Joining connection, power module assembly and method for attaching a first joining partner to a second joining partner
A patterned intermetallic phase layer in the joining connection addresses the uneven stress distribution in conventional soldering by varying the heights of the layer, enhancing reliability and strength in power semiconductor modules.
Patent Information
- Application Number
- PCT/EP2023/059768
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-14
- Publication Date
- 2024-10-17
AI Technical Summary
Conventional soldering techniques for power semiconductor modules result in uniform intermetallic phase layers, leading to uneven thermomechanical stress distribution, particularly during thermal cycling, which can weaken the joining connection and reduce reliability.
A joining connection with a patterned intermetallic phase layer having distinct regions of different heights, created by varying the diffusion of metals between the joining material and the connection portions, enhances mechanical stability and electrical conductivity, and includes a method for producing such a connection by applying a joining material between partners and controlling the heating process to form the patterned layer.
The patterned intermetallic phase layer improves the reliability of the joining connection by distributing stress more evenly, increasing ultimate strength and cycle times, and suppressing crack formation and delamination in critical regions.
Smart Images

Figure EP2023059768_17102024_PF_FP_ABST
Abstract
Description
[0001] DESCRIPTION
[0002] JOINING CONNECTION, POWER MODULE ASSEMBLY AND METHOD FOR ATTACHING A FIRST JOINING PARTNER TO A SECOND JOINING PARTNER
[0003] The present disclosure relates to a j oining connection for attaching a first j oining partner to a second j oining partner, a power module assembly and a method for producing a j oining connection .
[0004] Embodiments of the disclosure relate to a j oining connection, which is particularly reliable . Further embodiments of the disclosure relate to a module assembly with such a j oining connection and a method for producing such a j oining connection .
[0005] This is achieved by the subj ect-matter of the independent claims . Further embodiments are evident from the dependent claims in the following description .
[0006] A j oining connection for attaching a first j oining partner to a second j oining partner is described . Exemplarily, the j oining connection is formed in a power semiconductor module with at least one power semiconductor device . The term "power" here and in the following, for example , refers to power semiconductor modules , power semiconductor devices and / or power semiconductor chips adapted for processing voltages and currents of more than 100 V and / or more than 10 A, exemplary voltages up to 10 kV and currents of amperes up to 5000 A.
[0007] The first j oining partner comprises , for example , a first connection portion and / or the second j oining partner comprises, for example, a second connection portion. The first connection portion and / or the second connection portion are formed, in particular, of an electrically conductive material. The first connection portion and / or the second connection portion comprises or consists of, for example, a metal or a metal alloy. Exemplarily, the first connection portion and / or the second connection portion comprises, for example at least one of copper, Cu, aluminium, Al, and nickel, Ni . In particular, the first connection portion and / or the second connection portion comprises or consists of an alloy comprising at least two of the following materials: copper, Cu, aluminium, Al, nickel, Ni .
[0008] In particular, the first connection portion is a metallization of the first joining partner and the second connection portion is a metallization of the second joining partner. The metallization of the first joining partner or / and second joining partner, i.e. the first connection portion or / and second connection portion, can be a backside metallization of the chip being, for example, a thin coating, or it can be a substrate metallization being, for example, a bulk metal, or it can be a whole surface of the chip backside or it can be a portion of the surface of the substrate metallization. The substrate metallization can have at least locally an additional coating. In some cases, a connection portion can be a terminal foot or a joining portion of a clip .
[0009] The first joining partner and the second joining partner each extend within a main extension plane, wherein the main extension planes extend in lateral directions. The first joining partner and the second joining partner are arranged opposite one another in vertical direction, which is perpendicular to the lateral directions . In particular, the first connection portion faces the second connection portion, such that the first connection portion is arranged opposite the second connection portion in vertical direction . Exemplarily, the first connection portion completely overlaps in plan view with the second connection portion in lateral directions .
[0010] For example , at least one of the first connection portion and the second connection portion have a shape in plan view being circular, elliptical or polygonal , such as quadrangular . Exemplarily, the j oining connection has the same shape in plan view than the first connection portion and / or the second connection portion . For example , in plan view, an extent of the shape of at least one of the first connection portion and the second connection portion is equal or larger than the shape of the j oining connection .
[0011] According to an embodiment , the j oining connection comprises a j oining material . The j oining material is formed, in particular, of an electrically conductive material . The j oining material comprises or consists of , for example , a metal or a metal alloy . The j oining material comprises , for example at least one of tin, Sn, lead, Pb, silver, Ag, antimony, Sb, and copper, Cu . In particular, the j oining material comprises or consists of an alloy comprising at least two of the following materials : tin, Sn, lead, Pb, silver, Ag, antimony, Sb copper, Cu . The j oining material can comprise further substances like rare earth materials or bismuth or indium, to influence material properties like wetting behaviour and / or a di f fusion velocity . According to the embodiment, the joining connection comprises an intermetallic phase layer. The intermetallic phase layer comprises, for example, at least one of the metals of the joining material and at least one of the metals of one of the first connection portion or second connection portion.
[0012] Exemplarily, during a method step for producing the joining connection, the joining material is heated such that the joining material melts and wets a respective connection portion, creating a metallurgical bond. Exemplarily, atoms from the joining material and the connection portion diffuse across the interface of joining material and connection portion, forming the intermetallic phase layer. This is that the intermetallic phase layer comprises or consists of a metal alloy of at least one of the metals of the joining material and at least one of the metals of one of the first connection portion or second connection portion.
[0013] According to the embodiment of the joining connection, the joining material is arranged between the first joining partner and the second joining partner. The joining material is in particular arranged between the first connection portion and the second connection portion. This is, the first joining partner, the joining material and the second joining partner are stacked above one another along a stacking direction, which is oriented in vertical direction.
[0014] According to the embodiment of the joining connection, the intermetallic phase layer is arranged between the joining material and at least one of the first joining partner and the second joining partner. In particular, the intermetallic phase layer is an interface region between the joining material and at least one of the first joining partner and the second j oining partner . The intermetallic phase layer is , for example , in direct contact to the j oining material . Exemplarily, the intermetallic phase layer is in direct contact to at least one of the first j oining partner and the second j oining partner .
[0015] According to the embodiment of the j oining connection, the intermetallic phase layer has at least two regions comprising at least one first region with a first height and at least one second region with a second height being di f ferent to one another . The height is an extent of the intermetallic phase layer in vertical direction .
[0016] In particular, such di f ferent regions with the first height and the second height are not to compare with a roughness of an interface between the intermetallic phase layer and the j oining material and an interface between the intermetallic phase layer and at least one of the first j oining partner and the second j oining partner . Such a roughness of the corresponding interface is typically due to production tolerances . This is that a di f ference of the first height and the second height is larger than the roughness of the corresponding interfaces of the intermetallic phase layer . The roughness is typically in the range of maximum a few microns .
[0017] In particular, the j oining connection provides a mechanically stable as well as an electrically conductive connection and / or a thermally conductive connection of the first j oining partner and the second j oining partner .
[0018] Typically, soldering is a commonly used j oining technology in the assembly of power semiconductor devices and modules e . g . for joining of a first joining partner, i.e. a power semiconductor chip to a second joining partner, i.e. an isolating substrate, or vice versa or for joining of a substrate to a baseplate. Generally, conventional reflow soldering is still the mostly used joining technology. During the conventional soldering process, conventional intermetallic phase layers are generated by interdiffusion of material at the interfaces between a conventional joining material, i.e. a conventional solder, and joining partners. Such conventional intermetallic phase layers have a mainly homogeneous height in vertical direction. "Mainly" means that there can be fluctuations in height due to production tolerances .
[0019] However, a typical interface area between a substrate and a base plate is comparatively large. This results in locally different magnitudes of stress e.g. due to thermal cycling during operation. E.g. during thermal cycling, a thermomechanical stress in corners of a conventional soldered joining connection is significantly larger than in a central region. It is conceivable that a weakest region of the conventional soldered joining connection can be at a location, where the highest thermomechanical stress occurs.
[0020] In summary, such a joining connection with an intermetallic phase layer having a first and a second height can provide, inter alia, the following advantages.
[0021] As a height of the intermetallic phase layer has an influence on the stress resistivity of the joining connection, e.g. due to improved hardness of the intermetallic phase layer compared with a bare joining material, and consequently on the reliability especially during thermal cycling, the intermetallic phase layer has the first region and the second region with di f ferent heights . Consequently, the reliability of the soldered connection against thermo-mechanical stress is locally enhanced by this intended local modi fication of the heights such that the intermetallic phase layer is patterned .
[0022] Such patterned intermetallic phase layers lead to an improved reliability of the j oining connection with respect to thermomechanical stress . In particular, the pattered intermetallic phase layer results in a locally higher ultimate strength of the j oining connection especially in critical regions , where stress maxima occur, and consequently in higher cycle times .
[0023] I f a multiple pattern of the first and the second height is present , a cracking process similar to hooking may occur, such that crack formation and delamination due to stress may be suppressed, and consequently, the reliability may be improved .
[0024] According to a further embodiment of the j oining connection, the first height and the second height are di f ferent from one another by at least 50 % in vertical direction . Exemplarily, the first height is larger than the second height , in particular larger by a factor of at least 1 . 5 of the second height . Alternatively, the second height is larger than the first height , in particular larger by a factor of at least 1 . 5 of the first height .
[0025] For example , at least one of the first height and the second height are at least 1 pm and at most 100 pm . According to a further embodiment of the j oining connection, the first region is arranged in a central region of the j oining connection and the second region is arranged in a peripheral region of the j oining connection at least partially surrounding the central region .
[0026] Exemplarily, the central region is located at a center of mass of the j oining connection and extends in lateral directions in direction to edges of at least one of the first connection portion and the second connection portion . The peripheral region extends in lateral directions along an edge region of the j oining connection delimiting the central region . The peripheral region partially or completely surrounds the central region in lateral directions .
[0027] The second region is arranged at least regionally or completely in the peripheral region . For example , the second region surrounds the central region in a frame-like manner . " Frame-like" is to be understood as non-limiting with respect to the shape of the reinforcement structure .
[0028] According to a further embodiment of the j oining connection, the second region is formed of several parts being spaced apart from one another in lateral directions and each part has the second height . Exemplarily, the parts of the second region have each the second height . The parts of the second region are , for example , spaced apart from one another in lateral directions .
[0029] I f the second height is smaller than the first height , the parts of the second region are spaced apart from one another in lateral directions by the first region . This is , for example , that the first region is arranged between the parts of the second region .
[0030] I f the second height is larger than the first height , the parts of the second region are spaced apart from one another in lateral directions by the j oining material and / or by at least one of the first connection portion and the second connection portion . This is , for example , that the j oining material and / or at least one of the first connection portion and the second connection portion is arranged between the parts of the second region .
[0031] According to a further embodiment of the j oining connection, each part is arranged in a corner of the j oining connection . I f the j oining connection, in particular, at least one of the first connection portion and the second connection portion, has a shape in plan view being polygonal , each part is arranged in a region at one of the corners of the polygonal shape .
[0032] According to a further embodiment of the j oining connection, at least one of the first region and the second region has a width of at least 100 pm in lateral directions . The width is a minimal extent of the first region and the second region, respectively, in lateral directions .
[0033] According to a further embodiment of the j oining connection, the intermetallic phase layer comprises a plurality of first regions with the first height and a plurality of second regions with the second height . Each of the first regions have the same first height and each of the second regions have the same second height . According to a further embodiment of the j oining connection, the first regions and the second regions are arranged on virtual grid points of a virtual grid in lateral directions . The virtual grid is solely used for clari fying positions of the first regions and the second regions . The virtual grid is , for example , a regular one dimensional or a regular two dimensional grid . I f the virtual grid is a regular two dimensional grid, the virtual grid is a polygonal grid, such as a triangular grid, a quadrangular grid, in particular a squared grid, or a hexagonal grid .
[0034] According to a further embodiment of the j oining connection, the first regions are each formed as a first stripe and the second regions are each formed as a second stripe . I f the first regions and the second regions are arranged on the virtual grid points of the regular one dimensional grid, each first region is formed as a first stripe and each second region is formed as a second stripe .
[0035] A stripe has an extent in lateral directions with a width and a length . The length extends along a main extension direction of the stripe . The length is larger than the width, in particular the length is at least 20 % or at least 50 % larger than the width .
[0036] According to a further embodiment of the j oining connection, the first stripes and the second stripes are arranged alternating next to one another in one of the lateral directions . In particular, the first stripes and the second stripes are arranged alternating next to one another along an arrangement direction being perpendicular to the main extension direction of the stripes . According to a further embodiment of the j oining connection, the first regions are each formed as a first quadrangle and the second regions are each formed as a second quadrangle . Exemplarily, the first quadrangles and / or the second quadrangles have each the same extent in lateral directions . In particular, the first quadrangles and / or the second quadrangles are each squares with the same side lengths .
[0037] According to a further embodiment of the j oining connection, the first quadrangles and the second quadrangles are arranged alternating next to one another in lateral directions such that each first quadrangle has a side adj acent to one of the second quadrangles and vice versa . This is that the first quadrangles and the second quadrangles form a checkerboard pattern .
[0038] According to a further embodiment of the j oining connection, the first height continuously increases or decreases to the second height . In particularly, the intermetallic phase layer increases from the first height to the second height gradually, wherein the first height and the second height are maximal and minimal extents in vertical direction .
[0039] According to a further embodiment of the j oining connection, the first height and the second height change periodically in one of the lateral directions , and a width of one period is at least 200 pm in lateral directions . This is , i f the j oining connection comprises several first regions and second regions being arranged alternating along one another, directly neighboring maximal heights of the first region, corresponding to the first heights , and / or directly neighboring minimal heights of the second region, corresponding to the second heights , are each spaced apart from one another by at least 200 pm in lateral directions .
[0040] According to a further embodiment of the j oining connection, the first height increases or decreases to the second height discontinuously . Exemplarily, the first height increases or decreases to the second height within an interface region between the first region and the second region . The interface region has , for example , a width in lateral directions , which is at least one order of magnitude smaller than the width of at least one of the first region and the second region . Exemplarily, the intermetallic phase layer has in side view a step shape , in a region of the first region and the second region, directly neighboring one another .
[0041] According to a further embodiment , the j oining connection is at least one of a soldered connection, a di f fusion soldered connection, and a sintered connection .
[0042] According to a further embodiment of the j oining connection for a power module assembly comprising a semiconductor chip, the first j oining partner and the second j oining partner comprise at least one of a substrate and a baseplate , a substrate and a terminal , a semiconductor chip and a substrate , and a terminal or a clip and a semiconductor chip .
[0043] The baseplate , the substrate and / or the terminal can be part of a power semiconductor module . The semiconductor chip is , in particular, a power semiconductor chip . In particular, the first j oining partner and the second j oining partner are comprised in a power semiconductor module . In this case , at least one of the first j oining partner and the second j oining partner is formed of a power semiconductor chip . For example, the first joining partner is the substrate and the second joining partner is the baseplate, or the first joining partner is the substrate and the second joining partner is the terminal, or the first joining partner is the semiconductor chip and the second joining partner is the substrate, or vice versa.
[0044] Furthermore, a power module assembly is described here, which can comprise a joining connection as described herein above. Therefore, the features in connection with the joining connection are disclosed also in connection with the power module assembly and vice versa.
[0045] According to an embodiment, the power module assembly comprises a first joining partner, in particular the first joining partner described herein above.
[0046] According to the embodiment, the power module assembly comprises a second joining partner, in particular the second joining partner described herein above.
[0047] According to the embodiment, the power module assembly comprises a joining connection, in particular the joining connection described herein above.
[0048] According to the embodiment of the power module assembly, the joining connection comprises a joining material and at least one intermetallic phase layer.
[0049] According to the embodiment of the power module assembly, the joining material is arranged between the first joining partner and the second joining partner. According to the embodiment of the power module assembly, the intermetallic phase layer is arranged between the j oining material and at least one of the first j oining partner and the second j oining partner .
[0050] According to the embodiment of the power module assembly, the intermetallic phase layer has at least two regions comprising a at least one first region with a first height and at least one second region with a second height being di f ferent to one another .
[0051] According to a further embodiment of the power module assembly, wherein the first j oining partner is a substrate , and the second j oining partner is a power semiconductor device or vice versa . This is that the power module assembly is in particular part of a power semiconductor module . The power semiconductor device can comprise a power semiconductor chip .
[0052] Exemplarily, the power semiconductor device is an electronic component configured to process high levels of electrical power as speci fied herein above . The power semiconductor device is exemplarily configured to control and convert electrical power, e . g . from AC to DC or vice versa or to change a frequency of voltage and / or current by corresponding switching operations . The power semiconductor device comprises or consists , for example , of at least one of a thyristor, a power metal-oxide-semiconductor field-ef fect transistor, MOSFET , an insulated-gate bipolar transistor, IGBT , a high electron mobility transistor, HEMT and a power diode . For example, a power semiconductor module comprises one or more of the power semiconductor devices along with further components such as a substrate, a baseplate, a heat sink, at least one terminal and a control circuitry.
[0053] For example, the joining connection can be arranged between two of the following entities of the power semiconductor module: power semiconductor device, substrate, baseplate, heat sink, at least one terminal and control circuitry.
[0054] Furthermore, a method for attaching a first joining partner to a second joining partner is described here, with which a joining connection as described herein above can be produced or is produced. Therefore, the features in connection with the joining connection are disclosed also in connection with the method and vice versa.
[0055] According to an embodiment of the method, a first joining partner and a second joining partner are provided.
[0056] According to the embodiment of the method, a joining material is applied to the first joining partner. The joining material is for example applied to the first connection portion.
[0057] According to the embodiment of the method, the second joining partner is applied to the joining material. This is that the first joining partner, the joining material and the second joining partner are stacked above one another in the stacking direction and are in particular in direct and immediate contact to one another.
[0058] According to the embodiment of the method, an assembly is heated comprising the first joining partner, the joining material and the second j oining partner such that an intermetallic phase layer is produced . During heating, the j oining material melts and wets , e . g . , the first connection portion . During heating, atoms from the j oining material and the connection portion di f fuse across the interface of j oining material and the first connection portion .
[0059] In particular, the heating of the assembly is subsequently cooled down, such that the melted material of the j oining material solidi fies and atoms from the j oining material forming the intermetallic phase layer .
[0060] According to the embodiment of the method, the intermetallic phase layer is modi fied having at least two regions comprising at least one first region with a first height and at least one second region with a second height being di f ferent to one another .
[0061] This is that also conventional j oining connections prepared by existing standard solder alloys and / or standard soldering processes can be advantageously manipulated for an improved reliability . Additionally, the proposed method can provide a further impact and variation option on the soldering process by a local manipulation of the j oining connection besides the standard reflow process with a defined temperature profile .
[0062] According to a further embodiment of the method, while heating the assembly a local magnetic field is applied to one of the at least two regions , wherein a height of the intermetallic phase layer is dependent on a magnetic flux of the local magnetic field . I f the magnetic flux is applied to the second regions during heating and / or cooling of the assembly, the second height is smaller than the first height . This is that the magnetic flux reduces the di f fusion velocity .
[0063] According to a further embodiment of the method, while heating the assembly a local electric current is applied to one of the at least two regions , wherein a height of the intermetallic phase layer is dependent on an electric current density of the local electric current .
[0064] I f the electric current is applied to the second regions during heating and / or cooling of the assembly, the second height is smaller than the first height . This is that the electric current reduces the di f fusion velocity .
[0065] According to a further embodiment of the method, while heating the assembly an additional heat is applied to one of the at least two regions , wherein a height of the intermetallic phase layer is dependent on a temperature of the heat . For example , the additional heat is applied with a local heat source or a local heat probe .
[0066] Alternatively or additionally to the application of additional heat , an additional cooling is applied to one of the at least one regions , wherein a height of the intermetallic phase layer is dependent on a temperature of the cooling . For example , the additional cooling is applied with a local cooling source or a local cooling probe .
[0067] According to a further embodiment of the method, the j oining material comprises at least two material systems being di f ferent to one another corresponding to the at least two regions to be produced. For example, the material system of the joining material arranged on the first region of the intermetallic phase layer to be produced is different from the material system of the joining material arranged on the second region of the intermetallic phase layer to be produced. The material systems can differ by their substances and / or by a proportion of the substances comprised in both material systems.
[0068] According to a further embodiment of the method, the joining material comprises at least two maximal doping concentrations being different to one another corresponding to the at least two regions to be produced. For example, the maximal doping concentrations of the joining material arranged on the first region of the intermetallic phase layer to be produced is different from the maximal doping concentrations of the joining material arranged on the second region of the intermetallic phase layer to be produced.
[0069] Exemplarily, the joining material comprises a doping material up to the maximal doping concentration. The maximal doping concentration is at most 2 % or at most 1 % with respect to the joining material per unit volume. The doping material can be, e.g., a rare earth material or, e.g., bismuth, Bi, or indium, In. Exemplarily, a wettability and / or a diffusion of the joining material is dependent of the doping concentration .
[0070] If the maximal doping concentration is larger in the first region than in the second region, the first height is larger than the second height in the intermetallic phase layer to be produced, or vice versa. Alternatively or additionally, the joining material comprises at least two doping materials being different to one another corresponding to the at least two regions to be produced. For example, the doping material of the joining material arranged on the first region of the intermetallic phase layer to be produced is different from the doping material of the joining material arranged on the second region of the intermetallic phase layer to be produced.
[0071] According to a further embodiment of the method, a joining surface of the first joining partner and / or a joining surface of the second joining partner comprises at least two metallization materials being different to one another corresponding to the at least two regions to be produced. For example, the metallization material of the first connection portion arranged at the first region of the intermetallic phase layer to be produced is different from the metallization material arranged at the second region of the intermetallic phase layer to be produced.
[0072] In particular the at least two metallization materials can differ by at least one metal of the connection portions described herein above.
[0073] According to a further embodiment of the method, a first joining surface of the first joining partner and / or a second joining surface of the second joining partner comprises at least two surface roughnesses being different to one another corresponding to the at least two regions to be produced.
[0074] For example, the first joining surface of the first joining partner is a top surface of the first connection portion facing the second joining partner. Exemplarily, the second joining surface of the second joining partner is a bottom surface of the second connection portion facing the first joining partner.
[0075] For example, the surface roughness of the first joining surface at the first region of the intermetallic phase layer to be produced is different from the surface roughness at the second region of the intermetallic phase layer to be produced. For example the surface roughnesses are different by at least 10 % or at least 50 %.
[0076] According to a further embodiment of the method, a first joining surface of the first joining partner and / or a second joining surface of the second joining partner comprises a diffusion barrier at a region corresponding to the at least one of the two regions to be produced. The diffusion barrier is, exemplarily, applied by a coating process.
[0077] If the diffusion barrier is arranged on the second regions, and when the assembly is heated, the second height is smaller than the first height. This is that the diffusion barrier reduces or blocks the diffusion in the second region and thus the second height.
[0078] The accompanying Figures are included to provide a further understanding. In the Figures, elements of the same structure and / or functionality may be referenced by the same reference signs. It is to be understood that the embodiments shown in the Figures are illustrative representations and are not necessarily drawn to scale.
[0079] Figure 1 shows a schematic view of a joining connection according to an exemplary embodiment, Figures 2 and 3 each shows a schematic view of method stages for producing a j oining connection according to an exemplary embodiment , and
[0080] Figures 4 and 5 each shows a diagram characteristic for heights of the intermetallic phase layer of a j oining connection according to an exemplary embodiment .
[0081] The j oining connection 1 according to the exemplary embodiment of Figure 1 attaches a first j oining partner 2 to a second j oining partner 3 . A j oining material 4 and an intermetallic phase layer 5 is arranged between the first j oining partner 2 and the second j oining partner 3 . In particular, the intermetallic phase layer 5 comprises or consists of materials of the j oining material 4 and the first connection portion 12 . This is that the intermetallic phase layer 5 is located partially within the j oining material 4 and the first connection portion 12 , wherein a height of the intermetallic phase layer 5 is in particular dependent on a wetting behavior and / or especially on a di f fusion velocity described more detailed in Figure 2 .
[0082] The first j oining partner 2 comprises a first connection portion 12 and the second j oining partner 3 comprises a second connection portion 13 . The first connection portion 12 and the second connection portion 13 each are a metalli zation of the respective j oining partners .
[0083] The first connection portion 12 , the intermetallic phase layer 5 , the j oining material 4 and the second connection portion 13 are arranged above one another along a stacking direction being a vertical direction . The intermetallic phase layer 5 is located within an interface of the j oining material 4 and the first connection portion 12 , extending over a first region 6 and a second region 7 .
[0084] The first region 6 is arranged in a central region of the j oining connection 1 and the second region 7 is arranged in a peripheral region of the j oining connection 1 completely surrounding the central region in lateral directions , which extend perpendicular to the vertical direction . This is that in plan view, the second region 7 completely surrounds the first region 6 in lateral directions . The plan view corresponds to a view along the vertical direction on the j oining connection 1 .
[0085] The j oining connection 1 has a first height 8 in the first region 6 and a second height 9 in the second region 7 . The first height 8 is larger than the second height 9 . The intermetallic phase layer 5 increases from the second height 9 to the first height 8 gradually . In particular, the intermetallic phase layer 5 has a shape corresponding to one of the periods shown in Figure 4 , extending from one of the minima to a directly neighboring minima . This is that the first height 8 corresponds to a maximal height of the first region 6 and the second height 9 corresponds to a minimal height in the second region 7 .
[0086] A width of the first region 6 is , for example , at least at least 100 pm in lateral directions .
[0087] The first j oining partner 2 and the second j oining partner 3 , which are connected in a mechanically stable manner by the j oining connection 1 is a power module assembly 11 , according to an exemplary embodiment . For example, the first joining partner 2 is a substrate for a power semiconductor device, and the second joining partner 3 is the power semiconductor device. This is that the power module assembly 11 is in this case a power semiconductor module .
[0088] Exemplarily, the power semiconductor device comprises or consists, for example, of at least one of a thyristor, a power metal-oxide-semiconductor field-effect transistor, MOSFET, an insulated-gate bipolar transistor, IGBT, a high electron mobility transistor, HEMT and a power diode.
[0089] According to the exemplary embodiment of Figure 2, an assembly comprising the first connection portion 12, the joining material 4 and the second connection portion 13 are heated for producing the intermetallic phase layer 5. Subsequently, the assembly is cooled. In particular, a joining connection 1 with an intermetallic phase layer 5 is produced with such a process, corresponding to the exemplary embodiment of Figure 1.
[0090] During heating and / or cooling the assembly, a local magnetic field is applied to the second region 7. As a magnetic flux of the local magnetic field is applied to the second region 7, a diffusion velocity is reduced in the second region 7 compared to the first region 6. Due to the reduced diffusion velocity in the second region 7, the resulting second height 9 in the second region 7 is smaller than the resulting first height 8 in the first region 6.
[0091] According to the exemplary embodiment of Figure 3, a diffusion barrier 10 is arranged on a first joining surface of the first joining partner 2, wherein the first joining surface of the first joining partner 2 is a top surface of the first connection portion 12 facing the second joining partner 3. The diffusion barrier 10 has different height. The height increases from an edge of the first joining surface to a central region of the first joining surface.
[0092] During heating and / or cooling the assembly, the diffusion velocity is reduced dependent on the height of the diffusion barrier 10. The diffusion velocity is inversely proportional to the height of the diffusion barrier 10. This is that the resulting second height 9 of the intermetallic phase layer 5 in the second region 7 is larger than the resulting first height 8 in the first region 6.
[0093] On the y axis of the diagram of Figures 4 and 5, a height of the intermetallic phase layer 5 is shown, dependent on an extent of the intermetallic phase layer 5 along one of the lateral directions, shown on the x axis.
[0094] The intermetallic phase layer 5 according to Figures 4 and 5 comprises a plurality of first regions 6 with the first height 8 and a plurality of second regions 7 with the second height 9. The first regions 6 and the second regions 7 are arranged alternating next to one another in lateral directions .
[0095] In the diagram of Figure 4, the first height 8 continuously decreases to the second height 9, in particularly, gradually. This is that the intermetallic phase layer 5 has a sinusoidal shape from a side view comprising a plurality of periods. For example , the maxima of the sinusoidal shape are spaced apart in lateral directions by a distance which is at least 200 pm . This is that a period has a width of at least 200 pm .
[0096] The first height 8 and the second height 9 have a maximal di f ference in height . An interface of directly neighboring first regions 6 and second regions 7 is , for example , at a height of the intermetallic phase layer 5 corresponding to hal f of the maximal di f ference in height .
[0097] In the diagram of Figure 5 , the first height 8 decreases to the second height 9 discontinuously . This is that the first height 8 decreases to the second height 9 within an interface region between the first region 6 and the second region 7 .
[0098] This is that the intermetallic phase layer 5 has a step shape from a side view comprising a plurality of periods .
[0099] For example , the first regions 6 are spaced apart in lateral directions by a distance which is at least 100 pm . This is that widths in lateral directions of the first regions 6 and the second regions 7 each is at least 100 pm .
[0100] Reference Signs
[0101] 1 j oining connection
[0102] 2 first j oining partner 3 second j oining partner
[0103] 4 j oining material
[0104] 5 intermetallic phase layer
[0105] 6 first region
[0106] 7 second region 8 first height
[0107] 9 second height
[0108] 10 di f fusion barrier
[0109] 11 power module assembly
[0110] 12 first connection portion 13 second connection portion
Claims
Claims1. Joining connection (1) for attaching a first joining partner (2) to a second joining partner (3) , with- a joining material (4) , and- an intermetallic phase layer (5) , wherein- the joining material (4) is arranged between the first joining partner (2) and the second joining partner (3) ,- the intermetallic phase layer (5) is arranged between the joining material (4) and at least one of the first joining partner (2) and the second joining partner (3) ,- the intermetallic phase layer (5) has at least two regions comprising at least one first region (6) with a first height(8) and at least one second region (7) with a second height(9) being different to one another.
2. Joining connection (1) according to claim 1, wherein- the first height (8) and the second height (9) are different from one another by at least 50 % in vertical direction .
3. Joining connection (1) according to one of the claims 1 or 2, wherein- the first region (6) is arranged in a central region of the joining connection (1) and the second region (7) is arranged in a peripheral region of the joining connection (1) at least partially surrounding the central region.
4. Joining connection (1) according to one of claims 1 to 3, wherein- the second region (7) is formed of several parts are spaced apart from one another and each part has the second height, and- each part is arranged in a corner of the joining connection(1) •5. Joining connection (1) according to one of claims 1 to 4,- at least one of the first region (6) and the second region (7) has a width of at least 100 gm in lateral directions.
6. Joining connection (1) according to one of claims 1 to 5, wherein- the intermetallic phase layer (5) comprises a plurality of first regions (6) with the first height (8) and a plurality of second regions (7) with the second height (9) .
7. Joining connection (1) according to claim 6, wherein- the first regions (6) and the second regions (7) are arranged on virtual grid points of a virtual grid in lateral directions .
8. Joining connection (1) according to one of claims 6 or 7, wherein- the first regions (6) are each formed as a first stripe and the second regions (7) are each formed as a second stripe, and- the first stripes and the second stripes are arranged alternating next to one another in one of the lateral directions .
9. Joining connection (1) according to one of claims 6 or 7, wherein- the first regions (6) are each formed as a first quadrangle and the second regions (7) are each formed as a second quadrangle, and- the first quadrangles and the second quadrangles are arranged alternating next to one another in lateral directions such that each first quadrangle has a side adjacent to one of the second quadrangles.
10. Joining connection (1) according to one of claims 1 to 9, wherein- the first height (8) continuously increases or decreases to the second height (9) , or- the first height (8) increases or decreases to the second height (9) discontinuously.
11. Joining connection (1) according to one of claims 6 to10, wherein- the first height (8) of the first regions (6) and the second height (9) of the second regions (7) change periodically in one of the lateral directions, and a width of one period is at least 200 pm in lateral directions.
12. Joining connection (1) according to one of claims 1 to11, wherein the joining connection (1) is at least one of- a soldered connection,- a diffusion soldered connection, and- a sintered connection.
13. Joining connection (1) according to one of claims 1 to 12 for a power module assembly comprising a semiconductor chip, wherein the first joining partner (2) and the second joining partner (3) comprise at least one of- a substrate and a baseplate,- a substrate and a terminal,- a substrate and the semiconductor chip, and- a terminal or a clip and the semiconductor chip.
14. Power module assembly (11) , comprising- a first joining partner (2) ,- a second joining partner (3) , and- a joining connection (1) , wherein- the joining connection (1) comprises a joining material (4) and at least one intermetallic phase layer (5) ,- the joining material (4) is arranged between the first joining partner (2) and the second joining partner (3) ,- the intermetallic phase layer (5) is arranged between the joining material (4) and at least one of the first joining partner (2) and the second joining partner (3) , and- the intermetallic phase layer (5) has at least two regions comprising a at least one first region (6) with a first height (8) and at least one second region (7) with a second height (9) being different to one another.
15. Power module assembly (11) according to claim 14, wherein- first joining partner (2) is a substrate for a power semiconductor device, and- the second joining partner (3) is a power semiconductor device .
16. Method for attaching a first joining partner (2) to a second joining partner (3) , comprising- providing a first joining partner (2) and a second joining partner ( 3 ) ,- applying a joining material (4) to the first joining partner ( 2 ) , and- applying the second joining partner (3) to the joining material (4) , and- heating an assembly comprising the first joining partner(2) , the joining material (4) and the second joining partner(3) such that an intermetallic phase layer (5) is produced,- modifying the intermetallic phase layer (5) having at least two regions comprising at least one first region (6) with a first height (8) and at least one second region (7) with a second height (9) being different to one another.
17. Method according to claim 16, wherein while heating the assembly, at least one of- a local magnetic field is applied to one of the at least two regions, wherein a height of the intermetallic phase is dependent on a magnetic flux of the local magnetic field,- a local electric current is applied to one of the at least two regions, wherein a height of the intermetallic phase is dependent on an electric current density of the local electric current, and- an additional heat and / or an additional cooling is applied to one of the at least two regions, wherein a height of the intermetallic phase is dependent on a temperature of the heat .
18. Method according to one of claims 16 or 17, wherein at least one of- the joining material (4) comprises at least two material systems being different to one another corresponding to the at least two regions to be produced, and- the joining material (4) comprises at least two maximal doping concentrations being different to one another corresponding to the at least two regions to be produced.
19. Method according to one of claims 16 to 18, wherein at least one of- a joining surface of the first joining partner (2) and / or a joining surface of the second joining partner (3) comprises at least two metallization materials being different to one another corresponding to the at least two regions to be produced,- a first joining surface of the first joining partner (2) and / or a second joining surface of the second joining partner (3) comprises at least two surface roughnesses being different to one another corresponding to the at least two regions to be produced.
20. Method according to one of claims 16 to 19 wherein- a joining surface of the first joining partner (2) and / or a joining surface of the second joining partner (3) comprises a diffusion barrier (10) at a region corresponding to the at least one of the two regions to be produced.
Citation Information
Patent Citations
Power Semiconductor Module, Method for Producing a Power Semiconductor Module, and Semiconductor Chip
US20080230905A1
Method for Fabricating a Circuit Substrate Assembly and a Power Electronics Module Comprising an Anchoring Structure for Producing a Changing Temperature-Stable Solder Bond
US20110053319A1
Semiconductor device and method for manufacturing the same
US20160358875A1