Calculating method and calculating program for macro direct-current mobility of semiconductor, and device simulation method using same

The new method for calculating macro DC mobility in semiconductors using intragranular mobility models addresses the inaccuracy of existing models for oxide semiconductors, enabling precise mobility calculations and scattering factor analysis, enhancing device simulation accuracy.

WO2024225482A1PCT designated stage expired Publication Date: 2024-10-31IDEMITSU KOSAN CO LTD

Patent Information

Application Number
PCT/JP2024/016604
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-28
Filing Date
2024-04-26
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Current methods for calculating the mobility of amorphous oxide semiconductors, such as the a-Si model, are inaccurate for amorphous oxide semiconductors like IGZO, and existing models for polycrystalline oxide semiconductors with higher mobility also fail to provide accurate results.

Method used

A new method for calculating macro DC mobility in semiconductors, involving the calculation of intragranular mobility using various physical parameters, specifically through the formula μ_in-grain(T) = 1/(exp(β/T)-1) with temperature dependence expressed as a linear combination of terms, and applying this model to simulate the mobility of polycrystalline oxide semiconductors to accurately determine mobility and scattering factors.

Benefits of technology

This approach allows for accurate calculation of mobility in various oxide semiconductor materials, including polycrystalline and amorphous oxide semiconductors, effectively reproducing measured mobility-carrier concentration lines and quantifying the contribution of scattering factors, thereby improving device simulation accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024016604_31102024_PF_FP_ABST
    Figure JP2024016604_31102024_PF_FP_ABST
Patent Text Reader

Abstract

This method is for calculating the macro direct-current mobility μ (T) of a semiconductor, wherein an in-grain mobility μin-grain (T) calculated in the process thereof is represented by a linear combination of two or more terms in which, when the temperature T [K] is a variation factor, the multiplicative inverse of the in-grain mobility μin-grain is selected from the group consisting of 1 / (exp(β / T)-1), T0, T-3 / 2, T1 / 2, T3 / 2, T1, and T2. [Here, β [K] is a coefficient.]
Need to check novelty before this filing date? Find Prior Art

Description

Method and program for calculating macroscopic DC mobility of semiconductor, and device simulation method using the same

[0001] The present invention relates to a method and program for calculating macroscopic DC mobility of a semiconductor, and a device simulation method using the same.

[0002] Thin-film transistors using amorphous silicon (a-Si) or low-temperature polysilicon (LTPS) have been used for example in display manufacturing. Device simulation technology has already been established to calculate the mobility of a-Si semiconductors and design devices based on the results.

[0003] In recent years, thin-film transistors using amorphous oxide semiconductors (IGZO) have come to be used in display manufacturing and the like. However, in the case of amorphous oxide semiconductors (IGZO), when the above-mentioned mobility calculation method (a-Si model) is used, the calculated mobility may deviate from the actual measured value, and it has been found that the a-Si model cannot be applied. Therefore, a method capable of accurately calculating the mobility of amorphous oxide semiconductors (IGZO) has been developed, and an amorphous oxide semiconductor (IGZO) device simulation technology (Tokyo Model) has been established (see Non-Patent Document 1).

[0004] Meanwhile, in recent years, there has been progress in the development of polycrystalline oxide semiconductors containing In as a main component, which have higher mobility than amorphous oxide semiconductors (see Non-Patent Document 2).

[0005] "Temperature Properties of Amorphous In-Ga-Zn-O Thin-Film Transistors with a new Mobility Model", The Simulation Standard, October 1, 2017 (https: / / silvaco.com / dynamicweb / jsp / downloads / DownloadDocStepsAction.do?req=download&nm=simstd_Q4_2017_a3.pdf)Kazuaki Ebata, "High-Mobility Thin-Film Transistors with Polycrystalline In-Ga-O Channel Fabricated by DC Magnetron Sputtering ", The Japan Society of Applied Physics Applied Physics Express, 6 January 2012, Volume 5, Number 1, page.011102John Y. W. Seto, J. Appl. Phys. 46 5247 (1975)C. H. Seager, T. G. Castner J Appl Phys 49, 3879 (1978)H. Frohlich, Advances in Physics 3 325 (1954)J. J. Wang et. al., Phys. Lett. A 374 2286 (2010)M. Stokey. et. al., J. Appl. Phys. 129 225102 (2021)J. Ederth et. al., Phys. Rev. B 68 155410 (2003)A. Bikowski, K. Ellmer, J. Appl. Phys. 116 143704 (2014)E. Conwell, V.F.Weisskopf, Phys. Rev. 69 258 (1946)E. Conwell, V.F.Weisskopf, Phys. Rev. 77 388 (1946)H. Brooks, Phys. Rev. 83 879 (1951)H. Brooks, Adv. Electron.Phys. 7 85 (1955)D. Chattopadhyay, H. Queisser J. Rev. Mod. Phys. 53 745 (1981)T. Pisarkiewicz, et. al., Thin Solid Films 174 217 (1989)C. Erginsoy, Phys. Rev.79 1013 (1950)T. Quisse, Physica B 270 262 (1999)C. Kittel, H. Kroemer, "Thermal Physics" Freeman, New York, 2nd ed. (1980) Chap.13 pp.367R.B. Dingle, Philos. Mag. 46 831 (1955).

[0006] However, it has become clear that even if the mobility calculation method (Tokyo Model) that has been used for the above-mentioned amorphous oxide semiconductor is applied to calculate the mobility of a polycrystalline oxide semiconductor having a higher mobility, accurate results cannot be obtained.

[0007] Therefore, the present inventors have investigated various physical parameters to develop a method for accurately calculating the mobility of various oxide semiconductor materials such as polycrystalline oxide semiconductors and amorphous oxide semiconductors. As a result, first, the intragranular mobility μ in-grain The present inventors have found that accurate mobility can be calculated for various oxide semiconductor materials by calculating the mobility μ(T) of the semiconductor using the calculation results, and have completed the present invention.

[0008] The inventors further investigated the issue, creating a mobility model by physically modeling each physical parameter that is a scattering factor for polycrystalline oxide semiconductors. When this mobility model was applied to a simulator, it accurately reproduced the measured mobility-carrier concentration curve, confirming that the mobility model functions correctly. Furthermore, it became possible to quantify the contribution of scattering factors to carrier concentration, advancing our understanding of the phenomenon. Furthermore, it was confirmed that reverse extraction of scattering parameters for polycrystalline oxide semiconductors (thin films) is also possible.

[0009] An object of the present invention is to provide a mobility calculation method, a mobility calculation program, and a device simulation method that can accurately calculate the mobility of various oxide semiconductor materials.

[0010] According to the present invention, the following semiconductor mobility calculation method and program using the same are provided: 1. Mobility μ in semiconductor grains in-grain A method for calculating (T), in which when the temperature T [K] is a fluctuation factor, the intra-grain mobility μ in-grain The reciprocal of (T) is 1 / (exp(β / T)-1), T 0 , T -3/2 , T 1/2 , T 3/2 , T 1 , and T 2 The mobility μ within the grains of a semiconductor, expressed as a linear combination of two or more terms selected from the group consisting of in-grain (T) calculation method. [Here, β[K] is a coefficient.] 2. The mobility μ in-grain The reciprocal of (T) is 1 / (exp(β / T)-1), T 0 , T -3/2 , T 1/2 , T 3/2 , T 1 , and T 2 and further, the temperature dependence is a function of the carrier concentration n, 1 / μ NI The intra-grain mobility μ of the semiconductor according to 1, wherein the (T, n) terms are linearly combined. in-grain 3. A method for calculating macroscopic DC mobility μ(T) of a semiconductor, wherein temperature T[K] is a fluctuation factor, and the calculation method is for calculating macroscopic DC mobility μ(T) of a semiconductor, which is expressed by the following formula (10): [In formula (10), μ is the mobility of the semiconductor [cm 2 / Vs], T is temperature [K], γ[K] and θ[K 2 ] is a coefficient and a positive number including 0, μ in-grain (T) is the intragranular mobility μ of the semiconductor described in 1. in-grain The mobility in the semiconductor grains [cm2 / Vs]. 4. The method for calculating the macroscopic DC mobility μ(T) of a semiconductor according to 3, which is represented by the following formula (A10): [In formula (A10), q is the elementary charge [C], V B is the grain boundary barrier height [eV], k B is the Boltzmann constant [eV / K], T is the temperature [K], μ in-grain (T) is the intra-grain mobility of the semiconductor [cm 2 / Vs].

[0011] 5. A device simulation method for determining the macroscopic DC mobility μ(T) of a semiconductor, comprising the step of using the method for calculating the macroscopic DC mobility μ(T) of a semiconductor described in 3. 6. A method for manufacturing a thin-film transistor, comprising the steps of calculating the macroscopic DC mobility μ(T) of a semiconductor using the method for calculating the macroscopic DC mobility μ(T) of a semiconductor described in 3, and manufacturing a thin-film transistor based on the calculated macroscopic DC mobility μ(T). 7. An electronic device comprising a thin-film transistor manufactured using the method for manufacturing a thin-film transistor described in 6.

[0012] 8. The following formulas (1) and (10) [In formula (1), μ in-grain is the mobility within the semiconductor grains [cm 2 / Vs], T is temperature [K], β[K], a 1 [cm -2 Vs], a 2 [cm -2 Vs], a 3 [cm -2 Vs. K 3/2 ], a 4 [cm -2 Vs. K -1/2 ], and a 5 [cm -2 Vs. K -3/2 ] respectively represent coefficients. However, in the above formula (1), 1 / (exp(β / T)-1) and T 0 , T -3/2 , T 1/2 and T 3/2Using two or more terms selected from the group consisting of: 1 ~a 5 is set to 0.] [In formula (10), μ is the mobility of the semiconductor [cm 2 / Vs], T is temperature [K], γ[K] and θ[K 2 ] is a coefficient and a positive number including 0, μ in-grain (T) is the intragranular mobility μ of the semiconductor described in 1. in-grain The mobility in the semiconductor grains [cm 2 / Vs].], the program for calculating the macroscopic DC mobility μ(T) of a semiconductor using the temperature T [K] and the carrier concentration n [cm -3 a means for receiving an input of the type of material of the semiconductor; and a coefficient a 1 ~a 5 a program for causing the program to function as a means for selecting values ​​of β, γ, and θ; and a means for calculating the macroscopic DC mobility μ(T) of the semiconductor using the formulas (1) and (10).

[0013] 9. Temperature T [K] and carrier concentration n [cm -3 ], the macroscopic DC mobility μ(T, n) [cm 2 / Vs], causing a computer to function as a means for deriving the macroscopic DC mobility μ(T, n) by performing regression using: a means for accepting data input of μ(T, n) for T and n measured from a semiconductor film; a means for accepting input of the type of semiconductor material for obtaining initial values ​​of each coefficient in the following formula (1); and the program described in 8. [In formula (1), μ in-grain is the mobility within the semiconductor grains [cm 2 / Vs], T is temperature [K], β[K], a 1 [cm -2 Vs], a 2 [cm -2 Vs], a 3 [cm -2 Vs. K 3/2 ], a 4[cm -2 Vs. K -1/2 ], and a 5 [cm -2 Vs. K -3/2 ] respectively represent coefficients. However, in the above formula (1), 1 / (exp(β / T)-1) and T 0 , T -3/2 , T 1/2 and T 3/2 Using two or more terms selected from the group consisting of: 1 ~a 5 is set to 0.]

[0014] According to the present invention, it is possible to provide a mobility calculation method, a mobility calculation program, and a device simulation method that can accurately calculate the mobility of various oxide semiconductor materials.

[0015] The actual measured value μ of the mobility of the specimen 1 with respect to the carrier concentration n obs. and the calculated value μ of the macro DC mobility obtained in Example 1. calc The horizontal axis is the measured value μ of the mobility of specimen 1. obs. The vertical axis represents the calculated value μ of the macro DC mobility obtained in Example 1. calc 1 is a graph plotting the measured mobility μ of specimen 2 against the carrier concentration n. obs. and the calculated value μ of the macro DC mobility obtained in Example 2 calc The horizontal axis represents the measured value μ of the mobility of the specimen 2. obs. The vertical axis represents the calculated value μ of the macro DC mobility obtained in Example 2. calc 1 is a graph plotting the measured mobility μ of specimen 1 against the carrier concentration n. obs. and the calculated value μ of the macro DC mobility obtained in Comparative Example 1 calc The horizontal axis is the measured value μ of the mobility of specimen 1. obs. The vertical axis represents the calculated value μ of the macro DC mobility obtained in Comparative Example 1. calc 1 is a graph plotting the measured mobility μ of specimen 2 against the carrier concentration n. obs. and the calculated value μ of the macro DC mobility obtained in Comparative Example 2 calcThe horizontal axis represents the measured value μ of the mobility of the specimen 2. obs. The vertical axis represents the calculated value μ of the macro DC mobility obtained in Comparative Example 2. calc 1 is a graph plotting the macroscopic DC mobility μ(T) [cm 2 1 is a flow chart showing an outline of a program for calculating the macroscopic DC mobility μ(T, n) [cm / Vs] of a semiconductor according to one embodiment of the present invention. 2 1 is a flow chart showing an outline of a program for deriving the macroscopic DC mobility μ(T) [cm / Vs] of a semiconductor according to one embodiment of the present invention. 2 1 is a flow chart showing an outline of a machine learning program for calculating the intra-grain mobility μ of the semiconductor used in the present invention. in-grain 1 is a graph showing the mobility-carrier concentration characteristics of each measurement sample at room temperature. 2 is an EBSD (Electron Backscattering Diffraction) image showing information about the crystal orientation and grain size of each measurement sample. 3 is a graph plotting each scattering parameter extracted by parameter fitting for each measurement sample. 4 is a graph showing the carrier concentration dependence of each scattering parameter common to each measurement sample. 5 is a graph showing the carrier concentration dependence of each scattering parameter common to each measurement sample. 6 is a graph showing the carrier concentration dependence of each scattering parameter common to each measurement sample. 0 2 -ka 0 In a log-log graph, each q s a 0 Q / πa in 0 2 -ka 0 Q / πa in the Quisse model, which regards the curve as the upper base and hypotenuse of a right-angled trapezoid 0 2 This is a conceptual diagram for approximating each q s a 0 Noka 0 Q / πa at =0 0 2 The value of (Q 0 @k ‘ = 0) was obtained from the Quisse model, and each q s a 01 is a graph showing an approximation of the upper-base value in . ... obs. 1 is a graph plotting the relationship between the carrier concentration of each measurement sample on the horizontal axis and the scattering rate of each scattering parameter on the vertical axis.

[0016] 1. Mobility μ within semiconductor grains in-grain Calculation method of (T) Intra-grain mobility μ of the semiconductor according to one embodiment of the present invention in-grain The calculation method of (T) (hereinafter sometimes abbreviated as "calculation method of intragranular mobility") is as follows: When temperature T [K] is used as a variable factor, intragranular mobility μ in-grain The reciprocal of (T) is 1 / (exp(β / T)-1), T 0 , T -3/2 , T 1/2 , T 3/2 , T 1 , and T 2 where β[K] is a coefficient.

[0017] The mobility of semiconductors is a physical quantity that is affected by the effective mass, crystal structure, crystal transition, crystal grains, and defect amount specific to the semiconductor material, and varies with temperature, carrier concentration, scattering parameters, and potential barriers. in-grain "(T)" is the mobility inside one crystal grain. By calculating this, it is possible to know the macroscopic DC mobility in a single crystal state and the macroscopic DC mobility when the potential barrier at the grain boundary is extremely small.

[0018] In one embodiment, a method for calculating intragranular mobility includes: in-grain As the reciprocal of (T), 1 / (exp(β / T)-1), T 0 , T -3/2 , T 1/2 and T 3/2 Two or more terms selected from the group consisting of: [In formula (1), μ in-grain is the mobility within the semiconductor grains [cm 2 / Vs], T is temperature [K], β[K], a 1 [cm -2 Vs], a 2 [cm -2 Vs], a 3 [cm -2 Vs. K 3/2 ], a 4 [cm -2 Vs. K -1/2 ], and a 5 [cm -2 Vs. K -3/2 ] respectively represent coefficients. However, in the above formula (1), 1 / (exp(β / T)-1) and T 0 , T -3/2 , T 1/2 and T 3/2 The coefficient a of the unselected term 1 ~a 5 is set to 0.]

[0019] In one embodiment, the β[K] is represented by the following formula (2). [In formula (2), hω op / 2π is the energy of the optical phonon [eV], which varies depending on the carrier concentration, k B is the Boltzmann constant (8.617 x 10 -5 [eV / K]), h is Planck's constant (4.1357 × 10 -15 [eVs]).

[0020] In one embodiment, 1 [cm -2 Vs] is the carrier concentration n [cm -3 ], which varies depending on 1 (n), wherein the a1 (n) is expressed by the following formula (3). [In formula (3), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), A 1 [cm -2 Vs], B 1 , and C 1 [cm -2 Vs] are the coefficients, N 01 Haa 1 (n) is the carrier concentration corresponding to the inflection point in equation (3).

[0021] In one embodiment, the A 1 is 0 cm -2 Vs or more 0.1cm -2 Vs or less (preferably 0.0005 cm -2 Vs or more 0.09cm -2 Vs or less, more preferably 0.001 cm -2 Vs or more 0.08cm -2 Vs or less), and 1 is 0 or more (B 1 The upper and lower limits of C are not particularly limited. 1 is 1 cm -2 Vs or less (preferably 1×10 -1 cm -2 Vs or less, more preferably 8×10 -2 cm -2 Vs or less, more preferably 5×10 -2 cm -2 Vs or less, and the lower limit is not particularly limited, and is 0 cm -2 Vs), and the N 01 is 1 x 10 18 cm -3 1x10 or more 23 cm -3 or less (preferably 3 × 10 18 cm -3 5x10 or more 22 cm -3 Less than or equal to 5×10, more preferably 18 cm -3 1x10 or more 22 cm -3 (See below). A1 , B 1 , C 1 , and N 01 When A is within the above range, the intragranular mobility can be calculated more accurately. 1 is 0 cm -2 Vs, and the C 1 is 1 cm -2 It may be Vs or less.

[0022] In one embodiment, 2 [cm -2 Vs] is the carrier concentration n [cm -3 ], which varies depending on 2 (n), wherein the a 2 (n) is expressed by the following formula (4). [In formula (4), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), A 2 [cm -2 Vs], B 2 , and C 2 [cm -2 Vs] are the coefficients, N 02 Haa 2 (n) is the carrier concentration corresponding to the inflection point in equation (4).

[0023] In one embodiment, the A 2 is 0.005 cm -2 Vs or more 0.5cm -2 Vs or less (preferably 0.006 cm -2 Vs or more 0.08cm -2 Vs or less, more preferably 0.008 cm -2 Vs or more 0.06cm -2 Vs or less), and 2 is 1000 or less (the lower limit is not particularly limited and may be a negative value, and the upper limit is preferably 800 or less, more preferably 500 or less, and even more preferably 100 or less), and 2 is 1 x 10 -1 cm -2 Vs (preferably 8 × 10 -2 cm-2 Vs or less, more preferably 15×10 -3 cm -2 Vs or less, and the lower limit is not particularly limited, and is 0 cm -2 Vs), and the N 02 is 1 x 10 17 cm -3 1x10 or more 22 cm -3 or less (preferably 1 × 10 18 cm -3 5x10 or more 21 cm -3 (See below). A 2 , B 2 , C 2 , and N 02 When is within the above range, the intragranular mobility can be calculated more accurately.

[0024] In one embodiment, 3 [cm -2 Vs. K 3/2 ] is the carrier concentration n [cm -3 ], which varies depending on 3 (n), wherein the a 3 (n) is expressed by the following formula (5). [In formula (5), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), A 3 [cm -8 Vs. K 3/2 ] and B 3 , C 3 [cm -2 Vs. K 3/2 ] 、 D 3 [cm 3 ] and F 3 [cm -2 Vs. K 3/2 ] are the coefficients, N 03 Haa 3 The maximum carrier concentration [cm -3 ].]

[0025] In one embodiment, the A 3 But, 10-39 cm -8 Vs. K 3/2 10 above -33 cm -8 Vs. K 3/2 or less (preferably 10 -38 cm -2 Vs or more 10 -33 cm -2 Vs or less, more preferably 10 -37 cm -2 Vs or more 10 -34 cm -2 Vs or less), and 3 is 1 or more and 5000 or less (preferably 5 or more, more preferably 6 or more, and the upper limit is preferably 4000 or less, more preferably 3000 or less, and even more preferably 2000 or less), and 3 is 10 8 cm -2 Vs. K 3/2 Less than (preferably 10 7 cm -2 Vs. K 3/2 Less than 10, more preferably 6 cm -2 Vs. K 3/2 Hereinafter, the lower limit is not limited and may be a negative value), and 3 is 10 -20 cm 3 The above and F 3 is 500 cm -2 Vs. K 3/2 is less than 03 is 1 x 10 16 cm -3 1x10 or more 20 cm -3 or less (preferably 5 × 10 16 cm -3 5x10 or more 19 cm -3 or less, more preferably 1 × 10 17 cm -3 1x10 or more 19 cm -3 (See below). A 3 , B 3 , C 3 , and N 03 When is within the above range, the intragranular mobility can be calculated more accurately.

[0026] In one embodiment, 3 is the carrier concentration n [cm -3 ], which varies depending on 3 (n), and N 03 [cm -3 ] and N 13 [cm -3 ] is an arbitrary carrier concentration, 3 (n) is n<N 03 When N 03 ≦n≦N 13 When n>N, it is expressed by equation (5-2). 13 In this case, it is expressed by the following formula (5-3). [In the formulas (5-1), (5-2) and (5-3), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), A' 3 [cm -8 Vs. K 3/2 ], C' 3 [cm -2 Vs. K 3/2 ] and D' 3 [cm 3 ] are coefficients, B' 3 [cm -2 Vs. K 3/2 ] is a constant.

[0027] In one embodiment, A' 3 But, 10 -39 cm -8 Vs. K 3/2 10 above -33 cm -8 Vs. K 3/2 or less (preferably 10 -38 cm -2 Vs. K 3/2 10 above -33 cm -2 Vs. K 3/2 Less than 10, more preferably -37 cm -2 Vs. K 3/2 10 above -34 cm -2 Vs. K3/2 hereinafter), and 3 is 5000 cm -2 Vs. K 3/2 or less (preferably 4000 cm -2 Vs. K 3/2 or less, more preferably 3000 cm -2 Vs. K 3/2 The lower limit is not particularly limited below), and 3 is 10 -20 cm 3 That's all. A' 3 , C' 2 , and D' 3 When is within the above range, the intragranular mobility can be calculated more accurately.

[0028] In one embodiment, the a 4 [cm -2 Vs. K -1/2 ] is a coefficient that varies depending on the carrier concentration.

[0029] In one embodiment, 5 [cm -2 Vs. K -3/2 ] is a coefficient that varies depending on the carrier concentration.

[0030] In one embodiment, the semiconductor is a non-degenerate semiconductor, and the a 1 is the optical phonon scattering constant A op [cm -2 Vs], the above a 2 is the neutral impurity scattering coefficient A neutral [cm -2 Vs. K 3/2 ], the a 3 is the ionized impurity scattering coefficient A ion [cm -2 Vs. K -1/2 ], the a 4 is the weak localization constant [cm -2 VsK -1/2 ], the a 5 is the acoustic phonon scattering constant [cm -2 Vs. K -3/2 ].

[0031] The optical phonon scattering constant A op [cm-2 The neutral impurity scattering coefficient A is a constant that represents the degree of scattering that occurs when carriers responsible for electrical conduction collide with optical phonons (quantized phonons, which are electric polarizations caused by ionic vibrations among lattice vibrations). As the value increases, the mobility decreases. neutral [cm -2 Vs. K 3/2 ] is a constant that represents the degree of scattering that occurs when carriers responsible for electrical conduction collide with electrically neutral impurities, and as the value increases, the mobility decreases. ion [cm -2 Vs. K -1/2 ] is a constant that represents the degree of scattering that occurs when carriers responsible for electrical conduction collide with non-electrically neutral ionized impurities, and as the value increases, the mobility decreases. -2 Vs. K -1/2 ] represents the degree of effect of carriers responsible for electrical conduction forming standing waves due to the influence of impurities and lattice defects and being slightly localized, and as the value increases, the mobility decreases. -2 Vs. K -3/2 ] is a constant that represents the degree of scattering that occurs when carriers responsible for electrical conduction collide with acoustic phonons (quantized lattice vibrations in which atoms vibrate in phase), and as the value increases, mobility decreases.

[0032] Here, a "non-degenerate semiconductor" is a semiconductor with a low carrier concentration in which the Fermi energy does not exist in the conduction band or valence band, and the statistical average of the number of electrons occupying the energy level E cannot be expressed by the Boltzmann approximation, but is expressed by the Fermi-Dirac distribution.

[0033] (Type of Semiconductor Material) The method for calculating intra-grain mobility according to this embodiment can be applied to various semiconductor materials such as crystalline oxide semiconductors and amorphous oxide semiconductors. In one embodiment, the semiconductor is a polycrystalline semiconductor. In one embodiment, the polycrystalline semiconductor is an oxide semiconductor containing In as a main component.

[0034] "Containing In as a main component" means that the content ratio of In to all metal elements in the crystalline oxide semiconductor ([In] / ([In]+[all metal elements other than In])×100) (atomic %) is higher than the content ratio of each metal element other than In. In one embodiment, the content ratio of In to all metal elements in the polycrystalline semiconductor is 33 atomic % or more, preferably 50 atomic % or more, and more preferably 70 atomic % or more. A higher In content ratio is likely to result in more accurate calculation results.

[0035] In one embodiment, the polycrystalline semiconductor is in the form of an oxide thin film. In semiconductor devices, such as thin film transistors, semiconductors are used in the form of thin films, and the method for calculating intra-grain mobility of this aspect is suitable for cases where the semiconductor is in the form of a thin film.

[0036] In one embodiment, the polycrystalline semiconductor thin film has a bixbyite structure. A polycrystalline semiconductor thin film having a bixbyite structure is likely to produce more accurate calculation results. Whether a polycrystalline semiconductor thin film has a bixbyite structure can be confirmed by the following method.

[0037] (Method for Evaluating Whether or Not a Semiconductor Film Has a Bixbyite Structure) Whether or not a semiconductor film has a bixbyite structure can be determined by obtaining a diffraction pattern by electron diffraction and comparing it with an electron diffraction pattern that can be calculated from crystal structure data of the bixbyite structure in the Inorganic Crystal Structure Database (ICSD: Chemical Information Association).

[0038] 2. Method for Calculating Macroscopic DC Mobility μ(T) of a Semiconductor A method for calculating macroscopic DC mobility μ(T) of a semiconductor according to one aspect of the present invention (hereinafter, may be abbreviated as "method for calculating macroscopic DC mobility") is characterized in that, when temperature T [K] is a fluctuation factor, it is expressed by the following formula (10): [In formula (10), μ is the mobility of the semiconductor [cm 2 / Vs], T is temperature [K], γ[K] and θ[K 2 ] is a coefficient and a positive number including 0, μ in-grain(T) is the intra-grain mobility μ of the semiconductor according to one embodiment of the present invention described above. in-grain The mobility in the semiconductor grains [cm 2 / Vs].

[0039] The macroscopic DC mobility μ(T) of a semiconductor obtained by the calculation method of this embodiment is a calculated value of mobility used in actual device simulation. Here, the "macroscopic DC mobility of a semiconductor" refers to the mobility of carriers responsible for electrical conduction, calculated from the resistance value, which is the real part of the complex impedance obtained when a voltage is applied across a semiconductor material formed as a thin film and the current is measured.

[0040] First, the mobility within the semiconductor grains [cm 2 / Vs] and then using this to calculate the macroscopic DC mobility, it is possible to calculate separately the mobility affected by scattering within the crystal grains and the mobility affected by scattering due to the potential barrier.

[0041] In one embodiment, γ[K] or θ[K 2 ] is 0.

[0042] In the above formula (10), γ[K] and θ[K 2 ] and the macroscopic DC mobility calculated using θ[K 2 The difference in the macroscopic DC mobility calculated by setting θ[K 2 When [0] is set to 0, the mobility is calculated in the case where the atomic arrangement is highly ordered and the contribution of percolation conduction is extremely low.

[0043] In one embodiment, the γ is represented by the following formula (12). [In formula (12), q is the elementary charge of 1.602 × 10 -19 [C], V Bis the potential barrier value [eV], k B is the Boltzmann constant (8.617 x 10 -5 [eV / K]).

[0044] In one embodiment, the potential barrier value V B [eV] is the carrier concentration n [cm -3 The potential barrier value V varies depending on B (n), wherein V B (n) is expressed by the following formula (13). [In formula (13), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), A 6 [eV], B 6 , C 6 [eV], and D 6 are the coefficients, respectively. 06 [eV] is V B (n) is the carrier concentration corresponding to the inflection point in equation (13).

[0045] In one embodiment, the A 6 is 0 eV or more and 1.0 eV or less (preferably 0 eV or more and 0.8 eV or less, more preferably 0 eV or more and 0.2 eV or less), and 6 is 0.1 or more (preferably 0.7 or more, more preferably 1 or more, and the upper limit is not particularly limited), 6 is 2 x 10 -1 Less than (preferably 5 x 10 -2 or less, more preferably 1 × 10 -3 Hereinafter, the lower limit is not particularly limited and may be a negative value), and 6 is 0.1 eV or less (preferably 0.08 eV or less, more preferably 0.05 eV or less, and the lower limit is not particularly limited), 06 is 1 x 10 17 cm -3 1x10 or more 21 cm -3 or less (preferably 5 × 10 17 cm -3 5x10 or more 20cm -3 or less, more preferably 1 × 10 18 cm -3 1x10 or more 20 cm -3 (See below). A 6 , B 6 , C 6 , D 6 , and N 06 When is within the above range, the macroscopic DC mobility can be calculated more accurately.

[0046] (Type of Semiconductor Material) The method for calculating macroscopic DC mobility according to this embodiment can be applied to various semiconductor materials, such as crystalline oxide semiconductors and amorphous oxide semiconductors. In one embodiment, the semiconductor is a polycrystalline semiconductor. In one embodiment, the polycrystalline semiconductor is an oxide semiconductor containing In as a main component. In one embodiment, the content of In in all metal elements of the polycrystalline semiconductor is 50 atomic % or more.

[0047] In one embodiment, the polycrystalline semiconductor has a shape of an oxide thin film. The polycrystalline semiconductor thin film includes a bixbyite structure. As with the method for calculating intragranular mobility according to one aspect of the present embodiment, the method for calculating macroscopic DC mobility according to this aspect can more accurately calculate mobility when the semiconductor material is one of the above.

[0048] The effect obtained when the polycrystalline semiconductor thin film has a bixbyite structure, and confirmation that the polycrystalline semiconductor thin film has a bixbyite structure, are as described in the calculation method for intragranular mobility.

[0049] 3. Physical Modeling of Various Scattering Parameters In order to create physical models of various scattering parameters, the following study was conducted. Here, the term "scattering factor" refers to the scattering ability of conduction electrons or holes that are present in a semiconductor and cause a decrease in mobility, and the term "scattering parameter" refers to a numerical value that represents the mobility decrease index of each "scattering factor."

[0050] (1) Measurement data and its acquisition method As a scattering parameter, the grain boundary scattering barrier height V B , optical phonon scattering a OP, ionized impurity scattering in the non-degenerate region (hereinafter referred to as "ionized impurity scattering (non-degenerate)") a II_nonDeg , ionized impurity scattering in the degenerate region (hereinafter referred to as "ionized impurity scattering (degenerate)") a II_Deg , neutral impurity scattering a NI The scattering parameters can be obtained by measuring the temperature-dependent Hall effect for each carrier concentration on samples formed under the same film formation conditions.

[0051] The samples analyzed (hereinafter, sometimes referred to as specimens) were six types of oxide semiconductor thin films (30 nm thick, annealed at 400°C for 1 hour in air) listed in Table 4 of the Examples. The mobility-carrier concentration characteristics (hereinafter, sometimes referred to as μ-n characteristics or μ-n lines) of each sample at room temperature are shown in Figure 9, and information on crystal orientation and grain size is shown in Figure 10. Although IO, IGO (L.G.), IGO (Ref), and IGO (111) (Specimens 3 to 6 listed in Table 4) differ in crystal orientation and grain size, there is no significant difference in μ-n line performance compared to IGO (Amo.) and IGO (L.Q.) (Specimens 7 and 8 listed in Table 4). Therefore, IO, IGO (L.G.), IGO (Ref), and IGO (111) were used as model samples when creating a mobility model for polycrystalline oxide semiconductors.

[0052] Next, the scattering parameters extracted by parameter fitting are summarized in Figure 11. -3/2 Assuming that the coefficient of is due to ionized impurity scattering, a II However, in conclusion, ionized impurity scattering (non-degenerate) a II_nonDeg and ionized impurity scattering (degenerate) a II_Deg Therefore, it is necessary to distinguish between the two. -3/2 The coefficient of a II_nonDeg Similarly, T 0 Assuming that the coefficient of a is due to neutral impurities, NI However, the conclusion is that 0 It has become clear that the coefficient of is largely affected by neutral impurity scattering and ionized impurity scattering (degeneracy). 0 It was expressed as.

[0053] (2) Study on carrier concentration dependence of scattering parameters in polycrystalline oxide semiconductors In order to physically model the μ-n line of polycrystalline oxide semiconductors, we first considered the scattering parameter-carrier concentration dependence of each scattering parameter (hereinafter sometimes referred to as an line). The carrier concentration dependence of each scattering parameter common to the model samples is shown in FIG. 12. The dashed lines in each graph represent V B It corresponds to the -n line or the an line.

[0054] (3) Grain boundary scattering model The grain boundary barrier-carrier concentration dependence (V B To explain the V-n line, we first examined the Seto model [John YW Seto, J. Appl. Phys. 46 5247 (1975)], which is commonly used in discussions of grain boundary barriers in polycrystalline semiconductors. However, in the Seto model, V B The carrier concentration dependence of "V B The graph of -n is downward convex, and V in Fig. 12(a) B It was found that there was a large deviation from the -n line. Here, after an intensive literature search, it was found that by using the Seager model [CH Seager, TG Castner J Appl Phys 49, 3879 (1978)], V B -n line behavior is well reflected, B The Seto model has the drawback of not having a concept of energy levels for traps (they change automatically), but the Seager model overcomes this drawback by using the energy levels and trap amounts as independent variables, and then calculating V B Since equation (n) has been derived, it is considered to match the experimental behavior. B The −n line is based on the Seager model, where the Fermi level difference between the grain boundary and the grain interior is 25 meV and the grain boundary trap density is 7.5 × 10 13 cm -2 eV -1 As mentioned above, V BThe Seager model, which well represents the behavior of (n), was adopted to obtain the following equation (A11).

[0055] [In formula (A11), V B is the grain boundary barrier height [eV], and α is (In the formula, ε 0 is the dielectric constant of vacuum [F / cm], ε r is the relative dielectric constant (static), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), e is the elementary charge [C], N T is the grain boundary trap density [cm -2 eV -1 ], and δ EF is the Fermi energy difference between the grain boundary and the grain interior (E F GB -E F B ) [eV], where V B ≧0.]

[0056] Here, the grain boundary barrier height V B corresponds to the above formula (13).

[0057] (4) Study of optical phonon scattering model Several models based on temperature dependence have been proposed for optical phonon scattering. OP teeth, As a result, we adopted the following equation (A2-2) [J. J. Wang et. al., Phys. Lett. A 374 2286 (2010)] based on the Frohlich model [H. Frohlich, Advances in Physics 3 325 (1954)] for optical phonon scattering.

[0058]

[0059] Actually ω opt = 360 cm -1 , ε opt = 4, εr Substituting the value of 14 into the above formula (A2-2), the value of a shown in FIG. OP The (n) line was obtained. This assigned value corresponds to the frequency of the TO phonon, which is the most dominant vibration mode of indium oxide, at 363.4 cm. -1 [M. Stokey et al., J. Appl. Phys. 129 225102 (2021)], the optical dielectric constant of ITO thin film is 4 [J. Ederth et al., Phys. Rev. B 68 155410 (2003)], and the relative dielectric value of 11.85 extracted from impedance measurements. OP Based on the reproducibility of the above, the Frohlich model selected in this study was deemed appropriate.

[0060] Furthermore, in the low carrier concentration region (<5×10 18 cm -3 ) experimental point could not be confirmed, but this is a OP Temperature dependence term and the temperature dependence of grain boundary scattering <exp(-qV B / k B This is because the contribution of grain boundary scattering is large in the low carrier concentration region, and the above a OP This is because it becomes difficult to extract the temperature-dependent term. In fact, it has been reported that the mobility equation for optical phonon scattering remains almost constant even when the carrier concentration changes from the degenerate region to the non-degenerate region [A. Bikowski, K. Ellmer, J. Appl. Phys. 116 143704 (2014)]. Based on the above, we assumed that the above equation (A2-2), based on the Frohlich model, holds true across the entire carrier concentration range as the optical phonon scattering model.

[0061] In one embodiment, the coefficient of the 1 / (exp(β / T)−1) term is a 1 [cm -2 Vs], and the mobility μ determined by the optical phonon scattering model OP and the mobility μ determined by the optical phonon scattering model OP [cm 2 / Vs] is expressed by the following formula (A2). [In formula (A2), T is temperature [K], and β [K] is a coefficient.]

[0062] That is, 1 / μ expressed by the above formula (A2) OP is the term in the formula (1) Corresponds to.

[0063] In one embodiment, the coefficient β[K] can be expressed by the following formula.

[0064] In one embodiment, the coefficient a 1 [cm -2 Vs] can be expressed by the following formula (A2-1).

[0065] In one embodiment, the mobility μ determined by the optical phonon scattering model OP [cm 2 / Vs] can be expressed by the following formula (A2-2).

[0066] (5) Ionized impurity scattering (non-degenerate) model Well-known mobility models for ionized impurity scattering (non-degenerate) include the Conwell-Weisskopf model (commonly known as the CW model) [E. Conwell, V.F. Weisskopf, Phys. Rev. 69 258 (1946), and E. Conwell, V.F. Weisskopf, Phys. Rev. 77 388 (1946)] and the Brooks-Herring model (commonly known as the BH model) [H. Brooks, Phys. Rev. 83 879 (1951), and H. Brooks, Adv. Electron. Phys. 7 85 (1955)]. Comparing the CW model and the BH model, the long-range component term of the Coulomb potential (the screening function F in ionized impurity scattering in Equation (A3-2) described later) is II ) are either truncated or screened, but otherwise they are the same equations. In addition, the truncation term in the CW model uses the distance between ionized impurities as an index, so the ionized impurity concentration N II[D. Chattopadhyay, H. Queisser J. Rev. Mod. Phys. 53 745 (1981)]. On the other hand, in the BH model, ionized impurities are screened by the influence of the surrounding electron concentration, so F II is N II It is not a function of , but a function of the free carrier concentration n [D. Chattopadhyay, H. Queisser J. Rev. Mod. Phys. 53 745 (1981)]. In a typical single-crystal semiconductor, the ionized impurity concentration N II and the free carrier concentration n are almost equal, i.e., N II The relationship between 1 and n often holds, and many documents do not strictly distinguish between them, so care must be taken when selecting an equation.

[0067] The dashed line in FIG. II_nonDeg The dashed line in the low carrier concentration portion of FIG. 12(c) is the result of applying the following formula (A5-CW) which is a CW model. As is clear from the definition formula of the CW model, the scattering parameter a II_nonDeg does not show carrier concentration dependence. On the other hand, when the BH model is applied, F II The influence of the free carrier concentration n in the term was large, and the scattering parameter monotonically increased toward the low carrier concentration region, and the actual measurement results were not reproduced. Therefore, in consideration of the continuity with the ionized impurity scattering (degenerate) model described later, F in the CW model II The Pisarkiewicz type shielding parameters [T. Pisarkiewicz, et. al., Thin Solid Films 174 217 (1989)] were applied to the following equations (A5-BH) and (F). As a result, the scattering parameter a II_nonDeg Here, the non-degenerate and degenerate regions are divided into two regions, c However, since the mobility function becomes discontinuous, a continuous change using a sigmoid function was selected.

[0068] In one embodiment, the mobility μ determined by the ionized impurity scattering (non-degenerate) modelII (nonDeg) [cm 2 / Vs] can be expressed by the mobility equation (A5-BH) of the Conwell-Weisskopf model or the Brooks-Herring model.

[0069] In one embodiment, the mobility μ determined by the ionized impurity scattering (non-degenerate) model II (nonDeg) [cm 2 / Vs] can be expressed by the following mobility equation (A5-CW) of the Conwell-Weisskopf model type.

[0070] [In formula (A5-CW), ε 0 is the dielectric constant of vacuum [F / cm], ε r is ε r is the relative permittivity (static), k B is the Boltzmann constant [eV / K], T is the temperature [K], m * is the effective mass normalized by the speed of light [eV / c 2 ] (c is the speed of light [cm / s]), e is the elementary charge [C], Z is the ion valence of the ionized impurity, N II_nonDeg is the ionized impurity concentration [cm -3 ].]

[0071] In one embodiment, the mobility μ determined by the ionized impurity scattering (non-degenerate) model II (nonDeg) [cm 2 / Vs] can be expressed by the following mobility equation (A5-BH) of the Brooks-Herring model. {In formula (A5-BH), F II is the screening function for ionized impurity scattering, and ε 0 is the dielectric constant of vacuum [F / cm], ε r is the relative permittivity (static), k B is the Boltzmann constant [eV / K], T is the temperature [K], m * is the effective mass normalized by the speed of light [eV / c 2 ] (c is the speed of light [cm / s]), e is the elementary charge [C], Z is the ion valence of the ionized impurity, N II_nonDegis the ionized impurity concentration [cm -3 ].

[0072] The shielding function F in the Brooks-Herring model mobility equation II is the shielding function F in Pisarkiewicz-type ionized impurity scattering, which is expressed by the following formula (F): II is.

[0073] In one embodiment, the mobility determined by the ionized impurity scattering (non-degenerate) model that can be expressed by the mobility formula of the Conwell-Weisskopf model type or the Brooks-Herring model type is μ II_CW-BH (nonDeg) [cm 2 / Vs], the mobility μ determined by the ionized impurity scattering (non-degenerate) model II (nonDeg) [cm 2 / Vs] can be expressed by the following sigmoid function formula (A5-S) with respect to the carrier concentration n.

[0074] [In formula (A5-S), N C is the effective density of states [cm -3 ], n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), and a is a parameter that represents the rate of change of the sigmoid function.

[0075] Here, the T -3/2 The coefficient of the term is a3 [cm -2 VsK 3/2 ], and the coefficient a 3 and T -3/2 The product of these is the mobility μ determined by the ionized impurity scattering (non-degenerate) model. II (nonDeg) [cm -2 Vs] reciprocal 1 / μ II (nonDeg) It can be expressed as:

[0076] (6) Scattering parameter a 0Discussion and modeling of the scattering parameter behavior to be elucidated in Fig. 12(a) to (d), 0 (n) shows that the mobility does not depend on temperature (μ(T) ∝ T 0 ) means the scattering parameter, where a 0 (n) is a complex issue, as it is the dominant factor in the mobility characteristics during TFT operation (the most important scattering parameter), two scattering factors (neutral impurity scattering and ionized impurity scattering (degenerate)) are mixed, and conventional models cannot be applied to neutral impurity scattering. Therefore, it will be discussed separately as follows.

[0077] (6-1) Neutral impurity scattering Erginsoy model In a strict sense, when a hydrogen-like atom is assumed as a neutral impurity scatterer, the cross section of the hydrogen-like atom (Bohr radius a 0 The total scattering cross section is approximately the square of the scattering cross section, which corresponds to the total scattering cross section, and is the mechanism by which conduction carriers are scattered. Furthermore, this scattering assumes elastic scattering and quantum scattering due to the potential of hydrogen-like atoms, and the total scattering cross section is generally treated as a phase shift in wavenumber space. Furthermore, the Erginsoy model [C. Erginsoy, Phys. Rev.79 1013 (1950)] has been widely used as a model for neutral impurity scattering. This is thought to be due to the use of bold approximations when calculating the total scattering cross section, and the mathematical formula is simple. However, because the scattering cross section is linearly approximated, there is a tendency for scattering in the high-energy region to be overestimated, which has the problem of causing a significant mobility reduction even at low scatterer concentrations. In fact, when the Erginsoy model is used for Figure 12(d), the low carrier concentration region (<3 × 10 17 cm -3 ) the model corresponds to the plateau component in the high carrier concentration region, but 0 (n) Not applicable to changes. 0 Since there were no factors other than neutral impurity scattering that showed dependence, except for ionized impurity scattering (degenerate), which will be described later, further investigation was carried out on the known neutral impurity scattering model and ionized impurity scattering (degenerate).

[0078] In one embodiment, T 0 The coefficient of the term is a 2 [cm -2 Vs], and the mobility μ determined by the neutral impurity scattering model NI [cm 2 / Vs] reciprocal 1 / μ NI , and the mobility μ determined by the ionized impurity scattering (degenerate) model II (Deg) [cm 2 / Vs] reciprocal 1 / μ II (Deg) It can be expressed by either one or both of the following.

[0079] In one embodiment, the mobility μ determined by the neutral impurity scattering model NI [cm 2 / Vs] can be expressed by an Erginsoy-type mobility model or a Quisse-type mobility approximation formula.

[0080] In one embodiment, the mobility μ determined by the Erginsoy-type mobility model NI [cm 2 / Vs] is expressed by the following formula (A3E).

[0081]

[0082] (6-2) Quisse model of neutral impurity scattering As a result of a literature survey on the neutral impurity scattering model, it was found that the total scattering cross section Q exhibits carrier concentration dependence, i.e., a 0 We have found the Quisse model [T. Quisse, Physica B 270 262 (1999)], which may be able to explain the carrier concentration change in (n). The Quisse model incorporates the concept of the effective Bohr radius, which takes into account the Debye screening length due to the carrier concentration change, and further combines a number of analytical expressions in the trial wave function, making it possible to calculate the total scattering cross section and mobility for hydrogen-like atoms without approximation.

[0083] First, to determine whether the Quisse model can be applied to this system, we performed a retest of Quisse's paper [T. Quisse, Physica B 270 262 (1999)]. As a result of the retest, we found that the same Q / πa 0 2 -ka 0 The graph can be drawn and the scattering parameter a NI The change in a 0 Furthermore, a comparison of the Erginsoy model and the Quisse model revealed that the mobility is independent of both temperature and carrier concentration, while the mobility is affected by both temperature and carrier concentration.

[0084] In one embodiment, the mobility μ determined by the Quisse-type mobility model NI [cm 2 / Vs] is expressed by the following formulas (Q-1) to (Q-26).

[0085]

[0086]

[0087]

[0088] [In formulas (Q-1) to (Q-26), μ NI is the mobility [cm ] determined by the Quisse model. 2 / Vs], N NI is the neutral impurity concentration [cm -3 ], k is the wave vector [cm -1 ], q is the elementary charge [C],

[0089]

[0090] Next, the Debye screening parameter q used in Quisse's paper s It has been found that the formula is difficult to apply to high carrier concentration regions, so the Debye screening parameter q sModified from [C. Kittel, H. Kroemer, "Thermal Physics" Freeman, New York, 2nd ed. (1980) Chap.13 pp.367].

[0091] In one embodiment, the Debye shielding parameter q s is selected from the group consisting of the following formulas (Qq-1) to (Qq-5).

[0092] [In formulas (Qq-1) to (Qq-5), ε 0 is the dielectric constant of vacuum [F / cm], ε r is the relative permittivity (static), k B is the Boltzmann constant [eV / K], T is the temperature [K], n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), N C is the effective density of states [cm -3 ].]

[0093] In one embodiment, q represented by the following formula s is used. [Wherein, e is the elementary charge [C], k B is the Boltzmann constant [eV / K], T is the temperature [K], ε 0 is the dielectric constant of vacuum [F / cm], ε r is the relative dielectric constant (static), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), N c is the effective density of states [cm -3 ].]

[0094] The Debye screening parameter q s By applying the above formula, the Quisse model is 1×10 20 cm -3 It was confirmed that the carrier concentration range can be expanded to about 1000 s. NIAs a result of examining the carrier concentration dependence and temperature dependence of the scattering parameter a NI (the reciprocal of the mobility) to T -3/2 When plotted, the extrapolated values ​​converge to one point. 0 Dependent a NI The experimental results were supported by the Quisse model.

[0095] In addition, 1 x 10 18 cm -3 In the above high carrier concentration region, a NI This result is consistent with the a in Fig. 12(d) in the high carrier concentration region. 0 (n) Although it does not directly explain the change, it is not a deviation from the Erginsoy model, and it is suggested that it can be explained in combination with other scattering factors.

[0096] (6-3) Approximate analytical formulation of the Quisse model for neutral impurity scattering So far, we have described the verification results of the Quisse paper, but when considering the application of the model formula to a simulator, the Quisse model requires a combination of 24 analytical formulas in total to calculate the total scattering cross section Q, and furthermore, numerical calculations are required when calculating mobility, which places constraints on the program that incorporates the model formula. Therefore, we attempted to analytically formulate the mobility by making the behavior of the total scattering cross section Q in the Quisse model an integrable approximate formula. Specifically, we used Q / πa in the Quisse paper. 0 2 -ka 0 Regarding the double logarithmic graph, we consider it as a right-angled trapezoid with a fixed hypotenuse, and as shown in Figure 13, the height D of the upper base is q s a 0 Taking advantage of the fact that it is a function of (n, T), it was incorporated into the integral calculation when calculating the mobility.

[0097] By expanding the equation, a Quisse-type approximate analytical equation represented by the following equation (A3Q-app) was obtained. In one embodiment, the mobility μ determined by the Quisse-type mobility model NI [cm 2 / Vs] can be expressed by the following approximate formula (A3Q-app).

[0098] C is represented by the following formula:

[0099] In one embodiment, the parameters D and k′ in the formula (A3Q-app) 1 can be expressed by the following formulas, respectively.

[0100] (Wherein, e is the elementary charge [C], k B is the Boltzmann constant [eV / K], T is the temperature [K], ε 0 is the dielectric constant of vacuum [F / cm], ε r is the relative dielectric constant (static), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), N C is the effective density of states [cm -3 ]. )] [In the formula, k' 1 is the Q / πa of the Quisse model 0 2 -ka 0 Q / πa in the graph 0 2 = D (upper base of the right-angled trapezoid) and Q / πa 0 2 = 4 (ka 0 ) -3 (Hypotenuse of the right-angled trapezoid) ka at the intersection 0 The value, D, is as defined above.]

[0101] In addition, the approximate formula for D and the Quisse model Q / πa 0 2 -ka 0 The equation for the hypotenuse of a right-angled trapezoid on a graph is The approximation formula may be adjusted depending on the purpose.

[0102] FIG. 14 shows the respective q s a 0 Noka 0 Q / πa at =0 0 2 The value of (Q0 @k ‘ = 0) was obtained from the Quisse model, and each q s a 0 In fact, it was confirmed that the results of the Quisse model and the above approximate analytical formula (A3Q-app) show good agreement. From the above, the neutral impurity scattering parameter a NI It is now possible to express (n) using a Quisse-type approximate analytical formula.

[0103] (6-4) Ionized impurity scattering (degenerate) model As mentioned above, we were able to model the neutral impurity scattering, but the scattering parameter a 0 Of (n), the carrier concentration (3 × 10 17 cm -3 ) The above behavior is difficult to explain solely by neutral impurity scattering. 0 Since (n) is the dominant factor of TFT mobility, it is necessary to investigate scattering models other than those mentioned above and clarify the behavior of all carrier concentration regions. As a result of intensive investigation, it was found that ionized impurity scattering (degenerate) is μ(T) ∝ T 0 It was found that there is a relationship between the above and the scattering mechanism of transparent conductive films, and that there have been many reports of this phenomenon.

[0104] Here, the mobility model of ionized impurity scattering (degenerate) is the Dingle model [RB Dingle, Philos. Mag. 46 831 (1955)], which was generally used, and this was investigated in detail. Furthermore, the screening parameter F II After careful selection, it was found that the best method for this is to use the Pisarkiewicz type [T. Pisarkiewicz, et. al., Thin Solid Films 174 217 (1989)], as with the ionized impurity scattering (non-degenerate) mentioned above.

[0105] In one embodiment, the mobility μ determined by the ionized impurity scattering (degenerate) model II (Deg) [cm 2 / Vs] can be expressed by a Dingle-type mobility model. In one embodiment, the mobility μ determined by the ionized impurity scattering (degenerate) model is II (Deg) [cm 2 / Vs] can be expressed by the following Dingle-type mobility equation (A4D).

[0106]

[0107] On the other hand, there is a concern that ionized impurities may be neutralized as the carrier concentration increases, so when examining the scattering effect, it is necessary to consider the ionized impurities as donors and consider the influence of the energy position and shape of the donor level. 2 Since the carrier concentration is increased by the annealing treatment, in other words, the electrons increase along with the oxygen vacancies, the self-formation process of donors must also be taken into consideration. On the other hand, in the non-degenerate region, there are many ionized donors, and the self-formed donors are fewer than the initial donors, so these effects can be ignored.

[0108] When calculations are performed that take into account the contribution of the neutralization of the donor level and the self-formed donor, it is found that even if the donor level is Gaussian or the donor has no energy level width (hereinafter referred to as a simple donor), by placing the donor level 30 meV or more on the vacuum level side from the CBM (conduction band minimum) and setting an appropriate impurity concentration, a high carrier concentration region (1 × 10 19 cm -3 a in the above area 0 In conclusion, we adopted a model in which a simple donor level, which is easier to handle, exists at a sufficiently high energy level relative to the CBM and does not neutralize, and obtained the following formula (A4-1).

[0109] In one embodiment, the mobility μ determined by the ionized impurity scattering (degenerate) model II (Deg) [cm 2 / Vs] is a Dingle type, and can be expressed by the following mobility equation (A4-1), which takes into account the self-formation process of the donor.

[0110]

[0111] In one embodiment, the shielding function F in the Dingle-type mobility equation (A4D) or (A4-1) II is the shielding function F in Pisarkiewicz-type ionized impurity scattering expressed by the following formula (F): II is.

[0112]

[0113] (6-5) T 0 Verification of the scattering model with dependence Next, T 0 Regarding the scattering model with dependence, the scattering parameter a in FIG. 12(d) is calculated by the approximate analytical formula of the neutral impurity scattering Quisse model obtained so far and the ionized impurity scattering (degenerate) Dingle model adapted to the polycrystalline oxide semiconductor system. 0 We confirmed whether the behavior of (n) can be explained. Specifically, Fig. 15 shows the results of inputting parameters into (A4-S), which is an approximate analytical formula for the neutral impurity scattering Quisse model and the ionized impurity scattering (degenerate) Dingle model, and into the formula (A3Q-app) (A4-1) (A4-S), which is an approximate analytical formula for the neutral impurity scattering Quisse model).

[0114] As shown in Figure 15, the formulas (A3Q-app) and (A4-S) incorporating (A4-1) reproduced the experimental results well. It should be noted that the formula (A3Q-app) exhibited some temperature dependence. Furthermore, the formula (A4-S) exhibited an effective density of states N C (In this system, 2 × 10 18 cm -3 ) is used as a boundary to express the change from degenerate to non-degenerate (in Figure 15, the sigmoid a parameter is set to 2). In any case, by adjusting the parameter, a 0 It was verified that the behavior of (n) can be explained, and that (A4-S), which incorporates the formulas (A3Q-app) and (A4-1), is actually usable.

[0115] In one embodiment, the Dingle mobility formula represented by formula (A4D) or (A4-1) is μ II_Dingle (Deg) [cm 2 / Vs], the mobility μ determined by the ionized impurity scattering (degenerate) model II (Deg) [cm 2 / Vs] can be expressed by the following sigmoid function formula (A4-S) with respect to the carrier concentration n. [In formula (A4-S), N C is the effective density of states [cm -3 ], n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), and a is a parameter that represents the rate of change of the sigmoid function.

[0116] Here, the neutral impurity scattering represented by the formulas (AE3), (Q-1) and (A3Q-app) and the ionized impurity scattering (degenerate) represented by the formulas (A4) and (A4-1) (the T 0 The scattering model having a dependence is expressed by the term a in the above formula (1). 2 T 0 Corresponds to.

[0117] 4. Modeling of intra-grain mobility μ in-grain(T) By using the model formula obtained in the above 3. Physical modeling of various scattering parameters, a model for calculating intra-grain mobility μ in-grain(T) can be constructed.

[0118] In one embodiment, the intra-grain mobility μ in-grain The reciprocal of (T) is 1 / (exp(β / T)-1), T 0 , T -3/2 , T 1/2 , T 3/2 , T 1 , and T 2 and further, the temperature dependence is a function of the carrier concentration n, 1 / μ NI The (T,n) terms are linearly combined.

[0119] In one embodiment, the 1 / μ NI The (T, n) term is expressed by the following formulas (Q-1) to (Q-26) determined by the Quisse mobility model.

[0120]

[0121]

[0122]

[0123] [In formulas (Q-1) to (Q-26), μ NI is the mobility [cm 2 / Vs], N NI is the neutral impurity concentration [cm -3 ], k is the wave vector [cm -1 ], q is the elementary charge [C],

[0124] In one embodiment, the Debye shielding parameter q s is selected from the group consisting of the following formulas (Qq-1) to (Qq-5).

[0125] [In formulas (Qq-1) to (Qq-5), ε 0 is the dielectric constant of vacuum [F / cm], ε r is the relative permittivity (static), k B is the Boltzmann constant [eV / K], T is the temperature [K], n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), N C is the effective density of states [cm -3 ].]

[0126] In one embodiment, the 1 / μ NI The (T, n) term is expressed by the following approximate formula (A5Q-app) determined by the Quisse mobility model.

[0127] C is represented by the following formula:

[0128] In one embodiment, the effective mass m* can be expressed by either of the following formulas (M-1) and (M-2).

[0129] In one embodiment, the parameters D and k′ in the formula (A5Q-app) 1 can be expressed by the following formulas, respectively.

[0130]

[0131] (Wherein, e is the elementary charge [C], k B is the Boltzmann constant [eV / K], T is the temperature [K], ε 0 is the dielectric constant of vacuum [F / cm], ε r is the relative dielectric constant (static), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), N C is the effective density of states [cm -3 ]. )] [In the formula, k' 1 is the Q / πa of the Quisse model 0 2 -ka 0 Q / πa in the graph 0 2 = D (upper base of the right-angled trapezoid) and Q / πa 0 2 = 4 (ka 0 ) -3 (Hypotenuse of the right-angled trapezoid) ka at the intersection 0 The value, D, is as defined above.]

[0132] In addition, the approximate formula for D and the Quisse model Q / πa 0 2 -ka 0 The equation for the hypotenuse of a right-angled trapezoid on a graph is The approximation formula may be adjusted depending on the purpose.

[0133] In one embodiment, in the following formula (1-1), the intragranular mobility μ in-grain As the reciprocal of (T), 1 / (exp(β / T)-1), T 0 , T -3/2 , T1/2 and T 3/2 and 1 / μ, the temperature dependence of which is a function of carrier concentration n. NI Use the (T, n) term.

[0134] [In formula (1-1), μ in-grain is the mobility within the semiconductor grains [cm 2 / Vs], T is temperature [K], β[K], a 1 [cm -2 Vs], a 2 [cm -2 Vs], a 3 [cm -2 Vs. K 3/2 ], a 4 [cm -2 Vs. K -1/2 ], and a 5 [cm -2 Vs. K -3/2 ] respectively represent coefficients. However, in the above formula (1-1), 1 / (exp(β / T)-1) and T 0 , T -3/2 , T 1/2 and T 3/2 The coefficient a of the unselected term 1 ~a 5 is set to 0.]

[0135] In one embodiment, a in the formula (1-1) 2 T 0 In one embodiment, the term a in the formula (1-1) can be expressed by the neutral impurity scattering model. 2 T 0 In one embodiment, the term a in the formula (1-1) can be expressed by the ionized impurity scattering (degenerate) model. 2 T 0 The term can be expressed by any of the above ionized impurity scattering (degenerate) models, and 1 / μ NI The (T, n) term can be expressed by any of the neutral impurity scattering models described above.

[0136] In one embodiment, the reciprocal of the intra-grain mobility μ in-grain(T) of the semiconductor expressed by the formula (1) can be expressed by the following formula (A1-1): [In formula (A1-1), μ OP is as defined in the formula (A2) or (A2-2), and μ NI is as defined in the formula (A3E), (Q-1), or (A3Q-app), and μ II (Deg) is as defined in the formula (A4), (A4-1), or (A4-S), and μ II (nonDeg) is as defined in the formula (A5-CW), (A5-BH), or (A5-S).

[0137] In one embodiment, the formula (1-1) can be expressed by the following formula (A1-2): [In formula (A1-2), μ OP is as defined in the formula (A2) or (A2-2), and μ II (Deg) is as defined in the formula (A4D), (A4-1), or (A4-S), and μ II (nonDeg) is as defined in the formula (A5-CW), (A5-BH), or (A5-S), and μ NI (T, n) are as defined in the formula (A3E), (Q-1), or (A3Q-app).

[0138] In one embodiment, μ in formula (A1-2) OP is the formula (A2-2), and μ II (Deg) is the formula (A4-1) or (A4-S), and μ II (nonDeg) is the formula (A5-BH) or (A5-S), and μ NI (T, n) is represented by the formula (A3E), (Q-1), or (A5Q-app).

[0139] In one embodiment, the mobility μ determined by the ionized impurity scattering (degenerate) model represented by the formula (A4D) or (A4-1) II (Deg) and the mobility μ determined by the ionized impurity scattering (non-degenerate) model represented by the formula (A5-CW) or (A5-BH) II(nonDeg) For carrier concentration n, the effective density of states N C are linearly combined with a sigmoid function with the boundary, and each shielding function F II is a Pisarkiewicz type F represented by the formula (F) II is.

[0140] 5. Modeling of Macroscopic DC Mobility μ(T) By using the intragrain mobility μ in-grain(T) of a semiconductor obtained by the above formula (1), (1-1), (A1-1), or (A1-2), it is possible to calculate the macroscopic DC mobility μ(T) of a semiconductor expressed by the following formula (A10).

[0141] In one embodiment, the macroscopic DC mobility μ(T) of the semiconductor can be calculated by the following formula (A10): 2 ] is 0. [In formula (A10), q is the elementary charge [C], V B is the grain boundary barrier height [eV], k is the wave vector [cm -1 ], T is temperature [K], μ in-grain (T) is the intra-grain mobility of the semiconductor [cm 2 / Vs].

[0142] In one embodiment, V in formula (10A) B is expressed by the following formula (A11).

[0143] In one embodiment, the mobility μ in formula (A10) in-grain The reciprocal of (T) can be expressed by any of the above formulas (1-1), (A1-1) and (A1-2).

[0144] In this specification, q (elementary charge 1.602 x 10 -19 [C]) is the same as the above e (elementary charge [C]).

[0145] It will be demonstrated in the examples described later that the intragrain mobility μ in-grain(T) of a semiconductor calculated by the above formula (A-1) and the macroscopic DC mobility μ(T) of a semiconductor calculated by the above formula (A10) are in good agreement with the actual measured values ​​of a measurement sample.

[0146] 6. Device Simulation Method A device simulation method for calculating the macroscopic DC mobility μ(T) of a semiconductor according to one aspect of the present invention is characterized by including a step of using the method for calculating the macroscopic DC mobility μ(T) of a semiconductor according to one aspect of the present invention described above.

[0147] By using the device simulation method of this aspect, it is possible to perform highly reliable device design before actually fabricating a semiconductor device.

[0148] (Simulation Service) By using the device simulation method of this aspect, it is possible to provide a simulation service that accepts input of necessary physical property values ​​from a customer and presents the simulation results to the customer.

[0149] 7. Thin Film Transistor Manufacturing Method A thin film transistor manufacturing method according to one aspect of the present invention is characterized by comprising the steps of: calculating the macroscopic DC mobility μ(T) of a semiconductor using the method for calculating the macroscopic DC mobility μ(T) of a semiconductor according to the above-described aspect of the present invention; and manufacturing a thin film transistor based on the calculated macroscopic DC mobility μ(T) of the semiconductor.

[0150] Furthermore, a method for manufacturing a thin film transistor according to one aspect of the present invention is characterized by comprising the steps of: calculating a macroscopic DC mobility μ(T) of a semiconductor using the device simulation method according to the aspect of the present invention; and designing a device based on the calculated macroscopic DC mobility μ(T) of the semiconductor.

[0151] By calculating the macroscopic DC mobility μ(T) of a semiconductor using the above-described method for calculating the macroscopic DC mobility μ(T) of a semiconductor according to one embodiment of the present invention or the device simulation method, a thin film transistor having a desired mobility can be efficiently manufactured.

[0152] 8. Electronic Device An electronic device according to an aspect of the present invention is characterized by including a thin film transistor manufactured using the method for manufacturing a thin film transistor according to the aspect of the present invention described above.

[0153] 9. Program for calculating macroscopic DC mobility μ(T) of semiconductor The program for calculating the macroscopic DC mobility μ(T) of a semiconductor according to one embodiment of the present invention (hereinafter, sometimes abbreviated as "macroscopic DC mobility calculation program") is a program for calculating the macroscopic DC mobility μ(T) of a semiconductor according to one embodiment of the present invention, using the following formulas (1) and (10):

[0154] [In formula (1), μ in-grain is the mobility within the semiconductor grains [cm 2 / Vs], T is temperature [K], β[K], a 1 [cm -2 Vs], a 2 [cm -2 Vs], a 3 [cm -2 Vs. K 3/2 ], a 4 [cm -2 Vs. K -1/2 ], and a 5 [cm -2 Vs. K -3/2 ] respectively represent coefficients. However, in the above formula (1), 1 / (exp(β / T)-1) and T 0 , T -3/2 , T 1/2 and T 3/2 Using two or more terms selected from the group consisting of: 1 ~a 5 is set to 0.] [In formula (10), μ is the mobility of the semiconductor [cm 2 / Vs], T is temperature [K], γ[K] and θ[K 2 ] is a coefficient and a positive number including 0, μ in-grain(T) is the intra-grain mobility μ of the semiconductor according to one embodiment of the present invention described above. in-grain The mobility in the semiconductor grains [cm 2 / Vs].] and the computer is used to calculate the temperature T [K] and the carrier concentration n [cm -3 a means for receiving an input of the type of material of the semiconductor; and a coefficient a 1 ~a 5 , β, γ, and θ; and calculating the macroscopic DC mobility μ(T) of the semiconductor using the formulas (1) and (10).

[0155] Details of the coefficients in the formula (1) are as explained in the method for calculating intragranular mobility according to one embodiment of the present invention, and details of the coefficients in the formula (10) are as explained in the method for calculating macroscopic DC mobility according to one embodiment of the present invention, and therefore will not be explained here.

[0156] A macro DC mobility calculation program according to one embodiment will be described with reference to FIG.

[0157] 5 is a flow chart showing the operation procedure of one embodiment of the present invention. First, in step S1, the temperature T [K] and the carrier concentration n cm -3 ] is input into the computer. Next, in step S2, the type of semiconductor material is input into the computer. The type of semiconductor material to be input here is selected from a database. The database used here is constructed by inputting actual measured values ​​corresponding to the type of semiconductor material and performing calculations to accumulate data. The type of material to be selected includes the semiconductor composition, crystalline state (amorphous, single crystal, polycrystalline, etc.), crystalline structure (space group, lattice constant, and atomic coordinates), etc.

[0158] In step S3, the computer selects the values ​​of the coefficients in the formula (1) based on the data input in steps S1 and S2. Here, the coefficients in the formula (1) refer to all the coefficients in the formulas (1) to (5) and (5-1) to (5-3). Specifically, the coefficient a 1 ~a5 In step S4, the values ​​of the coefficients selected in step S3 are substituted into the formula (1), and the computer calculates the mobility μ in-grain Calculate (T).

[0159] In step S5, the coefficients γ[K] and θ[K] in the formula (10) are calculated based on the type of material input in step S2. 2 Finally, in step S6, the values ​​of the coefficients selected in step S5 are substituted into the above equation (10), and the computer calculates and outputs the macroscopic DC mobility μ(T) of the semiconductor, and the flow ends.

[0160] In one embodiment, a program for causing a computer to function as a means for calculating a macroscopic DC mobility μ(T) of a semiconductor is a program for calculating a macroscopic DC mobility μ(T) of a semiconductor using the formula (1-1), (A1-1) or (A1-2), and the formula (A10), and includes causing the computer to: -3 a means for receiving an input of the type of material of the semiconductor; and a coefficient a 1 ~a 5 , β, γ, and θ; and calculating the macroscopic DC mobility μ(T) of the semiconductor using the formulas (1-1), (A1-1) or (A1-2), and (A10).

[0161] 10. Program for deriving macroscopic DC mobility μ(T, n) of semiconductor Temperature T [K] and carrier concentration n [cm -3 ], the macroscopic DC mobility μ(T, n) [cm 2 The program for deriving μ(T, n) for T and n measured from a semiconductor film (hereinafter, sometimes abbreviated as "derivation program") includes a computer, a means for receiving input of data on μ(T, n) for T and n measured from a semiconductor film, a means for receiving input of the type of semiconductor material for obtaining initial values ​​of each coefficient in the formula (1), and a coefficient a 1 ~a 5, β, γ, and θ; and deriving the macroscopic DC mobility μ(T, n) by regression using a program for calculating the macroscopic DC mobility μ(T) of the semiconductor of one embodiment of the present invention.

[0162] In one embodiment, the temperature T [K] and the carrier concentration n [cm -3 ], the macroscopic DC mobility μ(T, n) [cm 2 The program for deriving the macroscopic DC mobility μ(T, n) causes a computer to function as a means for deriving the macroscopic DC mobility μ(T, n) by performing regression using: a means for accepting input of data on μ(T, n) for T and n measured from a semiconductor film; a means for accepting input of the type of semiconductor material for obtaining initial values ​​of each coefficient in the formula (1-1) or (A1-2); and a program for calculating the macroscopic DC mobility μ(T) of the semiconductor.

[0163] According to the derivation program of this embodiment, the carrier concentration n [cm -3 ] and the temperature T [K] at the time of measurement, the macroscopic DC mobility of the semiconductor can be predicted. Another example of using the derivation program of this embodiment is to derive the contribution of each scattering parameter and potential barrier to the mobility by regressing the actually measured mobility and the predicted mobility.

[0164] Furthermore, by incorporating the derivation program of this embodiment into a device simulation program, it is possible to predict the voltage-current characteristics when the device is operating. Also, by regressing the predicted results of the device simulation with the current-voltage characteristics of the device that are actually measured, it is possible to calculate the contribution of each scattering parameter and potential barrier to the mobility.

[0165] A program for deriving macroscopic DC mobility μ(T) in one embodiment will be described with reference to FIG. 6. First, in step S11, the carrier concentration n [cm -3 ], and the mobility μ obs. [cm -3] are input into the computer. The carrier concentration and mobility input here are data measured for each thin film sample using the Hall effect at the measurement temperature T [K]. In step S12, the type of semiconductor material from which the initial values ​​of each coefficient in equation (1) are obtained is input into the computer. In step S13a, the computer selects the initial values ​​of each coefficient in equation (1) from a database based on the type of semiconductor material input in step S12. Note that the database used here is constructed by inputting actual measured values ​​corresponding to the type of semiconductor material and performing calculations to accumulate data. If the corresponding type of semiconductor material is not in the database, an arbitrary value is input into the computer in step S13b. The coefficients in equation (1) include all of the coefficients in equations (2) to (5) and (5-1) to (5-3) related to equation (1).

[0166] Next, the computer substitutes the initial values ​​of the coefficients of the formula (1) selected in step S13a or any values ​​of the coefficients input in step S13b into the formula (1), and calculates the macroscopic DC mobility μ(T) of the semiconductor according to the above-described one embodiment in steps S4 to S6. (Hereinafter, the calculated values ​​obtained will be referred to as "mobility μ calc (T)

[0167] In step S14, the actually measured mobility (hereinafter referred to as mobility μ obs. ) and the mobility μ obtained by executing steps S4 to S6 on a computer. calc The variables in the formulas (1) to (13) are used as fitting parameters to perform fitting by the least squares method so that the sum of the squares of the errors in (T) is minimized. Here, in step S14, room temperature values ​​are used for the carrier concentrations in the formulas (3) to (5) and (13).

[0168] Next, in step S15, the computer determines whether the values ​​of each parameter have converged. If the computer determines that they have not converged, the process proceeds to step S16, where the values ​​of each coefficient in equation (1) are updated and steps S4 to S6 and S14 are repeated, and the computer determines whether the values ​​of each parameter have converged in step S15. Steps S16, S4 to S6, and S14 to S15 are repeated until the computer determines that the values ​​of each parameter have converged in step S15.

[0169] In step S15, if the computer determines that the values ​​of the parameters have converged, the process proceeds to step S17, where the computer outputs the values ​​of the parameters in the formulas (1) to (13). obs. and the macroscopic DC mobility μ of the semiconductor calc Coefficient of determination R for (T) 2 The computer calculates this and the flow ends.

[0170] By executing a regression such as that shown in FIG. 6 on a computer, it becomes possible to obtain a calculated value of the macroscopic DC mobility μ(T) of a semiconductor with higher accuracy, that is, with higher reproducibility.

[0171] (Method of calculating mobility - machine learning) Temperature T [K] and carrier concentration n [cm -3 ], the calculation method of the macro DC mobility μ (T, n) that depends on the temperature T [K] and carrier concentration n [cm -3 ] can be input to obtain the optimum macro DC mobility.

[0172] Using machine learning, the temperature T [K] and carrier concentration n [cm -3 The method for calculating the macroscopic DC mobility μ(T, n) of a semiconductor that depends on [T, n] is to use machine learning on the data of μ(T, n) for T and n actually measured from a semiconductor film, and calculate it using a non-parametric model that does not assume a mathematical model.

[0173] In one embodiment, in the calculation using the nonparametric model, the objective variable is μ(T, n), and the explanatory variables are temperature T and carrier concentration n, and the calculation is performed by regression.

[0174] In one embodiment, the regression is performed by a method selected from the group consisting of Gaussian process regression, linear regression, Ridge regression, LASSO regression, Elastic Net regression, Random Forest regression, Support Vector Machine regression, SGD regression, Quadratic regression, and derivatives thereof. In one embodiment, the regression is performed by Gaussian process regression.

[0175] A machine learning flow of a method for calculating macroscopic DC mobility μ(T, n) in one embodiment will be described with reference to FIG. 7. First, in step S21, the carrier concentration n [cm -3 ], and the mobility μ obs. [cm -3 The carrier concentration and mobility input here are data measured for each thin film sample using the Hall effect at the measurement temperature T [K]. Next, the carrier concentration n [cm -3 ], and the mobility μ obs. [cm -3 ] is used to perform machine learning using a machine learning flow. Because the machine learning algorithm uses a nonparametric model that combines polynomials, Gaussian functions, sigmoid functions, etc., the mathematical model for the mobility's dependence on T and n is not self-evident. For this reason, the trained model is a black box (hereinafter, a black box machine learning model will be referred to as a "black box flow").

[0176] Next, in step S22, a machine learning algorithm and hyperparameters (constants used within the model of the algorithm) are selected and input. If no algorithm is selected, the computer determines to use a Gaussian process regression as the initial value of the algorithm. In step S23, the selected and input or determined machine learning algorithm is used to calculate the mobility μ obs.The objective function is set as follows: the carrier concentration at room temperature and the measurement temperature are used as descriptors. Machine learning is performed by dividing the data into training data and validation data. In this case, there is no obvious mathematical model, and the computer performs the calculations using machine learning.

[0177] In step S24, the computer determines whether the learning model has predictive performance (generalization performance) and whether the actual measured values ​​and the calculation results match by using an evaluation index to determine whether there is a large difference in the evaluation index between the training data and the validation data. The evaluation indexes for determining whether the actual measured values ​​and the calculation results match include the maximum absolute error (MAE), the mean squared error (MSE), and the coefficient of determination R 2 etc. Steps S22 to S24 are repeated until the agreement between the actual measurement value and the calculation result reaches a predetermined tolerance (i.e., a certain error range). When the determination is made using the maximum absolute error MAE, the "predetermined tolerance" is, for example, a range of 10% or less of the mobility. The flow ends when the agreement between the actual measurement value and the calculation result reaches the predetermined tolerance. The flow of steps S21 to S23 is called the learning period.

[0178] Next, a step of utilizing the machine learning program that has undergone the learning period will be described. In step 31, the carrier concentration n [cm] at room temperature and the measurement temperature T [K] for each thin film sample is calculated. -3 ], mobility μ obs. [cm -3 ], the computer calculates the macroscopic DC mobility μ(T) of the semiconductor in step 23, and outputs the calculated value, thereby completing the flow.

[0179] By using a computer to perform machine learning, it becomes possible to obtain a more accurate calculated value of the macroscopic DC mobility μ(T) of a semiconductor.

[0180] The present invention will be specifically described below based on examples, but the present invention is not limited to these examples in any way.

[0181] (A-1) Preparation of Semiconductor Thin Film Specimens for Measurement Specimen 1 Using an oxide target having the metal composition ratio shown in Table 1, an oxide layer was formed on a glass substrate by sputtering under the film formation conditions shown in Table 1, aiming for a film thickness of 30 nm. The oxide target and metal composition ratio (at %) were calculated using the following formula: [In] / ([In]+[M])*100 (where [In] represents the number of moles of In in the oxide target, and [M] represents the number of moles of metal elements other than In in the oxide target). Next, a first heat treatment (first annealing) was performed under the conditions shown in Table 1 to prepare Specimen 1. The crystallinity of the obtained Specimen 1 was evaluated by XRD measurement. The results are shown in Table 1. Thereafter, a second heat treatment (second annealing) was performed under conditions 1 to 5 shown in Table 1 to obtain Specimens 1-1 to 1-5.

[0182] Specimen 2 was prepared in the same manner as Specimen 1, except that the composition of the oxide target, the film formation conditions, and the conditions for the first annealing were changed, and the crystallinity was evaluated. Thereafter, a second heat treatment (second annealing) was carried out in the same manner as Specimen 1, and Specimens 2-1 to 2-5 were obtained.

[0183]

[0184] (A-2) Measurement of Physical Properties of Semiconductor Thin Film for Measurement The following physical properties were measured for each of the obtained samples.

[0185] (carrier concentration [cm -3 ], and the mobility μ obs. [cm 2 / Vs]) Carrier concentration of semiconductor thin film (cm -3 ), and the mobility μ obs. [cm 2 To evaluate the electrical properties, resistivity measurements using the van der Pauw method and Hall effect measurements (AC Hall effect measurements) were used. For the measurements, thin film samples cut to 1 cm square were used with Ti electrodes formed at the four corners, and AC Hall measurements were performed on each sample at 50 K intervals over a temperature range of 20 to 300 K. The measurement conditions are as follows: - Measurement device: Resitest 8400 manufactured by Toyo Corporation - Maximum applied voltage: 20 V - Applied magnetic field: 0.4 T

[0186] Examples 1 and 2 For the samples 1 and 2 obtained above, the macroscopic DC mobility μ(T) according to one embodiment of the present invention was calculated.

[0187] (B) Intragranular mobility μ in-grain Calculation of (T) Using the above formula (1) and formula (2), the mobility μ in-grain (T) was calculated. Here, each A for each carrier concentration neutral、 A op、 The weak localization constant and the acoustic phonon scattering constant were calculated using the values ​​shown in Table 2 below and the formulas (3), (4), and (5) for the value of n (300 K). in-grain The values ​​of the parameters used in calculating (T) are shown in Table 2 below.

[0188] (C) Calculation of macroscopic DC mobility μ (T) For calculation of macroscopic DC mobility μ (T) for each temperature T and carrier concentration n, the intra-grain mobility μ calculated above is in-grain (T), the potential barrier V B The values ​​calculated using the values ​​shown in Table 2 and equation (13) were used. obs. When the agreement between the macroscopic DC mobility μ(T) and the ρ(T) was poor, regression was performed using the nonlinear least squares method, and convergence was confirmed by repeating the fitting multiple times without any change, and the parameters were used as experimental results. The values ​​of each parameter used in calculating the macroscopic DC mobility μ(T) are shown in Table 2 below.

[0189] Comparative Examples 1 and 2 For the above specimens 1 and 2, the mobility μ d was calculated.

[0190] (D) Mobility μ by Tokyo Model d Calculation of mobility μ by Tokyo Model for each temperature T and carrier concentration n d [cm 2 / Vs] was calculated using the following formulas (I) and (II). where n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), T is the temperature [K], and μ d0 [cm 2 / Vs], n cr [cm -3 ], T γ [K], γ 0 is a coefficient.

[0191] Actual measured value μ obs. and mobility μ by Tokyo Model d In cases where the agreement was poor, regression was performed using the nonlinear least squares method, and convergence was confirmed by repeating the fitting multiple times without any change, and the parameters were then used as experimental results. d The values ​​of each parameter used in the calculation are shown in Table 3 below.

[0192] (E) Evaluation of the calculation results (R 2 Coefficient of determination) The actual measured value μ of the mobility obtained in (A-2) above obs. and the macroscopic DC mobility μ (T) calculated in (C) above, or the mobility μ calculated by the Tokyo Model in (D) above, 2 was calculated using the following formula (X). The obtained coefficient of determination R 2 The values ​​are shown in Tables 2 and 3 below, respectively.

[0193]

[0194] The horizontal axis shows the actual measured value of macro DC mobility μ obs. The vertical axis is the macroscopic DC mobility μ calculated using each model. calc When plotting, the coefficient of determination R 2 The closer to 1, the more appropriate the model used is. In the table, "E" is an exponential notation, and the integer after "E" represents the power of 10 applied to the value. For example, "4.60E-2" is 4.60 x 10 -2 Represents.

[0195]

[0196]

[0197] In addition, the actual measured value μ of the mobility of each sample relative to the carrier concentration n obs. 1a to 4a are graphs plotting the relationship between the calculated mobility values ​​obtained in Examples and Comparative Examples and the measured mobility values ​​μ of each sample on the horizontal axis. obs. , the vertical axis represents the calculated mobility value μ calc Graphs plotting these are shown in Figures 1b to 4b, respectively. It can be seen from Figures 1 to 4 that the mobility calculation values ​​using the Tokyo Model (Comparative Examples 1 and 2) showed some discrepancy with the measured values, whereas the values ​​calculated using the method for calculating macroscopic DC mobility μ(T) of the present invention (Examples 1 and 2) showed good agreement for both crystalline oxide semiconductors and amorphous oxide semiconductors, demonstrating high reproducibility.

[0198] <Verification of Mobility Model> (F-1) Measurement Semiconductor Thin Film Specimens 3 to 8 Thin films were prepared and their crystallinity was evaluated in the same manner as for Specimen 1, except that the oxide target composition, film formation conditions, and first annealing conditions were changed as shown in Tables 4-1 to 4-3 below. Thereafter, a second heat treatment (second annealing) was carried out in the same manner as for Specimen 1, resulting in Specimens 3 to 8.

[0199]

[0200]

[0201]

[0202] A graph plotting the mobility-carrier concentration of each sample is shown in Figure 9. Also, Figure 10 shows an EBSD orientation map (Electron Backscatter Diffraction Pattern IPF Map) showing the crystal grain size and crystal orientation of each sample.

[0203] (F-2) Measurement of Physical Properties of Semiconductor Thin Film for Measurement The following physical properties were measured for each of the obtained samples.

[0204] (carrier concentration [cm -3 ], and the mobility μ obs. [cm 2 / Vs]) Carrier concentration of semiconductor thin film (cm -3 ), and the mobility μobs. [cm 2 To evaluate the electrical properties of the thin film samples, resistivity measurements using the van der Pauw method and Hall effect measurements (AC Hall effect measurements) were used. For the measurements, thin film samples cut to 1 cm square were used with Ti electrodes formed at the four corners, and AC Hall measurements were carried out for each sample at temperatures ranging from 20 to 300 K every 50 K. The measurement conditions are as follows: - Measurement device: Resitest 8400 manufactured by Toyo Corporation - Maximum applied voltage: 20 V - Applied magnetic field: 0.4 T

[0205] (G) Calculation of Macroscopic DC Mobility μ(T) <Examples 3 to 8> Using the group of equations (mobility model equations) shown in Tables 5-1 and 5-2 below described in the detailed description, and inputting the fitting parameters shown in Table 6 below, mobility-carrier concentration lines (μ-n lines) for each scattering parameter at temperatures of 200.0 K, 250.0 K, and 300.0 K were obtained. These lines are shown in FIG. 16 together with plots of the measured values ​​for Samples 3 to 8.

[0206]

[0207] Note: In Table 5-1, μ on the left side of formula (A4-1) and formula (A4-S) II (Deg) Since the notation is the same, the left side of the formula (A4-1) is μ' II (Deg) Similarly, the left side μ of the formula (A5-BH) and the formula (A5-S) II (non(Deg) Since the notation is the same, the left side of the formula (A5-BH) is μ' II (nonDeg) It was distinguished by notation.

[0208] Note: In Table 6, Z is the ionic valence of the ionized impurity, but in the above table, the ionic valence (degenerate) is represented as Z and the ionic valence (non-degenerate) is represented as Z'.

[0209] 16(a) to 16(f) show that the values ​​calculated by the method for calculating macroscopic DC mobility μ(T) using a physical model according to the present invention are in good agreement both in the case of polycrystalline oxide semiconductors and in the case of amorphous oxide semiconductors, and are highly reproducible.

[0210] Similar to FIG. 16, FIG. 17 shows the mobility-carrier concentration curves at 300 K obtained by inputting the parameters in Table 7 below into the formula list in Table 5 above. The upper limit values ​​of each plot of mobility-carrier concentration for polycrystalline oxide semiconductor materials are well reproduced. FIG. 18 shows the μ and μ at each carrier concentration when FIG. 17 was obtained. OP , μ NI , μ II (Deg) , and μ II (nonDeg) The scattering rate of each scattering parameter was calculated by using the above formula. The scattering rate S of each scattering parameter is μ / μ x where μ x is μ OP , μ NI , μ II (Deg) , μ II (nonDeg) and μ GB Here, the mobility at the grain boundary (GB) μ GB is the V from the macroscopic DC mobility μ B The mobility reduction due to the GB was defined.

[0211] Note: In Table 7, Z is the ionic valence of the ionized impurity, but in the above table, the ionic valence (degenerate) is represented as Z and the ionic valence (non-degenerate) is represented as Z'.

[0212] (H) Calculation of Scattering Rate A graph in which the carrier concentration of each sample is plotted on the horizontal axis and the scattering rate of each scattering parameter is plotted on the vertical axis is shown in Figure 18. As the mobility model has been clarified in this way, it has become possible to visualize the scattering rate, which is the degree of influence of each scattering factor at each carrier concentration.

[0213] The macroscopic DC mobility calculation method and calculation program according to one aspect of the present invention are useful as simulation means in the device design of semiconductor devices that use crystalline oxide thin films containing In as a main component.

[0214] Although several embodiments and / or examples of the present invention have been described in detail above, those skilled in the art will readily be able to make numerous modifications to these exemplary embodiments and / or examples without substantially departing from the novel teachings and advantages of the present invention. Accordingly, these numerous modifications are within the scope of the present invention. The contents of all documents cited in this specification and of the applications from which this application claims priority under the Paris Convention are incorporated by reference in their entirety.

Claims

1. Mobility in semiconductor grains μ in-grain A method for calculating the mobility μ (T) within a grain when the temperature T [K] is a fluctuation factor in-grain The reciprocal of (T) is 1 / (exp(β / T)-1), T 0 , T -3/2 , T 1/2 , T 3/2 , T 1 , and T 2 Mobility μ within the grains of a semiconductor, expressed as a linear combination of two or more terms selected from the group consisting of in-grain A method for calculating (T). [Here, β[K] is a coefficient.] 2. In the following formula (1), the mobility in the grain μ in-grain As the reciprocal of (T), 1 / (exp(β / T)-1), T 0 , T -3/2 , T 1/2 and T 3/2 The intragranular mobility μ of the semiconductor according to claim 1 is determined by using two or more terms selected from the group consisting of in-grain Method for calculating (T). [In formula (1), μ in-grain is the mobility in the grains of the semiconductor [cm 2 / Vs], T is temperature [K], β[K], a 1 [cm -2 Vs], a 2 [cm -2 Vs], a 3 [cm -2 Vs.K. 3/2 ], a 4 [cm -2 Vs.K. -1/2 ], and a 5 [cm -2 Vs.K. -3/2 In the above formula (1), 1 / (exp(β / T)−1) and T 0 , T -3/2 , T 1/2 and T 3/2 The coefficient a of the term not selected 1 ~a 5 is set to 0.] 3. The intragranular mobility μ according to claim 1 or 2, wherein β[K] is expressed by the following formula (2): in-grainMethod for calculating (T). [In formula (2), hω op / 2π is the energy of the optical phonon [eV] that varies depending on the carrier concentration, k B is the Boltzmann constant (8.617 x 10 -5 [eV / K]), h is Planck's constant (4.1357×10 -15 [eVs]).

4. The above a. 1 [cm -2 Vs] is the carrier concentration n [cm -3 ], the coefficient a 1 (n), wherein a 1 The intragranular mobility μ of the semiconductor according to claim 2 or 3, wherein (n) is represented by the following formula (3): in-grain Method for calculating (T). [In formula (3), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), A 1 [cm -2 Vs], B 1 , and C 1 [cm -2 Vs] are the coefficients, N 01 Is 1 (n) is the carrier concentration corresponding to the inflection point in formula (3).

5. Section A above 1 is 0 cm -2 Vs or more 0.1cm -2 Vs or less, and 1 is 0 or more, 1 is 1 cm -2 Vs or less, and 01 is 1 x 10 18 cm -3 Above 1 x 10 23 cm -3 The intragranular mobility μ according to claim 4, in-grain Method for calculating (T).

6. The above a. 2 [cm -2 Vs] is the carrier concentration n [cm -3 ], the coefficient a 2(n), wherein a 2 The intragranular mobility μ of the semiconductor according to any one of claims 2 to 5, wherein (n) is represented by the following formula (4): in-grain Method for calculating (T). [In formula (4), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), A 2 [cm -2 Vs], B 2 , and C 2 [cm -2 Vs] are the coefficients, N 02 Is 2 (n) is the carrier concentration corresponding to the inflection point in formula (4).

7. Section A above 2 is 0.005 cm -2 Vs or more 0.5cm -2 Vs or less, and 2 is 1000 or less, 2 is 1 x 10 -1 cm -2 Less than Vs - and said N 02 is 1 x 10 17 cm -3 Above 1 x 10 22 cm -3 The intragranular mobility μ according to claim 6 is equal to or less than in-grain Method for calculating (T).

8. The above a. 3 [cm -2 Vs.K. 3/2 ] is the carrier concentration n [cm -3 ], the coefficient a 3 (n), wherein a 3 The intragranular mobility μ of the semiconductor according to any one of claims 2 to 7, wherein (n) is represented by the following formula (5): in-grain Method for calculating (T). [In formula (5), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), A 3 [cm -8 Vs.K.3/2 ] and B 3 , C 3 [cm -2 Vs.K. 3/2 ], D 3 [cm 3 ] and F 3 [cm -2 Vs.K. 3/2 ] are the coefficients, N 03 Is 3 The maximum carrier concentration [cm -3 ] 9. Section A above 3 But, 10 -39 cm -8 Vs.K. 3/2 More than 10 -33 cm -8 Vs.K. 3/2 The above B 3 is 1 or more and 5000 or less, 3 is 10 4 cm -2 Vs.K. 3/2 is less than D 3 is 10 -20 cm 3 The above and F 3 is 500 cm -2 Vs.K. 3/2 is less than N 03 is 1 x 10 16 cm -3 Above 1 x 10 20 The intragranular mobility μ according to claim 8, in-grain Method for calculating (T).

10. The above a. 3 is the carrier concentration n [cm -3 ], the coefficient a 3 (n), where N 03 [cm -3 ] and N 13 [cm -3 ] is an arbitrary carrier concentration, 3 (n) is n<N 03 In this case, it is expressed by the following formula (5-1), and N 03 ≦n≦N 13 When n>N, it is expressed by the formula (5-2). 13When the above formula (5-3) is used, the intragranular mobility μ of the semiconductor according to claim 8 or 9 is expressed by the following formula (5-3). in-grain Method for calculating (T). [In the formulas (5-1), (5-2) and (5-3), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), A' 3 [cm -8 Vs.K. 3/2 ], C' 3 [cm -2 Vs.K. 3/2 ] and D' 3 [cm 3 ] are coefficients, B' 3 [cm -2 Vs.K. 3/2 ] is a constant.

11. The above A' 3 But, 10 -39 cm -8 Vs.K. 3/2 More than 10 -33 cm -8 Vs.K. 3/2 and C' is the same as above. 3 is 5000 cm -2 Vs.K. 3/2 is equal to or less than D' 3 is 10 -20 cm 3 The intragranular mobility μ according to claim 10 is equal to or greater than the above. in-grain Method for calculating (T).

12. The above a. 4 [cm -2 Vs.K. -1/2 12. The intragranular mobility μ of the semiconductor according to claim 2, wherein μ is a coefficient that varies depending on the carrier concentration. in-grain Method for calculating (T).

13. The above a. 5 [cm -2 Vs.K. -3/2 13. The intragranular mobility μ of the semiconductor according to claim 2, wherein μ is a coefficient that varies depending on the carrier concentration. in-grain Method for calculating (T).

14. The semiconductor is a non-degenerate semiconductor, and1 is the optical phonon scattering constant A op [cm -2 Vs], the above a 2 is the neutral impurity scattering coefficient A neutral [cm -2 Vs.K. 3/2 ], the a 3 is the ionized impurity scattering coefficient A ion [cm -2 Vs.K. -1/2 ], the a 4 is the weak localization constant [cm -2 VsK -1/2 ], the a 5 is the acoustic phonon scattering constant [cm -2 Vs.K. -3/2 The intragranular mobility μ in-grain Method for calculating (T).

15. The coefficient of the 1 / (exp(β / T)-1) term is a 1 [cm -2 Vs], and the mobility μ determined by the optical phonon scattering model OP The mobility μ determined by the optical phonon scattering model OP [cm 2 The intragranular mobility μ of the semiconductor according to claim 1, wherein the reciprocal of [Vs] is represented by the following formula (A2): in-grain Method for calculating (T). [In formula (A2), T is temperature [K], and β [K] is a coefficient.] 16. The intragranular mobility μ of the semiconductor according to claim 15, wherein the coefficient β[K] can be expressed by the following formula: in-grain Method for calculating (T).

17. The coefficient a 1 [cm -2 The intragranular mobility μ of the semiconductor according to claim 15, wherein Vs] can be expressed by the following formula (A2-1): in-grain Method for calculating (T).

18. Mobility μ determined by the optical phonon scattering model OP [cm 2 The intragranular mobility μ of the semiconductor according to claim 15, wherein the intergranular mobility μ in-grainMethod for calculating (T).

19. T 0 The coefficient of the term is a 2 [cm -2 Vs], and the mobility μ determined by the neutral impurity scattering model NI [cm 2 / Vs] reciprocal 1 / μ NI , and the mobility μ determined by the ionized impurity scattering (degenerate) model II (Deg) [cm 2 / Vs] reciprocal 1 / μ II (Deg) The method for calculating the intra-grain mobility μ in-grain(T) of a semiconductor according to claim 1, wherein the intra-grain mobility μ in-grain(T) can be expressed by either one or both of the following:

20. Mobility μ determined by the neutral impurity scattering model NI [cm 2 The method for calculating intra-grain mobility μ in-grain(T) of a semiconductor according to claim 19, wherein the mobility μ in-grain(T) in a semiconductor grain is expressed by an Erginsoy-type mobility model, a Quisse-type mobility model, or a Quisse-type mobility approximation formula.

21. Mobility μ determined by the Erginsoy-type mobility model NI [cm 2 The method for calculating intragrain mobility μ in-grain(T) of a semiconductor according to claim 20, wherein μ in-grain(T) is represented by the following formula (A3E):

22. Mobility μ determined by the Quisse-type mobility model NI [cm 2 The method for calculating the intragrain mobility μ in-grain(T) of a semiconductor according to claim 20, wherein the intergrain mobility μ in-grain(T) is represented by the following formulas (Q-1) to (Q-26): [In formulas (Q-1) to (Q-26), μ NI is the mobility [cm] determined by the Quisse-type mobility model. 2 / Vs], N NI is the neutral impurity concentration [cm -3 ], k is the wave vector [cm -1 ], q is the elementary charge [C], 23. Mobility μ determined by the Quisse-type mobility model NI [cm 2 The method for calculating the intragrain mobility μ in-grain(T) of a semiconductor according to claim 20, wherein the intergrain mobility μ in-grain(T) can be expressed by the following approximate formula (A3Q-app): C is represented by the following formula:

24. Mobility μ determined by the ionized impurity scattering (degenerate) model II (Deg) [cm 2 20. The method for calculating intragrain mobility μ in-grain(T) of a semiconductor according to claim 19, wherein the inter-grain mobility μ in-grain(T) can be expressed by a Dingle-type mobility model.

25. Mobility μ determined by the ionized impurity scattering (degenerate) model II (Deg) [cm 2 25. The method for calculating intragrain mobility μ in-grain(T) of a semiconductor according to claim 19 or 24, wherein the mobility μ in-grain(T) in a semiconductor grain is expressed by the following Dingle-type mobility equation (A4D):

26. Mobility μ determined by the ionized impurity scattering (degenerate) model II (Deg) [cm 2 / Vs] is a Dingle type, and can be expressed by the following mobility formula (A4-1) taking into account a self-formation process of donors.

27. The shielding function F in the Dingle type mobility equation (A4D) or (A4-1) II is the shielding function F in the Pisarkiewicz type ionized impurity scattering represented by the following formula (F) II The method for calculating the intragrain mobility μ in-grain(T) of a semiconductor according to claim 25 or 26, 28. The mobility equation of the Dingle type represented by the formula (A4D) or (A4-1) is μ II_Dingle (Deg) [cm 2 / Vs], the mobility μ determined by the ionized impurity scattering (degenerate) model II (Deg) [cm 2 / Vs] can be expressed by the following sigmoid function type formula (A4-S) with respect to the carrier concentration n. [In formula (A4-S), N C is the effective density of states [cm -3 ], n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ], and a is a parameter that represents the rate of change of the sigmoid function.

29. Said T -3/2 The coefficient of the term is a3 [cm -2 VsK 3/2 ], where coefficient a 3 and T -3/2 The product of these is the mobility μ determined by the ionized impurity scattering (non-degenerate) model. II (nonDeg) [cm -2 Vs] reciprocal 1 / μ II (nonDeg) The method for calculating the intra-grain mobility μ in-grain(T) of a semiconductor according to claim 1, which can be expressed as follows:

30. Mobility μ determined by the ionized impurity scattering (non-degenerate) model II (nonDeg) [cm 2 The method for calculating intra-grain mobility μ in-grain(T) of a semiconductor according to claim 29, wherein the mobility μ in-grain(T) in a semiconductor grain is expressed by a mobility equation of the Conwell-Weisskopf model type or the Brooks-Herring model type.

31. Mobility μ determined by the ionized impurity scattering (non-degenerate) model II (nonDeg) [cm 2 31. The method for calculating the intragrain mobility μ in-grain(T) of a semiconductor according to claim 29 or 30, wherein the mobility μ in-grain(T) can be expressed by the following mobility equation (A5-CW) of the Conwell-Weisskopf model type. [In formula (A5-CW), ε0 is the dielectric constant of a vacuum [F / cm], ε r is the relative dielectric constant (static), k B is the Boltzmann constant [eV / K], T is the temperature [K], m * is the effective mass normalized by the speed of light [eV / c 2 ] (c is the speed of light [cm / s]), e is the elementary charge [C], Z is the ion valence of the ionized impurity, N II_nonDeg is the ionized impurity concentration [cm -3 ] 32. Mobility μ determined by the ionized impurity scattering (non-degenerate) model II (nonDeg) [cm 2 31. The method for calculating intragrain mobility μ in-grain(T) of a semiconductor according to claim 29 or 30, wherein the mobility μ in-grain(T) can be expressed by the following mobility equation (A5-BH) of the Brooks-Herring model. [In formula (A5-BH), F II is the screening function for ionized impurity scattering, and ε 0 is the dielectric constant of a vacuum [F / cm], ε r is the relative dielectric constant (static), k B is the Boltzmann constant [eV / K], T is the temperature [K], m * is the effective mass normalized by the speed of light [eV / c 2 ] (c is the speed of light [cm / s]), e is the elementary charge [C], Z is the ion valence of the ionized impurity, N II_nonDeg is the ionized impurity concentration [cm -3 ] 33. The shielding function F in the Brooks-Herring model mobility equation II is a shielding function F in Pisarkiewicz-type ionized impurity scattering, which is represented by the following formula (F): II The method for calculating the intra-grain mobility μ in-grain(T) of a semiconductor according to claim 32.

34. The mobility determined by the ionized impurity scattering (non-degenerate) model that can be expressed by the mobility equation of the Conwell-Weisskopf model type or the Brooks-Herring model type is μII_CW-BH (nonDeg) [cm 2 / Vs], the mobility μ determined by the ionized impurity scattering (non-degenerate) model II (nonDeg) [cm 2 / Vs] can be expressed by the following sigmoid function type formula (A5-S) with respect to the carrier concentration n. [In formula (A5-S), N C is the effective density of states [cm -3 ], n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ], and a is a parameter that represents the rate of change of the sigmoid function.

35. Mobility μ within the grains of the semiconductor in-grain The reciprocal of (T) is 1 / (exp(β / T)-1), T 0 , T -3/2 , T 1/2 , T 3/2 , T 1 , and T 2 and further, the temperature dependence is a function of the carrier concentration n, 1 / μ NI The intra-grain mobility μ of the semiconductor of claim 1 is a linear combination of the (T, n) terms. in-grain A method for calculating (T). [Here, β[K] is a coefficient.] 36. Said 1 / μ NI The method for calculating the intragrain mobility μ in-grain (T) of a semiconductor according to claim 35, wherein the (T, n) term is represented by the following formulas (Q-1) to (Q-26) determined by a Quisse type mobility model. [In formulas (Q-1) to (Q-26), μ NI is the mobility [cm] determined by the Quisse model 2 / Vs], N NI is the neutral impurity concentration [cm -3 ], k is the wave vector [cm -1], q is the elementary charge [C], 37. Said 1 / μ NI The method for calculating the intragrain mobility μ in-grain (T) of a semiconductor according to claim 35 or 36, wherein the (T, n) term is expressed by the following approximate formula (A5Q-app) determined by the Quisse type mobility model. C is represented by the following formula:

38. The effective mass m * The method for calculating the intragrain mobility μ in-grain (T) of a semiconductor according to any one of claims 17, 18, 21, 22, 23, 25, 26, 27, 31, 32, 33, 36 and 37, wherein the mobility μ in-grain (T) can be expressed by any one of the following formulas (M-1) and (M-2):

39. The Debye shielding parameter q s The method for calculating the intragrain mobility μ in-grain(T) of a semiconductor according to any one of claims 22, 23, 36 and 37, wherein is selected from the group consisting of the following formulas (Qq-1) to (Qq-5): [In formulas (Qq-1) to (Qq-5), ε 0 is the dielectric constant of a vacuum [F / cm], ε r is the relative dielectric constant (static), k B is the Boltzmann constant [eV / K], T is the temperature [K], n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), N C is the effective density of states [cm -3 ] 40. The parameters D and k' 1 The method for calculating the intragrain mobility μ in-grain (T) of a semiconductor according to claim 23 or 37, wherein each of these can be expressed by the following formulas. (Wherein, e is the elementary charge [C], k B is the Boltzmann constant [eV / K], T is the temperature [K], ε 0 is the dielectric constant of a vacuum [F / cm], ε r is the relative dielectric constant (static), n is the free carrier concentration [cm -3] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), N C is the effective density of states [cm -3 ])] [In the formula, k' 1 is the Q / πa of the Quisse model 0 2 -ka 0 Q / πa in the graph 0 2 = D (upper base of right-angled trapezoid) and Q / πa 0 2 = 4 (k 0 ) -3 (The hypotenuse of the right-angled trapezoid) 0 The value, D, is as described above.

41. In the following formula (1-1), the mobility μ in-grain As the reciprocal of (T), 1 / (exp(β / T)-1), T 0 , T -3/2 , T 1/2 and T 3/2 and 1 / μ, in which the temperature dependence is a function of carrier concentration n. NI The intragranular mobility μ of the semiconductor according to any one of claims 35 to 40, using the term (T, n). in-grain Method for calculating (T). [In formula (1-1), μ in-grain is the mobility in the grains of the semiconductor [cm 2 / Vs], T is temperature [K], β[K], a 1 [cm -2 Vs], a 2 [cm -2 Vs], a 3 [cm -2 Vs.K. 3/2 ], a 4 [cm -2 Vs.K. -1/2 ], and a 5 [cm -2 Vs.K. -3/2 In the above formula (1-1), 1 / (exp(β / T)−1) and T 0 , T -3/2 , T 1/2and T 3/2 The coefficient a of the term not selected 1 ~a 5 is set to 0.] 42. a in the above formula (1-1) 2 T 0 The intragranular mobility μ of the semiconductor according to any one of claims 20 to 23 can be expressed by the neutral impurity scattering model. in-grain Method for calculating (T).

43. a in the above formula (1-1) 2 T 0 The intragranular mobility μ of the semiconductor according to any one of claims 24 to 28 can be expressed by the ionized impurity scattering (degenerate) model. in-grain Method for calculating (T).

44. In the formula (1-1), a 2 T 0 can be expressed by an ionized impurity scattering (degenerate) model according to any one of claims 24 to 28, and 1 / μ NI The mobility μ in the grains of the semiconductor according to claim 1, wherein the (T, n) term can be expressed by the neutral impurity scattering model according to any one of claims 35 to 37. in-grain Method for calculating (T).

45. The intragrain mobility μ of the semiconductor according to claim 2, wherein the reciprocal of the intragrain mobility μ in-grain(T) of the semiconductor expressed by the formula (1) can be expressed by the following formula (A1-1): in-grain Method for calculating (T). [In formula (A1-1), μ OP is as defined in the formula (A2) or (A2-2), NI is as defined in the above formula (A3E), (Q-1), or (A3Q-app), II (Deg) is as defined in formula (A4D), (A4-1), or (A4-S), II (nonDeg) is as defined in the above formula (A5-CW), (A5-BH), or (A5-S).

46. ​​The intragranular mobility μ of the semiconductor according to claim 41, wherein the formula (1-1) can be expressed by the following formula (A1-2): in-grain Method for calculating (T). [In formula (A1-2), μ OP is as defined in the formula (A2) or (A2-2), II (Deg) is as defined in formula (A4D), (A4-1), or (A4-S), II (nonDeg) is as defined in the above formula (A5-CW), (A5-BH), or (A5-S), and μ NI (T, n) are as defined in formula (A3E), (Q-1), or (A3Q-app) above.] 47. In the formula (A1-2), μ OP is the formula (A2-2), and μ II (Deg) is the formula (A4-1) or (A4-S), and μ II (nonDeg) is the formula (A5-BH) or (A5-S), and μ NI The intragranular mobility μ of the semiconductor according to claim 46, wherein (T, n) is represented by the formula (A3E), (Q-1), or (A5Q-app). in-grain Method for calculating (T).

48. Mobility μ determined by the ionized impurity scattering (degenerate) model represented by the above formula (A4D) or (A4-1) II (Deg) and the mobility μ determined by the ionized impurity scattering (non-degenerate) model represented by the above formula (A5-CW) or (A5-BH) II (nonDeg) For carrier concentration n, the effective density of states N C are linearly combined with a sigmoid function with the boundary, and each shielding function F II is a Pisarkiewicz type F represented by the formula (F) II The intragranular mobility μ of the semiconductor of claim 1 is in-grain Method for calculating (T).

49. The intragranular mobility μ of any one of claims 1 to 48, wherein the semiconductor is a polycrystalline semiconductor. in-grain Method for calculating (T).

50. The intra-grain mobility μ of claim 49, wherein the polycrystalline semiconductor is an oxide semiconductor containing In as a main component.in-grain Method for calculating (T).

51. The intragranular mobility μ of claim 50, wherein the content of In in all metal elements of the polycrystalline semiconductor is 50 atomic % or more. in-grain Method for calculating (T).

52. The intragranular mobility μ of any one of claims 49 to 51, wherein the polycrystalline semiconductor is in the form of an oxide thin film. in-grain Method for calculating (T).

53. The intragranular mobility μ of claim 52, wherein the polycrystalline semiconductor thin film comprises a bixbyite structure. in-grain Method for calculating (T).

54. A method for calculating a macroscopic DC mobility μ(T) of a semiconductor, the method being represented by the following formula (10) when temperature T [K] is a fluctuation factor. [In formula (10), μ is the mobility of the semiconductor [cm 2 / Vs], T is temperature [K], γ[K] and θ[K 2 ] is a coefficient and a positive number including 0, μ in-grain (T) is the intragranular mobility μ of the semiconductor according to any one of claims 1 to 53. in-grain Mobility in the grains of semiconductors [cm 2 / Vs].

55. γ[K] or θ[K 2 ] is 0. A method for calculating the macroscopic DC mobility μ(T) of a semiconductor according to claim 54.

56. A method for calculating macroscopic DC mobility μ(T) according to claim 54 or 55, wherein γ is expressed by the following formula (12): [In formula (12), q is the elementary charge 1.602×10 -19 [C], V B is the potential barrier value [eV], k B is the Boltzmann constant (8.617 x 10 -5 [eV / K].

57. The potential barrier value V B [eV] is the carrier concentration n [cm -3 The potential barrier value V varies depending on B(n), wherein V B 57. A method for calculating the macroscopic DC mobility μ(T) of a semiconductor according to claim 56, wherein (n) is represented by the following formula (13): [In formula (13), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), A 6 [eV], B 6 , C 6 [eV], and D 6 are the coefficients, N 06 [eV] is V B (n) is the carrier concentration corresponding to the inflection point in formula (13).

58. The above A 6 is 0 eV or more and 1.0 eV or less, and the B 6 is 0.1 or more, 6 is 2 x 10 -1- is less than D 6 is 1.0 eV or less, and the N 06 is 1 x 10 17 cm -3 Above 1 x 10 21 58. A method for calculating the macroscopic DC mobility μ(T) of a semiconductor according to claim 57, wherein:

59. A method for calculating the macroscopic DC mobility μ(T) of a semiconductor according to claim 54, represented by the following formula (A10): [In formula (A10), q is an elementary charge [C], V B is the grain boundary barrier height [eV], k B is the Boltzmann constant [eV / K], T is the temperature [K], μ in-grain (T) is the intragrain mobility [cm 2 / Vs].

60. V in the above formula (10A) B A method for calculating the macroscopic DC mobility μ(T) of a semiconductor according to claim 59, wherein is represented by the following formula (A11):

61. Mobility μ in the above formula (A10) in-grain61. The method for calculating the macroscopic DC mobility μ(T) of a semiconductor according to claim 59 or 60, wherein the reciprocal of (T) can be expressed by any one of the formulas (1-1), (A1-1) and (A1-2).

62. A method for calculating the macroscopic DC mobility μ(T) of a semiconductor according to any one of claims 54 to 61, wherein the semiconductor is a polycrystalline semiconductor.

63. A method for calculating the macroscopic DC mobility μ(T) of a semiconductor according to claim 62, wherein the polycrystalline semiconductor is an oxide semiconductor containing In as a main component.

64. A method for calculating macroscopic DC mobility μ(T) of a semiconductor as described in claim 63, wherein the content ratio of In in all metal elements of the polycrystalline semiconductor is 50 atomic % or more.

65. A method for calculating the macroscopic DC mobility μ(T) of a semiconductor according to any one of claims 62 to 64, wherein the polycrystalline semiconductor is in the form of an oxide thin film.

66. A method for calculating the macroscopic DC mobility μ(T) of a semiconductor according to claim 65, wherein the polycrystalline semiconductor thin film comprises a bixbyite structure.

67. A device simulation method for determining the macroscopic DC mobility μ(T) of a semiconductor, the method comprising a step of using the method for calculating the macroscopic DC mobility μ(T) of a semiconductor according to any one of claims 54 to 66.

68. A method for manufacturing a thin-film transistor, comprising: a step of calculating the macroscopic DC mobility μ(T) of a semiconductor using the method for calculating the macroscopic DC mobility μ(T) of a semiconductor according to any one of claims 54 to 66; and a step of manufacturing a thin-film transistor based on the calculated macroscopic DC mobility μ(T) of the semiconductor.

69. A method for manufacturing a thin film transistor, comprising: a step of calculating a macroscopic DC mobility μ(T) of a semiconductor using the device simulation method described in claim 67; and a step of designing a device based on the calculated macroscopic DC mobility μ(T) of the semiconductor.

70. An electronic device comprising a thin film transistor manufactured using the method for manufacturing a thin film transistor according to claim 68 or 69.

71. The following formulas (1) and (10) [In formula (1), μin-grain is the mobility in the grains of the semiconductor [cm 2 / Vs], T is temperature [K], β[K], a 1 [cm -2 Vs], a 2 [cm -2 Vs], a 3 [cm -2 Vs.K. 3/2 ], a 4 [cm -2 Vs.K. -1/2 ], and a 5 [cm -2 Vs.K. -3/2 In the above formula (1), 1 / (exp(β / T)−1) and T 0 , T -3/2 , T 1/2 and T 3/2 Using two or more terms selected from the group consisting of: 1 ~a 5 is set to 0.] [In formula (10), μ is the mobility of the semiconductor [cm 2 / Vs], T is temperature [K], γ[K] and θ[K 2 ] is a coefficient and a positive number including 0, μ in-grain (T) is the intragranular mobility μ of the semiconductor according to any one of claims 1 to 53. in-grain Mobility in the grains of semiconductors [cm 2 / Vs].] is a program for calculating a macroscopic DC mobility μ(T) of a semiconductor, the program comprising: -3 a means for receiving an input of a type of material of the semiconductor; 1 ~a 5 a program for causing the device to function as a means for selecting values ​​of β, γ, and θ; and a means for calculating the macroscopic DC mobility μ(T) of the semiconductor using the formulas (1) and (10).

72. The program according to claim 71, wherein β[K] is expressed by the following formula (2): [In formula (2), hω op / 2π is the energy of the optical phonon [eV] that varies depending on the carrier concentration, k B is the Boltzmann constant (8.617 x 10 -5 [eV / K]), h is Planck's constant (4.1357×10 -15 [eVs]).

73. The above a. 1 [cm -2 Vs] is the carrier concentration n [cm -3 ], the coefficient a 1 (n), wherein a 1 73. The program according to claim 71 or 72, wherein (n) is represented by the following formula (3): [In formula (3), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), A 1 [cm -2 Vs], B 1 , and C 1 [cm -2 Vs] are the coefficients, N 01 Is 1 The carrier concentration [cm -3 ] 74. The above A 1 But 0 cm -2 Vs or more 0.1cm -2 Vs or less, and 1 is 0 or more, 1 is 1 cm -2 Vs or less, and 01 is 1 x 10 18 cm -3 Above 1 x 10 23 cm -3 74. The program of claim 73, wherein:

75. The above a. 2 [cm -2 Vs] is the carrier concentration n [cm -3 ], the coefficient a 2 (n), wherein a 2 The program according to any one of claims 71 to 74, wherein (n) is represented by the following formula (4): [In formula (4), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), A 2 [cm -2 Vs], B 2 , and C 2 [cm -2 Vs] are coefficients, N 02 Is 2 The carrier concentration [cm -3 ] 76. The above A 2 is 0.005 cm -2 Vs or more 0.5cm -2 Vs or less, and 2 is 1000 or less, 2 is 1 x 10 -1 cm -2 Vs, and the N 02 is 1 x 10 17 cm -3 Above 1 x 10 22 cm -3 76. The program of claim 75, wherein:

77. The above a. 3 [cm -2 Vs.K. 3/2 ] is the carrier concentration n [cm -3 ], the coefficient a 3 (n), wherein a 3 The program according to any one of claims 71 to 74, wherein (n) is represented by the following formula (5): [In formula (5), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), A 3 [cm -8 Vs.K. 3/2 ] and B 3 , C 3 [cm -2 Vs.K. 3/2 ], D 3 [cm 3 ] and F 3 [cm-2 Vs.K. 3/2 ] are the coefficients, N 03 Is 3 The maximum carrier concentration [cm -3 ] 78. The above A 3 But, 10 -39 cm -8 Vs.K. 3/2 More than 10 -33 cm -8 Vs.K. 3/2 The above B 3 is 1 or more and 5000 or less, 3 is 10 4 cm -2 Vs.K. 3/2 is less than D 3 is 10 -20 cm 3 The above and F 3 is 500 cm -2 Vs.K. 3/2 is less than N 03 is 1 x 10 16 cm -3 Above 1 x 10 20 78. The program of claim 77, wherein:

79. The above a. 3 is the carrier concentration n [cm -3 ], the coefficient a 3 (n), where N 03 [cm -3 ] and N 13 [cm -3 ] is an arbitrary carrier concentration, 3 (n) is n<N 03 In this case, it is expressed by the following formula (5-1), and N 03 ≦n≦N 13 When n>N, it is expressed by the formula (5-2). 13 The program according to any one of claims 71 to 78, which is represented by the following formula (5-3). [In the formulas (5-1), (5-3) and (5-3), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3]), A' 3 [cm -8 Vs.K. 3/2 ], C' 3 [cm -2 Vs.K. 3/2 ] and D' 3 [cm 3 ] are coefficients, B' 3 [cm -2 Vs.K. 3/2 ] is a constant.

80. The above A' 3 But, 10 -39 cm -8 Vs.K. 3/2 More than 10 -33 cm -8 Vs.K. 3/2 and C' is the same as above. 3 is 5000 cm -2 Vs.K. 3/2 is equal to or less than D' 3 is 10 -20 cm 3 The program according to claim 79.

81. The above a. 4 [cm -2 Vs.K. -1/2 81. The program according to any one of claims 71 to 80, wherein ] is a coefficient that varies depending on the carrier concentration.

82. The above a. 5 [cm -2 Vs.K. -3/2 ] is a coefficient that varies depending on the carrier concentration.

83. The semiconductor is a non-degenerate semiconductor, and the a 1 is the optical phonon scattering constant A op [cm -2 Vs], the above a 2 is the neutral impurity scattering coefficient A neutral [cm -2 Vs], the above a 3 is the ionized impurity scattering coefficient A ion [cm -2 Vs.K. 3/2 ], the a 4 is the weak localization constant [cm -2 Vs.K. -1/2], the a 5 is the acoustic phonon scattering constant [cm -2 Vs.K. -3/2 ]. The program according to any one of claims 71 to 82.

84. A program according to any one of claims 71 to 83, wherein γ is expressed by the following equation (12): [In formula (12), q is the elementary charge 1.602×10 -19 [C], V B is the potential barrier value [eV], k B is the Boltzmann constant (8.617 x 10 -5 [eV / K].] 85. The potential barrier value V B [eV] is the carrier concentration n [cm -3 The potential barrier value V varies depending on B (n), wherein V B The program according to claim 84, wherein (n) is represented by the following formula (13): [In formula (13), n is the free carrier concentration [cm -3 ] (In the oxide semiconductors used in this specification, the free electron density [cm -3 ]), A 6 [eV], B 6 , C 6 [eV] and D 6 are the coefficients, N 06 is V B The carrier concentration [cm -3 ] 86. The above A 6 is 0.005 eV or more and 1.0 eV or less, and the B 6 is 0.1 or more, 6 is 1 x 10 -1 eV or less, 6 is 0.1 eV or less, and the N 06 is 1 x 10 17 cm -3 Above 1 x 10 21 86. The program of claim 85, wherein:

87. A program for calculating a macroscopic DC mobility μ(T) of a semiconductor using formula (1-1) according to claim 41, formula (A1-1) according to claim 45, or formula (A1-2) according to claim 46, and formula (A10) according to claim 59, comprising: a computer; -3 a means for receiving an input of a type of material of the semiconductor; 1 ~a 5 a program for functioning as a means for selecting values ​​of β, γ, and θ, and a means for calculating the macroscopic DC mobility μ(T) of a semiconductor using the formulas (1-1), (A1-1) or (A1-2), and (A10).

88. The program according to any one of claims 71 to 87, wherein the semiconductor is a crystalline oxide thin film containing In as a main component.

89. Temperature T [K] and carrier concentration n [cm -3 ] depends on the macroscopic DC mobility μ(T, n) [cm 2 / Vs], the program causing a computer to function as a means for deriving the macroscopic DC mobility μ(T, n) by performing regression using: a means for accepting data input of μ(T, n) for T and n actually measured from a semiconductor film; a means for accepting input of a type of semiconductor material for obtaining initial values ​​of each coefficient in the following formula (1); and a program according to any one of claims 71 to 88. [In formula (1), μ in-grain is the mobility in the grains of the semiconductor [cm 2 / Vs], T is temperature [K], β[K], a 1 [cm -2 Vs], a 2 [cm -2 Vs], a 3 [cm -2 Vs.K. 3/2 ], a 4 [cm -2 Vs.K. -1/2 ], and a 5 [cm -2 Vs.K. -3/2In the above formula (1), 1 / (exp(β / T)−1) and T 0 , T -3/2 , T 1/2 and T 3/2 Using two or more terms selected from the group consisting of: 1 ~a 5 is set to 0.] 90. Temperature T [K] and carrier concentration n [cm -3 ] depends on the macroscopic DC mobility μ(T, n) [cm 2 / Vs], causing a computer to function as a means for deriving the macroscopic DC mobility μ(T,n) by regression using: a means for accepting data input of μ(T,n) for T and n actually measured from a semiconductor film; a means for accepting input of a type of semiconductor material for obtaining initial values ​​of each coefficient in formula (1-1) described in claim 41 or formula (A1-2) described in claim 46; and a program for calculating the macroscopic DC mobility μ(T) of a semiconductor described in claim 87.

Citation Information

Patent Citations

  • Method for simulation by simulator for obtaining electric characteristics of thin-film transistor disposed in crystallized region and physical analysis model for calculating and extracting coulomb scattering central density included in channel region of thin-film transistor disposed in crystallized region

    JP2009253043A

Cited By

  • Semiconductor device simulation method and calculation program

    WO2026071211A1