Semiconductor structure and manufacturing method
Through ion beam deposition technology, the combination of sputtering and auxiliary ion beams is used to form a high-quality adhesive barrier layer and seed layer, which solves the coverage and purity problems in the existing technology and achieves efficient integrated circuit device manufacturing.
Patent Information
- Application Number
- PCT/CN2024/095973
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-11
- Filing Date
- 2024-05-29
- Publication Date
- 2024-10-17
AI Technical Summary
The existing technology has challenges in preparing trench adhesion barrier layers and seed layers with high purity and high step coverage. The traditional magnetron sputtering process has low coverage, the ALD deposition failure rate is high, and the purity and performance are poor, making it difficult to meet the requirements. Manufacturing needs after integrated circuit device size shrinks.
Ion beam deposition technology is used to generate a neutral ion beam through a sputtering ion source and an auxiliary ion source, bombard the target along a specific angle, and form a high-quality adhesive barrier layer and seed layer. The sputtering ion source and the auxiliary ion source are used to Cooperate to ensure that sputtered particles effectively enter the bottom of the trench to achieve high step coverage and shape retention.
The preparation of trench adhesion barrier layer and seed layer with high quality and high step coverage is achieved, which improves the performance and manufacturing efficiency of integrated circuit devices and solves the problem of filling the adhesion layer and seed layer after the device size is reduced.
Smart Images

Figure CN2024095973_17102024_PF_FP_ABST
Abstract
Description
Semiconductor structure and preparation method
[0001] This application claims priority to the Chinese patent application filed with the China Patent Office on April 11, 2023, with application number 202310380302.5 and invention name “A semiconductor structure and preparation method”, the entire contents of which are incorporated by reference into this application. Technical Field
[0002] The present application relates to the field of semiconductor technology, and in particular to a semiconductor structure and a preparation method thereof. Background Art
[0003] As integrated circuit device sizes continue to shrink, their manufacturing process requirements are also facing significant challenges. In particular, in back-end copper interconnects and back-gate wire connections, as device dimensions shrink, via sizes become smaller and aspect ratios become higher. Uniform and void-free trench filling with adhesion barrier and seed layers is a significant challenge in existing integrated circuit manufacturing technologies.
[0004] Conventional technology has traditionally used magnetron sputtering, a PVD (Physical Vapor Deposition) technique, to fill conventional trench adhesion barrier and seed layers. However, the film deposited in the trench by conventional magnetron sputtering has low step coverage, and the overhang at the top of the trench can seriously affect the quality of subsequent electroplating, resulting in a failure to fill the bottom, which in turn affects the performance of the entire device.
[0005] ALD (atomic layer deposition) metal deposition has a high failure rate, poor purity and performance, and is limited by precursor separation, resulting in a very slow ALD deposition rate. Consequently, the preparation of high-purity, high-step coverage trench adhesion and seed layers remains a significant challenge.
[0006] Summary of the Invention
[0007] In view of this, this Summary of the Invention section is provided to briefly introduce the concepts that will be described in detail in the Detailed Description of the Invention section below. This Summary of the Invention section is not intended to identify key features or essential features of the claimed technical solution, nor is it intended to limit the scope of the claimed technical solution.
[0008] The purpose of this application is to provide a semiconductor structure and a preparation method, which can prepare a trench adhesion barrier layer and a seed layer with high quality and high step coverage.
[0009] To achieve the above objectives, this application has the following technical solutions:
[0010] In a first aspect, an embodiment of the present application provides a method for preparing a semiconductor structure, comprising:
[0011] Step 1: providing a substrate with grooves;
[0012] Step 2: bombarding the first target material with a neutral ion beam generated by a sputtering ion source of an ion beam deposition device to generate first sputtered particles;
[0013] Step 3: using a neutral ion beam generated by an auxiliary ion source of the ion beam deposition device to change the incident direction of the first sputtered particles to form an adhesion barrier layer on the inner wall of the trench;
[0014] Step 4: bombarding a second target material with the neutral ion beam generated by the sputtering ion source to generate second sputtered particles;
[0015] Step 5: Using the neutral ion beam generated by the auxiliary ion source, change the incident direction of the second sputtered particles to form a seed layer on the inner wall of the groove; the angle between the auxiliary ion source and the normal of the substrate surface is an acute angle.
[0016] In a possible implementation, providing a substrate with grooves includes:
[0017] providing an initial substrate;
[0018] Depositing a hard mask on the initial substrate and defining structured regions by photolithography;
[0019] The initial substrate in the structure area is etched to form the substrate with grooves.
[0020] In a possible implementation, the opening width of the trench is equal to the bottom width of the trench.
[0021] In a possible implementation, the opening width of the trench is greater than the bottom width of the trench.
[0022] In a possible implementation, forming an adhesion barrier layer on an inner wall of the trench includes: forming an adhesion barrier layer on a sidewall of the trench;
[0023] Forming a seed layer on an inner wall of the trench includes: forming a seed layer on a sidewall of the trench.
[0024] In a possible implementation, after providing the substrate with grooves and before bombarding the first target material with a neutral ion beam generated by a sputtering ion source of an ion beam deposition device to generate first sputtered particles, the method further includes:
[0025] The trench is pre-cleaned using a neutral ion beam generated by the auxiliary ion source to remove impurities on the surface of the trench.
[0026] In a possible implementation, during the forming of the adhesion barrier layer and the forming of the seed layer, the substrate is controlled to maintain self-rotation.
[0027] In a possible implementation, the neutral ion beam of the sputtering ion source includes an ion beam formed by any one or more inert gases of He, Ne, Ar, Kr, and Xe.
[0028] In a possible implementation, the neutral ion beam used by the auxiliary ion source includes: an ion beam formed by one or more inert gases.
[0029] In a possible implementation, the ion beam used by the auxiliary ion source includes a mixed gas of one or more inert gases and nitrogen.
[0030] In one possible implementation, the adhesion barrier layer is made of one or more of titanium, tantalum, titanium nitride, and tantalum nitride. In one possible implementation, the seed layer is made of one or more of aluminum, copper, and tungsten.
[0031] In a possible implementation, the aspect ratio of the trench is in the range of [2:1, 15:1].
[0032] In a possible implementation, the purity of the first target material and the second target material is greater than or equal to 99.9% and less than or equal to 99.9999%.
[0033] In a possible implementation, an angle between the auxiliary ion source and the normal direction of the substrate surface is greater than 0° and less than or equal to 30°.
[0034] In a possible implementation, the rotation speed range is greater than or equal to 5 rpm and less than or equal to 200 rpm.
[0035] In a possible implementation, the thickness of the adhesion barrier layer is greater than or equal to 2 nm and less than or equal to 100 nm.
[0036] In a possible implementation, the thickness of the seed layer is greater than or equal to 2 nm and less than or equal to 100 nm.
[0037] In one possible implementation, the grid of the sputtering ion source is arc-shaped to focus the ion beam onto the target surface, and the radius of the arc is greater than or equal to 300 mm and less than or equal to 800 mm. In another possible implementation, the grid of the sputtering ion source is planar, and the grid is provided with a plurality of through holes, and the coverage area of the plurality of through holes is [0.25 times, 0.75 times] the area of the first target or the second target.
[0038] In a possible implementation, a deposition rate of the adhesion barrier layer is greater than or equal to 3 nm / min and less than or equal to 30 nm / min.
[0039] In a possible implementation, the deposition rate of the seed layer is greater than or equal to 3 nm / min and less than or equal to 30 nm / min.
[0040] In a possible implementation, the sample temperature for depositing the first target material is [50° C., 300° C.], and the sample temperature for depositing the second target material is (0° C., 100° C.).
[0041] In a second aspect, an embodiment of the present application provides a semiconductor structure, including a structure prepared using the method described above.
[0042] Compared with the prior art, the embodiments of the present application have the following beneficial effects:
[0043] The present invention provides a semiconductor structure and preparation method, which includes: providing a substrate with a groove; bombarding a first target material with a neutral ion beam generated by a sputtering ion source of an ion beam deposition device to generate first sputtered particles; changing the incident direction of the first sputtered particles with a neutral ion beam generated by an auxiliary ion source of the ion beam deposition device to form an adhesion barrier layer on the inner wall of the groove; bombarding a second target material with a neutral ion beam generated by the sputtering ion source to generate second sputtered particles; changing the incident direction of the second sputtered particles with a neutral ion beam generated by the auxiliary ion source to form a seed layer on the inner wall of the groove; and forming an acute angle between the auxiliary ion source and the normal of the substrate surface. Ion beam deposition can guide the sputtered particles to be incident at a certain angle so that the sputtered particles can better enter the bottom of the groove, achieving better step coverage and conformality. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the following briefly introduces the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0045] FIG1 shows a schematic diagram of a conventional trench structure;
[0046] FIG2 shows a flow chart of a method for preparing a semiconductor structure provided in an embodiment of the present application;
[0047] FIG3 is a schematic diagram showing a structure of a semiconductor structure during a preparation process provided by an embodiment of the present application;
[0048] FIG4 shows a schematic diagram of an ion beam deposition device provided in an embodiment of the present application;
[0049] FIG5 is a schematic diagram showing a structure of another semiconductor structure during preparation according to an embodiment of the present application;
[0050] FIG6 shows a schematic diagram of a semiconductor structure provided by an embodiment of the present application;
[0051] FIG7 shows a schematic diagram of a grid structure in a sputtering ion source provided in an embodiment of the present application;
[0052] FIG8 is a schematic diagram showing another grid structure in a sputtering ion source provided in an embodiment of the present application;
[0053] FIG9 shows a schematic diagram of another semiconductor structure provided by an embodiment of the present application;
[0054] FIG10 shows a schematic diagram of another semiconductor structure provided in an embodiment of the present application. DETAILED DESCRIPTION
[0055] In order to make the above-mentioned purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are described in detail below with reference to the accompanying drawings.
[0056] In the following description, many specific details are set forth to facilitate a full understanding of the present application. However, the present application may also be implemented in other ways different from those described herein. Those skilled in the art may make similar generalizations without violating the connotation of the present application. Therefore, the present application is not limited to the specific embodiments disclosed below.
[0057] As described in the background technology, the applicant has found through research that integrated circuits (ICs) often include millions of electronic devices. With the development of technology and the continuous improvement of application requirements, integrated circuits are developing towards miniaturization, multi-layering, flattening and thinning. Ultra-large-scale integrated circuit trench filling is an important link in three-dimensional integrated circuits.
[0058] As integrated circuit device sizes continue to shrink, their manufacturing process requirements are also facing significant challenges. In particular, in back-end copper interconnects and back-gate wire connections, as device dimensions shrink, via sizes become smaller and aspect ratios become higher. Uniform and void-free trench filling with adhesion barrier and seed layers is a significant challenge in existing integrated circuit manufacturing technologies.
[0059] In conventional technology, people have always used magnetron sputtering, a PVD (Physical Vapor Deposition) technology, to fill conventional trench adhesion barrier layers and seed layers. The conventional magnetron sputtering process does not have high step coverage of the film deposited in the trench. For example, see Figure 1, which is a schematic diagram of a conventional trench structure, including a substrate 1, a trench 5 formed by etching the substrate 1, and a seed layer 3 formed on the inner wall of the trench 5. The overhang 4 of the seed layer 3 at the top of the trench 5 will seriously affect the quality of subsequent electroplating, resulting in the inability to fill the bottom, thereby affecting the performance of the entire device.
[0060] IMP (Ion Metal Plasma) is a new type of magnetron sputtering that improves the step coverage of the trench, but the M + (charged metal particles) and Ar + At the same time, the magnetic field on the target and the magnetic field generated by the coil on the wafer cannot distinguish the M + and Ar + , which will affect the deposition effect. In addition, applying a negative bias on the sample surface will also attract M + with Ar + , cannot be filtered, Ar + This can cause secondary sputtering of thin films. While ALD (atomic layer deposition) offers excellent step coverage, it also suffers from a high failure rate for deposited metals, poor purity, and poor performance. ALD is also limited by precursor separation, resulting in a very low deposition rate. Therefore, the preparation of high-purity, high-step coverage trench adhesion and seed layers remains a significant challenge.
[0061] How to prepare a trench adhesion barrier layer and a seed layer with high quality and high step coverage is a technical problem that needs to be solved in this field.
[0062] Based on the above technical problems, an embodiment of the present application provides a semiconductor structure and a preparation method, which includes: providing a substrate with grooves; a neutral ion beam generated by a sputtering ion source of an ion beam deposition device bombards a first target material to generate first sputtering particles; a neutral ion beam generated by an auxiliary ion source of the ion beam deposition device changes the incident direction of the first sputtering particles to form an adhesion barrier layer on the inner wall of the groove; a neutral ion beam generated by the sputtering ion source bombards a second target material to generate second sputtering particles; a neutral ion beam generated by the auxiliary ion source changes the incident direction of the second sputtering particles to form a seed layer on the inner wall of the groove; the angle between the auxiliary ion source and the normal of the substrate surface is an acute angle. Through ion beam deposition, the sputtering particles can be guided to be incident at a certain angle so that the sputtering particles can better enter the bottom of the groove, achieving better step coverage and conformality.
[0063] In order to better understand the technical solutions and technical effects of the present application, specific embodiments will be described in detail below with reference to the accompanying drawings.
[0064] Exemplary Methods
[0065] Referring to FIG. 2 , FIG. 2 is a flow chart of a method for preparing a semiconductor structure provided in an embodiment of the present application, comprising:
[0066] S101: providing a substrate with grooves.
[0067] In an embodiment of the present application, referring to FIG3 , which is a schematic diagram of a structure in a process of preparing a semiconductor structure provided in an embodiment of the present application, the substrate 1 with grooves may be a semiconductor substrate, such as a Si substrate, a Ge substrate, a SiGe substrate, an SOI (Silicon On Insulator) or a GOI (Germanium On Insulator), etc. In other embodiments, the semiconductor substrate may also be a substrate comprising other elemental semiconductors or compound semiconductors, such as GaAs, InP or SiC, etc., or a stacked structure, such as Si / SiGe, etc., or other epitaxial structures, such as SGOI (Silicon Germanium On Insulator), etc. In a possible implementation, the substrate 1 with grooves provided in an embodiment of the present application may be obtained specifically by the following steps:
[0068] An initial substrate is provided, a hard mask is deposited on the initial substrate, and a structure area is defined by photolithography; the initial substrate in the structure area is etched to form a substrate 1 with grooves.
[0069] Optionally, the hard mask may be made of an insulating material, for example, may include at least one of a silicon oxide layer, a silicon nitride layer and a silicon oxynitride layer. Optionally, in this embodiment, the hard mask is a silicon oxide layer.
[0070] In order to form a subsequent interconnection structure or other structures, the embodiment of the present application can etch the initial substrate to form a groove 5, and the groove 5 is etched along the thickness direction of the initial substrate.
[0071] S102: Utilizing a neutral ion beam generated by a sputtering ion source of an ion beam deposition device to bombard a first target material to generate first sputtered particles.
[0072] S103: using a neutral ion beam generated by an auxiliary ion source of the ion beam deposition device to change the incident direction of the first sputtered particles, so as to form an adhesion barrier layer on the inner wall of the trench.
[0073] In an embodiment of the present application, referring to FIG4 , there is shown a schematic diagram of an ion beam deposition device provided in an embodiment of the present application.
[0074] The ion beam deposition device provided in the embodiment of the present application may include a sputtering ion source 10 , and the neutral ion beam generated by the sputtering ion source 10 of the ion beam deposition device may be used to bombard a first target material 11 to generate first sputtered particles.
[0075] For example, the sputtering ion source 10 and the first target 11 can be placed opposite to each other, the direction of the neutral ion beam generated by the sputtering ion source 10 can be shown by arrow A in the figure, and the direction of the first sputtered particles generated after bombarding the first target 11 can be shown by arrow B in the figure.
[0076] 4 and 5 , FIG5 is a schematic diagram of a structure during the preparation process of another semiconductor structure provided in an embodiment of the present application.
[0077] The ion beam deposition device provided in the embodiment of the present application may further include an auxiliary ion source 12. The neutral ion beam generated by the auxiliary ion source 12 of the ion beam deposition device may be used to change the incident direction of the first sputtered particles to form an adhesion barrier layer 6 on the inner wall of the groove 5 and the substrate 1 with the groove 5.
[0078] Therefore, the present application can guide the first sputtered particles to be incident along a certain angle through the auxiliary ion source 12, so that the first sputtered particles can better enter the bottom of the groove 5, achieve better step coverage and conformality, and prepare a groove adhesion barrier layer 6 with high quality and high step coverage.
[0079] The embodiment of the present application can prevent the subsequently sputtered material from diffusing into the substrate 1 with the grooves 5 by means of the adhesion barrier layer 6, and can also prevent impurities in the substrate 1 with the grooves 5 from diffusing into the subsequently deposited film layer structure.
[0080] S104: bombarding a second target material with the neutral ion beam generated by the sputtering ion source to generate second sputtered particles;
[0081] S105: using the neutral ion beam generated by the auxiliary ion source to change the incident direction of the second sputtered particles to form a seed layer on the inner wall of the groove; the angle between the auxiliary ion source and the normal of the substrate surface is an acute angle.
[0082] In the embodiment of the present application, as shown in FIG. 4 , the neutral ion beam generated by the sputtering ion source 10 can be used to bombard the second target material 22 to generate second sputtered particles.
[0083] That is, after depositing the adhesion barrier layer 6 in the embodiment of the present application, the neutral ion beam generated by the sputtering ion source 10 can be used to bombard the second target material 22 to generate second sputtered particles, which can be used to deposit and form the seed layer 7.
[0084] Specifically, in order to enable the second sputtered particles to better enter the bottom of the trench 5 to achieve a high step coverage, the auxiliary ion source 12 can be used to further control the direction of the second sputtered particles.
[0085] That is, in an embodiment of the present application, referring to Figures 4 and 6, Figure 6 is a schematic diagram of a semiconductor structure provided in an embodiment of the present application, and the neutral ion beam generated by the auxiliary ion source 12 can be used to change the incident direction of the second sputtered particles to form a seed layer 7 on the inner wall of the groove 5 and the side of the adhesion barrier layer 6 away from the substrate 1; the angle C between the auxiliary ion source 12 and the surface normal of the substrate 1 is an acute angle.
[0086] Therefore, the present application can guide the second sputtered particles to be incident along a certain angle through the auxiliary ion source 12, so that the second sputtered particles can better enter the bottom of the groove 5, achieve better step coverage and conformality, and prepare a groove seed layer 7 with high quality and high step coverage.
[0087] In one possible implementation, after providing the substrate 1 with the grooves 5, and before bombarding the first target 11 with a neutral ion beam generated by a sputtering ion source 10 of an ion beam deposition device to generate first sputtered particles, the method provided in the embodiment of the present application may further include:
[0088] The trench 5 is pre-cleaned using a neutral ion beam generated by the auxiliary ion source 12 to remove impurities on the surface of the trench 5 .
[0089] That is, in the embodiment of the present application, before preparing the two thin films of adhesion barrier layer 6 and seed layer 7, the groove 5 can be pre-cleaned using the auxiliary ion source 12 of the ion beam deposition equipment (IBD, Ion Beam Deposition). This process can remove the dirt and oxide layer on the surface of the groove 5, increase the adhesion of the subsequent film layer, save transmission time and the risk of oxidation. This process can be carried out in the same chamber cleaning, eliminating one chamber.
[0090] In a possible implementation, in the embodiment of the present application, when the adhesion barrier layer 6 and the seed layer 7 are formed, the substrate 1 can be controlled to maintain self-rotation.
[0091] The substrate 1 and the film layer thereon provided in the embodiment of the present application maintain self-rotation during the deposition process, so that particles can be evenly deposited on the sidewalls and bottom of the groove 5 to ensure the integrity of the filling of the groove 5 and achieve full filling of the groove 5 without holes.
[0092] The present invention provides an ion beam deposition method for filling the trench. Ion beam deposition is a type of physical vapor deposition (PVD) that uses a grid in an ion source to produce a broad ion beam. High-energy ions bombard the target surface, sputtering material particles that are deposited onto the sample surface, forming a suitable film layer.
[0093] In one possible implementation, the neutral ion beam of the sputtering ion source 10 provided in an embodiment of the present application may include an ion beam formed by one or more inert gases selected from the group consisting of He, Ne, Ar, Kr, and Xe. For example, an argon ion beam may be obtained by passing argon gas through a grid. Optionally, the flow rate of the argon gas introduced into the reaction chamber may be greater than or equal to 10 sccm and less than or equal to 100 sccm.
[0094] The grid can adjust the direction and energy of the plasma so that the plasma is evenly focused and bombards the inside of the target material. The deposited thin film will not introduce foreign elements. In addition, during the preparation process of the semiconductor structure of the embodiment of the present application, neutral particles are generated. The plasma and sputtered target particles are not affected by electromagnetic interference from the outside world or the inside of the chamber, which effectively improves the purity of the prepared semiconductor structure.
[0095] In a possible implementation, see FIG7 , which is a schematic diagram of a grid structure in a sputtering ion source provided in an embodiment of the present application.
[0096] The grid of the sputtering ion source 10 provided in the embodiment of the present application can be arc-shaped, and the target material is arranged on one side of the arc grid 101 close to the center of the arc to focus the ion beam onto the target surface. The radius of the arc is greater than or equal to 300 mm and less than or equal to 800 mm.
[0097] In a possible implementation, see FIG8 , which is a schematic diagram of another grid structure in a sputtering ion source provided in an embodiment of the present application.
[0098] The grid of the sputtering ion source 10 provided in the embodiment of the present application can also be planar, with the planar grid 102 having a plurality of through holes, each of which covers an area of [0.25 times, 0.75 times] the area of the first target or the second target. Optionally, the plurality of through holes can be disposed in a central region of the planar grid 102 to achieve focusing of the ion beam.
[0099] In a possible implementation, the material of the adhesion barrier layer 6 provided in the embodiment of the present application may include: one or more materials selected from titanium, tantalum, titanium nitride, and tantalum nitride.
[0100] The above materials have a high step coverage and can be better deposited on the inner wall of the trench 5 , that is, the material of the adhesion barrier layer 6 can be: Ti, Ta, TiN or TaN, or a combination of Ti / TiN, Ta / TaN, etc.
[0101] In a possible implementation, in the embodiment of the present application, when the deposited adhesion barrier layer 6 does not contain N element, the neutral ion beam used by the auxiliary ion source 12 may include: an ion beam formed by one or more inert gases.
[0102] In one possible implementation, in an embodiment of the present application, when the deposited adhesion barrier layer 6 contains N elements, such as TiN or TaN, the ion beam used by the auxiliary ion source 12 may include one or more inert gases and a mixed gas of nitrogen, so as to deposit an adhesion barrier layer 6 containing N elements such as TiN or TaN.
[0103] In a possible implementation, the material of the seed layer 7 provided in the embodiment of the present application may include: one or more of aluminum, copper, and tungsten.
[0104] The above materials have good electrical conductivity, so that the semiconductor structure prepared in the embodiment of the present application has good electrical conductivity.
[0105] In one possible implementation, the trench 5 provided in the embodiment of the present application has an aspect ratio range of [2:1, 15:1]. That is, in the embodiment of the present application, the ion beam deposition method can accommodate trenches 5 with a wide range of aspect ratios, ensuring complete filling in shallow trenches and ensuring complete filling in deep trenches.
[0106] Optionally, in an embodiment of the present application, for a trench 5 with a high aspect ratio, a structure that is wide at the top and narrow at the bottom can be formed. See FIG9 , which is a schematic diagram of another semiconductor structure provided in an embodiment of the present application.
[0107] In a possible implementation, the purity of the first target material 11 and the second target material 22 provided in the embodiment of the present application is greater than or equal to 99.9% and less than or equal to 99.9999%.
[0108] That is, in the embodiments of the present application, since IBD is a type of physical vapor deposition, the quality of the deposited film is related to the purity of the target material. The higher the purity of the target material, the higher the purity of the produced film. The quality of the film is also related to the chamber's vacuum and leak rate properties, and IBD has better performance in these areas than CVD. Therefore, the embodiments of the present application use high-purity first target material 11 and second target material 22 to produce films of higher purity.
[0109] In a possible implementation, an angle C between the auxiliary ion source 12 and the surface normal of the substrate 1 is greater than 0° and less than or equal to 30°.
[0110] That is, in the embodiment of the present application, in order to ensure that the sputtered particles can be smoothly deposited into the groove 5 with a high aspect ratio, the relative positions of the IBD target, substrate and ion source can be adjusted, and the sputtered particles are incident at a certain angle with a low divergence angle. Adjusting the angle can make the sputtered particles enter the bottom of the groove, achieving better coverage and conformality. In addition, the auxiliary ion source can further control the direction of the sputtered particles.
[0111] Optionally, in an embodiment of the present application, referring to FIG10 , which is a schematic diagram of another semiconductor structure provided in an embodiment of the present application, in some semiconductor device structures, in order to avoid deposition of the adhesion barrier layer 6 and the seed layer 7 at the bottom of the trench 5, the angle can be adjusted so that the adhesion barrier layer 6 and the seed layer 7 are deposited only on the sidewalls of the trench 5, thereby preventing the adhesion barrier layer 6 and the seed layer 7 on the sidewalls from communicating with each other, causing a short circuit in the semiconductor device and affecting the electrical performance of the device.
[0112] In a possible implementation, the rotation speed range of the substrate 1 in the embodiment of the present application is greater than or equal to 5 rpm and less than or equal to 200 rpm.
[0113] That is, in the embodiment of the present application, the rotation speed of the substrate 1 should not be set too small or too large. If the rotation speed is set too small, it is not conducive to the uniform deposition of the film layer; if the rotation speed is set too large, the centrifugal force is large, which may cause the sputtered particles to be unable to deposit on the film layer.
[0114] In one possible implementation, the adhesion barrier layer 6 provided in the embodiment of the present application has a thickness greater than or equal to 2 nm and less than or equal to 100 nm. The seed layer 7 has a thickness greater than or equal to 2 nm and less than or equal to 100 nm.
[0115] That is, in the embodiment of the present application, the thickness of the adhesion barrier layer 6 and the seed layer 7 can be set according to the needs of the actual device. The embodiment of the present application does not make specific limitations here, and can be set by those skilled in the art according to actual conditions.
[0116] In one possible implementation, the energy range of the neutral ion beam generated by the sputtering ion source 10 of the embodiment of the present application is greater than or equal to 400V and less than or equal to 1000V; the energy range of the neutral ion beam generated by the auxiliary ion source 12 is greater than or equal to 50V and less than or equal to 500V.
[0117] That is, in the embodiment of the present application, the energy of the neutral ion beam generated by the sputtering ion source 10 can be set to be relatively high, so that a relatively high-energy neutral ion beam can be used to bombard the target material to generate sputtered particles. The auxiliary ion source 12 does not need to bombard the target material to generate sputtered particles; it only needs to change the path of generating sputtered particles. Therefore, the neutral ion beam generated by the auxiliary ion source 12 does not need to be set to a relatively high energy, which can reduce the power consumption of the device.
[0118] In one possible implementation, the current range of the sputtering ion source 10 provided in the embodiment of the present application is greater than or equal to 0.5 A and less than or equal to 1.5 A. The current range of the auxiliary ion source 12 is greater than or equal to 0.1 A and less than or equal to 1.5A.
[0119] Similarly, since the energy of the neutral ion beam generated by the sputtering ion source 10 is relatively high, the current of the sputtering ion source 10 can be set to be relatively high to generate a neutral ion beam with relatively high energy. The current range of the auxiliary ion source 12 generates a neutral ion beam with relatively low energy, thereby generating a neutral ion beam with relatively low energy.
[0120] In one possible implementation, in the embodiment of the present application, the deposition rate of the adhesion barrier layer 6 is greater than or equal to 3 nm / min and less than or equal to 30 nm / min. The deposition rate of the seed layer 7 is greater than or equal to 3 nm / min and less than or equal to 30 nm / min. Therefore, in the embodiment of the present application, the deposition rates of the adhesion barrier layer 6 and the seed layer 7 should not be set too fast or too slow. Setting the deposition rate at [3 nm / min, 30 nm / min] can improve the film density of the deposited adhesion barrier layer 6 and the seed layer 7, and deposition at this speed can accurately control the thickness of the film and improve the deposition efficiency of the film.
[0121] In one possible implementation, in the embodiment of the present application, the RF power of the sputtering ion source 10 and the auxiliary ion source 12 is greater than or equal to 200 W and less than or equal to 1000 W. Thus, in the embodiment of the present application, by setting the RF power range of the sputtering ion source 10 and the auxiliary ion source 12, the energy density of the emitted ion beam can be guaranteed, the film density of the deposited adhesion barrier layer 6 and the seed layer 7 can be improved, and the efficiency of film deposition can be improved.
[0122] In one possible implementation, in the embodiment of the present application, the sample temperature for depositing the first target material 11 is [50°C, 300°C], and the sample temperature for depositing the second target material 22 is (0°C, 100°C]. Therefore, in the embodiment of the present application, since the material of the first target material 11 may need to react with nitrogen to form the adhesion barrier layer 6, the deposition temperature of the first target material 11 is set to be higher to achieve reaction with nitrogen at high temperature. The second target material 22 does not need to react with other substances, and therefore, can be deposited at a low temperature, which can effectively prevent the diffusion of the deposited seed layer 7 elements and improve the reliability of the semiconductor structure.
[0123] For example, referring to FIG6 , the groove 5 provided in the embodiment of the present application may have a width of 250 nm and a depth of 500 nm. An insulating layer (not shown) may be provided on the inner wall of the groove 5 . The distance between two adjacent grooves 5 is 500 nm. The groove 5 may be a circular groove, a square groove, or a long strip groove with the same width at the top and bottom. The adhesion barrier layer 6 and the seed layer 7 may be sequentially deposited on the sidewall and bottom of the groove 5 using an ion beam deposition process. The sample rotation speed during all deposition processes is 100 rpm. The specific steps are as follows:
[0124] (1) The auxiliary ion source 12 is used to ion-beam etch Ar with an energy of 400 eV. The angle C between the auxiliary ion source 12 and the surface normal of the substrate 1 is 25°, and the impurities on the sidewall and bottom of the trench 5 are etched away by 10 nm.
[0125] (2) The auxiliary ion source 12 introduces O2 at a low energy of 50 eV to modify the groove 5 to form an insulating layer. The angle C between the auxiliary ion source 12 and the surface normal of the substrate 1 is 25°, and a 10 nm insulating layer is deposited on the bottom and side of the groove 5;
[0126] (3) The sputtering ion source 10 is used to introduce Ar at a high energy of 1000 eV to sputter the first target material 11, and the auxiliary ion source 12 is used to introduce Ar at a low energy of 50 eV to adjust the movement direction of the sputtered particles to form a single element adhesion barrier layer 6 or introduce a mixed gas of Ar and N2 to form a nitride adhesion barrier layer 6 with a changed direction. The angle C between the auxiliary ion source 12 and the surface normal of the substrate 1 is 27°, and the thickness of the adhesion barrier layer 6 is 10 nm.
[0127] (4) The sputtering ion source 10 is provided with high energy 1000eV Ar to sputter the second target material 22, and the auxiliary ion source is provided with low energy 50eV Ar to adjust the movement direction of the sputtered particles to form a seed layer 7. The angle C between the auxiliary ion source 12 and the surface normal of the substrate 1 is 27°, and the thickness of the seed layer 7 is 10nm.
[0128] That is, in the embodiment of the present application, the groove 5 with the same width at the top and bottom can be formed by adjusting the angles of the sputtering ion source 10 and the auxiliary ion source 12 .
[0129] In addition, in a possible implementation, as shown in FIG9 , the top width of the groove 5 provided in the embodiment of the present application may be 300 nm, the bottom width of the groove 5 may be 250 nm, the depth may be 1500 nm, the sidewall of the groove 5 may have an insulating layer, and the distance between two adjacent grooves 5 may be 600 nm. The groove 5 may be a circular groove, a square groove, or a long strip groove that is wide at the top and narrow at the bottom. The adhesion barrier layer 6 and the seed layer 7 may be sequentially deposited on the sidewall and bottom of the groove 5 using an ion beam deposition process. The sample rotation speed during all deposition processes is 100 rpm. The specific steps are as follows:
[0130] (1) The auxiliary ion source 12 is used to ion-beam etch Kr with an energy of 400 eV. The angle C between the auxiliary ion source 12 and the surface normal of the substrate 1 is 5°, and the impurities on the sidewall and bottom of the trench 5 are etched away by 10 nm.
[0131] (2) The auxiliary ion source 12 introduces O2 at a low energy of 50 eV to modify the groove 5 to form an insulating layer. The angle C between the auxiliary ion source 12 and the surface normal of the substrate 1 is 5°, and a 10 nm insulating layer is deposited on the bottom and side of the groove 5;
[0132] (3) The sputtering ion source 10 introduces Kr at a high energy of 1000 eV to sputter the first target material 11, and the auxiliary ion source 12 introduces Ar at a low energy of 50 eV to adjust the movement direction of the sputtered particles to form a single element adhesion barrier layer 6 or introduces a mixed gas of Kr and N2 to form a nitride adhesion barrier layer 6 with a changed direction. The angle C between the auxiliary ion source 12 and the surface normal of the substrate 1 is 7°, and the thickness of the adhesion barrier layer 6 is 10 nm.
[0133] (4) The sputtering ion source 10 injects Kr at a high energy of 1000 eV to sputter the second target material 22, and the auxiliary ion source 12 injects Kr at a low energy of 50 eV to adjust the movement direction of the sputtered particles to form a seed layer 7. The angle C between the auxiliary ion source 12 and the surface normal of the substrate 1 is 7°, and the thickness of the seed layer 7 is 10 nm.
[0134] That is, in the embodiment of the present application, a trench 5 that is wide at the top and narrow at the bottom can be formed by adjusting the angles of the sputtering ion source 10 and the auxiliary ion source 12 , which is generally suitable for forming a trench 5 with a high aspect ratio.
[0135] In another possible implementation, as shown in FIG10 , the groove 5 provided in the embodiment of the present application may have a width of 500 nm and a depth of 1500 nm. The sidewalls of the groove 5 are provided with an insulating layer. The distance between two adjacent grooves 5 is 1000 nm. The groove 5 is a circular groove, a square groove, and a long strip groove with the same width at the top and bottom. The adhesion barrier layer 6 and the seed layer 7 are sequentially deposited on the sidewalls of the groove 5 using an ion beam deposition process. To prevent the sidewalls on both sides from being connected, the adhesion barrier layer 6 and the seed layer 7 are not deposited at the bottom of the groove 5. The sample rotation speed during all deposition processes is 100 rpm. The specific steps are as follows:
[0136] (1) The auxiliary ion source 12 is used to inject Xe with an energy of 400 eV for ion beam etching. The angle C between the auxiliary ion source 12 and the surface normal of the substrate 1 is 15°, and the impurities on the sidewall and bottom of the trench 5 are etched away by 10 nm.
[0137] (2) The auxiliary ion source 12 introduces O2 at a low energy of 50 eV to modify the groove 5 to form an insulating layer. The angle C between the auxiliary ion source 12 and the surface normal of the substrate 1 is 15°, and a 10 nm insulating layer is deposited on the bottom and side of the groove 5;
[0138] (3) The sputtering ion source 10 introduces Xe at a high energy of 1000 eV to sputter the first target material 11, and the auxiliary ion source 12 introduces Ar at a low energy of 50 eV to adjust the movement direction of the sputtered particles to form a single element adhesion barrier layer 6 or introduces a mixed gas of Xe and N2 to form a nitride adhesion barrier layer 6 with a changed direction. The angle C between the auxiliary ion source 12 and the surface normal of the substrate 1 is 22°, and the thickness of the adhesion layer is 10 nm.
[0139] (4) The sputtering ion source 10 injects Xe at a high energy of 1000 eV to sputter the second target material 22, and the auxiliary ion source 12 injects Xe at a low energy of 50 eV to adjust the movement direction of the sputtered particles to form a seed layer 7. The angle C between the auxiliary ion source 12 and the surface normal of the substrate 1 is 22°, and the thickness of the seed layer 7 is 10 nm.
[0140] That is, in the embodiment of the present application, the angles of the sputtering ion source 10 and the auxiliary ion source 12 can be adjusted so that in certain semiconductor device structures, the adhesion barrier layer 6 and the seed layer 7 are only deposited on the side walls of the groove 5. To prevent the side walls on both sides from being connected, the adhesion barrier layer 6 and the seed layer 7 will not be deposited at the bottom of the groove 5, thereby avoiding causing a short circuit in the semiconductor device and affecting the electrical performance of the device.
[0141] An embodiment of the present application provides a method for preparing a semiconductor structure, comprising: providing a substrate with a groove; bombarding a first target material with a neutral ion beam generated by a sputtering ion source of an ion beam deposition device to produce first sputtered particles; changing the incident direction of the first sputtered particles with a neutral ion beam generated by an auxiliary ion source of the ion beam deposition device to form an adhesion barrier layer on the inner wall of the groove; bombarding a second target material with a neutral ion beam generated by the sputtering ion source to produce second sputtered particles; changing the incident direction of the second sputtered particles with the neutral ion beam generated by the auxiliary ion source to form a seed layer on the inner wall of the groove; and forming an acute angle between the auxiliary ion source and the normal to the substrate surface. Ion beam deposition can guide the sputtered particles to be incident at a certain angle so that the sputtered particles can better enter the bottom of the groove, achieving good step coverage and conformality.
[0142] An embodiment of the present application also provides a semiconductor structure, including a structure prepared using the method described above.
[0143] The various embodiments in this specification are described in a progressive manner. Similar parts between the various embodiments can be referred to in conjunction with each other. Each embodiment focuses on the differences from the other embodiments. In particular, the structural embodiments are described briefly because they are generally similar to the method embodiments. For relevant parts, refer to the description of the method embodiments.
[0144] The above is only a preferred embodiment of the present application. Although the present application has been disclosed as a preferred embodiment, it is not intended to limit the present application. Any technician familiar with the art can use the above-disclosed methods and technical contents to make many possible changes and modifications to the technical solution of the present application without departing from the scope of the technical solution of the present application, or modify it into an equivalent embodiment with equivalent changes. Therefore, any simple modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present application without departing from the content of the technical solution of the present application are still within the scope of protection of the technical solution of the present application.
Claims
1. A method for preparing a semiconductor structure, characterized in that: include: Step 1, providing a substrate with grooves; Step 2: bombarding the first target material with a neutral ion beam generated by a sputtering ion source of an ion beam deposition device to generate first sputtered particles; Step 3: using a neutral ion beam generated by an auxiliary ion source of the ion beam deposition device to change the incident direction of the first sputtered particles, so as to form an adhesion barrier layer on the inner wall of the groove; Step 4: bombarding a second target material with the neutral ion beam generated by the sputtering ion source to generate second sputtered particles; Step 5: Using the neutral ion beam generated by the auxiliary ion source, change the incident direction of the second sputtered particles to form a seed layer on the inner wall of the groove; the angle between the auxiliary ion source and the normal of the substrate surface is an acute angle.
2. The method according to claim 1, characterized in that The method of providing a substrate with grooves comprises: providing an initial substrate; Depositing a hard mask on the initial substrate to define structured regions by photolithography; The initial substrate in the structure area is etched to form the substrate with grooves.
3. The method according to claim 1, characterized in that The opening width of the groove is equal to the bottom width of the groove.
4. The method according to claim 1, characterized in that: The opening width of the groove is greater than the bottom width of the groove.
5. The method according to claim 1, characterized in that Forming an adhesion barrier layer on the inner wall of the groove includes: forming an adhesion barrier layer on the side wall of the groove; Forming a seed layer on the inner wall of the trench includes: forming a seed layer on the side wall of the trench.
6. The method according to claim 1, characterized in that After providing the substrate with grooves, and before bombarding the first target material with a neutral ion beam generated by a sputtering ion source of an ion beam deposition device to generate first sputtered particles, the method further includes: The groove is pre-cleaned by using a neutral ion beam generated by the auxiliary ion source to remove impurities on the surface of the groove.
7. The method according to claim 1, characterized in that During the forming of the adhesion barrier layer and the forming of the seed layer, the substrate is controlled to keep rotating.
8. The method according to claim 1, characterized in that The neutral ion beam of the sputtering ion source includes an ion beam formed by any one or more inert gases among He, Ne, Ar, Kr and Xe.
9. The method according to claim 1, characterized in that: The neutral ion beam used by the auxiliary ion source includes: an ion beam formed by one or more inert gases.
10. The method according to claim 1, wherein the ion beam used by the auxiliary ion source comprises a mixed gas of one or more inert gases and nitrogen.
11. The method according to claim 1, characterized in that: The material of the adhesion barrier layer includes one or more of titanium, tantalum, titanium nitride and tantalum nitride.
12. The method according to claim 1, characterized in that The material of the seed layer includes: one or more of aluminum, copper and tungsten.
13. The method according to claim 1, characterized in that The aspect ratio of the groove is in the range of [2:1, 15:1].
14. The method according to claim 1, characterized in that The purity of the first target material and the second target material is greater than or equal to 99.9% and less than or equal to 99.9999%.
15. The method according to claim 1, characterized in that The angle between the auxiliary ion source and the substrate surface normal is greater than 0° and less than or equal to 30°.
16. The method according to claim 7, characterized in that The rotation speed range of the rotation is greater than or equal to 5 rpm and less than or equal to 200 rpm.
17. The method according to claim 1, characterized in that The thickness of the adhesion barrier layer is greater than or equal to 2 nm and less than or equal to 100 nm.
18. The method according to claim 1, characterized in that The thickness of the seed layer is greater than or equal to 2 nm and less than or equal to 100 nm.
19. The method according to claim 1, characterized in that The grid of the sputtering ion source is in an arc shape to focus the ion beam onto the surface of the target material, and the radius of the arc is greater than or equal to 300 mm and less than or equal to 800 mm.
20. The method according to claim 1, characterized in that The grid of the sputtering ion source is in a plane, and the grid is provided with a plurality of through holes, wherein the coverage area of the plurality of through holes is [0.25 times, 0.75 times] the area of the first target material or the second target material.
21. The method according to claim 1, characterized in that The deposition rate of the adhesion barrier layer is greater than or equal to 3 nm / min and less than or equal to 30 nm / min.
22. The method according to claim 1, characterized in that The deposition rate of the seed layer is greater than or equal to 3 nm / min and less than or equal to 30 nm / min.
23. The method according to claim 1, characterized in that The sample temperature for depositing the first target material is [50°C, 300°C], and the sample temperature for depositing the second target material is (0°C, 100°C].
24. A semiconductor structure, characterized in that: include: A structure prepared by the method according to any one of claims 1 to 23.
Citation Information
Patent Citations
Multifunctional ion beam sputtering and etching and in-situ physical property analysis system
CN102486465A
Sputtering device and sputtering method
CN104060234A
A light extraction film having hollow bubbles and an organic light-emitting diode and a processing method thereof
CN108389980A
Method and device for forming functional deposit film by sputtering method
JP1989309958A
Cited By
Grating manufacturing method and grating ruler
CN119162557A
Grating manufacturing method and grating ruler
CN119162557B