Method for manufacturing optical isolator, optical isolator, and polarizing glass

WO2024204402A1PCT designated stage expired Publication Date: 2024-10-03HOYA CORPORATION
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/012356
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-31
Filing Date
2024-03-27
Publication Date
2024-10-03

Smart Images

  • Figure JP2024012356_03102024_PF_FP_ABST
    Figure JP2024012356_03102024_PF_FP_ABST
Patent Text Reader

Abstract

Provided is a method for manufacturing an optical isolator that is extremely less susceptible to the film stress of an antireflection film although being thinner than conventional ones. A method for manufacturing an optical isolator according to one embodiment is a method for manufacturing an optical isolator comprising a Faraday rotator and a polarizing glass that is attached to the Faraday rotator, the method being characterized by comprising: a step for bonding the polarizing glass to the Faraday rotator; and a step for forming an antireflection film on the surface of the bonded polarizing glass.
Need to check novelty before this filing date? Find Prior Art

Description

Optical isolator manufacturing method, optical isolator and polarizing glass

[0001] The present invention relates to a method for manufacturing an optical isolator, an optical isolator, and polarizing glass used in an optical isolator.

[0002] Conventionally, optical isolators are used in semiconductor laser modules used in optical communications, measurement, etc. to prevent reflected light from returning to the semiconductor laser element and causing instability in laser oscillation. A typical optical isolator is constructed by placing a flat Faraday rotator between two polarizers, and these three components are housed in a cylindrical magnet. Typically, the Faraday rotator is adjusted to a thickness that rotates the polarization plane of light with a specified wavelength by 45° in a saturation magnetic field, and the two polarizers are rotated so that their respective transmission polarization directions are shifted by 45°.

[0003] Furthermore, in such optical isolators, since reflected light from the polarizer surface can cause noise and the like, a configuration in which an anti-reflection film is provided on the polarizer surface so that the reflectance for the wavelength band of light used (for example, a wavelength band of 1250 to 1650 nm when used in optical communications) is a predetermined value or less (for example, 0.3% or less) is also used (for example, Patent Document 1).

[0004] Such an optical isolator is generally manufactured by the following steps: (1) manufacturing a polarizer (polarizing glass); (2) forming an anti-reflection film on one surface of the polarizer (1); and (3) bonding the polarizer (2) to both surfaces of a Faraday rotator.

[0005] However, when an antireflection film is formed on one surface of a polarizer in this manner, the polarizer may warp due to film stress. This makes it difficult to bond the polarizer to the Faraday rotator, and there is also a risk of the polarizer peeling off (falling off) from the Faraday rotator. Furthermore, in recent years, in order to miniaturize optical isolators, even thinner polarizers (e.g., thickness: 0.1 mm or less) than conventional polarizers are required. However, when the polarizer is made thinner, the influence of the film stress of the antireflection film becomes more pronounced (i.e., the amount of warping of the polarizer increases), making the bonding process more difficult and increasing the risk of polarizer peeling off.

[0006] Fig. 3 shows the results of an experiment conducted by the inventors, showing the relationship between the thickness of the polarizing glass and the amount of warping of the polarizing glass (i.e., the effect of film stress on the anti-reflection film). In this experiment, 11 mm square polarizing glass samples of different thicknesses (thickness: 0.1 mm, 0.12 mm, 0.2 mm) were coated with Ta on one side of each sample. 2 O 5 and SiO 2 The surface roughness of each sample was measured using a measuring device (Zygo Model: Newview 8200), and the maximum height was taken as the amount of warpage.

[0007] As shown in FIG. 3, as the thickness of the polarizing glass becomes thinner, the influence of the film stress of the anti-reflection film becomes non-negligible, and it can be seen that the amount of warping increases.

[0008] In order to solve this problem, it has been proposed to form a warpage suppressing film on the other surface of the polarizer (the surface opposite to the antireflection film) to suppress warpage of the polarizer (i.e., to counteract the film stress of the antireflection film) (for example, Patent Document 2).

[0009] JP 2013-54323 JP 2020-91443

[0010] However, the configuration of Patent Document 2 has the following problems: (i) the cost increases due to the additional warp suppression film; and (ii) since there is variation (tolerance) in the thickness of the antireflection film and the thickness of the warp suppression film, it is not possible to completely eliminate the influence of film stress (i.e., warpage of the polarizer).

[0011] The present invention has been made in view of the above circumstances, and its object is to provide a method for manufacturing an optical isolator that is thinner than conventional ones and has extremely little warping of the polarizing glass, to provide an optical isolator, and to provide polarizing glass for use in such an optical isolator.

[0012] In order to achieve the above object, one embodiment of a method for manufacturing an optical isolator is a method for manufacturing an optical isolator comprising a Faraday rotator and a polarizing glass attached to the Faraday rotator, and is characterized by including the steps of bonding the polarizing glass to the Faraday rotator and forming an anti-reflection film on the surface of the bonded polarizing glass.

[0013] According to this method, the polarizing glass is bonded to the Faraday rotator before the anti-reflection coating is formed, and then the anti-reflection coating is formed on the surface of the polarizing glass (i.e., the polarizing glass is bonded to the Faraday rotator before warping occurs). This allows the polarizing glass to be firmly attached to the Faraday rotator (i.e., the risk of peeling is reduced). Furthermore, because the polarizing glass is attached with almost no warping, the anti-reflection coating functions to its maximum potential (as designed). Furthermore, because the polarizing glass is attached with almost no warping, the polarizing glass can be made extremely thin. Furthermore, because the anti-reflection coating is formed while the polarizing glass is attached to the Faraday rotator, there is no need to consider warping of the polarizing glass. This allows for the formation of thicker anti-reflection coatings than conventional methods, and the film structure and thickness of the anti-reflection coating can be freely adjusted to suit the specifications of the optical isolator.

[0014] Furthermore, it is desirable that the anti-reflection film be formed by alternately laminating low-refractive-index films having a relatively low refractive index and high-refractive-index films having a relatively high refractive index.

[0015] The anti-reflection film preferably has a thickness of 400 to 2000 nm.

[0016] The thickness of the polarizing glass is preferably 0.028 to 0.20 mm.

[0017] It is also desirable that the amount of warping of the bonded polarizing glass be 3 μm or less.

[0018] It is also preferable to further include a step of forming the anti-reflection film into a predetermined size after the anti-reflection film is formed.

[0019] The polarizing glass is preferably composed of a first polarizing glass whose polarization axis is oriented at 0° and a second polarizing glass whose polarization axis is oriented at 45°, and the step of bonding the polarizing glasses preferably involves bonding the first polarizing glass to one side of the Faraday rotator and bonding the second polarizing glass to the other side.

[0020] From another perspective, an optical isolator according to another embodiment includes a Faraday rotator and a polarizing glass laminated to the Faraday rotator, the polarizing glass having a thickness of 0.10 mm or less, and an anti-reflection film having a thickness of 650 nm or more on only the outer surface of the polarizing glass. In this case, it is desirable that the amount of warping of the polarizing glass be 3 μm or less. It is also desirable that the inner surface of the polarizing glass facing the outer surface not have a functional film for suppressing warping of the polarizing glass.

[0021] From another perspective, one embodiment of the polarizing glass is a polarizing glass for an optical isolator, one surface of which is bonded to a Faraday rotator, and is characterized in that it has a thickness of 0.028 to 0.20 mm and has an anti-reflection film of 400 to 2000 nm in thickness on the other surface, which is formed after the polarizing glass is bonded to the Faraday rotator. In this case, it is desirable that the amount of warping of the polarizing glass is 3 μm or less.

[0022] As described above, these embodiments provide a method for manufacturing an optical isolator that is thinner than conventional ones and has an extremely small amount of warpage in the polarizing glass, and realize such an optical isolator. Also, polarizing glass for use in such an optical isolator is realized.

[0023] Fig. 1 is a schematic diagram illustrating the configuration of an optical isolator according to an embodiment of the present specification. Fig. 2 is a flowchart illustrating a method for manufacturing an optical isolator according to an embodiment of the present specification. Fig. 3 is a diagram illustrating the relationship between the thickness of a conventional polarizing glass and the amount of warpage of the polarizing glass.

[0024] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, embodiments of the present invention will be described in detail with reference to the drawings. In the drawings, the same or corresponding parts are designated by the same reference numerals and their description will not be repeated.

[0025] (Configuration of Optical Isolator) FIG. 1 is a schematic diagram illustrating the configuration of an optical isolator 1 according to one embodiment, with FIG. 1(a) being a plan view and FIG. 1(b) being a side cross-sectional view. As shown in FIG. 1, the optical isolator 1 of this embodiment comprises a pair of polarizing elements 20 and 30 bonded to both sides of a Faraday rotator 10 so that their optical axes are common. The wavelength band in which the optical isolator 1 of this embodiment is used is not particularly limited, and it can be used for light in the wavelength band of 1250 to 1650 nm or wavelength bands of 1650 nm or longer. In this embodiment, the polarization axis of the polarizing element 20 and the polarization axis of the polarizing element 30 are inclined at 45° to each other. The size of the optical isolator 1 of this embodiment is not particularly limited, but is, for example, 0.4 to 0.7 mm square when viewed from the polarizing element 20 side.

[0026] The Faraday rotator 10 is an element fabricated by depositing a magneto-optical thin film (e.g., a Bi-substituted magnetic garnet film) on a non-magnetic garnet substrate by a liquid phase epitaxy (LPE), sputtering, aerosol deposition, or the like, and has a first main surface 11 and a second main surface 12 facing each other. The refractive index of the Faraday rotator 10 of this embodiment at 1550 nm is 2.34, and the thickness of the Faraday rotator 10 is 0.35 to 0.5 mm.

[0027] The pair of polarizing elements 20, 30 are optical elements attached to the first principal surface 11 and the second principal surface 12 of the Faraday rotator 10, respectively, and each comprises a polarizing glass 21, 31 and an anti-reflection film 22, 32. In this embodiment, the polarizing glass 21 is a polarizing glass whose polarization axis is in a specific first direction (0° direction), and the polarizing glass 31 is a polarizing glass whose polarization axis is in a second direction (45° direction) that forms an angle of 45° with respect to the polarization axis of the polarizing glass 21.

[0028] As shown in FIG. 1 , the polarizing glass 21, 31 of this embodiment has an appearance of a rectangular plate (e.g., 0.7 mm (horizontal) × 0.7 mm (vertical), thickness: 0.028 to 0.20 mm), and has metal layers (not shown) formed on both the front and back surfaces, in which a large number of roughly needle-shaped metal particles are oriented and dispersed in parallel, and a metal halide layer (not shown) containing metal halide particles formed between the metal layers. The metal layer is a layer of a predetermined thickness (e.g., 0.010 to 0.045 mm) formed by precipitating needle-shaped metal particles made of silver or copper through a reduction step described below. The metal halide layer is a layer of a predetermined thickness (e.g., 0.001 to 0.060 mm) formed inside the metal layer by the reduction step described below.

[0029] The anti-reflection films 22 and 32 are, for example, low refractive index films (e.g., SiO 2 : refractive index 1.46) and a high refractive index film having a relatively high refractive index (for example, Ta 2 O 5 : Refractive index 2.1, TiO 2The antireflection coating 22 and the antireflection coating 32 are alternately laminated in multiple layers, with the thickness of each layer being selected to obtain the desired reflectance distribution curve. In this embodiment, the antireflection coatings 22 and 32 have the same configuration, e.g., an eight-layer structure with a thickness of 400 to 800 nm, thereby suppressing the reflectance to 0.3% or less over a wide wavelength band of 1250 to 1650 nm. Since the antireflection coatings 22 and 32 are formed on the surfaces of the polarizing glass plates 21 and 31 after the polarizing glass plates 21 are bonded to the Faraday rotator 10 (details will be described later), no film stress is generated by the antireflection coatings 22 and 32. Therefore, the film configuration and film thickness of the antireflection coatings 22 and 32 can be appropriately changed depending on the specifications of the optical isolator 1 (e.g., the center wavelength and bandwidth of the laser light, etc.), and the film thickness can be freely set within the range of 400 to 2000 nm, for example.

[0030] (Manufacturing Method of Optical Isolator) Next, a manufacturing method of the optical isolator 1 of this embodiment will be described. FIG. 2 is a flowchart (steps 101 to 107) showing the manufacturing method of the optical isolator 1 of this embodiment. The optical isolator 1 of this embodiment is manufactured by the following procedure: 1. Prepare (manufacture) the polarizing glasses 21 and 31 (manufacturing process of the polarizing glasses 21 and 31). 2. Prepare the Faraday rotator 10, and bond the polarizing glasses 21 and 31 to the Faraday rotator 10 (bonding process). 3. Deposit anti-reflection films 22 and 32 on the surfaces of the polarizing glasses 21 and 31, respectively (film deposition process). 4. Molding to a predetermined size (molding process). Each procedure (step) will be described in detail below.

[0031] [1. Manufacturing Process of Polarizing Glasses 21, 31] The polarizing glasses 21, 31 of this embodiment are manufactured by the following procedure: (1) Prescribed glass materials containing copper or silver are blended to the desired composition, melted at approximately 1450°C, and then slowly cooled to room temperature (glass base manufacturing process). (2) Heat treatment is performed to precipitate cuprous chloride or silver chloride particles in the glass (metal halide particle precipitation process). (3) A preform having an appropriate shape (e.g., 120 x 250 x 4 mm) is manufactured by machining (preform manufacturing process). (4) The preform is heated and stretched under specified conditions to obtain a glass sheet (e.g., width: approximately 18 mm, thickness: approximately 0.5 mm) (glass stretching process). (5) The glass sheet is cut and double-sided polished to produce a double-sided polished product (e.g., 11 mm square, thickness: 0.028 to 0.20 mm) (polished product manufacturing process). (6) The polished piece is reduced in a hydrogen atmosphere (reduction step). This reduction step precipitates needle-shaped metal (copper or silver) particles, forming a metal layer (not shown) and a metal halide layer (not shown) within the polarizing glass pieces 21 and 31, resulting in the polarizing glass pieces 21 and 31 (FIG. 2: step 101). As described above, the polarizing glass piece 21 has a polarization axis in the first direction (0°), while the polarizing glass piece 31 has a polarization axis in the second direction (45°). In this embodiment, the thickness of the polarizing glass pieces 21 and 31 is set to a range of 0.028 to 0.20 mm, but this is not necessarily limited to this configuration.

[0032] [2. Bonding Step] The bonding step is a step of preparing a Faraday rotator 10 and bonding polarizing glass pieces 21 and 31 to the first and second main surfaces 11 and 12 of the Faraday rotator 10. Specifically, an organic adhesive, EPO-TEK 353ND (refractive index 1.5694 @ 589 nm) manufactured by Epoxy Technology, is applied to the first and second main surfaces 11 and 12 of the Faraday rotator 10, and the polarizing glass pieces 21 and 31 are superimposed with high positional accuracy and fixed by curing (thermal hardening) at 150°C for 1 hour ( FIG. 2 : Step 103).

[0033] [3. Film Forming Step] The film forming step is a step of forming anti-reflection films 22 and 32 on the surfaces of the bonded polarizing glass sheets 21 and 31, respectively. 2 O 5 and SiO 2 A total of eight antireflection films 22, 32 (film thickness: 400 to 800 nm) consisting of alternating layers of the above are formed by ion beam assisted deposition (hereinafter referred to as IAD) (FIG. 2: step 105). This antireflection film is designed to be compatible with a wide band in which the reflectance for light in the 1250 to 1650 nm wavelength range used in optical communications is 0.3% or less.

[0034] 4. Molding Step The molding step is a step of molding to a predetermined size. In this embodiment, the optical isolator 1 of this embodiment is obtained by cutting into pieces of, for example, 0.4 to 0.7 mm square (FIG. 2: step 107).

[0035] As described above, in the optical isolator 1 of this embodiment, the polarizing glasses 21, 31 are bonded to the Faraday rotator 10 before the antireflection films 22, 32 are formed, and then the antireflection films 22, 32 are formed on the surfaces of the polarizing glasses 21, 31. Therefore, according to the manufacturing method of this embodiment, the polarizing glasses 21, 31 are bonded and fixed to the Faraday rotator 10 in a state where they are almost (substantially) free of warping (for example, 3 μm or less), and therefore the polarizing glasses 21, 31 are firmly attached to the Faraday rotator 10 (i.e., the risk of peeling is reduced).

[0036] Furthermore, since the polarizing glasses 21 and 31 are attached in a state with almost no warping (for example, warping amount: 3 μm or less), the anti-reflection films 22 and 32 function to the maximum extent (as designed).

[0037] Furthermore, since the polarizing glasses 21 and 31 can be attached with almost no warping (for example, 3 μm or less), the polarizing glasses 21 and 31 can be made extremely thin (for example, preferably 0.028 to 0.10 mm, and more preferably 0.028 to 0.050 mm).

[0038] Furthermore, since the antireflection films 22, 32 are formed with the polarizing glasses 21, 31 attached to the Faraday rotator 10, there is no need to consider warping of the polarizing glasses 21, 31, and it is possible to form antireflection films with a thickness greater than conventional ones (for example, in the range of 400 to 2000 nm, preferably 650 to 2000 nm, and more preferably 800 to 2000 nm). Furthermore, the film structure and thickness of the antireflection films 22, 32 can be freely changed according to the specifications of the optical isolator 1.

[0039] The above is a description of the embodiment of the present invention, but the present invention is not limited to the configuration of the above embodiment, and various modifications are possible within the scope of the technical concept thereof.

[0040] For example, the optical isolator 1 of this embodiment has been described as having a pair of polarizing elements 20 and 30, but is not necessarily limited to this configuration, and may have only one of them.

[0041] In addition, in this embodiment, anti-reflection films 22, 32 are formed on the surfaces of the polarizing glasses 21, 31, but other functional films (e.g., band-pass filters) may be formed instead of or in addition to the anti-reflection films.

[0042] In addition, in this embodiment, the molding step is carried out after the film formation step, but if the Faraday rotator 10 and the polarizing glasses 21 and 31 of predetermined sizes are prepared in advance, the molding step is not necessarily required.

[0043] It should be noted that the embodiments disclosed herein are illustrative in all respects and should not be considered limiting. The scope of the present invention is defined by the claims, not by the above description, and is intended to include all modifications within the meaning and scope of the claims.

[0044] 1: Optical isolator 10: Faraday rotator 11: First main surface 12: Second main surface 20: Polarizing element 21: Polarizing glass 22: Anti-reflection film 30: Polarizing element 31: Polarizing glass 32: Anti-reflection film

Claims

1. A method for manufacturing an optical isolator comprising a Faraday rotator and a polarizing glass attached to the Faraday rotator, the method comprising the steps of: bonding the polarizing glass to the Faraday rotator; and forming an anti-reflection film on the surface of the bonded polarizing glass.

2. The method for manufacturing an optical isolator according to claim 1, wherein the step of forming the anti-reflection film comprises alternately laminating a low refractive index film having a relatively low refractive index and a high refractive index film having a relatively high refractive index.

3. The method for producing an optical isolator according to claim 1 or 2, wherein the anti-reflection film has a thickness of 400 to 2000 nm.

4. The method for producing an optical isolator according to claim 1, wherein the polarizing glass has a thickness of 0.028 to 0.20 mm.

5. The method for manufacturing an optical isolator according to claim 1, wherein the amount of warping of the bonded polarizing glass is 3 μm or less.

6. The method for producing an optical isolator according to claim 1, further comprising the step of forming said anti-reflection film into a predetermined size after said anti-reflection film is formed.

7. A method for manufacturing an optical isolator as described in claim 1, wherein the polarizing glass is composed of a first polarizing glass whose polarization axis is oriented in a direction of 0° and a second polarizing glass whose polarization axis is oriented in a direction of 45°, and the step of bonding the polarizing glass comprises bonding the first polarizing glass to one side of the Faraday rotator and bonding the second polarizing glass to the other side.

8. An optical isolator comprising a Faraday rotator and a polarizing glass bonded to the Faraday rotator, wherein the polarizing glass has a thickness of 0.10 mm or less, and an anti-reflection film having a thickness of 650 nm or more is provided only on the outer surface of the polarizing glass.

9. An optical isolator according to claim 8, wherein the amount of warping of said polarizing glass is 3 μm or less.

10. An optical isolator according to claim 8, characterized in that the inner surface of the polarizing glass opposite the outer surface does not have a functional film for suppressing warping of the polarizing glass.

11. A polarizing glass for an optical isolator, one surface of which is bonded to a Faraday rotator, the polarizing glass having a thickness of 0.028 to 0.20 mm, and the other surface having an anti-reflection film having a thickness of 400 to 2000 nm that is formed after the glass is bonded to the Faraday rotator.

12. The polarizing glass according to claim 11, wherein the amount of warping of the polarizing glass is 3 μm or less.

Citation Information

Patent Citations

  • Optical part for optical isolator or optical magnetic field sensor, production and optical isolator connected to optical fiber

    JP2001051235A

  • Optical isolator and method for processing polarizing glass

    JP2003156623A

  • Polarizing glass, polarizing glass structure, polarizing glass assembly and optical isolator

    JP2013054323A

  • Polarizer and optical isolator

    JP2020091443A