Blade for table tennis racket having improved performance and manufacturing method therefor
The method of varying the density and thickness of table tennis racket blades through chemical treatments and reinforcement layers addresses the limitations of uniform blades, enhancing the sweet spot area and performance while adhering to regulations.
Patent Information
- Application Number
- PCT/KR2023/005928
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-28
- Publication Date
- 2024-10-31
AI Technical Summary
Table tennis racket blades have limited performance due to uniform thickness and density, which restricts the size of the 'sweet spot' where optimal hitting characteristics occur, violating International Table Tennis Federation regulations when attempts to enhance it fail to maintain continuous and uniform thickness.
A manufacturing method that varies the density and thickness of the blade by processing wood to increase hardness and elasticity differently across the blade, using chemical treatments and reinforcement layers, while maintaining the same overall thickness to enhance the sweet spot area.
The method improves the sweet spot area by increasing density and repulsion force towards the outside, maintaining compliance with regulations and enhancing the overall performance of the table tennis racket blade.
Smart Images

Figure KR2023005928_31102024_PF_FP_ABST
Abstract
Description
Blade for table tennis racket with improved performance and method for manufacturing the same
[0001] The present invention relates to a blade for a table tennis racket with improved performance, which improves the performance of the blade by varying the density depending on the position of the blade, which is a component of the table tennis racket, and a method for manufacturing the same.
[0002] A table tennis racket is made with a blade, usually made of wood, and rubber bonded to one or both sides. The blade is usually made of one to nine layers of wood, cork, fiberglass, carbon fiber, aluminum fiber, or Kevlar laminate. According to the International Table Tennis Federation (ITTF) regulations for table tennis rackets, the blade layer must contain at least 85% natural wood, and the adhesive layer inside the blade may be reinforced with fibrous materials such as carbon fiber, fiberglass, or compressed paper, but must not exceed 7.5% of the total thickness or 0.35 mm. However, there are no restrictions on the size, shape, or weight of the racket, and the blade must be flat and solid. Common types of wood used as blade materials include balsa, limba, walnut, cypress, and hinoki. The average blade size is 16.5 cm (6.5 inches) long and 15 cm (6 inches) wide, and although there are no specific restrictions on the size or shape of the blade, the above size is known to be the most suitable size for playing.
[0003] Existing blade products are manufactured by laminating thin layers of wood, each a few millimeters thick, with a layer of fiber material, allowing for limited control of blade characteristics. Furthermore, because blade weight and ball rebound characteristics vary depending on the material used, blades are manufactured using a fiber-reinforced plastic layer containing various layers of wood and fabric made by weaving fibers to achieve the desired characteristics.
[0004] The rebound characteristics and feel of a table tennis ball hit vary depending on where it is struck on the blade. Specifically, there is a designated location, such as the center of the racket, known as the "sweet spot," where the optimal striking characteristics are achieved. Typically, the sweet spot appears in the center of the blade, with the feel and rebound characteristics deteriorating as the blade moves outward. Various ideas have been proposed to maximize the sweet spot area, but many have violated the International Table Tennis Federation's regulation, which requires all layers of the striking surface to be "continuously uniform in thickness."
[0005] Therefore, there is a need for a method to develop a blade with improved performance to maximize the sweet spot while satisfying the above regulations.
[0006] In order to solve the above problems, the present invention aims to provide a blade for a table tennis racket with improved performance, in which the thickness of the blade is the same but the density varies depending on the location to expand the sweet spot, and a method for manufacturing the same.
[0007] In order to achieve the above object, the present invention provides a method for manufacturing a blade for a table tennis racket with improved performance, comprising the steps of: (a) processing wood into a blade shape and processing the thickness of the wood so that it has different hardness and elasticity depending on the position; (b) placing the processed wood into a press groove in the shape of a blade; (c) compressing the wood placed in the press groove with a press; and (d) finishing the compressed wood to complete the blade.
[0008] The step (a) of the present invention is characterized by comprising: (a-1) a chemical treatment step for increasing the hardness and elasticity of a blade manufactured by controlling the content of cellulose, lignin, and hemicellulose of wood; (a-2) a step for cleaning and drying the chemically treated wood; and (a-3) a step for processing the thickness of the dried wood so that it has different hardness and elasticity depending on the position of the blade manufactured.
[0009] In step (a) of the present invention, the step of processing the thickness of the wood is characterized in that the wood is processed so that the thickness increases from the center to the outside. The processing of the wood is characterized in that the thickness increases from the center line (C) of the longitudinal direction of the wood to the ends on both sides, and the thickness increases from the center to the front end of the center line.
[0010] In step (a) of the present invention, the step of processing the thickness of the wood is characterized in that reinforcing wood of different widths is processed to form a stepped shape so that the thickness increases toward the outer side of the wood. The reinforcing wood is manufactured separately and laminated onto the wood in a stepped shape, and the reinforcing wood is characterized in that the reinforcing wood is made of the same material as the wood processed into the shape of a blade or a different material. In addition, the reinforcing wood laminated in a stepped shape is characterized in that the thickness becomes thinner or thicker toward the upper side.
[0011] In step (a) of the present invention, the step of processing the thickness of the wood is characterized in that the wood is processed by forming a groove or hole in the wood so that the thickness increases toward the outside of the wood, and a cylindrical reinforcing wood is installed in the groove or hole.
[0012] In step (a) of the present invention, the step of processing the thickness of the wood is characterized by processing the wood so that a cylindrical reinforcing wood is formed whose height sequentially increases as it goes outward.
[0013] In the present invention, the pressing of the press is characterized by being performed at a temperature range of 14 to 350°C and a pressure of 0.1 to 30 MPa.
[0014] The finishing in step (d) of the present invention is characterized by comprising: (d-1) a step of finely processing the flatness of both sides of the blade so that they are uniform; and (d-2) a step of removing burrs along the edges of the blade.
[0015] In addition, the present invention provides a blade for a table tennis racket with improved performance manufactured by the method described in any one of the claims to achieve the above object.
[0016] The method for manufacturing a blade for a table tennis racket with improved performance according to the present invention has the advantage of being simple to manufacture and reducing costs, as the performance of the blade can be improved by adjusting the thickness of the wood used as the blade.
[0017] In addition, the method for manufacturing a blade for a table tennis racket with improved performance according to the present invention has the advantage of being able to maximize the sweet spot because the density, strength, and repulsive force increase toward the outer side of the blade, thereby improving the performance of the table tennis racket.
[0018] In addition, the blade for a table tennis racket according to the present invention has the advantage of improved density, strength, and resilience because it is formed with the same thickness but the density increases toward the outside.
[0019] In addition, the blade for a table tennis racket according to the present invention has the advantage of being able to manufacture a blade with increased density at a point desired by the user or at a point where a table tennis ball is frequently hit.
[0020] Figure 1 is an exploded perspective view of a typical table tennis racket.
[0021] Figure 2 is a flowchart of a method for manufacturing a blade for a table tennis racket with improved performance according to the present invention.
[0022] Figure 3 is a plan view and a side view of a first embodiment showing wood for manufacturing a blade processed with different thicknesses according to the present invention.
[0023] Figure 4 is a plan view and a side view of a second embodiment showing wood for manufacturing blades processed with different thicknesses according to the present invention.
[0024] FIG. 5 is a plan view and a side view of a third embodiment showing wood for manufacturing blades processed with different thicknesses according to the present invention.
[0025] Figure 6 is an enlarged view of the side view of Figure 5.
[0026] Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the accompanying drawings. However, this description is intended to be sufficiently detailed to enable those skilled in the art to easily practice the invention, and is not intended to limit the technical spirit or scope of the present invention.
[0027]
[0028] Fig. 1 is an exploded perspective view of a typical table tennis racket (1). As shown in the drawing, the table tennis racket (1) comprises a blade (10) made of one or more layers of wood or synthetic wood, rubber (20) and sponge (30) attached to the front and rear surfaces of the blade, and a handle (40) attached to the end of the blade (10). The present invention relates to a blade (10) which is a component of a table tennis racket (1) and a manufacturing method thereof.
[0029] FIG. 2 is a flowchart illustrating a method for manufacturing a table tennis racket blade with improved performance according to the present invention. As illustrated in the drawing, the blade manufacturing method comprises the steps of (a) processing wood into a blade shape and processing the thickness of the wood so that it has different hardness and elasticity depending on the position (S1), (b) placing the processed wood into a blade-shaped press groove (S2), (c) compressing the wood placed into the press groove with a press (S3), and (d) finishing the compressed wood to complete the blade (S4). Each step will be described in detail below.
[0030] First, the wood (11) is processed into a blade shape and the thickness of the wood is processed to have different hardness and elasticity depending on the location (S1). According to the International Table Tennis Federation's regulations on table tennis rackets, the material used for the blade must contain natural wood at a ratio of 85% or more, and the adhesive layer inside the blade may be reinforced with fiber materials such as carbon fiber, glass fiber, or compressed paper, but must not exceed 7.5% of the total thickness or 0.35 mm. However, there are no restrictions on the size, shape, or weight of the racket, and the blade must be flat and hard. Common types of wood used as blade materials include balsa, limba, walnut, cypress, and hinoki. The characteristics of these woods are that they have the same thickness and density, so they inevitably have the same density, strength, and resilience throughout the blade. However, the point on the blade with the best resilience is called the sweet spot, which is usually the center. Accordingly, as the blade moves further away from the sweet spot, the feel and rebound characteristics of the ball when struck inevitably deteriorate. Therefore, the blade needs to be machined so that the outer edge of the blade possesses the same feel and rebound characteristics as the sweet spot.
[0031] FIG. 3 illustrates a first embodiment of a method for processing the thickness of wood. As illustrated in the drawing, wood is first processed into a blade (10) shape, and then wood (11) is processed so that the thickness increases from the inside to the outside. Wood (11) is composed of a central portion (111), outer sides (112) in both directions, and outer sides (113) in the front-back direction. As illustrated in FIG. 3(a), the wood is processed so that the thickness (t2) increases in the direction (b-b') (112) from the center (O) of the wood processed into a blade shape. As illustrated in FIG. 3(c), the thickness (t2) increases in the direction (b-b') from the center. FIG. 3(b) illustrates that the thickness (t1) increases in the direction (a-a') (113) in the front-back direction. Likewise, the thickness (t1) is processed to become thicker from the center in the front-back direction (a-a') (113). In addition, as shown in FIGS. 3(b) and 3(c), the thickness in the bilateral directions (b-b') (112) and the thickness in the front-back direction (a-a') (113) may be the same or different. Normally, when a table tennis ball is hit on the end side in the front-back direction (a-a') (113), the torque may not be large because the handle is held, but when a table tennis ball is hit on the end side in the bilateral directions (b-b') (112), a large torque is applied, which reduces the feeling of hitting. Accordingly, it is preferable that the thickness in the bilateral directions (b-b') (112) be formed to be the same as or thicker than the thickness in the front-back direction (a-a') (113). In addition, since the rear side of the wood (11) to which the handle is attached is close to the user's hand, a strong blow can be made, so the rear (a) side in the front-back direction (a-a') may not be thick.
[0032] Fig. 4 illustrates a second embodiment of a method for processing the thickness of wood. As illustrated in the drawing, reinforcing wood (112', 113') of a certain thickness is provided so that the thickness becomes thicker toward the outside of the wood (11'). The wood (11') is composed of a wood body (111') and reinforcing wood (112', 113'), and the reinforcing wood (112', 113') can be processed integrally in a step shape to have a thickness. In addition, the reinforcing wood (112', 113') can be processed so that it is laminated in a step shape using separate reinforcing wood. Fig. 4(b) is a cross-sectional view viewed from both sides (b-b'), and Fig. 4(c) is a cross-sectional view viewed from the front-back direction (a-a'). As illustrated in the drawing, the reinforcing timber (112', 113') that is integrally processed or separately laminated in a step shape may become thicker or thinner as it goes upward. The reinforcing timber (112', 113') may be installed in both directions and in the front direction of the center with respect to the center portion (O). As illustrated in Fig. 4(b), it may be formed with a plurality of reinforcing timbers (112': 112a', 112b', 112c', 112d') on both sides. In addition, as illustrated in Fig. 4(c), the front reinforcing timbers (113': 113a', 113b', 113c', 113d') may also be formed with a plurality. In cases where the reinforcing wood (112', 113') is laminated separately, wood of the same material as the wood body (111') or wood of a different material may be used.
[0033] FIG. 5 illustrates a third embodiment of a method for processing the thickness of wood (11"). As illustrated in the drawing, constant grooves or holes (111a", 111b") are formed on both sides or the front of the wood (11"). Constant grooves or holes are formed in the wood (11"), and reinforcing wood (112", 113") is processed so that the height of the grooves or holes sequentially increases toward the outside. FIG. 5(b) is a cross-sectional view viewed from both sides (b-b'), and as illustrated in the drawing, reinforcing wood (112": 112a", 112b", 112c", 112d") is illustrated in which the height sequentially increases toward the outside. FIG. 5(c) is a cross-sectional view taken in the front-rear direction (a-a'), and as shown in the drawing, it is illustrated that the reinforcing wood (113": 113a", 113b", 113c", 113d")) is configured to become higher toward the outside. The reinforcing wood installed in the front-rear direction can be installed in both the front-rear direction, but the reinforcing wood (113") can be installed only on the front side where the impact feeling is reduced. FIG. 6 illustrates a state in which the reinforcing wood (112", 113") is installed. The reinforcing wood (112", 113") can be the same wood as the wood body (111") or wood of a different material. In addition, the reinforcing wood can be made of a different material, such as carbon fiber, to further enhance strength. Additionally, the reinforcing wood (112", 113") can be processed as a single piece and the length can be made longer towards the outside, thereby obtaining the effect of the thickness becoming thicker towards the outside.
[0034] In addition, the step of processing the thickness of the wood can be subdivided into (a-1) a chemical treatment step (S11) to increase the hardness and elasticity of the blade manufactured by controlling the content of cellulose, lignin, and hemicellulose of the wood, (a-2) a step of cleaning and drying the chemically treated wood (S12), and (a-3) a step of processing the thickness of the dried wood so that it has different hardness and elasticity depending on the position of the blade manufactured (S13). First, the blade manufactured by controlling the content of cellulose, lignin, and hemicellulose of the wood (11) is subjected to a chemical treatment step (S11) to increase the hardness and elasticity. As a chemical treatment method for controlling the content of lignin and hemicellulose, the content of lignin and hemicellulose can be controlled by treating at high temperature and high pressure using an alkaline agent. In addition, the content of lignin and hemicellulose can be controlled by treating wood with high temperature and high pressure using steam sintering to break down the cell walls. In addition, lignin can be decomposed through chemical oxidation, and the content of lignin can be controlled by breaking down the chemical bonds of lignin using oxygen. Next, the chemically treated wood is washed and dried (S12). Typically, washing and drying are performed to remove chemicals after chemical treatment. Next, the dried wood is processed to have different hardness and elasticity depending on the position of the blade being manufactured (S13). The process of processing the thickness of the wood is the same as in the first to third embodiments mentioned above, so a detailed description thereof will be omitted.
[0035]
[0036] Next, a step (S3) is performed to press the wood that has been placed in the press groove with a press. This is to produce a blade with a constant thickness by pressing with a press. First, the wood (11, 11', 11") is placed in the press groove of the press machine. Once the wood (11, 11', 11") is placed in the press groove, the press is operated to press the wood at a constant temperature and pressure. When the press is operated, the temperature ranges from 14 to 350℃ and the pressure is 0.1 to 30㎫.
[0037]
[0038] Next, the pressed wood is finished to complete the blade (10) in a step (S4). Even if the wood is pressed into a blade using a press, burrs or the like may remain on the surface or sides of the wood. Therefore, it is necessary to perform surface processing to make the blade surface uniform or to remove burrs or the like that may be generated when the wood on the sides is partially broken or protruding. Once the finishing process is completed in this manner, the manufacturing of the blade (10) is complete.
[0039]
[0040] The blade (10) manufactured by the above method can have a strength and repulsive force similar to the central part where the sweet spot is mainly located, so that the hitting feel and repulsive force of the table tennis ball can be maximized, and thus there is an advantage in that the sweet spot part can be enlarged.
[0041]
[0042] Although the embodiments described above are illustrative, it will be apparent to those skilled in the art that the present invention can be embodied in many other forms without departing from the spirit and scope thereof. Therefore, the above-described embodiments should be considered illustrative rather than restrictive, and all implementations within the scope of the appended claims and their equivalents are intended to be included within the scope of the present invention.
[0043] The present invention is an invention with high industrial applicability that enables the production of a table tennis racket in which the performance of the blade is improved by varying the density according to the position of the blade, which is a component of the table tennis racket.
Claims
1. A method for manufacturing a blade for a table tennis racket with improved performance, (a) A step of processing wood into a blade shape and processing the thickness of the wood so that it has different hardness and elasticity depending on the location; (b) a step of placing the processed wood into a blade-shaped press groove; (c) a step of pressing the wood placed in the press groove with a press; and (d) a step of finishing the pressed wood to complete the blade; A method for manufacturing a blade for a table tennis racket with improved performance, characterized by comprising:
2. In paragraph 1, Step (a) above, (a-1) A chemical treatment step for increasing the hardness and elasticity of a blade manufactured by controlling the content of wood fiber, lignin and hemicellulose; (a-2) A step of cleaning and drying the chemically treated wood; (a-3) A step of processing the thickness of the dried wood to have different hardness and elasticity depending on the position of the blade being manufactured; A method for manufacturing a blade for a table tennis racket with improved performance, characterized by comprising:
3. In paragraph 1, In step (a) above, The step of processing the thickness of the above wood is: A method for manufacturing a blade for a table tennis racket with improved performance, characterized in that the wood is processed so that the thickness increases from the center to the outside.
4. In paragraph 3, A method for manufacturing a blade for a table tennis racket with improved performance, characterized in that the processing of the wood increases in thickness from the longitudinal center line (C) of the wood toward the ends on both sides of the center line, and increases in thickness from the central portion of the wood toward the front end of the center line.
5. In paragraph 1, In step (a) above, The step of processing the thickness of the above wood is: A method for manufacturing a blade for a table tennis racket with improved performance, characterized in that reinforcing wood of different widths is processed to form a stepped shape so that the thickness increases toward the outer side of the wood.
6. In paragraph 5, The above reinforcing wood is manufactured separately and laminated in a step-like manner on the wood, A method for manufacturing a blade for a table tennis racket with improved performance, characterized in that the reinforcing wood is made of the same material as the wood processed into the shape of the blade or of a different material.
7. In paragraph 5, A method for manufacturing a blade for a table tennis racket with improved performance, characterized in that the reinforcing wood laminated in the above step shape becomes thinner or thicker as it goes toward the upper side.
8. In paragraph 1, In step (a) above, The step of processing the thickness of the above wood is: A method for manufacturing a blade for a table tennis racket with improved performance, characterized in that a groove or hole is formed in the wood so that the thickness of the wood increases toward the outside, and a cylindrical reinforcing wood that sequentially becomes longer toward the outside is processed to be seated in the groove or hole.
9. In paragraph 1, In step (a) above, The step of processing the thickness of the above wood is: A method for manufacturing a blade for a table tennis racket with improved performance, characterized in that the above wood is processed to form cylindrical reinforcing wood whose height increases sequentially as it goes outward.
10. In paragraph 1, A method for manufacturing a blade for a table tennis racket with improved performance, characterized in that the pressing of the above press is performed at a temperature range of 14 to 350°C and a pressure of 0.1 to 30 MPa.
11. In paragraph 1, In the above step (d), the finishing is: (d-1) a step of micro-machining so that the flatness of both sides of the blade is uniform; and (d-2) A step of removing a burr along the edge of the blade; A method for manufacturing a blade for a table tennis racket with improved performance, characterized by comprising:
12. A blade for a table tennis racket with improved performance manufactured by any one of claims 1 to 11.
Citation Information
Patent Citations
Anti-slipping and moisture-proof table tennis bat
CN109481919A
Ultra-light amorphous reinforced carbon fiber table tennis bat and preparation method thereof
CN111420375A
Table tennis bat provided with a frame having a differentiated structure, particularly for sporting games and competitions
EP0701844A2
Table tennis racket and blade for table tennis racket
JP2005124911A
Racket for table tennis and process for preparing the same
KR101442757B1