Can container and manufacturing method for can container
The can container manufacturing method addresses lubricant-related issues by controlling lubricant amounts and incorporating resin film lamination, resulting in improved printing quality and hygiene through controlled lubricant application and removal processes.
Patent Information
- Application Number
- PCT/JP2024/009352
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-28
- Filing Date
- 2024-03-11
- Publication Date
- 2024-10-31
AI Technical Summary
Existing can container manufacturing processes face challenges in preventing defects in printing and maintaining hygiene due to excessive lubricant amounts in the reduced diameter portion, which can lead to ink repellency and insertion failures during shrink film application.
A method involving controlled lubricant application and removal steps, ensuring the lubricant amount in the reduced diameter portion is 2 mg/can or less, combined with a manufacturing process that includes molding, lubrication, diameter reduction, and ink printing, with optional resin film lamination and removal processes to enhance lubricity and prevent ink repellency.
The method effectively reduces defects in printing and improves hygiene by maintaining the optimal lubricant amount, ensuring proper ink printing and shrink film integration, while reducing resource usage and operational complexity.
Smart Images

Figure JP2024009352_31102024_PF_FP_ABST
Abstract
Description
Can container and method for manufacturing can container
[0001] The present invention relates to a can container and a method for manufacturing a can container.
[0002] It is known that a protective layer is formed on the surface of a can body to protect the can body when the can container, such as a beverage can, is reduced in diameter. For example, Patent Document 1 states, "A base coater (BC) and an over burnisher (OV) are provided before a necker flanger (SDN), and an inside spray (INS) is also provided. As a result, in this embodiment, neck treatment is performed after protective layers are formed on the outer and inner surfaces of the can body, making the can body less susceptible to scratches (paragraph 0025)." Furthermore, Patent Document 2 describes the lamination technique as follows: "A method for manufacturing an organic resin-coated metal sheet, in which a heated and molten organic resin is extruded from a T-die in the form of a film directly onto a continuously supplied long strip-shaped metal sheet, and the two are sandwiched and pressure-bonded between a pair of laminating rolls, wherein the laminating roll is opened when the seam of the metal sheet (hereinafter referred to as the "stitcher") passes through the laminating roll section, and the metal sheet is sandwiched and pressure-bonded with a pair of auxiliary laminating rolls (hereinafter referred to as the "auxiliary rolls") instead of the laminating roll, and after passing through the stitcher, the auxiliary roll is opened, and the metal sheet is sandwiched and pressure-bonded with the laminating rolls. (Claim 1)" [Prior Art Documents] [Patent Documents] [Patent Document 1] JP 2019-025521 A [Patent Document 2] JP 2004-25640 A General disclosure
[0003] In a first aspect of the present invention, there is provided a can container having a necked portion and a can body, wherein the amount of lubricant present in the necked portion may be 2 mg / can or less.
[0004] In the above, the can container may have a layer structure including a cylindrical can body and an ink-printed layer formed on the outer surface of the can body, and the amount of lubricant present on the outer surface side of the can body at the reduced diameter portion may be 2 mg / can or less.
[0005] In the above, the ink-printed layer may be a layer formed directly on the can body and then cured.
[0006] In the above, the ink-printed layer may be a shrink film that further covers the can body from the outside and has an ink image printed on it.
[0007] In the above, the can container may have a layer structure including a cylindrical can body and a resin film layer covering at least the outer surface of the can body, and the amount of lubricant present on the outer surface of the resin film layer in the reduced diameter portion may be 2 mg / can or less.
[0008] In the above-mentioned can container, an ink-printed layer may be formed on the outer surface of the resin film layer, and the amount of lubricant present on the outer surface side of the resin film layer in the reduced diameter portion may be 2 mg / can or less.
[0009] In the above, the ink-printed layer may be a layer formed directly on the resin film layer and made by curing the ink.
[0010] In the above, the ink-printed layer may be a shrink film that further covers the resin film layer from the outside and has an ink image printed on it.
[0011] In the above, the can container may be a container filled with a beverage or food for consumption.
[0012] In a second aspect of the present invention, there is provided a method for manufacturing a can container, comprising a molding step, a lubricating step, a diameter reduction step, and a printed layer forming step. In the molding step, a cylindrical can body may be formed from a sheet material having a metal sheet and a resin film layer covering at least one side of the metal sheet, or from a sheet material having a metal sheet. In the lubricating step, a lubricant may be applied to the formed can body. In the diameter reduction step, the diameter of a portion of the can body may be reduced to form a reduced diameter portion. In the printed layer forming step, an ink printed layer may be formed on the outer peripheral surface of the can body.
[0013] In the above, the forming step may be a step of forming a can body from a sheet material having a metal sheet, a resin film, and a lubricating layer formed on one side of the resin film.
[0014] In the above, the forming step may be a step of forming a can body from a sheet material having a metal sheet and a lubricating layer formed on one or both sides of the metal sheet.
[0015] In the above, the method for manufacturing a can container may further include a removing step of removing at least a part of the lubricating layer between the forming step and the lubricating step.
[0016] In a third aspect of the present invention, there is provided a method for manufacturing a can container, comprising a molding step, a diameter reduction step, and a printed layer forming step. In the molding step, a cylindrical can body may be formed from a sheet material having a metal sheet, a resin film covering at least one side of the metal sheet, and a lubricating layer formed on one side of the resin film, or a sheet material consisting of a metal sheet and a lubricating layer formed on one or both sides of the metal sheet. In the diameter reduction step, a reduced diameter portion may be formed by reducing the diameter of a portion of the formed can body without applying a lubricant to the formed can body. In the printed layer forming step, an ink printed layer may be formed on the outer circumferential surface of the can body.
[0017] In the removing step, the lubricant applied in the lubricating step or at least a portion of the lubricating layer may be removed between the diameter reducing step and the print layer forming step.
[0018] In a fourth aspect of the present invention, there is provided a method for manufacturing a can container, comprising a lubrication step, a diameter reduction step, and a storage step. In the lubrication step, a lubricant may be applied to a can body consisting of a cylindrical can body and a resin film layer covering at least the outer surface of the can body, or to a can body consisting of a cylindrical can body. In the diameter reduction step, a diameter of a portion of the can body may be reduced to form a reduced diameter portion. The can body may be stored in a plain state without any printing.
[0019] In a fifth aspect of the present invention, there is provided a method for manufacturing a can container, comprising a forming step, a diameter reduction step, and a storage step. In the forming step, a cylindrical can body may be formed from a sheet material having a metal sheet, a resin film covering at least one side of the metal sheet, and a lubricating layer formed on one side of the resin film. In the diameter reduction step, a reduced diameter portion may be formed by reducing the diameter of a portion of the can body without applying a lubricant to the can body. In the storage step, the can body may be stored in a plain state without being printed.
[0020] In the above, the manufacturing method may further include a removing step of removing a portion of the lubricant from the can body between the diameter reducing step and the storing step.
[0021] In the above, the storage step may be carried out in a light-shielding state so that the can body is not irradiated with ultraviolet light.
[0022] In the above, the storing step may include storing the can body in a light-shielded state for one month or more.
[0023] In the above, the printing layer forming step may include printing on the outer surface of the can body by one or more of inkjet printing and printing with a printing plate.
[0024] In the above, the print layer forming step may include covering the outer surface of the can body with a shrink film on which an ink image is printed.
[0025] In the above, the removal step may use thermal energy (heat set oven), plasma treatment, or flame treatment.
[0026] In the above, the print layer forming step may include covering the outer surface of the can body with an adhesive label (tack label) on which an ink image is printed.
[0027] The above summary of the invention does not list all of the features of the present invention, and subcombinations of these features may also be inventions.
[0028] 4 shows an example of an overall view of a can container 10 in this embodiment. FIG. 4 shows an example of a cross section of a can container 10 in this embodiment. FIG. 4 shows another example of a cross section of a can container 10 in this embodiment. FIG. 4 shows an example of a flow of a method for manufacturing a can container 10 in this embodiment. FIG. 4 shows an example of a subflow (wet molding) of S100 in FIG. 4 shows another example of a subflow (dry molding) of S100 in FIG. 4 shows another example of a flow of a method for manufacturing a can container 10 in this embodiment. FIG. 4 shows another example of a flow of a method for manufacturing a can container 10 in this embodiment. FIG. 4 shows another example of a flow of a method for manufacturing a can container 10 in this embodiment. FIG. 4 shows another example of a flow of a method for manufacturing a can container 10 in this embodiment.
[0029] The present invention will be described below through embodiments of the invention, but the following embodiments do not limit the scope of the invention as claimed. Furthermore, not all of the combinations of features described in the embodiments are necessarily essential to the solution of the invention.
[0030] 1 shows an example of an overall view of a can container 10 according to this embodiment. The can container 10 according to the present invention can prevent defects in the can body and / or printing formed on the can body surface and improve hygiene by limiting the amount of lubricant present in the reduced diameter portion to 2 mg / can or less.
[0031] The can container 10 may be used for consumption by being filled with beverages or food. The can container 10 may also be filled with contents other than food and beverages, such as medicines, chemicals, gases, liquids and / or solids.
[0032] The can container 10 has a reduced diameter portion 20 provided on one end side, a bottom portion 30 provided on the other end side, and a can body portion 40.
[0033] The reduced diameter portion 20 is a portion where one end of the can container 10 is reduced in diameter. The reduced diameter portion 20 may be provided at the opening of the can container 10. The reduced diameter portion 20 may be formed so that the outer diameter gradually decreases as it approaches the one end of the can container 10.
[0034] The reduced diameter portion 20 may be formed by necking the end of the can container 10 before the diameter is reduced. The reduced diameter portion 20 may have a flange formed simultaneously with the necking. A can lid can be attached by the formed flange. By providing the reduced diameter portion 20 on the can container 10, the amount of can lids used to attach to the opening of the can container 10 can be reduced. The can container 10 may have a can lid attached.
[0035] The bottom 30 is a bottom formed at the other end of the can container 10. The bottom 30 allows the can container 10 to hold a filled product such as a beverage. The bottom 30 may be formed so that the outer diameter gradually decreases toward the other end of the can container 10. The bottom surface of the bottom 30 may be formed in a dome shape that is convex upward.
[0036] The can body 40 is the region between the reduced diameter portion 20 and the bottom portion 30 of the can container 10. The can body 40 may have a cylindrical shape with a substantially constant outer diameter in the longitudinal direction (the vertical direction in FIG. 1 ) of the can container 10. The can body 40 has a larger outer peripheral surface area than the reduced diameter portion 20 and the bottom portion 30, and has a substantially constant outer diameter, making it a region suitable for printing on the surface.
[0037] The can body 40 may have a uniform, flat surface overall, or alternatively, the can body 40 may be formed with irregularities such as embossing, or with bent portions, etc.
[0038] As described in Fig. 1 , the can container 10 may include three regions: the narrowed diameter portion 20, the bottom portion 30, and the can body portion 40. Alternatively, the can container 10 may not have the narrowed diameter portion 20. For example, if the can container 10 is a straight can or a cup, it may not have the narrowed diameter portion 20.
[0039] 2 shows an example of a cross section of a can container 10 in this embodiment. The can container 10 includes a can body 110 and an ink-printed layer 120. The can body 110 side (left side of the figure) is the inside of the can container 10, and the ink-printed layer 120 side (right side of the figure) is the outside of the can container 10.
[0040] The can body 110 has a cylindrical shape and forms the structure of the can container 10. The can body 110 may be a seamless can such as a two-piece can or a welded can such as a three-piece can. The can body 110 may also be a cup without a metal lid. The can body 110 may be formed of a single metal that can be used for beverage cans and food cans. For example, the can body 110 may be formed of aluminum, steel, or the like.
[0041] The ink printed layer 120 is a layer of ink images that express symbols, letters, designs, and / or pictures. The ink printed layer 120 is formed on the outer peripheral surface of the can body 110. The ink printed layer 120 is formed on at least one of the reduced diameter portion 20 and the can barrel portion 40. Alternatively, the ink printed layer 120 may not be present.
[0042] The ink-printed layer 120 may be a layer formed directly on the can body 110 and formed by curing the ink. The ink-printed layer 120 may include a coloring material such as a pigment or a dye, a binder resin, and other solid components of an ink composition. The ink composition may be, but is not limited to, a water-based ink, a solvent ink, an ultraviolet-curable ink, or an electron beam-curable ink.
[0043] Alternatively, the ink-printed layer 120 may be a shrink film on which an ink image is printed, which further covers the outside of the can body 110. For example, the ink-printed layer 120 may be formed by printing an ink composition on one or both sides of a shrink film and then attaching the film to the can body 110.
[0044] The ink print layer 120 may be a monochrome image containing a single color or a color image containing multiple colors. The ink print layer 120 may also be a mixture of monochrome and color images in different regions.
[0045] A lubricating layer 117, which is a layer of lubricant, may be provided between the can body 110 and the ink-printed layer 120. The lubricating layer 117 may be provided at least in the narrowed diameter portion 20. The lubricating layer 117 may further be provided on the bottom portion 30 and / or the can body portion 40. The presence of the lubricating layer 117 at least in the narrowed diameter portion 20 protects the can body 110 from damage during narrowing.
[0046] The amount of lubricant present in the reduced diameter portion 20 is 2 mg / can or less. In particular, the amount of lubricant present on the outer surface of the can body 110 in the reduced diameter portion 20 may be 2 mg / can or less. "mg / can" indicates the amount of lubricant in the lubricating layer 117 present in one can container 10. By setting the amount of lubricant to 2 mg / can or less, it is possible to prevent ink from being repelled when forming the ink-printed layer 120. By setting the amount of lubricant to 2 mg / can or less in places such as the reduced diameter portion 20 that may come into direct contact with a person's mouth, it is possible to improve the hygienic properties of the can container 10.
[0047] Furthermore, when the ink-printed layer 120 includes a shrink film, if the amount of lubricant is too large (for example, if the amount of lubricant in the reduced diameter portion 20 exceeds 2 mg / can), insertion failure is likely to occur when the shrink film is inserted into the can body 110. From this perspective, too, it is desirable that the amount of lubricant present in the reduced diameter portion 20 be 2 mg / can or less.
[0048] The amount of lubricant may be 0.01 mg / can or more. In particular, the amount of lubricant present on the outer surface of the can body 110 in the reduced diameter portion 20 may be 0.01 mg / can or more. By setting the amount of lubricant to 0.01 mg or more, lubrication during reduction can be maintained without causing ink repellency or compromising hygiene. Furthermore, by including a certain amount of lubricant, when the ink-printed layer 20 is formed using a shrink film, the extrapolation property of the shrink film can be improved, thereby reducing defects in the can container 10.
[0049] The lubricant may be, for example, one or a combination of one or more selected from waxes of animal or vegetable origin, petroleum wax, petrolatum, solid paraffin, liquid paraffin, lanolin, polyethylene glycol, edible oil, food-grade lubricating oil, mineral oil, food-grade grease, and varnish.
[0050] In particular, when the ink-printed layer 120 includes a shrink film, the lubricant is preferably a solid material, such as wax, petroleum wax, or solid paraffin.
[0051] In this embodiment, the entire or a portion of the can container 10 (e.g., the reduced diameter portion 20) may be immersed in an organic solvent (e.g., a lipophilic solvent such as an alkane or a ketone) to extract the lubricant into the organic solvent, and the lubricant dissolved in the organic solvent may be dried and the measured dry weight may be used as the amount of lubricant. While this method may result in the dissolution of components other than the lubricant from the can container 10, since the lubricant is the main extract, the amount determined by this method may be used as the amount of lubricant. On the other hand, if the extracted components and their content ratios can be identified by chemical analysis such as gas chromatography-mass spectrometry, the total weight of the lubricant components may be used as the amount of lubricant.
[0052] As an example, the amount of lubricant may be measured by the following method. 10 mL of an acetone-hexane mixture (1:9) is placed in a 300 mL glass beaker, and the narrowed portion and the flange at the tip of the narrowed portion of the can container held inverted are immersed therein to extract the lubricant, obtaining an extract. The extract obtained from five can containers is transferred to an eggplant flask and evaporated to dryness under reduced pressure, and then redissolved in 1 mL of an acetone-hexane mixture (1:9). This is transferred to an aluminum dish and stored in a constant temperature dryer at 75°C for 30 minutes. After cooling to room temperature, the weight is measured using an electronic balance. The amount of lubricant present in the narrowed portion 20 per can can be measured by dividing the weight of the dried product by 5.
[0053] In this embodiment, the ink printed layer 120 is formed on both the reduced diameter portion 20 and the can body portion 40. Alternatively, the ink printed layer 120 does not have to be formed on the reduced diameter portion 20.
[0054] The ink printed layer 120 may not be formed on the bottom portion 30. Alternatively, the ink printed layer 120 may be formed on the bottom portion 30.
[0055] The can container 10 may have other layers not shown. For example, an inner surface protective layer may be formed on the inside of the can body 110 (left side of the figure), and / or an outer surface protective layer such as a base coat or varnish may be formed between the can body 110 and the lubricating layer 117. Furthermore, for example, a protective layer may be further formed on the outer surface of the ink-printed layer 120.
[0056] 3 shows a modified cross section of the can container 10 according to this embodiment. In this example, the can body 110 is not made of metal alone, but has a layered structure including a can body 112 as a core, and resin film layers 114 and 116 that cover the inner and / or outer surfaces of the can body 112. Furthermore, for example, a protective layer may be further formed on the outer surface of the ink-printed layer 120.
[0057] The can body 112 may be a metal layer such as aluminum or steel that can be used for beverage cans and food cans. The resin film layers 114 and 116 may be polyethylene terephthalate (PET) films. For example, the can body 110 may be formed by laminating PET films onto the inner and outer surfaces of a metal plate.
[0058] By using the can body 110 coated with the resin film in this manner, it is possible to prevent the can body 110 from being corroded by the contents. In addition, it is possible to reduce the amount of lubricant and water used when forming the can body 110.
[0059] In this embodiment, the lubricating layer 117 and the ink-printed layer 120 may have the same configuration as previously described unless otherwise specified. For example, the ink-printed layer 120 may be a layer formed directly on the resin film layer 116 and formed by hardening the ink. Furthermore, for example, the ink-printed layer 120 may be a shrink film that further covers the resin film layer 116 from the outside and has an ink image printed on it. For example, the amount of lubricant in the lubricating layer 117 present on the outer surface of the resin film layer 116 in the reduced diameter portion 20 may be 2 mg / can or less. Alternatively, the ink-printed layer 120 may not be present.
[0060] Fig. 4 shows an example of a flow chart of a method for manufacturing the can container 10 according to the present embodiment. The can container 10 according to the present embodiment can be manufactured by the processes of S100 to S800 shown in Fig. 4. For convenience of explanation, the processes of S100 to S800 will be explained in order, but the processes may be interchanged and / or some of the processes may be omitted without departing from the spirit of the present invention.
[0061] First, in S100, the bottom 30 and can body 40 of the can container 10 are formed, and a molding process is performed to form a cylindrical can body 110. There are two types of molding: wet molding, which uses a coolant, a lubricant for cooling, and dry molding, which does not use a coolant.
[0062] In the forming process, a cylindrical can body may be formed from a sheet material. For example, in the case of wet forming, the sheet material may include a metal sheet. Here, a lubricating layer may be formed on one or both sides of the metal sheet. In this case, the forming process may be a process of forming the can body 110 from the metal sheet and the sheet material having the lubricating layer formed on one or both sides of the metal sheet.
[0063] For example, in the case of dry molding, the sheet material may have a metal sheet and a resin film layer covering at least one side of the metal sheet. Here, a lubricating layer may be formed on one side of the resin film layer. In this case, the molding process may be a process of molding the can body 110 from the sheet material having the metal sheet, the resin film layer, and the lubricating layer formed on one side of the resin film layer.
[0064] Fig. 5 shows an example of a subflow (wet molding) of S100 in Fig. 4. S100 (wet molding) may be performed by executing S105 to S140 in Fig. 5.
[0065] In step S105, a metal sheet, which is a metal plate material wound into a coil, is uncoiled and stretched (uncoiler). The metal sheet may be, but is not limited to, an aluminum plate or a steel plate. After forming, the metal sheet becomes a can body 110.
[0066] In S110, a lubricant is applied to the rolled metal sheet (lubricator). Known lubricants may be used. Lubricants include solids such as wax and liquids such as oils and fats. For example, the lubricant may be one or a combination of one or more selected from the group consisting of animal and vegetable wax, petroleum wax, petrolatum, solid paraffin, liquid paraffin, lanolin, polyethylene glycol, edible oil, food-grade lubricating oil, mineral oil, food-grade grease, and emulsions thereof.
[0067] In particular, the lubricant in S110 preferably contains wax. In addition to wax, the lubricant may further contain a liquid oil or grease that functions as a coolant. This results in a sheet material having a lubricating layer of lubricant formed on one or both sides of the metal sheet.
[0068] Instead of forming a lubricating layer on the metal sheet after uncoiling, a metal sheet with a lubricating layer preformed on one or both sides may be wound into a coil and uncoiled. A lubricant may also be applied to the metal sheet with a lubricating layer preformed on it.
[0069] In S120, a process of punching the sheet material into a cup shape (cupping press) is carried out.
[0070] In S130, the cup-shaped member is drawn and ironed to thin and stretch the sides of the cup. A dome-shaped bottom is also formed at the same time, thereby forming the can body 40 and bottom 30 (body maker). In S130, a lubricant (coolant) similar to that described in S110 may be additionally used for cooling.
[0071] In S140, unnecessary portions of the formed member are removed (trimmer), thereby forming the can body 110.
[0072] Fig. 6 shows an example of a subflow (dry molding) of S100 in Fig. 4. S100 (dry molding) may be performed by executing S105 to S140 in Fig. 6.
[0073] The process of S105 (uncoiler) may be the same as S105 in FIG.
[0074] In S115, a resin film is laminated on one or both sides of the metal sheet. This results in a sheet material having a metal sheet and a resin film layer. The lamination can be performed by a known method, such as the method described in JP 2004-25640 A. After molding, the metal sheet becomes the can body 112, and the resin film becomes the resin film layer 114 and the resin film layer 116.
[0075] The resin film may be made of a thermoplastic resin such as polyethylene terephthalate (PET). Instead of the thermoplastic resin, a thermosetting resin such as a thermosetting acrylic resin, a thermosetting epoxy resin, a thermosetting polyurethane resin, or a thermosetting polyester resin may be used. By using the resin film, the same effect as the lubricant used in steps S110 and S130 of FIG. 5 can be achieved without using a lubricant.
[0076] The thickness of the resin film may be 0.5 μm or more and 30 μm or less. If the thickness of the resin film is less than 0.5 μm, the surface of the resin film will be less slippery, which may cause scratches on the can body 110 or metal powder to adhere to the tool when forming the reduced diameter portion 20. If the thickness of the resin film exceeds 30 μm, there is a risk of poor resin adhesion after the reduced diameter processing and the flanging processing.
[0077] Before laminating the resin film, a primer composition may be applied to the laminating surface of the metal sheet. For example, a primer composition containing a polyester resin, a curing agent, and / or a solvent may be roll-coated onto the metal sheet, followed by baking to form a primer layer, and then the resin film may be laminated onto the primer layer. The curing agent may be, for example, a resol-type phenolic resin derived from m-cresol.
[0078] The primer composition may further contain a coloring material such as a pigment and / or a food coloring, thereby enhancing the decorative properties of the can container 10 even in a portion thereof where the ink-printed layer 120 is not provided (e.g., the bottom 30, etc.).
[0079] After lamination, a lubricant may be applied to one side of the resin sheet to form a lubricating layer, thereby obtaining a sheet material having a metal sheet, a resin film, and a lubricating layer formed on one side of the resin film.
[0080] Instead of steps S105 to S115, a coiled member may be unwound in advance, which is made of a metal sheet, a resin film, and, if necessary, a sheet material having a lubricating layer formed on one or both sides of the resin film. For example, after lamination in step S115, the sheet material may be wound on a coiler to produce a coiled sheet material, which may then be unwound again as necessary for subsequent processing. Alternatively, for example, a coiled sheet material may be obtained, unwound, and then subjected to subsequent processing.
[0081] The processes in S120 to S140 may be the same as those described in Fig. 5. In this way, the can body 110 is formed.
[0082] In S200, a removal step is performed to remove at least a portion of the lubricating layer of the can body 110. The removal step may use a water washing treatment, a heat treatment (i.e., thermal energy), a plasma treatment, or a flame treatment.
[0083] In particular, when the sheet material includes a resin film layer, the heat treatment can also simultaneously remove distortion of the resin film caused by molding. For example, the heat treatment may involve heating the molded member at 180 to 220°C for 20 to 90 seconds. The heat treatment may be performed using a hot air heating device, an induction heating (IH) device, and / or an infrared (IR) heating device.
[0084] The water rinse may be with cold or hot water, and the water temperature may be lowered if more lubricant is required, or raised if less lubricant is required.
[0085] The plasma treatment may be atmospheric pressure plasma treatment. The type of gas used in the atmospheric pressure plasma treatment may be at least one of nitrogen, hydrogen, helium, argon, and oxygen. The gas flow rate may be 1 to 200 L per minute. The treatment speed of the atmospheric pressure plasma treatment may be 1 to 100 m per minute. The plasma irradiation time may be 0.5 to 10 seconds.
[0086] In atmospheric pressure plasma treatment, the minimum distance between the can body 110 and the plasma electrode may be 50 mm or less. Preferably, the minimum distance between the can body 110 and the plasma electrode may be 2 mm or less. One or more electrodes may be used. Using multiple electrodes can increase treatment capacity and shorten treatment time.
[0087] Flame treatment is a treatment in which a reducing flame obtained by mixing and burning a combustible gas such as methane or propane with air or oxygen is applied to the object, and can be performed by a known method. For example, the flame treatment may be performed by using a burner with a heat power of 35 to 40 μA, setting the distance between the tip of the burner and the container surface at about 25 to 75 mm, uniformly heat-treating the container surface for 0.5 to 2.0 seconds, and then allowing it to cool to room temperature.
[0088] In the removing step, a plurality of treatments may be combined. For example, in the removing step, water washing and one or more of a heat treatment, a plasma treatment, and a flame treatment may be performed in sequence.
[0089] If the sheet material does not include either a resin film or a lubricating layer, the removal step of S200 may be omitted.
[0090] In S300, a lubrication step is performed in which a lubricant is applied to the molded can body 110. The lubricant may be the same as that used in S110. A particularly highly volatile solvent may be used as the lubricant. For example, hexane may be used. This forms a lubricating layer 117.
[0091] After S300 and before S400, an inner surface protective layer may be formed on the inner circumferential surface of the can body 110. For example, the inner surface protective layer may be formed by applying paint to the inner circumferential surface and baking the paint. This prevents scratches on the inner circumferential surface. In the examples of the embodiments shown in FIG. 7 and subsequent figures, the inner surface protective layer may be formed before the diameter reduction step of S400.
[0092] In S400, a diameter reducing step is performed in which the formed can body 110 is necked to reduce the diameter of a portion of the can body 110 and form a reduced diameter portion 20. The necking may be performed using a known die-necking tool. Simultaneously with or after the necking, the can body 110 may be flanged to form a flange for attaching a can lid.
[0093] A process for removing the lubricating layer may be performed after necking. As an example, at least a portion of the lubricating layer may be removed by washing with water or heating, as in S200. A hot air heating device, an induction heating (IH) device, and / or an infrared (IR) heating device may be used as the heating method. In particular, when the printing layer forming step S500 is performed after S200, it is preferable to remove the lubricating layer to prevent ink repellency, etc.
[0094] In S500, a printing layer forming process is performed to form an ink printing layer 120 on the outer peripheral surface of the can body 110. The ink printing layer 120 may be formed by printing the outer surface of the can body 110 using one or more of inkjet printing and / or printing using a printing plate.
[0095] Inkjet printing may be a method in which an ink composition is ejected directly onto the can body 110 from an inkjet head (IJH) of an inkjet printing device, or an offset method in which an ink composition ejected from the IJH onto a blanket (i.e., a transfer plate) is transferred to the can body 110.
[0096] Printing using a printing plate may be printing using a plate-based printing device. For example, printing using a printing plate may be a method of transferring the ink composition to the can body 110 using a plate such as a relief plate. The ink composition may be transferred directly to the can body 110 using the relief plate, or an offset method may be used in which the ink composition transferred to a blanket (i.e., a transfer plate) is further transferred to the can body 110.
[0097] The ink composition may be a water-based ink, a solvent ink, an ultraviolet-curable ink, or an electron beam-curable ink. The ink composition may contain a colorant selected from pigments, dyes, etc., a resin binder, a monomer / oligomer, an initiator, a solvent, and / or additives such as a dispersant, as needed.
[0098] After printing, the ink composition may be subjected to a drying / curing treatment, such as air drying, heat treatment, ultraviolet irradiation, electron beam irradiation, or a combination thereof, depending on the type of ink composition.
[0099] In particular, by using ultraviolet curable ink or electron beam curable ink, it is possible to reduce the number of heating processes, reduce the number of opportunities for applying a thermal load to the can body 110, and shorten the cooling time. As an example, inkjet printing may be performed using ultraviolet curable ink or electron beam curable ink.
[0100] In addition to or instead of printing ink on the can body 110, the print layer forming step may be performed by covering the outer surface of the can body 110 with a shrink film on which an ink image is printed. For example, an ink image may be printed on a shrink film in the same manner as above, and the shrink film may be wrapped around the can body 110 and shrunk, thereby forming the shrink film on which the image is printed as the ink print layer 120. A tack label may be used instead of a shrink film and attached to the outer surface of the can body 110. The tack label may be made of plastic or paper.
[0101] When using a pre-printed shrink label or tack label, there is an advantage in that the problem of the printing being repelled by the lubricant on the surface of the can body 110 does not occur. Furthermore, by including 0.01 mg / can or more of lubricant in the entire can body 110 or in the reduced diameter portion 20, the extrapolation properties of the shrink film can be improved.
[0102] Known materials can be used for the shrink film, for example, a material selected from polypropylene, polyethylene, polystyrene, polyvinyl chloride, polyvinylidene chloride, polyolefin, polyethylene terephthalate, and the like.
[0103] The ink-printed layer 120 may be formed on the entire or a portion of the outer peripheral surface of the can body 110. For example, the ink-printed layer 120 may be formed on the entire or only a portion of the can body 40. For example, the ink-printed layer 120 may be formed on the entire or only a portion of the reduced diameter portion 20 and the entire or only a portion of the can body 40.
[0104] The ink printing layer 120 may be formed in parallel. For example, the process of S500 may be performed simultaneously by a plurality of inkjet printing devices and / or a plurality of plate-based printing devices. This will be described in detail later.
[0105] The ink-printed layer 120 may be formed in multiple steps. For example, a common design, common pattern, and / or common characters may be formed in advance by printing with a printing plate or inkjet printing, and then individual designs, individual patterns, and / or individual characters that differ for each product or lot may be formed on demand by inkjet printing later. When the ink-printed layer 120 is not formed, such as when manufacturing plain or white cans to be later printed, the process of S500 may be omitted.
[0106] After S500 and before S600, a protective layer may be further formed on the outer surface of the ink printed layer 120. For example, by forming a layer containing a UV curable resin or the like as a protective layer on the outer surface of the ink printed layer 120, the ink printed layer 120 can be protected.
[0107] In S600, the can container 10 on which each layer has been formed is inspected. The outer or inner surface of the can container 10 may be inspected for dents, holes, and / or scratches. The printed image of the ink-printed layer 120 may be inspected for chips, misalignments, and / or unclear areas.
[0108] In S700, the contents are filled into the can container 10. For example, the can container 10 may be filled with beverages, food, medicines, chemical products, gases, liquids and / or solids.
[0109] In S800, a can lid is attached to the can container 10. For example, the can lid may be attached by placing the lid on the flange portion of the can container 10 and tightening it using a lid tightening machine.
[0110] 4 to 6 show the basic process flow for manufacturing the can container 10, but as will be described later, the order of the processes may be changed or parallelized. This can improve the efficiency of the can manufacturing process. Furthermore, if the can container 10 is a cup, the processes of S700 to S800 may be omitted.
[0111] S100 to S800 may be performed by a single entity / location, or by multiple different entities / locations. For example, S100 to S600 may be performed at a can manufacturing plant, and S700 and subsequent steps may be performed at a filling plant (also called a packer or bottler).
[0112] Alternatively, for example, steps S100 to S400 may be performed in a can manufacturing factory, and steps S500 and after may be performed in a filling factory. This allows a printing device to be installed in the filling factory, and the number of can containers 10 bearing any desired image required for filling cans to be quickly manufactured and shipped.
[0113] 7 shows another example of the flow of the method for manufacturing the can container 10 according to this embodiment. In this embodiment, the removal step S200 is performed between the diameter reduction step S400 and the print layer formation step S500. In other words, S200 is performed after S400.
[0114] In this embodiment, the removal step S200 removes the lubricant applied in S110, S115, and S300 and / or a portion of the formed lubricant layer. This significantly reduces the amount of lubricant remaining on the can container 10. The removal step may completely remove the lubricant layer 117, or may leave a portion of it. For example, the amount of lubricant present in the reduced diameter portion 20 (particularly on the outer surface of the can body 110 in the reduced diameter portion 20) may be 2 mg / can or less. This prevents printing from being repelled when the printing layer formation step S500 is performed.
[0115] Furthermore, the removal step may be carried out so that the amount of lubricant present in the reduced diameter portion 20 (particularly on the outer surface side of the can body 110 in the reduced diameter portion 20) is 0.01 mg / can or more. This allows the extrapolation property of the shrink film to be improved when the ink printed layer 120 is formed using a shrink film.
[0116] Preferably, the removal step may include water washing and / or heat treatment. Heat treatment can simultaneously remove the lubricating layer and remove distortion from the resin film. For example, the heat treatment involves heating the molded member at 180 to 220°C for 20 to 90 seconds, thereby reducing the amount of lubricant to 0.01 mg or more and 2 mg or less per can.
[0117] 8 shows another example of the flow of the method for manufacturing the can container 10 according to this embodiment. In this embodiment, the removal step S200 is performed between the molding step S100 and the lubrication step S300, and between the diameter reduction step S400 and the print layer formation step S500. In other words, the lubrication step is performed twice.
[0118] In this embodiment, the first removal step (S200A) removes the lubricant applied and / or a portion of the lubricant layer formed in S110 and S115. The second removal step (S200B) removes the lubricant applied and / or a portion of the lubricant layer formed in S300. This further significantly reduces the amount of lubricant remaining on the can container 10. The removal step may completely remove the lubricant layer 117, or may leave a portion of it remaining. For example, the amount of lubricant present in the reduced diameter portion 20 (particularly on the outer surface of the can body 110 in the reduced diameter portion 20) may be 2 mg / can or less. This prevents printing from being repelled when the printing layer formation step S500 is performed. If the amount of lubricant applied and / or the lubricant layer formed in S300 is sufficiently small, the second removal step S200 may not be performed.
[0119] This allows for a further significant reduction in the amount of lubricant remaining on the can container 10. The lubricant layer 117 may be completely removed in the removal process, or a portion may be left behind. For example, the amount of lubricant present in the reduced diameter portion 20 (particularly on the outer surface of the can body 110 in the reduced diameter portion 20) may be 2 mg / can or less. This prevents printing from being repellent when performing the printing layer formation process S500. If the amount of lubricant applied and / or the lubricant layer formed in S300 is sufficiently small, the second removal process S200 may not be performed.
[0120] In S100, when the process of Figure 5 (wet molding) is performed, it is preferable to perform water washing in the first removal step (S200A) to thoroughly remove the lubricant, and it is desirable to perform frame treatment and / or plasma treatment in the second removal step (S200B), which can be expected to have a surface modification effect on the can body 110.
[0121] In S100, when the process of Figure 6 (dry molding) is performed, it is preferable to perform a heat treatment in the first removal step (S200A) that can also remove distortion from the resin film, and it is desirable to perform a frame treatment and / or plasma treatment in the second removal step (S200B) that can also be expected to have a surface modification effect on the can body 110.
[0122] Other aspects may be the same as those of the embodiment described in Fig. 7. After the removal step of S200B, the printing layer forming step (S500) to the can lid attachment (S800) may be performed as in Fig. 7. Alternatively, the inspection step (S600) and / or the storage step (S900) may be performed as in Figs. 10 and 11 described below.
[0123] 9 shows another example of the flow of the method for manufacturing the can container 10 according to this embodiment. In this embodiment, the lubrication step S300 is not performed, and the removal step S200 is performed after the diameter reduction step S400.
[0124] As a result, a diameter reduction step is performed in which a portion of the can body 110 is reduced in diameter to form reduced diameter portion 20 without applying a lubricant to the formed can body 110 in the lubrication step S300. In this embodiment, a lubricating layer is formed on the sheet material before forming in S110 or S115, or the forming step S100 is performed using a sheet material on which a lubricating layer has been formed in advance on a metal sheet or a resin film.
[0125] The removal step S200 may be performed in the same manner as in the embodiment of Fig. 7. In the embodiment of Fig. 9, the lubrication step S300 is not present, and therefore the removal step may be performed more simply than in Fig. 7. For example, in this embodiment, the application time of the heat treatment may be 20 to 40 seconds, the irradiation time of the plasma treatment may be 0.5 to 5 seconds, and the heating time of the flame treatment may be 0.5 to 1 second.
[0126] According to this embodiment, the forming and diameter-reducing processes are performed using the lubricating layer of sheet material applied for the forming process S100, eliminating the need for a lubrication process. This reduces the resources and time required for the lubrication process, such as lubricant. This reduces the amount of lubricant present in the reduced diameter portion 20 (particularly on the outer surface of the can body 110 in the reduced diameter portion 20) to 2 mg / can or less. If the lubricating layer of the sheet material is sufficiently thin, the removal process S200 may be unnecessary.
[0127] Fig. 10 shows another example of the flow of the method for manufacturing the can container 10 in this embodiment. In this embodiment, the molding step S100, the lubrication step S300, the diameter reduction step S400, and the removal step S200 may be performed in the same manner as in the embodiment of Fig. 7. After S200, the inspection step S600 may be performed without performing the printing layer formation step.
[0128] In this embodiment, the removal step S200 is performed between the diameter reduction step S400 and the storage step S900. The processes of S100 to S600 may be performed in the same manner as described above.
[0129] The storage step S900 may be performed after the inspection step S600. In the storage step, the can body 110 is stored in a plain state without any printing. The storage step may be performed in a light-shielded state to prevent ultraviolet light from irradiating the can body. In particular, it is preferable to store the can body in a light-shielded state for one month or more during the storage step. This protects the ink-printed layer 120 from ultraviolet light and prevents deterioration such as fading. Storing the can body for one month or more can further reduce the amount of lubricant (especially volatile lubricant) present on the surface of the can body 110.
[0130] After the storage step of S900, the can body 110 may be shipped as needed. For example, the can body 110 may be shipped to a filling factory, where one or more of the printing layer formation step of S500, the can container inspection step of S600, the filling step of S700, and the can lid attachment step of S800 may be performed.
[0131] In this embodiment, the removal process can reduce the amount of lubricant present on the surface of the can body 110. For example, the amount of lubricant present in the reduced diameter portion 20 can be reduced to 2 mg / can or less. This can prevent the printing from being repelled when the printing layer formation process S500 is performed later at a filling factory.
[0132] Furthermore, in this embodiment, the removal process can also be expected to have a cleaning effect on the can body 110. Therefore, it is possible to prevent the lubricant from deteriorating or absorbing moisture during the storage process of S900. In particular, when plasma treatment or flame treatment is used in the removal process, a significant effect can be expected.
[0133] The amount of lubricant present in the reduced diameter portion 20 (particularly the outer surface side of the can body 110 in the reduced diameter portion 20) may be 0.01 mg / can or more. This improves the extrapolation property of the shrink film when the ink-printed layer 120 is later formed using the shrink film at a filling factory.
[0134] On the other hand, the removal step of S200 may be omitted. For example, it is desirable to omit the removal step when there is little concern about the printing being repelled, such as when the ink printing layer 120 is later formed using a shrink film at a filling factory.
[0135] Figure 11 shows another example of the flow of the method for manufacturing the can container 10 according to this embodiment. The embodiment of Figure 11 differs from the embodiment of Figure 10 in that it does not include the lubrication step S300 and the removal step S200. In this embodiment, a portion of the can body 110 is subjected to the diameter reduction step without applying a lubricant to the can body 110. In S100 of this embodiment, a lubricating layer is formed on the surface of the sheet material before the coupling press step S120, as described in the embodiment of Figures 4 and 5.
[0136] According to this embodiment, the forming step S100 and the diameter reduction step S400 are performed using a lubricating layer of sheet material applied for the forming step S100, eliminating the need for a lubrication step. This reduces the resources and time required for the lubrication step, such as lubricant. This reduces the amount of lubricant present in the reduced diameter portion 20 (particularly on the outer surface of the can body 110 in the reduced diameter portion 20) to 2 mg or less. A removal step S200 may be added after the diameter reduction step S400.
[0137] According to this embodiment, the storage step S900 protects the ink-printed layer 120 from ultraviolet light and prevents deterioration such as fading. By storing the can body for one month or more, the amount of lubricant (especially volatile lubricant) present on the surface of the can body 110 can be reduced without undergoing a removal step.
[0138] Although the present invention has been described above using the embodiments, the technical scope of the present invention is not limited to the scope described in the above embodiments. It will be apparent to those skilled in the art that various modifications and improvements can be made to the above embodiments. It is clear from the claims that such modifications and improvements can also be included within the technical scope of the present invention.
[0139] It should be noted that the order of execution of each process, such as operations, procedures, steps, and stages, in the can bodies, can containers, and methods shown in the claims, specification, and drawings is not specifically stated as "before," "prior to," etc., and can be realized in any order unless the can bodies or can containers from a previous process are used in a later process. Even if the operational flow in the claims, specification, and drawings is described using "first," "next," etc. for convenience, it does not mean that it is necessary to perform the process in this order.
[0140] REFERENCE SIGNS LIST 10 Can container 20 Reduced diameter portion 30 Bottom portion 40 Can body portion 110 Can body 112 Can main body 114 Resin film layer 116 Resin film layer 117 Lubricating layer 120 Ink printed layer
Claims
1. A can container having a reduced diameter portion and a can body portion, wherein the amount of lubricant present in the reduced diameter portion is 2 mg / can or less.
2. A can container as described in claim 1, having a layer structure including: a cylindrical can body; and an ink-printed layer formed on the outer surface of the can body, and the amount of lubricant present on the outer surface side of the can body at the narrowed portion is 2 mg / can or less.
3. The can container according to claim 2, wherein the ink-printed layer is a layer formed directly on the can body and the ink is cured.
4. The can container according to claim 2, wherein the ink-printed layer further covers the can body from the outside and is a shrink film on which an ink image is printed.
5. A can container as described in claim 1 or 2, having a layer structure including: a cylindrical can body; and a resin film layer covering at least the outer surface of the can body, wherein the amount of lubricant present on the outer surface of the resin film layer in the narrowed portion is 2 mg / can or less.
6. A can container as described in claim 5, further comprising an ink-printed layer formed on the outer surface of the resin film layer, wherein the amount of lubricant present on the outer surface side of the resin film layer in the narrowed portion is 2 mg / can or less.
7. The can container according to claim 6, wherein the ink-printed layer is formed directly on the resin film layer and is a layer in which the ink is cured.
8. The can container according to claim 6, wherein the ink-printed layer further covers the resin film layer from the outside and is a shrink film on which an ink image is printed.
9. A can container according to any one of claims 1 to 8, which is filled with a beverage or food for consumption.
10. A method for manufacturing a can container, comprising: a molding process for molding a cylindrical can body from a sheet material having a metal sheet and a resin film layer covering at least one side of the metal sheet, or a sheet material having a metal sheet; a lubrication process for applying a lubricant to the molded can body; a diameter reduction process for reducing the diameter of a part of the can body to form a reduced diameter portion; and a printing layer formation process for forming an ink printing layer on the outer peripheral surface of the can body.
11. The method for manufacturing a can container according to claim 10, wherein the forming step is a step of forming a can body from a sheet material having the metal sheet, the resin film layer, and a lubricating layer formed on one side of the resin film layer.
12. The method for manufacturing a can container according to claim 10, wherein the forming step is a step of forming a can body from the metal sheet and a sheet material having a lubricating layer formed on one or both sides of the metal sheet.
13. The method for producing a can container according to claim 11, further comprising a removing step of removing at least a part of the lubricating layer between the forming step and the lubricating step.
14. A method for manufacturing a can container, comprising: a molding step of molding a cylindrical can body from a sheet material having a metal sheet, a resin film covering at least one side of the metal sheet, and a lubricating layer formed on one side of the resin film, or a sheet material consisting of a metal sheet and a lubricating layer formed on one or both sides of the metal sheet; a diameter reduction step of reducing the diameter of a part of the molded can body to form a reduced diameter portion without applying a lubricant to the molded can body; and a printing layer formation step of forming an ink printing layer on the outer circumferential surface of the can body.
15. The method for manufacturing a can container according to any one of claims 10 to 14, further comprising a removal step between the diameter reduction step and the printing layer formation step, of removing the lubricant applied in the lubricating step or at least a part of the lubricating layer.
16. A method for manufacturing a can container, comprising: a lubrication step of applying a lubricant to a can body consisting of a cylindrical can body and a resin film layer covering at least the outer surface of the can body, or to a can body consisting of a cylindrical can body; a diameter reduction step of reducing the diameter of a part of the can body to form a reduced diameter portion; and a storage step of storing the can body in a plain state without any printing.
17. A method for manufacturing a can container, comprising: a forming step of forming a cylindrical can body from a sheet material having a metal sheet, a resin film covering at least one side of the metal sheet, and a lubricating layer formed on one side of the resin film; a diameter reducing step of reducing the diameter of a part of the can body to form a reduced diameter portion without applying a lubricant to the can body; and a storage step of storing the can body in a plain, unprinted state.
18. The method for manufacturing a can container according to claim 16, further comprising a removing step of removing a portion of the lubricant from the can body between the diameter reducing step and the storage step.
19. The method for manufacturing can containers according to claim 16 or 17, wherein the storage step is carried out in a light-shielding state so that the can body is not irradiated with ultraviolet light.
20. The method for manufacturing a can container according to claim 19, wherein the storage step includes storing the can body in a light-shielded state for one month or more.
21. A method for manufacturing a can container according to any one of claims 10 to 15, wherein the printing layer forming step includes printing on the outer surface of the can body by one or more of inkjet printing or printing with a printing plate.
22. A method for manufacturing a can container according to any one of claims 10 to 15, wherein the printing layer forming step includes covering the outer surface of the can body with a shrink film on which an ink image is printed.
23. The method for manufacturing a can container according to claim 13, wherein the removing step uses thermal energy, plasma treatment, or flame treatment.
24. The method for manufacturing a can container according to claim 15, wherein the removing step uses thermal energy, plasma treatment, or flame treatment.
Citation Information
Patent Citations
Manufacturing method for organic resin coated metal plate and manufacturing apparatus therefor
JP2004025640A
Method for manufacturing can for beverage and beverage can manufacturing method
JP2019025521A
Resin coated aluminum alloy sheet for can of drawing / ironing
JP1997276949A
Two-piece can, manufacturing method therefor, and steel sheet for two-piece can
JP2007045506A
Elongated tubular member
JP2011191784A