Modified siloxanes, method for modifying siloxanes and their use
By heat-treating siloxane powders to modify their properties from siloxane-like to silica-like, the filler materials for optoelectronic devices address the gap in properties between existing fillers, enhancing the performance and reliability of PiMoS and PiM converters.
Patent Information
- Application Number
- PCT/EP2024/063598
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-18
- Filing Date
- 2024-05-16
- Publication Date
- 2024-11-21
AI Technical Summary
Current filler materials for optoelectronic devices, such as phosphor-in-matrix-on-substrate (PiMoS) and phosphor-in-matrix (PiM) wavelength converters, exhibit significant differences in physical properties between polymethylsiloxane and fused silica powders, creating a gap where fillers with intermediate properties are needed to optimize performance and reliability.
Modified siloxane powders are produced by subjecting siloxane to a heat treatment in an oxygen-containing environment at temperatures between 200°C to 500°C, altering their chemical composition and properties to span the range from siloxane-like to silica-like, thereby tuning their properties to match the requirements of PiMoS and PiM converters.
The modified siloxane fillers effectively reduce delamination at the PiM-substrate interface, enhance brightness, and optimize mechanical and thermal properties, filling the gap between siloxane and fused silica fillers, thus improving the performance and reliability of LED optoelectronic devices.
Smart Images

Figure IMGF000005_0001 
Figure IMGF000005_0002 
Figure IMGF000005_0003
Abstract
Description
[0001] 2022PF02477 - 1 - MODIFIED SILOXANES, METHOD FOR MODIFYING SILOXANES AND THEIR USE The present application claims priority of US application US 63 / 503,081 dated May 18, 2023, the content of which is incorporated herein by reference in its entirety. The present invention concerns modified siloxanes, a method for modifying siloxanes, use of the modified siloxanes as filler, a filler containing or consisting of said modified siloxanes and optoelectronic devices containing said fillers. BACKGROUND Filler materials are commonly added to various types of chemical formulations to alter properties (such as physical, optical, and / or mechanical properties) to optimize performance or robustness of the resulting component / product. In this case, the term filler material includes a wide range of solid materials that can take various physical forms such as powders, fibres, whiskers, platelets, and nano-materials. The chemical make-up of the filler material varies depending on the desired properties of the filler. In particular, filler materials can be used in optoelectronic devices that make use of phosphor-converted LEDs (Light Emitting Diodes) to generate light with a desired emission spectrum. A particular class of wavelength converter are phosphor-in-matrix-on-substrate (PiMoS) and phosphor-in matrix (PiM) wavelength converter. Fillers can be added to the matrix phase to optimize properties and performance of the optoelectronic device. At present, the most common fillers for PiMoS and PiM converter elements include fumed silica, fused silica powder (0.5-10µm particle size) and polymethylsiloxane powders (0.8-8µm particle size). While these materials are available as spherical powders with similar particle sizes, the material properties are very different. For example, the polymethylsilioxane powders (hybrid organic / inorganic structure) have similar chemistry and properties to the methyl polysiloxane matrix material of PiM layers, while silica powders are high temperature inorganic materials that have very low coefficient of thermal expansion (CTE). The significant difference in 2022PF02477 - 2 - physical properties between polymethysiloxane and fused silica powders leaves a large gap where fillers with intermediate properties would be beneficial to meet the demands of various end-use applications. This issue will be described in the following in more detail. The primary filler material for PiMoS wavelength converters is fused silica powder. Fused silica fillers are commonly made using a powder flame- spray process, where the powder typically has spherical shaped particles with a fairly-wide particle size distribution. The chemical purity of the material depends on the precursor material used in the process. A second class of silica filler is produced using high purity precursors and a sol-gel processing method. Silica powders can be made with spherical particles, narrow particles distribution and high chemical purity. These type of silica fillers are currently being evaluated in PiMoS wavelength converters. Siloxane (polymethylsiloxane) powder materials are currently being evaluated for use in PiMoS and PiM wavelength converters. While siloxane powders are used for various technical applications, they are widely used in the cosmetic industry; they are available from many vendors in a wide range of particle sizes and typically have narrow particle size distributions. Siloxane powders have very different material properties than fused silica. Properties such as lower storage modulus and similar properties to the methyl polysiloxane matrix component are advantageous, but siloxane powders have a high thermal expansion that can lead to problems with stress in PiMoS wavelength converters. It is an object of the present application to provide a substance as well as a method of preparing it and its use avoiding the drawbacks of the prior art. SUMMARY OF THE INVENTION 2022PF02477 - 3 - This and other objects are addressed by the subject matter of the independent claims. Features and further aspects of the proposed principles are outlined in the dependent claims. There is provided a modified siloxane obtainable by subjecting a siloxane to a heat treatment at a temperature of about 200 °C to about 500 °C in an oxygen-containing environment. Furthermore, there is provided a method for modifying a siloxane, wherein the siloxane is subjected to a heat treatment at a temperature of about 200 °C to about 500 °C in an oxygen-containing environment. The term “modifying” as used herein means that the chemical composition and / or the properties of the siloxane after the heat treatment in an oxygen-containing environment (modified siloxane) are different from the chemical composition and / or properties of the siloxane used as the starting material. Siloxanes are chemical compounds that comprise a backbone of alternating silicon-oxygen [Si-O] units with organic side groups attached to each silicon atom. In contrast to silanes, the silicon atoms are not linked to each other, but to their neighbouring silicon atom by exactly one oxygen atom: Si-O-Si. Siloxanes with organic side groups R = CH3are called polydimethylsiloxanes, which can be used according to the present invention. Oligomeric or polymeric organosiloxanes (siloxanes with R ≠ H) are called silicones. They have long Si-O main chains and are viscous or permanently elastic, depending on their molar mass and crosslinking. If they are liquid, they are also called silicone oils. The siloxanes used can be those siloxanes which are known to be used in filler materials in optoelectronic devices which for example make use of phosphor-converted LEDs (Light Emitting Diodes) to generate light with a desired emission spectrum, for example phosphor-in-matrix- on substrate (PiMoS) and phosphor-in-matrix (PiM). 2022PF02477 - 4 - In particular, siloxane powders used as the starting material in the present invention, in particular polymethylsiloxane, are based on CH3(SiO3 / 2) (T-units). Other polysiloxane materials that contain a combination of Q-unit, T-unit, D-unit and M-unit bonding and some combination of methyl and phenyl groups could be used. The general formula for the starting polysiloxane powder would be [RSiO3 / 2]x[R2SiO]y[R3SiO1 / 2]z, where R can be any combination of methyl and phenyl groups, and x, y, and z are the relative amounts of T-unit, D-unit, and M-unit siloxane bonding, respectively. In this case, x + y + z = 1, 0.5 ≤ x 1.0, 0 0.5, and 0 z < 0.1. It is pointed out that this general formula does not attempt to indicate the overall number of repeat units, just their relative proportions to one another. The modification of the polysiloxane powder obtained according to the present invention would result in a decrease in the T-unit, D-unit and / or M-unit content, while the Q-unit (SiO2) content increases. An Example where x=1 is: --[RSiO3 / 2]-- → --[RSiO3 / 2]A[SiO2]B-- where the ratio of A to B depends on the desired property. The present invention relates to a method for preparing modified siloxane powder fillers to tune the properties from siloxane-like to silica-like behaviour. The ability to tune the properties of the filler is for example suitable when working to balance (or optimize) the properties of PiMoS or PiM wavelength converters. The composite structure of the PiMoS or PiM converter is sensitive to any change in properties, where there is a fine balance required to achieve the desired properties. Modified siloxane-based fillers can be tuned to fill the large gap in properties between siloxane and fused silica fillers. The present invention provides a method to make filler materials that range in properties from siloxane-like to silica-like so that for example PiM and PiMoS converter properties can be optimized for performance and reliability. The structure and properties of siloxane powders can be modified with controlled thermal treatment (for example in air) of the powder at specified temperatures as indicated above to decrease the silanol (Si- OH) and CH3-group content of the material. Material properties can be 2022PF02477 - 5 - tuned from siloxane-like to silica-like, by using different thermal treatments, to optimize the performance of the end-use application. The ability to tune the properties of the filler is important when working to balance (or optimize) the properties of PiMoS or PiM wavelength converters. The composite structure of the PiMoS or PiM converter is sensitive to any change in properties, where there is a fine balance required to achieve the desired properties. For example, PiMoS formulation changes that shift the balance of stress in the converter can result in increased delamination at the PiM-substrate interface. In the case of PiM, camber (or strong curl) of the converter can result when the properties are not balanced. Therefore, having the ability to tune the properties of the filler material is beneficial to meeting the final requirements of the converter. Advantageously, the siloxane powders have a high purity and are low-cost precursor materials for fabrication of heat-treated modified siloxane fillers. A basic thermal process is used to modified siloxane fillers once the appropriate thermal profile has been identified. A range of siloxane- based filler properties (tuneable properties) can be achieved by altering the thermal profile. To make it more specific, the primary advantage of this invention is the ability to tune properties of the siloxane-based filler material to meet the specifications of the end-product, which in this case is a wavelength converter for LED optoelectronic devices. PiMoS wavelength converters have a complex, composite structure that requires a fine- tuned balance / optimization of properties. A tunable filler is advantageous in striking a balance in the overall properties, performance, and reliability of the LED optoelectronic device. The siloxane powder precursor material is a high purity material that is readily available as spherical particles in the 0.8 to 15 µm range, with narrow particles size distributions. These siloxane powders are commercially available wherein the vendor indicates the particle size. 2022PF02477 - 6 - As pointed out above, the siloxanes are subjected to a heat treatment at a temperature of about 200 °C to about 500 °C, for example about 200 °C to about 425 °C, like about 370 °C to about 410 °C. The heating can be achieved in any apparatus suitable for adjusting these temperatures. For example, the apparatus can be a usual furnace. The heat treatment is carried out in that the siloxane used as the starting material is maintained at the desired temperature as outlined above. According to the present invention, it is possible that the heat treatment is carried out at one temperature or alternatively at at least two different temperatures, for example 2, 3, 4 or 5 different temperatures, each lying within the temperature range of about 200 °C to about 500 °C. That is, the siloxane can be maintained at a first temperature for a certain time and then at a second and optionally further temperatures for further periods of time, wherein the temperatures are different from each other and each of the temperature is lying within the temperature range of about 200 °C to about 500 °C. According to the method of the present invention, in order to reach the desired temperature for the heat treatment, the temperature can be increased from ambient temperature, for example room temperature, or at least a temperature lower than the temperature of the heat treatment, in a thermal ramp rate of about 1.0°C / min. to about 20°C / min., for example about 2 °C / min. to about 5°C / min., like about 2°C / min. The heat treatment can be carried out for about 0.5 hour to about 24 hours, for example about 2 hours to about 8 hours, like about 6 hours for achieving the heat treatment. The term “oxygen-containing environment” used according to the present invention means that the siloxane used as the starting material is surrounded by a gas / gaseous mixture at least containing oxygen. Such gas / gaseous mixture containing oxygen can be the mixture of oxygen with other gases, for example inert gases, like nitrogen and / or argon. The oxygen-containing environment can contain about 5 vol.-% to about 30 vol.-% oxygen. For example, the oxygen-containing environment is air. 2022PF02477 - 7 - This excludes that the siloxane to be modified is present in a solid matrix. Siloxane (polymethysiloxane) fillers have the chemical composition of CH3(SiO3 / 2), while silica fillers have the chemical composition of SiO2. Heating siloxanes to temperatures of about 200°C to about 500°C results in decreasing the silanol (Si-OH) content by forming Si-O-Si bonds (i.e., condensation reactions), thus changing the properties of the filler. There is also a small temperature window (about 370°C -about 410°C) where the CH3-groups in the structure can be selectively decomposed to further alter the properties of the material, where the properties can be tuned from siloxane-like to silica-like. A variety of modified siloxane fillers can be made by using slightly different thermal treatments, thus producing fillers with a range of properties that fill the gap between siloxane and fused silica fillers. For example, modified siloxane filler (with silica-like properties) according to the present invention was substituted for siloxane filler for a PiMoS converter. The delamination at the PiM-substrate interface decreased from 14% to 2.2% following a slow thermal ramp 200 °C cure. In addition, the PiMoS converter platelets showed increased brightness vs. use of the fused silica filler (made with powder flame-spray process). Tuning the properties of the filler resulted in optimizing the properties of the PiMoS converter. In a further aspect, the present invention relates to the use of the modified siloxane according to the present invention or the modified siloxane obtained by the method according to the present invention as a filler, for example as a filler employed in a wavelength converter, wherein the wavelength converter for example can be a phosphor-in- matrix wavelength converter or a phosphor-in-matrix-on-substrate wavelength converter. Such converters are known to the person skilled in the art so that the skilled person knowns how to use the fillers of the present invention in a matrix of such converters. Furthermore, according to the present invention there is provided a filler containing or consisting of the modified siloxane according to 2022PF02477 - 8 - the present invention and / or the modified siloxane obtainable by the method according to the present invention. The filler can have the form of spherical powders with various particle sizes. The filler can have an average size of about 0.8µm to about 10µm, for example about 0.8µm to about 8µm. The average particle size mentioned in the present application means the d50 value. The siloxanes are commercially available and the particle sizes have been indicated by the vendors. According to the present invention, there is also provided an LED optoelectronic device component having a matrix containing a filler, wherein the filler comprises or consist of the modified siloxane according to the present invention and / or the modified siloxane obtained by the method according to the present invention. Examples of such LED optoelectronic device components are phosphor-in-matrix-on- substrate and phosphor-in-matrix wavelength converters. In the following, the components of wavelength converters for phosphor- converted LED optoelectronic devices are exemplified: Matrix Material: The matrix material can be a polysiloxane. The polysiloxane can be a methyl polysiloxane with exclusively T-unit bonding. Alternative embodiments would allow for some combination of T-unit, D-unit, and M- unit bonding and some combination of methyl and phenyl groups. The general formula for the cured polysiloxane would be [RSiO3 / 2]x[R2SiO]y[R3SiO1 / 2]z, where R could be any combination of methyl and phenyl groups, and x, y, and z are the relative amounts of T-unit, D-unit, and M-unit siloxane bonding, respectively. In this case, x + y + z = 1, and 0.5 z < 0.1. The matrix material could also be a type of glass. There should be no carbon-carbon bonds in the polymer chain. That is, the crosslinking throughout the entire matrix should be made from silicon-oxygen bonds. In the case where R = phenyl, there will be carbon-carbon bonds in the phenyl groups, but those groups are not part of the crosslinked network. Instead, they are merely side groups. This lack of carbon-carbon bonds in the main polymer chain differentiates 2022PF02477 - 9 - this invention from any invention that uses silicones (or siloxanes) that are based on addition curing, i.e., systems that crosslink via a Si-H group on one material and vinyl group on another. Examples of the Phosphors: ^ (RE1-xCex)3(Al1-yA´y)5O12 0.1 ^ (RE1-xCex)3(Al5-2yMgySiy)O12 0.1 ^ (RE1-xCex)3Al5-ySiyO12-yNy 0.1 0.5, ^ (RE1-xCex)2CaMg2Si3O12 0.1, ^ (AE1-xEux)2Si5N8with 0 < x ≤ 0.1, ^ (AE1-xEux)AlSiN3with 0 < x ≤ 0.1, ^ (AE1-xEux)2Al2Si2N6with 0 < x ≤ 0.1, ^ (Sr1-xEux)LiAl3N4with 0 < x ≤ 0.1, ^ (AE1-xEux)3Ga3N5with 0 < x ≤ 0.1, ^ (AE1-xEux)Si2O2N2with 0 < x ≤ 0.1, ^ (AExEuy)Si12-2x-3yAl2x+3yOyN16-ywith 0.2 2.2 0.1, ^ (AE1-xEux)2SiO4with 0 < x ≤ 0.1, ^ (AE1-xEux)3Si2O5with 0 < x ≤ 0.1, ^ K2(Si1-x-yTiyMnx)F6 0.2 ^ (AE1-xEux)5(PO4)3Cl with 0 < x ≤ 0.2, ^ (AE1-xEux)Al10O17with 0 < x ≤ 0.2, ^ wherein RE is one or more of Y, Lu, Tb and Gd, AE is one or more of Mg, Ca, Sr, Ba, A´ is one or more of Sc and Ga. Other options are Europium(II)-doped β-SiAlON, Cr3+, Ni2+, Co2+, Cu2+, or other optically active dopants used in luminescent materials. The above list is for example only, and not meant to be exclusive. In fact, any material that absorbs in the wavelength range of ~360 nm to ~500 nm and emits in the visible and / or near-IR region of the spectrum can be used. This includes classes of materials beyond traditional phosphor powders, e.g., quantum dots could also be used if the surface chemistry was compatible with the matrix. Optional Fillers: 2022PF02477 - 10 - Fumed silica could be present in the phosphor-in-matrix layer in the range of 0vol.-% to 15vol-.%. The fumed silica would be preferably of hydrophobic type and have surface area greater than 175m2 / g. Fused silica could be present in the phosphor-in-matrix layer in the range of 0vol.-% to 35vol.-%. The fused silica particle diameter would be in the range of 0.1 μm to 15 μm. The fused silica should be spherical- like in shape. The particles could be porous or non-porous. Polysilsesquioxane particles could be present in the phosphor-in-matrix layer in the range of 0vol.-% to 35vol.-%. The polysilsesquioxane particles can be spherical-like in shape and be in the size range of 0.1μm to 10μm. Filler material should not be limited to the above examples. It could be sapphire spheres, ZnO, TiO2, etc. or materials transparent in the UV / visible / IR wavelengths. Substrate: The substrate can be glass. The type of glass can be borosilicate, but other types of glass could be used, such as aluminosilicate or others. The substrate can also be fused silica. The substrate can be sapphire, quartz, or any other transparent crystalline or polycrystalline material. The surface of the substrate, opposite the phosphor-in-matrix layer, could be modified to change the way light propagates through the converter. For example, an anti-reflective coating can be applied to the exit surface of the substrate. A dielectric stack can be coated on the exit surface of the substrate to modify the transmittance of the light as a function of wavelength and / or angle. The exit surface of the substrate can be roughened to change the light extraction behavior. A micro-lens array, meta-lens, or photonic crystal can be made on the exit surface of the substrate to alter the light propagation according to the needs of a given application. Dimensions: 2022PF02477 - 11 - The converter could be made to the size needed for a given application. SHORT DESCRIPTION OF THE DRAWINGS Further aspects and embodiments in accordance with the proposed principle will become apparent in relation to the various embodiments and examples described in detail in connection with the accompanying drawings in which Figure 1 shows schematically a phosphor-in-matrix-on-substrate (PiMoS) wavelength converter. Figure 2 shows an overview of polymethysiloxane (siloxane) filler and fused silica filler properties with respect to PiM formulations; a large gap in properties exists between these two filler materials. Figure 3 illustrates schematically a polymethylsiloxane (siloxane) particle based on CH3(SiO3 / 2) chemistry, containing T-units in a 3- dimentional structure; the T-unit content in the structure may vary for various commercially available products. Figure 4 shows a TGA plot of weight loss of siloxane powders as a function of temperature; TGA evaluation at 10°C / min to 600°C in air. Figure 5 shows a TGA evaluation of the heat-treated 4µm siloxane powders to determine the weight loss of the powder as a function of temperature, i.e., how much silanol and CH3is left in the structure following thermal treatment of the powder. TGA evaluation at 10°C / min to 600°C in air. Figure 6 shows SEM images of original siloxane powders and heat-treated modified siloxane powders (5,000x magnification for all powders). Figure 7 shows the % reflectance as a function of wavelength for various siloxane powder fillers (powder plaque measurements with a spectrophotometer). 2022PF02477 - 12 - Figures 8a and b show heat-treated siloxane powders: (a) high processing temperatures and limited air flow resulted in carbon trapped in the structure, as indicated by the grey powder, and (b) optimized processing temperatures and improved air flow resulted in a high purity modified siloxane powder. Figure 9 shows a % reflectance comparison for the original 4µm siloxane powder vs. modified 4µm-HT400. Figure 10 shows methyl polysiloxane-based matrix samples containing various filler types: siloxane, modified siloxane, and fused silica powder. Figure 11 shows % transmittance spectra for matrix samples containing various filler types: siloxane, modified siloxane, and powders (samples were 0.34-0.35mm thick). Figures 12a, b and c show % transmittance curves for matrix samples containing various filler types: (a) siloxane, (b) modified siloxane and (c) silica powder, subjected to thermal storage at 250°C for 24 hours. Figures 13a and b show mechanical properties (3-point bend test) for matrix samples containing various filler types: siloxane, modified siloxane, and silica powder, (a) Breaking Force and (b) Youngs Modulus. Figure 14a and b show an overview for two different thermally modified siloxane fillers: (a) 4µm-HT360 is siloxane-like with improved thermal stability, and (b) 4µm-HT410 is silica-like with lower CTE, higher breaking force and some scattering. The 4µm-HT360 modified siloxane powder is not moisture sensitive and has a good thermal stability (>400°C); the CH3content is still the same as the starting siloxane powder. The thermal stability of the material has been significantly improved without losing the benefits of having an organic / inorganic hybrid structure. Properties will be siloxane-like but without a weight loss until >400°C. The 4µm-HT410 modified siloxane powder is most likely porous with a moisture sensitivity. The powder has a good thermal 2022PF02477 - 13 - stability (500°C) and only little if any CH3groups left. The thermal stability of the material has been significantly improved and the properties will be silica-like. A low CTE of the material can help decrease stress when blended with Methyl Polysiloxane. Figure 15 shows an overview of polymethysiloxane (siloxane) and fused silica filler properties with respect to PiM formulations; modified siloxane fillers can be prepared with a range of properties that falls between these filler materials to optimize wavelength converters for LED optoelectronic device performance and robustness. For Polymethylsiloxane powder, the CH3content may vary. It is available in a wide range of sizes, with high purity available. The Fused Silica powder contains SiO2with high purity available, a low CTE, blending with LRI (low refractive index) liquid Siloxanes and high temperature stability. The modified Siloxane powder according to the present invention combines the benefits and advantages of both with additional a variable CTE, variable scattering in LRI liquid siloxanes, high thermal stability (>400°C) and variable mechanical properties. Figure 16 shows % reflectance as a function of wavelength for siloxane and modified siloxane powder plaque measurements. Figures 17a and 17b show a Trial 1 delamination at the PiM-glass interface was evaluated using an optical microscope with coaxial lighting, where the light-colored regions indicate delamination: (a) shows about 21% delamination for PiMoS converters cured at 200°C, while (b) shows about 14% delamination for PiMoS converters cured at 200°C using a slow thermal ramp rate. Figures 18a and 18b show a Trial 2 delamination at the PiM-glass interface was evaluated using an optical microscope with coaxial lighting, where the light-colored regions indicate delamination: (a) shows about 6.5% delamination for PiMoS converters cured at 200°C, while (b) shows about 2.2% delamination for PiMoS converters cured at 200°C using a slow thermal ramp rate, which helped to reduce stress. 2022PF02477 - 14 - Figure 19 shows probability plots of surface roughness measurements for Trial 2 PiMoS 1” x 1” coupon; Sa, Sp, Sv and Sz are specified. Figure 20a and 20b show SEM images of Trial 2 PiMoS surface at 3,000x magnification to evaluate surface features: (a) electron backscatter mode, and (b) topography mode. Figures 21a and 21b show photometry data for Trial 2 PiMoS converter platelets, with comparison to the control PiMoS converter platelets: (a) color coordinate comparison, and (b) conversion efficiency comparison. Figures 22a and 22b show delamination as a function of thermal storage at 250°C storage (1,188 hours) for Trial 2 PiMoS converter platelets: (a) Trial 2 cured with standard 200°C profile, and (b) Trial 2 cured with slow thermal ramp rate 200°C profile. Inserted photos show delamination measurements of platelets, where the light-colored regions indicate delamination at the PiM-glass interface. Figures 23a and 23b show color coordinate (Cx) thermal stability at 250°C storage (1,188 hours) for Trial 2 PiMoS converter platelets: (a) Trial 2 cured with 200°C profile, and (b) Trial 2 cured with slow thermal ramp rate 200°C profile. DETAILED DESCRIPTION The following embodiments and examples disclose various aspects and their combinations according to the proposed principle. The embodiments and examples are not always to scale. Likewise, different elements can be displayed enlarged or reduced in size to emphasize individual aspects. It goes without saying that the individual aspects of the embodiments and examples shown in the figures can be combined with each other without further ado, without this contradicting the principle according to the invention. Some aspects show a regular structure or form. It should be noted that in practice slight differences and deviations from the ideal form may occur without, however, contradicting the inventive idea. 2022PF02477 - 15 - In addition, the individual figures and aspects are not necessarily shown in the correct size, nor do the proportions between individual elements have to be essentially correct. Some aspects are highlighted by showing them enlarged. However, terms such as "above", “over”, "below", "under" "larger", "smaller" and the like are correctly represented with regard to the elements in the figures. So, it is possible to deduce such relations between the elements based on the figures. In the tables and figures heat treatment sample identifications use abbreviations. For example, HT360 means heat treated (HT) at 360°C. Particle sizes mentioned throughout the present application that are stated for the siloxane and silica powders were provided from the vendors; the particle size is the d50 value. Siloxane particles in the range of 0.8µm to 15µm (d50 values from vendor) as starting material. SEM evaluation of powders was done at ams-OSRAM to compare the starting Siloxane powder vs. the modified Siloxane powder with regard to general particle size, particle distribution and whether or not significant fusing / agglomeration of the particles occurred during the thermal treatment. Filler materials are commonly added to various types of chemical formulations to alter properties (such as physical, optical, and / or mechanical), to optimize performance or robustness of the resulting component / product. In this case, the term “filler” material includes a wide range of solid materials that can take various physical forms such as powders, fibers, whiskers, platelets, and / or nano-materials. The chemical make-up of the filler material varies depending on the desired properties of the material. Filler materials can be used in optoelectronic devices that make use of phosphor-converted LEDs (Light Emitting Diodes) to generate light with a desired emission spectrum. The main purpose of the phosphor component of such a device is to convert light of one wavelength range to another wavelength range, typically from higher energy to lower energy, e.g., blue to green. These wavelength converters can come in 2022PF02477 - 16 - many different forms. This invention addresses optimized performance of a particular class of wavelength converter: phosphor-in-matrix-on- substrate (PiMoS) and phosphor-in-matrix (PIM). Fillers can be added to the matrix phase of the wavelength converter to optimize properties and performance of the LED optoelectronic device. A schematic of a PiMoS wavelength converter is shown in Figure 1, where the PiM layer is attached (bonded) to a substrate. PiM wavelength converters are stand-alone converters where there is no substrate. Figure 1 shows schematically a PiMoS wavelength converter. Typically, the substrate is some type of glass, and the matrix is some type of polymer, or polymer blend. Other substrate materials could be used, e.g., sapphire, and other matrix materials could be used, e.g., low melting glass. There are many combinations of substrate, phosphor, and matrix materials that could be used. The PiMoS is a complex composite structure that relies on a balance of properties to meet performance and reliability requirements. Modifying the matrix phase is one way to optimize the PiMoS converter performance. This invention focuses on modification of the matrix phase using solid filler additions, where the primary component of the matrix is a polysiloxane, and the polysiloxane can be a methy polysiloxane. Filler materials can be added to the matrix formulation to tune the properties for optimum performance of the phosphor-converted LED. Fillers can be added to the matrix phase to: ^ alter the rheology of the PiM slurry, ^ increase solids loading to decrease the shrinkage of the liquid methyl polysiloxane during the curing process, thus decreasing stress in the PiMoS, ^ modify matrix properties such as storage modulus, thermal expansion coefficient, optical scattering, thermal stability, and robustness / reliability, ^ decrease the surface roughness of the top surface of PiMoS or PiM, ^ decrease cracking in the PiM layer of the PiMoS or PiM, ^ decrease delamination at the PiM and substrate interface. 2022PF02477 - 17 - In the case of phosphor-converted LEDs the choice of filler materials for the matrix phase is limited to materials with select properties such as: ^ high purity, ^ low absorbance in the visible wavelength region, ^ thermal stability at minimum of 200°C, and in particular thermal stability at 250°C for extended times (e.g., 1,000 hours), ^ variable particle sizes in particular in the range of 10s of nanometers to 15µm, ^ narrow size particle range desired, ^ and readily available in large quantities and low cost desired. Optoelectronic devices, that make use of phosphor-converted LEDs, can have different end-use applications where construction of the PiMoS has different materials (e.g., different phosphors or phosphor loading) and construction parameters (e.g., PiM and substrate layer thicknesses). For this reason, there is need for a variety of filler materials to be able to tune the PiMoS properties for different end- use applications. At present, the most common fillers for PiMoS and PiM converter elements include fumed silica, fused silica powder (0.5-10µm particle size) and polymethylsiloxane powders (0.8- 10µm particle size). Fumed silica is often used to adjust the rheology of the matrix. Additional fillers are used to modify the properties of the PiM layer to produce a stable PiMoS, or flat, crack-free PiM converters. Figure 2 provides an overview of the properties and uses of polymethylsiloxane and fused silica fillers in PiM formations. While both of these materials are available as spherical powders with similar particle sizes, the material properties are very different. For example, the polymethylsilioxane powders (hybrid organic / inorganic structure) have similar chemistry and properties to the methy polysiloxane matrix material, while silica powders are high temperature inorganic materials that have very low thermal expansion coefficient. The large difference in physical properties between polymethysiloxane and fused silica powders leave a large gap where fillers with intermediate properties would be beneficial to meet the demands of various end-use 2022PF02477 - 18 - applications. In the following text polymethylsiloxane powders will be referred to as siloxane powders and can be used interchangeably. This invention describes a method for preparing modified siloxane powder fillers to tune the properties from siloxane-like to silica- like powders, thus spanning the gap shown in Figure 2. The siloxane structure is a hybrid, organic / inorganic material that is based on a 3-dimension structure that contains T-units (CH3-groups), as shown in Figure 3; the actual number of T-units may be different for various commercially available siloxane powder products. The structure and properties of siloxane powders can be modified with controlled thermal treatment (for example in air) of the powder at specified temperatures to decrease the silanol (Si-OH) and CH3-group content of the material. Figure 4 shows TGA (thermogravimetric analysis) measurements for weight loss of siloxane powders (0.8-6µm size particles) as a function of temperature. While there are slight differences in the TGA curves between the various particle size siloxane powders, there are three distinct temperature regions of weight loss: ^ RT-200°C: weight loss due to moisture (OH surface groups), ^ 200-400°C: weight loss due to condensation reactions in the siloxane structure (i.e., decrease in silanol (Si-OH) content and formation of Si-O-Si bonds), ^ 400-600°C: weight loss due to decomposition of CH3-groups in the structure. These TGA data indicate that a small temperature window exists where CH3-groups can be selectively decomposed to alter the properties of the material, where the properties can be tuned from siloxane-like to silica-like. Thermal treatment of 4µm siloxane powder was conducted at different temperatures to produce filler materials with a range of CH3-grous (T- groups); as CH3-groups decompose from the structure the properties of the powder become more silica-like. Thermal treatment (i.e., modification) of siloxane powder was conducted using the following procedure. 2022PF02477 - 19 - ^ Siloxane powder was placed in a furnace with air atmosphere; air is required for a clean burn-out of CH3-groups. ^ Slow thermal ramp rate (about 2°C / min) to the target temperatures: 360°C, 370°C, 390°C, and 410°C. ^ Hold at target temperature for 6 hours to allow reactions to stabilize. ^ Slow cool with furnace. ^ In one case, the powder was heated to 410°C (hold 4 hours), followed by a slow thermal ramp to 500°C (hold 2 hours). ^ Run TGA on the modified siloxane powder to evaluate the amount of silanol and CH3-groups remaining in the material; these data provide a relative measure of the amount of silanol and CH3-groups that were removed during thermal treatment of the siloxane powder. Figure 5 shows TGA evaluation of heat-treated siloxane powders to determine the weight loss of each powder as a function of temperature, i.e., how much silanol and CH3is left in the structure following thermal treatment of the powder. Weight loss values are calculated for three distinct temperature regions (discussed previously). Comparisons are made with the original 4µm siloxane powder to estimate the amount of silanol (Si-OH) and CH3-groups remaining in the powder. Table 1 provides a summary of the TGA weight loss and comments for each powder, for the 3 temperature regions.
[0002] 2022PF02477 - 20 - 4µm Siloxane Powder % Weight Loss Summary: TGA runs of Modified 4µmSiloxane Powder RT-200C: Loss due to moisture during the TGA run 200-400C: loss due to condensation reactions during the TGA run 400-600C: loss due to CH3 decomposition during the TGA run Modified 4µm Siloxane PowdersRT-200°C 200-400°C 400-600°CComments • starting material has very little moisture 4µm Siloxane Powder 0.23% 1.77% 9.34% • some condensation reactions in structure • starting material has 9.3wt% CH • very low moisture powder HT3606hr 0.06% 0 9.34%• condensation reactions have been completed• no CH3 decomposition at this temperature • Some moisture content (particles may have some porosity) HT370 6hr* 1.78 0.18% 4.34% • condensation reactions have been completed • 5wt% decomposition of CH3 (53.5wt% CH3 loss) • Some moisture content (particles may have some porosity) HT3906hr 1.74% 0.03 1.34% • condensation reactions have been completed • 8wt% decomposition of CH3 (85.7wt% CH3 loss) • Some moisture content (particles may have some porosity) HT410 for 6h* 1.46% 0.17% 1.16% • condensation reactions have been completed • 8.18wt% decomposition of CH3 (87.6wt% CH3 loss) • Some moisture content (particles may have some porosity) HT4106h_500C for 2hr 1.44% 0.13% 0.22% • condensation reactions have been completed •9.12wt% decomposition of CH3(97.6wt% CH3loss)* Sample sat out in atomosphere for days then it was dried at 120C prior to measurement Table 1. Summary of TGA weight loss for heat-treated 4µm siloxane powders for 3 distinct temperature regions; comments added to indicate the structural changes in the modified siloxane filler material. The data provided in Table 1 shows that a temperature range exists such that the siloxane powders can be changed from siloxane-like to silica- like powder. The ability to tune the properties of the powder is important when working to balance (or optimize) the properties of PiMoS or PiM wavelength converters. The composite structure of the PiMoS or PiM converter is sensitive to any change in properties, where there is a fine balance required to achieve the desired properties. For example, PiMoS formulation changes that shift the balance of stress in the converter can result in increased delamination at the PiM-substrate interface. In the case of PiM, camber (or strong curl) of the converter can result when the properties are not balanced. Therefore, having the ability to tune the properties of the filler material is beneficial to meeting the final requirements of the converter. Based on the data summarized in Table 1 it is clear that siloxane-based filler materials can be made that have properties ranging from siloxane-like to silica- like, thus the ability to tune filler properties. 2022PF02477 - 21 - A variety of siloxane powders were subjected to thermal treatment for use in methyl polysiloxane matrix formulations. While the treatment temperatures result in decreasing the CH3content of the material, the temperatures were not high enough to result in significant densification, or fusing, of the particles; i.e., the particles have porosity. Figure 6 shows SEM evaluation of the original and heat- treated powders for 0.8µm, 2µm and 4µm siloxane powders. The siloxane powders shown in Figure 6 have a spherical shape with narrow particle size distribution (PSD). Thermal treatment of the powders shown in Figure 6 ranged from 390°C to 500°C, with significant CH3loss for all powders. Comparison of SEM images indicate that there was minimal change in the particle size / shape and nominal particle fusing was observed. In the case of the original 4µm powder, and heat- treated 4µ-HT400 and 4µm-HT500 powders there are some fused particles in both the original and the heat-treated powders. The original siloxane powders are high purity and show very high reflectance values (powder plaque measurement with a spectrophotometer), as shown in Figure 7. High purity, low absorption filler materials are essential to maximizing the brightness of phosphor-converted LEDs. Thermal treatment of the siloxane powders requires processing parameters such that the CH3-groups decompose, but carbon does not get trapped in the structure. Residual carbon in the structure results in strong absorption in the visible spectrum. Figures 8a and b show samples of heat-treated siloxane powders with different thermal processing conditions. If the heating ramp rate and / or the hold temperature is too high, or the air supply is insufficient then carbon can be trapped in the structure and the material may have a black to grey appearance (as shown in Figure 8a). Fine tuning the thermal treatment of siloxane powders results in high purity (low carbon) powder, as shown in Figure 8b. Reflectance measurements of the heat-treated siloxane powders can be used to identify low-level carbon contamination. Figure 9 shows 2022PF02477 - 22 - reflectance measurements for original vs. modified 4µm siloxane powder. Figure 9 confirms that there was no carbon trapped in the structure for the modified 4µm-HT400 powder, where the reflectance spectra lie on top of each other. Data in Figure 9 shows that CH3-groups can be burned-out cleanly, with no apparent carbon left in the structure. Modified siloxane powders, with tunable properties, can be included as candidates for high purity filler materials for PiM formulations. Modified siloxane powders can be made from thermal treatment of siloxane powders; siloxane powders from vendor A are a high purity, low cost material that is available in many particle sizes. Modified siloxane powder properties and % reflectance values look promising for use as filler in PiM formulations. Matrix formulations were prepared with various fillers to evaluate potential advantages of using modified siloxane fillers; the general matrix formulation is shown in Table 2a, while the fillers are provided in Table 2b. High purity fillers include siloxane powders, modified siloxane powders and fused silica powders; a blend of 1, or 0.8 µm, and 4µm particle sizes were used for each filler type. Samples were prepared using the following procedure: ^ matrix components were blended with planetary mixing and 3-roll milling of the slurry (no solvent), ^ Dr. Blade cast on mylar using a blade gap sufficient for a dried film thickness of approximately 0.35 mm, ^ room temperature cure at about 50% RH for 4 days, ^ samples cut and trimmed, ^ 200°C cure. Fillers Blend Component Formulation Siloxane 0.8 and 4µm blend Methyl Siloxane 58.2v% 0.8 and 4µm blend Modified Siloxane Fumed Silica 11.5v%0.8µm- HT3904µm- HT400Filler Material 30.3v% Silica 1 and 4µm blend (a) (b) Table 2a and b. General matrix formulation shown in (a), and various filler blends are provided in (b). 2022PF02477 - 23 - Figure 10 provides a visual comparison of cured matrix samples (about 0.35mm thick). The siloxane filler matrix sample is colorless and transparent; this is expected because the siloxane filler has essentially the same chemistry and refractive index as the methyl polysiloxane. The modified siloxane filler sample shows a hazy appearance, while the fused silica filler sample had a cloudy appearance. Transmittance measurements, shown in Figure 11, help to quantify the differences in these samples. Figure 11 shows distinct differences between the matrix samples, with % transmittance decreasing across the visible spectrum as the filler material goes from siloxane to silica; the modified siloxane filler falls in-between. All filler powders show high reflectance for powder plaque measurements, so material absorption losses should be low. Therefore, these data indicate that there is an increase in scattering in the methyl siloxane-based matrix as the filler goes form siloxane to silica powder. Optical scattering is a property that is sometimes desired, and other times not desired, in matrix properties for wavelength converters; the ability to tune this property could be beneficial for optimizing component properties. For some of the modified siloxane and silica fillers, an increase in % transmission with decreasing wavelength was observed for wavelengths below 400nm. This behavior can be attributed to fluorescence in the material during the measurement (spectrophotometer with single monochromator). Thermal stability of the matrix phase is very important to ensure robustness of wavelength converter properties. Matrix samples were subjected to thermal storage at 250°C for 24 hours, with the % transmittance curves shown in Figures 12a, b and c. Table 3 summarizes the transmittance data at 450nm wavelength. The matrix containing siloxane filler showed a small shift in the transmittance curve, but overall, there was very good thermal stability at 250°C. The modified siloxane and silica fillers, however, showed a significant shift in the curve to lower transmittance values, indicating a further increase in scattering. Once again, these matrix formulations show a range of 2022PF02477 - 24 - behavior, with the modified siloxane filler filling the gap between siloxane and silica filler properties. Storage time at 250°C FillerMatrix0.34-0.35mm 0 hours 24 hours Siloxane %T at 450µm94.6 93.4Modified Siloxane%T at 450µm 90.5 81.7Silica %T at 450µm 78.2 68.6 Table 3. % Transmittance data at 450nm for matrix samples containing various filler types; siloxane, modified siloxane, and silica powder (samples were 0.34-0.35 mm thick). Filler materials have an impact on the mechanical properties of wavelength converters. The ability to tune the properties of the filler is advantageous in balancing the properties of the converters. Figures 13a and b show the range of breaking force and Youngs modulus for matrix samples prepared with various fillers (see Table 2a and b). Siloxane filler additions result in the lowest values, while silica filler additions show the highest values for both breaking force and Youngs modulus. Modified siloxane fillers can be made to have intermediate mechanical properties, thus providing a lot of flexibility in tuning the properties of the wavelength converter. Figures 14a and 14b profile two different modified siloxane powders: (a) shows siloxane-like properties, while (b) displays silica-like properties. Modified siloxane powders can be prepared to fill the gap between these examples to tune the properties of PiMoS and PiM wavelength converters. The 4µm-HT360 (siloxane-like) powder extends the thermal stability of the material to temperatures of about 400°C, while keeping the CH3content the same (see Table 1), while 4µ-HT410 (silica-like) powder has very little (if any) CH3content left in the structure resulting in improved thermal stability and decreased thermal expansion coefficient (CTE). Finally, Figure 15 provides an updated view of Figure 1, where modified siloxane powders can be prepared with tunable properties from siloxane- 2022PF02477 - 25 - like to silica-like and can be used to optimize optoelectronic devices that use phosphor-converted LEDs. Example: Phosphor wavelength converters with modified siloxane according to the present invention. The properties of PiMoS wavelength converters for use in automotive headlamp optoelectronic devices are sensitive to the absorption / scattering properties of filler materials in the PiM layer. In particular, the chemical purity of the filler material and the filler content in the PiM layer can impact the brightness of the wavelength converter, where increased impurity and increased filler content can result in decreased brightness. The chemical purity of fused silica filler made by the flame-spray process depends on the precursor material and can vary for different sources. Studies are ongoing to evaluate new silica filler sources and new filler materials to increase brightness, while maintaining other converter properties such as low delamination and excellent thermal stability. Filler Materials: The search for new filler materials has stressed the need for high purity (high reflectance) materials. Reflectance measurements have been used to screen candidates for evaluation, with a flame-sprayed fused silica filler used as the benchmark to surpass. Figure 16 shows the reflectance spectra for siloxane and modified siloxane powder fillers compared to the flame-sprayed fused silica filler. The siloxane and modified siloxane powders show excellent reflectance and move forward for evaluation in wavelength converter formulations. The PiM formulation and fillers used for evaluation are shown in Tables 4a and b. The base matrix formulation is similar to an automotive white headlamp PiMoS matrix formulation. New fillers were evaluated as a direct volume percent substitution for the fused silica filler. 2022PF02477 - 26 - Component Formulation Methyl Siloxane 38v% Fumed Silica 12v% Trial # Fillers Blend Filler Material 15v% 1 Siloxane 4 and 6µm blend Total Phosphor 35v% 2 Modified Siloxane 4µm- HT410 (a) (b) Tables 4a and b. The matrix formulation for the filler study is shown in (a), and two filler blends are provided in (b). Wavelength Converter Evaluation (PiMoS): The phosphor-containing slurry is made by combining the polymer precursor, phosphor powder(s), and filler materials using standard batching, mixing, and milling techniques. The polymer precursor can be a low molecular weight methyl methoxy siloxane. The siloxane bonding would be primarily T-unit bonding, meaning that each silicon atom in the siloxane is connected to three oxygen atoms and one carbon atom. T-unit bonding is important for two reasons: (i) T-unit siloxanes often cure into harder materials than traditional D-unit types, and (ii) T- unit siloxanes, like the ones claimed here, do not have any carbon- carbon bonds in the polymer chain. The benefit of these two features is that the harder siloxanes can be saw diced without smudging or tearing and the lack of any C-C bonds means the cured polysiloxane is more thermally stable than a typical silicone. The phosphor powder(s) could be any of the known LED phosphors. For example, a cerium doped yttrium aluminum garnet phosphor would be used to make cool white devices. Fumed silica is added to give the slurry the rheological properties needed for coating the substrate with a uniform layer. Fillers could be added optionally to tune mechanical, thermal, or optical properties. In a last step before coating the glass, a curing agent is added to the slurry. The curing agent could be a metal alkoxide such as titanium n-butoxide, or any other curing agent known to cure methoxy siloxanes. At the wafer / sheet level, the slurry is coated onto the hard substrate by either spray-coating, doctor-blading, tape-casting, slot-die coating, etc. The substrate can be a borosilicate glass. After coating, the siloxane precursor will react with the curing agent, and moisture 2022PF02477 - 27 - from the air, via hydrolysis and condensation to produce a cured film (PiM) on the glass. Final curing of the coating is achieved by heating the PiMoS to a temperature of 200°C. The formula of the fundamental repeat unit of the cured siloxane is [(CH3)SiO3 / 2]. The result is a highly crosslinked polysiloxane matrix with phosphor and filler particles contained therein. Once curing is complete the PiMoS can be evaluated at the wafer / sheet level or proceed to singulation into platelets. Properties such as surface roughness and delamination at the PiM and glass interface is often checked at the wafer / sheet of PiMoS first, and then the PiMoS is ready for the singulation process. The singulation process is carried out using saw dicing, using specified converter platelet dimensions. In the case of this study the converter platelets were diced to 1150µm x 1150µm. Data provided in this section were taken on both sheet level samples and converter platelet samples; sample type will be specified for each measurement. Trial 1 was conducted using siloxane powders (4 and 6µm blend) according to the formulation provided in Table 4a, where the substrate was a borosilicate glass. Slurry preparation and PiMoS tape-casting went very well. Cured PiMoS sheets were trimmed to 4” x 6” sheets and evaluated for surface roughness and delamination at the PiM-glass interface. While surface roughness of the PiM coating looked very good with an average surface roughness of 0.75 µm, delamination at the PiM-glass interface was unacceptable. Figures 17a and b show delamination at the PiM-glass interface for two different 200°C thermal cure profiles. The standard 200°C cure profile resulted in very high delamination at about 21%, and the slow thermal ramp rate 200°C cure profile resulted in lower, but still unacceptable delamination of about 14%; 1-5% delamination would be an acceptable range that is typical for fused silica filler. These data indicate that total substitution of fused silica powder with siloxane powder resulted in increased stress at the PiM-glass interface as indicated by the very high delamination values. While the stress level appears to decrease some by slowing the thermal ramp-rate of the 2022PF02477 - 28 - 200°C profile, the stress is still too high. Siloxane fillers are not an option for solving this problem when using this PiMoS processing method. Trial 2 was conducted using a 4µm modified siloxane powder according to the formulation provided in Table 4a, where the substrate was a borosilicate glass. The 4µm-HT410 powder (discussed in Figure 11b) was modified to display properties that are silica-like. Slurry preparation and PiMoS tape-casting went very well. Trial 2 PiMoS cast was trimmed to 4” x 6” sheets and evaluated for surface roughness and delamination. Figures 18a and b show delamination at the PiM-glass interface for two different 200°C thermal cure profiles. The standard 200°C cure profile resulted in slightly-high delamination of about 6.5%, and the slow thermal ramp-rate 200°C cure profile resulted in delamination of about 2.2%, which is excellent. In this case (Trial 2), total substitution of the fused silica filler with 4 µm modified siloxane filler looks good and the parts move forward in evaluation. Surface roughness for a Trial 2 PiMoS coupon (1” x 1”) was measured, and Figure 19 shows probability curves for surface roughness, with average values identified. The average surface roughness was 0.81µm which is acceptable for this study (<1.0 µm surface roughness is desired). Surface features and topography were evaluated use scanning electron microscopy (SEM), as shown in Figures 20a and 20b. Figure 20a shows an image with the modified siloxane particles (smaller particles) distributed in the matrix, while Figure 20b provides information regarding the topography of the surface. These data are consistent with what is expected for a HL PiMoS wavelength converter, so the parts move to the next stage of evaluation. Trial 2 PiMoS was singulated using saw dicing to prepare converter platelets for further evaluation; platelets were diced and cleaned. The main goal of this investigation is to identify filler materials that show potential in improving brightness for HL PiMoS optoelectronic devices. The next step in Trial 2 platelet evaluation is to measure 2022PF02477 - 29 - color coordinates and brightness (i.e., conversion efficiency) of the PiMoS platelets. Figures 21a and b provide the photometry results for Trial 2 PiMoS platelets: (a) color coordinates, and (b) conversion efficiency; data is plotted together with control HL PiMoS platelets that were measured at the same time. Color coordinates for Trial 2 with modified siloxane filler fall on the same color conversion line as the control HL PiMoS (see Figure 21a). Color steering for the Trial 2 formulation can be done by varying the PiM coating thickness. Figure 21b shows the conversion efficiency for Trial 2 PiMoS compared to the control HL PiMoS. Conversion efficiency (at the same Cx) is higher (brighter) for Trial 2 platelets with modified siloxane filler than for the control HL PiMoS. These data are encouraging for improving the brightness of HL PiMoS, but these data are for the isolated converter platelets and not for the LED optoelectronic device. One more property measurement to evaluate before moving to the LED optoelectronic device package-level testing is robustness, in particular, thermal stability at 250°C. Thermal stability at 250°C for control HL PiMoS containing fused silica filler is excellent; very stable delamination and color (Cx). Thermal stability at 250°C for Trial 2 PiMoS containing modified siloxane filler (silica-like) is shown in Figure 22 for delamination, and Figure 23 for color coordinate (Cx) stability; data are shown for both 200°C curing profiles. Figures 22a and b show that delamination can be decreased by using a slow thermal ramp rate 200°C cure profile. Figures 22a and 22b show that delamination is very stable for thermal storage at 250 °C for up to 1,188 hours. While the delamination starting values are significantly different for the two thermal profiles, the delamination level remains stable for 250°C storage. Figure 21b shows the case (slow thermal ramp rate 200°C curing profile) where the delamination remains very low following 250°C storage. 2022PF02477 - 30 - Figures 23a and 23b show that color coordinate Cx is very stable for thermal storage at 250°C for up to 1,188 hours. Figure 23b shows the case (slow thermal ramp rate 200°C curing profile to decrease stress) where delamination values are very low (Figure 22b), and both delamination and color coordinate Cx show excellent stability for 250°C thermal storage. Several screening tests were completed to evaluate the performance of modified 4µm siloxane filler (4µm-HT410) for HL PiMoS applications. PiMoS applications require balancing of various properties to achieve the desired results. In this case, the modified siloxane filler properties were tuned to obtain the desired results. Trial 2 PiMoS platelets have moved to the next stage and are currently being evaluatedin phosphor-converter LEDs.
Claims
2022PF02477 - 31 - CLAIMS 1. Modified siloxane obtainable by subjecting a siloxane to a heat treatment at a temperature of about 200 °C to about 500 °C in an oxygen-containing environment.
2. Method for modifying a siloxane, wherein the siloxane is subjected to a heat treatment at a temperature of about 200 °C to about 500 °C in an oxygen-containing environment.
3. The method according to claim 2, wherein the siloxane is polydimethylsiloxane.
4. The method according to claim 2, wherein the heat treatment is carried out at a temperature of about 200 °C to about 425 °C.
5. The method according to claim 4, wherein the heat treatment is carried out at a temperature of about 370 °C to about 410 °C.
6. The method according to claim 2, wherein the heat treatment is carried out at at least two different temperatures each selected within the range of about 200 °C to about 500 °C.
7. The method according to claim 2, wherein heating to the temperature of about 200°C to 500°C is carried out with a thermal ramp rate of about 1.0°C / min. to about 20°C / min.
8. The method according to claim 2, wherein the siloxane is maintained at the temperature of the heat treatment for about 0.5 hour to about 24 hours.
9. The method according to claim 2, wherein the oxygen- containing environment contains from about 5 vol.% to about 30 vol.% oxygen.
10. The method according to claim 9, wherein the oxygen- containing environment is air.2022PF02477 - 32 - 11. Use of the modified siloxane of claim 1 as a filler.
12. The use according to claim 11, wherein the filler is a filler employed in a wavelength converter. 13.converter is a phosphor-in-matrix wavelength converter or a phosphor- in-matrix-on-substrate wavelength converter.
14. Filler containing or consisting of the modified siloxane of claim 1.
15. The filler of claim 14 having the form of powders.
16. The filler of claim 14 having an average size of about 0.8µm to about 10µm.
17. Phosphor converted LED device having a wavelength converter containing a filler attached on its main emission surface, wherein the filler comprises or consists of the modified siloxane of claim 1 and / or the modified siloxane obtainable by the method of claim 2.
18. The phosphor converted LED device of claim 17, wherein the wavelength converter is selected from a phosphor-in-matrix-on- substrate or phosphor-in-matrix type wavelength converter.
Citation Information
Patent Citations
Pelletized silica
CA2653155A1
Spherical silicon dioxide micro powder as well as preparation method and application thereof
CN108083286A
Production method of active silica powder
CN115974089A
Silica and also epoxy resins
US20100286311A1
Photoresist patterning process supporting two step phosphor-deposition to form an LED matrix array
US20200203579A1