Solar cell and preparation method therefor

By adopting a three-layer structure electrode and flexible mask deposition process, the problems of poor bonding strength and high material cost in existing solar cell electrodes are solved, and higher bonding strength and lower preparation costs are achieved.

WO2024235143A1PCT designated stage expired Publication Date: 2024-11-21LONGI GREEN ENERGY TECH CO LTD

Patent Information

Application Number
PCT/CN2024/092527
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-16
Filing Date
2024-05-11
Publication Date
2024-11-21

AI Technical Summary

Technical Problem

In the preparation of electrodes of existing solar cells, the bonding strength between the silver electrode and the battery substrate is poor, and the silver paste material cost is relatively high.

Method used

Electrodes with a three-layer structure, in which the first layer is in direct contact with the battery substrate, the second and third layers have weak adhesion, the material is selected as aluminum or copper with lower cost, and the third layer has a low melting point or low Surface tension, electrodes are formed through flexible mask deposition process, simplifying the preparation process and reducing costs.

Benefits of technology

The bonding strength between the electrode and the battery substrate is improved, the preparation cost is reduced, the metal diffusion pollution is reduced, and the equipment production capacity and raw material utilization is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2024092527_21112024_PF_FP_ABST
    Figure CN2024092527_21112024_PF_FP_ABST
Patent Text Reader

Abstract

A solar cell and a preparation method therefor, which relate to the technical field of solar cells, and are used to solve the problem of high manufacturing costs. The solar cell comprises a cell substrate and electrodes provided on at least one surface of the cell substrate, wherein each electrode comprises a first layer, a second layer and a third layer, which are sequentially arranged in a stacked manner, the first layer being in contact with the surface of the cell substrate. The adhesion between the first layer and the surface of the cell substrate is greater than the adhesion between the second layer and the surface of the cell substrate and the adhesion between the third layer and the surface of the cell substrate, and the contact resistivity between the first layer and the surface of the cell substrate is less than the contact resistivity between the second layer and the surface of the cell substrate and the contact resistivity between the third layer and the surface of the cell substrate; or the melting point of the first layer is greater than the melting point of the second layer and the melting point of the third layer. The resistivity of the second layer is less than the resistivity of the first layer and the resistivity of the third layer; and the melting point or surface tension of the third layer is less than the melting point or surface tension of the first layer and the melting point or surface tension of the second layer. Thus, the adhesion between each electrode and a cell substrate can be increased, the contact resistivity can be reduced, and metals can also be prevented from diffusing into the cell substrate.
Need to check novelty before this filing date? Find Prior Art

Description

Solar cell and preparation method thereof

[0001] This application claims priority to the Chinese patent application filed with the China Patent Office on May 16, 2023, with application number 202310551547.X and entitled “A Solar Cell and Its Preparation Method”, the entire contents of which are incorporated by reference into this application. Technical Field

[0002] The present application relates to the technical field of solar cells, and in particular to a solar cell and a method for preparing the same. Background Art

[0003] Solar cells primarily consist of cells and electrodes. The cells absorb sunlight and convert it into electrical energy. The electrodes transmit the current generated by the cells to an external circuit.

[0004] At present, the electrodes of solar cells are generally prepared by screen-printing silver paste, which is formed into silver electrodes after high-temperature sintering. The bonding strength between the silver electrodes and the battery substrate is poor, and the cost of the silver paste material is high.

[0005] Summary of the Invention

[0006] The purpose of this application is to provide a solar cell and a method for preparing the same, so as to improve the bonding strength between the electrode and the cell substrate and reduce the production cost.

[0007] In a first aspect, the present application provides a solar cell comprising a cell substrate and an electrode disposed on at least one surface of the cell substrate, wherein the electrode comprises a first layer, a second layer, and a third layer stacked in sequence, and the first layer contacts the surface of the cell substrate;

[0008] The adhesion of the first layer to the surface of the battery substrate is greater than the adhesion of the second layer and the third layer to the surface of the battery substrate, and the contact resistivity of the first layer to the surface of the battery substrate is less than the contact resistivity of the second layer and the third layer to the surface of the battery substrate; or the melting point of the first layer is greater than the melting points of the second layer and the third layer;

[0009] The resistivity of the second layer is less than that of the first and third layers;

[0010] The melting point or surface tension of the third layer is lower than that of the first and second layers.

[0011] When using the above technical solution, the electrode on the battery substrate comprises a three-layer structure, wherein the first layer of the electrode directly contacts the battery substrate, the second layer of the electrode is disposed on the first layer, and the third layer of the electrode is disposed on the second layer. Because the first layer has greater adhesion to the battery substrate surface than the second and third layers, the adhesion and bonding strength of the electrode to the battery substrate are enhanced compared to existing silver electrode-battery substrate bonding. Furthermore, the direct contact of the first layer with the battery substrate has a lower contact resistivity than that of silver electrodes, making it easier to achieve good ohmic contact between the electrode and the battery substrate. Furthermore, since the electrode has a three-layer structure, the second layer can be made of a low-resistivity and low-cost material, such as aluminum, as the main conductive material. The third layer can be made of a material with a low melting point or low surface tension. Generally, materials with low surface tension allow molten liquid to flow easily on the surface, resulting in a small contact angle, which improves wettability with the solder ribbon and facilitates soldering. Materials with low melting points also tend to be easier to solder to the solder ribbon. Compared with existing electrodes made entirely of silver, costs can be reduced.

[0012] In addition, for some types of battery substrates, the melting point of the first layer is greater than that of the second and third layers. This higher melting point indicates that the interatomic bonding forces in the first layer are relatively strong, making diffusion less likely. Therefore, the diffusion barrier capability of the first layer is greater than that of the second and third layers, preventing metal atoms from diffusing into the battery substrate. Compared to existing silver electrodes that directly contact the battery substrate, the present invention can also prevent the metal in the second layer from diffusing into the battery substrate through the first layer, reducing contamination of the battery substrate.

[0013] In some possible implementations, the surface of the battery substrate in contact with the electrode is a transparent conductive oxide film, the adhesion between the first layer and the transparent conductive oxide film is greater than the adhesion between the second layer and the third layer and the transparent conductive oxide film, and the contact resistivity between the first layer and the transparent conductive oxide film is less than the contact resistivity between the second layer and the third layer and the transparent conductive oxide film;

[0014] Alternatively, the surface of the battery substrate in contact with the electrode is carrier transport, and the melting point of the first layer is greater than the melting points of the second layer and the third layer.

[0015] When the above technical solution is adopted, when the surface of the battery substrate in contact with the electrode is a transparent conductive oxide film, the role of the first layer of the electrode is mainly to increase the adhesion between the electrode and the surface of the battery substrate and reduce the contact resistance; when the surface of the battery substrate in contact with the electrode is a carrier transport layer, the melting point of the first layer is greater than the melting points of the second and third layers, so that the performance shows that the diffusion barrier ability of the first layer is greater than the diffusion barrier ability of the second and third layers, and the role of the first layer of the electrode is mainly to prevent metal from diffusing into the surface of the battery substrate.

[0016] In some possible implementations, the projections of the first layer, the second layer, and the third layer on the battery substrate overlap. Since the three-layer structure of the electrode is deposited using the same flexible mask, the three-layer structure has the same shape.

[0017] In some possible implementations, the thickness of the first layer is less than or equal to 10% of the thickness of the second layer; and / or the thickness of the third layer is less than or equal to 10% of the thickness of the second layer. This arrangement results in the first and third layers being relatively thin, with the second layer comprising the majority of the material. Since the second layer has the lowest resistivity of the three layers, the thinner first and third layers can minimize the distance current travels through the higher-resistivity material, thereby reducing current losses. Furthermore, the thinner first and third layers can reduce the amount of material used in these two layers, thereby lowering costs.

[0018] In some possible implementations, the line width of the electrode at any position is 5 μm to 1500 μm, the thickness of the electrode at any position is 0.5 μm to 21 μm, and the ratio between the thickness and width of the electrode is 0.001 to 0.2.

[0019] When the above technical solution is adopted, the electrode can reduce the aspect ratio to 0.001-0.2 by increasing the line width, reducing the thickness, and reducing the aspect ratio without changing the conductive effect (i.e., the resistance is constant). The electrode has good structural stability and is not prone to deformation or tipping. Due to the large line width of the electrode, a good conductive effect can be achieved using thinner materials, so that the electrode preparation can be completed with a shorter deposition time, which greatly improves the equipment production capacity. Since the shape of the hollow pattern on the flexible mask is consistent with the shape of the electrode, the line width of the hollow pattern is increased, the hollow area is larger, and the non-hollow area is reduced. Therefore, when the flexible mask is used to deposit the electrode material, the amount of electrode material deposited on the non-hollow part of the flexible mask is reduced. Therefore, the larger the line width of the hollow pattern, the higher the utilization rate of the raw materials, which reduces the amount of raw materials used. In addition, the wider electrode is arranged on the back of the battery substrate, and the formed back electrode or back contact electrode will not block the light absorption of the solar cell.

[0020] In some possible implementations, the electrode includes a collector grid line; or, the electrode includes intersecting collector grid lines and bus grid lines; wherein the collector grid line has a line width of 30 μm to 500 μm, and the bus grid line has a line width of 100 μm to 1500 μm.

[0021] When using this technical solution, the collector and busbar lines on the back of the battery substrate can be made wider than existing electrodes. This reduces the thickness of the electrode without changing the conductive effect, allowing for shorter deposition times and significantly improving equipment productivity. Furthermore, because the shape of the hollow pattern on the flexible mask matches the shape of the electrode, the line width of the hollow pattern is increased, the hollow area is larger, and the non-hollow area is reduced. Therefore, when using this flexible mask for electrode material deposition, the amount of electrode material deposited in the non-hollow areas of the flexible mask is reduced, thereby reducing the amount of raw material used.

[0022] In some possible implementations, the thickness of the first layer is 5 nm to 300 nm; and / or the thickness of the second layer is 0.5 μm to 20 μm; and / or the thickness of the third layer is 5 nm to 300 nm. A three-layer structure within this thickness range can meet the functional requirements of each layer and reduce costs.

[0023] In some possible implementations, the width of the electrode at any position is 5μm to 500μm, and the ratio between the thickness and width of the electrode is 0.001 to 0.2. In this way, without changing the conductive effect, compared with the existing electrodes with larger aspect ratios, the present application significantly reduces the aspect ratio of the electrode, and the electrode structure has good stability and is not prone to deformation or tipping. Because the smaller aspect ratio makes the width of the electrode larger, a good conductive effect can be achieved using thinner materials. This allows the electrode to be prepared in a shorter deposition time, greatly improving the equipment production capacity. Since the shape of the hollow pattern on the flexible mask used in electrode production is consistent with the shape of the electrode, the hollow area is larger and the non-hollow area is reduced. Therefore, when the flexible mask is used to deposit the electrode material, the amount of electrode material deposited on the non-hollow part of the flexible mask is reduced. Therefore, the larger the area of ​​the hollow pattern, the higher the utilization rate of the raw material, which reduces the amount of raw material used. In addition, the wider electrode can be set on the back of the battery substrate, and the formed back electrode or back contact electrode will not block the light absorption of the solar cell.

[0024] In some possible implementations, the material of the first layer includes one or more combinations of metal oxides, metal nitrides, metal fluorides, metal silicides, and metals. These materials enhance adhesion between the electrode and the battery substrate surface, reducing contact resistivity. For some battery types, these materials also prevent metal diffusion toward the battery substrate surface.

[0025] In some possible implementations, the metal oxide material includes AZO, TiO X 、Cu2O、MgO x 、TaO x , VO x CrO x , SnO2, B: ZnO and MoO x One or more combinations thereof; and / or, the material of the metal nitride includes TiN x and TiO x N y and / or, the material of the metal fluoride includes one or more combinations of MgF2, LiF, YF3 and CeF3; and / or, the material of the metal silicide includes TiSi2, TaSi2, M O Si2、CoSi 2、 The metal may be one or more combinations of Ni2Si and WSi2; and / or the metal may be one or more combinations of Ni, Ti, and Cr. The first layer may be formed of any one of the materials to form a single layer, or a stack of several different materials to form a single layer.

[0026] In some possible implementations, the second layer includes one or more combinations of aluminum and copper. By using lower-cost aluminum or copper as the main conductive portion of the electrode, costs are significantly reduced compared to existing silver electrodes.

[0027] In some possible implementations, the material of the third layer includes one or more combinations of nickel, silver, tin, aluminum-nickel alloy, and aluminum-tin alloy. These materials are easy to weld and have high strength after welding, which is conducive to welding and fixing the electrode to the welding strip.

[0028] In some possible implementations, the resistivity of the electrode is less than or equal to 3×10 -6 Compared with existing electrodes, the present invention reduces the resistivity of the electrode, and the main body of the electrode, that is, the second layer, can be made of a material with a lower resistivity to improve the conductive performance.

[0029] In some possible implementations, the electrode includes a collector grid line, or the electrode includes intersecting collector grid lines and bus grid lines; wherein the line width of the collector grid line is equal everywhere, and the line width of the bus grid line is equal everywhere. In this case, when the thickness of the collector grid line remains unchanged, the line width is equal everywhere, which can ensure that the resistance and stress of the collector grid line remain consistent, thereby avoiding excessive current damage and uneven stress. The line width of the bus grid line is equal everywhere. In this case, when the thickness of the bus grid line remains unchanged, the line width is equal everywhere, which can ensure that the resistance and stress of the bus grid line remain consistent, thereby avoiding excessive current damage and uneven stress.

[0030] In some possible implementations, the thickness of the electrode in the middle is greater than the thickness of the electrodes on both sides along the width direction. This creates a sloped surface along the width direction of the electrode. This sloped surface can dissipate some of the light that strikes the electrode to the surface of the battery substrate, thereby increasing the utilization of the incident light.

[0031] In a second aspect, the present application further provides a method for preparing a solar cell, comprising:

[0032] Providing a battery substrate and a flexible mask, wherein the battery substrate has two opposite surfaces;

[0033] Fixing a flexible mask to at least one side of a battery substrate, wherein the flexible mask has a hollow pattern;

[0034] Depositing a first layer, a second layer, and a third layer in a stacked arrangement on the flexible mask in sequence, wherein the first layer deposited at the hollow pattern contacts the surface of the battery substrate;

[0035] The flexible mask is removed so that the first layer, the second layer, and the third layer deposited at the hollow pattern remain on the surface of the battery substrate to form an electrode; wherein the adhesion of the first layer to the surface of the battery substrate is greater than the adhesion of the second layer and the third layer to the surface of the battery substrate, and the contact resistivity of the first layer to the surface of the battery substrate is less than the contact resistivity of the second layer and the third layer to the surface of the battery substrate; or, the melting point of the first layer is greater than the melting points of the second layer and the third layer; the resistivity of the second layer is less than the resistivity of the first layer and the third layer; and the melting point or surface tension of the third layer is less than the melting point or surface tension of the first and second layers.

[0036] When the above technical solution is adopted, a flexible mask is fixed on the surface of the battery substrate, and the flexible mask has a hollow pattern. The first layer, the second layer, and the third layer are sequentially deposited on the flexible mask to form a stacked arrangement. After removing the flexible mask, the three-layer structure deposited at the hollow pattern is retained to form an electrode, so that the first layer is in contact with the surface of the battery substrate. Since this preparation method can obtain the solar cell in the present application, it has the same beneficial effects as the first aspect and will not be described in detail here. In addition, since this preparation method uses a flexible mask to prepare the electrode, compared with the existing method of screen printing silver paste and sintering, the preparation process of the method of the present application is simpler, does not require sintering of the silver paste, and avoids damage to the battery substrate caused by high-temperature sintering.

[0037] In some possible implementations, a first layer, a second layer, and a third layer are sequentially deposited on a flexible mask by a physical vapor deposition method to form a stacked arrangement. In this way, the physical vapor deposition method can be vacuum evaporation, sputtering, ion plating, etc. The first layer, the second layer, and the third layer are sequentially deposited on the flexible mask by the physical vapor deposition method. Compared with the existing method of making electrodes by screen printing silver paste and sintering, the physical vapor deposition method of the present application is combined with a flexible mask to simplify the preparation process. Compared with the existing photoresist or ink preparation electrode process, the use of a flexible mask and a deposition process simplifies the preparation process. The cost of the flexible mask is low, which reduces the cost. The flexible mask can be removed by tearing, and there is no need to chemically etch the photoresist or ink, which reduces the generation of a large amount of wastewater and is more environmentally friendly.

[0038] In some possible implementations, the first layer is deposited on the flexible mask by a magnetron sputtering method; and / or, the second layer is deposited on the flexible mask by an evaporation method; and / or, the third layer is deposited on the flexible mask by a magnetron sputtering method or an evaporation method.

[0039] In some possible implementations, the side of the battery substrate to which the flexible mask is fixed has a dielectric layer. After the flexible mask is fixed to at least one surface of the battery substrate, and before the first layer, the second layer, and the third layer are sequentially deposited on the flexible mask to form a stacked arrangement, the preparation method further includes: etching the side of the battery substrate to which the flexible mask is fixed to remove the dielectric layer at the corresponding hollow pattern of the battery substrate; wherein the first layer deposited at the hollow pattern contacts the surface of the battery substrate, specifically: the first layer deposited at the hollow pattern contacts the surface of the battery substrate after the dielectric layer is removed.

[0040] In the case of sampling the above technical solution, when there is a dielectric layer on the surface of the battery substrate, since the dielectric layer is an insulating layer, the conductive contact effect between the dielectric layer and the electrode is not very good. In order to improve the good conductive contact between the electrode and the battery substrate, it is necessary to remove the dielectric layer from the part where the electrode is formed on the surface of the battery substrate.

[0041] In some possible implementations, the flexible mask is fixed to the surface of the battery substrate by gluing or pressing. This configuration, because the flexible mask itself is a single piece of flexible material, can be fixed and covered on the battery substrate by gluing or pressing. Compared to existing methods such as silk screen printing, transfer printing, and photoresist, the flexible mask is more convenient to use, simplifies the process, and reduces costs.

[0042] In some possible implementations, the flexible mask includes a polymer film layer and an adhesive film layer that are stacked, and the flexible mask is adhered and covered on the surface of the battery substrate through the adhesive film layer.

[0043] When adopting the above technical solution, the flexible mask is bonded and fixed to the surface of the battery substrate through the adhesive film layer. The polymer film layer provides good flexibility and toughness, and can fit more snugly on the surface of the battery substrate, ensuring the fitting accuracy and not prone to breakage. The pasted flexible mask is easy to tear off later.

[0044] In some possible implementations, the material of the polymer film layer is one or more combinations of polyethylene terephthalate, polyolefin film, polyimide, and polyvinyl chloride;

[0045] The material of the adhesive film layer is one or more combinations of silicone, acrylic glue, polyurethane, rubber, and polyisobutylene.

[0046] When the above technical solution is adopted, the material of the polymer film layer can provide good flexibility and toughness, can fit more closely to the surface of the battery substrate, ensure the fitting accuracy, and is not prone to breakage. The pasted flexible mask is easy to tear off later.

[0047] In some possible implementations, removing the flexible mask includes:

[0048] Performing viscosity reduction treatment on the flexible mask to reduce the peel strength of the flexible mask;

[0049] The flexible mask is peeled off from the surface of the battery substrate.

[0050] When the flexible mask is used, it adheres to the battery substrate. When it is necessary to remove the flexible mask from the battery substrate, the flexible mask is subjected to a viscosity-reducing treatment to reduce the peel strength of the flexible mask, making it easier to peel the flexible mask from the battery substrate without causing the battery substrate to break or crack.

[0051] In some possible implementations, the viscosity reduction treatment includes one or more combinations of cooling viscosity reduction treatment, heating viscosity reduction treatment, ultraviolet light irradiation viscosity reduction treatment, alternating magnetic field viscosity reduction treatment, and solvent immersion viscosity reduction treatment.

[0052] When the above technical solution is adopted, since the flexible mask has a sticky film layer, the viscosity of the sticky film layer can be reduced by cooling; or, the viscosity of the sticky film layer can be reduced by heating; or, the viscosity of the sticky film layer can be reduced by applying an alternating magnetic field; or, the viscosity of the sticky film layer can be reduced by ultraviolet light irradiation; or, the viscosity of the sticky film layer can be reduced by immersing the flexible mask in a solvent.

[0053] In some possible implementations, when a cooling viscosity reduction process is used, the viscosity reduction temperature in the cooling viscosity reduction process is 15° C. to 30° C., and the peel strength of the flexible mask after viscosity reduction is 1 gf / cm to 50 gf / cm.

[0054] When the above technical solution is adopted, when the flexible mask is working normally, the peel strength of the flexible mask is high and can be firmly adhered to the surface of the battery substrate. When the flexible mask is cooled to room temperature, the peel strength of the flexible mask is reduced to this range, and the flexible mask can be easily peeled off.

[0055] In some possible implementations, the viscosity reduction temperature in the heating viscosity reduction treatment is 60° C. to 180° C., and the peel strength of the flexible mask after viscosity reduction is 1 gf / cm to 50 gf / cm.

[0056] When the above technical solution is adopted, when the flexible mask is working normally, the peel strength of the flexible mask is high and can be firmly adhered to the surface of the battery substrate. When the flexible mask is heated to 60°C to 180°C, the peel strength of the flexible mask is reduced to within this range, and the flexible mask can be easily peeled off. BRIEF DESCRIPTION OF THE DRAWINGS

[0057] The drawings described herein are used to provide a further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:

[0058] Figures 1 to 5 are schematic diagrams of a process for preparing a solar cell according to an embodiment of the present application;

[0059] 6 to 9 are schematic diagrams of another process for preparing a solar cell according to an embodiment of the present application;

[0060] FIG10 is a schematic structural diagram of an electrode of a solar cell provided in an embodiment of the present application.

[0061] Reference numerals: 1 is a battery substrate, 11 is a dielectric layer, 2 is a flexible mask, 21 is a hollow pattern, 3 is an electrode, 31 is a first layer, 32 is a second layer, 33 is a third layer, 34 is a collector grid line, and 35 is a busbar line. Specific embodiments

[0062] In order to make the technical problems, technical solutions and beneficial effects to be solved by this application more clearly understood, this application is further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain this application and are not intended to limit this application.

[0063] It should be noted that when an element is referred to as being “fixed on” or “disposed on” another element, it may be directly on the other element or indirectly on the other element. When an element is referred to as being “connected to” another element, it may be directly connected to the other element or indirectly connected to the other element.

[0064] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, "multiple" means two or more, unless otherwise clearly and specifically defined. "Several" means one or more, unless otherwise clearly and specifically defined.

[0065] In the description of this application, it should be understood that the terms "up", "down", "front", "back", "left", "right", etc., indicating directions or positional relationships, are based on the directions or positional relationships shown in the accompanying drawings. They are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction. Therefore, they should not be understood as limitations on this application.

[0066] In the description of this application, it should be noted that, unless otherwise expressly specified or limited, the terms "installed," "connected," and "connected" should be understood in a broad sense. For example, they can refer to fixed connections, detachable connections, or integral connections; they can refer to mechanical connections or electrical connections; they can refer to direct connections or indirect connections through an intermediate medium; they can refer to internal communication between two components or the interaction between two components. Those skilled in the art will understand the specific meanings of the above terms in this application based on the specific circumstances.

[0067] Solar cells primarily consist of cells and electrodes. The cells absorb sunlight and convert it into electrical energy. The electrodes transmit the current generated by the cells to an external circuit.

[0068] At present, the electrodes of solar cells are generally prepared by screen-printing silver paste, which is formed into silver electrodes after high-temperature sintering. The bonding strength between the silver electrodes and the battery substrate is poor, and the cost of the silver paste material is high.

[0069] In view of this, an embodiment of the present application provides a solar cell, as shown in Figures 5 and 9, including a cell substrate 1 and an electrode 3 arranged on at least one surface of the cell substrate 1, the electrode 3 includes a first layer 31, a second layer 32 and a third layer 33 stacked in sequence, and the first layer 31 is in contact with the surface of the cell substrate 1.

[0070] The adhesion between the first layer 31 and the surface of the battery substrate 1 is greater than the adhesion between the second layer 32 and the third layer 33 and the surface of the battery substrate 1, and the contact resistivity between the first layer 31 and the surface of the battery substrate 1 is less than the contact resistivity between the second layer 32 and the third layer 33 and the surface of the battery substrate 1; alternatively, the melting point of the first layer 31 is greater than the melting points of the second layer 32 and the third layer 33. The resistivity of the second layer 32 is less than the resistivity of the first layer 31 and the third layer 33; and the melting point or surface tension of the third layer 33 is less than the melting points or surface tension of the first layer 31 and the second layer 32.

[0071] The adhesion between the first layer 31 and the surface of the battery substrate 1 is greater than the adhesion between the second layer 32 and the third layer 33. This means that the adhesion between the first layer 31 and the surface of the battery substrate 1 is greater than the adhesion between the second layer 32 and the surface of the battery substrate 1, and the adhesion between the first layer 31 and the surface of the battery substrate 1 is greater than the adhesion between the third layer 33 and the surface of the battery substrate 1. The adhesion between the second layer 32 and the surface of the battery substrate 1 refers to the adhesion between the second layer and the surface of the battery substrate 1 when the two layers are in contact; the adhesion between the third layer 33 and the surface of the battery substrate 1 refers to the adhesion between the third layer and the surface of the battery substrate 1 when the two layers are in contact.

[0072] When using the above technical solution, the electrode 3 on the battery substrate 1 comprises a three-layer structure, wherein the first layer 31 of the electrode 3 is in direct contact with the battery substrate 1, the second layer 32 of the electrode 3 is disposed on the first layer 31, and the third layer 33 of the electrode 3 is disposed on the second layer 32. Because the adhesion of the first layer 31 to the surface of the battery substrate 1 is greater than the adhesion of the second layer 32 and the third layer 33 to the surface of the battery substrate 1, the adhesion of the electrode 3 to the battery substrate 1 is increased, thereby improving the bonding strength between the electrode 3 and the battery substrate 1, compared to existing silver electrode-to-battery substrate bonding. Furthermore, the direct contact between the first layer 31 and the battery substrate 1 results in a lower contact resistivity than that of a silver electrode, making it easier to achieve good ohmic contact between the electrode 3 and the battery substrate 1. Because electrode 3 has a three-layer structure, the second layer 32 can be made solely of a material with low resistivity and low cost, such as aluminum, as the main conductive material. The third layer 33 can be made of a material with a low melting point or low surface tension. Generally, materials with low surface tension have a tendency to flow easily over their molten liquid, resulting in a small contact angle, which results in good wettability with the soldering ribbon and facilitates soldering. Furthermore, materials with low melting points are generally easier to solder to the soldering ribbon. Compared to existing electrodes made entirely of silver, the three-layer electrode structure of this application can reduce costs.

[0073] Furthermore, for some types of battery substrates 1, the melting point of the first layer 31 is greater than that of the second layer 32 and the third layer 33. This higher melting point indicates that the interatomic bonding forces within the first layer 31 are relatively strong, making diffusion less likely. Consequently, the diffusion barrier capability of the first layer 31 is greater than that of the second layer 32 and the third layer 33, effectively preventing metal atoms from diffusing into the battery substrate 1. Compared to existing silver electrodes that directly contact the battery substrate, the present invention utilizes the first layer 31 to prevent metal atoms in the second layer 32 from diffusing into the battery substrate 1, thereby reducing contamination of the battery substrate 1.

[0074] For example, the surface of the battery substrate 1 in contact with the electrode 3 is a transparent conductive oxide film (i.e., TCO film), the adhesion between the first layer 31 and the transparent conductive oxide film is greater than the adhesion between the second layer 32 and the third layer 33 and the transparent conductive oxide film, and the contact resistivity between the first layer 31 and the transparent conductive oxide film is less than the contact resistivity between the second layer 32 and the third layer 33 and the transparent conductive oxide film;

[0075] Alternatively, the surface of the battery substrate 1 in contact with the electrode 3 serves as a carrier transport layer, and the melting point of the first layer 31 is greater than that of the second layer 32 and the third layer 33, resulting in the performance showing that the diffusion barrier capability of the first layer 31 is greater than that of the second layer 32 and the third layer 33. The carrier transport layer herein does not include a TCO film; instead, the carrier transport layer may be a silicon substrate, a doped polycrystalline silicon layer, a doped amorphous silicon layer, a doped microcrystalline silicon layer, a doped nanocrystalline silicon layer, a hole transport layer, an electron transport layer, or the like. The hole transport layer may be a molybdenum oxide layer, a nickel oxide layer, a cuprous oxide layer, or the like; the electron transport layer may be a tin oxide layer, a tin oxide layer, a titanium oxide layer, or the like. Of course, other types of carrier transport layers can also be silicon oxide layers, aluminum oxide layers, silicon oxynitride layers, hafnium dioxide (HfO2) layers, gallium oxide (Ga2O3) layers, tantalum pentoxide (Ta2O5) layers, niobium pentoxide (Nb2O5) layers, silicon nitride layers, silicon carbonitride layers, aluminum nitride layers, titanium nitride (TiN) layers, titanium carbonitride (TiCN) layers, silicon carbide (SiC) layers, etc.

[0076] When the above technical solution is adopted, when the surface of the battery substrate 1 in contact with the electrode 3 is a transparent conductive oxide film, the first layer 31 of the electrode 3 mainly plays the role of increasing the adhesion between the electrode 3 and the surface of the battery substrate 1 and reducing the contact resistance.

[0077] When the surface of the battery substrate 1 in contact with the electrode 3 serves as the aforementioned carrier transport layer, the first layer 31 of the electrode 3 primarily serves to prevent metal atoms from diffusing into the surface of the battery substrate 1. Because the melting point of the first layer 31 is relatively high, the interatomic bonding forces within the first layer 31 are relatively strong, making diffusion less likely. Therefore, the first layer 31 can be used to prevent metal atoms from diffusing into the battery substrate 1.

[0078] In some embodiments, the first layer 31 includes one or more combinations of metal oxides, metal nitrides, metal fluorides, metal silicides, and metals. That is, the first layer 31 may have only one layer of metal oxide, or only one layer of metal nitride, or only one layer of metal fluoride, or only one layer of metal silicide, or only one layer of metal. Of course, the first layer 31 may also include multiple metal oxides, metal nitrides, metal fluorides, metal silicides, and metals. The first layer 31 may also have a multi-layer stacked structure, each layer of which may include any one or more of metal oxides, metal nitrides, metal fluorides, metal silicides, and metals.

[0079] Taking the example of a first layer 31 comprising a metal oxide, when the first layer 31 containing the metal oxide contacts the transparent conductive oxide film of the battery substrate 1, defects such as oxygen vacancy mismatch exist at the interface between the transparent conductive oxide film and the metal oxide of the first layer 31 due to the inevitable presence of defects in the crystal lattice of the doped element in the transparent conductive oxide film. During the preparation process of the electrode 3 of the present application, the deposited particles of the first layer 31 preferentially nucleate at the defects. As heat accumulates during the deposition process, the nucleated deposited particle clusters gain energy to continue diffusion, migration, and crystallization growth. Oxygen vacancies exist at the respective contact interfaces of the metal oxide and the transparent conductive oxide film. During the preparation process of the electrode of the present application, the transparent conductive oxide film and the metal oxide diffuse at the interface, bonding the metal and oxygen atoms to compensate for the oxygen vacancies, thereby forming a mutually meshed state in the microstructure. Macroscopically, this enhances the adhesion of the electrode to the battery substrate surface, improving surface adhesion, i.e., improving the adhesion of the electrode 3 to the transparent conductive oxide film of the battery substrate 1.

[0080] Similarly, the first layer 31 uses other materials such as metal nitrides, metal fluorides and metal silicides. These materials have a similar principle to metal oxides in that they can improve surface adhesion. Compared with silver electrodes, they can form vacancies or dangling bonds that can be combined with the transparent conductive oxide film, thereby improving surface adhesion.

[0081] In addition, compared with the existing silver electrode, the first layer 31 using the above-mentioned material can have more choices from metal oxides, metal nitrides, metal fluorides, and metal silicides. It can choose materials that are more compatible with the energy band of the transparent conductive oxide film and have smaller interface complexation. It can reduce the contact resistivity between the first layer 31 and the transparent conductive oxide film, that is, reduce the contact resistivity between the electrode 3 and the battery substrate 1.

[0082] For some types of batteries, such as batteries with carrier transport layers, the interatomic bonding forces of the above-mentioned metal oxides, metal nitrides, metal fluorides, metal silicides and metals are relatively strong. In this case, diffusion is not easy to occur, so they can prevent metal atoms from diffusing into the battery substrate 1, and have the effect of preventing metal from diffusing to the surface of the battery substrate 1.

[0083] For example, the metal oxide material includes AZO, TiO X 、Cu2O、MgO x 、TaO x , VO x CrO x , SnO2, B: ZnO and MoO xOne or more combinations thereof. That is, the metal oxide may be a single layer of the aforementioned metal oxide, or a laminated structure formed by multiple layers of the aforementioned metal oxides of different materials, or a layer formed by a mixture of the aforementioned multiple materials. To save materials and improve efficiency, a single layer of metal oxide may be sufficient.

[0084] In some embodiments, the material of the metal nitride includes TiN x and TiO x N y The metal nitride may be one or more combinations of the above materials. Specifically, the metal nitride may be a single layer of the above-mentioned metal nitride, or a laminated structure formed by multiple layers of the above-mentioned metal nitrides of different materials, or a layer formed by a mixture of the above-mentioned multiple materials. To save materials and improve efficiency, a single layer of metal nitride may be sufficient.

[0085] In other embodiments, the metal fluoride material includes one or more combinations of MgF2, LiF, YF3, and CeF3. Specifically, the metal fluoride can be a single layer of a single metal fluoride, a laminated structure formed by multiple layers of metal fluorides of different materials, or a layer formed by a mixture of multiple materials. To save material and improve efficiency, a single layer of metal nitride can suffice.

[0086] In some other embodiments, the material of the metal silicide includes TiSi2, TaSi2, M O The metal silicide may be a combination of one or more of Si2, CoSi2, Ni2Si, and WSi2. That is, the metal silicide may be a single layer of the aforementioned metal silicide, or a stacked structure formed by multiple layers of the aforementioned metal silicides of different materials, or a layer formed by a mixture of the aforementioned multiple materials. To save materials and improve efficiency, a single layer of metal silicide may be sufficient.

[0087] In some embodiments, the metal material includes one or more combinations of Ni, Ti, and Cr. That is, the metal can be a single layer of the aforementioned metal, or a laminated structure formed by multiple layers of the aforementioned metals of different materials, or a layer formed by a mixture of the aforementioned multiple materials. To save material and improve efficiency, a single layer of metal can be sufficient.

[0088] In this embodiment, the material of the second layer 32 includes one or more combinations of aluminum and copper. Specifically, the second layer 32 can be a single layer 32 of a single material, a laminated structure comprising multiple layers 32 of different materials, or a layer comprising a mixture of the aforementioned materials. Aluminum or copper has low resistivity and is relatively low cost. Therefore, by using relatively low-cost aluminum or copper as the primary conductive component of the electrode 3, costs can be significantly reduced without affecting electrode resistance, compared to existing silver electrodes.

[0089] In some possible implementations, the material of the third layer 33 includes one or more combinations of nickel, silver, tin, aluminum-nickel alloy, and aluminum-tin alloy. That is, the third layer 33 can be a single layer of the aforementioned material, or a laminated structure formed by multiple layers of the aforementioned different materials, or a layer formed by a mixture of the aforementioned materials. These materials are all easily welded and have high strength after welding, which facilitates the welding and fixing of the electrode 3 to the welding ribbon.

[0090] In some possible implementations, the projections of the first layer 31, the second layer 32, and the third layer 33 on the battery substrate 1 overlap. Since the three-layer structure of the electrode 3 is deposited through the same flexible mask 2, the three-layer structure has the same shape.

[0091] In some embodiments, the line width of the electrode 3 at any position is 5 μm to 1500 μm, the thickness of the electrode at any position is 0.5 μm to 21 μm, and the ratio between the thickness and width of the electrode is 0.001 to 0.2.

[0092] Under the condition of the same material, the resistance of the electrodes 3 with the same cross-sectional area is usually equal. In this case, the conductive effect of the electrodes 3 is also considered to be the same. This means that after significantly increasing the line width of the electrode 3, the thickness of the electrode 3 can be significantly reduced without changing the conductive effect. Therefore, by increasing the line width, reducing the thickness, and reducing the aspect ratio, the aspect ratio can be reduced to 0.001-0.2 without changing the conductive effect (i.e., the resistance is constant). The structural stability of the electrode is good and it is not easy to deform or fall. Due to the large line width of the electrode 3, a good conductive effect can be achieved using thinner materials. This allows the electrode to be prepared in a shorter deposition time, greatly improving the equipment capacity. Since the shape of the hollow pattern on the flexible mask 2 is consistent with the shape of the electrode 3, the line width of the hollow pattern is increased, the hollow area is larger, and the non-hollow area is reduced. Therefore, when the flexible mask 2 is used to deposit the electrode material, the amount of material deposited on the non-hollow part of the flexible mask 2 is reduced. Therefore, the larger the line width of the hollow pattern, the higher the utilization rate of the raw material, which reduces the amount of raw material used. In addition, the wider electrode 3 helps reduce the welding debris rate and improve the yield rate. The wider electrode 3 increases the contact area and can enhance the bonding strength between the electrode 3 and the battery substrate 1. Moreover, the wider electrode 3 can be placed on the back side of the battery substrate 1, and the formed back electrode or back contact electrode will not block the light absorption of the solar cell.

[0093] Of course, the ratio between the thickness and width of the electrode 3, i.e., the aspect ratio, can also be in other numerical ranges and can be greater than 0.2. For example, the aspect ratio can be 0.3, 0.5, 1, 1.5, 2, etc. The electrode 3 with this aspect ratio can meet the use requirements of a three-layer structure electrode. For an electrode 3 with a larger aspect ratio, it can be placed on the front surface of the battery substrate 1 to reduce light shading of the front electrode.

[0094] As shown in FIG10 , the electrode 3 includes a collector grid line 34 ; alternatively, the electrode 3 includes intersecting collector grid lines 34 and bus grid lines 35 ; wherein the width of the collector grid lines 34 is 30 μm to 500 μm, and the width of the bus grid lines 35 is 100 μm to 1500 μm. Typically, the width of the bus grid lines 35 is greater than the width of the collector grid lines 34 . For example, the width of the collector grid lines 34 can be 30 μm, 50 μm, 100 μm, 160 μm, 220 μm, 350 μm, 400 μm, 500 μm, etc., and the width of the bus grid lines 35 can be 100 μm, 200 μm, 300 μm, 400 μm, 500 μm, 600 μm, 800 μm, 1100 μm, 1300 μm, 1500 μm, etc.

[0095] When using the above technical solution, compared to existing electrodes, the collector grid lines 34 and bus grid lines 35 located on the back of the battery substrate 1 can be increased in line width. Without changing the conductive effect, the thickness of the electrode 3 is reduced, and the electrode preparation can be completed in a shorter deposition time, which greatly improves the equipment production capacity. Moreover, because the shape of the hollow pattern on the flexible mask 2 is consistent with the shape of the electrode 3, the line width of the hollow pattern is increased, the hollow area is larger, and the non-hollow area is reduced. Therefore, when using this flexible mask 2 for electrode material deposition, the amount of electrode material deposited in the non-hollow portion of the flexible mask 2 is reduced, thereby reducing the amount of raw material used.

[0096] In some embodiments, the thickness of the first layer 31 is less than or equal to 10% of the thickness of the second layer 32; and / or the thickness of the third layer 33 is less than or equal to 10% of the thickness of the second layer 32. This arrangement results in the first layer 31 and the third layer 33 being relatively thin, with the second layer 32 comprising the majority of the material. Since the second layer 32 has the lowest resistivity of the three layers, the thinner first and third layers 31 and 33 can minimize the distance current travels through the higher resistivity material, thereby reducing current losses. Furthermore, the thinner first and third layers 31 and 33 can also reduce the amount of material used in these two layers, thereby lowering costs.

[0097] Exemplarily, the thickness of the first layer 31 is 5 nm to 300 nm, for example, the thickness of the first layer 31 can be 10 nm to 200 nm, more preferably 30 nm to 100 nm. Specifically, the thickness of the first layer 31 can be 30 nm, 40 nm, 50 nm, 65 nm, 75 nm, 80 nm, 90 nm, 100 nm, etc.

[0098] Exemplarily, the thickness of the second layer 32 is 0.5 μm to 20 μm, for example, 2 μm to 15 μm, more preferably 3 μm to 7 μm. Specifically, the thickness of the second layer 32 can be 3 μm, 4 μm, 5 μm, 6 μm, 7 μm, etc.

[0099] Exemplarily, the thickness of the third layer 33 is 5 nm to 300 nm. For example, the thickness of the third layer 33 may be 50 nm to 200 nm, more preferably 80 nm to 120 nm. Specifically, the thickness of the third layer 33 may be 80 nm, 85 nm, 90 nm, 100 nm, 110 nm, 120 nm, etc.

[0100] The thickness range of the above three-layer structure can meet the functional requirements of each layer and can reduce costs.

[0101] In some embodiments, the total thickness of the electrode 3 is less than 10% of the thickness of the battery substrate 1 , which can reduce the total thickness of the battery substrate 1 and the welding ribbon cross section after welding, thereby reducing the risk of cracking during the packaging process.

[0102] Furthermore, in some embodiments, the widths of the first layer 31, the second layer 32, and the third layer 33 at any position of the electrode 3 are equal. Thus, the three-layer structure of the electrode 3 has the same width and can be deposited under the same flexible mask 2, simplifying the process. In some possible implementations, the resistivity of the electrode 3 is less than or equal to 3×10 -6 Ω·cm, the resistivity of the second layer 32 is lower than the resistivity of the first layer 31 and the third layer 33; the resistivity of the first layer 31 can be higher than the resistivity of the third layer 33, or the resistivity of the first layer 31 can be lower than the resistivity of the third layer 33, or they can be equal. Compared with existing electrodes, the present application reduces the resistivity of the electrode.

[0103] As shown in Figure 10, in some embodiments, the width of the current collecting yarn 34 is uniform throughout, and the width of the bus yarn 35 is uniform throughout. In this case, while the thickness of the current collecting yarn 34 remains unchanged, the uniform width ensures that the resistance and stress at all locations of the current collecting yarn 34 remain consistent, thereby avoiding damage from excessive current flow and uneven stress. The width of the bus yarn 35 is uniform throughout. In this case, while the thickness of the bus yarn 35 remains unchanged, the uniform width ensures that the resistance and stress at all locations of the bus yarn 35 remain consistent, thereby avoiding damage from excessive current flow and uneven stress. Of course, the width of each section of each current collecting yarn 34 may fluctuate within a certain error range, with the error being less than or equal to 10%. The width of each section of each bus yarn 35 may also fluctuate within a certain error range, with the error being less than or equal to 10%. For example, the error may be 10%, 9%, 8.5%, 8%, 7.5%, 7%, 6%, 5%, 4%, 3%, 2%, 1%, 0.5%, 0%, etc.

[0104] In some possible implementations, along the width direction of electrode 3, the thickness of the middle of electrode 3 is greater than the thickness of the sides of electrode 3. Thus, the widthwise edges of electrode 3 form sloped surfaces. In this case, the side surfaces of the electrode are inclined relative to the battery substrate 1. The inclined side surfaces of electrode 3 can dissipate some of the light incident on electrode 3 to the surface of battery substrate 1, thereby increasing the utilization rate of the incident light.

[0105] The present application also provides a method for preparing a solar cell, as shown in Figures 1 to 5. The method can be used to prepare the solar cell described in any of the above embodiments, and the method includes the following steps:

[0106] In step S100, a battery substrate 1 and a flexible mask 2 are provided. The battery substrate 1 has two opposing surfaces. The battery substrate 1 may be a semiconductor substrate, for example, a silicon substrate, a germanium substrate, or a germanium-silicon substrate. Different functional layers, such as a dielectric layer, an anti-reflection layer, and a tunneling layer, are provided on the semiconductor substrate according to different battery types.

[0107] In step S200, as shown in Figure 1, a flexible mask 2 is affixed to at least one side of the battery substrate 1. The flexible mask 2 has a hollow pattern. The flexible mask 2 is flexible and tough, primarily comprising a flexible film layer made of a polymer material. The hollow pattern on the flexible mask 2 extends through two opposing surfaces of the flexible mask 2. The area outside the hollow pattern serves as a shielding area, providing protection.

[0108] In step S300, as shown in Figures 2-4, a first layer 31, a second layer 32, and a third layer 33 are sequentially deposited on the flexible mask 2 to form a stacked arrangement. The first layer 31 deposited at the hollow pattern contacts the surface of the battery substrate 1. Specifically, as shown in Figure 2, the first layer 31 is first uniformly deposited on one surface of the battery substrate 1. The first layer 31 covers the entire area of ​​the flexible mask 2, including the hollow pattern area and the remaining blocked areas. The first layer 31 filling the hollow pattern directly contacts the surface of the battery substrate 1 for conductive contact. Then, as shown in Figure 3, the second layer 32 is uniformly deposited on the first layer 31. Then, as shown in Figure 4, the third layer 33 is uniformly deposited on the second layer 32.

[0109] In step S400, as shown in FIG5 , the flexible mask 2 is removed, leaving the first layer 31, the second layer 32, and the third layer 33 deposited at the hollow pattern on the surface of the battery substrate 1 to form the electrode 3. During the removal of the flexible mask 2, the first layer 31, the second layer 32, and the third layer 33 deposited and covering the shielded area of ​​the flexible mask 2 are removed along with the flexible mask 2, leaving only the three layers of material corresponding to the hollow pattern. The shape of the retained three layers of material is consistent with the pattern of the formed electrode 3.

[0110] In the above-described technical solution, a flexible mask 2 is applied to the surface of a battery substrate 1. The flexible mask 2 has a hollow pattern that matches the shape of the electrode. A first layer 31, a second layer 32, and a third layer 33 are sequentially deposited on the flexible mask 2 to form a stacked arrangement. After the flexible mask 2 is removed, the three-layer structure deposited in the hollow pattern remains, forming the electrode 3. The first layer 31 contacts the surface of the battery substrate 1. Because the adhesion of the first layer 31 to the surface of the battery substrate 1 is greater than that of the second and third layers 32 and 33, the adhesion and bonding strength of the electrode 3 to the battery substrate 1 are enhanced compared to existing silver electrode-to-battery substrate bonding methods. Furthermore, the direct contact between the first layer 31 and the battery substrate 1 results in a lower contact resistivity than with silver electrodes, making it easier to achieve good ohmic contact between the electrode 3 and the battery substrate 1. Because electrode 3 has a three-layer structure, the second layer 32 can be made solely of a material with low resistivity and low cost, such as aluminum, as the main conductive material. The third layer 33 can be made of a material with a low melting point or low surface tension. Generally, materials with low surface tension have a tendency to flow easily over their molten liquid, resulting in a small contact angle, which results in good wettability with the soldering ribbon and facilitates soldering. Furthermore, materials with low melting points are generally easier to solder to the soldering ribbon. Compared to existing electrodes made entirely of silver, the three-layer electrode structure of this application can reduce costs.

[0111] In addition, for some types of battery substrates 1, since the diffusion barrier capability of the first layer 31 is greater than that of the second layer 32 and the third layer 33, compared with the existing silver electrode directly contacting the battery substrate, the present application can also prevent the metal of the second layer 32 from diffusing into the interior of the battery substrate 1 through the first layer 31, thereby reducing contamination of the battery substrate 1.

[0112] In this embodiment, a first layer 31, a second layer 32, and a third layer 33 are sequentially deposited on a flexible mask by a physical vapor deposition method (PVD). The physical vapor deposition method may be vacuum evaporation, sputtering, ion plating, or the like. The first layer 31, the second layer 32, and the third layer 33 are sequentially deposited on the flexible mask 2 by the physical vapor deposition method. Compared to the existing method of making electrodes by screen printing silver paste, the physical vapor deposition method of the present application is simpler, and the contact resistance between the electrode 3 formed by PVD deposition and the battery substrate 1 is low. Furthermore, compared to the existing photoresist or ink electrode preparation process, the use of a flexible mask 2 and a deposition process simplifies the preparation process. The cost of the flexible mask 2 is low, reducing costs. The flexible mask 2 can be removed by tearing, without the need for chemical etching of the photoresist or ink, thereby reducing the generation of a large amount of wastewater and being more environmentally friendly. One or more PVD processes can be selected as needed to deposit each electrode layer.

[0113] For example, the first layer 31 is deposited on the flexible mask 2 by magnetron sputtering; and / or, the second layer 32 is deposited on the flexible mask 2 by evaporation; and / or, the third layer 33 is deposited on the flexible mask 2 by magnetron sputtering or evaporation. Of course, the appropriate deposition method can be selected according to actual work needs and is not limited to the methods listed in this embodiment.

[0114] As shown in Figures 6-9, an embodiment of the present application provides another method for preparing a solar cell. This method is basically the same as the first method, except that, as shown in Figure 6, the side of the cell substrate 1 covered with the flexible mask 2 has a dielectric layer 11. After the flexible mask 2 is covered on the dielectric layer 11 of the cell substrate 1 in step S200, and before the first layer 31, second layer 32, and third layer 33 are sequentially deposited on the flexible mask 2 in a stacked arrangement in step S300, as shown in Figure 8, the method further includes the following steps: as shown in Figure 7, etching the side of the cell substrate 1 covered with the flexible mask 2 to remove the dielectric layer 11 at the location corresponding to the hollow pattern of the cell substrate 1; wherein the first layer 31 deposited at the hollow pattern contacts the surface of the cell substrate 1, specifically: the first layer 31 deposited at the hollow pattern contacts the surface of the cell substrate 1 from which the dielectric layer 11 is removed. Finally, after removing the flexible mask 2, the solar cell shown in Figure 9 is obtained.

[0115] In the case where the surface of the battery substrate 1 has a dielectric layer 11, since the dielectric layer 11, such as SiNx, Al2O3, etc., is an insulating layer, the conductive contact effect between the dielectric layer 11 and the electrode 3 is not very good. In order to improve the good conductive contact between the electrode 3 and the battery substrate 1, it is necessary to remove the dielectric layer 11 from the part of the surface of the battery substrate 1 where the electrode 3 is formed.

[0116] Of course, in the case where there is no dielectric layer 11 on the back side of the cell substrate 1 , the step of removing the dielectric layer 11 is not necessary, and a suitable preparation step is selected according to different types of solar cells to be prepared.

[0117] In some embodiments, the flexible mask 2 is fixed and covered on the surface of the battery substrate 1 by pasting or pressing. Since the flexible mask 2 itself is a whole flexible material, it can be fixed and covered on the battery substrate 1 by pasting or pressing. Specifically, the flexible mask 2 can itself be a sticky material, or it can be pasted and fixed by an external sticky substance, such as applying glue. Alternatively, the flexible mask 2 is fixed and covered on the battery substrate 1 by pressing, specifically, by an external fixing component, such as a snap structure, after the flexible mask 2 is flattened and tightened, the flexible mask 2 is fixed to the battery substrate 1 by the snap structure. Compared with the conventional spin coating or coating method or silk screen printing or transfer method of existing photoresists, the use of the flexible mask 2 is more convenient, the process is simplified, and the cost is reduced.

[0118] In the case where the flexible mask 2 is inherently adhesive, in this embodiment, the flexible mask 2 may comprise a laminated polymer film layer and an adhesive film layer, with the flexible mask 2 adhered to the surface of the battery substrate 1 via the adhesive film layer. This provides excellent flexibility and toughness, allowing it to adhere closely to the surface of the battery substrate 1, ensuring precise adhesion and preventing breakage. The adhered flexible mask 2 is then easily removed. The flexible mask 2 is affixed and secured via its own adhesive film layer, which serves as a solidified part of the flexible mask 2. This facilitates the creation of the hollow pattern 21 prior to affixing the flexible mask 2, ensuring a more precise shape and size of the hollow pattern 21 and improving the precision of the patterning.

[0119] Specifically, the polymer film layer can be made of one or more combinations of polyethylene terephthalate (PET), polyolefin film (PO), polyimide (PI), and polyvinyl chloride (PVC). Preferably, the polyolefin film includes polyvinyl chloride and / or biaxially oriented polypropylene. The adhesive film layer can be made of one or more combinations of silicone, acrylic glue, polyurethane, rubber, and polyisobutylene. By using these materials, the polymer film layer possesses toughness and flexibility, allowing it to adhere closely to the surface of the battery substrate 1, ensuring precise adhesion and preventing breakage. The attached flexible mask 2 is also easy to remove later.

[0120] In some possible implementations, removing the flexible mask 2 in step S400 includes the following steps:

[0121] Step S401 : performing viscosity reduction treatment on the flexible mask 2 to reduce the peeling strength of the flexible mask 2 .

[0122] Step S402 : peeling the flexible mask 2 from the surface of the battery substrate 1 .

[0123] When using the above technical solution, the flexible mask 2 is adhered to the battery substrate 1 during use. When it is necessary to remove the flexible mask 2 from the battery substrate 1, the flexible mask 2 is subjected to a viscosity reduction treatment to reduce the peel strength of the flexible mask 2. This allows for easier peeling of the flexible mask 2 from the battery substrate 1, without causing breakage or cracking of the battery substrate 1. Furthermore, by reducing the viscosity of the flexible mask 2 before peeling and removing it, compared to existing photoresist or ink preparation methods, this method avoids the high cost of photolithography processes and is not subject to the large amounts of highly polluting wastewater generated by electroplating and chemical etching processes.

[0124] Illustratively, the viscosity reduction treatment includes one or more combinations of cooling viscosity reduction treatment, heating viscosity reduction treatment, ultraviolet light irradiation viscosity reduction treatment, alternating magnetic field viscosity reduction treatment, and solvent immersion viscosity reduction treatment.

[0125] Specifically, when a cooling viscosity reduction treatment is employed, the viscosity reduction temperature during the cooling viscosity reduction treatment is 15°C to 30°C, such as 20°C to 30°C, or 20°C to 25°C. The peel strength of the flexible mask 2 after viscosity reduction is 1 gf / cm to 50 gf / cm, such as 5 gf / cm to 30 gf / cm, or 6 gf / cm to 15 gf / cm. When the flexible mask 2 is operating normally, the peel strength is high, allowing it to be firmly bonded to the surface of the battery substrate 1. When the flexible mask 2 is cooled to room temperature, the peel strength of the flexible mask 2 decreases to within this range, allowing for easy peeling of the flexible mask 2.

[0126] When heat-induced viscosity reduction is used, the flexible mask 2 can be a heat-induced viscosity reduction tape, where the adhesive film layer is reduced in viscosity by heating. For example, the viscosity reduction temperature during the heat-induced viscosity reduction treatment is 60°C to 180°C, and the peel strength of the flexible mask after viscosity reduction is 1 gf / cm to 50 gf / cm. When the flexible mask 2 is operating normally, the peel strength is high, allowing it to firmly adhere to the surface of the battery substrate 1. When the flexible mask 2 is heated to 60°C to 180°C, the peel strength of the flexible mask 2 is reduced to within this range, allowing for easy peeling of the flexible mask 2.

[0127] When the flexible mask 2 is a magnetic de-viscosity tape, the viscosity of the sticky film layer is reduced by applying an alternating magnetic field; when the flexible mask 2 is a UV light de-viscosity tape, the viscosity of the sticky film layer is reduced by ultraviolet light irradiation; when the flexible mask 2 is a solvent de-viscosity tape, the flexible mask 2 is immersed in a solvent to reduce the viscosity of the sticky film layer. The solvent can be deionized water, an organic solvent, etc.

[0128] The present application provides a first specific solar cell manufacturing process, as shown in Figures 1 to 5, including the following steps:

[0129] In the first step, the flexible mask 2 made of polyimide is scratched according to the shape of the desired electrode 3 by ultrafast laser, that is, patterned, to form a patterned flexible mask 2 made of polymer material.

[0130] In the second step, the patterned flexible mask 2 is attached to the surface of the battery substrate 1 .

[0131] In the third step, magnetron sputtering is used to deposit TiN on the surface of the battery substrate 1 on which the flexible mask 2 is attached. x The first layer 31 is a TiN film. x The thickness of the film layer is 20nm~50nm.

[0132] In the fourth step, an aluminum film layer is deposited on the surface of the battery substrate 1 on which the first layer 31 has been deposited, as the second layer 32, by electron beam evaporation. The thickness of the deposited aluminum film layer is 3 μm to 7 μm.

[0133] In the fifth step, metal nickel is deposited on the surface of the battery substrate on which the first layer 31 and the second layer 32 have been deposited, as the third layer 33, by electron beam evaporation. The thickness of the deposited nickel film is 50nm to 100nm.

[0134] In the sixth step, the flexible mask 2 is removed by mechanical stripping, so that the electrode 3 is prepared on the surface of the battery substrate 1 to obtain a solar cell.

[0135] The present embodiment provides a second specific process for preparing a solar cell, comprising the following steps:

[0136] In the first step, the flexible mask 2 made of polyimide is scratched according to the desired electrode shape by ultrafast laser, that is, patterned, to form a patterned flexible mask 2 made of polymer material.

[0137] In the second step, the patterned flexible mask 2 is attached to the surface of the battery substrate 1 .

[0138] In the third step, a Cu2O film is deposited on the surface of the battery substrate 1 on which the flexible mask 2 has been attached, as the first layer 31, by electron beam evaporation. The thickness of the deposited Cu2O film is 10 nm to 40 nm.

[0139] In the fourth step, an aluminum film layer is deposited on the surface of the battery substrate 1 on which the first layer 31 has been deposited, as the second layer 32, by electron beam evaporation. The thickness of the deposited aluminum film layer is 3 μm to 7 μm.

[0140] In the fifth step, metal nickel is deposited on the surface of the battery substrate 1 on which the first layer 31 and the second layer 32 have been deposited, as the third layer 33, by electron beam evaporation. The thickness of the deposited nickel film is 50nm to 100nm.

[0141] In the sixth step, the flexible mask 2 is removed by mechanical stripping, so that the electrode 3 is prepared on the surface of the battery substrate 1 to obtain a solar cell.

[0142] The present embodiment provides a third specific process for preparing a solar cell, comprising the following steps:

[0143] In the first step, the flexible mask 2 made of polyimide is scratched according to the desired electrode shape by ultrafast laser, that is, patterned, to form a patterned flexible mask 2 made of polymer material.

[0144] In the second step, the patterned flexible mask 2 is attached to the surface of the battery substrate 1 .

[0145] In the third step, an AZO film layer is deposited on the surface of the battery substrate 1 on which the flexible mask 2 has been attached by magnetron sputtering as the first layer 31 . The thickness of the deposited AZO film layer is 10 nm to 40 nm.

[0146] In the fourth step, an aluminum film layer is deposited on the surface of the battery substrate 1 on which the first layer 31 has been deposited, as the second layer 32, by electron beam evaporation. The thickness of the deposited aluminum film layer is 3 μm to 7 μm.

[0147] In the fifth step, metallic silver is deposited on the surface of the battery substrate 1 on which the first layer 31 and the second layer 32 have been deposited, as the third layer 33, by electron beam evaporation. The thickness of the deposited silver film layer is 50nm to 100nm.

[0148] In the sixth step, the flexible mask 2 is removed by mechanical stripping, so that the electrode 3 is prepared on the surface of the battery substrate 1 to obtain a solar cell.

[0149] It should be noted that the above-mentioned solar cells can be PERC (Passivated Emitter and Rear Cell, passivated emitter and rear contact cell), back contact solar cell, HJT (Heterojunction Technology, heterojunction cell), TOPCon (Tunnel Oxide Passivated Contact, tunneling oxide passivated cell), etc., among which the back contact solar cell can be IBC (Interdigitated back contact, full back electrode contact solar cell), HBC (Heterojunction-IBC, back contact heterojunction solar cell), HPBC (composite passivated back contact solar cell), TBC (Topcon+IBC, back contact tunneling oxide passivated cell), etc.

[0150] For PERC cells, since the surface of the cell substrate 1 has a dielectric layer 11 (such as SiN x ), therefore, it is necessary to further include the step of etching the side of the battery substrate 1 covered with the flexible mask 2 after covering the battery substrate 1 with the flexible mask 2 in step S200 and before depositing the electrode layers in sequence on the flexible mask 2 in step S300, so as to remove the dielectric layer 11 at the hollow pattern corresponding to the battery substrate 1, as shown in FIG6-FIG. 9, so that the conductive film layer of the battery substrate 1 located below the dielectric layer 11 is in direct contact with the subsequently deposited first layer 31 to achieve good conductivity.

[0151] For HPBC and TOPcon cells, since the surface of the cell substrate 1 has a dielectric layer 11 (such as SiN x , Al2O3), therefore, it is necessary to further include the step of etching the side of the battery substrate 1 covered with the flexible mask 2 after covering the battery substrate 1 with the flexible mask 2 in step S200 and before depositing the electrode layers in sequence on the flexible mask 2 in step S300, so as to remove the dielectric layer 11 at the corresponding hollow pattern of the battery substrate 1, as shown in Figures 6 to 9, so that the conductive film layer of the battery substrate 1 located below the dielectric layer 11 is in direct contact with the subsequently deposited first layer 31 to achieve good conductivity.

[0152] For HBC cells and HJT cells, since the surface of the cell substrate 1 does not have the dielectric layer 11 , after completing step S200 of covering the cell substrate 1 with the flexible mask 2 , step S300 can be directly performed to deposit each electrode layer on the flexible mask 2 in sequence.

[0153] In the description of the above embodiments, specific features, structures, materials or characteristics may be combined in an appropriate manner in any one or more embodiments or examples.

[0154] The above description is merely a specific embodiment of the present application, but the scope of protection of the present application is not limited thereto. Any changes or substitutions that can be easily conceived by a person skilled in the art within the technical scope disclosed in this application should be included in the scope of protection of this application. Therefore, the scope of protection of this application should be based on the scope of protection of the claims.

Claims

1. A solar cell comprising a cell substrate and an electrode disposed on at least one surface of the cell substrate, The electrode comprises a first layer, a second layer and a third layer stacked in sequence, wherein the first layer contacts the surface of the battery substrate; The adhesion between the first layer and the surface of the battery substrate is greater than the adhesion between the second layer and the third layer and the surface of the battery substrate, and the contact resistivity between the first layer and the surface of the battery substrate is less than the contact resistivity between the second layer and the third layer and the surface of the battery substrate. ; Alternatively, the melting point of the first layer is greater than the melting points of the second layer and the third layer; The resistivity of the second layer is less than the resistivity of the first layer and the third layer; The melting point or surface tension of the third layer is lower than that of the first layer and the second layer.

2. The solar cell according to claim 1, in, The surface of the battery substrate in contact with the electrode is a transparent conductive oxide film, the adhesion between the first layer and the transparent conductive oxide film is greater than the adhesion between the second layer and the third layer and the transparent conductive oxide film, and the contact resistivity between the first layer and the transparent conductive oxide film is less than the contact resistivity between the second layer and the third layer and the transparent conductive oxide film; Alternatively, the surface of the battery substrate in contact with the electrode is a carrier transport layer, and the melting point of the first layer is greater than the melting points of the second layer and the third layer.

3. The solar cell according to claim 1, in, The projections of the first layer, the second layer and the third layer on the battery substrate overlap.

4. The solar cell according to claim 1, in, The thickness of the first layer is less than or equal to 10% of the thickness of the second layer; And / or, the thickness of the third layer is less than or equal to 10% of the thickness of the second layer.

5. The solar cell according to claim 1, in, The line width of the electrode at any position is 5 μm to 1500 μm, the thickness of the electrode at any position is 0.5 μm to 21 μm, and the ratio between the thickness and width of the electrode is 0.001 to 0.

2.

6. The solar cell according to claim 1, in, The electrode comprises a collector grid line; or, the electrode comprises an intersecting collector grid line and a bus grid line; Wherein, the line width of the collector grid line is 30 μm to 500 μm, and the line width of the bus grid line is 100 μm to 1500 μm.

7. The solar cell according to claim 1, in, The thickness of the first layer is 5nm to 300nm; and / or, the thickness of the second layer is 0.5 μm to 20 μm; And / or, the thickness of the third layer is 5nm to 300nm.

8. The solar cell according to claim 1, in, The material of the first layer includes one or more combinations of metal oxides, metal nitrides, metal fluorides, metal silicides and metals.

9. The solar cell according to claim 8, in, The metal oxides include AZO, TiO X , Cu 2 O、MgO x 、TaO x , VO x CrO x SnO 2 , B: ZnO and MoO x One or more combinations of; And / or, the metal nitride comprises TiN x and TiO x N y One or more combinations of; And / or, the metal fluoride comprises MgF 2 , LiF, YF 3 and CeF 3 One or more combinations of; And / or, the metal silicide comprises TiSi 2 、TaSi 2 、M O Si 2 、CoSi 2 、Ni 2 Si and WSi 2 One or more combinations of; And / or, the metal includes one or more combinations of Ni, Ti and Cr.

10. The solar cell according to claim 1, in, The material of the second layer includes one or more combinations of aluminum and copper.

11. The solar cell according to claim 1, in, The material of the third layer includes one or more combinations of nickel, silver, tin, aluminum-nickel alloy and aluminum-tin alloy.

12. The solar cell according to claim 1, in, The resistivity of the electrode is less than or equal to 3×10 -6 Ω·cm.

13. The solar cell according to claim 1, in, The total thickness of the electrode is less than or equal to 10% of the thickness of the battery substrate.

14. The solar cell according to claim 1, in, The electrode comprises a collector grid line, or the electrode comprises an intersecting collector grid line and a bus grid line; The line width of the collector grid lines is equal everywhere, and the line width of the bus grid lines is equal everywhere.

15. The solar cell according to claim 1, in, Along the width direction of the electrode, the middle thickness of the electrode is greater than the thickness of both sides of the electrode.

16. A method for preparing a solar cell, include: Providing a battery substrate and a flexible mask, wherein the battery substrate has two opposite surfaces; Fixing the flexible mask to at least one side of the battery substrate, wherein the flexible mask has a hollow pattern; Depositing a first layer, a second layer and a third layer in a stacked arrangement on the flexible mask in sequence, wherein the first layer deposited at the hollow pattern contacts the surface of the battery substrate; The flexible mask is removed so that the first layer, the second layer and the third layer deposited at the hollow pattern remain on the surface of the battery substrate to form the electrode; wherein the adhesion of the first layer to the surface of the battery substrate is greater than the adhesion of the second layer and the third layer to the surface of the battery substrate, and the contact resistivity of the first layer to the surface of the battery substrate is less than the contact resistivity of the second layer and the third layer to the surface of the battery substrate; or, the melting point of the first layer is greater than the melting points of the second layer and the third layer; the resistivity of the second layer is less than the resistivity of the first layer and the third layer; the melting point or surface tension of the third layer is less than the melting point or surface tension of the first layer and the second layer.

17. The preparation method according to claim 16, in, The first layer, the second layer and the third layer are sequentially deposited on the flexible mask by a physical vapor deposition method to form a stacked arrangement.

18. The preparation method according to claim 17, in, Depositing a first layer on the flexible mask by a magnetron sputtering method; and / or, depositing the second layer on the flexible mask by an evaporation method; And / or, the third layer is deposited on the flexible mask by a magnetron sputtering method or an evaporation method.

19. The preparation method according to claim 16, in, The side of the battery substrate on which the flexible mask is fixed has a dielectric layer. After the flexible mask is fixed to at least one surface of the battery substrate and before the first layer, the second layer and the third layer are sequentially deposited on the flexible mask to form a stacked arrangement, the preparation method further includes: The side of the battery substrate on which the flexible mask is fixed is etched to remove the battery The dielectric layer at the location of the pool substrate corresponding to the hollow pattern; The first layer deposited at the hollow pattern contacts the surface of the battery substrate, specifically: the first layer deposited at the hollow pattern contacts the surface of the battery substrate after the dielectric layer is removed.

20. The preparation method according to claim 16, in, The flexible mask is fixedly covered on the surface of the battery substrate by bonding or pressing.

21. The preparation method according to claim 16, in, The flexible mask comprises a polymer film layer and an adhesive film layer which are stacked, and the flexible mask is adhered and covered on the surface of the battery substrate through the adhesive film layer.

22. The preparation method according to claim 21, in, The material of the polymer film layer is one or more combinations of polyethylene terephthalate, polyolefin film, polyimide, and polyvinyl chloride; The material of the adhesive film layer is one or more combinations of silicone, acrylic glue, polyurethane, rubber, and polyisobutylene.

23. The preparation method according to claim 21, in, The removing the flexible mask comprises: Performing a viscosity reduction treatment on the flexible mask to reduce the peel strength of the flexible mask; The flexible mask is peeled off from the surface of the battery substrate.

24. The preparation method according to claim 23, in, The viscosity reduction treatment includes one or more combinations of cooling viscosity reduction treatment, heating viscosity reduction treatment, ultraviolet light irradiation viscosity reduction treatment, alternating magnetic field viscosity reduction treatment, and solvent immersion viscosity reduction treatment.

25. The preparation method according to claim 24, in, The viscosity reduction temperature in the cooling viscosity reduction treatment is 15° C. to 30° C., and the peel strength of the flexible mask after the viscosity reduction is 1 gf / cm to 50 gf / cm.

26. The preparation method according to claim 24, in, The viscosity reduction temperature in the heating viscosity reduction treatment is 60° C. to 180° C., and the peel strength of the flexible mask after the viscosity reduction is 1 gf / cm to 50 gf / cm.

Citation Information

Patent Citations

  • Electrode of flexible CIGS solar cell and manufacturing method

    CN111769165A

  • Crossed net-shaped electric contact back contact heterojunction battery and assembly manufacturing method

    CN111834470A

  • Solar cell

    CN219873549U

  • Photoelectric conversion element and imaging device

    US20170005126A1

  • Metal electrode of solar cell and preparation method therefor

    WO2022253281A1

Cited By

  • Semiconductor prefabricated member based on shadow mask process and prefabricated member preparation method

    CN119191224A

  • A semiconductor preform based on shadow mask process and a method for preparing the preform