Display panel

The display panel addresses durability and reliability issues by using a silicon oxynitride barrier layer in the optical structure layer to improve moisture and oxygen blocking, resulting in enhanced durability and efficiency.

WO2024205026A1PCT designated stage expired Publication Date: 2024-10-03SAMSUNG DISPLAY CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/KR2024/002100
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-27
Filing Date
2024-02-14
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Current display panels face challenges in durability and reliability, particularly in maintaining light conversion efficiency and preventing moisture and oxygen penetration, which affects their overall performance and longevity.

Method used

The display panel incorporates a light-emitting device with an optical structure layer that includes a light control layer with a barrier layer made of silicon oxynitride (SiON), a low refractive index layer, and additional barrier layers, which enhance moisture and oxygen blocking characteristics and improve light conversion efficiency.

Benefits of technology

This configuration improves the reliability and display efficiency of the panel by enhancing film durability and maintaining light extraction efficiency while preventing environmental damage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure KR2024002100_03102024_PF_FP_ABST
    Figure KR2024002100_03102024_PF_FP_ABST
Patent Text Reader

Abstract

A display panel according to one embodiment of the present invention comprises: a light-emitting element, which outputs source light and includes a first electrode, a light-emitting layer arranged on the first electrode and a second electrode arranged on the light-emitting layer; and an optical structure layer arranged on the light-emitting element, wherein the optical structure layer includes: a light control layer, which is arranged on the light-emitting element and includes at least one light control pattern; a low refractive index layer arranged on the light control layer; and a barrier layer, which is arranged between the light control layer and the low refractive index layer and includes silicon oxynitride (SiON), the barrier layer includes: a first layer, which is arranged to be adjacent to the low refractive index layer and has a nitrogen content of less than 1at%; a second layer, which is arranged to be spaced apart from the low refractive index layer with the first layer interposed therebetween and has a nitrogen content of 3at%-30at%; and a third layer, which is arranged to be spaced apart from the low refractive index layer with the first and second layers interposed therebetween and has a nitrogen content of less than 3.2at%.
Need to check novelty before this filing date? Find Prior Art

Description

Display panel

[0001] The present invention relates to a display panel, and more particularly, to a display panel having improved durability and reliability and increased display efficiency.

[0002] The display panel includes a transmissive display panel that selectively transmits source light generated from a light source and an emissive display panel that generates source light within the display panel itself. The display panel may include different types of light control patterns depending on the pixels to generate a color image. The light control patterns may transmit only a portion of the wavelength range of the source light or change the color of the source light. Some light control patterns may change the characteristics of the light without changing the color of the source light.

[0003] The purpose of the present invention is to provide a display panel with improved durability, reliability and display efficiency.

[0004] According to one embodiment of the present invention, a display panel includes a light-emitting element that outputs source light and includes a first electrode, a light-emitting layer disposed on the first electrode, and a second electrode disposed on the light-emitting layer, and an optical structure layer disposed on the light-emitting element, wherein the optical structure layer includes a light control layer disposed on the light-emitting element and including at least one light control pattern, a low-refractive-index layer disposed on the light control layer, and a barrier layer disposed between the light control layer and the low-refractive-index layer and including silicon oxynitride (SiON), wherein the barrier layer includes a first layer disposed adjacent to the low-refractive-index layer and having a nitrogen content of less than 1 at%, a second layer disposed spaced apart from the low-refractive-index layer with the first layer interposed therebetween and having a nitrogen content of 3 at% or more and 30 at% or less, and a third layer disposed spaced apart from the low-refractive-index layer with the first layer and the second layer interposed therebetween and having a nitrogen content of less than 3.2 at%.

[0005] The refractive index of the third layer may be 1.3 or more and 1.5 or less for light in the wavelength range of 400 nm to 700 nm.

[0006] The first layer may be disposed directly on the low-refractive-index layer, the second layer may be disposed directly on the first layer, and the third layer may be disposed directly on the second layer.

[0007] The thickness of the first layer may be greater than or equal to 500 angstroms (Å).

[0008] The optical structure layer may further include a color filter layer spaced apart from the light control layer with the low refractive index layer interposed therebetween, and including a plurality of color filters.

[0009] The above light control pattern may include a first light control pattern that converts the source light into a first light and a second light control pattern that transmits the source light, and the first light control pattern may include a first quantum dot that converts the source light into the first light.

[0010] The above light control layer further includes a bank disposed between the light control patterns, and the barrier layer can be directly disposed on one surface of the light control pattern and the bank.

[0011] The low-refractive-index layer may include a base resin and a plurality of hollow particles dispersed in the base resin.

[0012] The above low-refractive layer may have a refractive index of 1.3 or less for light in the wavelength range of 400 nm to 700 nm.

[0013] The second layer may include a 2-1 layer disposed adjacent to the first layer, and a 2-2 layer disposed between the 2-1 layer and the third layer and having a nitrogen content different from that of the 2-1 layer.

[0014] The optical structure layer further includes an additional barrier layer spaced apart from the barrier layer with the light control layer therebetween, and the additional barrier layer can be directly disposed on one surface of the light control pattern.

[0015] A display panel according to one embodiment of the present invention may further include a filling layer disposed between the light-emitting element and the optical structure layer and covering the light-emitting element.

[0016] The first layer may have a refractive index of 1.3 or more and 1.5 or less for light in the wavelength range of 400 nm to 700 nm, and the second layer may have a refractive index of 1.4 or more and 1.8 or less for light in the wavelength range of 400 nm to 700 nm.

[0017] The third layer may be in contact with one surface of the light control pattern.

[0018] The light-emitting element is disposed between the first electrode and the second electrode, and includes a plurality of light-emitting stacks, each of which includes the light-emitting layer, wherein the plurality of light-emitting stacks are disposed on the first electrode and include a first light-emitting stack including a first light-emitting layer, a charge generation layer disposed on the first stack, and a second light-emitting stack disposed on the charge generation layer and including a second light-emitting layer, wherein the first light-emitting layer can emit light of a different color from the second light-emitting layer.

[0019] According to one embodiment of the present invention, a display panel outputs source light and includes a light-emitting element including a first electrode, a light-emitting layer disposed on the first electrode, and a second electrode disposed on the light-emitting layer, and an optical structure layer disposed on the light-emitting element, wherein the optical structure layer is disposed on the light-emitting element and includes a light control layer including at least one light control pattern, a low-refractive-index layer disposed on the light control layer, and a barrier layer disposed between the light control layer and the low-refractive-index layer, wherein the barrier layer is sequentially disposed from the low-refractive-index layer and includes a first layer, a second layer, and a third layer each including silicon oxynitride (SiON), and wherein the nitrogen content of the second layer is 3 to 60 times the nitrogen content of the first layer, and the nitrogen content of the third layer is less than 3.2 at%.

[0020] The first layer may be disposed directly under the low-refractive-index layer, the second layer may be disposed directly under the first layer, and the third layer may be disposed directly under the second layer.

[0021] According to one embodiment of the present invention, a display panel includes a light-emitting element that outputs source light and includes a first electrode, a light-emitting layer disposed on the first electrode, and a second electrode disposed on the light-emitting layer, and an optical structure layer disposed on the light-emitting element, wherein the optical structure layer is disposed on the light-emitting element and includes a light control layer including at least one light control pattern, a low-refractive-index layer disposed on the light control layer, and a barrier layer disposed between the light control layer and the low-refractive-index layer and including silicon oxynitride (SiON), wherein the barrier layer includes a first layer directly disposed under the low-refractive-index layer and having a nitrogen content of less than 1 at%, a second layer directly disposed under the first layer and having a nitrogen content of 3 at% or more and 30 at% or less, and a third layer directly disposed under the second layer, and wherein the light control layer is directly disposed under the third layer.

[0022] The first layer may have a refractive index of 1.3 or more and 1.5 or less for light in the wavelength range of 400 nm to 700 nm, the second layer may have a refractive index of 1.4 or more and 1.8 or less for light in the wavelength range of 400 nm to 700 nm, and the third layer may have a refractive index of 1.3 or more and 1.5 or less for light in the wavelength range of 400 nm to 700 nm.

[0023] The thickness of the first layer may be 500 angstroms (Å) or more, the thickness of the second layer may be 600 angstroms (Å) or more, and the thickness of the third layer may be 500 angstroms (Å) or more.

[0024] According to a display panel of one embodiment of the present invention, the moisture and oxygen blocking properties and film durability of a barrier layer included in a light control layer can be improved, and the light conversion efficiency of the light control layer including the barrier layer can be improved. Accordingly, the reliability and display efficiency of a display panel including a light control layer can be improved.

[0025] Figure 1a is a perspective view of a display panel according to one embodiment of the present invention.

[0026] Figure 1b is a cross-sectional view of a display panel according to one embodiment of the present invention.

[0027] Figure 1c is a plan view of a display panel according to one embodiment of the present invention.

[0028] FIG. 2 is an enlarged plan view of a portion of a display panel according to one embodiment of the present invention.

[0029] Figure 3 is a cross-sectional view of a display panel according to one embodiment of the present invention.

[0030] FIGS. 4A to 4C are enlarged views of a portion of a cross-section of a display panel according to one embodiment of the present invention.

[0031] Figure 5 is a cross-sectional view of a light emitting device according to one embodiment of the present invention.

[0032] FIG. 6A is a cross-sectional view of a portion of a display panel according to one embodiment of the present invention.

[0033] FIG. 6b is an enlarged cross-sectional view of a portion of a display panel according to one embodiment of the present invention.

[0034] Figure 7 is a cross-sectional view of a portion of a display panel according to one embodiment of the present invention.

[0035] Hereinafter, embodiments of the present invention will be described with reference to the drawings.

[0036] In this specification, when it is said that a component (or region, layer, portion, etc.) is “on,” “connected to,” or “coupled to” another component, it means that it can be directly connected / coupled to the other component, or a third component may be disposed between them.

[0037] Identical drawing numbers indicate identical components. Furthermore, in the drawings, the thicknesses, proportions, and dimensions of components are exaggerated for the purpose of effectively illustrating the technical content. "And / or" encompasses any combination of one or more of the associated components.

[0038] While terms such as "first" and "second" may be used to describe various components, these components should not be limited by these terms. These terms are used solely to distinguish one component from another. For example, without departing from the scope of the present invention, a first component may be referred to as a "second component," and similarly, a second component may also be referred to as a "first component." Singular expressions include plural expressions unless the context clearly indicates otherwise.

[0039] Additionally, terms such as "below," "lower," "above," and "upper" are used to describe the relationships between components depicted in the drawings. These terms are relative concepts and are described based on the directions indicated in the drawings.

[0040] Terms such as "include" or "have" should be understood to specify the presence of a feature, number, step, operation, component, part, or combination thereof described in the specification, but not to exclude in advance the possibility of the presence or addition of one or more other features, numbers, steps, operations, components, parts, or combinations thereof.

[0041] In this specification, "directly disposed" may mean that there are no additional layers, films, regions, plates, etc., between a portion of a layer, film, region, plate, etc. and another portion. For example, "directly disposed" may mean disposed between two layers or two members without using an additional member, such as an adhesive member.

[0042] Unless otherwise defined, all terms (including technical and scientific terms) used herein have the same meaning as commonly understood by those skilled in the art to which this invention pertains. Furthermore, terms defined in commonly used dictionaries should be interpreted to have a meaning consistent with their meaning in the context of the relevant technology, and should not be interpreted in an overly idealistic or overly formal sense unless explicitly defined herein.

[0043] Hereinafter, a display panel according to one embodiment of the present invention will be described with reference to the drawings.

[0044] FIG. 1A is a perspective view of a display panel according to an embodiment of the present invention. FIG. 1B is a cross-sectional view of a display panel according to an embodiment of the present invention. FIG. 1C is a plan view of a display panel according to an embodiment of the present invention.

[0045] As illustrated in FIG. 1A, the display panel (DP) can display an image through a display surface (DP-IS). The display surface (DP-IS) is parallel to a plane defined by a first direction (DR1) and a second direction (DR2). The display surface (DP-IS) can include a display area (DA) and a non-display area (NDA). Pixels (PX) are arranged in the display area (DA), and pixels (PX) are not arranged in the non-display area (NDA). The non-display area (NDA) is defined along the border of the display surface (DP-IS). The non-display area (NDA) can surround the display area (DA). However, the present invention is not limited thereto, and in one embodiment of the present invention, the non-display area (NDA) may be omitted or arranged only on one side of the display area (DA).

[0046] The normal direction of the display surface (DP-IS), i.e., the thickness direction of the display panel (DP), is indicated by the third direction (DR3). The front (or upper surface) and the back (or lower surface) of each layer or unit described below are distinguished by the third direction (DR3). However, the first to third directions (DR1, DR2, DR3) illustrated in this embodiment are merely examples.

[0047] In one embodiment of the present invention, a display panel (DP) having a flat display surface (DP-IS) is illustrated, but is not limited thereto. The display panel (DP) may include a curved display surface or a three-dimensional display surface. The three-dimensional display surface may include a plurality of display areas pointing in different directions.

[0048] As illustrated in FIG. 1b, the display panel (DP) includes a base substrate (BS), a circuit element layer (DP-CL), a display element layer (DP-LED), and an optical structure layer (OSL). The base substrate (BS) may include a synthetic resin substrate or a glass substrate. The circuit element layer (DP-CL) includes at least one insulating layer and circuit elements. The circuit elements include signal lines, pixel driving circuits, etc. The circuit element layer (DP-CL) may be formed through a process of forming an insulating layer, a semiconductor layer, and a conductive layer by coating, deposition, etc., and a process of patterning the insulating layer, the semiconductor layer, and the conductive layer by a photolithography process. The display element layer (DP-LED) includes at least a display element. The optical structure layer (OSL) may convert the color of light provided from the display element. The optical structure layer (OSL) may include a light control pattern and a structure for increasing light conversion efficiency.

[0049] Fig. 1c illustrates the planar arrangement of signal lines (GL1 to GLn, DL1 to DLm) and pixels (PX11 to PXnm). The signal lines (GL1 to GLn, DL1 to DLm) may include a plurality of gate lines (GL1 to GLn) and a plurality of data lines (DL1 to DLm).

[0050] Each of the pixels (PX11 to PXnm) is connected to a corresponding gate line among a plurality of gate lines (GL1 to GLn) and a corresponding data line among a plurality of data lines (DL1 to DLm). Each of the pixels (PX11 to PXnm) may include a pixel driving circuit and a display element. Depending on the configuration of the pixel driving circuit of the pixels (PX11 to PXnm), more types of signal lines may be provided in the display panel (DP).

[0051] Pixels (PX11 to PXnm) in matrix form are illustrated as an example, but are not limited thereto. Pixels (PX11 to PXnm) are Pentile® ) can be arranged in the form of a diamond. For example, the points where pixels (PX11 to PXnm) are arranged may correspond to the vertices of a diamond. The gate driver circuit (GDC) can be integrated into the display panel (DP) through an oxide silicon gate driver circuit (OSG) or an amorphose silicon gate driver circuit (ASG) process.

[0052] Fig. 2 is an enlarged plan view of a portion of a display panel according to an embodiment of the present invention. Fig. 2 exemplarily illustrates a plane including three pixel areas (PXA-R, PXA-B, PXA-G) and an adjacent bank well area (BWA) in a display panel (DP, see Fig. 1a) of one embodiment. In an embodiment of the present invention, the three pixel areas (PXA-R, PXA-B, PXA-G) illustrated in Fig. 2 may be repeatedly arranged throughout the entire display area (DA, see Fig. 1a).

[0053] A peripheral region (NPXA) is arranged around the first to third pixel regions (PXA-R, PXA-B, PXA-G). The peripheral region (NPXA) sets a boundary of the first to third pixel regions (PXA-R, PXA-B, PXA-G). The peripheral region (NPXA) may surround the first to third pixel regions (PXA-R, PXA-B, PXA-G). A structure that prevents color mixing between the first to third pixel regions (PXA-R, PXA-B, PXA-G), for example, a pixel defining layer (PDL, see FIG. 3) or a bank (BMP, see FIG. 3), may be arranged in the peripheral region (NPXA).

[0054] In Fig. 2, first to third pixel areas (PXA-R, PXA-B, PXA-G) having the same planar shape and different planar areas are exemplarily illustrated, but the present invention is not limited thereto. At least two areas among the first to third pixel areas (PXA-R, PXA-B, PXA-G) may be the same. The areas of the first to third pixel areas (PXA-R, PXA-B, PXA-G) may be set according to the light emission color. Among the primary colors, the area of ​​the pixel area emitting red light may be the largest, and the area of ​​the pixel area emitting blue light may be the smallest.

[0055] Although the first to third pixel areas (PXA-R, PXA-B, PXA-G) are illustrated as rectangular in FIG. 2, the present invention is not limited thereto. In a plan view, the first to third pixel areas (PXA-R, PXA-B, PXA-G) may have a polygonal shape (including a substantial polygonal shape) of another shape, such as a rhombus or a pentagon. In one embodiment, the first to third pixel areas (PXA-R, PXA-B, PXA-G) may have a rectangular shape (a substantial rectangular shape) with rounded corner areas in a plan view.

[0056] In FIG. 2, the third pixel area (PXA-G) is arranged in the first row, and the first pixel area (PXA-R) and the second pixel area (PXA-B) are arranged in the second row. However, the present invention is not limited thereto, and the arrangement of the first to third pixel areas (PXA-R, PXA-B, PXA-G) may be variously changed. For example, the first to third pixel areas (PXA-R, PXA-B, PXA-G) may be arranged in the same row.

[0057] One of the first to third pixel areas (PXA-R, PXA-B, PXA-G) provides a second light corresponding to the source light, the other provides a first light different from the second light, and the remaining one provides a third light different from the first and second lights. In the present embodiment, the second pixel area (PXA-B) provides a second light corresponding to the source light. In the present embodiment, the first pixel area (PXA-R) can provide red light, the second pixel area (PXA-B) can provide blue light, and the third pixel area (PXA-G) can provide green light.

[0058] A bank well area (BWA) may be defined in a display area (DA, see FIG. 1a). The bank well area (BWA) may be an area where a bank well (BW, see FIG. 3) is formed to prevent defects due to misalignment in a process of patterning a plurality of light control patterns (CCP-R, CCP-B, CCP-G, see FIG. 4a) included in a light control layer (CCL, see FIG. 4a). That is, the bank well area (BWA) may be an area where a bank well formed by removing a portion of a bank (BMP, see FIG. 4a) is defined.

[0059] In Fig. 2, two bank well areas (BWAs) are defined adjacent to the third pixel area (PXA-G) as an example, but this is not limited thereto, and the shape and arrangement of the bank well areas (BWAs) may be variously changed.

[0060] Fig. 3 is a cross-sectional view of a display panel according to an embodiment of the present invention. Fig. 4a is an enlarged view of a portion of a cross-section of a display panel according to an embodiment of the present invention. Fig. 3 is a cross-sectional view of a light emitting element included in a display panel according to an embodiment of the present invention. Fig. 3 illustrates a cross-section corresponding to the line II' of Fig. 2. Fig. 4a illustrates a cross-section corresponding to the line II-II' of Fig. 2.

[0061] Referring to FIG. 3, a display panel (DP) of one embodiment may include a base substrate (BS), a circuit element layer (DP-CL) disposed on the base substrate (BS), and a display element layer (DP-LED) disposed on the circuit element layer (DP-CL). In the present specification, the base substrate (BS), the circuit element layer (DP-CL), and the display element layer (DP-LED) may be collectively referred to as a lower panel.

[0062] The base substrate (BS) may be a member that provides a reference surface on which components included in the circuit element layer (DP-CL) are placed. In one embodiment, the base substrate (BS) may be a glass substrate, a metal substrate, a polymer substrate, or the like. However, the embodiment is not limited thereto, and the base substrate (BS) may be an inorganic layer, a functional layer, or a composite material layer.

[0063] The base substrate (BS) may have a multilayer structure. For example, the base substrate (BS) may have a three-layer structure of a polymer resin layer, an adhesive layer, and a polymer resin layer. In particular, the polymer resin layer may include a polyimide-based resin. In addition, the polymer resin layer may include at least one of an acrylate-based resin, a methacrylate-based resin, a polyisoprene-based resin, a vinyl-based resin, an epoxy-based resin, a urethane-based resin, a cellulose-based resin, a siloxane-based resin, a polyamide-based resin, and a perylene-based resin. Meanwhile, in the present specification, an "α-based" resin means one that includes an "α" functional group.

[0064] A circuit element layer (DP-CL) may be arranged on a base substrate (BS). The circuit element layer (DP-CL) may include a transistor (TD) as a circuit element. The configuration of the circuit element layer (DP-CL) may vary depending on the design of the driving circuit of the pixel (PX, see FIG. 1a), and FIG. 3 illustrates one transistor (TD) as an example. The arrangement relationship of the active (AD), source (SD), drain (DD), and gate (GD) constituting the transistor (TD) is illustrated as an example. The active (AD), source (SD), and drain (DD) may be regions distinguished according to the doping concentration or conductivity of the semiconductor pattern.

[0065] The circuit element layer (DP-CL) may include a lower buffer layer (BRL), a first insulating layer (10), a second insulating layer (20), and a third insulating layer (30) disposed on a base substrate (BS). For example, the lower buffer layer (BRL), the first insulating layer (10), and the second insulating layer (20) may be inorganic layers, and the third insulating layer (30) may be an organic layer.

[0066] The display element layer (DP-LED) may include a light-emitting element (LED) as a display element. The light-emitting element (LED) may generate the source light described above. The light-emitting element (LED) includes a first electrode (EL1), a second electrode (EL2), and an emission layer (EML) disposed therebetween. In the present embodiment, the display element layer (DP-LED) may include an organic light-emitting diode as the light-emitting element. In one embodiment of the present invention, the light-emitting element may include a quantum dot light-emitting diode. That is, the emission layer (EML) included in the light-emitting element (LED) may include an organic light-emitting material as a light-emitting material, or the emission layer (EML) may include a quantum dot as a light-emitting material. Alternatively, the display element layer (DP-LED) in the present embodiment may include an ultra-small light-emitting element, which will be described later, as a light-emitting element. The ultra-small light-emitting element may include, for example, a micro LED element and / or a nano LED element. An ultra-small light-emitting device may be a light-emitting device having a micro- or nano-scale size and including an active layer disposed between a plurality of semiconductor layers.

[0067] A first electrode (EL1) is placed on the third insulating layer (30). The first electrode (EL1) can be directly or indirectly connected to the transistor (TD), and the connection structure of the first electrode (EL1) and the transistor (TD) is not shown in FIG. 3.

[0068] The display element layer (DP-LED) includes a pixel defining layer (PDL). For example, the pixel defining layer (PDL) may be an organic layer. An emission aperture (OH) is defined in the pixel defining layer (PDL). The emission aperture (OH) of the pixel defining layer (PDL) exposes at least a portion of the first electrode (EL1). In the present embodiment, a first emission area (EA1) may be defined by the emission aperture (OH).

[0069] A hole control layer (HTR), an emission layer (EML), and an electron control layer (ETR) overlap at least a pixel area (PXA-R). Each of the hole control layer (HTR), the emission layer (EML), the electron control layer (ETR), and the second electrode (EL2) may be commonly arranged in the first to third pixel areas (PXA-R, PXA-B, PXA-G, see FIG. 4a). Each of the hole control layer (HTR), the emission layer (EML), the electron control layer (ETR), and the second electrode (EL2) overlapping the first to third pixel areas (PXA-R, PXA-B, PXA-G, see FIG. 4a) may have an integral shape. However, without limitation thereto, at least one of the hole control layer (HTR), the emission layer (EML), and the electron control layer (ETR) may be formed separately for each of the first to third pixel areas (PXA-R, PXA-B, PXA-G, see FIG. 4a). In one embodiment, the emission layer (EML) may be patterned within the emission opening (OH) and formed separately for each of the first to third pixel areas (PXA-R, PXA-B, PXA-G, see FIG. 4a).

[0070] The hole control layer (HTR) includes a hole transport layer and may further include a hole injection layer.

[0071] The emission layer (EML) can generate a third light, which is a source light. The emission layer (EML) can generate blue light. The blue light can include light with a wavelength of 410 nm to 480 nm. The emission spectrum of the blue light can have a maximum peak in the wavelength range of 440 nm to 460 nm.

[0072] The electron control layer (ETR) includes an electron transport layer and may further include an electron injection layer.

[0073] The display element layer (DP-LED) may include a thin film encapsulation layer (TFE) that protects the second electrode (EL2). The thin film encapsulation layer (TFE) may include an organic material or an inorganic material. The thin film encapsulation layer (TFE) may have a multilayer structure in which inorganic layers / organic layers are repeated. In the present embodiment, the thin film encapsulation layer (TFE) may include a first encapsulation inorganic layer (IOL1) / encapsulation organic layer (OL) / second encapsulation inorganic layer (IOL2). The first and second encapsulation inorganic layers (IOL1 / IOL2) protect the light emitting element (LED) from external moisture, and the encapsulation organic layer (OL) may prevent the light emitting element (LED) from being damaged by foreign substances introduced during the manufacturing process. Although not shown, the display panel (DP) may further include a refractive index control layer on the upper side of the thin film encapsulation layer (TFE) to improve light emission efficiency.

[0074] As illustrated in FIG. 3, an optical structure layer (OSL) is disposed on a thin film encapsulation layer (TFE). The optical structure layer (OSL) may include a light control layer (CCL), a low refractive index layer (LR), a color filter layer (CFL), and a base layer (BL). In this specification, the optical structure layer (OSL) may be referred to as an upper panel.

[0075] A light control layer (CCL) can be disposed on a display element layer (DP-LED) including a light emitting element (LED). The light control layer (CCL) includes a bank (BMP), a light control pattern (CCP-R, CCP-B), and a barrier layer (CAP1).

[0076] A bank (BMP) may include a base resin and additives. The base resin may be composed of various resin compositions, which may be generally referred to as a binder. The additives may include a coupling agent and / or a photoinitiator. The additives may further include a dispersant.

[0077] The bank (BMP) may include a black coloring agent for light blocking. The bank (BMP) may include a black dye or pigment mixed into the base resin. In one embodiment, the black coloring agent may include carbon black, a metal such as chromium, or an oxide thereof.

[0078] The bank (BMP) includes a bank opening (BW-OH) corresponding to the light-emitting opening (OH). In a plan view, the bank opening (BW-OH) overlaps the light-emitting opening (OH) and has a larger area than the light-emitting opening (OH). That is, the bank opening (BW-OH) may have a larger area than the light-emitting area (EA1) defined by the light-emitting opening (OH). Meanwhile, in the present specification, "corresponds" means that two configurations overlap when viewed in the thickness direction (DR3) of the display panel (DP), and is not limited to the same area.

[0079] A light control pattern (CCP-R, CCP-B) is arranged inside the bank opening (BW-OH). At least some of the light control patterns (CCP-R, CCP-B) can change the optical properties of the source light. In one embodiment, the first light control pattern (CCP-R) can change the optical properties of the source light.

[0080] The first light control pattern (CCP-R) may include quantum dots for changing the optical properties of the source light. The first light control pattern (CCP-R) may include quantum dots for converting the source light into light of a different wavelength. In the first light control pattern (CCP-R) overlapping the first pixel area (PXA-R), the quantum dots may convert blue light, which is the source light, into red light.

[0081] In this specification, a quantum dot refers to a crystal of a semiconductor compound. Depending on the size of the crystal, a quantum dot can emit light of various emission wavelengths. Quantum dots can also emit light of various emission wavelengths by adjusting the element ratio within the quantum dot compound.

[0082] The diameter of the quantum dot may be, for example, about 1 nm to 10 nm.

[0083] The above quantum dots can be synthesized by a wet chemical process, an organometallic chemical vapor deposition process, a molecular beam epitaxy process, or a similar process.

[0084] The above wet chemical process is a method for growing quantum dot particle crystals by mixing an organic solvent and a precursor material. As the crystals grow, the organic solvent naturally acts as a dispersant coordinated to the quantum dot crystal surface, controlling the crystal growth. Therefore, the wet chemical process is easier and less expensive than vapor deposition methods such as metal-organic chemical vapor deposition (MOCVD) or molecular beam epitaxy (MBE), allowing for controlled growth of quantum dot particles.

[0085] The core of the quantum dot can be selected from a group II-VI compound, a group III-V compound, a group III-VI compound, a group I-III-VI compound, a group IV-VI compound, a group IV element, a group IV compound, and a combination thereof.

[0086] The group II-VI compound is a binary compound selected from the group consisting of CdSe, CdTe, CdS, ZnS, ZnSe, ZnTe, ZnO, HgS, HgSe, HgTe, MgSe, MgS and mixtures thereof; a ternary compound selected from the group consisting of CdSeS, CdSeTe, CdSTe, ZnSeS, ZnSeTe, ZnSTe, HgSeS, HgSeTe, HgSTe, CdZnS, CdZnSe, CdZnTe, CdHgS, CdHgSe, CdHgTe, HgZnS, HgZnSe, HgZnTe, MgZnSe, MgZnS and mixtures thereof; And it may be selected from the group consisting of a four-element compound selected from the group consisting of HgZnTeS, CdZnSeS, CdZnSeTe, CdZnSTe, CdHgSeS, CdHgSeTe, CdHgSTe, HgZnSeS, HgZnSeTe, HgZnSTe and mixtures thereof. Meanwhile, the II-VI group semiconductor compound may further include a Group I metal and / or a Group IV element. The Group I-II-VI compound may be selected from CuSnS or CuZnS, and the Group II-IV-VI compound may be selected from ZnSnS, etc. The Group I-II-IV-VI compound may be selected from a four-element compound selected from the group consisting of Cu2ZnSnS2, Cu2ZnSnS4, Cu2ZnSnSe4, Ag2ZnSnS2 and mixtures thereof.

[0087] The III-VI group compounds may include binary compounds such as In2S3, In2Se3, etc., ternary compounds such as InGaS3, InGaSe3, etc., or any combination thereof.

[0088] Group I-III-VI compounds are ternary compounds selected from the group consisting of AgInS, AgInS2, CuInS, CuInS2, AgGaS2, CuGaS2CuGaO2, AgGaO2, AgAlO2 and mixtures thereof, or AgInGaS2, It can be selected from four-element compounds such as CuInGaS2.

[0089] The group III-V compound may be selected from the group consisting of binary compounds selected from the group consisting of GaN, GaP, GaAs, GaSb, AlN, AlP, AlAs, AlSb, InN, InP, InAs, InSb, and mixtures thereof, ternary compounds selected from the group consisting of GaNP, GaNAs, GaNSb, GaPAs, GaPSb, AlNP, AlNAs, AlNSb, AlPAs, AlPSb, InGaP, InAlP, InNP, InNAs, InNSb, InPAs, InPSb, and mixtures thereof, and quaternary compounds selected from the group consisting of GaAlNP, GaAlNAs, GaAlNSb, GaAlPAs, GaAlPSb, GaInNP, GaInNAs, GaInNSb, GaInPAs, GaInPSb, InAlNP, InAlNAs, InAlNSb, InAlPAs, InAlPSb, and mixtures thereof. Meanwhile, the group III-V compound may further include a group II metal. For example, InZnP may be selected as the group III-II-V compound.

[0090] The group IV-VI compound may be selected from the group consisting of binary compounds selected from the group consisting of SnS, SnSe, SnTe, PbS, PbSe, PbTe and mixtures thereof; ternary compounds selected from the group consisting of SnSeS, SnSeTe, SnSTe, PbSeS, PbSeTe, PbSTe, SnPbS, SnPbSe, SnPbTe and mixtures thereof; and quaternary compounds selected from the group consisting of SnPbSSe, SnPbSeTe, SnPbSTe and mixtures thereof.

[0091] Examples of the above II-IV-V group semiconductor compounds may be ternary compounds selected from the group consisting of ZnSnP, ZnSnP2, ZnSnAs2, ZnGeP2, ZnGeAs2, CdSnP2, and CdGeP2 and mixtures thereof.

[0092] The group IV element may be selected from the group consisting of Si, Ge, and mixtures thereof. The group IV compound may be a binary compound selected from the group consisting of SiC, SiGe, and mixtures thereof.

[0093] Each element included in the multi-element compounds such as the above binary, ternary and quaternary compounds may exist in the particles in a uniform or non-uniform concentration. That is, the chemical formula indicates the type of elements included in the compound, and the element ratio within the compound may be different. For example, AgInGaS2 is AgIn x Ga 1-x It can mean S2 (where x is a real number between 0 and 1).

[0094] Here, binary, ternary, or quaternary compounds may exist within the particle at a uniform concentration, or may exist within the same particle with partially different concentration distributions. Furthermore, one quantum dot may have a core / shell structure, where one quantum dot surrounds another. In a core / shell structure, the concentration of the element present in the shell may have a concentration gradient, decreasing toward the core.

[0095] In some embodiments, the quantum dot may have a core-shell structure comprising a core comprising the aforementioned nanocrystals and a shell surrounding the core. The shell of the quantum dot may function as a protective layer to maintain semiconductor properties by preventing chemical modification of the core and / or as a charging layer to impart electrophoretic properties to the quantum dot. The shell may be a single layer or a multilayer. Examples of the shell of the quantum dot include a metal or non-metal oxide, a semiconductor compound, or a combination thereof.

[0096] For example, the oxide of the metal or non-metal may be a binary compound such as SiO2, Al2O3, TiO2, ZnO, MnO, Mn2O3, Mn3O4, CuO, FeO, Fe2O3, Fe3O4, CoO, Co3O4, NiO, or a ternary compound such as MgAl2O4, CoFe2O4, NiFe2O4, CoMn2O4, but the present invention is not limited thereto.

[0097] In addition, the semiconductor compound may be exemplified by CdS, CdSe, CdTe, ZnS, ZnSe, ZnTe, ZnSeS, ZnTeS, GaAs, GaP, GaSb, HgS, HgSe, HgTe, InAs, InP, InGaP, InSb, AlAs, AlP, AlSb, etc., but the present invention is not limited thereto.

[0098] Quantum dots can have a full width of half maximum (FWHM) of an emission wavelength spectrum of about 45 nm or less, preferably about 40 nm or less, and more preferably about 30 nm or less, and color purity and color reproducibility can be improved within this range. In addition, since light emitted by these quantum dots is emitted in all directions, a wide viewing angle can be improved.

[0099] In addition, the shape of the quantum dot is not particularly limited to a shape commonly used in the field, but more specifically, a shape such as a spherical, pyramidal, multi-arm, or cubic nanoparticle, nanotube, nanowire, nanofiber, or nanoplatelet particle can be used.

[0100] Since the energy band gap of quantum dots can be controlled by adjusting the size of the quantum dots or the element ratio within the quantum dot compound, light of various wavelengths can be obtained from the quantum dot light-emitting layer. Therefore, by using quantum dots as described above (using quantum dots of different sizes or varying the element ratio within the quantum dot compound), a light-emitting device that emits light of various wavelengths can be implemented. Specifically, the size of the quantum dots or the element ratio within the quantum dot compound can be selected to emit red, green, and / or blue light. In addition, the quantum dots can be configured to emit white light by combining light of various colors.

[0101] In one embodiment, a quantum dot included in a first light control pattern (CCP-R) overlapping a first pixel area (PXA-R) may have a red emission color. The smaller the particle size of the quantum dot, the more it may emit light in a shorter wavelength range. For example, among quantum dots having the same core, the particle size of a quantum dot that emits green light may be smaller than the particle size of a quantum dot that emits red light. Additionally, among quantum dots having the same core, the particle size of a quantum dot that emits blue light may be smaller than the particle size of a quantum dot that emits green light. However, the embodiment is not limited thereto, and even among quantum dots having the same core, the particle size may be controlled depending on a shell forming material, shell thickness, etc.

[0102] Meanwhile, if quantum dots have various emission colors such as blue, red, and green, quantum dots with different emission colors may have different core materials.

[0103] The first light control pattern (CCP-R) may further include a scatterer. The first light control pattern (CCP-R) may include quantum dots that convert blue light into red light and a scatterer that scatters light.

[0104] The scatterer may be an inorganic particle. For example, the scatterer may comprise at least one of TiO2, ZnO, Al2O3, SiO2, and hollow silica. The scatterer may comprise any one of TiO2, ZnO, Al2O3, SiO2, and hollow silica, or may be a mixture of two or more materials selected from TiO2, ZnO, Al2O3, SiO2, and hollow silica.

[0105] The first light control pattern (CCP-R) may include a base resin that disperses quantum dots and scatterers. The base resin, which serves as a medium in which quantum dots and scatterers are dispersed, may be composed of various resin compositions, which may generally be referred to as binders. For example, the base resin may be an acrylic resin, a urethane resin, a silicone resin, an epoxy resin, etc. The base resin may be a transparent resin.

[0106] In this embodiment, the first light control pattern (CCP-R) can be formed by an inkjet process. A liquid composition is provided within the bank opening (BW-OH). The composition, which is polymerized by a thermal or photo-curing process, reduces in volume after curing.

[0107] A step may occur between the lower surface of the bank (BMP) and the lower surface of the first light control pattern (CCP-R). That is, the lower surface of the bank (BMP) may be defined as higher than the lower surface of the first light control pattern (CCP-R). The height difference between the lower surface of the bank (BMP) and the lower surface of the first light control pattern (CCP-R) may be, for example, about 2 μm to about 3 μm.

[0108] The light control layer (CCL) includes a barrier layer (CAP1) disposed on one surface of the first light control pattern (CCP-R). The barrier layer (CAP1) may serve to prevent the penetration of moisture and / or oxygen (hereinafter referred to as “moisture / oxygen”) and to improve the optical characteristics of the optical structure layer (OSL) by controlling a refractive index. The barrier layer (CAP1) may be disposed on one upper surface or one lower surface of the first light control pattern (CCP-R) to block the first light control pattern (CCP-R) from being exposed to moisture / oxygen, and in particular, may block quantum dots included in the first light control pattern (CCP-R) from being exposed to moisture / oxygen. The barrier layer (CAP1) may also protect the first light control pattern (CCP-R) from external impact.

[0109] In one embodiment, the barrier layer (CAP1) may be disposed spaced apart from the display element layer (DP-LED) with the first light control pattern (CCP-R) interposed therebetween. That is, the barrier layer (CAP1) may be disposed on the upper surface of the first light control pattern (CCP-R). In one embodiment, the light control layer (CCL) may include an additional barrier layer (CAP2) disposed between the first light control pattern (CCP-R) and the display element layer (DP-LED). The barrier layer (CAP1) may cover the upper surface of the first light control pattern (CCP-R) adjacent to the low-refractive-index layer (LR), and the additional barrier layer (CAP2) may cover the lower surface of the first light control pattern (CCP-R) adjacent to the display element layer (DP-LED). Meanwhile, in this specification, the “upper surface” may be a surface located above in the third direction (DR3), and the “lower surface” may be a surface located below in the third direction (DR3).

[0110] Additionally, the barrier layer (CAP1) and the additional barrier layer (CAP2) may cover one side of the bank (BMP) as well as the first optical control pattern (CCP-R).

[0111] The barrier layer (CAP1) may cover one side of the bank (BMP) and the first light control pattern (CCP-R) adjacent to the low-refractive-index layer (LR). The barrier layer (CAP1) may be disposed directly under the low-refractive-index layer (LR). The additional barrier layer (CAP2) may be disposed to follow the step of the bank (BMP) and the first light control pattern (CCP-R). The additional barrier layer (CAP2) may be disposed directly on the filling layer (FML).

[0112] The barrier layer (CAP1) and the additional barrier layer (CAP2) may be formed of an inorganic material. In the display panel (DP) of one embodiment, the barrier layer (CAP1) includes silicon oxynitride (SiON). Both the barrier layer (CAP1) and the additional barrier layer (CAP2) may include silicon oxynitride. However, the present invention is not limited thereto, and the barrier layer (CAP1) disposed on the upper side of the first light control pattern (CCP-R) may include silicon oxynitride, and the additional barrier layer (CAP2) disposed on the lower side of the first light control pattern (CCP-R) may include silicon oxide (SiOx). However, the present invention is not limited thereto.

[0113] The barrier layer (CAP1) including silicon oxynitride has a silicon, oxygen, and nitrogen content limited to a certain range in order to prevent moisture / oxygen from penetrating into the first light control pattern (CCP-R), increase film durability, and have a refractive index range that does not lower the light efficiency of the display panel. Hereinafter, the content and detailed laminated structure of the barrier layer (CAP1) of one embodiment will be described in more detail in the description of FIGS. 6A and 6B, etc.

[0114] A color filter layer (CFL) is disposed on the light control layer (CCL). The color filter layer (CFL) includes at least one color filter. The color filter transmits light within a specific wavelength range and blocks light outside the wavelength range. The first color filter (CF1) of the first pixel area (PXA-R) can transmit red light and block green and blue light.

[0115] The first color filter (CF1) includes a base resin and a dye and / or pigment dispersed in the base resin. The base resin is a medium in which the dye and / or pigment is dispersed and may be composed of various resin compositions, which may generally be referred to as a binder.

[0116] The first color filter (CF1) may have a uniform thickness within the first pixel area (PXA-R). Light converted from a blue source light to red light through the first light control pattern (CCP-R) may be provided to the outside with uniform brightness within the first pixel area (PXA-R).

[0117] The optical structure layer (OSL) includes a low-refractive-index layer (LR). The low-refractive-index layer (LR) may be disposed between a light control layer (CCL) and a color filter layer (CFL). The low-refractive-index layer (LR) may be disposed on the light control layer (CCL) to block the first light control pattern (CCP-R) from being exposed to moisture / oxygen. In addition, the low-refractive-index layer (LR) may be disposed between the first light control pattern (CCP-R) and the first color filter (CF1) to function as an optical functional layer, such as increasing light extraction efficiency or preventing reflected light from entering the light control layer (CCL). The low-refractive-index layer (LR) may be a layer having a lower refractive index than an adjacent layer.

[0118] The low-refractive-index layer (LR) may include at least one inorganic layer. For example, the low-refractive-index layer (LR) may include silicon nitride, aluminum nitride, zirconium nitride, titanium nitride, hafnium nitride, tantalum nitride, silicon oxide, aluminum oxide, titanium oxide, tin oxide, cerium oxide, and silicon oxynitride, or a metal thin film having secured light transmittance. However, the embodiment is not limited thereto, and the low-refractive-index layer (LR) may include an organic film. The low-refractive-index layer (LR) may have a structure in which a plurality of hollow particles are dispersed in an organic polymer resin, for example. The low-refractive-index layer (LR) may be composed of a single layer or a plurality of layers.

[0119] In one embodiment, the display panel (DP) may further include a base layer (BL) disposed on a color filter layer (CFL). The base layer (BL) may be a member that provides a reference surface on which the color filter layer (CFL), the low-refractive layer (LR), and the light control layer (CCL) are disposed. The base layer (BL) may be a glass substrate, a metal substrate, a plastic substrate, or the like. However, the embodiment is not limited thereto, and the base layer (BL) may be an inorganic layer, an organic layer, or a composite material layer. In addition, unlike the embodiment illustrated, the base layer (BL) may be omitted in one embodiment.

[0120] Although not shown, an anti-reflection layer may be disposed on the base layer (BL). The anti-reflection layer may be a layer that reduces the reflectance of external light incident from the outside. The anti-reflection layer may be a layer that selectively transmits light emitted from the display panel (DP). In one embodiment, the anti-reflection layer may be a single layer including a dye and / or pigment dispersed in a base resin. The anti-reflection layer may be provided as a single continuous layer that completely overlaps the entire first to third pixel areas (PXA-R, PXA-B, PXA-G, see FIG. 4a).

[0121] The anti-reflection layer may not include a polarizing layer. Accordingly, light passing through the anti-reflection layer and incident on the display element layer (DP-LED) may be unpolarized light. The display element layer (DP-LED) can receive unpolarized light from above the anti-reflection layer.

[0122] In one embodiment, a display panel (DP) includes a lower panel including a display element layer (DP-LED) and an upper panel (optical structure layer, OSL) including a light control layer (CCL) and a color filter layer (CFL). In one embodiment, a filling layer (FML) may be disposed between the lower panel and the upper panel (OSL). In one embodiment, the filling layer (FML) may fill a space between the display element layer (DP-LED) and the light control layer (CCL). The filling layer (FML) may be disposed directly on an encapsulation layer (TFE), and an additional barrier layer (CAP2) may be disposed directly on the filling layer (FML). A lower surface of the filling layer (FML) may be in contact with an upper surface of the encapsulation layer (TFE), and an upper surface of the filling layer (FML) may be in contact with a lower surface of the additional barrier layer (CAP2).

[0123] The filling layer (FML) can function as a buffer between the display element layer (DP-LED) and the light control layer (CCL). In one embodiment, the filling layer (FML) can have a shock absorption function, etc., and can increase the strength of the display panel (DP). The filling layer (FML) can be formed from a filling resin including a polymer resin. For example, the filling layer (FML) can be formed from a filling layer resin including an acrylic resin or an epoxy resin.

[0124] The filling layer (FML) may be formed in a separate process step with a configuration distinct from the encapsulating layer (TFE) positioned underneath and the additional barrier layer (CAP2) positioned above. Meanwhile, the filling layer (FML) may be formed of a different material from each of the encapsulating layer (TFE) and the additional barrier layer (CAP2).

[0125] Referring to FIG. 4A, the display panel (DP) may include a base substrate (BS) and a circuit element layer (DP-CL) disposed on the base substrate (BS). The circuit element layer (DP-CL) may be disposed on the base substrate (BS). The circuit element layer (DP-CL) may include an insulating layer, a semiconductor pattern, a conductive pattern, a signal line, and the like. The insulating layer, the semiconductor layer, and the conductive layer may be formed on the base substrate (BS) by a coating, deposition, or the like, and then the insulating layer, the semiconductor layer, and the conductive layer may be selectively patterned through multiple photolithography processes. Thereafter, the semiconductor pattern, the conductive pattern, and the signal line included in the circuit element layer (DP-CL) may be formed. In one embodiment, the circuit element layer (DP-CL) may include a transistor, a buffer layer, and a plurality of insulating layers.

[0126] According to one embodiment, a light emitting device (LED) may include a first electrode (EL1), a second electrode (EL2) facing the first electrode (EL1), and an emission layer (EML) disposed between the first electrode (EL1) and the second electrode (EL2). The emission layer (EML) included in the light emitting device (LED) may include an organic light emitting material as a light emitting material or may include quantum dots. The light emitting device (LED) may further include a hole control layer (HTR) and an electron control layer (ETR). Meanwhile, although not shown, the light emitting device (LED) may further include a capping layer (not shown) disposed on the second electrode (EL2).

[0127] A pixel defining layer (PDL) is disposed on a circuit element layer (DP-CL) and can cover a portion of a first electrode (EL1). A light-emitting aperture (OH) is defined in the pixel defining layer (PDL). The light-emitting aperture (OH) of the pixel defining layer (PDL) exposes at least a portion of the first electrode (EL1). In the present embodiment, light-emitting areas (EA1, EA2, EA3) are defined to correspond to a portion of the first electrode (EL1) exposed by the light-emitting aperture (OH).

[0128] The display element layer (DP-LED) may include a first light-emitting area (EA1), a second light-emitting area (EA2), and a third light-emitting area (EA3). The first light-emitting area (EA1), the second light-emitting area (EA2), and the third light-emitting area (EA3) may be areas defined by a pixel defining layer (PDL). The first light-emitting area (EA1), the second light-emitting area (EA2), and the third light-emitting area (EA3) may correspond to the first pixel area (PXA-R), the second pixel area (PXA-B), and the third pixel area (PXA-G), respectively.

[0129] The light-emitting areas (EA1, EA2, EA3) may overlap with the pixel areas (PXA-R, PXA-B, PXA-G) and may not overlap with the bank well area (BWA). When viewed in a plan view, the area of ​​the pixel areas (PXA-R, PXA-B, PXA-G) defined by the bank (BMP) may be larger than the area of ​​the light-emitting areas (EA1, EA2, EA3) defined by the pixel defining layer (PDL).

[0130] In a light-emitting diode (LED), a first electrode (EL1) is disposed on a circuit element layer (DP-CL). The first electrode (EL1) may be an anode or a cathode. Additionally, the first electrode (EL1) may be a pixel electrode. The first electrode (EL1) may be a transmissive electrode, a semi-transmissive electrode, or a reflective electrode.

[0131] A hole control layer (HTR) may be disposed between the first electrode (EL1) and the light emitting layer (EML). The hole control layer (HTR) may include at least one of a hole injection layer, a hole transport layer, and an electron blocking layer. The hole control layer (HTR) may be disposed as a common layer so as to overlap the entire light emitting areas (EA1, EA2, EA3) and the pixel defining layer (PDL) that separates the light emitting areas (EA1, EA2, EA3). However, the embodiment is not limited thereto, and the hole control layer (HTR) may be patterned and provided so as to be disposed separately corresponding to each of the light emitting areas (EA1, EA2, EA3).

[0132] An emission layer (EML) is disposed on a hole control layer (HTR). In one embodiment, the emission layer (EML) may be provided as a common layer so as to overlap the entire emission areas (EA1, EA2, EA3) and the pixel defining layer (PDL) that separates the emission areas (EA1, EA2, EA3). In one embodiment, the emission layer (EML) may emit blue light. The emission layer (EML) may overlap the entire hole control layer (HTR) and the electron control layer (ETR).

[0133] However, the embodiment is not limited thereto, and in one embodiment, the light-emitting layer (EML) may be disposed within the light-emitting aperture (OH). That is, the light-emitting layer (EML) may be formed separately to correspond to light-emitting areas (EA1, EA2, EA3) defined by the pixel defining layer (PDL). The light-emitting layers (EML) formed separately to correspond to the light-emitting areas (EA1, EA2, EA3) may all emit blue light, or may emit light in different wavelength regions.

[0134] The light-emitting layer (EML) may have a multilayer structure having a single layer made of a single material, a single layer made of multiple different materials, or multiple layers made of multiple different materials. The light-emitting layer (EML) may include a fluorescent or phosphorescent material. In the light-emitting device of one embodiment, the light-emitting layer (EML) may include an organic light-emitting material, a metal-organic complex, or a quantum dot as a light-emitting material. Meanwhile, although FIGS. 3 and 4A illustrate a light-emitting device (LED) including one light-emitting layer (EML), in one embodiment, the light-emitting device (LED) may include multiple light-emitting stacks, each of which includes at least one light-emitting layer.

[0135] Fig. 5 is a cross-sectional view of a light-emitting device according to one embodiment of the present invention. Unlike the light-emitting device of the embodiment illustrated in Figs. 3 and 4a, Fig. 5 exemplarily illustrates a light-emitting device (LED) including a plurality of light-emitting stacks (ST1, ST2, ST3, ST4).

[0136] Referring to FIG. 5, a light emitting element (LED) of one embodiment may include a first electrode (EL1), a second electrode (EL2) facing the first electrode (EL1), and first to fourth light emitting stacks (ST1, ST2, ST3, ST4) disposed between the first electrode (EL1) and the second electrode (EL2). Meanwhile, FIG. 5 exemplarily illustrates that the light emitting element (LED) includes four light emitting stacks, but the number of light emitting stacks included in the light emitting element (LED) may be less or more than this.

[0137] The light emitting diode (LED) may include first to third charge generation layers (CGL1, CGL2, CGL3) disposed between first to fourth light emitting stacks (ST1, ST2, ST3, ST4).

[0138] When voltage is applied, each of the first to third charge generation layers (CGL1, CGL2, CGL3) can generate charges (electrons and holes) by forming a complex through an oxidation-reduction reaction. Thereafter, the first to third charge generation layers (CGL1, CGL2, CGL3) can provide the generated charges to the adjacent stacks (ST1, ST2, ST3, ST4), respectively. The first to third charge generation layers (CGL1, CGL2, CGL3) can double the efficiency of current generated in the adjacent stacks (ST1, ST2, ST3, ST4) and can play a role in controlling the balance of charges between the adjacent stacks (ST1, ST2, ST3, ST4).

[0139] Each of the first to third charge generation layers (CGL1, CGL2, CGL3) may include an n-type layer and a p-type layer. The first to third charge generation layers (CGL1, CGL2, CGL3) may have a structure in which the n-type layer and the p-type layer are bonded to each other. However, the present invention is not limited thereto, and the first to third charge generation layers (CGL1, CGL2, CGL3) may include only one of the n-type layer and the p-type layer. The n-type layer may be a charge generation layer that provides electrons to an adjacent stack. The n-type layer may be a layer in which an n-dopant is doped into a base material. The p-type layer may be a charge generation layer that provides holes to an adjacent stack.

[0140] In one embodiment, the thickness of each of the first to third charge generation layers (CGL1, CGL2, CGL3) may be 1 angstrom (Å) or more and 150 angstroms (Å) or less. The concentration of the n-dopant doped in the first to third charge generation layers (CGL1, CGL2, CGL3) may be 0.1% or more and 3% or less, and specifically, 1% or less. When the concentration is less than 0.1%, the effect of the first to third charge generation layers (CGL1, CGL2, CGL3) controlling the balance of charges may hardly occur. When the concentration is greater than 3%, the light efficiency of the light emitting diode (LED) may be reduced.

[0141] Each of the first to third charge generation layers (CGL1, CGL2, CGL3) may include a charge generation compound composed of an aryl amine organic compound, a metal, an oxide, carbide, fluoride of a metal, or a mixture thereof. For example, the aryl amine organic compound may include α-NPD, 2-TNATA, TDATA, MTDATA, sprio-TAD, or sprio-NPB. The metal may include cesium (Cs), molybdenum (Mo), vanadium (V), titanium (Ti), tungsten (W), barium (Ba), or lithium (Li). The oxide, carbide, and fluoride of the metal may include Re2O7, MoO3, V2O5, WO3, TiO2, Cs2CO3, BaF, LiF, or CsF. However, the materials of the first to third charge generation layers (CGL1, CGL2, CGL3) are not limited to the above examples.

[0142] Each of the first to fourth light-emitting stacks (ST1, ST2, ST3, and ST4) may include a light-emitting layer. The first light-emitting stack (ST1) may include a first light-emitting layer (BEML-1), the second light-emitting stack (ST2) may include a second light-emitting layer (BEML-2), the third light-emitting stack (ST3) may include a third light-emitting layer (BEML-3), and the fourth light-emitting stack (ST4) may include a fourth light-emitting layer (GEML). Some of the light-emitting layers included in the first to fourth light-emitting stacks (ST1, ST2, ST3, and ST4) may emit substantially the same color light, and some may emit different color light.

[0143] In one embodiment, the first to third light-emitting layers (BEML-1, BEML-2, BEML-3) of the first to third light-emitting stacks (ST1, ST2, ST3) can emit substantially the same first color light. For example, the first color light can be blue light, which is the source light described above. The wavelength range of the light emitted by the first to third light-emitting layers (BEML-1, BEML-2, BEML-3) can be about 420 nm or more and 480 nm or less.

[0144] The fourth light-emitting layer (GEML) of the fourth light-emitting stack (ST4) can emit a second color light different from the first color light. For example, the second color light can be green light. The wavelength range of the light emitted by the fourth light-emitting layer (GEML) can be about 520 nm or more and 600 nm or less.

[0145] At least some of the first to fourth light-emitting layers (BEML-1, BEML-2, BEML-3, GEML) may have a bilayer structure including different host materials. For example, one layer of the bilayer structure may include a hole-transporting host material, and the other layer may include an electron-transporting host material. The electron-transporting host material may be a material including an electron-transporting moiety within its molecular structure.

[0146] The first light-emitting stack (ST1) may include a hole control layer (HTR) that transports holes provided from the first electrode (EL1) to the first light-emitting layer (BEML-1), and a first intermediate electron control layer (METL1) that transports electrons generated from the first charge generation layer (CGL1) to the first light-emitting layer (BEML-1).

[0147] The hole control layer (HTR) may include a hole injection layer (HIL) disposed on the first electrode (EL1) and a hole transport layer (HTL) disposed on the hole injection layer (HIL). However, the present invention is not limited thereto, and the hole control layer (HTR) may further include at least one of a hole buffer layer, a light-emitting auxiliary layer, and an electron blocking layer. The hole buffer layer may be a layer that compensates for a resonance distance according to a wavelength of light emitted from the light-emitting layer to increase light emission efficiency. The electron blocking layer may be a layer that serves to prevent electron injection from the electron control layer to the hole control layer.

[0148] The first intermediate electron control layer (METL1) may include a first intermediate electron transport layer disposed on the first light-emitting layer (BEML-1). However, the present invention is not limited thereto, and the first intermediate electron control layer (METL1) may further include at least one of an electron buffer layer and a hole blocking layer.

[0149] The second light-emitting stack (ST2) may include a first intermediate hole control layer (MHTR1) that transports holes generated from the first charge generation layer (CGL1) to the second light-emitting layer (BEML-2), and a second intermediate electron control layer (METL2) that transports electrons provided from the second charge generation layer (CGL2) to the second light-emitting layer (BEML-2).

[0150] The first intermediate hole control layer (MHTR1) may include a first intermediate hole injection layer (MHIL1) disposed on the first charge generation layer (CGL1) and a first intermediate hole transport layer (MHTL1) disposed on the first intermediate hole injection layer (MHIL1). The first intermediate hole control layer (MHTR1) may further include at least one of a hole buffer layer, an emission auxiliary layer, and an electron blocking layer disposed on the first intermediate hole transport layer (MHTL1).

[0151] The second intermediate electron control layer (METL2) may include a second intermediate electron transport layer disposed on the second light-emitting layer (BEML-2). However, the present invention is not limited thereto, and the second intermediate electron control layer (METL2) may further include at least one of an electron buffer layer and a hole blocking layer disposed between the second intermediate electron transport layer and the second light-emitting layer (BEML-2).

[0152] The third light-emitting stack (ST3) may include a second intermediate hole control layer (MHTR2) that transports holes generated from the second charge generation layer (CGL2) to the third light-emitting layer (BEML-3), and a third intermediate electron control layer (METL3) that transports electrons provided from the third charge generation layer (CGL3) to the third light-emitting layer (BEML-3).

[0153] The second intermediate hole control layer (MHTR2) may include a second intermediate hole injection layer (MHIL2) disposed on the second charge generation layer (CGL2) and a second intermediate hole transport layer (MHTL2) disposed on the second intermediate hole injection layer (MHIL2). However, the present invention is not limited thereto, and the second intermediate hole control layer (MHTR2) may further include at least one of a hole buffer layer, an emission auxiliary layer, and an electron blocking layer disposed on the second intermediate hole transport layer (MHTL2).

[0154] The third intermediate electron control layer (METL3) may include a third intermediate electron transport layer disposed on the third light-emitting layer (BEML-3). However, the present invention is not limited thereto, and the third intermediate electron control layer (METL3) may further include at least one of an electron buffer layer and a hole blocking layer disposed between the third intermediate electron transport layer and the third light-emitting layer (BEML-3).

[0155] The fourth light-emitting stack (ST4) may include a third intermediate hole control layer (MHTR3) that transports holes generated from the third charge generation layer (CGL3) to the fourth light-emitting layer (GEML), and an electron control layer (ETR) that transports electrons provided from the second electrode (EL2) to the fourth light-emitting layer (GEML).

[0156] The third intermediate hole control layer (MHTR3) may include a third intermediate hole injection layer (MHIL3) disposed on the third charge generation layer (CGL3) and a third intermediate hole transport layer (MHTL3) disposed on the third intermediate hole injection layer (MHIL3). However, the present invention is not limited thereto, and the third intermediate hole control layer (MHTR3) may further include at least one of a hole buffer layer, an emission auxiliary layer, and an electron blocking layer disposed on the third intermediate hole transport layer (MHTL3).

[0157] The electron control layer (ETR) may include an electron transport layer (ETL) disposed on the fourth light-emitting layer (GEML), and an electron injection layer (EIL) disposed on the electron transport layer (ETL). However, the present invention is not limited thereto, and the electron control layer (ETR) may further include at least one of an electron buffer layer and a hole blocking layer disposed between the electron transport layer (ETL) and the fourth light-emitting layer (GEML).

[0158] In one embodiment, the light emitting element (LED) can emit light from the first electrode (EL1) toward the second electrode (EL2), and, based on the direction of emitting light, the hole control layer (HTR) can be disposed below the plurality of light emitting stacks (ST1, ST2, ST3, ST4), and the electron control layer (ETR) can be disposed above the plurality of light emitting stacks (ST1, ST2, ST3, ST4). However, the present invention is not limited thereto, and may have an inverted device structure in which, based on the direction of emitting light, the electron control layer (ETR) is disposed below the plurality of light emitting stacks (ST1, ST2, ST3, ST4), and the hole control layer (HTR) is disposed above the plurality of light emitting stacks (ST1, ST2, ST3, ST4).

[0159] Referring back to FIG. 4A, the electron control layer (ETR) may be disposed between the light emitting layer (EML) and the second electrode (EL2). The electron control layer (ETR) may include at least one of an electron injection layer, an electron transport layer, and a hole blocking layer. Referring to FIG. 4A, the electron control layer (ETR) may be disposed as a common layer so as to overlap the entire light emitting areas (EA1, EA2, EA3) and the pixel defining layer (PDL) that separates the light emitting areas (EA1, EA2, EA3). However, the embodiment is not limited thereto, and the electron control layer (ETR) may be patterned and provided so as to be disposed separately corresponding to each of the light emitting areas (EA1, EA2, EA3).

[0160] The second electrode (EL2) is provided on the electronic control layer (ETR). The second electrode (EL2) may be a common electrode. The second electrode (EL2) may be a cathode or an anode, but the embodiment is not limited thereto. For example, when the first electrode (EL1) is an anode, the second electrode (EL2) may be a cathode, and when the first electrode (EL1) is a cathode, the second electrode (EL2) may be an anode. The second electrode (EL2) may be a transmissive electrode, a semi-transmissive electrode, or a reflective electrode.

[0161] The encapsulation layer (TFE) may be disposed on the light emitting element (LED). For example, in one embodiment, the encapsulation layer (TFE) may be disposed on the second electrode (EL2). In addition, when the light emitting element (LED) includes a capping layer (not shown), the encapsulation layer (TFE) may be disposed on the capping layer (not shown). As described above, the encapsulation layer (TFE) may include at least one organic film and at least one inorganic film, and the inorganic films and the organic films may be disposed alternately.

[0162] A display panel (DP) of one embodiment may include an optical structure layer (OSL) disposed on a display element layer (DP-LED). The optical structure layer (OSL) may include a light control layer (CCL), a color filter layer (CFL), and a base layer (BL).

[0163] The light control layer (CCL) may include a light converter. The light converter may be a quantum dot or a phosphor, etc. The light converter may convert the wavelength of the light provided and emit it. That is, the light control layer (CCL) may be a layer including quantum dots at least in a portion or a layer including a phosphor.

[0164] The light control layer (CCL) may include a plurality of light control patterns (CCP-R, CCP-B, CCP-G). The light control patterns (CCP-R, CCP-B, CCP-G) may be spaced apart from each other. The light control patterns (CCP-R, CCP-B, CCP-G) may be arranged to be spaced apart from each other by a bank (BMP). The light control patterns (CCP-R, CCP-B, CCP-G) may be arranged within a bank opening (BW-OH) defined in the bank (BMP). However, the embodiment is not limited thereto. In Fig. 4a, the bank (BMP) is depicted as having a rectangular shape in cross-section and not overlapping with the light control patterns (CCP-R, CCP-B, CCP-G), but the edges of the light control patterns (CCP-R, CCP-B, CCP-G) may overlap at least partly with the bank (BMP). The bank (BMP) may have a trapezoidal shape in cross-section. The bank (BMP) may have a shape whose cross-sectional width increases as it approaches the display element layer (DP-LED).

[0165] The light control pattern (CCP-R, CCP-B, CCP-G) may be a portion that converts the wavelength of light provided from the display element layer (DP-LED) or transmits the provided light. The light control pattern (CCP-R, CCP-B, CCP-G) may be formed by an inkjet process. A liquid ink composition may be provided within the bank opening (BW-OH), and the provided ink composition may be polymerized by a thermal curing process or a photocuring process to form the light control pattern (CCP-R, CCP-B, CCP-G).

[0166] The light control layer (CCL) may include a first light control pattern (CCP-R) including a first quantum dot that converts source light provided from a light emitting diode (LED) into a first light, a second light control pattern (CCP-B) that transmits the source light, and a third light control pattern (CCP-G) including a second quantum dot that converts the source light into a second light.

[0167] In one embodiment, the first light control pattern (CCP-R) may provide red light, which is the first light, and the second light control pattern (CCP-B) may transmit and provide blue light, which is the source light provided by the light-emitting element (LED). The third light control pattern (CCP-G) may provide green light, which is the second light. For example, the first quantum dot may be a red quantum dot and the second quantum dot may be a green quantum dot.

[0168] Additionally, the light control layer (CCL) may further include scatterers. The first light control pattern (CCP-R) may include first quantum dots and scatterers, the third light control pattern (CCP-G) may include second quantum dots and scatterers, and the second light control pattern (CCP-B) may not include quantum dots but include scatterers.

[0169] Each of the first light control pattern (CCP-R), the second light control pattern (CCP-B), and the third light control pattern (CCP-G) may include a base resin in which quantum dots and scatterers are dispersed. In one embodiment, the first light control pattern (CCP-R) may include first quantum dots and scatterers dispersed within the base resin, the third light control pattern (CCP-G) may include second quantum dots and scatterers dispersed within the base resin, and the second light control pattern (CCP-B) may include scatterers dispersed within the base resin.

[0170] The light control layer (CCL) includes a barrier layer (CAP1) arranged on one surface of the light control unit. The light control layer (CCL) may include a barrier layer (CAP1) spaced apart from the display element layer (DP-LED) with a light control pattern (CCP-R) therebetween and an additional barrier layer (CAP2) adjacent to the display element layer (DP-LED).

[0171] In a display panel (DP), an optical structure layer (OSL) includes a color filter layer (CFL) disposed on a light control layer (CCL). The color filter layer (CFL) may include color filters (CF1, CF2, CF3). The color filter layer (CFL) may include a first color filter (CF1) that transmits first light, a second color filter (CF2) that transmits source light, and a third color filter (CF3) that transmits the second light. In one embodiment, the first color filter (CF1) may be a red filter, the second color filter (CF2) may be a blue filter, and the third color filter (CF3) may be a green filter.

[0172] Each of the filters (CF1, CF2, CF3) includes a polymer photosensitive resin and a colorant. The first color filter (CF1) may include a red colorant, the second color filter (CF2) may include a blue colorant, and the third color filter (CF3) may include a green colorant. The first color filter (CF1) may include a red pigment or a red dye, the second color filter (CF2) may include a blue pigment or a blue dye, and the third color filter (CF3) may include a green pigment or a green dye.

[0173] Each of the first to third color filters (CF1, CF2, CF3) may be arranged to correspond to each of the first pixel area (PXA-R), the second pixel area (PXA-B), and the third pixel area (PXA-G). In addition, each of the first to third color filters (CF1, CF2, CF3) may be arranged to correspond to each of the first to third light control patterns (CCP-R, CCP-B, CCP-G).

[0174] In addition, a plurality of color filters (CF1, CF2, CF3) that transmit different light may be overlapped and arranged corresponding to the peripheral area (NPXA) arranged between the pixel areas (PXA-R, PXA-B, PXA-G). A plurality of color filters (CF1, CF2, CF3) may be overlapped and arranged in the third direction (DR3), which is the thickness direction, to distinguish the boundary between adjacent pixel areas (PXA-R, PXA-B, PXA-G). Meanwhile, unlike the drawing, the color filter layer (CFL) may include a light-shielding portion (not shown) that distinguishes the boundary between adjacent color filters (CF1, CF2, CF3). The light-shielding portion (not shown) may be formed by including a blue filter, or an organic light-shielding material including a black pigment or a black dye, or an inorganic light-shielding material.

[0175] The optical structure layer (OSL) may include a low-refractive-index layer (LR) disposed between a light control layer (CCL) and a color filter layer (CFL). The low-refractive-index layer (LR) may be disposed between light control patterns (CCP-R, CCP-B, CCP-G) and color filters (CF1, CF2, CF3). The low-refractive-index layer (LR) may be disposed on the light control layer (CCL) to block the light control patterns (CCP-R, CCP-B, CCP-G) from being exposed to moisture / oxygen. In addition, the low-refractive-index layer (LR) may be disposed between the light control patterns (CCP-R, CCP-B, CCP-G) and the color filters (CF1, CF2, CF3) to increase light extraction efficiency or may function as an optical functional layer to prevent reflected light from entering the light control layer (CCL). A low-refractive-index layer (LR) may be a layer with a lower refractive index compared to other adjacent layers.

[0176] The low-refractive-index layer (LR) may include at least one inorganic layer. For example, the low-refractive-index layer (LR) may include silicon nitride, aluminum nitride, zirconium nitride, titanium nitride, hafnium nitride, tantalum nitride, silicon oxide, aluminum oxide, titanium oxide, tin oxide, cerium oxide, and silicon oxynitride, or a metal thin film having secured light transmittance. However, the embodiment is not limited thereto, and the low-refractive-index layer (LR) may include an organic film. The low-refractive-index layer (LR) may have a structure in which a plurality of hollow particles are dispersed in an organic polymer resin, for example. The low-refractive-index layer (LR) may be composed of a single layer or a plurality of layers.

[0177] In one embodiment, the optical structure layer (OSL) may further include a base layer (BL) disposed on the color filter layer (CFL). The base layer (BL) may be a member that provides a base surface on which the color filter layer (CFL) and the light control layer (CCL) are disposed. The base layer (BL) may be a glass substrate, a metal substrate, a plastic substrate, or the like. However, the embodiment is not limited thereto, and the base layer (BL) may be an inorganic layer, an organic layer, or a composite material layer. In addition, unlike the embodiment illustrated, the base layer (BL) may be omitted in one embodiment.

[0178] FIGS. 4B and 4C each illustrate enlarged views of a portion of a cross-section of a display panel according to one embodiment of the present invention. FIGS. 4B and 4C each illustrate a display panel (DP) according to one embodiment of FIG. 4A and display panels (DP-1, DP-2) according to other embodiments.

[0179] Referring to FIG. 4B, a display panel (DP-1) according to one embodiment may include a lower panel including a base substrate (BS), a circuit element layer (DP-CL) disposed on the base substrate (BS), and a display element layer (DP-LED) disposed on the circuit element layer (DP-CL), and an optical structure layer (OSL-1) disposed on the lower panel. In the display panel (DP-1) according to one embodiment, the optical structure layer (OSL-1) may include a light control layer (CCL-1), a low-refractive-index layer (LR-1), a color filter layer (CFL-1), and a base layer (BL-1) sequentially laminated on a thin film encapsulation layer (TFE). The optical structure layer (OSL-1) may include a barrier layer (CAP1) and an additional barrier layer (CAP2) disposed on the upper and lower surfaces of the light control layer (CCL-1).

[0180] The light control layer (CCL-1) may be disposed on the display element layer (DP-LED) and the thin film encapsulation layer (TFE) with an additional barrier layer (CAP2) therebetween. The light control layer (CCL-1) may include a plurality of banks (BMP) and light control portions (CCP-B, CCP-G, CCP-R) disposed between the banks (BMP). A low-refractive-index layer (LR) may be disposed on the light control layer (CCL-1).

[0181] The color filter layer (CFL-1) may include a plurality of color filters (CF1, CF2, CF3) and a light-shielding portion (BM).

[0182] Compared to the display panel (DP) illustrated in FIG. 4a, the display panel (DP-1) according to an embodiment illustrated in FIG. 4b is an example in which a light control layer (CCL-1), a low-refractive layer (LR), and a color filter layer (CFL-1) are arranged with the upper surface of a thin film encapsulation layer (TFE) as a base surface. That is, the light control parts (CCP-B, CCP-G, CCP-R) of the light control layer (CCL-1) may be formed on the thin film encapsulation layer (TFE) through a continuous process, and the color filters (CF1, CF2, CF3) of the color filter layer (CFL-1) may be formed sequentially on the light control layer (CCL-1) through a continuous process. The light control layer (CCL-1) is formed using the upper surface of the additional barrier layer (CAP2) disposed on the thin film encapsulation layer (TFE) as a base surface, and may have a shape that is upside-down inverted from the shape of the light control layer (CCL) illustrated in FIG. 4a. Specifically, each of the plurality of banks (BMP) and the plurality of light control portions (CCP-B, CCP-G, CCP-R) may have a shape that is upside-down inverted from the shape illustrated in FIG. 4a. The color filter layer (CFL-1) is formed using the upper surface of the light control layer (CCL-1) as a base surface, and may have a shape different from the shape illustrated in FIG. 4a.

[0183] In one embodiment of the color filter layer (CFL-1), the light-shielding portion (BM) may be a black matrix. The light-shielding portion (BM) may be formed by including an organic light-shielding material or an inorganic light-shielding material including a black pigment or black dye. The light-shielding portion (BM) may prevent light leakage and demarcate boundaries between adjacent color filters (CF-B, CF-G, CF-R).

[0184] Referring to FIG. 4c, a display element layer (DP-ED1) included in a display panel (DP-2) of one embodiment includes a light-emitting element (LED-1), and the light-emitting element (LED-1) may be a micro LED element or a nano LED element. The light-emitting element (LED-1) may be disposed between pixel defining layers (PDLs) and may be electrically connected to a contact portion (SC), and the length and width of the light-emitting element (LED-1) may be between several hundred nanometers and several hundred micrometers. The light-emitting element (LED-1) may be an LED element including an active layer and at least one semiconductor material layer. The light-emitting element (LED-1) may further include an insulating layer covering surfaces of the active layer and the semiconductor material layer. The light-emitting element (LED-1) may be patterned and disposed to overlap each of the pixel areas (PXA-R, PXA-B, PXA-G). The display panel (DP) may include a buffer layer (BFL) disposed on the light-emitting element (LED-1). The buffer layer (BFL) may be disposed on the light-emitting element (LED-1) to cover the light-emitting element (LED-1). Meanwhile, in the display panel (DP-2) of the embodiment illustrated in FIG. 4C, the buffer layer (BFL) may be omitted.

[0185] FIG. 6A is a cross-sectional view of a portion of a display panel according to an embodiment of the present invention. FIG. 6B is an enlarged cross-sectional view of a portion of a display panel according to an embodiment of the present invention. FIG. 6A enlarges and illustrates a portion of a light control layer (CCL), a barrier layer (CAP1), an additional barrier layer (CAP2), a low-refractive layer (LR), and a color filter layer (CFL) included in an optical structure layer (OSL) of the display panel (DP) of an embodiment illustrated in FIG. 3. FIG. 6B enlarges and schematically illustrates the barrier layer (CAP1) of FIG. 6A and an adjacent portion thereof. Hereinafter, when describing the barrier layer (CAP1) included in the optical structure layer (OSL) of an embodiment with reference to FIGS. 6A and 6B, the third light control pattern (CCP-G) is referred to as a “light control pattern.” Meanwhile, in FIGS. 6a and 6b, the configuration illustrated in FIGS. 3 and 4a, etc. is rotated 180° to illustrate the configuration. The surface located above FIGS. 6a and 6b is described as the “bottom surface” and the surface located below is described as the “upper surface.”

[0186] Referring to FIGS. 3, 4a, 6a, and 6b, as described above, the optical structure layer (OSL) includes a barrier layer (CAP1) disposed on one surface of the light control pattern (CCP-G). The barrier layer (CAP1) may be disposed between the light control pattern (CCP-G) and the low-refractive-index layer (LR). That is, the barrier layer (CAP1) may be disposed on the upper surface of the light control pattern (CCP-G).

[0187] The barrier layer (CAP1) can be directly disposed on the upper surface of the light control pattern (CCP-G) and the bank (BMP). That is, the barrier layer (CAP1) can contact the upper surface of the light control pattern (CCP-G) and the bank (BMP).

[0188] The barrier layer (CAP1) is disposed between the light control pattern (CCP-G) and the low-refractive-index layer (LR), and may be disposed directly under the low-refractive-index layer (LR). The barrier layer (CAP1) may be in contact with the lower surface (LR-L) of the low-refractive-index layer (LR).

[0189] The barrier layer (CAP1) has a multi-layer structure, and each of the multi-layers included in the barrier layer (CAP1) includes silicon oxynitride (SiON). The barrier layer (CAP1) may have a multi-layer structure in which interfaces are defined therebetween and are distinguished from each other. The barrier layer (CAP1) has a multi-layer structure in order to prevent moisture / oxygen from penetrating into the light control pattern (CCP-G), increase film durability, and have a refractive index range that does not lower the light efficiency of the display panel, and limits the composition ratio of silicon, oxygen, and nitrogen of the multi-silicon oxynitride films to a certain range.

[0190] In one embodiment, the barrier layer (CAP1) includes a first layer (CAP1-1), a second layer (CAP1-2), and a third layer (CAP1-3) sequentially laminated from a low-refractive-index layer (LR). Each of the first layer (CAP1-1), the second layer (CAP1-2), and the third layer (CAP1-3) includes silicon oxynitride.

[0191] The first layer (CAP1-1) is disposed adjacent to the low-refractive-index layer (LR) and corresponds to a silicon oxynitride film having a relatively high oxygen content. The first layer (CAP1-1) may be a layer disposed directly under the low-refractive-index layer (LR). The first layer (CAP1-1) may be in contact with the low-refractive-index layer (LR). The upper surface (U1) of the first layer (CAP1-1) may be in contact with the lower surface (LR-L) of the low-refractive-index layer (LR).

[0192] The first layer (CAP1-1) is a layer having a low nitrogen content, and the nitrogen content of the first layer (CAP1-1) is less than 1 at%. The first layer (CAP1-1) may have, for example, a nitrogen content of 0.1 at% or more and 0.7 at% or less. The silicon oxynitride included in the first layer (CAP1-1) has a composition ratio of less than 1 at% of nitrogen, 45 at% or more and 70 at% or less of oxygen, and 30 at% or more and 55 at% or less of silicon. The silicon oxynitride included in the first layer (CAP1-1) may have, for example, a composition ratio of 0.5 at% or less of nitrogen, 58 at% or more and 70 at% or less of oxygen, and 30 at% or more and 42 at% or less of silicon. Since the first layer (CAP1-1) has a relatively low concentration of nitrogen atoms, film deterioration can be prevented under high temperature and high humidity conditions, etc. Additionally, it has the characteristics of not causing defects such as staining and lifting and of having a low amount of outgas emission.

[0193] The second layer (CAP1-2) is disposed on the first layer (CAP1-1) and corresponds to a silicon oxynitride film having a relatively high nitrogen content. The second layer (CAP1-2) may be a layer disposed spaced apart from the low-refractive-index layer (LR) with the first layer (CAP1-1) interposed therebetween. The second layer (CAP1-2) may be a layer disposed directly under the first layer (CAP1-1). The second layer (CAP1-2) may be in contact with the first layer (CAP1-1). The upper surface (U2) of the second layer (CAP1-2) may be in contact with the lower surface (L1) of the first layer (CAP1-1).

[0194] The second layer (CAP1-2) is a layer having a high nitrogen content, and the nitrogen content of the second layer (CAP1-2) is 3 at% or more and 30 at% or less. The second layer (CAP1-2) may have, for example, a nitrogen content of 15 at% or more and 22 at% or less. The silicon oxynitride included in the second layer (CAP1-2) has a composition ratio of 3 at% or more and 30 at% or less of nitrogen, 25 at% or more and 50 at% or less of oxygen, and 30 at% or more and 55 at% or less of silicon. The silicon oxynitride included in the second layer (CAP1-2) may have, for example, a composition ratio of 15 at% or more and 22 at% or less of nitrogen, 38 at% or more and 48 at% or less of oxygen, and 30 at% or more and 42 at% or less of silicon. The second layer (CAP1-2) has a relatively high concentration of nitrogen atoms and thus has high robustness characteristics in plasma. Since the optical structure layer (OSL) includes a barrier layer (CAP1) including a second layer (CAP1-2), the organic material included in the low-refractive-index layer (LR) can be prevented from being damaged by plasma or the like applied during formation of the barrier layer (CAP1). In addition, since the second layer (CAP1-2) satisfies the above composition ratio, the amount of surface moisture adsorption is reduced, and thus it can have excellent moisture blocking properties.

[0195] The third layer (CAP1-3) is disposed adjacent to the second layer (CAP1-2) and corresponds to a silicon oxynitride film having a relatively high oxygen content. The third layer (CAP1-3) may be a layer disposed directly below the second layer (CAP1-2). The third layer (CAP1-3) may be in contact with the second layer (CAP1-2). The upper surface (U3) of the third layer (CAP1-3) may be in contact with the lower surface (L2) of the second layer (CAP1-2). Meanwhile, the third layer (CAP1-3) may be directly disposed on the light control pattern (CCP-G) disposed below. The third layer (CAP1-3) may be in contact with the light control pattern (CCP-G) disposed below. The lower surface (L3) of the third layer (CAP1-3) may be in contact with the upper surface of the light control pattern (CCP-G).

[0196] The third layer (CAP1-3) is a layer having a low nitrogen content, and the nitrogen content of the third layer (CAP1-3) is less than 3.2 at%. The third layer (CAP1-3) may have, for example, a nitrogen content of 0.1 at% or more and 3 at% or less. The silicon oxynitride included in the third layer (CAP1-3) has a composition ratio of less than 3.2 at% of nitrogen, 45 at% or more and 70 at% or less of oxygen, and 30 at% or more and 55 at% or less of silicon. The silicon oxynitride included in the third layer (CAP1-3) may have, for example, a composition ratio of 0.5 at% or less of nitrogen, 58 at% or more and 70 at% or less of oxygen, and 30 at% or more and 42 at% or less of silicon. Since the third layer (CAP1-3) has a relatively low concentration of nitrogen atoms, film deterioration can be prevented under high temperature and high humidity conditions, etc. In addition, it has the characteristics of not causing defects such as staining and lifting and of having a low amount of outgassing. In addition, the third layer (CAP1-3) has a low refractive index by satisfying the above composition ratio, so that the light output efficiency of the display panel can be improved.

[0197] In the silicon oxynitride included in the first layer (CAP1-1) and the silicon oxynitride included in the second layer (CAP1-2), the nitrogen content of the second layer (CAP1-2) is 3 to 60 times the nitrogen content of the first layer (CAP1-1). For example, the nitrogen content of the second layer (CAP1-2) may be 15 to 40 times the nitrogen content of the first layer (CAP1-1). The barrier layer (CAP1) can prevent film quality degeneration under high temperature and high humidity conditions by arranging the first layer (CAP1-1) having a relatively low nitrogen content adjacent to the low-refractive-index layer (LR), and can effectively block moisture entering from the low-refractive-index layer (LR).

[0198] The total thickness of the barrier layer (CAP1) may be 2000Å or more and 12000Å or less.

[0199] The thickness (d1) of the first layer (CAP1-1) may be 500 angstroms (Å) or more and 5000 angstroms (Å) or less. When the thickness (d1) of the first layer (CAP1-1) is less than 500 Å, the barrier layer (CAP1) may undergo film quality transformation in which the barrier layer expands under high temperature and high humidity conditions, thereby deteriorating the moisture barrier properties of the barrier layer (CAP1). When the thickness (d1) of the first layer (CAP1-1) exceeds 5000 Å, it may be difficult to implement a film having a uniform thickness and composition during the process, thereby deteriorating the film properties, and the stress applied to the optical structure layer (OSL) may increase due to the thick barrier layer (CAP1), which may cause damage to the substrate, etc.

[0200] The thickness (d2) of the second layer (CAP1-2) may be 600 angstroms (Å) or more and 5000 angstroms (Å) or less. If the thickness (d2) of the second layer (CAP1-2) is less than 600 Å, the low refractive index layer (LR) may be damaged by the plasma applied during the film formation process. If the thickness (d2) of the second layer (CAP1-2) exceeds 5000 Å, it may be difficult to implement a film with a uniform thickness and composition during the process, which may result in deterioration of film characteristics, and the stress applied to the optical structure layer (OSL) may increase due to the thick barrier layer (CAP1), which may result in damage to the substrate, etc.

[0201] The thickness (d3) of the third layer (CAP1-3) may be 500 angstroms (Å) or more and 5000 angstroms (Å) or less. If the thickness (d3) of the third layer (CAP1-3) is less than 500 Å, recycling of light through the third layer (CAP1-3) having a low refractive index may not be realized. If the thickness (d3) of the third layer (CAP1-3) exceeds 5000 Å, it may be difficult to realize a film having a uniform thickness and composition during the process, which may result in deterioration of film characteristics, and the stress applied to the optical structure layer (OSL) may increase due to the thick barrier layer (CAP1), which may result in damage to the substrate, etc.

[0202] The third layer (CAP1-3) included in the barrier layer (CAP1) may have a lower refractive index compared to the adjacent layer. The third layer (CAP1-3) may have a lower refractive index compared to the adjacent second layer (CAP1-2) and the light control pattern (CCP-G).

[0203] The refractive index of the third layer (CAP1-3) may be 1.3 or more and 1.5 or less. For example, the third layer (CAP1-3) may have a refractive index of 1.3 or more and 1.5 or less for light in the wavelength range of 400 nm to 700 nm.

[0204] The refractive index of the first layer (CAP1-1) may be 1.3 or more and 1.5 or less. For example, the first layer (CAP1-1) may have a refractive index of 1.3 or more and 1.5 or less for light in the wavelength range of 400 nm to 700 nm.

[0205] The refractive index of the second layer (CAP1-2) may be 1.4 or more and 1.8 or less. For example, the second layer (CAP1-2) may have a refractive index of 1.4 or more and 1.8 or less for light in the wavelength range of 400 nm to 700 nm.

[0206] In one embodiment, the third layer (CAP1-3) included in the barrier layer (CAP1) has a lower refractive index than the adjacent light control pattern (CCP-G), and the difference between the refractive index of the third layer (CAP1-3) and the refractive index of the light control pattern (CCP-G) may be 0.1 or more and 0.25 or less. For example, the difference between the refractive index of the third layer (CAP1-3) and the refractive index of the light control pattern (CCP-G) may be 0.15 or more and 0.2 or less. In one embodiment, the refractive index of the light control pattern (CCP-G) may be 1.5 or more and 1.7 or less.

[0207] In one embodiment, the refractive index of the third layer (CAP1-3) included in the barrier layer (CAP1) can be adjusted to be lower than the refractive index of the light control pattern (CCP-G), while the difference between the refractive index of the third layer (CAP1-3) and the refractive index of the light control pattern (CCP-G) can be adjusted to 0.1 or more. Specifically, the third layer (CAP1-3) of one embodiment can be adjusted to have a refractive index of the third layer (CAP1-3) 0.1 or more lower than the refractive index of the light control pattern (CCP-G) by adjusting the composition ratio of silicon, oxygen, and nitrogen as described above. Through this, the light extraction efficiency of the light control pattern (CCP-G) can be increased, and reflected light can be prevented from entering the light control pattern (CCP-G).

[0208] In one embodiment, the first layer (CAP1-1) included in the barrier layer (CAP1) may have a higher refractive index than the adjacent low-refractive layer (LR). The low-refractive layer (LR) may have a low refractive index of 1.3 or less for light in the wavelength range of 400 nm to 700 nm. The first layer (CAP1-1) may have a higher refractive index than the adjacent low-refractive layer (LR), thereby allowing the low-refractive layer (LR) to have characteristics of increasing light extraction efficiency and anti-reflection characteristics.

[0209] According to one embodiment, the light control layer (CCL) may further include an additional barrier layer (CAP2). The additional barrier layer (CAP2) may be disposed under the light control pattern (CCP-G). More specifically, the additional barrier layer (CAP2) may be disposed between the light control pattern (CCP-G) and the filling layer (FML).

[0210] The additional barrier layer (CAP2) may include silicon oxynitride, similarly to the barrier layer (CAP1). The composition ratio of silicon, oxygen, and nitrogen in the additional barrier layer (CAP2) including silicon oxynitride may be in the same range as the composition ratio of any one of the plurality of layers included in the aforementioned barrier layer (CAP1). The additional barrier layer (CAP2) includes silicon oxynitride, and may have a composition ratio of less than 1 at% of nitrogen, 45 at% or more and 70 at% or less of oxygen, and 30 at% or more and 55 at% or less of silicon, similarly to the first layer (CAP1-1). However, the present invention is not limited thereto, and the additional barrier layer (CAP2) may include silicon oxynitride, but may have a composition ratio of silicon, oxygen, and nitrogen in a different range from the composition ratios of the plurality of layers included in the barrier layer (CAP1). Alternatively, the additional barrier layer (CAP2) may not include silicon oxynitride, but may include silicon oxide or silicon nitride. The additional barrier layer (CAP2) may also include titanium oxide, aluminum oxide, or the like.

[0211] The additional barrier layer (CAP2) may have a lower refractive index than the adjacent light control pattern (CCP-G). The refractive index of the additional barrier layer (CAP2) may be 1.3 or more and 1.8 or less. For example, the additional barrier layer (CAP2) may have a refractive index of 1.4 or more and 1.5 or less for light in the wavelength range of 400 nm to 700 nm.

[0212] In one embodiment, the additional barrier layer (CAP2) has a lower refractive index than the adjacent light control pattern (CCP-G), and the difference between the refractive index of the additional barrier layer (CAP2) and the refractive index of the light control pattern (CCP-G) may be 0.1 or more and 0.25 or less. For example, the difference between the refractive index of the additional barrier layer (CAP2) and the refractive index of the light control pattern (CCP-G) may be 0.15 or more and 0.2 or less. In one embodiment, the refractive index of the light control pattern (CCP-G) may be 1.6 or more and 1.95 or less. Through this, total reflection of light moving from the light control pattern (CCP-G) toward the additional barrier layer (CAP2) may be induced, thereby enabling recycling of light moving downward. Therefore, the light conversion efficiency of the light control pattern (CCP-G) may be increased, and when applied to a display panel, the display efficiency of the display panel may be improved.

[0213] In one embodiment, the additional barrier layer (CAP2) has a lower refractive index than that of the filling layer (FML), and the difference between the refractive index of the additional barrier layer (CAP2) and the filling layer (FML) can be controlled to 0.1 or less. Specifically, as described above, the additional barrier layer (CAP2) in one embodiment can be controlled by controlling the composition ratio of silicon, oxygen, and nitrogen so that the refractive index of the additional barrier layer (CAP2) is lower than that of the filling layer (FML), but the difference is within a range of 0.1 or less. Through this, the problem of light traveling from the filling layer (FML) toward the additional barrier layer (CAP2) being prevented from having its path changed through refraction, total reflection, etc. and not traveling toward the light control pattern (CCP-G) can be prevented.

[0214] The thickness of the additional barrier layer (CAP2) may be 2000 Å or more and 12000 Å or less. The additional barrier layer (CAP2) may have a thickness (d2) of, for example, 4000 Å or more and 8000 Å or less. If the thickness of the additional barrier layer (CAP2) is less than 2000 Å, the moisture and oxygen barrier properties may deteriorate, causing moisture, etc. to penetrate into the light control pattern (CCP-G), and the durability may decrease, resulting in defects such as lifting or film breakage. If the thickness of the additional barrier layer (CAP2) exceeds 12000 Å, it may be difficult to implement a film with a uniform thickness and composition in the process, causing film properties to deteriorate, and the stress applied to the optical structure layer (OSL) may increase due to the thick additional barrier layer (CAP2), which may cause damage to the substrate, etc.

[0215] A barrier layer (CAP1) according to one embodiment of the present invention has a multi-layer structure including silicon oxynitride, and by controlling the nitrogen content of each layer differently, it has excellent moisture and oxygen blocking properties, and has excellent film durability under high temperature and high humidity conditions, so that defects such as film denaturation and breakage due to external factors can be prevented. In addition, by controlling the refractive index of the barrier layer (CAP1) to correspond to the refractive index of an adjacent layer, the light conversion efficiency of the light control pattern can be improved. More specifically, the barrier layer (CAP1) includes a structure in which a first layer (CAP1-1) having a relatively low nitrogen content, a second layer (CAP1-2) having a relatively high nitrogen content, and a third layer (CAP1-3) having a low nitrogen content and a low refractive index are sequentially laminated, so that film degeneration under high temperature and high humidity conditions can be prevented, moisture entering from the low refractive index layer (LR) can be effectively blocked, and damage to the low refractive index layer (LR) due to plasma or the like applied during formation of the barrier layer (CAP1) can be prevented. In addition, through the third layer (CAP1-3) having a low refractive index, the light output efficiency of the optical structure layer (OSL) including the barrier layer (CAP1) and the display panel (DP) can be improved.

[0216] The low-refractive-index layer (LR) is disposed on top of the barrier layer (CAP) with respect to the third direction (DR3) and may have a structure in which a plurality of hollow particles are dispersed in the organic base layer. As illustrated in Fig. 6b, the low-refractive-index layer (LR) may include a base resin (PY) and a plurality of hollow particles (VD) dispersed in the base resin (PY). The low-refractive-index layer (LR) may have a low refractive index by including a plurality of hollow particles (VD).

[0217] Based on the total weight of the low refractive index layer (LR), the weight of the base resin (PY) may be 50 wt% or more and 90 wt% or less. The base resin (PY) may include at least one of an acrylic resin, a silicone resin, and an epoxy resin. For example, the base resin (PY) may include silicone acrylate.

[0218] In one embodiment, the hollow particles (VD) may be derived from a porogen. The low refractive index layer (LR) may be formed from a composition comprising a polymer resin and a porogen. The polymer resin of the composition may be solidified to form a base resin (PY), and the porogen may be thermally decomposed to form the hollow particles (VD). The hollow particles (VD) formed from the porogen may be spherical. The hollow particles (VD) may be vacuum or contain a very small amount of gas. Alternatively, each of the hollow particles (VD) may be filled with air or liquid.

[0219] Based on the total weight of the low-refractive-index layer (LR), the porogen may be provided in an amount of 10 wt% or more and 40 wt% or less. The low-refractive-index layer (LR) including hollow particles (VD) formed from the porogen in an amount of 10 wt% or more and 30 wt% or less may satisfy the refractive index range of the low-refractive-index layer (LR) according to one embodiment and exhibit excellent durability.

[0220] Although not shown, the low refractive index layer (LR) may further include additional materials, such as inorganic particles, in addition to the base resin (PY) and hollow particles (VD). The inorganic particles may include, for example, at least one of SiO2, MgF2, and Fe3O4.

[0221] The low-refractive-index layer (LR) can be formed using methods such as slit coating, spin coating, roll coating, spray coating, and inkjet printing. However, these are merely examples, and the method of forming the low-refractive-index layer (LR) is not limited thereto. The low-refractive-index layer (LR) can be formed using various methods, such as the transfer method.

[0222] The low-refractive-index layer (LR) may have a lower refractive index than adjacent components. The refractive index of the low-refractive-index layer (LR) may be lower than the refractive indices of each of the light control pattern (CCP-G) included in the light control layer (CCL) and the barrier layer (CAP1). In one embodiment, the refractive index of the low-refractive-index layer (LR) may be 1.21 or more and 1.25 or less. The low-refractive-index layer (LR) may totally reflect some of the blue light emitted from the light control layer (CCL) toward the color filter layer (CFL) and re-incident into the light control layer (CCL). The low-refractive-index layer (LR) having a refractive index of 1.21 or more and 1.25 or less may exhibit a characteristic of easy total reflection due to the difference in refractive index with respect to the light control layer (CCL).

[0223] The low refractive index (LR) layer may have a haze value less than 0.40%. A low refractive index (LR) layer having a haze value less than 0.40% may be optically transparent.

[0224] Fig. 7 is a cross-sectional view of a portion of a display panel according to one embodiment of the present invention. Fig. 7 illustrates an optical structure layer (OSL) of a different embodiment from the optical structure layer (OSL) illustrated in Fig. 6a in a cross-section corresponding to Fig. 6a.

[0225] Referring to FIG. 7, the second layer (CAP1-2') included in the barrier layer (CAP1') may have a multi-layer structure. The second layer (CAP1-2') may include a second-first layer (CAP1-21) disposed adjacent to the first layer (CAP1-1), and a second-second layer (CAP1-22) disposed between the second-first layer (CAP1-21) and the third layer (CAP1-3). Meanwhile, FIG. 7 exemplarily illustrates that the second layer (CAP1-2') having a multi-layer structure includes two layers, but the present invention is not limited thereto, and the second layer (CAP1-2') may include three or more layers.

[0226] The second-1 layer (CAP1-21) and the second-2 layer (CAP1-22) may each include silicon oxynitride, but may have different composition ratios. The second-1 layer (CAP1-21) and the second-2 layer (CAP1-22) may have different nitrogen contents. The second-1 layer (CAP1-21) and the second-2 layer (CAP1-22) may have different composition ratios while conforming to the composition ratio limitation range of silicon, oxygen, and nitrogen of the second layer (CAP1-2') described above. The second-1 layer (CAP1-21) and the second-2 layer (CAP1-22) included in the second layer (CAP1-2') may each have a composition ratio of silicon, oxygen, and nitrogen adjusted to a different range in order to improve the durability and optical properties of the optical structure layer (OSL).

[0227] Table 1 below shows the results of reliability evaluation under high temperature and high humidity conditions according to the laminated structure of the display panel including the aforementioned barrier layer and the nitrogen content of each layer. In Table 1, the barrier layer of the embodiment is a barrier layer having a three-layer laminated structure of the first layer, the second layer, and the third layer as shown in FIGS. 6a and 6b, and the barrier layer of the comparative example corresponds to a barrier layer having a two-layer laminated structure, unlike the embodiment. Meanwhile, the reliability evaluation was conducted by checking whether the barrier layer was lifted after being left for 500 hours under the conditions of 95°C and 85% humidity, and if lifted, it was evaluated as “defective.”

[0228] Number of times defects occur in the laminated structure / number of times of evaluation Defect occurrence time Example 11th layer (N 0.5%) 700Å / 2nd layer (N 19.1%) 1500Å / 3rd layer (N 0.4%) 800Å 0 / 2-Example 21st layer (N 0.5%) 500Å / 2nd layer (N 19.1%) 800Å / 3rd layer (N 0.4%) 700Å 0 / 2-Comparative example 1st layer (N 19.1%) 2000Å / 2nd layer (N 0.4%) 2000Å 16 / 21500hr(3)200hr(4)168hr(6)336hr(3)

[0229] Referring to the results in Table 1 above, in the case of including a barrier layer having a two-layer structure as in the comparative example, many defects occurred in which the barrier layer was lifted under high temperature and high humidity conditions, but in the case of the example, it can be confirmed that the barrier layer lifting defect did not occur under high temperature and high humidity conditions. Through the results in Table 1, in the case of the barrier layer of the example, since the first layer adjacent to the low refractive index layer was formed with a nitrogen content of less than 1 at%, it can be confirmed that the barrier layer lifting due to moisture permeation did not occur under high temperature and high humidity reliability evaluation conditions. Accordingly, it can be expected that the reliability and durability of the optical structure layer and display panel including the barrier layer of the example will increase.

[0230] While the present invention has been described above with reference to preferred embodiments, it will be understood by those skilled in the art or those with ordinary knowledge in the art that various modifications and changes can be made to the present invention without departing from the spirit and technical scope of the present invention as set forth in the claims below. Accordingly, the technical scope of the present invention should not be limited to the contents described in the detailed description of the specification, but should be defined by the claims.

[0231]

[0232] Recent display devices include different types of light control patterns for each pixel to generate color images, resulting in a wide viewing angle and excellent color reproducibility. Meanwhile, display devices including light control patterns may have light conversion efficiency reduced due to corrosion of light-emitting elements, such as quantum dots, included in the light control patterns by moisture and oxygen, which may lower the display efficiency of the display panel. According to an embodiment of the present invention, a display panel has excellent moisture and oxygen blocking properties of a barrier layer formed on one surface of the light control pattern, and excellent film durability under high temperature and high humidity conditions, thereby preventing defects, such as film degeneration and breakage, caused by external factors. Therefore, the present invention, which provides a display panel according to an embodiment, has high industrial applicability.

Claims

1. A light-emitting element that outputs source light and includes a first electrode, a light-emitting layer disposed on the first electrode, and a second electrode disposed on the light-emitting layer; and An optical structure layer disposed on the light-emitting element; The above optical structure layer A light control layer disposed on the light emitting element and including at least one light control pattern; A low refractive index layer disposed on the above light control layer; and A barrier layer is disposed between the light control layer and the low refractive index layer and includes silicon oxynitride (SiON). The above barrier layer A first layer disposed adjacent to the low refractive index layer and having a nitrogen content of less than 1 at%; A second layer spaced apart from the low-refractive-index layer with the first layer interposed therebetween, and having a nitrogen content of 3 at% or more and 30 at% or less; and A display panel comprising: a third layer, which is spaced apart from the low-refractive-index layer and interposed between the first layer and the second layer, and has a nitrogen content of less than 3.2 at%; 2. In paragraph 1, A display panel having a refractive index of the third layer of 1.3 or more and 1.5 or less for light in the wavelength range of 400 nm to 700 nm.

3. In paragraph 1, The above first layer is directly disposed on the low refractive index layer, The second layer is placed directly on the first layer, The third layer above is a display panel directly placed on the second layer above.

4. In paragraph 1, A display panel wherein the thickness of the first layer is 500 angstroms (Å) or more.

5. In paragraph 1, The above optical structure layer A display panel further comprising a color filter layer, spaced apart from the light control layer with the low refractive index layer interposed therebetween, and including a plurality of color filters.

6. In paragraph 1, The above light control pattern includes a first light control pattern that converts the source light into a first light and a second light control pattern that transmits the source light, A display panel wherein the first light control pattern includes a first quantum dot that converts the source light into the first light.

7. In paragraph 1, The above optical control layer further includes a bank arranged between the optical control patterns, A display panel in which the above barrier layer is directly disposed on one surface of the light control pattern and the bank.

8. In paragraph 1, A display panel comprising: the low-refractive-index layer; and a plurality of hollow particles dispersed in the base resin.

9. In paragraph 1, A display panel wherein the above low-refractive layer has a refractive index of 1.3 or less for light in the wavelength range of 400 nm to 700 nm.

10. In paragraph 1, The second layer above A 2-1 layer positioned adjacent to the above 1st layer; and A display panel comprising a 2-2 layer disposed between the 2-1 layer and the 3rd layer and having a different nitrogen content from the 2-1 layer.

11. In paragraph 1, The above optical structure layer Further comprising an additional barrier layer spaced apart from the barrier layer with the light control layer interposed therebetween, A display panel wherein the additional barrier layer is directly disposed on one side of the light control pattern.

12. In paragraph 1, A display panel further comprising a filling layer disposed between the light-emitting element and the optical structure layer and covering the light-emitting element.

13. In paragraph 1, The above first layer has a refractive index of 1.3 or more and 1.5 or less for light in the wavelength range of 400 nm to 700 nm, A display panel wherein the second layer has a refractive index of 1.4 or more and 1.8 or less for light in the wavelength range of 400 nm to 700 nm.

14. In paragraph 1, The third layer is a display panel that contacts one side of the light control pattern.

15. In paragraph 1, The light emitting element is disposed between the first electrode and the second electrode, and includes a plurality of light emitting stacks, each of which includes the light emitting layer. The above multiple light emitting stacks A first light-emitting stack disposed on the first electrode and including a first light-emitting layer; a charge generation layer disposed on the first stack; and a second light-emitting stack disposed on the charge generating layer and including a second light-emitting layer; A display panel in which the first light-emitting layer emits light of a different color from the second light-emitting layer.

16. A light-emitting element that outputs source light and includes a first electrode, a light-emitting layer disposed on the first electrode, and a second electrode disposed on the light-emitting layer; and An optical structure layer disposed on the light-emitting element; The above optical structure layer A light control layer disposed on the light emitting element and including at least one light control pattern; A low refractive index layer disposed on the above light control layer; and Including a barrier layer disposed between the light control layer and the low refractive index layer, The above barrier layer is sequentially arranged from the low refractive index layer, and includes a first layer, a second layer, and a third layer, each of which includes silicon oxynitride (SiON). The nitrogen content of the second layer is 3 times or more and 60 times or less than the nitrogen content of the first layer, A display panel having a nitrogen content of the third layer of less than 3.2 at%.

17. In paragraph 16, The above first layer is placed directly below the low-refractive layer, The second layer is placed directly below the first layer, The third layer is a display panel placed directly below the second layer.

18. A light-emitting element that outputs source light and includes a first electrode, a light-emitting layer disposed on the first electrode, and a second electrode disposed on the light-emitting layer; and An optical structure layer disposed on the light-emitting element; The above optical structure layer A light control layer disposed on the light emitting element and including at least one light control pattern; A low refractive index layer disposed on the above light control layer; and A barrier layer is disposed between the light control layer and the low refractive index layer and includes silicon oxynitride (SiON). The above barrier layer A first layer disposed directly below the low-refractive-index layer and having a nitrogen content of less than 1 at%; A second layer disposed directly below the first layer and having a nitrogen content of 3 at% or more and 30 at% or less; and a third layer disposed directly below the second layer; A display panel in which the above light control layer is placed directly under the third layer.

19. In paragraph 18, The above first layer has a refractive index of 1.3 or more and 1.5 or less for light in the wavelength range of 400 nm to 700 nm, The second layer has a refractive index of 1.4 or more and 1.8 or less for light in the wavelength range of 400 nm to 700 nm, The third layer is a display panel having a refractive index of 1.3 or more and 1.5 or less for light in the wavelength range of 400 nm to 700 nm.

20. In paragraph 18, The thickness of the first layer is 500 angstroms (Å) or more, The thickness of the second layer is greater than or equal to 600 angstroms (Å), A display panel wherein the thickness of the third layer is 500 angstroms (Å) or more.

Citation Information

Patent Citations

  • Electroluminescent display with improved light outcoupling

    KR1020050072424A

  • Tile measuring device and method saving power consumption

    KR102701542B1

  • Color change member, light emitting device, display device and electronic apparatus

    US20150276175A1

  • Organic device, display apparatus, image capturing apparatus, illumination apparatus, and moving body

    US20220359849A1

  • KR20210091384A