Sic power MOS structure and manufacturing method therefor
By using a combination of shielding area and shielded gate structure in SiC power MOS devices, the problem of easy breakdown of the gate silicon oxide layer is solved, the voltage resistance and long-term reliability of the device are improved, and the on-resistance is reduced.
Patent Information
- Application Number
- PCT/CN2023/136346
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-25
- Filing Date
- 2023-12-05
- Publication Date
- 2024-10-31
AI Technical Summary
The gate silicon oxide layer in SiC power MOS devices is easily broken down, which affects the performance of the device, especially the electric field concentration problem of trench gate devices, which affects its voltage resistance and long-term reliability.
A double shielding structure is formed by using a shielding area and a shielding gate structure. By introducing a medium doping area between the trench and the shielding area, the electric field at the corner of the gate oxide layer is reduced, and through the depth of the shielding area and the design of the shielding gate, the electric field is reduced. The electric field is concentrated to form a more stable electric field distribution.
It effectively improves the voltage withstand capability of SiC power MOS devices and the long-term reliability of the gate oxide layer, and reduces the on-resistance. Compared with using the masking area structure alone, the on-resistance is reduced by more than 20%.
Smart Images

Figure CN2023136346_31102024_PF_FP_ABST
Abstract
Description
SiC power MOS structure and manufacturing method thereof
[0001] Related applications
[0002] This application claims priority to Chinese patent application No. 2023104568338, filed on April 25, 2023, entitled “A SiC power MOS structure and manufacturing method,” the entire text of which is hereby incorporated by reference. Technical Field
[0003] The present application belongs to the field of semiconductor device technology, and specifically relates to a silicon carbide (SiC) power metal-oxide-semiconductor (MOS) structure and a manufacturing method thereof. Background Art
[0004] SiC MOS devices are currently the mainstream semiconductor devices. The electric field strength experienced by the gate silicon oxide surface in a SiC MOSFET is approximately 2.5 times that of its corresponding silicon carbide surface. Because silicon carbide has a high critical breakdown electric field strength (approximately 10 times that of silicon), the electric field strength experienced by the gate silicon oxide in a SiC MOSFET is extremely high, an order of magnitude higher than that experienced by the gate silicon oxide in Si MOSFETs and insulated gate bipolar transistors (IGBTs). This is particularly true for trench-gate SiC MOSFETs, where the gate silicon oxide experiences even higher electric field strength. This can lead to problems such as the gate silicon oxide layer being susceptible to breakdown, thus affecting device performance.
[0005] It should be noted that the above introduction to the technical background is only for the convenience of providing a clear and complete description of the technical solutions of this application and for the convenience of understanding by those skilled in the art. It cannot be considered that the above technical solutions are well known to those skilled in the art simply because these solutions are described in the background technology part of this application.
[0006] Summary of the Invention
[0007] In one aspect, the present application provides a method for manufacturing a SiC power MOS structure, comprising the following steps:
[0008] Providing a first conductive type substrate, and forming a first conductive type epitaxial layer on the substrate, wherein the doping concentration of the substrate is greater than the doping concentration of the epitaxial layer;
[0009] forming a second conductive type base region at a predetermined position of the epitaxial layer, and forming a second conductive type masking region outside the base region, wherein the doping concentration of the masking region is greater than the doping concentration of the base region, and the depth of the masking region is greater than the depth of the base region;
[0010] forming a first conductive type source region in the base region, and forming a trench in the epitaxial layer, the trench penetrating the source region and the base region in a vertical direction;
[0011] forming a shield gate structure in the trench, the shield gate structure comprising a gate oxide layer, a shield gate, and a control gate, wherein the gate oxide layer comprises a bottom oxide layer and a sidewall oxide layer, the bottom oxide layer is located at the bottom of the trench, the sidewall oxide layer is located above the bottom oxide layer and on the sidewalls of the trench, the shield gate is located in the bottom oxide layer, and the control gate is located inside the sidewall oxide layer;
[0012] A source electrode and a gate electrode are formed on the upper surface of the epitaxial layer, wherein the source electrode is electrically connected to the source region, the gate electrode is electrically connected to the control gate, and the shielding gate is electrically connected to the source electrode or the gate electrode.
[0013] In some embodiments, the shielding gate is spaced apart from the control gate by a predetermined distance, and the shielding gate is electrically connected to the source electrode.
[0014] In some embodiments, an upper surface of the shielding gate is electrically connected to a lower surface of the control gate, and the shielding gate is electrically connected to the gate electrode.
[0015] In some embodiments, before forming a second conductive type base region at a predetermined position of the epitaxial layer and forming a second conductive type masking region outside the base region, the following steps are further included:
[0016] A middle doped region of the first conductivity type is formed in the epitaxial layer, wherein the doping concentration of the middle doped region is greater than the doping concentration of the epitaxial layer, wherein the base region is located in the middle doped region, and the trench also extends into the middle doped region in a vertical direction.
[0017] In some embodiments, the first conductivity type is N-type, and the second conductivity type is P-type.
[0018] In some embodiments, the first conductivity type is P-type, and the second conductivity type is N-type.
[0019] In some embodiments, the source electrode is further located above the masking region and electrically connected to the masking region.
[0020] In some embodiments, the method further includes: forming a drain electrode on the lower surface of the substrate.
[0021] On the other hand, the present application also provides a SiC power MOS structure, including:
[0022] a first conductive type substrate, with a first conductive type epitaxial layer disposed above the substrate, wherein the doping concentration of the substrate is greater than the doping concentration of the epitaxial layer;
[0023] A second conductive type base region is located in the epitaxial layer;
[0024] a second conductive type shielding region located outside the base region, wherein the doping concentration of the shielding region is greater than the doping concentration of the base region, and the depth of the shielding region is greater than the depth of the base region;
[0025] A first conductive type source region, located in the base region;
[0026] a trench located in the epitaxial layer, wherein the trench vertically penetrates the source region and the base region;
[0027] a shield gate structure located in the trench, the shield gate structure comprising a gate oxide layer, a shield gate, and a control gate, wherein the gate oxide layer comprises a bottom oxide layer and a sidewall oxide layer, the bottom oxide layer is located at the bottom of the trench, the sidewall oxide layer is located above the bottom oxide layer and on the sidewalls of the trench, the shield gate is located in the bottom oxide layer, and the control gate is located inside the sidewall oxide layer;
[0028] a source electrode, located on an upper surface of the epitaxial layer, the source electrode being electrically connected to the source region;
[0029] A gate electrode is located on the upper surface of the epitaxial layer, and the gate electrode is electrically connected to the control gate.
[0030] In some embodiments, the shielding gate is spaced apart from the control gate by a predetermined distance, and the shielding gate is electrically connected to the source electrode.
[0031] In some embodiments, an upper surface of the shielding gate is electrically connected to a lower surface of the control gate, and the shielding gate is electrically connected to the gate electrode.
[0032] In some embodiments, a first conductive type middle doping region is further included, wherein the middle doping region is located between the masking region and the shielding gate structure, and the doping concentration of the middle doping region is greater than the doping concentration of the epitaxial layer.
[0033] In some embodiments, the first conductivity type is N-type, and the second conductivity type is P-type.
[0034] In some embodiments, the first conductivity type is P-type, and the second conductivity type is N-type.
[0035] In some embodiments, the doping concentration of the intermediate doping region is lower than the doping concentration of the substrate.
[0036] In some embodiments, the depth of the masking region is greater than the depth of the control gate.
[0037] The details of one or more embodiments of the present application are set forth in the following drawings and description. Other features, objects, and advantages of the present application will become apparent from the description, drawings, and claims. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the conventional technology, the following briefly introduces the drawings required for use in the embodiments or the conventional technology descriptions. Obviously, the drawings described below are merely embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on the disclosed drawings without any creative work.
[0039] FIG1 is a schematic structural diagram of a first trench-gate SiC power MOS device in the related art.
[0040] FIG2 is a schematic structural diagram of a second trench-gate SiC power MOS device in the related art.
[0041] FIG. 3 is a process flow chart showing a method for fabricating a SiC power MOS structure according to an embodiment of the present application.
[0042] FIG. 4 is a schematic diagram showing a method for fabricating a SiC power MOS structure according to an embodiment of the present application, wherein a substrate is provided and an epitaxial layer is formed on the substrate.
[0043] FIG. 5 is a schematic diagram showing a method for fabricating a SiC power MOS structure according to an embodiment of the present application, wherein a mid-doped region is formed in an epitaxial layer.
[0044] FIG. 6 is a schematic diagram showing the formation of a base region and a masking region in an epitaxial layer in a method for fabricating a SiC power MOS structure according to an embodiment of the present application.
[0045] FIG. 7 is a schematic diagram showing a method for fabricating a SiC power MOS structure according to an embodiment of the present application, wherein a source region is formed in a base region and a trench is formed in an epitaxial layer.
[0046] FIG. 8 is a schematic diagram showing a first shield gate structure formed in a trench in a method for fabricating a SiC power MOS structure according to an embodiment of the present application.
[0047] FIG. 9 is a schematic diagram showing a second shield gate structure formed in a trench in a method for fabricating a SiC power MOS structure according to an embodiment of the present application.
[0048] FIG. 10 is a schematic diagram showing a method for fabricating a SiC power MOS structure according to an embodiment of the present application, wherein a source electrode and a gate electrode are formed on the upper surface of the epitaxial layer, and a drain electrode is formed on the lower surface of the substrate. DETAILED DESCRIPTION
[0049] The following describes the embodiments of the present application through specific examples. Those skilled in the art will readily understand the other advantages and benefits of the present application from the disclosure herein. The present application may also be implemented or applied through various other specific embodiments, and the details in this specification may be modified or altered based on different viewpoints and applications without departing from the spirit of the present application.
[0050] FIG1 shows a schematic structural diagram of a trench-gate SiC power MOS device known to the applicant, comprising an N+ substrate 01, an N-drift region 02, a P+ contact region 03, a P-base region 04, an N+ source region 05, a trench gate 06, a gate oxide 07, a source electrode 08, and a gate electrode 09. The applicant discovered that a trench gate corner approaching 90° causes electric field concentration, making the gate oxide 07 at this corner extremely susceptible to breakdown. FIG2 shows a schematic structural diagram of a second trench-gate SiC power MOS device known to the applicant. To reduce electric field concentration at the trench gate corner and improve device voltage resistance and gate oxide reliability, the device structure shown in FIG2 increases the depth of the P+ contact region 03 to form a deep P+ junction shielding structure, which can reduce electric field concentration at the trench gate corner. However, the applicant discovered that due to the thin gate oxide 07, the electric field in the oxide layer at the corner remains high, affecting the long-term reliability of the device. In addition, since the deep P+ junction shielding structure occupies part of the drift region, the conductive area is reduced and the Rsp (on-resistance per unit area) of the device is increased.
[0051] Based on this, how to improve the voltage resistance of SiC power MOS devices, improve the long-term reliability of the gate oxide layer, and reduce the on-resistance are technical problems to be solved by those skilled in the art.
[0052] Referring to Figures 1 to 10 , embodiments of the present application provide a SiC power MOS structure and a method for fabricating the same. It should be noted that the diagrams provided in the embodiments of the present application are merely schematic illustrations of the basic concept of the present application. Therefore, the diagrams only show components relevant to the present application and are not drawn according to the number, shape, and size of components in actual implementation. In actual implementation, the type, quantity, and proportion of each component may be arbitrarily varied, and the component layout may also be more complex.
[0053] Example 1
[0054] This embodiment provides a method for manufacturing a SiC power MOS structure. Please refer to FIG3 , which shows a process flow chart of the method, including the following steps:
[0055] S1: providing a first conductive type substrate, and forming a first conductive type epitaxial layer on the substrate, wherein the doping concentration of the substrate is greater than the doping concentration of the epitaxial layer;
[0056] S2: forming a second conductive type base region at a predetermined position of the epitaxial layer, and forming a second conductive type masking region outside the base region, wherein the doping concentration of the masking region is greater than the doping concentration of the base region, and the depth of the masking region is greater than the depth of the base region;
[0057] S3: forming a first conductivity type doped source region in the base region, and forming a trench in the epitaxial layer, wherein the trench vertically penetrates the source region and the base region;
[0058] S4: forming a shield gate structure in the trench, the shield gate structure comprising a gate oxide layer, a shield gate, and a control gate, wherein the gate oxide layer comprises a bottom oxide layer and a sidewall oxide layer, the bottom oxide layer is located at the bottom of the trench, the sidewall oxide layer is located above the bottom oxide layer and on the sidewalls of the trench, the shield gate is located in the bottom oxide layer, and the control gate is located inside the sidewall oxide layer;
[0059] S5: forming a source electrode and a gate electrode on the upper surface of the epitaxial layer, wherein the source electrode is electrically connected to the source region and the masking region, the gate electrode is electrically connected to the control gate, and the shielding gate is electrically connected to the source electrode or the gate electrode.
[0060] First, referring to FIG. 4 , step S1 is performed: providing a first conductive type substrate 1 , and forming a first conductive type epitaxial layer 2 on the substrate 1 , wherein the doping concentration of the substrate 1 is greater than the doping concentration of the epitaxial layer 2 .
[0061] As an example, in this embodiment, the first conductivity type is N-type, and the second conductivity type is P-type; in other examples, the first conductivity type may be P-type, and the second conductivity type may be N-type.
[0062] As an example, the substrate 1 is heavily N-type doped, and the epitaxial layer 2 is lightly N-type doped.
[0063] Next, please refer to Figures 5 to 6 and execute step S2: form a second conductive type base region 4 at a preset position of the epitaxial layer 2, and form a second conductive type masking region 5 outside the base region 4, wherein the doping concentration of the masking region 5 is greater than the doping concentration of the base region 4, and the depth of the masking region 5 is greater than the depth of the base region 4.
[0064] As an example, please refer to Figure 5. Before forming a base region 4 at a preset position of the epitaxial layer 2 and forming a masking region 5 outside the base region 4, the method also includes a step of forming a first conductive type middle doping region 3 in the epitaxial layer 2, wherein the doping concentration of the middle doping region 3 is greater than the doping concentration of the epitaxial layer 2, and the doping concentration of the middle doping region 3 is less than the doping concentration of the substrate 1.
[0065] As an example, referring to FIG6 , the base region 4 is formed at a predetermined position of the epitaxial layer 2, and the masking region 5 is formed outside the base region 4, wherein the base region 4 and the masking region 5 are located in the medium-doped region 3. Specifically, the base region 4 is P-type doped, and the masking region 5 is heavily P-type doped.
[0066] Next, referring to FIG. 7 , step S3 is performed: forming a first conductivity type source region 6 in the base region 4 , and forming a trench in the epitaxial layer 2 , the trench vertically penetrating the source region 6 and the base region 4 .
[0067] As an example, the source region 6 is heavily N-type doped, and the trench also penetrates the medium-doped region 3 in the vertical direction.
[0068] Next, please refer to Figures 8 to 9, and perform step S4: forming a shield gate structure in the trench, the shield gate structure includes a gate oxide layer 7, a shield gate 8 and a control gate 9, wherein the gate oxide layer 7 includes a bottom oxide layer and a sidewall oxide layer, the bottom oxide layer is located at the bottom of the trench, the sidewall oxide layer is located above the bottom oxide layer and on the sidewall of the trench, the shield gate 8 is located in the bottom oxide layer, and the control gate 9 is located on the inner side of the sidewall oxide layer.
[0069] As an example, please refer to FIG8 , which is a schematic diagram showing a first shielding gate structure formed in a trench, wherein the shielding gate 8 is spaced apart from the control gate 9 by a preset distance, and the shielding gate 8 is electrically connected to the source electrode 10 (as shown in FIG10 ).
[0070] As an example, please refer to Figure 9, which shows a schematic diagram of forming a second shielding gate structure in a trench, wherein the upper surface of the shielding gate 8 is electrically connected to the lower surface of the control gate 9, that is, the shielding gate 8 is electrically connected to the gate electrode 11.
[0071] As an example, the depth of the masking region 5 is greater than the depth of the control gate 9. The masking region 5 and the epitaxial layer 2 form a PN junction, which can change the electric field distribution within the device and reduce the electric field at the corner of the gate oxide layer 7. In addition, a shielded gate structure is formed in the trench, further improving the device's withstand voltage capability. In other words, in this embodiment, the masking region and the shielded gate form a double-shielding structure. Furthermore, because there are no 90° trench corners in the gate oxide layer, the electric field in the gate oxide layer is very low when the device is turned off, ensuring the long-term reliability of the gate oxide layer.
[0072] As an example, the middle doped region 3 is introduced between the trench and the masking region 5. Since the doping concentration of the middle doped region 3 is higher than the doping concentration of the epitaxial layer 2, the on-resistance of this region is reduced. Under the same withstand voltage condition, Rsp can be reduced by more than 20% compared with the structure in which only the masking region is set.
[0073] As an example, referring to FIG. 10 , step S5 is performed: a source electrode 10 and a gate electrode 11 are formed on the upper surface of the epitaxial layer 2 , wherein the source electrode 10 is electrically connected to the source region 6 , and the gate electrode 11 is electrically connected to the control gate 9 .
[0074] As an example, the source electrode 10 is also located above the masking area 5 and is electrically connected to the masking area 5 .
[0075] As an example, the method further includes a step of forming a drain electrode 12 on the lower surface of the substrate 1 .
[0076] As described above, in the fabrication method of the SiC power MOS structure of this embodiment, the masking region and the shielded gate form a double-shielded structure. This ensures a very low electric field in the gate oxide layer when the device is off, thus ensuring the long-term reliability of the gate oxide layer. Furthermore, a mid-doped region is introduced between the trench and the masking region to reduce the on-resistance of this region. Under the same withstand voltage, Rsp can be reduced by over 20% compared to a structure with only a masking region.
[0077] It should be understood that, although the various steps in the flowcharts involved in the embodiments described above are shown in sequence as indicated by the arrows, these steps are not necessarily performed in sequence in the order indicated by the arrows. Unless otherwise specified herein, there is no strict order restriction on the execution of these steps, and these steps can be performed in other orders. Moreover, at least a portion of the steps in the flowcharts involved in the embodiments described above can include multiple steps or multiple stages, and these steps or stages are not necessarily performed at the same time, but can be performed at different times, and the execution order of these steps or stages is not necessarily performed in sequence, but can be performed in turn or alternately with other steps or at least a portion of the steps or stages in other steps.
[0078] Example 2
[0079] This embodiment provides a SiC power MOS structure, which can be manufactured by the manufacturing method described in the first embodiment, but is not limited to the manufacturing method described in the first embodiment.
[0080] Referring to Figure 10 , the SiC power MOS structure includes a substrate 1, an epitaxial layer 2, a base region 4, a shielding region 5, a source region 6, a trench, a shielded gate structure, a source electrode 10, and a gate electrode 11. The substrate 1 is of the first conductivity type, the epitaxial layer 2 is located above the substrate 1, and the doping concentration of the epitaxial layer 2 is greater than that of the epitaxial layer 2. The base region 4 is of the second conductivity type and is located within the epitaxial layer 2. The shielding region 5 is of the second conductivity type and is located outside the base region 4. The doping concentration of the shielding region 5 is greater than that of the base region 4, and the depth of the shielding region 5 is greater than that of the base region 4. The source region 6 is of the first conductivity type and is located within the base region 4. The trench is located within the epitaxial layer 2 and vertically penetrates the source region 6 and the base region 4. The shielded gate structure is located within the trench and includes a gate oxide layer 7, a shielding gate 8, and a control gate 9. The gate oxide layer 7 includes a bottom oxide layer and a sidewall oxide layer. The bottom oxide layer is located at the bottom of the trench, and the sidewall oxide layer is located above the bottom oxide layer and on the sidewalls of the trench. The shield gate 8 is located in the bottom oxide layer, and the control gate 9 is located inside the sidewall oxide layer. The source electrode 10 is located on the upper surface of the epitaxial layer 2 and is electrically connected to the source region 6. The gate electrode 11 is located on the upper surface of the epitaxial layer 2 and is electrically connected to the control gate 9.
[0081] As an example, in this embodiment, the first conductivity type is N-type, and the second conductivity type is P-type; in other examples, the first conductivity type may be P-type, and the second conductivity type may be N-type.
[0082] Specifically, the substrate 1 is heavily N-type doped, the epitaxial layer 2 is lightly N-type doped, the base region 4 is P-type doped, the masking region 5 is heavily P-type doped, and the source region 6 is heavily N-type doped.
[0083] As an example, the shield gate 8 is spaced a predetermined distance from the control gate 9, and the shield gate 8 is electrically connected to the source electrode 10. In another example, as shown in FIG9 , the upper surface of the shield gate 8 is electrically connected to the lower surface of the control gate 9, that is, the shield gate 8 is electrically connected to the gate electrode 11.
[0084] As an example, the source electrode 10 is also located above the masking area 5 and is electrically connected to the masking area 5 .
[0085] As an example, the depth of the masking region 5 is greater than the depth of the control gate 9. The masking region 5 and the epitaxial layer 2 form a PN junction, which can change the electric field distribution inside the device and reduce the electric field at the corner of the gate oxide layer 7; and a shielding gate structure is provided in the groove to further improve the voltage resistance of the device. That is, in this embodiment, a double shielding structure is formed by using the masking region and the shielding gate. At the same time, since there is no 90° trench corner at the gate oxide layer, the electric field in the gate oxide layer is very low when the device is turned off, thereby ensuring the long-term reliability of the gate oxide layer.
[0086] As an example, a middle doped region 3 is also included, and the middle doped region 3 is located between the masking region 5 and the trench, wherein the middle doped layer 3 is of the first conductive type and the doping concentration is greater than the doping concentration of the epitaxial layer 2. By setting the middle doped region 3, the on-resistance of the region is reduced. Under the same withstand voltage condition, Rsp can be reduced by more than 20% compared with the structure in which only the masking region is set.
[0087] In summary, in the SiC power MOS structure and fabrication method of this application, the masking region and shielded gate form a double-shielded structure. This ensures a very low electric field in the gate oxide layer when the device is off, ensuring the long-term reliability of the gate oxide layer. Furthermore, a mid-doped region is introduced between the trench and the masking region to reduce the on-resistance of this region. Under the same withstand voltage, Rsp can be reduced by over 20% compared to a structure with only a masking region. Therefore, this application effectively overcomes the various shortcomings of the prior art and has high industrial value.
[0088] The technical features of the above-mentioned embodiments can be combined arbitrarily. In order to make the description concise, not all possible combinations of the technical features in the above-mentioned embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0089] The above-described embodiments merely represent several implementation methods of the present application. While the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the patent application. It should be noted that a person of ordinary skill in the art may make various modifications and improvements without departing from the spirit of the present application, and these modifications and improvements fall within the scope of protection of the present application. Therefore, the scope of protection of the present patent application shall be determined by the appended claims.
Claims
1. A method for manufacturing a SiC power MOS structure, comprising the following steps: Providing a first conductive type substrate, and forming a first conductive type epitaxial layer on the substrate, wherein the doping concentration of the substrate is greater than the doping concentration of the epitaxial layer; Forming a second conductive type base region at a preset position of the epitaxial layer, and forming a second conductive type masking region outside the base region, wherein the doping concentration of the masking region is greater than the doping concentration of the base region, and the depth of the masking region is greater than the depth of the base region; Forming a first conductive type source region in the base region, and forming a trench in the epitaxial layer, wherein the trench vertically penetrates the source region and the base region; Forming a shield gate structure in the trench, the shield gate structure comprising a gate oxide layer, a shield gate and a control gate, wherein the gate oxide layer comprises a bottom oxide layer and a sidewall oxide layer, the bottom oxide layer is located at the bottom of the trench, the sidewall oxide layer is located above the bottom oxide layer and at the sidewall of the trench, the shield gate is located in the bottom oxide layer, and the control gate is located on the inner side of the sidewall oxide layer; A source electrode and a gate electrode are formed on the upper surface of the epitaxial layer, wherein the source electrode is electrically connected to the source region, the gate electrode is electrically connected to the control gate, and the shielding gate is electrically connected to the source electrode or the gate electrode.
2. The method for manufacturing a SiC power MOS structure according to claim 1, wherein: The shielding gate is spaced apart from the control gate by a preset distance, and the shielding gate is electrically connected to the source electrode.
3. The method for manufacturing a SiC power MOS structure according to claim 1, wherein: An upper surface of the shielding gate is electrically connected to a lower surface of the control gate, and the shielding gate is electrically connected to the gate electrode.
4. The method for manufacturing a SiC power MOS structure according to any one of claims 1 to 3, wherein: Before forming a second conductive type base region at a preset position of the epitaxial layer and forming a second conductive type masking region outside the base region, the following steps are also included: A middle doped region of the first conductivity type is formed in the epitaxial layer, wherein the doping concentration of the middle doped region is greater than the doping concentration of the epitaxial layer, wherein the base region is located in the middle doped region, and the trench also extends into the middle doped region in a vertical direction.
5. The method for manufacturing a SiC power MOS structure according to any one of claims 1 to 4, wherein: The first conductivity type is N type, and the second conductivity type is P type; or the first conductivity type is P type, and the second conductivity type is N type.
6. The method for manufacturing a SiC power MOS structure according to claims 1-5, wherein: The source electrode is also located above the shielding region and is electrically connected to the shielding region.
7. The method for manufacturing a SiC power MOS structure according to claims 1-6, wherein: The method further comprises: A drain electrode is formed on the lower surface of the substrate.
8. A SiC power MOS structure, comprising: A first conductive type substrate, a first conductive type epitaxial layer is disposed on the substrate, wherein the doping concentration of the substrate is greater than the doping concentration of the epitaxial layer; A second conductive type base region, located in the epitaxial layer; A second conductive type shielding region, located outside the base region, wherein the doping concentration of the shielding region is greater than the doping concentration of the base region, and the depth of the shielding region is greater than the depth of the base region; A first conductive type source region, located in the base region; A trench, located in the epitaxial layer, the trench vertically penetrating the source region and the base region; A shielding gate structure is located in the trench, the shielding gate structure comprises a gate oxide layer, a shielding gate and a control gate, wherein the gate oxide layer comprises a bottom oxide layer and a sidewall oxide layer, the bottom oxide layer is located at the bottom of the trench, the sidewall oxide layer is located above the bottom oxide layer and at the sidewall of the trench, the shielding gate is located in the bottom oxide layer, and the control gate is located on the inner side of the sidewall oxide layer; A source electrode, located on the upper surface of the epitaxial layer, the source electrode being electrically connected to the source region; A gate electrode is located on the upper surface of the epitaxial layer, and the gate electrode is electrically connected to the control gate.
9. The SiC power MOS structure according to claim 8, wherein: The shielding gate is spaced apart from the control gate by a preset distance, and the shielding gate is electrically connected to the source electrode.
10. The SiC power MOS structure according to claim 8, wherein: An upper surface of the shielding gate is electrically connected to a lower surface of the control gate, and the shielding gate is electrically connected to the gate electrode.
11. The SiC power MOS structure according to any one of claims 8 to 10, wherein: It also includes a first conductive type middle doping region, the middle doping region is located between the masking region and the shielding gate structure, and the doping concentration of the middle doping region is greater than the doping concentration of the epitaxial layer.
12. The SiC power MOS structure according to any one of claims 8 to 11, wherein: The first conductivity type is N type, and the second conductivity type is P type.
13. The SiC power MOS structure according to any one of claims 8 to 11, wherein: The first conductivity type is P type, and the second conductivity type is N type.
14. The SiC power MOS structure according to any one of claims 8 to 13, wherein: The doping concentration of the middle doping region is lower than the doping concentration of the substrate.
15. The SiC power MOS structure according to any one of claims 8 to 14, wherein: The depth of the masking region is greater than the depth of the control gate.
Citation Information
Patent Citations
Low-on-resistance double-trench silicon carbide IGBT device with floating region and manufacturing method thereof
CN107731893A
Silicon carbide semiconductor device and preparation method thereof
CN113972261A
Double-groove silicon carbide MOSFET structure and manufacturing method
CN114005871A
Shield gate MOSFET device and manufacturing method thereof
CN114823343A
Insulated gate semiconductor device and method of manufacturing same
US20190288104A1
Cited By
Semiconductor structure and preparation method thereof
CN120529632A