Power storage device and method for manufacturing same
The introduction of a seal reinforcement portion made from a mixture of resin, metal, ceramics, and rubber addresses the dimensional mismatch issue between the lid and exterior film, significantly improving sealing performance and preventing leakage in power storage devices.
Patent Information
- Application Number
- PCT/JP2024/013388
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-06-28
- Filing Date
- 2024-03-29
- Publication Date
- 2024-10-03
AI Technical Summary
Existing power storage devices face challenges in achieving reliable sealing between the lid and exterior film due to dimensional mismatches, leading to poor sealing performance and potential leakage or moisture ingress.
The implementation of a seal reinforcement portion, composed of a mixture of resin, metal, ceramics, and rubber, is used to enhance the sealing between the lid and exterior film, covering areas where the seal portion is not formed, and specifically designed to cover corners and ridgelines of the electrode body, ensuring improved sealing performance.
This solution effectively enhances the sealing performance between the lid and exterior film, preventing leakage and moisture ingress, even in cases of dimensional mismatches, thereby improving the reliability and durability of the power storage device.
Smart Images

Figure JP2024013388_03102024_PF_FP_ABST
Abstract
Description
Electricity storage device and manufacturing method thereof
[0001] The present invention relates to an electricity storage device and a method for manufacturing the same.
[0002] Patent Document 1 discloses an all-solid-state battery as an example of an electricity storage device. This all-solid-state battery includes an electrode body, an electrode terminal, and an exterior body that seals the electrode body. The exterior body includes an exterior film that is wrapped around the electrode body to have an opening, and a lid body that is placed in the opening. One end of the electrode terminal is electrically connected to the electrode body. The other end of the electrode terminal is exposed to the outside of the lid body. The electrode terminal penetrates the lid body. The side of the lid body and the exterior film are bonded via a sealant layer or an adhesive layer formed thereon.
[0003] Japanese Patent Application Laid-Open No. 2019-153504
[0004] In an electricity storage device such as that described in Patent Document 1, from the viewpoint of ensuring a reliable seal between the lid and the exterior film, it is preferable that the dimensions of the side of the lid and the dimensions of the exterior film facing the side of the lid match. However, in reality, there may be a difference between the dimensions of the two, and such a difference may lead to a poor seal between the lid and the exterior film. This fact is not taken into consideration in Patent Document 1.
[0005] An object of the present invention is to provide an electricity storage device with improved sealing performance between a lid and an exterior film.
[0006] The electricity storage device according to a first aspect of the present invention comprises an electrode assembly, an exterior film, a lid, a seal portion, and a seal reinforcement portion. The exterior film wraps the electrode assembly to form an opening and has a first seal area. The lid is disposed in the opening and has a second seal area facing the first seal area. The seal portion is formed between the first seal area and the second seal area and at least partially seals between the first seal area and the second seal area. The seal reinforcement portion reinforces the sealing provided by the seal area.
[0007] An electric storage device according to a second aspect of the present invention is an electric storage device according to the first aspect, wherein the material forming the seal reinforcement portion includes at least one of resin, metal, ceramic, and rubber, a mixture of at least two of these, and a composite of at least two of these.
[0008] An electric storage device according to a third aspect of the present invention is an electric storage device according to the first or second aspect, wherein the seal reinforcement portion is formed between the first seal area and the second seal area, at least in a portion where the seal portion is not formed.
[0009] An electric storage device according to a fourth aspect of the present invention is an electric storage device according to any one of the first to third aspects, wherein the lid body has a polygonal shape with an apex when viewed from the front, and the seal reinforcement portion is formed so as to at least partially cover at least one apex of the polygonal shape of the lid body from the outside.
[0010] An energy storage device according to a fifth aspect of the present invention is an energy storage device according to any one of the first to fourth aspects, wherein the seal reinforcement portion covers at least a portion of the first seal area and at least a portion of the second seal area from the outside of the exterior film and the lid body.
[0011] An electricity storage device according to a sixth aspect of the present invention is an electricity storage device according to any one of the first to fifth aspects, wherein the electrode body has a three-dimensional shape including a plurality of corners, and the seal reinforcement portion covers at least one of the plurality of corners from the outside of the exterior film.
[0012] An electricity storage device according to a seventh aspect of the present invention is an electricity storage device according to any one of the first to sixth aspects, wherein the electrode body has a three-dimensional shape including two surfaces that intersect with each other and a ridge portion formed by the two surfaces, and the seal reinforcement portion covers the ridge portion from the outside of the exterior film.
[0013] A manufacturing method for an energy storage device according to an eighth aspect of the present invention includes preparing an electrode body, wrapping the electrode body with an exterior film having a first sealing area so as to form an opening, arranging a lid body having a second sealing area at the opening so that the second sealing area faces the first sealing area, forming a sealing portion between the first sealing area of the exterior film and the second sealing area of the lid body to at least partially seal the space between the first sealing area and the second sealing area, and forming a sealing reinforcement portion between the first sealing area and the second sealing area at least in a portion where the sealing portion is not formed to reinforce the sealing portion.
[0014] A manufacturing method for an energy storage device according to a ninth aspect of the present invention includes preparing an electrode body, wrapping the electrode body with an exterior film having a first sealing area so as to form an opening, placing a lid body having a second sealing area at the opening so that the second sealing area faces the first sealing area, forming a seal portion between the first sealing area of the exterior film and the second sealing area of the lid body to at least partially seal the space between the first sealing area and the second sealing area, impregnating at least a portion of the first sealing area and at least a portion of the second sealing area with a material in a fluid state, and solidifying the material in a fluid state to form a seal reinforcement portion that reinforces the seal portion.
[0015] A manufacturing method for an energy storage device according to a tenth aspect of the present invention includes preparing an electrode body, wrapping the electrode body in an exterior film having a first sealing area so as to form an opening, arranging a lid body having a second sealing area at the opening so that the second sealing area faces the first sealing area, forming a sealing portion between the first sealing area of the exterior film and the second sealing area of the lid body that at least partially seals the space between the first sealing area and the second sealing area, preparing a reinforcing member that is configured to be attachable to the lid body and that covers at least a portion of the first sealing area and at least a portion of the second sealing area from the outside of the lid body, and attaching the reinforcing member to the lid body to form a sealing reinforcement portion that reinforces the sealing portion.
[0016] According to the present invention, an electricity storage device is provided in which the sealing performance between the lid and the exterior film is improved.
[0017] 1 is a perspective view of an electricity storage device according to a first embodiment. FIG. 2 is a perspective view of an electrode body of FIG. 1. FIG. 3 is a cross-sectional view showing the layer structure of an exterior film provided in the electricity storage device of FIG. 1. FIG. 4 is a perspective view showing a schematic structure of an end portion of an exterior film. FIG. 5 is a perspective view showing a schematic structure of a lid. FIG. 6 is a front view showing a schematic structure of the periphery of the lid. FIG. 7 is a flowchart showing a method for manufacturing an electricity storage device according to the first embodiment. FIG. 8 is a perspective view of a lid unit. FIG. 9 is a perspective view showing a schematic structure of the periphery of the lid of an electricity storage device according to a second embodiment. FIG. 10 is a diagram illustrating a method for forming a seal reinforcement part according to the second embodiment. FIG. 11 is a perspective view showing a schematic structure of the periphery of the lid of an electricity storage device according to a third embodiment. FIG. 12 is a perspective view showing a schematic structure of an electricity storage device according to a fourth embodiment. FIG. 13 is a perspective view showing a schematic structure of an electricity storage device according to a modified example. FIG. 14 is a diagram showing an example of a state in which an electricity storage device is in use.
[0018] Hereinafter, an electricity storage device according to one embodiment of the present invention will be described with reference to the drawings. Note that identical or corresponding parts in the drawings are designated by the same reference numerals, and their description will not be repeated. Furthermore, the drawings do not necessarily reflect the actual dimensions of each component. Note that, in this embodiment, a numerical range indicated by "to" means "greater than or equal to" or "less than or equal to." For example, the notation 2 to 15 mm means 2 mm or greater and 15 mm or less. In the numerical ranges described in stages in this embodiment, the upper or lower limit value described in a certain numerical range may be replaced with the upper or lower limit value of another numerical range described in stages. Furthermore, separately described upper and lower limits, upper and lower limits, or lower and lower limits may each be combined to form a numerical range.
[0019] 1. First Embodiment 1-1. Configuration of Electricity Storage Device Fig. 1 is a perspective view that schematically shows an electricity storage device 10 according to a first embodiment. The electricity storage device 10 includes an electrode body 20, a pair of electrode terminals 30, and an exterior body 40. In Fig. 1, the direction of arrow UD indicates the thickness direction of the electricity storage device 10, the direction of arrow LR indicates the width direction of the electricity storage device 10, and the direction of arrow FB indicates the depth direction of the electricity storage device 10. The directions indicated by the arrows UD, LR, and FB are the same in the subsequent figures.
[0020] [Electrode Assembly] FIG. 2 is a side view schematically illustrating the configuration of the electrode assembly 20. The electrode assembly 20 includes electrodes (positive and negative electrodes) constituting a storage member such as a lithium-ion battery, a capacitor, an all-solid-state battery, a semi-solid battery, a quasi-solid battery, a polymer battery, an all-resin battery, a lead-acid battery, a nickel-metal hydride battery, a nickel-cadmium battery, a nickel-iron battery, a nickel-zinc battery, a silver oxide-zinc battery, a metal-air battery, a polyvalent cation battery, or a capacitor, as well as a separator. In this embodiment, the electrode assembly 20 has a substantially rectangular parallelepiped shape. Note that the term "substantially rectangular parallelepiped" includes not only a perfect rectangular parallelepiped, but also a solid that can be considered a rectangular parallelepiped by modifying the shape of a portion of its outer surface, for example. However, the electrode assembly 20 may have a three-dimensional shape including multiple corners, such as a substantially polygonal prism, or may have a substantially cylindrical shape.
[0021] As shown in FIG. 2 , in this embodiment, the electrode body 20 has a front surface 21, a back surface 22, an upper surface 23, a lower surface 24, a first side surface 25, and a second side surface 26. However, the front surface 21, the back surface 22, the first side surface 25, and the second side surface 26 are imaginary surfaces when the electrode body 20 is viewed as a substantially rectangular parallelepiped. The front surface 21 faces one of the lid bodies 60. The back surface 22 faces the other lid body 60. The upper surface 23 constitutes one of the first surfaces 41 of the exterior body 40, which will be described later. The lower surface 24 constitutes the other of the pair of first surfaces 41 of the exterior body 40, which will be described later. The first side surface 25 constitutes one of the pair of second surfaces 42 of the exterior body 40, which will be described later. The second side surface 26 constitutes the other of the pair of second surfaces 42 of the exterior body 40, which will be described later. The electrode body 20 has ridge portions 20A, 20B, 20C, and 20D. Ridge portion 20A is formed at the boundary between the upper surface 23 and the first side surface 25. Ridge portion 20B is formed at the boundary between the upper surface 23 and the second side surface 26. Ridge portion 20C is formed at the boundary between the first side surface 25 and the lower surface 24. Ridge portion 20D is formed at the boundary between the second side surface 26 and the lower surface 24. In other words, a ridge portion refers to the boundary between two surfaces that intersect with each other. The ends of each of ridge portions 20A to 20D form corner portions 230 that correspond to the vertices of a substantially rectangular parallelepiped.
[0022] [Exterior Body] The exterior body 40 seals the electrode body 20. The exterior body 40 includes an exterior film 50 and a pair of lid bodies 60. The exterior film 50 wraps the electrode body 20 so as to form a pair of openings 40A. In this embodiment, the exterior film 50 is wrapped around the electrode body 20 so as to form a pair of openings 40A. The exterior film 50 has a protruding portion 50X that protrudes outward from the portion wrapping the electrode body 20 when the exterior film 50 wraps around the electrode body 20. The pair of lid bodies 60 are respectively arranged on the sides of the electrode body 20 so as to close the pair of openings 40A.
[0023] For example, there is a method of forming a storage portion (recess) in the exterior film 50 through cold forming to store the electrode assembly 20. However, it is not necessarily easy to form a deep storage portion using such a method. Attempting to form a deep storage portion (recess) through cold forming (for example, a forming depth of 15 mm) increases the likelihood of pinholes or cracks occurring in the exterior film 50, resulting in a decrease in battery performance. On the other hand, in the present embodiment, the exterior body 40 seals the electrode assembly 20 by wrapping the exterior film 50 around the electrode assembly 20, and therefore can easily seal the electrode assembly 20 regardless of the thickness of the electrode assembly 20. Note that in order to reduce the dead space between the electrode assembly 20 and the exterior film 50 to improve the volumetric energy density of the power storage device 10 and to improve cooling efficiency, it is preferable that the exterior film 50 be wrapped so as to contact the outer surface of the electrode assembly 20. Furthermore, in an all-solid-state battery, it is necessary to apply a high pressure uniformly from the outer surface of the battery in order to exert battery performance, and therefore it is necessary to eliminate the space between the electrode body 20 and the exterior film 50. Therefore, it is preferable that the exterior film 50 is wrapped around the electrode body 20 so as to contact the outer surface of the electrode body 20.
[0024] [Exterior Film] Fig. 3 is a cross-sectional view showing the layer structure of the exterior film 50. As shown in Fig. 3, the exterior film 50 is a laminate (laminate film) having, for example, a base material layer 51, a barrier layer 52, and a heat-sealable resin layer 53 in this order. Note that the exterior film 50 does not need to include all of these layers, and for example, it may not include the barrier layer 52. In other words, the exterior film 50 only needs to be made of a flexible and easily bendable material, and may be made of, for example, a resin film. Note that the exterior film 50 is preferably heat-sealable.
[0025] The substrate layer 51 included in the exterior film 50 is a layer that imparts heat resistance to the exterior film 50 and suppresses the occurrence of pinholes that may occur during processing or distribution. The substrate layer 51 is composed of, for example, at least one layer of a stretched polyester resin layer and a stretched polyamide resin layer. For example, by including at least one layer of a stretched polyester resin layer and a stretched polyamide resin layer in the substrate layer 51, the barrier layer 52 can be protected during processing of the exterior film 50 and breakage of the exterior film 50 can be suppressed. Furthermore, from the viewpoint of increasing the tensile elongation of the exterior film 50, the stretched polyester resin layer is preferably a biaxially stretched polyester resin layer, and the stretched polyamide resin layer is preferably a biaxially stretched polyamide resin layer. Furthermore, from the viewpoint of excellent puncture strength or impact strength, the stretched polyester resin layer is more preferably a biaxially stretched polyethylene terephthalate (PET) film, and the stretched polyamide resin layer is more preferably a biaxially stretched nylon (ONy) film. The substrate layer 51 may be composed of both a stretched polyester resin layer and a stretched polyamide resin layer. From the viewpoint of film strength, the thickness of the substrate layer 51 is preferably, for example, 5 to 300 μm, and more preferably 20 to 150 μm.
[0026] The barrier layer 52 is a layer that prevents at least moisture penetration. The barrier layer 52 is bonded to the substrate layer 51 via, for example, an adhesive layer 54. Examples of the barrier layer 52 include metal foils, vapor-deposited films, and resin layers with barrier properties. Vapor-deposited films include metal vapor-deposited films, inorganic oxide vapor-deposited films, and carbon-containing inorganic oxide vapor-deposited films. Resin layers include fluorine-containing resins such as polyvinylidene chloride, polymers based on chlorotrifluoroethylene (CTFE), polymers based on tetrafluoroethylene (TFE), polymers having fluoroalkyl groups, and polymers based on fluoroalkyl units, as well as ethylene-vinyl alcohol copolymers. The barrier layer 52 may also be a resin film having at least one of these vapor-deposited films and resin layers. The barrier layer 52 may be formed of multiple layers. The barrier layer 52 preferably includes a layer made of a metal material. Specific examples of the metal material constituting the barrier layer 52 include aluminum alloys, stainless steel, titanium steel, and steel plates. When used as a metal foil, it is preferable that the metal material contains at least one of an aluminum alloy foil and a stainless steel foil.
[0027] In the barrier layer 52, the layer made of the aforementioned metal material may contain recycled metal material. Examples of recycled metal material include recycled aluminum alloy, stainless steel, titanium steel, and steel plate. These recycled materials can be obtained by known methods. Recycled aluminum alloy material can be obtained, for example, by the manufacturing method described in International Publication No. 2022 / 092231. The barrier layer 52 may be made of recycled material alone, or may be made of a mixture of recycled and virgin material. Note that recycled metal material refers to metal material that has been made reusable by collecting, isolating, and refining various products used in the market or waste from manufacturing processes. Furthermore, virgin metal material refers to new metal material refined from natural metal resources (raw materials) and is not recycled material.
[0028] From the viewpoint of improving the formability or conformability of the exterior film 50, the aluminum alloy foil is preferably a soft aluminum alloy foil made of, for example, an annealed aluminum alloy, and from the viewpoint of further improving the formability or conformability, an aluminum alloy foil containing iron is preferable. In the aluminum alloy foil containing iron (100% by mass), the iron content is preferably 0.1 to 9.0% by mass, and more preferably 0.5 to 2.0% by mass. By having an iron content of 0.1% by mass or more, an exterior film 50 with better formability can be obtained. By having an iron content of 9.0% by mass or less, an exterior film 50 with better flexibility can be obtained. Examples of soft aluminum alloy foils include aluminum alloy foils having a composition specified in JIS H4160:1994 A8021H-O, JIS H4160:1994 A8079H-O, JIS H4000:2014 A8021P-O, or JIS H4000:2014 A8079P-O. Silicon, magnesium, copper, manganese, and the like may also be added as needed. Softening can be achieved by annealing or other methods. From the perspective of improving the mechanical strength of the exterior film 50, the aluminum alloy foil is preferably a hard aluminum alloy foil made of, for example, a work-hardened aluminum alloy. Examples of hard aluminum alloy foils include aluminum alloy foils having a composition defined by JIS H4160:1994 A8021H-H18, JIS H4160:1994 A8079H-H18, JIS H4000:2014 A8021P-H14, or JIS H4000:2014 A8079P-H14.
[0029] Examples of the stainless steel foil include austenitic, ferritic, austenitic-ferritic, martensitic, and precipitation hardened stainless steel foils. Furthermore, from the viewpoint of providing an exterior film 50 with excellent formability, the stainless steel foil is preferably made of austenitic stainless steel.
[0030] Specific examples of austenitic stainless steels that form the stainless steel foil include SUS304, SUS301, and SUS316L, with SUS304 being particularly preferred.
[0031] In the case of a metal foil, the thickness of the barrier layer 52 should be sufficient to at least function as a barrier layer that prevents moisture penetration, and may be, for example, approximately 5 to 200 μm. The thickness of the barrier layer 52 is preferably approximately 85 μm or less, more preferably approximately 50 μm or less, even more preferably approximately 40 μm or less, and particularly preferably approximately 35 μm or less. The thickness of the barrier layer 52 is preferably approximately 9.0 μm or more, more preferably approximately 20 μm or more, and more preferably approximately 25 μm or more. Preferred ranges for the thickness of the barrier layer 52 include about 9.0 to 85 μm, about 9.0 to 50 μm, about 9.0 to 40 μm, about 9.0 to 35 μm, about 20 to 85 μm, about 20 to 50 μm, about 20 to 40 μm, about 20 to 35 μm, about 25 to 85 μm, about 25 to 50 μm, about 25 to 40 μm, and about 25 to 35 μm. When the barrier layer 52 is made of aluminum alloy foil, the above-mentioned ranges are particularly preferred. From the viewpoint of imparting high formability and high rigidity to the exterior film 50, the thickness of the barrier layer 52 is preferably about 35 μm or more, more preferably about 45 μm or more, even more preferably about 50 μm or more, and even more preferably about 55 μm or more, and is preferably about 200 μm or less, more preferably about 85 μm or less, even more preferably about 75 μm or less, and even more preferably about 70 μm or less. Preferred ranges are approximately 35 to 200 μm, approximately 35 to 85 μm, approximately 35 to 75 μm, approximately 35 to 70 μm, approximately 45 to 200 μm, approximately 45 to 85 μm, approximately 45 to 75 μm, approximately 45 to 70 μm, approximately 50 to 200 μm, approximately 50 to 85 μm, approximately 50 to 75 μm, approximately 50 to 70 μm, approximately 55 to 200 μm, approximately 55 to 85 μm, approximately 55 to 75 μm, and approximately 55 to 70 μm. The high formability of the exterior film 50 facilitates deep drawing, which can contribute to increasing the capacity of the electricity storage device. Furthermore, while increasing the capacity of the electricity storage device increases the weight of the electricity storage device, increasing the rigidity of the exterior film 50 can contribute to high sealing performance of the electricity storage device.In particular, when the barrier layer 52 is made of stainless steel foil, the thickness of the stainless steel foil is preferably about 60 μm or less, more preferably about 50 μm or less, even more preferably about 40 μm or less, even more preferably about 30 μm or less, and particularly preferably about 25 μm or less. The thickness of the stainless steel foil is preferably about 10 μm or more, more preferably about 15 μm or more. Preferred ranges for the thickness of the stainless steel foil include about 10 to 60 μm, about 10 to 50 μm, about 10 to 40 μm, about 10 to 30 μm, about 10 to 25 μm, about 15 to 60 μm, about 15 to 50 μm, about 15 to 40 μm, about 15 to 30 μm, and about 15 to 25 μm.
[0032] Furthermore, when the barrier layer 52 is a metal foil, it is preferable that a corrosion-resistant coating be provided on at least the surface opposite the substrate layer 51 to prevent dissolution and corrosion. The barrier layer 52 may be provided with a corrosion-resistant coating on both sides. Here, the corrosion-resistant coating refers to a thin film that is provided with corrosion resistance (e.g., acid resistance, alkali resistance, etc.) by performing, for example, a hydrothermal conversion treatment such as boehmite treatment, a chemical conversion treatment, an anodizing treatment, a plating treatment of nickel or chromium, or a corrosion prevention treatment such as applying a coating agent on the surface of the barrier layer 52. Specifically, the corrosion-resistant coating refers to a coating that improves the acid resistance of the barrier layer 52 (acid-resistant coating), a coating that improves the alkali resistance of the barrier layer 52 (alkali-resistant coating), or the like. The corrosion-resistant coating may be formed by one type of treatment or a combination of two or more types. Furthermore, the barrier layer 52 may be formed not only as a single layer but also as a multi-layer. Furthermore, among these treatments, hydrothermal conversion treatment and anodizing treatment are treatments in which the surface of the metal foil is dissolved with a treatment agent to form a metal compound with excellent corrosion resistance. Note that these treatments may also be included in the definition of chemical conversion treatment. Furthermore, if the barrier layer 52 has a corrosion-resistant coating, the corrosion-resistant coating is also included in the barrier layer 52.
[0033] The corrosion-resistant coating prevents delamination between the barrier layer 52 (e.g., aluminum alloy foil) and the substrate layer 51 during molding of the exterior film 50, prevents dissolution and corrosion of the surface of the barrier layer 52 due to hydrogen fluoride produced by a reaction between an electrolyte and water, and in particular prevents dissolution and corrosion of aluminum oxide present on the surface of the barrier layer 52 when the barrier layer 52 is an aluminum alloy foil, and also improves the adhesion (wettability) of the surface of the barrier layer 52, thereby preventing delamination between the substrate layer 51 and the barrier layer 52 during heat sealing and between the substrate layer 51 and the barrier layer 52 during molding.
[0034] The heat-sealable resin layer 53 is bonded to the barrier layer 52 via, for example, an adhesive layer 55. The heat-sealable resin layer 53 included in the exterior film 50 is a layer that imparts heat-sealing properties to the exterior film 50. Examples of the heat-sealable resin layer 53 include resin films made of polyester resins such as polyethylene terephthalate resins and polybutylene terephthalate resins, polyolefin resins such as polyethylene resins and polypropylene resins, cyclic polyolefin resins, or acid-modified polyolefin resins obtained by graft-modifying these polyolefin resins with an acid such as maleic anhydride. From the standpoint of sealability and strength, the thickness of the heat-sealable resin layer 53 is preferably, for example, 20 to 300 μm, and more preferably 40 to 150 μm.
[0035] The exterior film 50 preferably has one or more layers having a buffer function (hereinafter referred to as "buffer layer") outside the heat-sealable resin layer 53, more preferably outside the barrier layer 52. The buffer layer may be laminated on the outside of the base material layer 51, or the base material layer 51 may also function as a buffer layer. When the exterior film 50 has multiple buffer layers, the multiple buffer layers may be adjacent to each other, or may be laminated with the base material layer 51, the barrier layer 52, or the like interposed therebetween.
[0036] The material constituting the buffer layer can be arbitrarily selected from materials having cushioning properties. Examples of the material having cushioning properties include rubber, nonwoven fabric, and foam sheet. Examples of rubber include natural rubber, fluororubber, and silicone rubber. The rubber hardness is preferably about 20 to 90. The material constituting the nonwoven fabric is preferably a material having excellent heat resistance. When the buffer layer is made of nonwoven fabric, the lower limit of the thickness of the buffer layer is preferably 100 μm, more preferably 200 μm, and even more preferably 1000 μm. When the buffer layer is made of nonwoven fabric, the upper limit of the thickness of the buffer layer is preferably 5000 μm, and even more preferably 3000 μm. The thickness of the buffer layer is preferably in the range of 100 μm to 5000 μm, 100 μm to 3000 μm, 200 μm to 5000 μm, 200 μm to 3000 μm, 1000 μm to 5000 μm, or 1000 μm to 3000 μm, with the most preferred range being 1000 μm to 3000 μm.
[0037] When the buffer layer is made of rubber, the lower limit of the thickness of the buffer layer is preferably 0.5 mm. When the buffer layer is made of rubber, the upper limit of the thickness of the buffer layer is preferably 10 mm, more preferably 5 mm, and even more preferably 2 mm. When the buffer layer is made of rubber, the preferred range of the thickness of the buffer layer is 0.5 mm to 10 mm, 0.5 mm to 5 mm, or 0.5 mm to 2 mm.
[0038] When the exterior film 50 has a buffer layer, the buffer layer functions as a cushion, thereby preventing the exterior film 50 from being damaged by impact when the energy storage device 10 is dropped or by handling during manufacturing of the energy storage device 10.
[0039] In this embodiment, the first sealed portion 70 is formed by heat-sealing the opposing surfaces (heat-fusible resin layers 53) of the exterior film 50 wrapped around the electrode body 20 and the lid body 60. In this embodiment, the first sealed portion 70 extends in the longitudinal direction (FB direction) of the exterior body 40. The position on the exterior body 40 where the first sealed portion 70 is formed can be selected arbitrarily. In this embodiment, the base 70X of the first sealed portion 70 is located on the edge 43 at the boundary between the first surface 41 and the second surface 42 of the exterior body 40. The first surface 41 has a larger area than the second surface 42. The base 70X of the first sealed portion 70 may be located on any surface of the exterior body 40. In this embodiment, the first sealed portion 70 is folded, for example, toward the second surface 42 of the exterior body 40. The first sealing portion 70 may protrude outward beyond the electrode body 20 in a plan view, or may be folded toward the first surface 41 .
[0040] FIG. 4 is a perspective view showing a schematic configuration of the end portion of the exterior film 50 in the FB direction. As shown in FIG. 4, the exterior film 50 has a first sealing region 500. The first sealing region 500 is a virtual region present in the peripheral portion of the opening 40A. The heat-sealable resin located in the first sealing region 500 is heat-sealed with a lid seal portion 63 of the lid body 60, which will be described later, to form the second sealing portion 80. Preferably, the first sealing region 500 includes a peripheral portion 5000 that defines the periphery of the opening 40A. The second sealing portion 80 is an example of a sealing portion of the present invention. Note that while FIG. 4 shows only one end portion of the exterior film 50 in the FB direction, the other end portion of the exterior film 50 in the FB direction also has a first sealing region 500.
[0041] [Lid] Fig. 5 is a perspective view showing a schematic configuration of the lid 60. The lid 60 is a member arranged to close the opening 40A, and is, for example, a plate-like member having a polygonal shape when viewed from the FB direction of the power storage device 10. The lid 60 is made of, for example, resin. The lid 60 may be formed by, for example, cold-forming the exterior film 50. Alternatively, the lid 60 may be a metal molded product. Furthermore, the material constituting the lid 60 may include at least one of metal, metal oxide, carbon fiber reinforced plastic, and rubber.
[0042] The lid body 60 has a first surface 61, a second surface 62, and a lid seal portion 63. The first surface 61 faces the electrode body 20. The second surface 62 is the surface opposite to the first surface 61. The lid seal portion 63 is connected to the first surface 61 and the second surface 62, and is heat-sealed to the heat-fusible resin layer 53 of the exterior film 50 to form a second sealing portion 80. In other words, the lid seal portion 63 is an example of the second sealing region of the present invention.
[0043] The lid seal portion 63 includes a first seal surface 63A, a second seal surface 63B, a third seal surface 63C, and a fourth seal surface 63D. The first seal surface 63A constitutes the upper surface of the lid body 60. The first seal surface 63A extends in a first direction (the LR direction in this embodiment) in a front view of the lid body 60. The second seal surface 63B and the third seal surface 63C are connected to the first seal surface 63A and constitute the side surfaces of the lid body 60. The second seal surface 63B and the third seal surface 63C extend in a second direction (the UD direction in this embodiment) that intersects with the first direction in a front view of the lid body 60. In this embodiment, the first direction and the second direction are orthogonal in a front view of the lid body 60. The first direction and the second direction do not have to be orthogonal in a front view of the lid body 60. The fourth seal surface 63D constitutes the lower surface of the lid body 60. The fourth sealing surface 63D extends in a first direction (the LR direction in this embodiment) when the lid 60 is viewed from the front.
[0044] When the lid body 60 is plate-shaped, it is preferable that the lid body 60 have a certain thickness so that deformation of the exterior body 40 is suppressed even when the power storage device 10 is placed on top of it. From another perspective, when the lid body 60 is plate-shaped, it is preferable that the lid seal portion 63 of the lid body 60 have a certain thickness so that the lid seal portion 63 of the lid body 60 and the exterior film 50 can be suitably heat-sealed when forming the second sealing portion 80. The minimum thickness of the lid body 60 is, for example, 1.0 mm, more preferably 3.0 mm, and even more preferably 4.0 mm. The maximum thickness of the lid body 60 is, for example, 20 mm, more preferably 15 mm, and even more preferably 12 mm. Preferred ranges for the thickness of the material constituting the lid body 60 are 1.0 mm to 20 mm, 1.0 mm to 15 mm, 1.0 mm to 12 mm, 3.0 mm to 20 mm, 3.0 mm to 15 mm, 3.0 mm to 12 mm, 4.0 mm to 20 mm, 4.0 mm to 15 mm, and 4.0 mm to 12 mm. In this embodiment, when the lid body 60 is described as being plate-shaped, this does not include embodiments in which the lid body 60 is composed solely of a film as defined by the JIS (Japanese Industrial Standards) [Packaging Terminology] standard. The thickness of the lid body 60 may vary depending on the region of the lid body 60. When the thickness of the lid body 60 varies depending on the region, the thickness of the lid body 60 is the thickness of the thickest portion.
[0045] The lid seal portion 63 further includes boundaries 64, 65, 66, and 67. The boundary 64 is the boundary between the first seal surface 63A and the second seal surface 63B. The boundary 65 is the boundary between the first seal surface 63A and the third seal surface 63C. The boundary 66 is the boundary between the fourth seal surface 63D and the second seal surface 63B. The boundary 67 is the boundary between the fourth seal surface 63D and the third seal surface 63C. In other words, the boundaries 64 to 67 form the top of the lid 60. The shapes of the boundaries 64 to 67 may be angular, or may be rounded by applying a rounding process. In this embodiment, the boundaries 64 to 67 are angular.
[0046] From the viewpoint of appropriately heat-sealing the lid 60 and the exterior film 50, it is preferable that the material constituting the lid 60 and the material constituting the heat-sealable resin layer 53 of the exterior film 50 are primarily made of the same material. In this embodiment, the materials constituting the lid 60 and the heat-sealable resin layer 53 are primarily made of polypropylene. That is, the second sealing portion 80 according to this embodiment is formed primarily from polypropylene. Note that the "primary material" refers to a material that accounts for 50% by mass or more, preferably 80% by mass or more, more preferably 90% by mass or more, and even more preferably 95% by mass or more, when the total mass of the materials contained in the constituent elements is taken as 100% by mass.
[0047] In the present embodiment, the lid body 60 has a through hole 60X formed therein, into which an electrode terminal 30 (described later) is inserted. The through hole 60X penetrates the first surface 61 and the second surface 62. When the electrode body 20 is stored, the electrode terminal 30 passes through the through hole 60X formed in the lid body 60 and protrudes to the outside of the exterior body 40. A small gap between the through hole 60X of the lid body 60 and the electrode terminal 30 is filled with, for example, resin. Note that, in the energy storage device 10, the position from which the electrode terminal 30 protrudes to the outside can be selected arbitrarily. For example, the electrode terminal 30 may protrude to the outside from a hole formed in any one of the six surfaces of the exterior body 40. In this case, a small gap between the exterior body 40 and the electrode terminal 30 is filled with, for example, resin. In the energy storage device 10, the lid body 60 and the electrode terminal 30 are provided as separate bodies; however, the lid body 60 and the electrode terminal 30 may be integrally formed. If the electrode terminals 30 do not protrude from the edge of the exterior body 40, the lid body 60 does not need to have the through-holes 60X formed therein.
[0048] [Electrode Terminals] Referring again to FIG. 1 , the power storage device 10 according to this embodiment includes a pair of electrode terminals 30. The electrode terminals 30 are metal terminals used for inputting and outputting electric power to and from the electrode body 20. One end of the electrode terminal 30 is electrically connected to the electrode body 20 (positive electrode or negative electrode). The other end of the electrode terminal 30 protrudes outward from, for example, an edge of the exterior body 40. Note that the electrode terminals 30 may be any terminal as long as they are capable of inputting and outputting electric power to and from the electrode body 20, and may not, for example, protrude from the exterior body 40. When the lid body 60 described below is made of, for example, metal, the lid body 60 may also function as the electrode terminals 30. In this case, the lid body 60, which functions as an electrode terminal, may or may not protrude from the exterior body 40.
[0049] The metal material constituting the electrode terminal 30 is, for example, aluminum, nickel, copper, etc. For example, when the electrode body 20 is a lithium ion battery, the electrode terminal 30 connected to the positive electrode is usually made of aluminum, etc., and the electrode terminal 30 connected to the negative electrode is usually made of copper, nickel, etc.
[0050] [Seal reinforcement portion] Fig. 6 is a front view showing the configuration around the lid body 60. As shown in Fig. 6, the electricity storage device 10 further includes one or more seal reinforcement portions 90. The seal reinforcement portion 90 is a portion that reinforces the sealing by the second sealing portion 80. In the example shown in Fig. 6, the seal reinforcement portion 90 is formed between the first sealing region 500 of the exterior film 50 and the lid seal portion 63 (second sealing region) of the lid body 60, at least in a portion where the second sealing portion 80 is not formed. The portion where the second sealing portion 80 is not formed may be one location or two or more locations.
[0051] The second sealing portion 80 is formed by arranging the lid seal portion 63 and the first sealing region 500 face to face and wrapping the entire lid seal portion 63 in the exterior film 50. At this time, the length of the exterior film 50 wrapping the lid seal portion 63 (i.e., the circumferential length of the lid body 60) may not match the length of the exterior film 50, resulting in sagging portions in the exterior film 50. In the example of FIG. 6 , the sagging portions are indicated by reference numerals 501 and 502. For ease of explanation, the size of the sagging portions 501 and 502 is emphasized in FIG. 6 , but the sagging portions 501 and 502 do not necessarily protrude beyond the surface of the exterior film 50 that forms the second sealing portion 80. In the sagging portions 501 and 502 of the exterior film 50, the heat-sealable resin of the lid seal portion 63 and the heat-sealable resin of the first sealing region 500 do not make sufficient contact, resulting in unsealed portions where the second sealing portion 80 is not formed. If such an unsealed portion exists, when the electrode body 20 contains an electrolyte, the electrolyte may leak out of the exterior body 40 or at least one of gas and moisture may penetrate into the interior of the exterior body 40, which may have an undesirable effect on the performance of the electricity storage device 10. The seal reinforcement portion 90 compensates for the unsealed portion that may cause a decrease in performance of the electricity storage device 10, thereby improving the seal between the lid body 60 and the exterior film 50. Note that the unsealed portion is not necessarily limited to one caused by sagging of the exterior film 50, but may also be one caused by other factors or one that has been intentionally formed, for example, for reasons of convenience in manufacturing.
[0052] In the example shown in FIG. 6 , two seal reinforcements 90 are formed in the sagging portions 501 and 502 to fill the gap between the lid seal portion 63 and the first sealing region 500. The seal reinforcement 90 formed in the sagging portion 501 more effectively improves the seal between the lid body 60 and the exterior film 50 compared to the seal reinforcement 90 formed in the sagging portion 502. The sagging portion 501 is located closer to the protruding portion 50X (first sealing portion 70). Because the protruding portion 50X is movable relative to the base 70X of the first sealing portion 70, a greater load is applied to the second sealing portion 80 near the base 70X than in other portions. In other words, there is a greater need to reinforce the seal provided by the second sealing portion 80 near the base 70X. Therefore, it can be said that a seal reinforcement portion 90 formed closer to the base 70X is more effective in improving the sealing between the lid body 60 and the outer casing film 50 than a seal reinforcement portion 90 formed further distal to the base 70X.
[0053] The seal reinforcement portion 90 is formed by the method described below. The material forming the seal reinforcement portion 90 includes, for example, at least one of resin, metal, ceramic, and rubber. The material also includes, for example, a mixture of at least two of resin, metal, ceramic, and rubber, and a composite of at least two of resin, metal, ceramic, and rubber. The composite includes, for example, a composite formed by bonding different materials at the molecular level. The resin includes at least one of thermoplastic resin, photocurable resin, room-temperature curable resin, thermosetting resin, and electron beam curable resin (hereinafter, these resins may be collectively referred to as "curable resin"). Examples of thermoplastic resins include polyester resins such as polyethylene terephthalate resin and polybutylene terephthalate resin, polyolefin resins such as polyethylene resin and polypropylene resin, cyclic polyolefin resin, and acid-modified polyolefin resin obtained by graft-modifying these polyolefin resins with an acid such as maleic anhydride. Photocurable resins are resins that harden when irradiated with light of a specific wavelength. Examples of photocurable resins include radical polymerization resins, which undergo radicalization of a photopolymerization initiator upon irradiation with ultraviolet light and cure through a radical chain reaction with the functional groups of a monomer or oligomer, and cationic polymerization resins, which cure through a cationic polymerization reaction upon irradiation with ultraviolet light. Examples of radical polymerization resins include acrylic resins, and examples of cationic polymerization resins include epoxy resins and vinyl ethers. Examples of room-temperature curable resins include resins based on epoxy resins, ester resins, or acrylic resins that cure when mixed with a curing agent. Examples of thermosetting resins include phenolic resins, epoxy resins, melamine resins, urea resins, unsaturated polyester resins, alkyd resins, silicone resins, polyurethanes, and thermosetting polyimides. Examples of electron beam curable resins include acrylic resins.
[0054] 7A is a flowchart showing an example of a method for manufacturing the power storage device 10. The method for manufacturing the power storage device 10 according to the first embodiment will be described below. However, the order in which steps S1 to S8 are performed is not limited to the following order and can be changed as appropriate.
[0055] In step S1, each element of the electricity storage device 10 is prepared. Specifically, the electrode body 20, the pair of electrode terminals 30, the exterior film 50, and the pair of lid bodies 60 are prepared.
[0056] In step S2, each electrode terminal 30 is joined to the lid body 60. In the present embodiment, each electrode terminal 30 is joined to the lid body 60 so as to protrude toward the second surface 62 through the through hole 60X. Here, the gap between the peripheral surface of the electrode terminal 30 and the inner wall surface of the through hole 60X of the lid body 60 may be filled with resin. Completion of step S2 results in the creation of a lid unit 600 (see FIG. 7B ) in which the electrode terminal 30 is joined to the lid body 60.
[0057] In step S3, the lid unit 600 is placed so as to face the front surface 21 and rear surface 22 of the electrode body 20, and the electrode terminals 30 and the electrode body 20 are joined together.
[0058] Alternatively, the manufacturing method for the electricity storage device 10 may include, instead of steps S2 and S3, a step of first joining the electrode body 20 and the electrode terminal 30, and then joining the lid body 60 to the electrode terminal 30 joined to the electrode body 20. In this example, the electrode terminal 30 may protrude to the outside of the exterior body 40 from between any one of the sealing surfaces 63A to 63D and the exterior film 50.
[0059] In step S4, the electrode body 20 is wrapped in the exterior film 50 so as to form a pair of openings 40A. The method for wrapping the electrode body 20 is not particularly limited, and for example, the exterior film 50 may be wrapped around the electrode body 20 and the lid body 60. At this time, the portion of the exterior film 50 located on the periphery of the opening 40A becomes the first sealing region 500. As a result, the first sealing region 500 faces the lid seal portions 63 of the pair of lid bodies 60.
[0060] In step S5, the opposing heat-sealable resin layers 53 of the exterior film 50 are heat-sealed to form a first sealed portion 70 (hereinafter referred to as a "temporary first sealed portion") having a partial unsealed portion. The unsealed portion can be formed, for example, by using a sealing bar shaped so that a portion of the bar does not come into contact with the exterior film 50. In another example, the unsealed portion can be formed by interposing a fluororesin film or the like between the opposing surfaces (heat-sealable resin layers 53) of the exterior film 50. By forming the temporary first sealed portion before the second sealed portion 80, the electrode body 20 can be held by the exterior film 50, making it less likely for the electrode body 20 to shift position relative to the exterior film 50. This reduces the occurrence of wrinkles when forming the second sealed portion 80.
[0061] In step S6, the second sealed portion 80 is formed by heat-sealing the heat-fusible resin layer 53 of the first sealed region 500 of the exterior film 50 and the lid seal portion 63 of the lid body 60. Note that step S6 may be performed before step S5.
[0062] In step S7, the seal reinforcement portion 90 is formed. More specifically, in step S6, a material for forming the seal reinforcement portion 90 is injected into the portion between the first sealing region 500 and the lid seal portion 63 where the second sealing portion 80 has not been formed (the unsealed portion of the second sealing portion 80). The portion where the second sealing portion 80 has not been formed is identified, for example, by a leak test or the like. The injection of the material for forming the seal reinforcement portion 90 can be performed, for example, by injecting the material in a fluid state into the unsealed portion of the second sealing portion 80 using a nozzle or the like and then solidifying it. Alternatively, the fluidized material can be forced into the unsealed portion of the second sealing portion 80 under pressure. This forms the seal reinforcement portion 90 in the unsealed portion of the second sealing portion 80.
[0063] In step S8, an electrolyte solution is injected through the unsealed portion of the temporary first sealed portion, and aging and degassing are performed. Note that, if the power storage device 10 is an all-solid-state battery, the step of injecting the electrolyte solution through the unsealed portion of the temporary first sealed portion is omitted.
[0064] In step S9, the exterior film 50 is evacuated as necessary, and then the unsealed portion of the temporary first sealed portion is heat-sealed to form the first sealed portion 70.
[0065] <1-3. Functions and Effects of the Electricity Storage Device> According to the electricity storage device 10, even if the second sealing portion 80 is not formed between the exterior film 50 and the lid body 60 and an unsealed portion occurs in the second sealing portion 80, that portion is filled by the seal reinforcing portion 90. This makes it possible to more reliably seal the area between the exterior film 50 and the lid body 60.
[0066] [2. Second Embodiment] The power storage device 10A of the second embodiment differs from the first embodiment in the configuration and formation method of the seal reinforcement portion 90A, but the other configurations are the same as those of the first embodiment. The following describes the power storage device 10A of the second embodiment, focusing on the differences from the first embodiment.
[0067] 2-1. Configuration of the Electricity Storage Device FIG. 8 is a perspective view showing the configuration of the periphery of the lid body 60 of the electricity storage device 10A of the second embodiment (however, the electrode terminals 30 are omitted from the illustration). As shown in FIG. 8, in the electricity storage device 10A, a seal reinforcement portion 90A (the shaded portion in FIG. 8) entirely covers the first seal area 500 and the second seal area (the lid seal portion 63 of the lid body 60) from the outside of the exterior film 50, and further entirely covers the second surface 62 of the lid body 60. Preferably, the seal reinforcement portion 90A extends in the F-B direction of the electricity storage device 10A and reaches the position on the outer surface of the exterior film 50 where the corner 230 of the electrode body 20 is located. In other words, the seal reinforcement portion 90A preferably covers at least one of the multiple corners 230 of the electrode body 20 from the outside of the exterior film 50. Note that while FIG. 8 only shows the configuration of the periphery of one lid body 60, the configuration of the periphery of the other lid body 60 is similar.
[0068] 8, the seal reinforcement portion 90A is formed to a range that reaches a portion of the protruding portion 50X. When the seal reinforcement portion 90A is formed to reach at least a portion of the protruding portion 50X, the seal reinforcement portion 90A can also reinforce the protruding portion 50X, particularly its base. However, the seal reinforcement portion 90A may be formed excluding the protruding portion 50X.
[0069] The material for forming the seal reinforcement portion 90A may be the same as the material for forming the seal reinforcement portion 90.
[0070] <2-2. Manufacturing method of electricity storage device> The manufacturing method of the electricity storage device 10A according to the second embodiment differs from the manufacturing method of the electricity storage device 10 in the method of forming the seal reinforcement portion 90. That is, the manufacturing method of the electricity storage device 10A differs from the manufacturing method of the electricity storage device 10 in the specific content of step S7. This will be described below.
[0071] FIG. 9 is a diagram illustrating a method for forming the seal reinforcement portion 90A shown in FIG. 8 . The container 990 shown in FIG. 9 is a container capable of housing the lid body 60 and its periphery, and may be, for example, a flexible container made of silicone resin. First, the lid body 60 and its periphery on one side of the power storage device 10A assembled in the processes up to step S6 are housed in the container 990. A material 91 (in a fluid state) for forming the seal reinforcement portion 90A is poured into the container 990, and the lid body 60, including the entire first sealing region 500 and the entire second sealing region (lid seal portion 63), is impregnated with the material 91. Next, after the material 91 solidifies, the lid body 60 and the like are removed from the container 990, and excess material 91 is removed. According to this method, the first sealing region 500 and the lid seal portion 63, including the unsealed portion of the second sealing portion 80, are externally covered by the seal reinforcement portion 90A. By making the depth of the container 990 longer than the distance from the second surface 62 of the lid body 60 to the front surface 21 or back surface 22 of the electrode body 20 facing it, a seal reinforcement portion 90A can be formed to cover at least one of the corner portions 230 from the outside of the exterior film 50.
[0072] A slit (not shown) through which the electrode terminal 30 passes may be formed in the bottom of the container 990. In this case, when the lid 60 and its periphery are housed in the container 990, the end of the electrode terminal 30 is protruded from the slit to the outside of the bottom of the container 990, and the electrode terminal 30 is kept in close contact with the periphery of the slit, thereby preventing the electrode terminal 30 from being covered with the material 91.
[0073] <2-3. Functions and Effects of the Electricity Storage Device> According to the electricity storage device 10A of the second embodiment, even if the second sealing portion 80 is not formed between the exterior film 50 and the lid body 60 and an unsealed portion occurs, that portion is covered by the seal reinforcement portion 90A. This makes it possible to more reliably seal the area between the exterior film 50 and the lid body 60. Furthermore, if the seal reinforcement portion 90A reaches the protruding portion 50X, it can reinforce the protruding portion 50X. Furthermore, if the seal reinforcement portion 90A covers at least one corner portion 230 of the electrode body 20 from the outside of the exterior film 50, it is possible to prevent the corner portion 230 from breaking through and protruding from the exterior film 50.
[0074] When the seal reinforcement portion 90A extends onto the outer surface of the exterior film 50 so as to cover at least one of the corners 230 of the electrode assembly 20, the seal reinforcement portion 90A can be formed from a material with relatively low stretching and deformability, thereby imparting the seal reinforcement portion 90A with an additional function of suppressing deformation of the exterior body 40. In the electricity storage device 10A, the internal pressure of the electricity storage device 10A may increase due to volume changes of the positive electrode active material and negative electrode active material of the electrode assembly 20 associated with charging and discharging, as well as gas generation. When the internal pressure of the electricity storage device 10A increases, the exterior body 40 may expand. Furthermore, when vacuuming is performed in the manufacturing process of the electricity storage device 10B, the exterior body 40 may shrink. By extending onto the outer surface of the exterior film 50, the seal reinforcement portion 90A reinforces the exterior film 50 at least in that portion, thereby limiting the above-mentioned deformation of the exterior body 40.
[0075] 3. Third Embodiment An electricity storage device 10B according to a third embodiment differs from the first embodiment in the configuration and formation method of a seal reinforcement portion 90B, but the other configurations are the same as those of the first embodiment. The following describes the electricity storage device 10B according to the third embodiment, focusing on the differences from the first embodiment.
[0076] 3-1. Configuration of the Electricity Storage Device FIG. 10 is a perspective view showing the configuration around the lid body 60 of the electricity storage device 10B of the third embodiment (however, the electrode terminals 30 are omitted from the illustration). As shown in FIG. 10, in the electricity storage device 10B, a seal reinforcement portion 90B (the shaded portion in FIG. 10) covers the entire first seal area 500 and the entire second seal area (the lid seal portion 63 of the lid body 60) from the outside of the exterior film 50, and further covers the entire second surface 62 of the lid body 60. Preferably, the seal reinforcement portion 90B extends in the F-B direction of the electricity storage device 10B and reaches the position on the outer surface of the exterior film 50 where the corner 230 of the electrode body 20 is located. In other words, the seal reinforcement portion 90B preferably covers at least one of the multiple corners 230 of the electrode body 20 from the outside of the exterior film 50. Note that while FIG. 10 only shows the configuration around one lid body 60, the configuration around the other lid body 60 is similar.
[0077] Unlike the seal reinforcement portion 90A, the seal reinforcement portion 90B is formed by placing a reinforcing member formed separately from the exterior film 50 on the outside of the exterior film 50 and the lid body 60. The material forming the seal reinforcement portion 90B may include, for example, resin, metal, rubber, metal oxide, a compound of metal oxide and resin, carbon fiber reinforced plastic, etc. When the electrode body 20 contains an electrolyte, the seal reinforcement portion 90B is preferably formed including a material that is impermeable to the electrolyte or a material that is resistant to the electrolyte. Furthermore, the seal reinforcement portion 90B is preferably formed including a material that is impermeable to gas and moisture, or including a layer that is impermeable to gas and moisture.
[0078] The shape and thickness of the seal reinforcement portion 90B are not particularly limited. The seal reinforcement portion 90B may be formed, for example, in a sheet shape. In this case, for example, multiple seal reinforcement portions 90B can be bonded to the outside of the lid body 60 or the exterior film 50. The sheet-shaped seal reinforcement portion 90B can be formed, for example, from a resin film. The resin film may be a single-layer film or a multi-layer film. Furthermore, for example, the seal reinforcement portion 90B may be formed in a cap shape that can be placed over the end of the exterior body 40 from the outside of the lid body 60. The cap-shaped seal reinforcement portion 90B can be formed, for example, from rubber, a molded resin product, ceramics, metal, or a resin film (including a cold-formed product). In this way, the seal reinforcement portion 90B may be formed entirely from a single part, or may be formed from two or more parts made of the same or different materials. Furthermore, the thickness by which the seal reinforcement portion 90B covers the exterior film 50 and the lid body 60 is not particularly limited.
[0079] The seal reinforcement portion 90B may or may not be bonded to the exterior body 40 (at least one of the lid body 60 and the exterior film 50). For example, if the seal reinforcement portion 90B contains an elastic material such as rubber and is formed in a cap shape, the elasticity of the seal reinforcement portion 90B can be utilized to attach the seal reinforcement portion 90B independently to the end of the exterior body 40. On the other hand, if the seal reinforcement portion 90B is bonded to the exterior body 40, the bonding method is not particularly limited. Examples of bonding methods include interposing an adhesive between the seal reinforcement portion 90B and the exterior body 40, pouring the above-mentioned curable resin between the seal reinforcement portion 90B and the exterior body 40 and curing it, and fusing the seal reinforcement portion 90B and the exterior body 40 with a heat-sealing resin. In other words, the seal reinforcement portion 90B can be combined with the seal reinforcement portion 90 of the first embodiment or the seal reinforcement portion 90A of the second embodiment.
[0080] 10, the seal reinforcement portion 90B is formed in a portion excluding the protruding portion 50X. However, the seal reinforcement portion 90B may be formed to extend to at least a portion of the protruding portion 50X. In this way, when the seal reinforcement portion 90B is formed to extend to at least a portion of the protruding portion 50X, the seal reinforcement portion 90B can also reinforce the protruding portion 50X, particularly its base.
[0081] <3-2. Functions and Effects of the Electricity Storage Device> According to the electricity storage device 10B of the third embodiment, even if the second sealing portion 80 is not formed between the exterior film 50 and the lid body 60 and an unsealed portion occurs, that portion is covered by the seal reinforcement portion 90B. This makes it possible to more reliably seal the area between the exterior film 50 and the lid body 60. Furthermore, if the seal reinforcement portion 90B reaches the protruding portion 50X, the protruding portion 50X can be reinforced. Furthermore, if the seal reinforcement portion 90B covers at least one corner portion 230 of the electrode body 20 from the outside of the exterior film 50, it is possible to prevent the corner portion 230 from breaking through and protruding from the exterior film 50.
[0082] Furthermore, by forming the seal reinforcement portion 90B from a material with relatively low stretching and deformability, the seal reinforcement portion 90B can be given an additional function of suppressing deformation of the exterior body 40. In the electricity storage device 10B, the internal pressure of the electricity storage device 10B may increase due to volume changes in the positive electrode active material and negative electrode active material of the electrode assembly 20 caused by charging and discharging, as well as gas generation. When the internal pressure of the electricity storage device 10B increases, the exterior body 40 may expand. However, since the seal reinforcement portion 90B, which has relatively low stretching and deformability, is located outside the exterior film 50, this expansion of the exterior body 40 can be limited. Furthermore, when vacuuming is performed during the manufacturing process of the electricity storage device 10B, the exterior body 40 may shrink. When the seal reinforcement portion 90B is at least partially bonded to the exterior film 50, the seal reinforcement portion 90B reinforces the exterior film 50 in that portion, thereby limiting the shrinkage of the exterior body 40.
[0083] [4. Fourth Embodiment] An electricity storage device 10C of a fourth embodiment differs from the third embodiment in that a seal reinforcement portion 90C covers at least one of the ridge portions 20A to 20D from the outside of the exterior body 40, but other configurations are similar to those of the third embodiment. The following describes the electricity storage device 10C of the fourth embodiment, focusing on the differences from the third embodiment.
[0084] 4-1. Configuration of the Power Storage Device FIG. 11 is a perspective view showing a schematic configuration of the power storage device 10C (however, the electrode terminals 30 are omitted from the illustration). As shown in FIG. 11, in the power storage device 10C, the seal reinforcement portion 90C has two end reinforcement portions 900C that cover both end portions of the exterior body 40 in the F-B direction. The power storage device 10C of the fourth embodiment additionally has four ridge reinforcement portions 901C that cover the ridge portions 20A to 20D of the electrode body 20 from the outside of the exterior body 40. That is, the end reinforcement portions 900C each entirely cover the first seal region 500 and the second seal region (the lid seal portion 63 of the lid body 60) from the outside of the exterior film 50, and further entirely cover the second surface 62 of the lid body 60. The ridge reinforcement portions 901C each cover at least a portion of the ridge portions 20A to 20D of the electrode body 20 from the outside of the exterior body 40. In this embodiment, the ridge reinforcement portions 901C are connected to the two end reinforcement portions 900C, respectively. Materials constituting the two end reinforcement portions 900C and the ridge reinforcement portion 901C can be the same as those exemplified in the description of the seal reinforcement portion 90B of the third embodiment.
[0085] The ridge line reinforcement portion 901C is preferably formed so as to be L-shaped when viewed from the F-B direction, spanning the two surfaces that form the ridge line portions 20A to 20D. However, in the portion of the overhanging portion 50X, the ridge line reinforcement portion 901C may be formed on only one surface of the overhanging portion 50X. The ridge line reinforcement portion 901C may be formed integrally with the both-end reinforcement portions 900C, or may be formed separately from the both-end reinforcement portions 900C and joined to at least one of the outer surface of the exterior body 40 and the both-end reinforcement portions 900C. For example, when the both-end reinforcement portions 900C and the ridge line reinforcement portion 901C are formed integrally with a flexible material, the exterior body 40 with the electrode assembly 20 sealed therein can be fitted into the space defined by the both-end reinforcement portions 900C and the ridge line reinforcement portion 901C to manufacture the electricity storage device 10C including the seal reinforcement portion 90C. Furthermore, when the both-end reinforcement portions 900C and the ridge reinforcement portion 901C are formed as separate bodies, the both-end reinforcement portions 900C and the ridge reinforcement portion 901C may be combined in advance, and the exterior body 40 with the electrode assembly 20 sealed therein may be fitted into the space defined by the both-end reinforcement portions 900C and the ridge reinforcement portion 901C. Alternatively, the both-end reinforcement portions 900C and the ridge reinforcement portion 901C may be attached to the exterior body 40, and then connected. Examples of methods for connecting the both-end reinforcement portions 900C and the ridge reinforcement portion 901C include inserting a protrusion formed on one side into a recess formed on the other side, bonding them together with an adhesive, or fusing them together with a thermally adhesive resin. Alternatively, the both-end reinforcement portions 900C and the ridge reinforcement portion 901C may simply be joined to the exterior body 40, respectively. The method for joining them to the exterior body 40 is as described in the second embodiment.
[0086] As in the second embodiment, the both-end reinforcing portions 900C preferably extend in the FB direction of the electricity storage device 10B and reach positions on the outer surface of the exterior film 50 where corners 230 of the electrode body 20 are located. That is, the both-end reinforcing portions 900C preferably cover at least one of the multiple corners 230 of the electrode body 20 from the outside of the exterior film 50. However, the both-end reinforcing portions 900C may not reach positions where the corners 230 of the electrode body 20 are located, and the ridge line reinforcing portion 901C may cover at least one of the corners 230 of the electrode body 20 from the outside of the exterior film 50.
[0087] <4-2. Functions and Effects of the Electricity Storage Device> According to the electricity storage device 10C of the fourth embodiment, even if the second sealing portion 80 is not formed between the exterior film 50 and the lid body 60 and an unsealed portion occurs, that portion is covered by the two-end reinforcement portions 900C. This makes it possible to more reliably seal the area between the exterior film 50 and the lid body 60. Furthermore, when at least one of the two-end reinforcement portions 900C and the ridge reinforcement portion 901C reaches the protruding portion 50X, the protruding portion 50X can be reinforced. Furthermore, when at least one of the two-end reinforcement portions 900C and the ridge reinforcement portion 901C covers at least one corner portion 230 of the electrode body 20 from the outside of the exterior film 50, it is possible to prevent the corner portion 230 from breaking through the exterior film 50 and protruding. Furthermore, the ridge line reinforcing portion 901C covers from the outside of the exterior film 50 the portions of the ridge line portions 20A to 20D of the electrode body 20 that are not covered by the end-end reinforcing portion 900C, thereby preventing the ridge line portions 20A to 20D of the electrode body 20 from breaking through and protruding from the exterior film 50. Note that the ridge line reinforcing portion 901C does not have to be formed corresponding to all of the ridge lines of the ridge line portions 20A to 20D; the above effect can be achieved even if only one ridge line reinforcing portion 901C is formed corresponding to any one of the ridge line portions.
[0088] Furthermore, when at least one of the end reinforcements 900C and the ridge reinforcement 901C is formed of an elastic material, the seal reinforcement 90C can deform in response to the expansion and contraction of the exterior body 40 that occurs during the manufacture and use of the power storage device 10C. More specifically, in the power storage device 10C, the internal pressure of the power storage device 10C may increase due to volumetric changes in the positive and negative electrode active materials of the electrode assembly 20 associated with charging and discharging, as well as gas generation. When the internal pressure of the power storage device 10C increases, the exterior body 40 may expand and the exterior film 50 may stretch. Furthermore, when vacuuming is performed during the manufacturing process of the power storage device 10C, the exterior film 50 may deform due to contraction of the exterior body 40. If the seal reinforcement 90C can follow such deformation of the exterior body 40, the seal reinforcement 90C is less likely to separate from the exterior film 50. This makes it easier for the seal reinforcement 90C to more reliably achieve the above-described effects.
[0089] On the other hand, when the end reinforcement portions 900C and the ridge reinforcement portion 901C are formed of a material with relatively low stretching and deformability, the seal reinforcement portion 90C has the additional effect of suppressing deformation of the exterior body 40. Specifically, the seal reinforcement portion 90C, which has relatively low stretching and deformability, is located on the outside of the exterior film 50, thereby limiting the expansion of the exterior body 40. Furthermore, when the seal reinforcement portion 90C is at least partially joined to the exterior film 50, the seal reinforcement portion 90C reinforces the exterior film 50 in that portion, thereby limiting the contraction of the exterior body 40.
[0090] [5. Modifications] The above-described embodiments are examples of possible forms of the electricity storage device and the method for manufacturing the electricity storage device according to the present invention, and are not intended to limit the forms. The electricity storage device and the method for manufacturing the electricity storage device according to the present invention may take forms different from those exemplified in the embodiments. Examples of such forms include forms in which part of the configuration of each embodiment is replaced, changed, or omitted, or forms in which a new configuration is added to each embodiment. Some examples of modifications of each embodiment are shown below. Note that the above-described embodiments and the following modifications can be combined with each other as long as there is no technical contradiction.
[0091] (1) In the power storage device 10A of the second embodiment, the seal reinforcement part 90A does not have to cover the entire first sealing area 500 and the entire lid seal part 63, but may at least partially cover the first sealing area 500 and the lid seal part 63. More specifically, as long as the seal reinforcement part 90A covers a peripheral portion 5000 (see FIG. 4 ) of the exterior film 50 that forms the periphery of the opening 40A and a portion of the lid seal part 63 that faces the peripheral portion 5000, the effect of reinforcing the seal by the second sealing part 80 is achieved. In other words, the seal reinforcement part 90A does not have to cover the entire first sealing area 500 and the entire lid seal part 63 in the FB direction of the power storage device 10. Furthermore, the seal reinforcement 90A does not have to cover the entire circumferential direction of the opening 40A, including the peripheral edge portion 5000 and the portion of the lid seal portion 63 facing the peripheral edge portion 5000. The same applies to the seal reinforcement 90B of the third embodiment and the seal reinforcement 90C of the fourth embodiment. Furthermore, in the power storage devices 10A to 10C of the second to fourth embodiments, the seal reinforcement 90A to 90C does not have to cover the entire second surface 62 of the lid body 60. That is, as long as the seal reinforcement 90A to 90C is formed to cover the boundary between the exterior film 50 (first seal region 500) and the lid body 60 (lid seal portion 63) in the FB direction, the seal reinforcement 90A to 90C does not have to be formed in the center of the lid body 60. Furthermore, the seal reinforcement 90A to 90C may simply be formed to cover at least one apex (boundary 64 to 67) of the lid body 60 and its surroundings. This is because an unsealed portion of the second sealing portion 80 is particularly likely to occur at the top of the lid body 60 .
[0092] (2) The manufacturing method of the power storage device 10A of the second embodiment is not limited to that of the above embodiment. For example, in the step of forming the seal reinforcement portion 90A, the container 990 may first be filled with a fluidized material 91, at least a portion of the first seal region 500 and at least a portion of the second seal region 500 may be impregnated with the filled material 91, and then the container 990 may be removed, and the material 91 may then be solidified.
[0093] (3) In the power storage device 10B of the third embodiment and the power storage device 10C of the fourth embodiment, the seal reinforcement portion 90B and the both-end reinforcement portion 900C may further include a cushioning material for protecting the corners 230 of the electrode assembly 20. FIG. 12 is a diagram illustrating an example of the configuration of the cushioning material. In the example of FIG. 12, the cushioning material 92 is formed in an L-shape when viewed from the FB direction and covers the corners 230 from the UD and LR directions. The cushioning material 93 is formed in a plate shape when viewed from the UD direction and is disposed, for example, on the upper surface of the protrusion portion 50X (the surface on the first surface 41 side of the exterior body 40). The cushioning materials 92 and 93 are fixed to the outside of the seal reinforcement portion 90B or the both-end reinforcement portion 900C, respectively, to cover the corners 230 of the electrode assembly 20 and mitigate impacts applied to the exterior film 50 from the outside. For this reason, the cushioning materials 92 and 93 are preferably made of an elastic material such as rubber or elastomer.
[0094] As already mentioned, even in the above case, the seal reinforcement portion 90B and the both-end reinforcement portions 900C do not have to reach the corners 230, as long as the cushioning material 92 or 93 covers the corners 230. Furthermore, in addition to or instead of the configuration shown in FIG. 12 , the cushioning material 92 may be fixed to the seal reinforcement portion 90B or the both-end reinforcement portions 900C so as to fit along the underside of the protrusion 50X and the second surface 42 of the exterior body 40. Furthermore, in addition to or instead of the configuration shown in FIG. 12 , the cushioning material 93 may be fixed to the seal reinforcement portion 90B or the both-end reinforcement portions 900C so as to fit along the underside of the protrusion 50X. Furthermore, the cushioning material 92 or 93 may be fixed to the inside (closer to the exterior film 50) of the seal reinforcement portion 90B or the both-end reinforcement portions 900C, rather than to the outside.
[0095] (4) In the power storage devices 10, 10A to 10C of the first to fourth embodiments, the external shape of the exterior body 40 can be changed as desired. For example, the lid body 60 does not have to be substantially rectangular when viewed from the FB direction of the power storage device 10, and may be another substantially polygonal shape, or may be a shape other than a substantially polygonal shape, such as a substantially circular shape or a substantially elliptical shape. The shape of the lid body 60 may be changed depending on the three-dimensional shape of the electrode body 20, for example.
[0096] (5) In the power storage devices 10, 10A to 10C of the first to fourth embodiments, an adhesive film (not shown) may be bonded to the outer peripheral surface of the electrode terminal 30. Any adhesive film can be selected as long as it can bond the electrode terminal 30 made of metal to the lid 60 made of, for example, resin. Examples of adhesive films that can be used include polyolefin resins such as polyethylene resins and polypropylene resins, cyclic polyolefin resins, and acid-modified polyolefin resins obtained by graft-modifying these polyolefin resins with an acid such as maleic anhydride. The adhesive film can be a single layer or two or more layers of these films.
[0097] (6) In step S4 of the above manufacturing method, the exterior film 50 may be formed in advance as a cylindrical body having the opening 40A, and the electrode body 20 and the lid body 60 may be disposed inside the cylindrical body. This applies to the power storage devices 10, 10A to 10C according to the first to fourth embodiments.
[0098] (7) The electricity storage device 10B including the cap-shaped reinforcing member of the third embodiment can be manufactured, for example, by modifying the manufacturing method of the electricity storage device 10 of the first embodiment as follows. In step S1, an electrode body 20, a pair of electrode terminals 30, an exterior film 50, a pair of lid bodies 60, and a pair of reinforcing members attachable to the lid bodies 60 are prepared. In step S8, each reinforcing member is attached to each lid body 60 to form a seal reinforcement portion 90B. Note that the preparation of the reinforcing members may be performed at a timing separate from step S1, as long as it is performed before step S8.
[0099] (8) When the seal reinforcements 90A to 90C of the second to fourth embodiments have the function of suppressing deformation of the exterior body 40 described above, the seal reinforcements 90A to 90C may be configured to selectively suppress deformation of a specific surface of the exterior body 4 depending on the manner in which the power storage devices 10A to 10C are used. For example, as shown in FIG. 13 , the power storage devices 10A to 10C are used by arranging them side by side so that one of the second surfaces 42 of the plurality of power storage devices 10A to 10C (hereinafter, this will be referred to as the second surface 42B, and the other second surface 42 will be referred to as the second surface 42A) is in contact with the cooling mechanism 200. 13, the second surface 42B contacts the cooling mechanism 200, and the first surface 41A contacts the first surface 41B of the adjacent power storage device 10A to 10C directly or indirectly via a plate-like member, a buffer material, or the like (one of the first surfaces 41 is referred to as the first surface 41A, and the other is referred to as the first surface 41B). Therefore, for example, when considering expansion as one mode of deformation of the exterior body 40, in the power storage devices 10A to 10C arranged as shown in FIG. 13, the first surface 41A, the first surface 41B, and the second surface 42B of the exterior body 40 are relatively resistant to expansion even when the internal pressure of the power storage devices 10A to 10C increases.
[0100] On the other hand, the second surface 42A of the exterior body 40 is not in contact with other elements such as the power storage devices 10A-10C, and is therefore prone to expansion when the internal pressure of the power storage devices 10A-10C increases. For this reason, the seal reinforcement portions 90A-90C can be arranged to extend over a wider area on the second surface 42A of the exterior body 40 and joined to the outer surface of the exterior film 50, for example, to suppress expansion of the second surface 42A. In this way, the seal reinforcement portions 90A-90C can be configured to suppress expansion of a specific surface of the exterior body 40. The above configuration applies not only to expansion of the exterior body 40, but also to contraction.
[0101] 10, 10A to 10C: Electricity storage device 20: Electrode body 20A to D: Ridge portion 30: Electrode terminal 40: Exterior body 40A: Opening 50: Exterior film 60: Lid 63: Sealing surface (second sealing area) 64 to 67: Boundary (top) 80: Second sealing portion (sealing portion) 90, 90A to 90C: Seal reinforcement portion 230: Corner portion 500: First sealing area
Claims
1. An energy storage device comprising: an electrode body; an exterior film wrapping the electrode body to form an opening and having a first sealing area; a lid body disposed at the opening and having a second sealing area facing the first sealing area; a sealing portion formed between the first sealing area and the second sealing area, at least partially sealing the area between the first sealing area and the second sealing area; and a seal reinforcing portion reinforcing the sealing provided by the sealing portion.
2. The electricity storage device according to claim 1, wherein the material forming the seal reinforcement portion includes at least one of a resin, a metal, a ceramic, and a rubber, a mixture of at least two of these, and a composite of at least two of these.
3. The electric storage device according to claim 1 or 2, wherein the seal reinforcement portion is formed between the first seal area and the second seal area, at least in a portion where the seal portion is not formed.
4. The electric storage device according to claim 1 or 2, wherein the lid body has a polygonal shape having apexes when viewed from the front, and the seal reinforcement portion is formed so as to at least partially cover at least one apex of the polygonal shape of the lid body from the outside.
5. The electricity storage device according to claim 1 or 2, wherein the seal reinforcement portion covers at least a portion of the first seal area and at least a portion of the second seal area from the outside of the exterior film and the lid body.
6. The energy storage device according to claim 1 or 2, wherein the electrode body has a three-dimensional shape including a plurality of corners, and the seal reinforcement portion covers at least one of the plurality of corners from the outside of the exterior film.
7. The energy storage device according to claim 6, wherein the electrode body has a three-dimensional shape including two intersecting faces and a ridge portion formed by the two faces, and the seal reinforcement portion covers the ridge portion from the outside of the exterior film.
8. A method for manufacturing an electricity storage device, comprising: preparing an electrode body; wrapping the electrode body in an exterior film having a first sealing area so as to form an opening; placing a lid body having a second sealing area at the opening so that the second sealing area faces the first sealing area; forming a seal portion between the first sealing area of the exterior film and the second sealing area of the lid body, which at least partially seals the area between the first sealing area and the second sealing area; and forming a seal reinforcement portion between the first sealing area and the second sealing area, at least in a portion where the seal portion is not formed, which reinforces the seal portion.
9. A method for manufacturing an electricity storage device, comprising: preparing an electrode body; wrapping the electrode body in an exterior film having a first sealing area so as to form an opening; placing a lid body having a second sealing area at the opening so that the second sealing area faces the first sealing area; forming a seal portion between the first sealing area of the exterior film and the second sealing area of the lid body, which at least partially seals between the first sealing area and the second sealing area; impregnating at least a portion of the first sealing area and at least a portion of the second sealing area with a material in a fluid state; and solidifying the material in a fluid state to form a seal reinforcement portion that reinforces the seal portion.
10. A method for manufacturing an electricity storage device, comprising: preparing an electrode body; wrapping the electrode body in an exterior film having a first sealing area so as to form an opening; placing a lid body having a second sealing area at the opening so that the second sealing area faces the first sealing area; forming a seal portion between the first sealing area of the exterior film and the second sealing area of the lid body, which at least partially seals between the first sealing area and the second sealing area; preparing a reinforcing member configured to be attachable to the lid body, and covering at least a portion of the first sealing area and at least a portion of the second sealing area from the outside of the lid body; and attaching the reinforcing member to the lid body to form a seal reinforcing portion that reinforces the seal portion.
Citation Information
Patent Citations
All-solid battery
JP2019153504A
Method for manufacturing recycled aluminum, manufacturing equipment, manufacturing system, recycled aluminum, and processed aluminum product
WO2022092231A1
JP1972002799U
Electrolytic capacitor and its manufacture
JP1999186115A
Battery
JP2004186060A