Fan member, fan, fan unit, air conditioner, heat pump device, and method for manufacturing fan member
By integrating a porous member with a resin member having controlled melt flow and flow resistance, the method addresses the issue of resin filling in fan components, achieving effective noise reduction and pressure increase while maintaining structural integrity.
Patent Information
- Application Number
- PCT/JP2024/012925
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-09-28
- Filing Date
- 2024-03-28
- Publication Date
- 2024-10-03
AI Technical Summary
Existing methods for manufacturing fan components with porous members to reduce noise often result in resin filling the pores, which can compromise the noise reduction effect due to insufficient control over resin flow and pore filling during insert molding.
The integration of a porous member with a resin member, where the resin has a controlled melt flow rate (MFR) and the porous member has specific flow resistance and porosity ranges, allowing for selective filling of pores to maintain noise reduction while ensuring proper bonding with the resin.
This approach effectively reduces noise while maintaining the porous structure's integrity, ensuring the fan components achieve both noise reduction and pressure increase effects efficiently.
Smart Images

Figure JP2024012925_03102024_PF_FP_ABST
Abstract
Description
Fan component, fan, fan unit, air conditioner, heat pump device, and method for manufacturing fan component
[0001] The present disclosure relates to a fan component, a fan, a fan unit, an air conditioner, a heat pump device, and a method for manufacturing a fan component.
[0002] It is known to use porous materials for fan components to reduce noise from fan units during rotation. Patent Document 1 discloses a fan having a porous material. When the fan rotates, the pores in the porous material allow airflow to pass from the top surface to the bottom surface of the fan. Therefore, fans with porous materials reduce noise from the fan unit during rotation.
[0003] Another known method for manufacturing a fan component having a porous member is to integrally mold the porous member and a resin component. Patent Documents 2 and 3 disclose, for example, an insert molding method in which a porous member is fixed in a mold and resin is injected into the mold.
[0004] JP 2021-134751, JP 4-012199, JP 6-025597
[0005] When a porous member is insert-molded as in Patent Documents 2 and 3, there is a problem in that the resin flows into the pores of the porous member, filling them with the resin. If the pores of the porous member are lost, there is a risk that the porous member will not be able to achieve a sufficient noise reduction effect.
[0006] An object of the present disclosure is to provide a fan component, a fan, a fan unit, an air conditioner, a heat pump device, and a method for manufacturing a fan component that can suitably integrally mold a porous component and a resin component while maintaining the noise reduction effect of the porous component.
[0007] A first aspect of the fan component that solves this problem is a fan component that includes a porous member having a plurality of pores and a resin member that is molded integrally with the porous member, wherein the resin that constitutes the resin member has a melt flow rate (MFR) of 2 g / 10 min or more and 45 g / 10 min or less, and some of the plurality of pores are filled with the resin.
[0008] With this configuration, the melt flow rate (MFR) of the resin is 45 g / 10 min or less, which reduces the number of pores in the porous member that the resin is filled in. This allows the porous member and the resin member to be suitably molded integrally while maintaining the noise reduction effect of the porous member.
[0009] A fan member according to a second aspect is the fan member according to the first aspect, wherein the resin has a melt flow rate (MFR) of 5 g / 10 min or more and 40 g / 10 min or less. With this configuration, the resin has a melt flow rate (MFR) of 40 g / 10 min or less, which makes it possible to reduce the number of pores in the porous member filled with the resin.
[0010] A fan member according to a third aspect is the fan member according to the second aspect, wherein the fan member is formed from a resin having a melt flow rate (MFR) of 5 g / 10 min or more and 35 g / 10 min or less. With this configuration, the resin has a melt flow rate (MFR) of 35 g / 10 min or less, which makes it possible to reduce the number of pores in the porous member filled with the resin.
[0011] A fan member according to a fourth aspect is the fan member according to any one of the first to third aspects, wherein the flow resistance of the porous member is 0.5 kPa or more and 1.1 kPa or less. With this configuration, since the flow resistance of the porous member is 0.5 kPa or more and 1.1 kPa or less, it is possible to maintain the noise reduction effect of the porous structure while integrally molding the porous member with the resin member.
[0012] A fan member according to a fifth aspect is the fan member according to any one of the first to fourth aspects, wherein the porosity of the porous member is 20% or more and 90% or less, and the pore diameter of the porous member is 50 μm or more and 500 μm or less. With this configuration, the porosity of the porous member is 20% or more and 90% or less, and the pore diameter of the porous member is 50 μm or more and 500 μm or less, so that the number of pores in the porous member that are filled with resin can be reduced.
[0013] A fan member according to a sixth aspect is the fan member according to the fifth aspect, wherein the porosity of the porous member is 30% or more and 90% or less, and the pore diameter of the porous member is 90 μm or more and 300 μm or less. With this configuration, the porosity of the porous member is 30% or more and 90% or less, and the pore diameter of the porous member is 90 μm or more and 300 μm or less, so that the number of pores in the porous member that are filled with resin can be reduced.
[0014] A fan member according to a seventh aspect is the fan member according to any one of the first to sixth aspects, wherein the porous member has a hole filling portion, and the pores of the porous member are filled with the resin in the hole filling portion. With this configuration, the pores of the porous member are filled with resin in the filling portion, so that the porous member can be suitably joined to the resin member.
[0015] According to an eighth aspect of the present invention, there is provided a fan member according to any one of the first to seventh aspects, wherein the porous member has a central portion and a peripheral portion located around the central portion, and the peripheral portion has a different flow resistance from the central portion. With this configuration, by differentiating the flow resistance of the central portion from the flow resistance of the peripheral portion, it is possible to suitably control the bonding condition between the porous member and the resin member.
[0016] A ninth aspect of the present invention provides a fan member including a porous member and a resin member integrally molded with the porous member, wherein the porosity of the porous member is 20% or more and 90% or less, and the pore diameter of the porous member is 50 μm or more and 500 μm or less. With this configuration, the porosity of the porous member is 20% or more and 90% or less, and the pore diameter of the porous member is 50 μm or more and 500 μm or less, so that the number of pores in the porous member that are filled with resin can be reduced. Therefore, the porous member and the resin member can be suitably molded integrally while maintaining the noise reduction effect of the porous member.
[0017] A fan according to a tenth aspect is configured with the fan component according to any one of the first to ninth aspects. According to this configuration, it is possible to provide a fan configured with the fan component. A fan unit according to an eleventh aspect includes the fan according to the tenth aspect and a bellmouth. According to this configuration, it is possible to provide a fan unit including a fan and a bellmouth.
[0018] An air conditioner according to a twelfth aspect includes the fan unit according to the eleventh aspect. According to this configuration, it is possible to provide an air conditioner including a fan unit. According to a thirteenth aspect, it is possible to provide a heat pump device including the fan unit.
[0019] A fourteenth aspect of the manufacturing method is a method for manufacturing a fan member including a porous member having a plurality of pores and a resin member integrally molded with the porous member, the method including the step of insert-molding the porous member with a resin having a melt flow rate (MFR) of 2 g / 10 min or more and 45 g / 10 min or less. According to this configuration, since the melt flow rate (MFR) of the resin is 2 g / 10 min or more and 45 g / 10 min or less, the resin is less likely to flow into the pores of the porous member when the porous member is insert-molded. Because the resin is less likely to flow into the pores of the porous member, the pores of the porous member are more likely to be maintained. By using a resin with such a melt flow rate (MFR), the porous member can be preferably insert-molded while maintaining the noise reduction effect of the porous member.
[0020] FIG. 1 is a schematic diagram of an outdoor unit. FIG. 2 is a front view of a fan. FIG. 3 is an enlarged view of fan blades. FIG. 4 is a schematic diagram showing a flow resistance measuring device. FIG. 5 is a schematic diagram showing steps in a method for manufacturing a fan member. FIG. 6 is a schematic diagram showing steps in a method for manufacturing a fan member. FIG. 7 is a diagram showing the relationship between the porosity, pore diameter, and flow resistance of a porous member. FIG. 8 is a diagram showing the relationship between the porosity, pore diameter, and noise reduction effect of a porous member. FIG. 9 is a diagram showing the noise reduction effect of a fan member relative to the MFR of a resin constituting the resin member, for each flow resistance of the porous member.
[0021] <Embodiment> An air conditioner 10A, a fan unit 20, a fan 30, a fan member 40, and a method for manufacturing the fan member 40 according to an embodiment will be described with reference to Figs. 1 to 9 .
[0022] 1, the air conditioner 10A of this embodiment is a device that adjusts the temperature of indoor air using a vapor compression refrigeration cycle. The air conditioner 10A of this embodiment includes an outdoor unit 10 and an indoor unit (not shown). Note that the air conditioner is not necessarily limited to devices that adjust the temperature of indoor air using a vapor compression refrigeration cycle, and the concept also includes, for example, air purifiers and ventilation devices.
[0023] <Outdoor Unit> The outdoor unit 10 is the outdoor unit 10 of the air conditioner 10A. The air conditioner 10A cools or heats indoor spaces such as homes, offices, etc. The air conditioner 10A may also cool or heat indoor spaces such as spaces in warehouses where goods are stored, or work spaces where goods are handled, for example.
[0024] Fig. 1 is a schematic diagram of an outdoor unit 10 as viewed from the front. In the example of Fig. 1, a vertically-mounted outdoor unit 10 is shown, but the outdoor unit 10 may also be a horizontally-mounted type. The outdoor unit 10 is connected to an indoor unit of an air conditioner 10A, for example, by a connecting pipe. The indoor unit is provided with devices such as an indoor expansion valve and an indoor heat exchanger.
[0025] The outdoor unit 10 includes, for example, a lower unit 11. The lower unit 11 has a lower casing 12. The lower casing 12 is provided with components of the refrigerant circuit, such as a compressor, an outdoor heat exchanger, an outdoor expansion valve, an accumulator, and an oil separator, as well as a control device having electronic components for controlling the refrigerant circuit. The air conditioner 10A includes a fan unit 20. The outdoor unit 10 includes the fan unit 20. The fan unit 20 is connected to, for example, the lower unit 11. The indoor unit of the air conditioner 10A may also include the fan unit 20.
[0026] <Fan Unit> The fan unit 20 includes a fan 30 and a bell mouth 21. In this embodiment, the fan 30 is arranged so that its central axis of rotation extends in the vertical direction. The fan unit 20 is configured, for example, so that air drawn in from the lower unit 11 is blown upward by the fan 30 through the bell mouth 21. The bell mouth 21 in this embodiment is arranged so that the airflow KR passes through it from bottom to top. The bell mouth 21 has a cylindrical portion 21A provided around the fan 30. The cylindrical portion 21A is made of, for example, resin.
[0027] The fan unit 20 includes, for example, a motor 22 and a fan casing 23. The rotating shaft of the motor 22 is connected to the fan 30 so as to rotate the fan 30. The motor 22 is housed in, for example, a motor case.
[0028] The fan casing 23 is disposed, for example, above the lower casing 12. The fan casing 23 houses, for example, the fan 30, the bell mouth 21, and the motor 22. The fan casing 23 has, for example, an air outlet 23A through which air blown out from the bell mouth 21 passes, and a support portion 23B that supports the air outlet 23A. The fan casing 23 is made of, for example, resin.
[0029] <Fan> As shown in Fig. 2, the fan 30 of this embodiment is an axial fan. The fan 30 may be a centrifugal fan. The fan 30 includes a hub 31 and blades 32 provided around the hub 31. The hub 31 is formed in a cylindrical shape. The hub 31 is formed integrally with the blades 32. The hub 31 has a shaft hole 31A into which the rotating shaft of the motor 22 is attached.
[0030] A plurality of blades 32 are arranged on the hub 31 at regular angular intervals in the circumferential direction. In this embodiment, the number of blades 32 is three, but the number may be less than or greater than three. The plurality of blades 32 are arranged so as to spread radially outward from the hub 31 in the rotational radius direction of the fan 30. Adjacent blades 32 do not overlap when viewed from the front or rear of the fan 30. The blades 32 are formed in the shape of a plate that is smoothly curved along the rotational radius direction and the rotational direction. The plurality of blades 32 have the same shape.
[0031] 1 and 2 , the fan unit 20 includes a fan member 40. The fan member 40 is disposed in the fan unit 20 so as to reduce noise generated in the fan unit 20 due to contact with the airflow KR. The member of the fan unit 20 that comes into contact with the airflow KR is formed, for example, by the fan member 40. In this embodiment, the fan 30 is formed by the fan member 40.
[0032] The fan member 40 includes a porous member 41 and a resin member 42 molded integrally with the porous member 41. The fan member 40 is formed of the resin member 42. In this embodiment, the blades 32 are configured with the porous member 41 and the resin member 42. The porous member 41 is disposed, for example, on the blade surface 32A of each blade 32. The blade surface 32A is, for example, a surface disposed to face the airflow KR. The thickness of the porous member 41 is approximately the same as the thickness of the resin member 42. The location where the porous member 41 is disposed is not limited to the blade 32. The hub 31 may also be configured to include the porous member 41.
[0033] The fan member 40 is formed by insert molding the porous member 41 into the resin 42A (see FIG. 6 ) that forms the resin member 42. The porous member 41 is formed, for example, from a porous body. Examples of materials for forming the porous member 41 include resin, ceramics, and metal. Examples of resin include resin foam. Specific examples of the resin porous member 41 include polystyrene resin (PS) foam, ABS resin foam, acrylic styrene (AS) foam, and polypropylene (PP) foam. The porous member 41 may be formed from glass fiber reinforced styrene-acrylonitrile (ASG) foam. The porous member 41 may also be a ceramic or metal porous sintered body. A metal mesh body may also be used as the porous member 41.
[0034] The porous member 41 has a plurality of pores. Some of the plurality of pores are filled with resin 42A. The porous member 41 has a porous structure. The porous structure has through holes that penetrate the blade 32 in the thickness direction. The through holes of the porous structure penetrate the blade 32 in the thickness direction by connecting the plurality of pores contained in the porous member 41. The pores allow the airflow KR to pass through. When the airflow KR passes through the pores of the porous member 41, noise caused by the fan unit 20 is reduced.
[0035] The resin member 42 is configured, for example, so that the air flow KR cannot pass through it. The resin member 42 is configured, for example, of a resin 42A. The resin member 42 is configured, for example, of a thermoplastic resin. The resin member 42 is configured, for example, of a polystyrene resin, an ABS resin, a glass fiber reinforced styrene-acrylonitrile resin (ASG), or a glass fiber reinforced polypropylene resin (PPGF).
[0036] The porous member 41 is formed, for example, from the same type of resin as the resin member 42. When the porous member 41 is a foam made of polystyrene resin, the resin member 42 is made of polystyrene resin. When the porous member 41 is a foam made of ABS resin, the resin member 42 is made of ABS resin. When the porous member 41 is a foam made of acrylic styrene, the resin member 42 is made of glass fiber reinforced styrene-acrylonitrile resin. When the porous member 41 is a foam made of polypropylene, the resin member 42 is made of glass fiber reinforced polypropylene resin. The porous member 41 may be formed from a different type of resin than the resin member 42, or may be formed from a material different from the resin.
[0037] If the porous member 41 is made of the same material as the resin member 42, the porous member 41 and the resin member 42 are likely to adhere to each other when the resin member 42 flows into the pores of the porous member 41 during insert molding of the fan member 40. The adhesion between the porous member 41 and the resin member 42 can improve the bonding strength between the porous member 41 and the resin member 42 during insert molding.
[0038] 3 and 6 , parameters indicating the ease of flow of the resin 42A through the porous member 41 include, for example, the melt flow rate (MFR) of the resin 42A under predetermined conditions. For example, the larger the MFR, the easier it is for the resin 42A to flow through the porous member 41 during insert molding. The MFR is, for example, the melt mass-flow rate. The predetermined conditions are, for example, test conditions in accordance with ISO 1133. As an example, when the resin member 42 is a polystyrene resin, the predetermined conditions for measuring the MFR of the resin 42A are a temperature of 200° C. and a load of 5 kg in accordance with ISO 1133.
[0039] Under predetermined conditions, the MFR of the resin 42A constituting the resin member 42 is 2 g / 10 min or more and 45 g / 10 min or less. Under predetermined conditions, the MFR of the resin 42A may be 2 g / 10 min or more and 40 g / 10 min or less. Under predetermined conditions, the MFR of the resin 42A may be 2 g / 10 min or more and 35 g / 10 min or less. Under predetermined conditions, the MFR of the resin 42A may be 2 g / 10 min or more and 30 g / 10 min or less. Under predetermined conditions, the MFR of the resin 42A may be 5 g / 10 min or more and 45 g / 10 min or less. Under predetermined conditions, the MFR of the resin 42A may be 5 g / 10 min or more and 40 g / 10 min or less. Under predetermined conditions, the MFR of the resin 42A may be 5 g / 10 min or more and 35 g / 10 min or less. Under predetermined conditions, the MFR of the resin 42A may be 5 g / 10 min or more and 25 g / 10 min or less. Under predetermined conditions, the MFR of the resin 42A may be 7 g / 10 min or more and 16.5 g / 10 min or less. Under predetermined conditions, the MFR of the resin 42A may be 7 g / 10 min or more, or may be 16.5 g / 10 min or less. As an example, if the resin 42A is a polystyrene resin, the predetermined conditions for measuring the MFR of the resin 42A are a temperature of 200°C and a load of 5 kg, in accordance with ISO 1133. If the MFR of the resin 42A is 2 g / 10 min or more and 45 g / 10 min or less, the resin 42A will have difficulty flowing through the porous member 41.
[0040] The parameter indicating the ease of flow of the resin 42A through the porous member 41 includes, for example, the flow resistance of the porous member 41. For example, the greater the flow resistance of the porous member 41, the more difficult it is for the resin 42A to flow through the porous member 41 during insert molding. The flow resistance of the porous member 41 is adjusted, for example, during the formation stage of the porous member 41. The flow resistance of the porous member 41 is adjusted, for example, by the crushed particle size of the material that makes up the porous member 41.
[0041] In the embodiment, the flow resistance of the porous member 41 indicates how difficult it is for air to flow in the porous structure of the porous member 41. For example, the greater the flow resistance of the porous member 41, the more difficult it is for the air flow KR to pass through the porous member 41. When the flow resistance of the porous member 41 is large, the pore diameter of the porous member 41 tends to be small or the porosity of the porous member 41 tends to be low, making it difficult for the resin 42A to flow through the porous member 41.
[0042] FIG. 4 shows an example of a measuring device 60 for measuring the flow resistance of a porous member 41. The measuring device 60 is a jig for measuring the flow resistance of a test piece 61. The measuring device 60 has a first case 62 and a second case 63. The first case 62 defines a first chamber 64. The second case 63 defines a second chamber 65. The first chamber 64 and the second chamber 65 communicate with each other via a communication hole 66. The communication hole 66 is provided so as to penetrate the first case 62 and the second case 63. A test piece 61 is placed in the communication hole 66. The test piece 61 has a porous structure with a through hole that penetrates from the first chamber 64 to the second chamber 65. Air can move between the first chamber 64 and the second chamber 65 by passing through the porous structure of the test piece 61.
[0043] The measuring device 60 has a first flow path 67, a second flow path 68, and a blower 69. The first flow path 67 connects to the first chamber 64 so as to communicate the first chamber 64 with the outside of the first case 62. The second flow path 68 connects to the second chamber 65 so as to communicate the second chamber 65 with the outside of the second case 63. The first flow path 67, the first chamber 64, the second chamber 65, and the second flow path 68 form an air flow path 70 in the measuring device 60. The blower 69 sends air from the first flow path 67 to the measuring device 60. The air sent by the blower 69 flows through the air flow path 70. The air that has flowed through the air flow path 70 flows out of the measuring device 60 through the second flow path 68.
[0044] The measuring device 60 has a first flow meter 71 and a second flow meter 72. The first flow meter 71 and the second flow meter 72 are, for example, air flow meters. The first flow meter 71 is configured to measure the air flow rate through the first flow path 67. The second flow meter 72 is configured to measure the air flow rate through the second flow path 68.
[0045] The measuring device 60 has a first differential pressure gauge 73 and a second differential pressure gauge 74. The first differential pressure gauge 73 and the second differential pressure gauge 74 are, for example, pressure gauges. The first differential pressure gauge 73 is configured to measure the pressure in the first chamber 64. The second differential pressure gauge 74 is configured to measure the pressure in the second chamber 65. When air is being blown into the measuring device 60 by the blower 69, the difference between the pressure in the first chamber 64 and the pressure in the second chamber 65 is the flow resistance of the test piece 61.
[0046] The measuring device 60 is configured so that when the airflow rate through the first flow path 67 is 100 L / min, the difference between the airflow rate through the first flow path 67 and the airflow rate through the second flow path 68 is less than 1% of the airflow rate through the first flow path 67. The first case 62 and the second case 63 are configured so that air cannot move between the first chamber 64 and the second chamber 65 from any portion other than the communication hole 66. The test specimen 61 is arranged so as to be sandwiched between the first case 62 and the second case 63. At this time, the contact portion between the first case 62 and the test specimen 61 and the contact portion between the second case 63 and the test specimen 61 are sealed with packing to prevent air leakage. The air passage area on the surface of the test specimen 61 is set to be the same regardless of the type of test specimen 61. The area of the test specimen 61 exposed to the first chamber 64 is set to be the same regardless of the type of test specimen 61. The area of the test piece 61 exposed to the second chamber 65 is set to be the same regardless of the type of test piece 61. The blower 69 is configured to ensure a flow rate of 100 L / min regardless of pressure loss due to the measuring device 60 and the test piece 61, so that the flow rate measured by the first flow meter 71 and the second flow meter 72 is stable.
[0047] The flow resistance of the porous member 41 is, for example, 0.2 kPa or more and 1.2 kPa or less. The flow resistance of the porous member 41 may be, for example, 0.3 kPa or more and 1.1 kPa or less. The flow resistance of the porous member 41 may be, for example, 0.35 kPa or more and 1.0 kPa or less. By setting the flow resistance of the porous member 41 to 0.2 kPa or more, the resin 42A does not easily flow through the porous member 41. On the other hand, by setting the flow resistance of the porous member 41 to 1.2 kPa or less, the resin 42A is appropriately filled into the pores of the porous member 41, allowing the resin member 42 to be bonded to the porous member 41.
[0048] The flow resistance of the porous member 41 may be, for example, 0.4 kPa or more and 1.1 kPa or less. The flow resistance of the porous member 41 may be, for example, 0.5 kPa or more and 1.1 kPa or less. By setting the flow resistance of the porous member 41 to 0.4 kPa or more, the porous structure of the porous member 41 is suitably maintained in the fan member 40. By setting the flow resistance of the porous member 41 to 1.1 kPa or less, the porous structure of the porous member 41 is maintained, and the resin member 42 can be suitably bonded to the porous member 41.
[0049] The flow resistance of the porous member 41 is greater than the value obtained by multiplying the MFR of the resin 42A by the gravitational acceleration and then dividing the product by the cross-sectional area of the porous member 41. The cross-sectional area of the porous member 41 is the cross-sectional area of the porous member 41 when the blade 32 is viewed from the thickness direction.
[0050] The flow resistance of the porous member 41 is determined by the pore diameter and porosity of the porous member 41. The smaller the pore diameter of the porous member 41, the greater the flow resistance of the porous member 41, and the larger the pore diameter of the porous member 41, the smaller the flow resistance of the porous member 41. The smaller the porosity of the porous member 41, the greater the flow resistance of the porous member 41, and the greater the porosity of the porous member 41, the smaller the flow resistance of the porous member 41.
[0051] The pore diameter of the porous member 41 is, for example, the average pore diameter of the pores in the porous member 41. There are no particular limitations on the method for measuring the average pore diameter, and the average pore diameter can be measured, for example, by a gas adsorption method also known as the BET method. The gas adsorption conditions are, for example, test conditions in accordance with JIS Z8831-2 2010 or ISO 15901-2 2006. The gas adsorption conditions may also be test conditions in accordance with JIS Z8830 2013 or ISO 9277 2010. The porosity of the porous member 41 is, for example, the total volume of pores in the porous member 41 relative to the total volume of the porous member 41.
[0052] The porosity of the porous member 41 is 20% or more and 90% or less, and the pore diameter of the porous member 41 is 50 μm or more and 500 μm or less. The porosity of the porous member 41 may be 30% or more and 90% or less, and the pore diameter of the porous member 41 may be 90 μm or more and 300 μm or less. The porosity of the porous member 41 may be 30% or more and 80% or less, and the pore diameter of the porous member 41 may be 100 μm or more and 200 μm or less.
[0053] As shown in Figure 3, porous member 41 has a central portion 43 and a peripheral portion 44. In Figure 3, the boundary between central portion 43 and peripheral portion 44 is indicated by a dashed line. Central portion 43 is a portion of porous member 41 where resin 42A does not flow and the porous structure is exposed. In central portion 43, the pores of porous member 41 are maintained so that the pores in porous member 41 form through-holes in porous member 41 after fan member 40 is insert-molded.
[0054] The area of the central portion 43 is, for example, 2400 mm 2 More than 6200mm 2 The area of the central portion 43 is, for example, 2800 mm 2 Above 5800mm 2 The area of the central portion 43 may be, for example, 3200 mm 2 More than 5,400 mm 2The area of the central portion 43 is, for example, the area of the central portion 43 of the porous member 41 arranged on one blade 32 .
[0055] The peripheral edge portion 44 is located, for example, around the central portion 43. The peripheral edge portion 44 is a portion of the porous member 41 through which the resin 42A flows. After the fan member 40 is insert-molded, the pores of the porous member 41 may or may not be maintained in the peripheral edge portion 44. The width D1 of the peripheral edge portion 44 is, for example, 2 mm or more and 6 mm or less. The width D1 of the peripheral edge portion 44 is, for example, 2.5 mm or more and 5.5 mm or less. The width D1 of the peripheral edge portion 44 is, for example, 3 mm or more and 5 mm or less. The width D1 of the peripheral edge portion 44 is, for example, the length from the end of the central portion 43 to the end of the porous member 41. The width D1 of the peripheral edge portion 44 is, for example, the shortest length between the end of the central portion 43 and the end of the porous member 41.
[0056] The pore diameter of the peripheral portion 44 may be the same as the pore diameter of the central portion 43, or may be smaller than the pore diameter of the central portion 43. The porosity of the peripheral portion 44 may be the same as the pore diameter of the central portion 43, or may be smaller than the porosity of the central portion 43. In this embodiment, when the pore diameter of the peripheral portion 44 is the same as the pore diameter of the central portion 43, the porosity of the peripheral portion 44 is smaller than the porosity of the central portion 43. In this embodiment, when the porosity of the peripheral portion 44 is the same as the porosity of the central portion 43, the pore diameter of the peripheral portion 44 is smaller than the pore diameter of the central portion 43.
[0057] The flow resistance of the peripheral portion 44 is different from the flow resistance of the central portion 43. In this embodiment, the flow resistance of the peripheral portion 44 is greater than the flow resistance of the central portion 43. The flow resistance of the peripheral portion 44 is set to be different from the flow resistance of the central portion 43 when the porous member 41 is formed. Because the flow resistance of the peripheral portion 44 is greater than the flow resistance of the central portion 43, it is difficult for the resin 42A to flow over the peripheral portion 44 and into the central portion 43 when the fan member 40 is insert molded. When the porous member 41 is compressed by the mold 50 during insert molding, the pores are compressed, reducing the porosity, so the flow resistance of the peripheral portion 44 may be greater than the flow resistance of the central portion 43 (see FIG. 6 ).
[0058] As shown in FIG. 3 , the porous member 41 has a hole filling portion 45. In the hole filling portion 45, the multiple pores of the porous member 41 are filled with resin 42A. The hole filling portion 45 is a portion formed by the resin 42A seeping into the pores of the porous member 41 when the fan member 40 is insert-molded. The porous member 41 is connected to the resin member 42 by the hole filling portion 45. The hole filling portion 45 is located around the central portion 43. The hole filling portion 45 may overlap the peripheral edge portion 44.
[0059] <Method for Manufacturing Fan Component> As shown in Figures 3 to 6, the manufacturing method is a method for manufacturing a fan component 40 including a porous component 41 having a plurality of pores and a resin component 42 integrally molded with the porous component 41. The manufacturing method includes a step of insert-molding the porous component 41 with a resin 42A having a melt flow rate (MFR) of 2 g / 10 min or more and 45 g / 10 min or less. The fan component 40 is molded, for example, by insert molding. In Figures 5 and 6, the right side of the figure corresponds to the hub 31 side of the blade 32 in the direction of the rotation radius. The left side of the figure corresponds to the outer end side of the blade 32 in the direction of the rotation radius. The manufacturing method includes a first step, a second step, and a third step.
[0060] The first step is a step of placing the porous member 41 in a mold 50. Fig. 5 shows the state in which the porous member 41 is placed in the mold 50 in the first step. The mold 50 is provided with pins 52 to be inserted into holes 51. In the first step, the pins 52 are placed so as to protrude from the holes 51. The porous member 41 is placed in the mold 50 so as to be in contact with the pins 52.
[0061] The second step is a step of pressing the porous member 41 with a mold 50. In the second step, the porous member 41 is compressed in the thickness direction by the mold 50 so that the thickness of the porous member 41 is reduced from the first dimension W1 to the second dimension W2. The compression amount of the porous member 41 is set based on, for example, the flow resistance of the porous member 41 after compression.
[0062] The third step is insert molding the porous member 41 with resin 42A. As shown by the arrow in FIG. 6 , the resin 42A is injected into the mold 50 from the right side of FIG. 6 . During the step of injecting the resin 42A, the movement of the porous member 41 is restricted by pins 52. When the resin 42A fills the mold 50, the pins 52 are pressed into the holes 51 by the pressure of the resin 42A. After the insert molding, traces 52A of the pins 52 may remain in the resin member 42 (see FIG. 3 ). If the porous member 41 can be placed in the mold 50 so that it does not move relative to the mold 50 during insert molding, the holes 51 and pins 52 may be omitted from the mold 50.
[0063] <Noise Reduction Effect of Porous Member> The noise reduction effect of the fan member 40 is achieved by arranging the porous member 41 so that the airflow KR passes through the pores of the porous member 41. If the pores of the porous member 41 are too small or the porosity of the porous member 41 is too low, the airflow KR cannot pass through the pores of the porous member 41, and sufficient noise reduction effect cannot be achieved. If the pores of the porous member 41 are large or the porosity of the porous member 41 is high, the amount of airflow KR passing through the pores of the porous member 41 increases. If the amount of airflow KR passing through the pores of the porous member 41 increases, there is a risk that the fan 30 will not achieve its intended pressure-boosting effect. In order to maintain sufficient noise reduction effect and to obtain the intended pressure-boosting effect of the fan 30, the flow resistance of the porous member 41 is set based on the pore size and porosity of the porous member 41.
[0064] 7, the flow resistance value of the porous member 41 is mapped against the pore size and porosity of the porous member 41. In FIG. 7, the line where the flow resistance is 0.2 kPa is indicated by a dashed line. In the region where the flow resistance of the porous member 41 is 0.2 kPa or more, the resin 42A does not easily flow into the porous member 41 during insert molding. In the region where the flow resistance of the porous member 41 is 0.2 kPa or more, not only does the resin 42A not easily flow into the porous member 41 during insert molding, but the fan 30 can also achieve a favorable pressure increase effect.
[0065] 8, the noise reduction effect of the porous member 41 is mapped against the pore size and porosity of the porous member 41. The noise reduction effect value is, for example, the sound pressure at which the porous member 41 can reduce noise. The porous member 41 can maintain its noise reduction effect when the pore size of the porous member 41 is in the range of 50 μm or more and 500 μm or less, and the porosity of the porous member 41 is in the range of 20% or more and 90% or less. The noise reduction effect is quantified as the noise level of the fan 30 provided with the porous member 41 relative to the noise level of the fan 30 without the porous member 41, for a fan 30 of the same shape.
[0066] 8, the region where the flow resistance is 0.2 kPa or more, the pore diameter of the porous member 41 is 50 μm or more and 500 μm or less, and the porosity of the porous member 41 is 20% or more and 90% or less is indicated by a two-dot chain line. In the region indicated by the two-dot chain line, not only can the noise reduction effect be maintained, but also the fan 30 can obtain a suitable pressure increase effect.
[0067] FIG. 9 shows the ratio of the noise reduction effect of the fan component 40 to the MFR of the resin 42A constituting the resin member 42 when the flow resistance of the porous member 41 is 0.4 kPa, 0.5 kPa, 0.8 kPa, or 1.1 kPa. To obtain the data shown in FIG. 9 , multiple test fans 30 were fabricated. Specifically, the test fans 30 were constructed using fan components 40 in which the flow resistance of the porous member 41 differed and the MFR of the resin 42A constituting the resin member 42 differed. The test fans 30 had the same shape. The porous members 41 of the fan components 40 constituting each of the test fans 30 were fabricated from the same material but with different flow resistances. The resin components 42 of the fan components 40 constituting each of the test fans 30 were fabricated from the same type of resin 42A but with different MFRs. The porous member 41 of the fan member 40 constituting the test fan 30 is made of a glass fiber reinforced styrene-acetallonitrile (ASG) foam. The resin member 42 of the fan member 40 constituting the test fan 30 is also made of glass fiber reinforced styrene-acetallonitrile (ASG). The data in Figure 9 was obtained by measuring the noise generated when each of the multiple test fans 30 rotated.
[0068] The noise reduction effect ratio in Figure 9 is the ratio of the noise reduction effect of the test fan 30 at each value of the MFR of the resin 42A to the maximum noise reduction effect of the test fan 30 when the flow resistance of the porous member 41 is a predetermined value. According to Figure 9, when the flow resistance of the porous member 41 is 1.1 kPa, the noise reduction effect reaches its maximum when the MFR of the resin 42A is 25 g / 10 min. When the flow resistance of the porous member 41 is 1.1 kPa and the MFR of the resin 42A is 35 g / 10 min, the fan 30 achieves a noise reduction effect of approximately 80% or more of the maximum noise reduction effect.
[0069] The greater the MFR of resin 42A, the more easily resin 42A flows into the through-holes of porous member 41 during insert molding, which tends to reduce the noise reduction effect of fan member 40. Note that in regions where the flow resistance of porous member 41 is high and the MFR of resin 42A is low, it is difficult to form fan 30, which may result in variations in the noise reduction effect of fan member 40.
[0070] The fan member 40 can achieve a noise reduction effect when the flow resistance of the porous member 41 is 0.4 kPa or more and 0.8 kPa or less and the MFR of the resin 42A is 2 g / 10 min or more and 45 g / 10 min or less. Furthermore, the fan member 40 can achieve a noise reduction effect of 20% or more of the maximum noise reduction effect when the flow resistance of the porous member 41 is 0.4 kPa or more and 1.1 kPa or less and the MFR of the resin 42A is 5 g / 10 min or more and 40 g / 10 min or less. Preferably, the fan member 40 can achieve a noise reduction effect of 30% or more of the maximum noise reduction effect when the flow resistance of the porous member 41 is 0.5 kPa or more and 1.1 kPa or less and the MFR of the resin 42A is 5 g / 10 min or more and 40 g / 10 min or less.
[0071] <Operation of the embodiment> The operation of the present embodiment will be described. In this embodiment, the fan member 40 includes the resin member 42 formed of the resin 42A having an MFR of 2 g / 10 min or more and 45 g / 10 min or less. The resin 42A having an MFR of 45 g / 10 min or less is less likely to flow into the pores of the porous member 41 during insert molding using the resin 42A.
[0072] In one example of the fan component 40 of this embodiment, the flow resistance of the porous component 41 is 0.5 kPa or more and 1.1 kPa or less. In FIG. 7 , the flow resistances of 0.5 kPa and 1.1 kPa are indicated by dashed lines. In FIG. 7 , the range of flow resistance from 0.5 kPa or more to 1.1 kPa or less is indicated by the area between the dashed lines. A flow resistance of 1.1 kPa or less allows the resin 42A to flow through the porous component 41 during insert molding with the resin 42A. This allows the porous component 41 and the resin component 42 to be suitably bonded together in the fan component 40. On the other hand, a flow resistance of 0.5 kPa or more maintains the porous structure of the porous component 41 during insert molding with the resin 42A, ensuring that the fan component 40 achieves the noise reduction effect of its porous structure.
[0073] The porous member 41 of this embodiment has a pore diameter of 50 μm or more and 500 μm or less, and a flow resistance such that the porosity of the porous member 41 is 20% or more and 90% or less. Because the flow resistance of the porous member 41 is sufficiently large, the resin 42A does not easily flow through the porous member 41. The fan member 40 not only maintains a sufficient noise reduction effect, but also makes it difficult for the resin 42A to flow into the pores of the porous member 41 during insert molding.
[0074] The porous member 41 of this embodiment has a peripheral portion 44. During insert molding of the fan member 40, the resin 42A first flows into the peripheral portion 44 and then flows through the peripheral portion 44 toward the central portion 43. Because the peripheral portion 44 of this embodiment has a width D1, it is possible to prevent the resin 42A from flowing into the central portion 43. The resin 42A flows into the peripheral portion 44, thereby forming a hole filling portion 45 in the porous member 41. Because the resin 42A flows into the pores in the hole filling portion 45, the porous member 41 and the resin member 42 are suitably joined by the hole filling portion 45.
[0075] Effects of the present embodiment The effects of the present embodiment will be described. (1) The fan member 40 includes a porous member 41 and a resin member 42. The resin 42A constituting the resin member 42 has an MFR of 2 g / 10 min or more and 45 g / 10 min or less. Some of the pores of the porous member 41 are filled with the resin 42A.
[0076] With this configuration, the MFR of the resin 42A is 45 g / 10 min or less, so the number of pores in the porous member 41 filled with the resin 42A can be reduced. Therefore, the porous member 41 and the resin member 42 can be suitably molded integrally while maintaining the noise reduction effect of the porous member 41.
[0077] When the resin 42A has an MFR of 45 g / 10 min or less, the resin 42A does not easily flow into the pores of the porous member 41 when the resin member 42 is integrally molded with the porous member 41. Because the resin 42A does not easily flow into the pores of the porous member 41, the pores of the porous member 41 are easily maintained.
[0078] If the MFR of the resin 42A is greater than 45 g / 10 min, the resin 42A flows more easily into the mold 50, thereby shortening the injection time during insert molding. However, if the MFR of the resin 42A is too high, the resin 42A will flow not only into the peripheral portion 44 of the porous member 41 but also into the central portion 43 of the porous member 41 during insert molding. If the resin 42A flows into the central portion 43 of the porous member 41, the resin 42A will fill the pores in the central portion 43, reducing the number of pores in the porous member 41. This reduction in the number of pores in the porous member 41 may reduce the noise reduction effect of the porous member 41. If the MFR of the resin 42A is 45 g / 10 min or less, the resin 42A can be prevented from penetrating into the central portion 43 of the porous member 41 during insert molding.
[0079] The resin 42A may have an MFR of 2 g / 10 min or more and 40 g / 10 min or less. With this configuration, the resin 42A is less likely to flow into the pores of the porous member 41, and therefore the pores of the porous member 41 are more likely to be maintained.
[0080] The resin 42A may have an MFR of 2 g / 10 min or more and 35 g / 10 min or less. With this configuration, the resin 42A is less likely to flow into the pores of the porous member 41, and therefore the pores of the porous member 41 are more likely to be maintained.
[0081] If the MFR of resin 42A is less than 2 g / 10 min, resin 42A will have difficulty flowing within mold 50 during insert molding, making it difficult to form fan member 40. If the MFR of resin 42A is too small, it will be even more difficult to use resin 42A to form fan member 40 when the fan member 40 is to be made thinner. If the MFR of resin 42A is 2 g / 10 min or greater, resin 42A will be able to flow smoothly within mold 50 during insert molding, making it possible to successfully form fan member 40.
[0082] Resin 42A may have an MFR of 5 g / 10 min or more and 45 g / 10 min or less. This configuration allows resin 42A to flow more efficiently within mold 50 during insert molding, thereby more efficiently forming fan member 40.
[0083] Furthermore, with this configuration, the pores to be filled with the resin 42A are appropriately set among the multiple pores of the porous member 41. By setting the MFR in this manner, it is possible to improve the bonding strength between the porous member 41 and the resin member 42 while maintaining the noise reduction effect due to the porous structure of the porous member 41.
[0084] (2) The MFR of the resin 42A is 5 g / 10 min or more and 40 g / 10 min or less. With this configuration, the MFR of the resin 42A is 40 g / 10 min or less, which reduces the number of pores in the porous member 41 filled with the resin 42A. Furthermore, when the MFR of the resin 42A is 5 g / 10 min or more, the resin 42A can flow smoothly within the mold 50 during insert molding, which allows the fan member 40 to be formed more efficiently.
[0085] (3) The MFR of the resin 42A is 5 g / 10 min or more and 35 g / 10 min or less. With this configuration, the MFR of the resin 42A is 35 g / 10 min or less, which reduces the number of pores in the porous member 41 filled with the resin 42A. Furthermore, when the MFR of the resin 42A is 5 g / 10 min or more, the resin 42A can flow smoothly within the mold 50 during insert molding, which allows the fan member 40 to be formed more efficiently.
[0086] (4) The flow resistance of the porous member 41 is 0.5 kPa or more and 1.1 kPa or less. With this configuration, since the flow resistance of the porous member 41 is 0.5 kPa or more, the number of pores in the porous member 41 that are filled with the resin 42A can be reduced. On the other hand, since the flow resistance of the porous member 41 is 1.1 kPa or less, the resin 42A can be filled into the pores of the porous member 41 to the extent that the porous member 41 and the resin member 42 are integrated together. In this way, since the flow resistance of the porous member 41 of the fan member 40 is 0.5 kPa or more and 1.1 kPa or less, the porous member 41 can be molded integrally with the resin member 42 while maintaining the noise reduction effect of the porous structure.
[0087] (5) The porosity of the porous member 41 is 20% or more and 90% or less, and the pore diameter of the porous member 41 is 50 μm or more and 500 μm or less. With this configuration, the porosity of the porous member 41 is 20% or more and 90% or less, and the pore diameter of the porous member 41 is 50 μm or more and 500 μm or less, so that the number of pores in the porous member 41 that are filled with the resin 42A can be reduced.
[0088] Increasing the flow resistance of the porous member 41 makes it difficult for the resin 42A to flow into the porous member 41. Because the resin 42A does not flow easily into the porous member 41, it does not easily flow into the pores of the porous member 41. By reducing the porosity and pore diameter so as to increase the flow resistance of the porous member 41, it becomes easier to maintain the pores of the porous member 41 when the porous member 41 is integrally molded with the resin member 42. A porous member 41 having a porosity of 20% or more and 90% or less and a pore diameter of 50 μm or more and 500 μm or less can not only maintain its noise reduction effect, but also maintain the flow resistance that makes it difficult for the resin 42A to flow into the pores of the porous member 41.
[0089] If the pore diameter of the porous member 41 is less than 50 μm, the noise reduction effect of the porous member 41 is reduced. If the pore diameter of the porous member 41 is greater than 500 μm, the flow resistance of the porous member 41 is reduced, so that the resin 42A easily flows into the pores of the porous member 41 during insert molding. If the porosity of the porous member 41 is less than 20%, the noise reduction effect of the porous member 41 is reduced. If the porosity of the porous member 41 is greater than 90%, the flow resistance of the porous member 41 is reduced, so that the resin 42A easily flows into the pores of the porous member 41 during insert molding.
[0090] (6) The porosity of the porous member 41 is 30% or more and 90% or less, and the pore diameter of the porous member 41 is 90 μm or more and 300 μm or less. With this configuration, the porosity of the porous member 41 is 30% or more and 90% or less, and the pore diameter of the porous member 41 is 90 μm or more and 300 μm or less, so that the number of pores in the porous member 41 that are filled with the resin 42A can be reduced.
[0091] (7) The porous member 41 has a hole filling portion 45. In the hole filling portion 45, the pores of the porous member 41 are filled with the resin 42A. According to this configuration, in the hole filling portion 45, the resin 42A fills the multiple pores of the porous member 41, and therefore the porous member 41 can be suitably bonded to the resin member 42 in the hole filling portion 45.
[0092] (8) The porous member 41 has a central portion 43 and a peripheral portion 44. The flow resistance of the peripheral portion 44 is different from the flow resistance of the central portion 43. According to this configuration, by making the flow resistance of the central portion 43 and the flow resistance of the peripheral portion 44 different in the porous member 41, it is possible to suitably control the bonding condition between the porous member 41 and the resin member 42. In this embodiment, by making the flow resistance of the peripheral portion 44 greater than the flow resistance of the central portion 43, it is possible to operate the porous member 41 and the resin member 42 so that they are bonded only at the peripheral portion 44.
[0093] (9) The fan member 40 includes a porous member 41 and a resin member 42 integrally molded with the porous member 41. The porosity of the porous member 41 is 20% or more and 90% or less, and the pore diameter of the porous member 41 is 50 μm or more and 500 μm or less. With this configuration, the porosity of the porous member 41 is 20% or more and 90% or less, and the pore diameter of the porous member 41 is 50 μm or more and 500 μm or less, so that the number of pores in the porous member 41 that are filled with the resin 42A can be reduced. Therefore, the porous member 41 and the resin member 42 can be suitably molded integrally while maintaining the noise reduction effect of the porous member 41.
[0094] (10) The fan 30 is composed of a fan member 40. This configuration makes it possible to provide a fan 30 composed of a fan member 40. (11) The fan unit 20 includes a fan 30 and a bellmouth 21. This configuration makes it possible to provide a fan unit 20 including a fan 30 and a bellmouth 21.
[0095] (12) The air conditioner 10A includes a fan unit 20. This configuration allows for the provision of an air conditioner 10A including the fan unit 20. (13) A method for manufacturing a fan member 40 includes insert-molding a porous member 41 having a plurality of pores with a resin 42A having an MFR of 2 g / 10 min or more and 45 g / 10 min or less. According to this configuration, since the resin 42A has an MFR of 2 g / 10 min or more and 45 g / 10 min or less, the resin 42A is less likely to flow into the pores of the porous member 41 when the porous member 41 is insert-molded. Because the resin 42A is less likely to flow into the pores of the porous member 41, the pores of the porous member 41 are more likely to be maintained. By using a resin member 42 with such an MFR, the porous member 41 can be preferably insert-molded while maintaining the noise reduction effect of the porous member 41.
[0096] <Variations> In addition to the above-described embodiments, the air conditioner, fan unit, fan, fan component, and method for manufacturing a fan component of the present disclosure may also be configured in a form that combines, for example, the variations shown below, or at least two variations that are not mutually contradictory.
[0097] The air conditioner 10A may be an air purifier. The fan unit 20 may constitute an intake or exhaust port of the air purifier. The air purifier, for example, treats the drawn-in air using a filter, a UV device, an ionizer device, a virus removal sprayer, a streamer device, or the like, and then blows out the air. The air purifier is configured to treat the air in an indoor space such as a home or an office. The air purifier may also be configured to treat the air in an indoor space such as a space in a warehouse where goods are stored or a work space where goods are handled.
[0098] The fan unit 20 may be provided in a heat pump device. The heat pump device of this modified example includes the fan unit 20. The heat pump device is, for example, a device having a refrigerant circuit. The heat pump device is, for example, an air conditioner or a water heater. With this configuration, a heat pump device including the fan unit 20 can be provided.
[0099] The member formed by the fan member 40 is not limited to the fan 30. The bell mouth 21 may be formed by the fan member 40, and the fan casing 23 may be formed by the fan member 40. When the fan casing 23 is formed by the fan member 40, the air outlet 23A or the support portion 23B may also be formed by the fan member 40.
[0100] The predetermined conditions may be test conditions conforming to ISO 1133-1 or ISO 1133-2. The predetermined conditions may be test conditions conforming to JIS K7210-1, JIS K7210-2, or ASTM D1238.
[0101] The MFR may be a melt volume-flow rate (MVR). The MVR is, for example, the product of the melt mass flow rate of the resin 42A and the melt density of the resin 42A.
[0102] The flow resistance of the peripheral portion 44 may be smaller than the flow resistance of the central portion 43. With this configuration, the resin 42A can easily permeate the peripheral portion 44, thereby improving the bonding strength between the porous member 41 and the resin member 42.
[0103] This specification discloses the following technology: (C1) A fan member (40) including a porous member (41) and a resin member (42) integrally molded with the porous member (41), wherein the porous member (41) has a central portion (43) and a peripheral portion (44) positioned around the central portion (43). The flow resistance of the peripheral portion (44) is different from the flow resistance of the central portion (43).
[0104] (C2) A fan member (40) according to (C1), wherein the porosity of the porous member (41) is 20% or more and 90% or less, and the pore diameter of the porous member (41) is 50 μm or more and 500 μm or less.
[0105] The above describes embodiments and variations of the fan components, fans, fan units, air conditioners, heat pump devices, and methods for manufacturing fan components. However, it will be understood that various changes in form and details are possible without departing from the spirit and scope of the fan components, fans, fan units, air conditioners, heat pump devices, and methods for manufacturing fan components as set forth in the claims.
[0106] 10A...air conditioner, 10...outdoor unit, 20...fan unit, 21...bell mouth, 30...fan, 40...fan member, 41...porous member, 42...resin member, 42A...resin, 43...central portion, 44...peripheral portion, 45...hole filling portion.
Claims
1. A fan component (40) comprising a porous member (41) having a plurality of pores and a resin member (42) molded integrally with the porous member (41), wherein the melt flow rate (MFR) of a resin (42A) constituting the resin member (42) is 2 g / 10 min or more and 45 g / 10 min or less, and a portion of the plurality of pores is filled with the resin (42A).
2. The fan member according to claim 1, wherein the melt flow rate (MFR) of the resin (42A) is 5 g / 10 min or more and 40 g / 10 min or less.
3. The fan component according to claim 2, wherein the melt flow rate (MFR) of the resin (42A) is 5 g / 10 min or more and 35 g / 10 min or less.
4. A fan member according to any one of claims 1 to 3, wherein the flow resistance of the porous member (41) is 0.5 kPa or more and 1.1 kPa or less.
5. A fan member according to any one of claims 1 to 4, wherein the porosity of the porous member (41) is 20% or more and 90% or less, and the pore diameter of the porous member (41) is 50 μm or more and 500 μm or less.
6. The fan member according to claim 5, wherein the porosity of the porous member (41) is 30% or more and 90% or less, and the pore diameter of the porous member (41) is 90 μm or more and 300 μm or less.
7. A fan member as claimed in any one of claims 1 to 6, wherein the porous member (41) has a hole filling portion (45), and in the hole filling portion (45), the plurality of pores of the porous member (41) are filled with the resin (42A).
8. A fan member as claimed in any one of claims 1 to 7, wherein the porous member (41) has a central portion (43) and a peripheral portion (44) located around the central portion (43), and the flow resistance of the peripheral portion (44) is different from the flow resistance of the central portion (43).
9. A fan member (40) comprising a porous member (41) and a resin member (42) molded integrally with the porous member (41), wherein the porosity of the porous member (41) is 20% or more and 90% or less, and the pore diameter of the porous member (41) is 50 μm or more and 500 μm or less.
10. A fan comprising the fan member (40) according to any one of claims 1 to 9.
11. A fan unit comprising: the fan (30) according to claim 10; and a bellmouth (21).
12. An air conditioner comprising the fan unit (20) according to claim 11.
13. A heat pump device comprising the fan unit (20) according to claim 11.
14. A method for manufacturing a fan member (40) comprising a porous member (41) having a plurality of pores and a resin member (42) molded integrally with the porous member (41), the method comprising a step of insert molding the porous member (41) with a resin (42A) having a melt flow rate (MFR) of 2 g / 10 min or more and 45 g / 10 min or less.
Citation Information
Patent Citations
fan shroud for axial fan
JP1994025597U
Fan unit and blower using the same
JP2021134751A
Blower impeller
JP1992012199A
Impeller for blower
JP2005155437A