphenylene ether resin accounts for 90% by mass or more of the thermoplastic resin (100% by mass), and that no thermoplastic resin other than the polyphenylene ether resin is contained, but a small amount may be contained as long as it does not impair the effects of the present invention. The proportion of thermoplastic resin other than the polyphenylene ether resin in 100% by mass of the thermoplastic resin is 10% by mass or less, preferably 5% by mass or less, more preferably 2% by mass or less, even more preferably 1% by mass or less, and particularly preferably 0% by mass.
[0015] Examples of thermoplastic resins other than polyphenylene ether resins include polyamide resins such as nylon 6, nylon 11, nylon 66, and nylon 46; polyester resins such as polyethylene terephthalate and polybutylene terephthalate; polyolefin resins such as polyethylene and polypropylene; polyether ketone resins; polyphenylene sulfide resins; polyetherimide resins; and polycarbonate resins.
[0016] The number of inorganic fiber layers is preferably 3 or more, more preferably 5 or more, and even more preferably 7 or more. There is no particular upper limit to the number of inorganic fiber layers, but if the thickness of the resin molded body is too large, the effect may be saturated or the physical properties may be reduced, so it is, for example, 100 or less.
[0017] The shape of the resin molded article of the present invention is not particularly limited, and may be, for example, a sheet, a rod, or a tube, but is preferably a sheet.
[0018] The inorganic fibers used in the present invention are not particularly limited as long as they are solid at the processing temperature of the thermoplastic resin used, and examples thereof include inorganic fibers such as carbon fibers, silicon carbide fibers, and glass fibers; and metal fibers such as boron fibers. From the viewpoint of production costs and the physical properties of the resulting resin molded product, it is preferable to contain at least one of glass fibers and carbon fibers, and it is more preferable to contain carbon fibers. Furthermore, it is preferable to use inorganic fibers that have been sufficiently opened, as sufficient opening can improve the impregnation of the thermoplastic resin into the inorganic fibers and can improve the physical properties of the resin molded product, such as the bending strength.
[0019] The volume content of inorganic fibers in the resin molded product of the present invention (hereinafter sometimes referred to as fiber volume content) is preferably 30 to 85 volume%, more preferably 35 to 60 volume%, and even more preferably 40 to 50 volume%. If it is less than 30 volume%, the reinforcing effect of the inorganic fibers on the resin molded product may not be obtained, and the physical properties of the resin molded product may be reduced. On the other hand, if it exceeds 85 volume%, not only will production efficiency be reduced, but the impregnation of the inorganic fibers with the thermoplastic resin may be insufficient, and the physical properties of the resin molded product may be reduced. The fiber volume content can be calculated by the direct ashing method in accordance with JIS K7250-1.
[0020] The inorganic fibers are preferably long fibers, and specifically, the average fiber length of the inorganic fibers is preferably 50 mm or more, more preferably 70 mm or more, even more preferably 100 mm or more, and particularly preferably 200 mm or more. The inorganic fibers may be long fibers, and the fiber length may be adjusted to the size of the mold to be used. Therefore, the upper limit of the average fiber length of the inorganic fibers is not particularly limited, but is, for example, 1500 mm or less.
[0021] The average fiber diameter of the inorganic fibers is preferably 2 to 30 μm, more preferably 3 to 20 μm, and even more preferably 5 to 15 μm. If the average fiber diameter is less than 2 μm, the reinforcing effect of the inorganic fibers on the resin molded article may be insufficient. If the average fiber diameter is more than 30 μm, the impregnation of the thermoplastic resin into the inorganic fibers may be insufficient.
[0022] The resin molded article of the present invention has multiple inorganic fiber layers, and the orientation direction of the inorganic fibers in each layer may be the same or different. However, it is preferable that the orientation direction of the inorganic fibers in each layer be substantially the same (the inorganic fibers are substantially oriented in one direction). "Substantially oriented in one direction" means that 50% by mass or more of the inorganic fibers are oriented at an angle of ±10 degrees or less. Of the inorganic fibers constituting the inorganic fiber layer, preferably 70% by mass or more of the inorganic fibers are oriented at an angle of ±10 degrees or less in a plane perpendicular to the thickness direction of the inorganic fiber layer, and more preferably 90% by mass or more of the inorganic fibers are oriented at an angle of ±10 degrees or less in a plane perpendicular to the thickness direction of the inorganic fiber layer. Note that when the inorganic fibers are laid out in one direction within a molding frame so as to form a single layer without gaps, as in the examples, naturally 50% by mass or more of the inorganic fibers are oriented at an angle of ±10 degrees or less in a plane perpendicular to the thickness direction of the inorganic fiber layer.
[0023] Since the inorganic fiber layer is impregnated with the thermoplastic resin (the thermoplastic resin is impregnated between the inorganic fibers in the inorganic fiber layer), the inorganic fiber layer contains not only inorganic fibers but also thermoplastic resin. When the fiber volume content of the resin molded body is 40%, the inorganic fibers account for approximately 20 to 60 area % and the thermoplastic resin for approximately 80 to 40 area % in the plane perpendicular to the thickness direction of the inorganic fiber layer.
[0024] The impregnation of the inorganic fiber layer with the thermoplastic resin, the orientation direction of the inorganic fibers in a plane perpendicular to the thickness direction of the inorganic fiber layer, and the proportion of inorganic fibers can be confirmed by examining a cross section perpendicular to the thickness direction of the inorganic fiber layer. Specifically, a sample is cut in the thickness direction of the inorganic fiber layer, embedded in epoxy resin, and the observation surface is polished, and then the cross section is observed using a microscope, thereby confirming the orientation direction of the inorganic fibers and the proportion of inorganic fibers contained in the cross section of the inorganic fiber layer. In addition to the above methods, the orientation direction of the inorganic fibers can also be confirmed using a method using 3D-X-ray CT, or, when inorganic fibers with high thermal conductivity are used, a method of determining the orientation direction from thermal conductivity.
[0025] Furthermore, the thermoplastic resin composition constituting the resin molded article of the present invention may contain additives such as antioxidants and ultraviolet absorbers, as necessary, for the purpose of improving physical properties, moldability, durability, etc. One type of additive may be contained, or two or more types may be contained, and the content of these additives may vary depending on the purpose, but it is preferable that the total content of the additives is 5% by mass or less relative to 100% by mass of the thermoplastic resin.
[0026] The flexural modulus of the resin molded article of the present invention is preferably 25 GPa or more, more preferably 35 GPa or more, even more preferably 50 GPa or more, and particularly preferably 70 GPa or more. The upper limit of the flexural modulus is not particularly limited, and is, for example, 250 GPa.
[0027] The flexural strength of the resin molded article of the present invention is preferably 400 MPa or more, more preferably 500 MPa or more, even more preferably 750 MPa or more, and particularly preferably 900 MPa or more. The upper limit of the flexural strength is not particularly limited, and is, for example, 2500 MPa.
[0028] The cross-sectional void ratio of the resin molded article of the present invention after a bending test is preferably 3.0% or less, and particularly preferably 2.7% or less. The lower limit of the void ratio is not particularly limited, and is, for example, 0.5%. The void ratio is calculated by the method described in the examples.
[0029] <Method for producing resin molded article> The method for producing the resin molded article of the present invention can be, for example, a film stacking method. Specifically, the method can include a first step of alternately laminating inorganic fiber layers and thermoplastic resin films to obtain a laminate, and a second step of heating the laminate to melt the thermoplastic resin and then press-molding the laminate. By using this manufacturing method, it is possible to improve the impregnation of the thermoplastic resin into the inorganic fibers, even though the thermoplastic resin has a polyphenylene ether resin content of 90 mass% or more.
[0030] The resin molded article of the present invention is preferably produced using a molding die, and the inorganic fiber layer is preferably formed by spreading inorganic fibers over the molding die. "Spreading inorganic fibers over the molding die" specifically means cutting continuous inorganic fibers to fit the size of the molding die and spreading the inorganic fibers over the entire surface of the molding die, which is perpendicular to the thickness direction, so that the inorganic fibers are oriented in substantially one direction. Therefore, the fiber length of the inorganic fibers is determined by the size of the molding die and the orientation direction of the inorganic fibers. Furthermore, since inorganic fibers in an open state are more easily impregnated with thermoplastic resins, it is preferable to use opened inorganic fibers.
[0031] Inorganic fibers drawn from multiple bobbins are spread, and the spread inorganic fibers are laid out in a molding die. Specifically, because contact between the inorganic fibers drawn out from each bobbin would cause damage, adjustments are made to prevent the inorganic fibers from coming into contact with each other using a yarn guide or the like. On the other hand, because separation of the inorganic fibers would result in areas in the molded product where the inorganic fibers are not positioned, which could result in a deterioration in the physical properties of the resin molding, adjustments are made to bring the inorganic fibers into close proximity using a yarn guide or the like. Furthermore, when laying the inorganic fibers out in the molding die, it is preferable to cut the inorganic fibers along the length of the die while applying a tensile force in the fiber direction to produce a preform.
[0032] When inorganic fiber layers and thermoplastic resin films are alternately laminated, the fiber volume content of the molded resin body can be adjusted by increasing or decreasing the thickness of the thermoplastic resin film. Specifically, the thickness of the thermoplastic resin film can be adjusted according to the volume of the inorganic fibers laid down so that the fiber volume content of the molded resin body is the desired value. With the above manufacturing method, the fiber volume content can be easily adjusted.
[0033] Furthermore, when adjusting the fiber volume content using the above-mentioned manufacturing method, the amount of substrate waste resulting from adjusting the fiber volume content can be reduced compared to other manufacturing methods. For example, when using a melt impregnation method in which inorganic fibers are impregnated with resin in a molten bath, preliminary preparations are required to adjust the resulting resin molded body to the target fiber volume content. Specifically, after starting operation of the machine, various machine components (such as the molten resin temperature, molten resin discharge pressure, and opening area of the molten bath outlet) are gradually adjusted to the desired settings. Therefore, the inorganic fibers and molten resin used until the target fiber volume content is reached are discarded. In contrast, when laminating inorganic fiber layers and thermoplastic resin films alternately, by fixing the volume of the inorganic fibers to be laid and preparing thermoplastic resin films with a predetermined thickness, a resin molded body adjusted to the target fiber volume content can be obtained immediately after the machine starts operating, thereby reducing the amount of substrate waste.
[0034] The thickness of the thermoplastic resin film is not particularly limited as long as it achieves the desired fiber volume content, but is preferably 30 μm to 250 μm on average, and more preferably 40 μm to 100 μm. By making the thickness of the thermoplastic resin film 30 μm or more, sufficient thermoplastic resin is present between the inorganic fiber layers, which can further increase the impregnation of the thermoplastic resin into the inorganic fibers and further reduce variation in impregnation.
[0035] The number of layers in the laminate (the total number of inorganic fiber layers and thermoplastic resin films) corresponds to the target thickness of the resin molded product after molding. The target thickness of the resin molded product after molding is preferably 0.5 mm to 10 mm, and more preferably 1 mm to 8 mm. That is, the thickness of the resin molded product of the present invention is preferably 0.5 mm to 10 mm, and more preferably 1 mm to 8 mm.
[0036] After lamination is complete, the upper mold of the molding die is placed on top and closed, after which the die is heated to heat the laminate. The set temperature is preferably equal to or higher than the glass transition temperature (hereinafter sometimes referred to as Tg) of the polyphenylene ether resin, more preferably Tg + 20°C to Tg + 140°C, even more preferably Tg + 30°C to Tg + 130°C, and particularly preferably Tg + 60°C to Tg + 120°C. From the viewpoint of resin impregnation, a higher temperature is preferable, but the higher the temperature, the more likely the resin is to deteriorate, so the temperature can be designed appropriately.
[0037] The laminate is preheated to a sufficient temperature to melt the thermoplastic resin, and then press-molded. Generally, the higher the pressure during melting and press-molding, the better the resin impregnation between the fibers. The pressure during melting and press-molding is 2 MPa or more, preferably 4 MPa or more, in terms of surface pressure. The upper limit of the surface pressure is not particularly limited, but is, for example, 20 MPa or less.
[0038] Finally, it is preferable to cool the laminate, and more preferably to cool the molding die while maintaining the pressure. Specifically, the pressure is preferably 2 MPa or more in terms of surface pressure, and more preferably 4 MPa or more. It is particularly preferable to perform melting, press molding, and cooling while maintaining a surface pressure of 2 MPa or more. The mold setting temperature during cooling is not particularly limited, and may be about 60°C or less, and is preferably room temperature (about 20 to 25°C). The pressure is preferably 2 MPa or more in terms of surface pressure, and more preferably 4 MPa or more. The upper limit of the surface pressure is not particularly limited, but is, for example, 20 MPa or less.
[0039] Although the above describes a method for producing a resin molded body using a film stacking method, there are no particular limitations as long as it can improve the impregnation of inorganic fibers with a thermoplastic resin, and a production method using a double belt press may also be used.
[0040] This application claims the benefit of priority based on Japanese Patent Application No. 2023-057749, filed on March 31, 2023. The entire contents of the specification of Japanese Patent Application No. 2023-057749, filed on March 31, 2023, are incorporated herein by reference.
[0041] The present invention will be described below with reference to examples, but the present invention is not limited to these examples. The evaluation methods used in each example and comparative example are as follows.
[0042] <Bending test> After cooling, the sample was removed from the molding die and cut into strips with a width of 15 mm and a length of 100 mm using a diamond cutter. The cut strip samples were subjected to a bending test by bending the samples along the fiber direction to measure the bending modulus and bending strength. The measurement conditions were in accordance with the three-point bending test (method A) of JIS K 7074.
[0043] <Void Ratio> To measure the void ratio of the surface perpendicular to the thickness direction of the inorganic fiber layer of the rectangular sample after the bending test, the sample was cut in the thickness direction of the inorganic fiber layer, embedded in epoxy resin, and the observation surface was polished. The cross section was observed using a microscope and photographed. The photograph was binarized into void areas and other areas, and the void area was divided by the total area of the cross section (the total area of the void area and other areas) to calculate the void ratio.
[0044] Example 1 First, continuous carbon fibers (TR700 manufactured by Toray Industries, Inc., fineness: 800 tex, average fiber diameter: 7 μm, number of fibers f: 12,000, winding length: 7,500 m) drawn from multiple bobbins were spread. Next, the spread carbon fibers were laid in a single layer without gaps in the longitudinal direction of a 470 mm × 230 mm UD (unidirectional composite) fabrication frame. When laying the carbon fibers, a yarn guide was used to adjust the laying so that the carbon fibers did not come into contact with each other. Furthermore, to prevent slack in the laid carbon fibers, a preform was produced by laying the carbon fibers while applying a tensile force in the fiber direction. In a separate process, a film adjusted to a thickness of 70 μm was produced using a polyphenylene ether resin having a glass transition temperature of 216°C, and a polyphenylene ether film was laid on the laid carbon fibers. The polyphenylene ether resin constituting the film was subjected to a shear rate of 40 s -1The melt viscosity at 330°C is 3000 Pa s. Carbon fiber and polyphenylene ether film were alternately laminated until the thickness reached 2 mm, resulting in a 19-layer laminate with a thickness of 2 mm. The resulting laminate was fitted into a molding die together with the frame, and the polyphenylene ether film was melted and press-molded at a set temperature of 330°C, a surface pressure on the sample surface of 5 MPa, preheating for 80 minutes, and a pressure time of 15 minutes. The resin was then cooled for 30 minutes to solidify, resulting in a thermoplastic resin sheet 1 with a fiber volume content of 40%.
[0045] The thermoplastic resin sheet 1 has a flexural modulus of 73 GPa, a flexural strength of 1027 MPa, and a void count of 525 / cm 2 The void ratio was 2.5%. When the appearance of the sample was checked before the bending test, no areas where the resin impregnation was poor were visible, and the resin had sufficiently impregnated the spread inorganic fibers. Furthermore, when the cross section of the thermoplastic resin sheet 1 was checked after the bending test, no areas where the resin impregnation was poor were visible, and the impregnation state was good.
[0046] (Comparative Example 1) In the same manner as in Example 1, continuous carbon fibers (TR700 manufactured by Toray Industries, Inc., fineness: 800 tex, number of bundles f: 12,000, winding length: 7,500 m) were spread. Next, a tank filled with polyphenylene ether resin having a glass transition temperature of 216 ° C was prepared, heated to 330 ° C, and a pressure of 1.5 MPa was applied to the resin. Subsequently, the spread carbon fibers were passed through the tank, the carbon fibers were continuously impregnated with the resin, and the resin-impregnated carbon fibers were crushed with a shaping roller and cooled and solidified to produce a thermoplastic resin sheet with a fiber volume content of 40%. However, immediately after the start, a thermoplastic resin sheet could not be obtained because the gear pump that sends the molten resin from the extruder side to the melt bath storing the molten resin caused the resin piping to become clogged.
[0047] In Comparative Example 2, instead of the method of alternately laminating carbon fibers and polyphenylene ether films described in Example 1, carbon fibers and a fiberized thermoplastic resin were uniformly mixed by the following blended yarn method. Note that the same carbon fibers and polyphenylene ether resin as in Example 1 were used in Comparative Example 2.
[0048] Polyphenylene ether resin fibers were produced using polyphenylene ether resin. However, the fineness of the polyphenylene ether resin fibers was adjusted to 702 tex so that the fiber volume content of the resulting thermoplastic resin sheet would be 40%. To spin the polyphenylene ether resin fibers into two bundles of 349.5 tex (233 fibers) and 352.5 tex (235 fibers), three bobbins were placed on a creel stand, one bobbin of carbon fiber and two bobbins of polyphenylene ether resin fiber. The carbon fiber was placed in the center and sandwiched between the polyphenylene ether resin fibers on the top and bottom of the bobbin. A UD material frame was attached to a wrap reel winder, and the carbon fiber and matrix resin fiber were simultaneously wound around the UD material frame. The resulting laminate was then wound and laminated using the wrap reel winder until a thickness equivalent to 2 mm was obtained. The obtained laminate was fitted into a molding die together with the frame, and melt-molded at a set temperature of 330°C, with a surface pressure of 5 MPa on the sample surface, preheated for 80 minutes, and pressed for 15 minutes. Thereafter, the resin was cooled for 30 minutes to solidify, and a thermoplastic resin sheet 2 was obtained.
[0049] The thermoplastic resin sheet 2 has a flexural modulus of 67 GPa, a flexural strength of 687 MPa, and a void count of 1,543 / cm 2 The void ratio was 3.1%, and the bending strength was inferior to that of Example 1, with numerous voids present. When the appearance of the sample was checked before the bending test, imperfect impregnation areas with carbon fibers protruding to the surface were found. Furthermore, when the cross section of the thermoplastic resin sheet 2 after the bending test was checked, there were areas where the carbon fibers and resin portions were clearly separated, revealing the presence of numerous voids.
[0050] The resin molded article of the present invention can improve the impregnation of inorganic fibers with a thermoplastic resin and can improve physical properties. Therefore, the resin molded article of the present invention can be used in applications requiring light weight and high physical properties, such as general industries such as electrical and electronic devices and building materials, and transportation equipment such as aircraft, automobiles, ships, and bicycles. Among these, it is preferably used in electrical and electronic devices, building materials, and automobile applications, and is particularly suitable for use in automotive exterior panels such as automobile engine hoods and trunk lids, which require high surface quality.
Claims
1. A resin molded product in which multiple inorganic fiber layers are laminated via a thermoplastic resin, characterized in that the content of polyphenylene ether resin in the thermoplastic resin is 90 mass% or more.
2. The resin molded article according to claim 1, wherein the volume content of said inorganic fibers is 30 to 85 volume %.
3. The resin molding according to claim 1 or 2, which is used for electrical / electronic devices, building materials, or automotive applications.
4. A method for producing a resin molded product containing inorganic fibers and a thermoplastic resin, comprising: a first step of alternately laminating inorganic fiber layers and thermoplastic resin films to obtain a laminate; and a second step of heating the laminate to melt the thermoplastic resin and then performing press molding, wherein the content of polyphenylene ether resin in the thermoplastic resin is 90 mass% or more.
5. The method for producing a resin molded article according to claim 4, wherein the thermoplastic resin film has an average thickness of 30 μm to 250 μm.
6. The method for producing a resin molded product according to claim 4 or 5, wherein the volume content of the inorganic fibers in the resin molded product is 30 to 85 volume %.
7. A method for producing a resin molded product according to claim 4 or 5, wherein further cooling is carried out after the press molding, and the melting, press molding and cooling are carried out under a surface pressure of 2 MPa or more.
8. A method for producing a resin molded article according to claim 4 or 5, wherein in the second step, the thermoplastic resin is melted at a temperature at least 20° C. higher than the glass transition temperature of the thermoplastic resin.
Citation Information
Patent Citations
Novel laminated board and its molding method
JP1983069052A
Laminated board and its manufacture
JP1983087041A
Laminate and method of manufacturing the same
JP2010046914A