Process for obtaining a biologically based bioadhesive from industrial waste
A bio-based adhesive from Plukenetia genus residual cake addresses the toxicity and fossil origin issues of conventional adhesives, offering comparable performance and stability at room temperature, utilizing carbohydrate hydrolysis and natural preservatives.
Patent Information
- Application Number
- PCT/PE2023/050008
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-21
- Filing Date
- 2023-05-13
- Publication Date
- 2024-10-24
AI Technical Summary
Conventional adhesives for the wood and paper industries, such as formaldehyde-based resins, rely on fossil raw materials, require high curing temperatures, and pose health risks due to toxicity, necessitating the development of bio-based alternatives from renewable sources.
A bio-based adhesive is produced from the residual cake of the Plukenetia genus, obtained through cold oil extraction, utilizing carbohydrate hydrolysis and pH adjustments, with optional essential oils as preservatives, allowing for room temperature curing and eliminating toxicity concerns.
The bioadhesive achieves comparable performance to traditional adhesives without health risks, utilizing natural sources entirely and avoiding conflicts with food production, with improved storage properties and thermal stability.
Smart Images

Figure 000015 
Figure 000016 
Figure 000017
Abstract
Description
[0001] PROCESS FOR OBTAINING A BIOLOGICALLY BASED BIOADHESIVE FROM INDUSTRIAL WASTE
[0002] TECHNICAL FIELD
[0003] The present invention relates to obtaining a bio-based adhesive from industrial waste with a high protein content, as an alternative to the use of raw materials of fossil origin conventionally used for the production of adhesives for, for example, wood, paper and cardboard.
[0004] The adhesive can be used, for example, for bonding paper and cardboard surfaces, and in the production of laminates and wood products such as plywood, oriented strand board (OSB), laminated veneer lumber (LVL), medium-density fiberboard (MDF), high-density fiberboard (HDF), wood flooring, curved plywood, particle board, veneer chipboard or MDF.
[0005] STATE OF THE ART (OR BACKGROUND OF THE INVENTION)
[0006] Currently, there are formaldehyde-based resins, mainly urea-formaldehyde (UF) and phenol-formaldehyde (PF) (M., 1998), for the manufacture of chipboard, medium-density fiberboard (MDF), oriented strand board (OSB), plywood and particle board.
[0007] The usual technique for the industrial production of urea-formaldehyde (UF) resins is from the condensation of formaldehyde and urea in an aqueous solution, using ammonia as an alkaline catalyst. The subsequent drying and pulverization has applications such as coatings and adhesives, and it can also be mixed with cellulose as a filler. Under the application of temperature and pressure, the resin, composed of low molecular weight prepolymers, is cured, forming a three-dimensional network of interrelated polymers. Phenol-formaldehyde (PF) resins are conventionally obtained from the reaction of phenols and aldehydes. During synthesis, temperature has a great effect on the characteristics of the final product, so that chain growth through condensations and alternating additions at temperatures below 100 °C (100 °F). sC, and the crosslinking and hardening of resins at temperatures above 100 s C, result in obtaining two types of PF resins: novolac and resoles.
[0008] The usual technique for the industrial production of novolac is the reaction of phenol and formaldehyde under acidic conditions with a molar excess of phenol with a phenol-formaldehyde molar ratio of 1:(0.75-0.85), using oxalic acid as catalyst, while the resoles are obtained by the reaction of phenol and formaldehyde under basic conditions with a molar excess of formaldehyde. The phenol-formaldehyde molar ratio is 1:(1.2-3) using NaOH (sodium hydroxide) as catalyst.
[0009] These adhesives have advantages such as high cost-effectiveness and rapid curing. However, they also have some disadvantages, such as their use of fossil-based raw materials and the need for high curing temperatures. Additionally, these resins have been shown to present drawbacks related to their toxicity and serious health problems as a result of their continuous use (Park, Kang, Park, & Park, 2011) (Ferguson, Mendon, Rawlins, & Thames, 2014).
[0010] This has encouraged the development of adhesives from diverse renewable sources that can replace or substitute conventional adhesives in the wood industry (Antov, Savov, & Neykov, 2020). Some of the raw materials highlighted in recent years include the synthesis of bioadhesives from lignin, tannins, starch, and proteins (Hemmilá, Adamopoulos, Karlsson, & Kumar, 2017) (Antov et al., 2020). Protein-based adhesives have traditionally been obtained from milk casein, collagen from animal hides, fishing industry waste, and soybeans, because proteins of both animal and plant origin have functional groups with ideal characteristics to be used as a base for wood adhesives.
[0011] Casein is the main protein in milk and its use as a glue in wooden frames has been evident since the Renaissance. By the early 19th century, casein-based glues were already being marketed, and a century later, the first adhesive mixtures containing dry casein, lime, and sodium salts were patented. Starting in the 1930s, it began to be replaced by adhesives with greater water resistance, such as phenolic resins (1931–1935), urea formaldehyde (1937), resorcinol (1943), and polyvinyl acetate copolymers (1970) (Bye, 1990).
[0012] The use of animal waste has also been considered to obtain low-cost adhesives. For example, the synthesis of adhesives using hydrolyzed collagen from leather industry waste as an initiator and silane coupling agent (SCA) as a crosslinking agent (Zhou et al., 2017).
[0013] There are mussel protein-based adhesives (MAPs) whose properties have been evaluated in recent years, due to their high adhesive strength and water resistance (Kord Forooshani & Lee, 2017). However, this raw material is not widely available and therefore its cost is high, additionally due to the high cost of adhesives obtained from mussels, this process is not profitable for applications in the wood industry (Song et al., 2016). However, based on these results, studies have been carried out on the modification of proteins from other sources, in order to increase tolerance to humidity (Y. Liu & L¡, 2004).
[0014] In recent years, attention has focused on soybean meal (SF) proteins, a by-product of soybean oil extraction, due to its low price, easy availability, and easy handling (Wescott et al., 2006). Obtaining adhesives from the proteins present in SF has been widely studied due to its extensive advantages (US2010 / 0035098 A1) (Vnucec, Kutnar, & Gorsek, 2017). On the one hand, the abundance of this resource since it is known that for each ton of crude soybean oil, about 5 tons of soybean meal with approximately 50% protein by weight can be obtained (Berk, 1992), (Fhhart & Birkeland, 2014).Additionally, products with a higher protein content can also be obtained from residual soybeans, such as soy protein concentrates (SPC) with approximately 65% protein (Lusas & Rhee, 1995), and soy protein isolate (SPI) which can have a protein content of up to 90% on a moisture-free basis (Frihart & Birkeland, 2014).
[0015] Protein hybrid adhesives that include a certain percentage of conventional adhesives (US2006 / 0234077 A1 ) (WO201 1 / 156380) and bioadhesives with additional fillers (D. Liu et al., 2010) have also been studied. Likewise, the production of bioadhesives from mixtures of different renewable raw materials has been evaluated, such as an adhesive composition comprising the reaction of functional groups from lignin and soy protein, together with curing agents of the amine, amide, ímine or ímide type with a heterocyclic functional group (Grot, 2009). In addition, it is also possible to obtain a wood adhesive from depolymerized lignin together with a byproduct of biodiesel production (Zhu, Wang, Li, & Sun, 2017).Wheat gluten (WG) is a by-product of wheat starch processing and bioethanol production that has also been used together with soy protein to obtain bioadhesives that can be applied in the manufacture of particle boards (Khosravi, Khabbaz, Nordqvist, & Johansson, 2010).
[0016] Likewise, in the state of the art there is patent document US8057892B2, which discloses a bioadhesive for wood which mainly comprises a protein material, an acidity regulator, an aromatic compound, a curing agent and a preservative, where the adhesive has the advantage that it can be stored at room temperature and its shelf life can last for a year without cold storage, no or almost no formaldehyde is released during production, the wood adhesive has high water resistance and can even reach the standard of grade I and grade II; The curing temperature of the wood adhesive is 1 10 ° C or more, which is beneficial for its use. However, this background requires its mixture with various additives to be functional.
[0017] DESCRIPTION OF THE INVENTION
[0018] As a solution to the aforementioned problems, the present invention was developed, which comprises the use of an industrial residue from the extraction of products from the Plukenetia genus, as an alternative to the use of raw material of fossil origin conventionally used for the production of adhesives for wood, paper and cardboard.
[0019] The cold-pressing or extrusion process is currently the most widely used method for extracting virgin seed oil, which is valued for its nutritional properties both in Peru and abroad. This process produces a byproduct of low commercial value, a residual cake with a high protein content that could be utilized using the proposed process.
[0020] This represents an improvement in the state of the art, as the final product produced with this process does not present toxicity or health problems as a result of its continuous use. Furthermore, it will not be mixed with conventional adhesives and is entirely derived from natural sources, specifically the residual cake. Another important improvement is that the bioadhesive cures at room temperature.
[0021] The inclusion of carbohydrate hydrolysis contributes to process improvement, as it allows for comprehensive utilization of the residual cake. This allows for higher yields, considering the large amount of carbohydrates present in the cake formed by cold-pressing seeds of the Plukenetia genus. It is possible to use strong inorganic acids at low concentrations, which ionize in aqueous solution, such as HNO3, H2SO4, or HCl, among others.
[0022] Additionally, since water-based bioadhesives such as the one proposed may have storage issues, additives such as essential oils with known antimicrobial properties, which act as a natural preservative for the bioadhesive, or other synthetic additives, are used.
[0023] The adhesive obtained from waste cake presents a similar performance and adhesive power compared to other natural adhesives. However, other natural adhesives use inputs that compete with food production, while the bioadhesive obtained from Plukenetia products uses the waste cake left over after oil extraction. For human food and protein supplements made from this waste cake, the problem is that it requires the use of toxic solvents in the procedures and cannot guarantee 100% effective removal of the solvent in the final product, which is unattractive to consumers.Therefore, the proposed bioadhesive would not conflict with food production, given the limitations of producing quality protein for human consumption from the residual cake. While it is possible to isolate the protein, it is very difficult to ensure it is suitable for consumption and free of traces of solvents used during its extraction, such as hexane. Furthermore, attempts have been made to use this residual cake for animal feed with little success due to its high content of antinutritional factors and the low added value of the final product.
[0024] The process starts with the residual cake obtained from the cold extraction of oil from products of the Plukenetia genus using an expeller. The process consists of removing the residual oil from the cake formed, then extracting the proteins contained in the residual cake and performing a hydrolyzation process on the carbohydrates present in the cake, ultimately obtaining the bioadhesive from the mixture of proteins and hydrolyzed carbohydrates.
[0025] Specifically, to obtain the bio-based bioadhesive from industrial waste, the following steps are carried out:
[0026] - Degreasing a residual cake obtained from the extraction of oil from seeds of the genus Plukenetia to obtain a degreased cake;
[0027] - Prepare a solution by mixing the defatted cake in distilled water at a concentration of 10 to 30% w / w;
[0028] - Adjust the pH of the solution from the previous step to a value of 7.5 to 9.0 with a pH modifying agent, so that a solution with adjusted pH is obtained;
[0029] - Centrifuge the pH-adjusted solution so that a centrifuged solution is obtained;
[0030] - Perform a first vacuum filtration of the centrifuged solution to separate it into two phases, obtaining a supernatant containing soluble carbohydrates and a precipitate containing insoluble carbohydrates;
[0031] - Adjust the pH of the supernatant until the isoelectric point is reached, so that a pH-adjusted supernatant is obtained;
[0032] - Centrifuge the pH-adjusted supernatant so that a centrifuged supernatant is obtained;
[0033] - Perform a second vacuum filtration of the centrifuged supernatant to separate two phases, obtaining a precipitated protein and soluble carbohydrates;
[0034] - Mix soluble and insoluble carbohydrates, so that mixed carbohydrates are obtained;
[0035] - Perform an acid hydrolysis of the mixed carbohydrates, in a range between 1 M to 4M, and between 80 and 150°C for a time between 1 and 5 hours, in such a way that hydrolyzed carbohydrates are obtained;
[0036] - Neutralize the hydrolyzed carbohydrates by slowly adding an alkaline solution, so that hydrolyzed and neutralized carbohydrates are obtained;
[0037] - Denature the protein present in the precipitate formed after the second vacuum filtration, using an alkalizing agent until reaching a pH of 1.1, so that denatured protein is obtained;
[0038] - Mix the denatured protein and the hydrolyzed and neutralized carbohydrates, maintaining the pH, so that a mixture of proteins and carbohydrates is obtained; and,
[0039] - Add between 1 to 5% v / v of essential oil or synthetic preservatives under stirring to the mixture of proteins and carbohydrates, so that the bioadhesive is obtained.
[0040] BRIEF DESCRIPTION OF THE FIGURES
[0041] FIGURE NO. 1: An operations diagram of the production process is shown.
[0042] FIGURE NO. 2: Comparison between FTIR spectra obtained from the cake of products of the Plukenetia genus and the bioadhesive obtained.
[0043] FIGURE NO. 3: A) Thermogravimetric curve of the bioadhesive and B) its derivative.
[0044] FIGURE NO. 4: Table of identification of characteristic peaks of the FTIR spectra obtained from the residual cake of products of the Plukenetia genus.
[0045] DETAILED DESCRIPTION AND / OR PREFERRED EMBODIMENTS
[0046] Figure 1 shows an operational flowchart of the production process. Upon reaching the first centrifugation stage, soluble carbohydrates are mixed with HCl on the right side, precipitating and denaturing proteins. On the left side, insoluble and soluble carbohydrates are mixed, and hydrolyzed carbohydrates are neutralized. Characterization of the residual cake of Plukenetia products and the resulting bioadhesive:
[0047] The result of the determination of the amount of proteins present in the raw material (residual cake of Plukenetia genus product) is attached. The FTIR spectrum of the bioadhesive was obtained using a Shimadzu IR Tracer-100 FTIR spectrophotometer. This analysis was carried out in order to understand the reaction mechanism between hydrolyzed carbohydrates and the protein residue of the defatted cake to form the bioadhesive. Table 1 summarizes the peaks identified in the residual cake, with the bond vibration of functional groups characteristic of carbohydrates, proteins and fats. On the other hand, characteristic peaks of the Amide I, II and III functional groups are observed, which are characteristic of proteins, this predicts that the residual cake of Plukenetia genus products is a protein-rich residue.
[0048] The FTIR assay performed on the obtained product was intended to evaluate the reaction mechanism between the hydrolyzed carbohydrates and the protein residue of the defatted residual cake to form the bioadhesive (Figure 2). The FTIR spectra obtained from the cake and the bioadhesive were compared, as shown in Figure 2. The results show differences in both spectra in the range of 1000 to 1700 cm 1 . Generally, the Maillard reaction refers to the interaction initiated between the amino groups of proteins and the aldehyde groups of reducing sugars, this reaction leads to the loss of NH2 bonds and the formation of compounds with (CO bonds), (CN bonds) and (CN bonds). This is demonstrated in the FTIR spectrum obtained from the bioadhesive, since the intensity of the characteristic peaks of the NH2 bonds present in the Amide I, II and III groups of the protein (located at 1652, 1545 and 1244 cnr 1respectively), is reduced compared to the FTIR spectrum of the Torta. In addition, the formation of a new peak at 1048 cm is observed. -1 , which is characteristic of the C-O bonds generated by the reaction. On the other hand, the intensity of the characteristic peaks of the CN bonds (located at 1085 and 1158 cm-1 ) increases in the bioadhesive spectrum. Therefore, these results validate the Maillard reaction mechanism that led to the formation of the bioadhesive.
[0049] On the other hand, the thermal stability of the bioadhesive was analyzed in the Renewable Energy Laboratory of the National Agrarian University La Molina. The equipment used was a LECO brand TGA701 thermogravimetric analyzer. The sample was heated from 25 to 600 °C at a heating rate of 10 °C / min under a nitrogen flow of 20 mL / min. In this test, the thermogravimetric curve of the sample and its derivative were obtained and analyzed. The TGA was carried out in order to evaluate the influence of the binding between proteins and reducing sugars, responsible for the formation of the bioadhesive, on its thermal stability. The obtained thermogravimetric curve and its derivative are shown in Figure 3. These were divided into 3 regions: 25-107 °C (Region I), 107-300 °C (Region II), and 300-500 °C (Region III). In the first region, the weight loss of the bioadhesive is attributed to the evaporation of residual moisture, which represents 4.26%. In the second region, the weight loss is considerable, reaching 30.47% due to the loss of protein micromolecules and, consequently, the decomposition of the chemical bond that unites the proteins and reducing sugars responsible for the formation of the bioadhesive. In the third and final region, there is a weight loss of 23.84%, which corresponds to the degradation of the bioadhesive. Therefore, the bioadhesive does not undergo significant changes at temperatures below 107°C; however, when this temperature is exceeded, its behavior can vary significantly as the proteins, essential components for the formation of the bioadhesive, begin to degrade.
[0050] In a preferred embodiment, before starting the bioadhesive synthesis process, the residual cake is degreased by Soxhlet extraction to remove the remaining oil. There are different solvents that can be used in this stage, such as petroleum ether or hexane.
[0051] In a preferred embodiment, some curing agents could be added which could increase the storage properties of the adhesive, for example, ammonium chloride, potassium pyrosulfate, sodium sulfite, sodium dihydrogen phosphate, sodium tetraborate, sodium hypophosphite, sodium bisulfate, ferric sulfate, sodium silicate, triethylamine, 3,3',4,4'-benzophenonetetracarboxylic acid dianhydze, 2-dodecen-1-ylsuccinic anhydride, decanedihydrazide, chlorendic anhydride, ammonium perchlorate or a mixture thereof. On the other hand, after adding between 1 to 5% v / v of essential oil or synthetic preservatives under stirring, the obtained bioadhesive can be filtered, dried or lyophilized and then the product can be stored in a cool, dry place at room temperature.
[0052] It can also be stored in gel form at room temperature as long as it is kept sealed, and once opened it is recommended to keep it refrigerated.
Claims
CLAIMS 1.- A process for obtaining a bio-based bioadhesive from industrial waste characterized in that it comprises: - Degreasing a residual cake obtained from the extraction of oil from seeds of the genus Plukenetia to obtain a degreased cake; - Prepare a solution by mixing the defatted cake in distilled water at a concentration of 10 to 30% w / w; - Adjust the pH of the solution from the previous step to a value of 7.5 to 9.0 with a pH modifying agent, so that a solution with adjusted pH is obtained; - Centrifuge the pH-adjusted solution so that a centrifuged solution is obtained; - Perform a first vacuum filtration of the centrifuged solution to separate it into two phases, obtaining a supernatant containing soluble carbohydrates and a precipitate containing insoluble carbohydrates; - Adjust the pH of the supernatant until the isoelectric point is reached, so that a pH-adjusted supernatant is obtained; - Centrifuge the pH-adjusted supernatant so that a centrifuged supernatant is obtained; - Perform a second vacuum filtration of the centrifuged supernatant to separate two phases, obtaining a precipitated protein and soluble carbohydrates; - Mix soluble and insoluble carbohydrates, so that mixed carbohydrates are obtained; - Perform an acid hydrolysis of the mixed carbohydrates, in a range between 1 M to 4M, and between 80 and 150°C for a time between 1 and 5 hours, in such a way that hydrolyzed carbohydrates are obtained; - Neutralize the hydrolyzed carbohydrates by slowly adding an alkaline solution, so that hydrolyzed and neutralized carbohydrates are obtained; - Denature the protein present in the precipitate formed after the second vacuum filtration, using an alkalizing agent until reaching a pH of 11, so that denatured protein is obtained; - Mix the denatured protein and the hydrolyzed and neutralized carbohydrates, maintaining the pH, so that a mixture of proteins and carbohydrates is obtained; and, - Add between 1 to 5% v / v of essential oil or synthetic preservatives under stirring to the mixture of proteins and carbohydrates, so that the bioadhesive is obtained. 2.- The process for obtaining a biological-based bioadhesive, according to claim 1, characterized in that the bioadhesive obtained after adding the essential oil or synthetic preservatives is filtered. 3.- The process for obtaining a biological-based bioadhesive, according to claim 1, characterized in that the bioadhesive obtained after adding the essential oil or synthetic preservatives is dried. 4.- The process for obtaining a biological-based bioadhesive, according to claim 1, characterized in that the bioadhesive obtained after adding the essential oil or synthetic preservatives is lyophilized.
Citation Information
Patent Citations
Synergistic effect modified soy protein cementing compound and preparation method thereof
CN101531884A
Preparation method for parthenocissus tricuspidata sucker polysaccharide biological adhesive
CN105062413A
Bioadhesive from distillers' dried grains with solubles (DDGS) and the methods of making those