Minority carrier lifetime determination method, crystal pulling method, and silicon wafer for solar cell
By determining and adjusting the minus sub-life data of pre-drawn silicon rods on the same furnace and optimizing the resistivity and thickness of the silicon wafer, the bottleneck of silicon wafer efficiency improvement in the photovoltaic industry is solved and the efficiency of the entire furnace silicon wafer of solar cells is improved.
Patent Information
- Application Number
- PCT/CN2024/089398
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-12
- Filing Date
- 2024-04-23
- Publication Date
- 2024-11-21
AI Technical Summary
The efficiency improvement of silicon wafers in the existing photovoltaic industry has entered a bottleneck period, and the resistivity cannot be flexibly regulated to match the optimal battery efficiency parameters, resulting in loss of the efficiency of the entire furnace silicon wafer.
By determining the life data of pre-drawn silicon rods on the same furnace, establishing a life calculation model for the life of the silicon wafer, adjusting the resistivity and thickness of the silicon wafer, optimizing the drawing process of the silicon wafer, and improving the efficiency of the silicon wafer.
A method to improve the preparation efficiency of silicon wafers on the same furnace has been realized, the bottleneck problem of improving silicon wafer efficiency has been solved, and the battery conversion efficiency has been enhanced.
Smart Images

Figure CN2024089398_21112024_PF_FP_ABST
Abstract
Description
Minority carrier lifetime determination method, crystal pulling method, and silicon wafer for solar cells
[0001] This application claims priority to the Chinese patent application filed with the China Patent Office on May 12, 2023, with application number 202310541810.7 and invention name “Minority Carrier Lifetime Determination Method, Crystal Pulling Method and Silicon Wafer for Solar Cells”, the entire contents of which are incorporated by reference into this application. Technical Field
[0002] The present application relates to the field of crystal growth technology, and in particular to a method for determining minority carrier lifetime, a crystal pulling method, and a silicon wafer for solar cells. Background Art
[0003] With increasingly stringent environmental requirements, the demand for clean energy is increasing, and the photovoltaic industry is a key component of this clean energy supply. In the photovoltaic industry, multi-charge crystal pulling is a key technology for pulling single-crystal silicon rods. The specific process involves pulling cylindrical single-crystal silicon rods. When the single-crystal silicon rods are subsequently used to make solar cells, the cylindrical silicon rods are sequentially cut, squared, and sliced to form silicon wafers for use in the cells.
[0004] However, at present, with the development of the photovoltaic industry, the improvement of silicon wafer efficiency has entered a bottleneck period.
[0005] Summary of the Invention
[0006] Based on this, the present application provides a method for determining the minority carrier lifetime, a crystal pulling method, and a silicon wafer for solar cells, which is used to improve the efficiency of solar cells prepared by silicon wafers on the same furnace by determining the minority carrier lifetime data of silicon rods pre-pulled on the same furnace.
[0007] In a first aspect, the present application provides a method for determining minority carrier lifetime, which is applied to a pre-drawn silicon rod. The method for determining minority carrier lifetime comprises:
[0008] Obtain minority carrier lifetime curve of silicon wafer sample;
[0009] A minority carrier lifetime calculation model is established based on the minority carrier lifetime curve of the silicon wafer sample and the minority carrier lifetime simulation model; wherein the silicon wafer sample and the pre-drawn silicon rod are prepared on the same furnace;
[0010] Based on the minority carrier lifetime calculation model, minority carrier lifetime data at different positions of the pre-drawn silicon rod are determined.
[0011] When the above technical solution is adopted, the minority carrier lifetime curve of the silicon wafer samples produced by the silicon rods produced on the same furnace is obtained, and then a minority carrier lifetime calculation model is established based on the known minority carrier lifetime simulation model. Finally, based on the minority carrier lifetime calculation model, the minority carrier lifetime data of the silicon wafer at different positions of the pre-drawn silicon rod can be calculated. It should be understood that the cell efficiency is related to the resistivity of the silicon wafer, the silicon wafer minority carrier lifetime data, and the thickness of the silicon wafer. Therefore, after obtaining the minority carrier lifetime data of the silicon wafer, the present application can improve the efficiency of the silicon wafers drawn on the same furnace by adjusting the resistivity and / or thickness of the silicon wafer. This can solve the problem in the prior art that the minority carrier lifetime of multiple silicon rods drawn continuously gradually decreases, and the resistivity cannot be flexibly adjusted to match the optimal cell efficiency parameters, resulting in efficiency loss of the entire furnace of silicon wafers.
[0012] In a possible implementation, obtaining a minority carrier lifetime curve of a silicon wafer sample includes:
[0013] Selecting multiple silicon wafers from different positions of multiple continuously drawn single crystal silicon rods as silicon wafer samples;
[0014] After the silicon wafer samples are passivated, minority carrier lifetime data of each silicon wafer sample is measured to obtain a minority carrier lifetime curve of the silicon wafer sample.
[0015] When adopting the above-mentioned technical solution, the present application selects multiple silicon wafers from different positions of multiple silicon rods continuously drawn in the same furnace as silicon wafer samples. That is to say, the silicon wafer sample and the pre-drawn silicon wafer are drawn in the same furnace. On this basis, the silicon wafer sample is measured to obtain the minority carrier lifetime data of the silicon wafer sample, which can relatively accurately characterize the minority carrier lifetime data at different positions of the pre-drawn silicon rod belonging to the same cycle segment as the silicon wafer sample. Based on the minority carrier lifetime data, the resistivity of the silicon wafer is adjusted, which can accurately improve the efficiency of the silicon wafers drawn in the same furnace.
[0016] It should be noted that the same furnace platform in this application can be the same type of single crystal furnace (that is, the model, structure, etc. of the single crystal furnace are the same), and can also refer to the same single crystal furnace for continuously drawing multiple silicon rods.
[0017] In one possible implementation, establishing a minority carrier lifetime calculation model based on the minority carrier lifetime curve of the silicon wafer sample and the minority carrier lifetime simulation model includes:
[0018] Determining the relationship between the impurity concentration and the solidification fraction in the minority carrier lifetime simulation model according to the minority carrier lifetime curve of the silicon wafer sample and the minority carrier lifetime simulation model;
[0019] A minority carrier lifetime calculation model is established based on the relationship between the impurity concentration and the solidification fraction and the minority carrier lifetime simulation model.
[0020] When employing the above technical solution, the relationship between impurity concentration and solidification fraction in the minority carrier lifetime simulation model can be determined based on the known minority carrier lifetime simulation model and the minority carrier lifetime curve of the silicon wafer sample. It should be understood that when the relationship between impurity concentration and solidification fraction in the minority carrier lifetime simulation model is known, a minority carrier lifetime calculation model can be established based on the minority carrier lifetime simulation model to calculate minority carrier lifetime data at various positions on the pre-drawn silicon rod. This shows that the method for determining the minority carrier lifetime calculation model in this application is simple and requires little computation.
[0021] In a possible implementation, determining minority carrier lifetime data at different positions of the pre-drawn silicon rod based on the minority carrier lifetime calculation model includes:
[0022] Based on the minority carrier lifetime calculation model, the resistivity at different positions of the pre-drawn silicon rod, and the solidification fraction of the pre-drawn silicon rod, minority carrier lifetime data at various positions of the pre-drawn silicon rod are obtained.
[0023] When the above technical solution is adopted, the present application can determine the minority carrier lifetime data at each position of the pre-drawn silicon rod based on the resistivity at different positions of the pre-drawn silicon rod, the solidification fraction of the pre-drawn silicon rod, and the established minority carrier lifetime calculation model. It should be understood that the resistivity at different positions of the pre-drawn silicon rod and the solidification fraction of the pre-drawn silicon rod are data that can be determined before drawing the silicon rod. In other words, according to the method of the present application, the minority carrier lifetime data at each position of the pre-drawn silicon rod can be determined before drawing the silicon rod. Then, based on the minority carrier lifetime data at each position of the pre-drawn silicon rod, the efficiency of silicon wafers drawn on the same furnace can be optimized. According to the above description, the method of determining the minority carrier lifetime data at each position of the pre-drawn silicon rod in the present application is simple and effective.
[0024] In a second aspect, the present application further provides a crystal pulling method, the crystal pulling method comprising the following steps:
[0025] Determining the silicon wafer efficiency of the furnace according to minority carrier lifetime data at different positions of the pre-drawn silicon rod and adjusting the resistivity at different positions of the pre-drawn silicon rod; wherein the silicon wafer efficiency of the furnace meets the target efficiency requirement;
[0026] determining the doping amount at different positions of the pre-drawn silicon rod according to the silicon wafer efficiency of the furnace;
[0027] When the furnace is used to prepare a silicon single crystal, the furnace is doped according to the doping amount at different positions of the pre-pulled silicon rod to perform a crystal pulling process.
[0028] When the above technical solution is adopted, the battery efficiency is related to the resistivity of the silicon wafer, the minority carrier lifetime data of the silicon wafer, and the thickness of the silicon wafer. When the thickness of the silicon wafer has been determined, the present application adjusts the resistivity of the pre-drawn silicon rod at different positions based on the aforementioned determined minority carrier lifetime data at different positions of the pre-drawn silicon rod, thereby obtaining the optimal silicon wafer efficiency of the furnace. It should be understood that the doping amount at different positions of the silicon rod is determined by the preset resistivity at the corresponding position of the silicon rod. On this basis, the doping amount at the corresponding position of the pre-drawn silicon rod can be obtained according to the resistivity of the pre-drawn silicon rod at different positions after the above adjustment; based on this doping amount, the furnace is doped to produce a silicon rod that meets the optimal silicon wafer efficiency of the furnace, and then the silicon rod can be used to produce silicon wafers, thereby obtaining a high-efficiency battery.
[0029] In one possible implementation, determining the silicon wafer efficiency of the furnace according to minority carrier lifetime data at different positions of the pre-drawn silicon rod and adjusting the resistivity at different positions of the pre-drawn silicon rod includes:
[0030] Based on the whole furnace silicon wafer efficiency prediction model, the minority carrier lifetime data at different positions of the pre-drawn silicon rod and the silicon wafer thickness corresponding to different positions of the pre-drawn silicon rod, the resistivity at different positions of the pre-drawn silicon rod is adjusted to obtain the silicon wafer efficiency of the furnace.
[0031] Furthermore, the whole furnace silicon wafer efficiency prediction model satisfies: eff = f(ρ, τ, W);
[0032] The eff is the silicon wafer efficiency of the furnace, the τ is the minority carrier lifetime curve at the target position in the pre-drawn silicon rod, the W is the silicon wafer thickness corresponding to the corresponding position of the pre-drawn silicon rod, and the ρ is the resistivity at the corresponding position of the pre-drawn silicon rod.
[0033] Wherein, the range of W includes 50mm-180mm, and / or the range of ρ includes 0.1ohm.cm-10ohm.cm.
[0034] In a possible implementation, determining the doping amount at different positions of the pre-drawn silicon rod according to the silicon wafer efficiency of the furnace includes:
[0035] Determining the resistivity at different positions of the pre-drawn silicon rod based on the whole furnace silicon wafer efficiency prediction model, the silicon wafer efficiency of the furnace, the minority carrier lifetime data at different positions of the pre-drawn silicon rod, and the silicon wafer thickness;
[0036] The doping amounts at different positions of the pre-drawn silicon rod are determined according to the resistivity at different positions of the pre-drawn silicon rod.
[0037] In a third aspect, the present application further provides a silicon wafer for a solar cell, which is obtained by cutting a silicon rod pulled by the above-mentioned crystal pulling method.
[0038] The thickness of the silicon wafer ranges from 50 mm to 180 mm.
[0039] When the silicon wafer is obtained by cutting the head of a silicon rod, the resistivity of the silicon wafer is 0.5 ohm.cm-4 ohm.cm. When the silicon wafer is obtained by cutting the tail of a silicon rod, the resistivity of the silicon wafer is 0.1 ohm.cm-10 hm.cm.
[0040] In a fourth aspect, the present application further provides a crystal pulling device, comprising a processor and a memory, wherein the memory stores at least one computer instruction, and the instruction is loaded and executed by the processor to implement the steps performed in the above-mentioned crystal pulling method.
[0041] In a fifth aspect, the present application also provides a computer storage medium, wherein the computer storage medium stores instructions, and when the instructions are executed, the above-mentioned crystal pulling method is implemented.
[0042] Compared with the prior art, the beneficial effects of the third, fourth and fifth aspects provided by this application are the same as the beneficial effects of the crystal pulling method described in the second aspect or any possible implementation of the second aspect, and will not be repeated here.
[0043] The above description is only an overview of the technical solution of the present application. In order to more clearly understand the technical means of the present application, it can be implemented in accordance with the contents of the specification. In order to make the above and other purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are listed below. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, a brief introduction will be given below to the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without any creative work.
[0045] FIG1 is a flowchart of a method for determining minority carrier lifetime according to an embodiment of the present application;
[0046] FIG2 is a flow chart of the steps of a crystal pulling method provided in an embodiment of the present application;
[0047] FIG3 is a schematic structural diagram of a crystal pulling device provided in an embodiment of the present application. Specific embodiments
[0048] To make the purpose, technical solutions, and advantages of the embodiments of this application more clear, the technical solutions in the embodiments of this application will be clearly and completely described below in conjunction with the drawings in the embodiments of this application. Obviously, the described embodiments are part of the embodiments of this application, not all of the embodiments. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of this application.
[0049] With increasingly stringent environmental requirements, the demand for clean energy is increasing, and the photovoltaic industry is a key component of this clean energy supply. In the photovoltaic industry, multi-charge crystal pulling is a key technology for pulling single-crystal silicon rods. The specific process involves pulling cylindrical single-crystal silicon rods. When the single-crystal silicon rods are subsequently used to make solar cells, the cylindrical silicon rods are sequentially cut, squared, and sliced to form silicon wafers for use in the cells.
[0050] However, at present, with the development of the photovoltaic industry, the improvement of silicon wafer efficiency has entered a bottleneck period.
[0051] In conventional RCZ (multiple charging crystal pulling technology), the process includes: furnace assembling, charging, calculating the doping amount m1 based on the RCZ1 target resistivity ρ1, adding doping, melting, pulling crystal, and extracting the crystal rod; secondary charging, calculating the doping amount m2 based on the RCZ2 target resistivity ρ2, melting, pulling crystal, and extracting the crystal rod; and repeating the cycle until the completion stage, and stopping the furnace after the crystal rod is pulled.
[0052] The target resistivity of each cycle segment is equal, that is, ρ1=ρ2=……=ρ n , which ensures that the resistivity of each silicon rod is equal. As the crystal pulling process progresses, impurities in the silicon melt continue to accumulate, causing the minority carrier lifetime of each silicon rod to gradually decrease. As a result, the resistivity cannot be flexibly adjusted to match the parameters for optimal cell efficiency, resulting in efficiency losses for the entire furnace of silicon wafers.
[0053] Based on this, with reference to FIG1 , an embodiment of the present application discloses a method for determining the minority carrier lifetime, which is used in a pre-drawn silicon rod. The method for determining the minority carrier lifetime comprises the following steps:
[0054] S100, obtain the minority carrier lifetime curve of the silicon wafer sample.
[0055] In practice, the minority carrier lifetime of a silicon wafer follows a curve related to the implantation level "Δn," primarily influenced by the doping level Nx, the impurity content Nt, and the characteristic parameters of each impurity (Et, σn, σp), as shown in Equation (1). Many impurities can affect minority carrier lifetime, but current simulations of minority carrier lifetime use a single-point model with a fixed implantation level, considering only the Fe content, and therefore cannot provide data for the entire lifetime curve.
[0056] Where, τ SRH represents the minority carrier lifetime data, △n represents the injection concentration, N x Indicates the doping level, N t represents the impurity content, Et, σn, σp represent the characteristic parameters of each impurity.
[0057] In the embodiment of the present application, silicon wafers cut from a silicon ingot currently being pulled are first selected as silicon wafer samples. As an implementation method, multiple silicon wafers can be selected from different positions of multiple continuously pulled single crystal silicon ingots as silicon wafer samples.
[0058] Specifically, the different positions of the single crystal silicon rod can be the two ends of the single crystal silicon rod after being squared, or can be at least one of the two ends and the middle of the single crystal silicon rod after being squared. For example, after each continuously drawn silicon rod is squared, 10 silicon wafers can be taken from each end of the resulting square rod as silicon wafer samples, thereby obtaining silicon wafer samples representing each position of the current furnace. Alternatively, after multiple continuously drawn single crystal silicon rods are squared, 5 silicon wafers can be taken from each end and the middle of the resulting square rod as silicon wafer samples, thereby obtaining silicon wafer samples representing each position of the current furnace.
[0059] After passivation treatment of the silicon wafer samples, the minority carrier lifetime data of each silicon wafer sample is measured to obtain a minority carrier lifetime curve for the silicon wafer sample. It should be understood that passivation treatment of the silicon wafer samples is intended to reduce surface recombination of charge carriers, thereby making the measured minority carrier lifetime data of the silicon wafer samples more accurate. In practice, each silicon wafer sample can be measured using a minority carrier lifetime tester to obtain minority carrier lifetime data for each silicon wafer sample.
[0060] After obtaining the minority carrier lifetime data of each silicon wafer sample, a minority carrier lifetime curve of the silicon wafer sample is established based on the minority carrier lifetime data of all silicon wafer samples.
[0061] Based on this, an embodiment of the present application selects multiple silicon wafers from different positions of multiple silicon rods continuously drawn in the same furnace as silicon wafer samples. That is to say, the silicon wafer sample and the pre-drawn silicon wafer are drawn in the same furnace. On this basis, the silicon wafer sample is measured to obtain the minority carrier lifetime data of the silicon wafer sample, which can relatively accurately characterize the minority carrier lifetime data at different positions of the pre-drawn silicon rod belonging to the same silicon rod as the silicon wafer sample. Based on the minority carrier lifetime data, the resistivity of the silicon wafer is adjusted, which can accurately improve the efficiency of the silicon wafers drawn in the same furnace.
[0062] S200, establishing a minority carrier lifetime calculation model based on the minority carrier lifetime curve of the silicon wafer sample and the minority carrier lifetime simulation model; wherein the silicon wafer sample and the pre-drawn silicon rod are prepared by the same furnace.
[0063] Among them, the expression of the above minority carrier lifetime simulation model can satisfy:
[0064] Among them, σ n represents the electron capture cross-sectional radius, σ p represents the hole capture cross-sectional radius, n0: equilibrium electron concentration, p0 represents the equilibrium hole concentration, Nc represents the conduction band effective state density, Nv represents the valence band effective state density, Ec represents the conduction band energy level, Ev represents the valence band energy level, E t represents the impurity energy level, k0 represents the Boltzmann constant, T represents the temperature, △n represents the injection concentration, V th Indicates the carrier thermal motion velocity, N t Indicates the impurity concentration.
[0065] Specifically, based on the minority carrier lifetime curve of the silicon wafer sample and the minority carrier lifetime simulation model, establishing the minority carrier lifetime calculation model includes:
[0066] According to the minority carrier lifetime curve of the silicon wafer sample and the minority carrier lifetime simulation model, the relationship between the impurity concentration and the solidification fraction in the minority carrier lifetime simulation model is determined.
[0067] Based on the above formula (2), a function is established with independent variables (△n, n0, p0) and dependent variable τ SRH , the parameter is (E ti ,σ ni ,σ pi , N t ), and the rest are constants.
[0068] Assuming i recombination centers, the minority carrier lifetime curve data from all sample silicon wafers is iteratively calculated until convergence, giving the optimal solution and obtaining the recombination parameters (Eti, σni, σpi) and concentration (Nt) of each recombination center. The minority carrier lifetime curve data from all sample silicon wafers can be calculated by using Python to iteratively calculate the four parameters Eti, σni, σpi, and Nt, obtaining the sum of the absolute differences (MAE) between the calculated minority carrier lifetime curves and the actual measured minority carrier lifetime curves in each cycle. The optimal solution is obtained by iteratively obtaining the set of parameters (Eti, σni, σpi, Nt) with the minimum MAE.
[0069] Then, based on the segregation formula, gN t Perform fitting and establish relationship N t=f(g), so far, the above (E ti ,σ ni ,σ pi ) are all known quantities, and a calculation model for the minority carrier lifetime under the current thermal field and crystal pulling conditions can be given.
[0070] A minority carrier lifetime calculation model is established based on the relationship between the impurity concentration and the solidification fraction and the minority carrier lifetime simulation model.
[0071] The relationship between impurity concentration and solidification fraction can also be expressed as:
[0072] Nt=kC0(1-g) k-1 +ag 2 +bg+c.
[0073] Where C0 represents the initial impurity concentration in the silicon solution before crystal pulling, k represents the impurity segregation coefficient, g is the solidification fraction, which represents the weight of the pulled crystal rod / total feed amount. Based on the segregation formula, gN t Perform fitting and obtain a, b, and c.
[0074] When the single crystal furnaces have the same size, after calculating a, b, and c, the silicon rods can be pulled from the same single crystal furnace or from single crystal furnaces of the same size. When the single crystal furnaces have different sizes, the S200 step can be looped to recalculate a, b, and c.
[0075] Given the above description, the embodiments of the present application can determine the relationship between impurity concentration and solidification fraction in the minority carrier lifetime simulation model based on the known minority carrier lifetime simulation model and the minority carrier lifetime curve of the silicon wafer sample. It should be understood that in the minority carrier lifetime simulation model, when the relationship between impurity concentration and solidification fraction is a known condition, a minority carrier lifetime calculation model can be established based on the minority carrier lifetime simulation model to calculate the minority carrier lifetime data at various positions of the pre-drawn silicon rod. It can be seen that the method for determining the minority carrier lifetime calculation model in the embodiments of the present application is simple, has a small amount of computational effort, is applicable to single crystal furnaces of different sizes, and has strong versatility.
[0076] S300 , determining minority carrier lifetime data at different positions of the pre-drawn silicon rod based on the minority carrier lifetime calculation model.
[0077] In an embodiment of the present application, the minority carrier lifetime data at each position of the pre-drawn silicon rod can be obtained based on the minority carrier lifetime calculation model, the resistivity at different positions of the pre-drawn silicon rod, and the solidification fraction of the pre-drawn silicon rod.
[0078] Specifically, the resistivity at different positions of the pre-drawn silicon rod may be the position of the target silicon wafer in the entire furnace of silicon rods, such as RCZ3 at the 300 mm position, or RCZ5 at the 260 mm position.
[0079] Based on the above description, the minority carrier lifetime determination method provided in the embodiments of the present application obtains a minority carrier lifetime curve for silicon wafer samples obtained from silicon rods previously produced on the same furnace. Then, based on an established minority carrier lifetime simulation model, a minority carrier lifetime calculation model is established. Finally, based on the minority carrier lifetime calculation model, minority carrier lifetime data for the silicon wafer at different positions on the pre-drawn silicon rod can be calculated. It should be understood that cell efficiency is related to the resistivity of the silicon wafer, the minority carrier lifetime data for the silicon wafer, and the thickness of the silicon wafer. In addition to the minority carrier lifetime data for the silicon wafer, both the resistivity and thickness of the silicon wafer can be adjusted. Therefore, after obtaining the minority carrier lifetime data for the silicon wafer, the embodiments of the present application can improve the efficiency of silicon wafers drawn on the same furnace by adjusting the resistivity and / or thickness of the silicon wafer. This addresses the prior art problem of the gradual decrease in minority carrier lifetime of multiple silicon rods drawn continuously, which prevents flexible resistivity control to match the optimal cell efficiency parameters, resulting in efficiency loss for the entire furnace of silicon wafers.
[0080] 2 , an embodiment of the present application further provides a crystal pulling method, including the aforementioned method for determining the minority carrier lifetime, wherein the crystal pulling method includes the following steps:
[0081] S10, determining the silicon wafer efficiency of the furnace according to the minority carrier lifetime data at different positions of the pre-drawn silicon rod and adjusting the resistivity at different positions of the pre-drawn silicon rod; wherein the silicon wafer efficiency of the furnace meets the target efficiency requirement.
[0082] It should be understood that based on the whole-furnace silicon wafer efficiency prediction model, the silicon wafer efficiency of the furnace is related to the resistivity of the silicon wafer, the minority carrier lifetime data of the silicon wafer, and the thickness of the silicon wafer. The minority carrier lifetime data of the silicon wafer can be obtained through the above-mentioned minority carrier lifetime determination method.
[0083] Furthermore, determining the silicon wafer efficiency of the furnace according to minority carrier lifetime data at different positions of the pre-drawn silicon rod and adjusting the resistivity at different positions of the pre-drawn silicon rod may include:
[0084] Based on the whole furnace silicon wafer efficiency prediction model, the minority carrier lifetime data at different positions of the pre-drawn silicon rod and the silicon wafer thickness corresponding to different positions of the pre-drawn silicon rod, the resistivity at different positions of the pre-drawn silicon rod is adjusted to obtain the silicon wafer efficiency of the furnace.
[0085] In the embodiments of the present application, the minority carrier lifetime data of the silicon wafer can be calculated, and the thickness of the silicon wafer can be predetermined. In this case, to ensure that the silicon wafer efficiency of the furnace meets the target efficiency requirement, the resistivity of the pre-drawn silicon rods at different positions can be adjusted to ensure that the silicon wafer efficiency of the furnace meets the requirement. In this case, the silicon wafer efficiency of the furnace is the target silicon wafer efficiency. In practice, the target silicon wafer efficiency can be such that the RCZ reaches the maximum efficiency.
[0086] S20, determining the doping amount of the silicon wafers at different positions of the pre-drawn silicon rod according to the silicon wafer efficiency of the furnace.
[0087] In the embodiment of the present application, the above-mentioned whole furnace silicon wafer efficiency prediction model satisfies: eff = f(ρ, τ, W);
[0088] The eff is the silicon wafer efficiency of the furnace, the τ is the minority carrier lifetime curve at the target position in the pre-drawn silicon rod, the W is the silicon wafer thickness corresponding to the corresponding position of the pre-drawn silicon rod, and the ρ is the resistivity at the corresponding position of the pre-drawn silicon rod.
[0089] Wherein, W ranges from 50 mm to 180 mm, and / or ρ ranges from 0.1 ohm.cm to 10 ohm.cm. The thickness of the silicon wafers and the resistivity at corresponding locations of the pre-drawn silicon rods are obtained based on multiple tests. Silicon wafers cut from silicon rods obtained within this range can be used to produce high-efficiency solar cells.
[0090] The above step S20 has determined the silicon wafer efficiency of the furnace that maximizes the RCZ efficiency by adjusting the resistivity at different positions of the pre-drawn silicon rod. At this time, the resistivity of the silicon wafer at the corresponding position of the silicon rod is determined based on the silicon wafer efficiency of the furnace, the minority carrier lifetime curve at the target position in the pre-drawn silicon rod, and the thickness of the silicon wafer at the corresponding position of the pre-drawn silicon rod. It should be understood that the doping amount of the silicon wafer at different positions of the pre-drawn silicon rod is related to the resistivity at the corresponding position. Therefore, once the resistivity of the silicon wafer at the corresponding position of the silicon rod is obtained, the doping amount of the silicon wafer at different positions of the pre-drawn silicon rod can be determined.
[0091] S30, when using the furnace to prepare a silicon single crystal, doping the furnace according to the doping amount at different positions of the pre-pulled silicon rod to perform a crystal pulling process.
[0092] It should be understood that after determining the doping amount of silicon wafers at different positions of the pre-drawn silicon rod, when drawing the silicon rod, the furnace is doped according to the doping amount of silicon wafers at different positions of the pre-drawn silicon rod, so that silicon wafers that meet the target efficiency requirements can be obtained.
[0093] Based on the above description, it should be understood that battery efficiency is related to the resistivity of the silicon wafer, the minority carrier lifetime data of the silicon wafer, and the thickness of the silicon wafer. When the thickness of the silicon wafer has been determined, this application adjusts the resistivity of the pre-drawn silicon rod at different positions based on the aforementioned determined minority carrier lifetime data at different positions of the pre-drawn silicon rod, thereby obtaining the optimal silicon wafer efficiency of the furnace. It should be understood that the doping amount at different positions of the silicon rod is determined by the preset resistivity at the corresponding position of the silicon rod. On this basis, according to the above-adjusted resistivity at different positions of the pre-drawn silicon rod, the doping amount of the silicon wafer at the corresponding position of the pre-drawn silicon rod can be obtained; based on this doping amount, the furnace is doped, and a silicon rod that meets the optimal silicon wafer efficiency of the furnace can be drawn, and then a high-efficiency battery can be made using the silicon rod.
[0094] In a third aspect, an embodiment of the present application further provides a silicon wafer for a solar cell. The silicon wafer for a solar cell is obtained by cutting a silicon rod pulled by the above-mentioned crystal pulling method.
[0095] The thickness of the silicon wafer ranges from 50 mm to 180 mm. For example, the thickness of the silicon wafer may be 50 mm, 90 mm, 120 mm, or 180 mm.
[0096] When the silicon wafer is obtained by cutting the head of a silicon rod, the resistivity of the silicon wafer is 0.5 ohm.cm-4 ohm.cm. For example, when the silicon wafer is obtained by cutting the head of a silicon rod, the resistivity of the silicon wafer is 0.5 ohm.cm, 1.2 ohm.cm, 1.5 ohm.cm, or 4 ohm.cm.
[0097] When the silicon wafer is obtained by cutting the tail of a silicon ingot, the resistivity of the silicon wafer is 0.1 ohm.cm-10 ohm.cm. For example, when the silicon wafer is obtained by cutting the tail of a silicon ingot, the resistivity of the silicon wafer is 0.1 ohm.cm, 3 ohm.cm, 7 ohm.cm, or 10 ohm.cm.
[0098] The above silicon wafer thickness and resistivity are determined based on multiple experiments. Silicon wafers within this range can be used to produce high-efficiency batteries.
[0099] It should be understood that because the doping level in the silicon rods pulled by the above-described crystal pulling method is determined based on the optimal efficiency of the entire furnace, the efficiency of silicon wafers cut from the silicon rods pulled by the above-described crystal pulling method can be maximized. Experiments have shown that the silicon wafers used in solar cells obtained in this embodiment of the present application can increase the cell-side conversion efficiency of the entire furnace of silicon wafers by 0.02%.
[0100] As a specific example, Table 1 shows the head resistivity and tail resistivity of a 32-inch silicon rod drawn by a hot field.
[0101] Table 1
[0102] 3 , the crystal pulling device 101 includes a processor 210 and a communication interface 230 . The communication interface 230 is coupled to the processor 210 . The processor 210 is configured to execute computer programs or instructions.
[0103] As shown in FIG3 , the processor 210 may be a general-purpose central processing unit (CPU), a microprocessor, an application-specific integrated circuit (ASIC), or one or more integrated circuits for controlling program execution of the present application. The communication interface 230 may be one or more. The communication interface 230 may utilize any transceiver or other device for communicating with other devices or a communication network.
[0104] 3 , the crystal pulling apparatus 101 may further include a communication circuit 240. The communication circuit 240 may include a path for transmitting information between the aforementioned components.
[0105] Optionally, as shown in FIG3 , the crystal pulling device 101 may further include a memory 220 . The memory 220 is used to store computer instructions for executing the solution of the present application, and is controlled by the processor 210 . The processor 210 is used to execute the computer instructions stored in the memory 220 .
[0106] As shown in FIG3 , the memory 220 may be a read-only memory (ROM) or other type of static storage device that can store static information and instructions, a random access memory (RAM) or other type of dynamic storage device that can store information and instructions, or an electrically erasable programmable read-only memory (EEPROM), a compact disc read-only memory (CD-ROM) or other optical disc storage, an optical disc storage (including a compact disc, laser disc, optical disc, digital versatile disc, Blu-ray disc, etc.), a magnetic disk storage medium or other magnetic storage device, or any other medium that can be used to carry or store desired program code in the form of instructions or data structures and can be accessed by a computer, but is not limited thereto. The memory 220 may exist independently and be connected to the processor 210 via a communication line 240. The memory 220 may also be integrated with the processor 210.
[0107] Optionally, the computer instructions in the embodiments of the present application may also be referred to as application code, which is not specifically limited in the embodiments of the present application.
[0108] In a specific implementation, as an embodiment, as shown in FIG3 , the processor 210 may include one or more CPUs, such as CPU0 and CPU1 in FIG3 .
[0109] In a specific implementation, as an embodiment, as shown in Figure 3, the crystal pulling device 101 may include multiple processors 210, such as the processor 210 and the processor 250 in Figure 3. Each of these processors may be a single-core processor or a multi-core processor.
[0110] The present application also provides a computer-readable storage medium having instructions stored therein, which, when executed, implement the functions performed by the crystal pulling device in the above-mentioned embodiment.
[0111] In the above embodiments, all or part of the embodiments can be implemented by software, hardware, firmware or any combination thereof. When implemented using software, all or part of the embodiments can be implemented in the form of a computer program product. The computer program product includes one or more computer programs or instructions. When the computer program or instructions are loaded and executed on a computer, the process or function of the embodiment of the present application is executed in whole or in part. The computer can be a general-purpose computer, a special-purpose computer, a computer network, a terminal, a user device or other programmable device. The computer program or instruction can be stored in a computer-readable storage medium or transmitted from one computer-readable storage medium to another computer-readable storage medium. For example, the computer program or instruction can be transmitted from one website, computer, server or data center to another website, computer, server or data center via wired or wireless means. The computer-readable storage medium can be any available medium that can be accessed by a computer or a data storage device such as a server or data center that integrates one or more available media. The available medium can be a magnetic medium, such as a floppy disk, a hard disk, or a magnetic tape; it can also be an optical medium, such as a digital video disc (DVD); it can also be a semiconductor medium, such as a solid state drive (SSD).
[0112] Although the present application is described herein in conjunction with various embodiments, in the process of implementing the claimed application, those skilled in the art may understand and implement other variations of the disclosed embodiments by reviewing the drawings, the disclosure, and the appended claims. In the claims, the word "comprising" does not exclude other components or steps, and "a" or "an" does not exclude multiple situations. A single processor or other unit may implement several functions listed in the claims. Certain measures are recorded in different dependent claims, but this does not mean that these measures cannot be combined to produce good results.
[0113] Although the present application is described herein in conjunction with various embodiments, in the process of implementing the claimed application, those skilled in the art may understand and implement other variations of the disclosed embodiments by reviewing the drawings, the disclosure, and the appended claims. In the claims, the word "comprising" does not exclude other components or steps, and "a" or "an" does not exclude multiple situations. A single processor or other unit may implement several functions listed in the claims. Certain measures are recorded in different dependent claims, but this does not mean that these measures cannot be combined to produce good results.
[0114] Although the present application has been described with reference to specific features and embodiments thereof, it is apparent that various modifications and combinations may be made thereto without departing from the spirit and scope of the present application. Accordingly, this specification and the drawings are merely illustrative of the present application as defined by the appended claims and are deemed to cover any and all modifications, variations, combinations or equivalents within the scope of the present application. Obviously, those skilled in the art may make various modifications and variations to the present application without departing from the spirit and scope of the present application. Thus, the present application is intended to include such modifications and variations as fall within the scope of the claims of the present application and their equivalents.
Claims
1. A method for determining minority carrier lifetime, wherein: Applied to a pre-drawn silicon rod, the minority carrier lifetime determination method includes: Obtain minority carrier lifetime curve of silicon wafer sample; A minority carrier lifetime calculation model is established according to the minority carrier lifetime curve of the silicon wafer sample and the minority carrier lifetime simulation model; wherein the silicon wafer sample and the pre-drawn silicon rod are prepared by the same furnace; Based on the minority carrier lifetime calculation model, minority carrier lifetime data at different positions of the pre-drawn silicon rod are determined.
2. The method for determining minority carrier lifetime according to claim 1, wherein: The method of obtaining the minority carrier lifetime curve of the silicon wafer sample comprises: Selecting a plurality of silicon wafers from different positions of a plurality of continuously drawn single crystal silicon rods as silicon wafer samples; After the silicon wafer samples are passivated, minority carrier lifetime data of each silicon wafer sample is measured to obtain a minority carrier lifetime curve of the silicon wafer sample.
3. The method for determining minority carrier lifetime according to claim 1, wherein: According to the minority carrier lifetime curve of the silicon wafer sample and the minority carrier lifetime simulation model, a minority carrier lifetime calculation model is established, including: Determining the relationship between the impurity concentration and the solidification fraction in the minority carrier lifetime simulation model according to the minority carrier lifetime curve of the silicon wafer sample and the minority carrier lifetime simulation model; A minority carrier lifetime calculation model is established based on the relationship between the impurity concentration and the solidification fraction and the minority carrier lifetime simulation model.
4. The method for determining minority carrier lifetime according to claim 1, wherein: Determining minority carrier lifetime data at different positions of the pre-drawn silicon rod based on the minority carrier lifetime calculation model includes: Based on the minority carrier lifetime calculation model, the resistivity at different positions of the pre-drawn silicon rod, and the solidification fraction of the pre-drawn silicon rod, the minority carrier lifetime data at each position of the pre-drawn silicon rod are obtained.
5. A crystal pulling method, wherein: The method for determining the minority carrier lifetime according to any one of claims 1 to 4, wherein the crystal pulling method comprises the following steps: Determining the silicon wafer efficiency of the furnace according to minority carrier lifetime data at different positions of the pre-drawn silicon rod and adjusting the resistivity at different positions of the pre-drawn silicon rod; wherein the silicon wafer efficiency of the furnace meets the target efficiency requirement; Determining the doping amount of the silicon wafers at different positions of the pre-drawn silicon rod according to the silicon wafer efficiency of the furnace; When the furnace is used to prepare silicon single crystals, the furnace is doped according to the doping amounts at different positions of the pre-pulled silicon rods to perform a crystal pulling process.
6. The crystal pulling method according to claim 5, wherein: Determining the silicon wafer efficiency of the furnace according to minority carrier lifetime data at different positions of the pre-drawn silicon rod and adjusting the resistivity at different positions of the pre-drawn silicon rod includes: Based on the whole furnace silicon wafer efficiency prediction model, the minority carrier lifetime data at different positions of the pre-drawn silicon rod and the silicon wafer thickness corresponding to different positions of the pre-drawn silicon rod, the resistivity at different positions of the pre-drawn silicon rod is adjusted to obtain the silicon wafer efficiency of the furnace.
7. The crystal pulling method according to claim 6, wherein: The whole furnace silicon wafer efficiency prediction model satisfies: eff = f(ρ, τ, W); The eff is the silicon wafer efficiency of the furnace, the τ is the minority carrier lifetime curve at the target position in the pre-drawn silicon rod, the W is the silicon wafer thickness corresponding to the corresponding position of the pre-drawn silicon rod, and the ρ is the resistivity at the corresponding position of the pre-drawn silicon rod.
8. The crystal pulling method according to claim 7, wherein: The range of W includes 50mm-180mm, and / or the range of ρ includes 0.1ohm.cm-10ohm.cm.
9. The crystal pulling method according to any one of claims 5 to 8, wherein: Determining the doping amount of the silicon wafers at different positions of the pre-drawn silicon rod according to the silicon wafer efficiency of the furnace comprises: Determine the resistivity at different positions of the pre-drawn silicon rod based on the whole furnace silicon wafer efficiency prediction model, the silicon wafer efficiency of the furnace, the minority carrier lifetime data at different positions of the pre-drawn silicon rod and the silicon wafer thickness corresponding to different positions of the pre-drawn silicon rod; The doping amounts of silicon slices at different positions of the pre-drawn silicon rod are determined according to the resistivity at different positions of the pre-drawn silicon rod.
10. A silicon wafer for a solar cell, wherein: The silicon wafer for solar cells is obtained by cutting a silicon rod pulled by the crystal pulling method according to any one of claims 5 to 9.
11. The silicon wafer for solar cells according to claim 10, wherein: The thickness of the silicon wafer ranges from 50 mm to 180 mm.
12. The silicon wafer for solar cells according to claim 10, wherein: When the silicon wafer is obtained by cutting the head of a silicon rod, the resistivity of the silicon wafer is 0.5ohm.cm-4ohm.cm. When the silicon wafer is obtained by cutting the tail of a silicon rod, the resistivity of the silicon wafer is 0.1ohm.cm-10ohm.cm.
13. A crystal pulling device, wherein: It comprises a processor and a memory, wherein the memory stores at least one computer instruction, and the instruction is loaded and executed by the processor to implement the steps performed in the crystal pulling method according to any one of claims 5 to 9.
14. A computer storage medium, wherein: The computer storage medium stores instructions, and when the instructions are executed, the crystal pulling method according to any one of claims 5 to 9 is implemented.
Citation Information
Patent Citations
Device and method for prolonging edge minority carrier lifetime of N-type silicon single crystal
CN102560625A
Manufacture technical process of solar battery
CN104465859A
Test method for minority carrier life of crystalline silicon solar cell
CN108983063A
Method for controlling resistivity of n-type single crystal
CN111676511A
Method for testing corresponding relation among service life, sample thickness and body service life of N-type silicon wafer