Semiconductor device and manufacturing method therefor

By using at least two stacked etch stop layers and protective layers during the manufacturing process of semiconductor devices, trenches are formed to connect the top metal layer, and the electrical connection problem caused by copper diffusion is solved and the yield of hybrid bonding is improved And reduces the risk of silicon nitride layer peeling.

WO2024234583A1PCT designated stage expired Publication Date: 2024-11-21WUHAN XINXIN SEMICON MFG CO LTD

Patent Information

Application Number
PCT/CN2023/130213
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-17
Filing Date
2023-11-07
Publication Date
2024-11-21

AI Technical Summary

Technical Problem

During the hybrid bonding process of semiconductor devices, copper diffusion leads to electrical connection problems and circuit breakage, which is difficult to effectively solve in the prior art, and increasing the thickness of the silicon nitride layer will lead to an increase in the risk of peeling.

Method used

The top metal layer is covered with at least two stacked etch stop layers, forming through holes and filling the protective layer, removing the protective layer and bonding layer to form trenches, exposing the top metal layer, and filling the trenches and through holes Metal layer to connect the top metal layer.

Benefits of technology

It effectively improves metal diffusion problems, improves the yield of hybrid bonding, avoids electrical connection problems and circuit breakers, and reduces the risk of silicon nitride layer peeling.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2023130213_21112024_PF_FP_ABST
    Figure CN2023130213_21112024_PF_FP_ABST
Patent Text Reader

Abstract

A semiconductor device and a manufacturing method therefor. The manufacturing method for the semiconductor device comprises: providing a wafer (21), a top metal layer (213) being formed on the wafer (21), an etching stop layer (22) covering the top metal layer (213), and the etching stop layer (22) being of a structure where at least two layers are stacked; forming a bonding layer (23) on the etching stop layer (22); etching the bonding layer (23), and stopping etching in the non-bottommost layer structure of the etching stop layer (22) so as to form a through hole (24); filling a protective layer (25) in the through hole (24); etching to remove part of the protective layer (25) in the through hole (24) and the bonding layer (23) at the top of the side wall of the through hole (24) so as to form a groove (26) at the top of the through hole (24); removing the rest of the protective layer (25); etching to remove the etching stop layer (22) on the bottom surface of the through hole (24) so as to expose the top metal layer (213); and filling a metal layer (27) in the groove (26) and the through hole (24), the metal layer (27) being connected to the top metal layer (213). Therefore, the problem of metal diffusion can be ameliorated, thereby increasing the hybrid bonding yield.
Need to check novelty before this filing date? Find Prior Art

Description

Semiconductor device and method for manufacturing the same Technical Field

[0001] The present invention relates to the field of semiconductor integrated circuit manufacturing, and in particular to a semiconductor device and a manufacturing method thereof. Background Art

[0002] With the development of chip technology, the multi-chip stacking process has received more and more attention in the industry, among which the hybrid bonding process is more widely used.

[0003] Before bonding, a silicon nitride layer and a bonding layer are formed on the wafers to be bonded; then, a through hole is etched in the bonding layer, and the etching stops in the silicon nitride layer; then, a bottom anti-reflection layer is filled in the through hole; then, the bonding layer and the bottom anti-reflection layer on the top of the through hole sidewall are etched to form a groove at the top of the through hole; then, the remaining bottom anti-reflection layer and the silicon nitride layer on the bottom of the through hole are removed; then, a metal layer is filled in the groove and the through hole to facilitate bonding between the bonding layers on the two wafers and bonding between the metal layers in the subsequent hybrid bonding process.

[0004] As shown in FIG1 , a silicon nitride layer 13 and a bonding layer 14 are formed on the wafer 11 to be bonded, and a top metal layer 12 is formed on the top of the wafer 11. In the wafer 11 to be bonded, the top metal layer 12 (for example, copper) is used as a redistribution layer and is usually thicker, which makes it easy for a hillock 121 to form on the top metal layer 12. The silicon nitride layer 13 on the hillock 121 is much thinner than the silicon nitride layer 13 at other locations, and silicon nitride is very brittle, which makes it easy for the hillock 121 to crack the silicon nitride layer 13 thereon. In addition, during the process of etching to form a through hole, a small amount of etching will also be performed on the silicon nitride layer 13, thereby exposing the hillock 121 and causing metal diffusion problems. As shown in FIG2 , after copper diffusion, pits 122 are formed in the top metal layer 12, and the metal diffuses to the inner wall of the through hole and the surface of the wafer 11, thereby causing electrical connection problems or even short circuits between the bonded wafers. Increasing the thickness of the silicon nitride layer 13 can prevent metal diffusion, but this will increase the risk of peeling of the silicon nitride layer 13 itself.

[0005] Therefore, how to improve the copper diffusion problem to increase the hybrid bonding yield is an issue that needs to be addressed urgently.

[0006] Summary of the Invention

[0007] An object of the present invention is to provide a semiconductor device and a method for manufacturing the same, which can improve the metal diffusion problem and thereby increase the hybrid bonding yield.

[0008] To achieve the above object, the present invention provides a method for manufacturing a semiconductor device, comprising:

[0009] Providing a wafer, wherein the wafer is formed with a top metal layer, an etch stop layer covers the top metal layer, and the etch stop layer is a stacked structure of at least two layers;

[0010] forming a bonding layer on the etch stop layer;

[0011] Etching the bonding layer, and stopping the etching at the non-bottommost structure of the etch stop layer to form a through hole;

[0012] Filling a protective layer in the through hole;

[0013] Etching and removing a portion of the protection layer in the through hole and the bonding layer on the top of the through hole sidewall to form a trench on the top of the through hole;

[0014] removing the remaining protective layer;

[0015] Etching and removing the etch stop layer on the bottom surface of the through hole to expose the top metal layer;

[0016] A metal layer is filled in the trench and the through hole, and the metal layer is connected to the top metal layer.

[0017] Optionally, the etch stop layer includes an oxide layer and a silicon nitride layer stacked from bottom to top, and when the through hole is formed, the etching stops in the silicon nitride layer; or, the etch stop layer includes a first silicon nitride layer, an oxide layer and a second silicon nitride layer stacked from bottom to top, and when the through hole is formed, the etching stops in the second silicon nitride layer or the oxide layer.

[0018] Optionally, the material of the oxide layer includes silicon oxide and / or silicon oxynitride.

[0019] Optionally, the bonding layer is a multi-layer stacked structure.

[0020] Optionally, the protective layer includes at least one of an anti-reflection layer, spin-on carbon, and spin-on glass.

[0021] Optionally, the method for manufacturing the semiconductor device further includes:

[0022] At least two wafers are bonded together, wherein the bonding layers on adjacent wafers are bonded together, and the metal layers on adjacent wafers are bonded together.

[0023] The present invention also provides a semiconductor device, comprising:

[0024] a substrate having a top metal layer formed thereon;

[0025] an etch-stop layer covering the top metal layer, wherein the etch-stop layer is a stacked structure of at least two layers, and a through hole is formed in the etch-stop layer to expose the top metal layer;

[0026] a bonding layer formed on the etch-stop layer, wherein a groove is formed in the bonding layer, the through hole extends from the etch-stop layer into the bonding layer and communicates with the groove, and the width of the groove is greater than the width of the through hole;

[0027] A metal layer is filled in the groove and the through hole, and the metal layer is connected to the top metal layer.

[0028] Optionally, the etch stop layer includes an oxide layer and a silicon nitride layer stacked from bottom to top, or the etch stop layer includes a first silicon nitride layer, an oxide layer, and a second silicon nitride layer stacked from bottom to top.

[0029] Optionally, the material of the oxide layer includes silicon oxide and / or silicon oxynitride.

[0030] Optionally, the semiconductor device includes at least two bonded substrates, wherein the bonding layers on adjacent substrates are bonded, and the metal layers on adjacent substrates are bonded.

[0031] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:

[0032] 1. The manufacturing method of the semiconductor device of the present invention comprises the following steps: forming an etch stop layer on a wafer, wherein the etch stop layer covers a top metal layer, and the etch stop layer is a structure of at least two stacked layers; forming a bonding layer on the etch stop layer; etching the bonding layer, and stopping the etching in a non-bottom structure of the etch stop layer to form a through hole; filling the through hole with a protective layer; etching away a portion of the protective layer in the through hole and the bonding layer on the top of the through hole sidewall to form a groove at the top of the through hole; removing the remaining protective layer; etching away the etch stop layer on the bottom surface of the through hole to expose the top metal layer; filling the metal layer in the groove and the through hole, wherein the metal layer is connected to the top metal layer, so that the metal diffusion problem can be improved, thereby improving the hybrid bonding yield.

[0033] 2. The semiconductor device of the present invention comprises: a substrate, a top metal layer is formed on the substrate; an etch stop layer, covering the top metal layer, the etch stop layer is a structure of at least two stacked layers, and a through hole exposing the top metal layer is formed in the etch stop layer; a bonding layer, formed on the etch stop layer, a groove is formed in the bonding layer, the through hole extends from the etch stop layer into the bonding layer and is connected to the groove, and the width of the groove is greater than the width of the through hole; a metal layer, filling the groove and the through hole, the metal layer is connected to the top metal layer, so that the metal diffusion problem can be improved, thereby improving the hybrid bonding yield. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] FIG1 is a schematic diagram of a hillock formed on a top metal layer in a wafer;

[0035] FIG2 is a scanning electron microscope image of metal diffusion occurring in the top metal layer of a wafer;

[0036] 3 is a flow chart of a method for manufacturing a semiconductor device according to an embodiment of the present invention;

[0037] 4 a to 4 k are schematic diagrams of devices in the method for manufacturing the semiconductor device shown in FIG. 3 .

[0038] Among them, the figure marks in Figures 1 to 4k are explained as follows: 11-wafer; 12-top metal layer; 121-hill; 122-pit; 13-silicon nitride layer; 14-bonding layer; 21-wafer; 211-substrate; 212-insulating dielectric layer; 213-top metal layer; 22-etch stop layer; 221-first silicon nitride layer; 222-oxide layer; 223-second silicon nitride layer; 23-bonding layer; 231-first dielectric layer; 232-second dielectric layer; 233-third dielectric layer; 24-through hole; 241-first patterned photoresist layer; 25-protective layer; 26-groove; 261-second patterned photoresist layer; 27-metal layer. DETAILED DESCRIPTION

[0039] To make the objectives, advantages, and features of the present invention more apparent, the semiconductor device and its manufacturing method proposed in the present invention are further described in detail below. It should be noted that the drawings are all in a very simplified form and are not to exact scale, and are only used to facilitate and clearly illustrate the purpose of the embodiments of the present invention.

[0040] An embodiment of the present invention provides a method for manufacturing a semiconductor device. Referring to FIG. 3 , it can be seen from FIG. 3 that the method for manufacturing a semiconductor device includes:

[0041] Step S1, providing a wafer, wherein the wafer is formed with a top metal layer, and an etch stop layer covers the top metal layer, wherein the etch stop layer is a stacked structure of at least two layers;

[0042] Step S2, forming a bonding layer on the etch stop layer;

[0043] Step S3, etching the bonding layer, and stopping the etching at the non-bottommost structure of the etch stop layer to form a through hole;

[0044] Step S4, filling the through hole with a protective layer;

[0045] Step S5, etching and removing a portion of the protection layer in the through hole and the bonding layer on the top of the through hole sidewall to form a trench on the top of the through hole;

[0046] Step S6, removing the remaining protective layer;

[0047] Step S7, etching away the etch stop layer on the bottom surface of the through hole to expose the top metal layer;

[0048] Step S8: Filling the grooves and the through holes with a metal layer, wherein the metal layer is connected to the top metal layer.

[0049] The manufacturing method of the semiconductor device provided in this embodiment will be described in detail below with reference to FIG. 4 a to FIG. 4 k . FIG. 4 a to FIG. 4 k are also schematic longitudinal cross-sectional views.

[0050] According to step S1 , referring to FIG. 4 a , a wafer 21 is provided. The wafer 21 is formed with a top metal layer 213 .

[0051] The wafer 21 includes a substrate 211 and an insulating dielectric layer 212 formed on the substrate 211, the top metal layer 213 is formed in the insulating dielectric layer 212, and the insulating dielectric layer 212 exposes the top metal layer 213; the insulating dielectric layer 212 also has structures such as a metal interconnection structure formed therein, and the top metal layer 213 serves as a redistribution layer and is electrically connected to the metal interconnection structure.

[0052] The wafer 21 may be a device wafer or a carrier wafer.

[0053] The device wafer can be a pixel wafer containing a pixel array of an image sensor, or a MEMS wafer containing a MEMS microstructure of a MEMS device, or a MOSFET wafer containing a power device, or an IGBT wafer, or a passive device wafer, etc. The type of device wafer depends on the function of the device to be manufactured. The carrier wafer may not contain a functional structure; or the carrier wafer may contain a functional structure, and the functional structure is located inside the carrier wafer rather than on the surface of the carrier wafer. In some embodiments, the functional structure contained in the carrier wafer may also be located inside and / or on the surface of the wafer edge.

[0054] The top metal layer 213 may be made of metal materials such as copper or aluminum.

[0055] In the wafer 21, the top metal layer 213 serves as a redistribution layer and is usually thicker, which makes the stress change of the top metal layer 213 more obvious under the high temperature environment during the process, and then the crystal recrystallization or growth will occur, resulting in the easy formation of hillocks on the top metal layer 213 (i.e., the hillock 121 shown in Figure 1); among them, when the material of the top metal layer 213 is copper, due to the very good diffusion of copper, it is easier to form hillocks on the top metal layer 213.

[0056] Furthermore, an etch stop layer 22 is formed on the wafer 21 . The etch stop layer 22 covers the top metal layer 213 . The etch stop layer 22 is a stacked structure of at least two layers.

[0057] In the embodiments shown in Figures 4a to 4k, the etch-stop layer 22 includes a first silicon nitride layer 221, an oxide layer 222, and a second silicon nitride layer 223 stacked from bottom to top. Alternatively, in another embodiment, the etch-stop layer 22 includes an oxide layer and a silicon nitride layer stacked from bottom to top. The structure of the etch-stop layer 22 is not limited to the above embodiment. In other embodiments, the etch-stop layer 22 may also be formed by alternating multiple oxide and silicon nitride layers.

[0058] The material of the oxide layer may include silicon oxide and / or silicon oxynitride.

[0059] According to step S2 , referring to FIG. 4 a , a bonding layer 23 is formed on the etch stop layer 22 .

[0060] Preferably, the bonding layer 23 is a multi-layer stacked structure.

[0061] In the embodiment shown in Figures 4a to 4j, the bonding layer 23 includes a first dielectric layer 231, a second dielectric layer 232, and a third dielectric layer 233 stacked from bottom to top. In one embodiment, the first dielectric layer 231 and the third dielectric layer 233 may be made of oxide layers such as silicon oxide and / or silicon oxynitride, and the second dielectric layer 232 may be made of nitrogen-doped silicon carbide. In other embodiments, the first dielectric layer 231, the second dielectric layer 232, and the third dielectric layer 233 may be made of other insulating materials.

[0062] According to step S3 , the bonding layer 23 is etched, and the etching stops at the non-bottommost structure of the etch stop layer 22 to form a through hole 24 .

[0063] Among them, it should be noted that etching stops at the non-bottom-most structure of the etch stop layer 22, including: etching stops at the top surface of the topmost structure of the etch stop layer 22, that is, the bonding layer 23 is just etched through; or, etching stops inside the non-bottom-most structure of the etch stop layer 22, that is, after the bonding layer 23 is etched through, the non-bottom-most structure of the etch stop layer 22 is also etched to remove part of its thickness; or, etching stops at the top surface of the bottom-most structure of the etch stop layer 22, that is, after the bonding layer 23 is etched through, the non-bottom-most structure of the etch stop layer 22 is also just etched through to expose the bottom-most structure of the etch stop layer 22.

[0064] If the etch stop layer 22 includes an oxide layer and a silicon nitride layer stacked from bottom to top, the etching stops in the silicon nitride layer when the through hole 24 is formed; if the etch stop layer 22 includes a first silicon nitride layer 221, an oxide layer 222 and a second silicon nitride layer 223 stacked from bottom to top, the etching stops in the second silicon nitride layer 223 or the oxide layer 222 when the through hole 24 is formed.

[0065] 4 b to 4 d , the steps of forming the through hole 24 may include: first, as shown in FIG 4 b , forming a first patterned photoresist layer 241 on the third dielectric layer 233 ; then, as shown in FIG 4 c , using the first patterned photoresist layer 241 as a mask, sequentially etching the third dielectric layer 233 , the second dielectric layer 232 , and the first dielectric layer 231 , and stopping in the second silicon nitride layer 223 ; and then, as shown in FIG 4 d , removing the first patterned photoresist layer 241 .

[0066] In addition, after forming the through hole 24 and before subsequently filling the through hole 24 with a protection layer 25 , the method for manufacturing the semiconductor device further includes: performing a wet cleaning process to remove byproducts generated by etching.

[0067] Since the etch stop layer 22 is a structure of at least two stacked layers, and when etching to form the through hole 24, the etching stops in the non-bottommost structure of the etch stop layer 22, compared with the single-layer silicon nitride layer 13 shown in Figure 1 as the etch stop layer, the etch stop layer 22 in the embodiment of the present invention has more layers and a thicker thickness, so that during the process of etching to form the through hole 24, the hillock on the top metal layer 213 can always be wrapped and protected by the thicker etch stop layer 22, and the bottommost structure of the etch stop layer 22 is pressed by the non-bottommost structure, which can improve the situation where the bottommost structure of the etch stop layer 22 is topped by the hillock on the top metal layer 213; and after etching to form the through hole 24, at least the bottommost structure of the etch stop layer 22 with the entire thickness wraps the top metal layer 213, so that during the subsequent wet cleaning process, the bottommost structure of the etch stop layer 22 can continue to protect the hillock on the top metal layer 213. Therefore, the embodiments of the present invention can prevent the hillocks on the top metal layer 213 from being exposed during and after etching to form the through hole 24, and further prevent the hillocks on the top metal layer 213 from reacting with the cleaning liquid during the wet cleaning process, thereby improving the metal diffusion problem.

[0068] Moreover, when the etch stop layer 22 includes a first silicon nitride layer 221, an oxide layer 222, and a second silicon nitride layer 223 stacked from bottom to top, or the etch stop layer 22 includes an oxide layer and a silicon nitride layer stacked from bottom to top, since the brittleness of oxides such as silicon oxide and / or silicon oxynitride is lower than that of silicon nitride, the oxide has better wrapping properties, and thus if the oxide layer wraps the first silicon nitride layer, the first silicon nitride layer is not easy to crack, and if the oxide layer directly wraps the hillock, the oxide layer is not easy to crack. Therefore, it is possible to further avoid the hillock on the top metal layer 213 from being exposed when etching to form the through hole 24.

[0069] Moreover, when the etch stop layer 22 includes a first silicon nitride layer 221, an oxide layer 222, and a second silicon nitride layer 223 stacked from bottom to top, and the etching stops at the second silicon nitride layer 223 when forming the through hole 24, even if the first silicon nitride layer 221 is cracked, the oxide layer 222 serves as a buffer layer to wrap the cracked first silicon nitride layer 221 and the hillock on the top metal layer 213, thereby further preventing the hillock on the top metal layer 213 from being exposed.

[0070] According to step S4 , referring to FIG. 4 e , the protection layer 25 is filled in the through hole 24 .

[0071] The protection layer 25 may also cover the surface of the bonding layer 23 .

[0072] The protective layer 25 includes at least one of an anti-reflection layer, spin-on carbon, and spin-on glass.

[0073] The anti-reflection layer may be formed of a nitride material, an organic material, an oxide material, or the like.

[0074] According to step S5, referring to Figures 4f to 4g, a portion of the protection layer 25 in the through hole 24 and the bonding layer 23 on the top of the sidewall of the through hole 24 are etched away to form a trench 26 on the top of the through hole 24. The width of the trench 26 is greater than the width of the through hole 24.

[0075] The step of forming the groove 26 at the top of the through hole 24 may include: first, as shown in Figure 4f, forming a second patterned photoresist layer 261 on the protective layer 25; then, as shown in Figure 4g, using the second patterned photoresist layer 261 as a mask, etching the protective layer 25 and the bonding layer 23 at the top of the side wall of the through hole 24 to form the groove 26 at the top of the through hole 24.

[0076] Among them, after etching to form the groove 26, a partial thickness of the protective layer 25 still remains in the through hole 24. The protective layer 25 can protect the etch stop layer 22 on the bottom surface of the through hole 24 during the process of etching to form the groove 26, thereby preventing the etch stop layer 22 on the bottom surface of the through hole 24 from being etched, thereby preventing the hillock on the top metal layer 213 from being exposed.

[0077] According to step S6 , referring to FIG. 4 h , the remaining protection layer 25 is removed.

[0078] The protective layer 25 remaining in the through hole 24 , the protective layer 25 on the bonding layer 23 , and the second patterned photoresist layer 261 may be removed by an ashing process.

[0079] According to step S7 , referring to FIG. 4 i , the etch stop layer 22 on the bottom surface of the through hole 24 is removed by etching to expose the top metal layer 213 .

[0080] Furthermore, while the etch stop layer 22 on the bottom surface of the through hole 24 is being etched away, a portion of the top surface of the bonding layer 23 and the inner wall of the trench 26 will also be etched away.

[0081] According to step S8 , referring to FIG. 4 j to FIG. 4 k , a metal layer 27 is filled in the trench 26 and the through hole 24 , and the metal layer 27 is electrically connected to the top metal layer 213 .

[0082] When the bonding layer 23 includes a first dielectric layer 231, a second dielectric layer 232 and a third dielectric layer 233 stacked from bottom to top, the step of filling the metal layer 27 in the groove 26 and the through hole 24 may include: first, as shown in Figure 4j, filling the metal layer 27 in the groove 26 and the through hole 24, and the metal layer 27 covers the third dielectric layer 233; then, as shown in Figure 4k, using a chemical mechanical polishing process to polish and remove the metal layer 27 and the third dielectric layer 233 above the second dielectric layer 232, so that in the subsequent bonding process, the second dielectric layers 232 on adjacent wafers 21 are bonded.

[0083] Among them, the part of the metal layer 27 located in the through hole 24 is a transfer layer, which is used to electrically connect with the top metal layer 213; the part of the metal layer 27 located in the groove 26 is a bonding pad, which is used for subsequent bonding processes.

[0084] The method for manufacturing the semiconductor device may further include: bonding at least two wafers 21 , wherein the bonding layers 23 on adjacent wafers 21 are bonded to each other, and the metal layers 27 on adjacent wafers 21 are bonded to each other.

[0085] From the above content, it can be seen that in the manufacturing process of the semiconductor device, since the etch stop layer 22 can always protect the hillock on the top metal layer 213 and avoid it from being exposed, the metal diffusion problem is improved, and the formation of pits in the top metal layer 213 (i.e., the pits 122 in Figure 2) is avoided, and the metal is prevented from diffusing to the surface of the through hole 24 and the groove 26, thereby avoiding electrical connection problems or even circuit breaks between the subsequently bonded wafers, thereby improving the hybrid bonding yield.

[0086] In addition, it should be noted that a wafer structure is formed by using the above-mentioned semiconductor device manufacturing method, and the wafer structure includes a chip structure arranged in an array, and a cutting path is provided between adjacent chip structures. The semiconductor device manufacturing method may also include: cutting the wafer structure along the cutting path to separate the chip structure arranged in an array.

[0087] Furthermore, the semiconductor device shown in FIG. 4 k may be a part of the wafer structure or the chip structure.

[0088] In summary, the present invention provides a method for manufacturing a semiconductor device, comprising: providing a wafer, wherein the wafer is formed with a top metal layer, an etch stop layer covers the top metal layer, and the etch stop layer is a structure of at least two stacked layers; forming a bonding layer on the etch stop layer; etching the bonding layer, and etching stops at the non-bottommost structure of the etch stop layer to form a through hole; filling a protective layer in the through hole; etching away a portion of the protective layer in the through hole and the bonding layer on the top of the through hole sidewall to form a groove at the top of the through hole; removing the remaining protective layer; etching away the etch stop layer on the bottom surface of the through hole to expose the top metal layer; filling a metal layer in the groove and the through hole, wherein the metal layer is connected to the top metal layer. The method for manufacturing a semiconductor device provided by the present invention can improve the metal diffusion problem, thereby improving the hybrid bonding yield.

[0089] An embodiment of the present invention provides a semiconductor device, comprising: a substrate, a top metal layer formed above the substrate; an etch stop layer, covering the top metal layer, the etch stop layer being a structure of at least two stacked layers, a through hole formed in the etch stop layer exposing the top metal layer; a bonding layer, formed on the etch stop layer, a groove formed in the bonding layer, the through hole extending from the etch stop layer into the bonding layer and connected to the groove, the width of the groove being greater than the width of the through hole; a metal layer filling the groove and the through hole, the metal layer being connected to the top metal layer.

[0090] The semiconductor device provided in this embodiment is described in detail below with reference to FIG4k , which is also a schematic longitudinal cross-sectional view.

[0091] A top metal layer 213 is formed on the substrate 211 .

[0092] An insulating dielectric layer 212 is formed on the substrate 211, and the top metal layer 213 is formed in the insulating dielectric layer 212, and the insulating dielectric layer 212 exposes the top metal layer 213; a metal interconnection structure and other structures are also formed in the insulating dielectric layer 212, and the top metal layer 213 serves as a redistribution layer and is electrically connected to the metal interconnection structure.

[0093] The top metal layer 213 may be made of metal materials such as copper or aluminum.

[0094] The top metal layer 213 serves as a redistribution layer and is usually thicker, which makes the stress change of the top metal layer 213 more obvious under the high temperature environment during the process, and then the crystal recrystallization or growth will occur, resulting in the easy formation of hillocks on the top metal layer 213 (i.e., the hillock 121 shown in Figure 1); among them, when the material of the top metal layer 213 is copper, due to the very good diffusion of copper, it is easier to form hillocks on the top metal layer 213.

[0095] The etch stop layer 22 is formed on the insulating dielectric layer 212 , and covers the top metal layer 213 . The etch stop layer 22 is a stacked structure of at least two layers, and a through hole exposing the top metal layer 213 is formed in the etch stop layer 22 .

[0096] In the embodiment shown in FIG4k , the etch-stop layer 22 includes a first silicon nitride layer 221, an oxide layer 222, and a second silicon nitride layer 223 stacked from bottom to top. Alternatively, in another embodiment, the etch-stop layer 22 includes an oxide layer and a silicon nitride layer stacked from bottom to top. The structure of the etch-stop layer 22 is not limited to the above embodiment. In other embodiments, the etch-stop layer 22 may also be formed by alternating multiple oxide and silicon nitride layers.

[0097] The material of the oxide layer may include silicon oxide and / or silicon oxynitride.

[0098] The bonding layer 23 is formed on the etch stop layer 22, and a groove is formed in the bonding layer 23. The through hole extends from the etch stop layer 22 to the bottom surface of the groove in the bonding layer 23, and the through hole is connected to the groove. The width of the groove is greater than the width of the through hole.

[0099] Preferably, the bonding layer 23 is a multi-layer stacked structure.

[0100] The bonding layer 23 may include a first dielectric layer 231, a second dielectric layer 232, and a third dielectric layer 233 stacked from bottom to top. In one embodiment, the first dielectric layer 231 and the third dielectric layer 233 may be made of oxide layers such as silicon oxide and / or silicon oxynitride, and the second dielectric layer 232 may be made of nitrogen-doped silicon carbide. In other embodiments, the first dielectric layer 231, the second dielectric layer 232, and the third dielectric layer 233 may be made of other insulating materials.

[0101] In the embodiment shown in FIG. 4 k , the bonding layer 23 includes a first dielectric layer 231 and a second dielectric layer 232 stacked from bottom to top.

[0102] The metal layer 27 fills the grooves and the through holes, and the metal layer 27 is electrically connected to the top metal layer 213 .

[0103] Among them, the part of the metal layer 27 located in the through hole is a transfer layer, which is used to electrically connect with the top metal layer 213; the part of the metal layer 27 located in the groove is a bonding pad, which is used for subsequent bonding processes.

[0104] The semiconductor device may include only a single substrate 211; or the semiconductor device may include at least two bonded substrates 211, wherein the bonding layers 23 on adjacent substrates 211 are bonded, and the metal layers 27 on adjacent substrates 211 are bonded. When the bonding layer 23 includes a first dielectric layer 231 and a second dielectric layer 232 stacked from bottom to top, the second dielectric layers 232 on adjacent substrates 211 are bonded.

[0105] Since the etch stop layer 22 is a structure of at least two stacked layers, when etching to form the through hole, etching can stop at the non-bottommost structure of the etch stop layer 22. Therefore, compared with the single-layer silicon nitride layer 13 shown in Figure 1 as the etch stop layer, the etch stop layer 22 in the embodiment of the present invention has more layers and a thicker thickness. Therefore, during the process of etching to form the through hole, the hillock on the top metal layer 213 can always be wrapped and protected by the thicker etch stop layer 22, and the bottommost structure of the etch stop layer 22 is pressed by the non-bottommost structure, which can improve the situation where the bottommost structure of the etch stop layer 22 is topped by the hillock on the top metal layer 213. Moreover, after etching to form the through hole, at least the bottommost structure of the etch stop layer 22 with the entire thickness wraps the top metal layer 213, so that during the subsequent wet cleaning process, the bottommost structure of the etch stop layer 22 can continue to protect the hillock on the top metal layer 213. Therefore, the embodiments of the present invention can prevent the hillocks on the top metal layer 213 from being exposed during and after etching to form the through holes, thereby preventing the hillocks on the top metal layer 213 from reacting with the cleaning liquid during the wet cleaning process, thereby improving the metal diffusion problem.

[0106] Moreover, when the etch stop layer 22 includes a first silicon nitride layer 221, an oxide layer 222, and a second silicon nitride layer 223 stacked from bottom to top, or the etch stop layer 22 includes an oxide layer and a silicon nitride layer stacked from bottom to top, since the brittleness of oxides such as silicon oxide and / or silicon oxynitride is lower than that of silicon nitride, the oxide has better wrapping properties, and thus if the oxide layer wraps the first silicon nitride layer, the first silicon nitride layer is not easy to crack, and if the oxide layer directly wraps the hillock, the oxide layer is not easy to crack. Therefore, it is possible to further avoid the hillock on the top metal layer 213 from being exposed when etching to form the through hole.

[0107] Moreover, when the etch stop layer 22 includes a first silicon nitride layer 221, an oxide layer 222, and a second silicon nitride layer 223 stacked from bottom to top, and the etching stops at the second silicon nitride layer 223 when forming the through hole, even if the first silicon nitride layer 221 is cracked, the oxide layer 222 serves as a buffer layer to wrap the cracked first silicon nitride layer 221 and the hillock on the top metal layer 213, thereby further preventing the hillock on the top metal layer 213 from being exposed.

[0108] From the above content, it can be seen that since the etch stop layer 22 can ensure that the hillock on the top metal layer 213 is always protected and avoided from being exposed during the manufacturing process of the semiconductor device, the metal diffusion problem is improved, and the formation of pits in the top metal layer 213 (i.e., the pits 122 in Figure 2) is avoided, and the metal is avoided from diffusing to the through hole and the groove surface, thereby avoiding electrical connection problems or even circuit breaks between subsequently bonded wafers, thereby improving the hybrid bonding yield.

[0109] In addition, it should be noted that the above-mentioned semiconductor device can be a wafer structure or a chip structure. The wafer structure includes the chip structures arranged in an array, and cutting paths are provided between adjacent chip structures. By cutting the wafer structure along the cutting paths, the chip structures arranged in an array can be separated.

[0110] Furthermore, the semiconductor device shown in FIG. 4 k may be a part of the wafer structure or the chip structure.

[0111] The wafer 21 in the wafer structure may be a device wafer or a carrier wafer.

[0112] The device wafer can be a pixel wafer containing a pixel array of an image sensor, or a MEMS wafer containing a MEMS microstructure of a MEMS device, or a MOSFET wafer containing a power device, or an IGBT wafer, or a passive device wafer, etc. The type of device wafer depends on the function of the device to be manufactured. The carrier wafer may not contain a functional structure; or the carrier wafer may contain a functional structure, and the functional structure is located inside the carrier wafer rather than on the surface of the carrier wafer. In some embodiments, the functional structure contained in the carrier wafer may also be located inside and / or on the surface of the wafer edge.

[0113] In summary, the present invention provides a semiconductor device comprising: a substrate having a top metal layer formed thereon; an etch-stop layer covering the top metal layer, the etch-stop layer being a stacked structure of at least two layers, the etch-stop layer having a through-hole formed therein that exposes the top metal layer; a bonding layer formed on the etch-stop layer, the bonding layer having a trench formed therein, the through-hole extending from the etch-stop layer into the bonding layer and communicating with the trench, the trench having a width greater than the width of the through-hole; and a metal layer filling the trench and the through-hole, the metal layer being connected to the top metal layer. The semiconductor device provided by the present invention can improve metal diffusion issues and thereby enhance hybrid bonding yield.

[0114] The above description is only a description of the preferred embodiments of the present invention and does not limit the scope of the present invention. Any changes and modifications made by ordinary technicians in the field of the present invention based on the above disclosure shall fall within the scope of protection of the claims.

Claims

1. A method for manufacturing a semiconductor device, characterized in that: include: A wafer is provided, wherein the wafer is formed with a top metal layer, an etch stop layer covers the top metal layer, and the etch stop layer is a structure of at least two stacked layers; forming a bonding layer on the etch stop layer; Etching the bonding layer, and stopping the etching in the non-bottommost structure of the etch stop layer to form a through hole; Filling a protective layer in the through hole; Etching and removing a portion of the protection layer in the through hole and the bonding layer on the top of the through hole sidewall to form a groove on the top of the through hole; removing the remaining protective layer; Etching and removing the etch stop layer on the bottom surface of the through hole to expose the top metal layer; A metal layer is filled in the groove and the through hole, and the metal layer is connected to the top metal layer.

2. The method for manufacturing a semiconductor device according to claim 1, wherein: The etch stop layer includes an oxide layer and a silicon nitride layer stacked from bottom to top, and when the through hole is formed, the etching stops in the silicon nitride layer; or, the etch stop layer includes a first silicon nitride layer, an oxide layer, and a second silicon nitride layer stacked from bottom to top, and when the through hole is formed, the etching stops in the second silicon nitride layer or the oxide layer.

3. The method for manufacturing a semiconductor device according to claim 2, wherein: The material of the oxide layer includes silicon oxide and / or silicon oxynitride.

4. The method for manufacturing a semiconductor device according to claim 1, wherein: The bonding layer is a multi-layer stacked structure.

5. The method for manufacturing a semiconductor device according to claim 1, wherein: The protective layer includes at least one of an anti-reflection layer, spin-on carbon, and spin-on glass.

6. The method for manufacturing a semiconductor device according to any one of claims 1 to 5, wherein: The method for manufacturing the semiconductor device further includes: At least two of the wafers are bonded, wherein the bonding layers on adjacent wafers are The metal layers on adjacent wafers are bonded.

7. A semiconductor device, characterized in that: include: A substrate having a top metal layer formed thereon; An etch stop layer, covering the top metal layer, wherein the etch stop layer is a structure of at least two stacked layers, and a through hole exposing the top metal layer is formed in the etch stop layer; A bonding layer is formed on the etch stop layer, a groove is formed in the bonding layer, the through hole extends from the etch stop layer into the bonding layer and is connected with the groove, and the width of the groove is greater than the width of the through hole; A metal layer is filled in the groove and the through hole, and the metal layer is connected to the top metal layer.

8. The semiconductor device according to claim 7, wherein: The etch stop layer includes an oxide layer and a silicon nitride layer stacked from bottom to top, or the etch stop layer includes a first silicon nitride layer, an oxide layer, and a second silicon nitride layer stacked from bottom to top.

9. The semiconductor device according to claim 8, characterized in that The material of the oxide layer includes silicon oxide and / or silicon oxynitride.

10. The semiconductor device according to any one of claims 7 to 9, wherein: The semiconductor device includes at least two bonded substrates, wherein the bonding layers on adjacent substrates are bonded, and the metal layers on adjacent substrates are bonded.

Citation Information

Patent Citations

  • Dual-damascene structure and manufacturing method thereof

    CN101625993A

  • Semiconductor device and manufacturing method thereof

    CN110581117A

  • Manufacturing method of semiconductor

    CN110911292A

  • Semiconductor device and manufacturing method thereof

    CN110931373A

  • Semiconductor structure and preparation method thereof

    CN115064513A

Cited By

  • Semiconductor manufacturing method and semiconductor structure

    CN119864322A

  • Manufacturing method of backside illuminated image sensor and backside illuminated image sensor